Method of manufacturing a composite tobacco sheet, aerosol-generating article and system

By preparing hollow cylindrical composite tobacco sheets, the matrix is ​​in direct contact with the aerosol generation matrix, which solves the problems of long volatilization time and insufficient aroma release in existing aerosol generation products, and achieves instant smoke production and good aerosol taste.

CN123147682APending Publication Date: 2026-11-24SHENZHEN FIRST UNION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510669144.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-22
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing aerosol-generating products take a long time to volatilize and produce aerosols under non-combustible conditions, resulting in insufficient aroma release and poor aerosol taste.

Method used

The method for preparing composite smoke sheets includes rolling, stacking and drying of solid slurry to form hollow cylindrical composite smoke sheets. The matrix is ​​in direct contact with the aerosol generation matrix, and heat is generated by heating elements to rapidly volatilize the aerosol.

Benefits of technology

It enables instant aerosol generation, full aroma release, good aerosol taste, and reduces user waiting time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123147682A_ABST
    Figure CN123147682A_ABST
Patent Text Reader

Abstract

The application provides a preparation method of a composite tobacco sheet, an aerosol generating article and a system. The composite tobacco sheet comprises a substrate capable of generating heat, which is configured in a hollow cylindrical shape. The composite tobacco sheet further comprises an aerosol generating substrate combined with the substrate and capable of being heated by the substrate to generate an aerosol. The preparation method of the composite tobacco sheet comprises: performing first rolling on a solid slurry to form a sheet-shaped body; stacking a sheet-shaped isolation piece, a sheet-shaped substrate and the sheet-shaped body, and performing second rolling to form a semi-finished product; drying the semi-finished product to obtain a composite tobacco sheet; and rolling the composite tobacco sheet into a hollow cylindrical shape. Through the above method, a cylindrical composite tobacco sheet can be prepared, which is convenient for users to use and can quickly generate an aerosol.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of heated non-combustible aerosol generation technology, and in particular to a method for preparing composite tobacco sheets, and an aerosol generation product and system having the composite tobacco sheets. Background Technology

[0002] Tobacco products (e.g., cigarettes, cigars, etc.) produce tobacco smoke by burning tobacco during use. Efforts are being made to replace these tobacco-burning products by creating products that release compounds without combustion. An example of such a product is an aerosol generating device that releases compounds by heating an aerosol generating product used in conjunction with it. This aerosol generating product may, for example, be tobacco or other non-tobacco products, which may or may not contain nicotine.

[0003] The aerosol generating device is equipped with a heating element that generates heat, which is then transferred to the aerosol generating product. When heated, the aerosol generating product volatilizes to produce aerosols. However, the existing aerosol generating products take a long time to volatilize and produce aerosols, resulting in insufficient aroma release and poor aerosol taste. Summary of the Invention

[0004] This application provides a method for preparing composite tobacco sheets, as well as an aerosol generating article and system having the composite tobacco sheets, to prepare a composite tobacco sheet capable of rapidly generating aerosols.

[0005] At least one embodiment of this application provides a method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix capable of generating heat, the matrix being constructed as a hollow column, and the composite tobacco sheet further comprising an aerosol generating matrix bonded to the matrix and capable of being heated by the matrix to generate aerosols, the method for preparing the composite tobacco sheet comprising:

[0006] The solid slurry is first rolled to form a sheet-like structure;

[0007] The sheet-shaped separator, the sheet-shaped substrate, and the sheet-shaped body are stacked and then subjected to a second roll forming to form a semi-finished product.

[0008] The semi-finished product is dried to obtain composite tobacco sheets;

[0009] The composite tobacco sheet is rolled into a hollow cylindrical shape.

[0010] In one embodiment, in the step of first rolling the solid slurry to form a sheet, the roller spacing ranges from 0.05 mm to 4.00 mm.

[0011] In one embodiment, after the step of stacking the sheet-like separator, the sheet-like substrate, and the sheet-like body, and performing a second rolling press to form a semi-finished product, the method further includes:

[0012] Remove the separator that is in contact with the substrate, stack another sheet onto the other surface of the substrate, stack two more separators onto the two sheets respectively, and perform a third roll press to bond the two sheets to both sides of the substrate.

[0013] In one embodiment, the roller spacing during the second rolling process is greater than the roller spacing during the third rolling process.

[0014] In one embodiment, the step of drying the semi-finished product to obtain composite tobacco sheets specifically includes:

[0015] Before drying the semi-finished product, the separator is removed and then the drying process begins.

[0016] In one embodiment, the step of drying the semi-finished product to obtain composite tobacco sheets specifically includes:

[0017] The drying temperature of the semi-finished product is 60℃~120℃, and the drying time is 1min~30mins.

[0018] In one embodiment, the thickness of the sheet is 0.05 mm to 4.00 mm.

[0019] In one embodiment, the thickness of the substrate is 0.005 mm to 0.05 mm.

[0020] In one embodiment, the thickness of the separator is 0.01 mm to 0.1 mm.

[0021] In one embodiment, the thickness of the composite tobacco sheet is 0.1 mm to 3.95 mm.

[0022] In one embodiment, the separator is aluminum foil, PI film, or cling film.

[0023] In one embodiment, the thickness of the composite tobacco sheet is 0.2 mm to 3.85 mm.

[0024] In one embodiment, the substrate is a porous and flexible magnetic foil material.

[0025] At least one embodiment of this application also provides an aerosol generating article, comprising:

[0026] The shell has a first section, a second section, and a third section arranged sequentially and interconnected along its length;

[0027] The composite tobacco sheet is prepared by the preparation method described in the above embodiments;

[0028] The composite smoke sheet is disposed in the first section, the second section is provided with an air inlet that communicates with the outside, the air inlet allows outside air to enter to cool the aerosol, and the third section is provided with a filter material for filtering the aerosol.

[0029] At least one embodiment of this application also provides an aerosol system, including the aerosol generating article described in the above embodiments, and an aerosol generating apparatus for containing at least a portion of the aerosol generating article;

[0030] When the aerosol generating product is housed in the housing chamber, the aerosol generating product and the aerosol generating device cooperate with each other to generate heat in the substrate.

[0031] The preparation method provided in the above embodiments first rolls the solid slurry to form a sheet, then stacks the sheet-shaped separator, sheet-shaped substrate, and sheet-shaped body in sequence for a second roll. After the second roll, a semi-finished product is formed. The semi-finished product is then dried, and a single-sided composite tobacco sheet is formed. Finally, the composite tobacco sheet is rolled up to form a hollow column shape, so as to resemble the shape of a traditional cigarette. Attached Figure Description

[0032] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.

[0033] Figure 1 This is a three-dimensional schematic diagram of a composite tobacco sheet provided in an embodiment of this application.

[0034] Figure 2 yes Figure 1 A cross-sectional schematic diagram of a composite tobacco sheet in one direction.

[0035] Figure 3 yes Figure 2 A three-dimensional schematic diagram of the matrix of composite tobacco sheets before rolling;

[0036] Figure 4 yes Figure 2 A three-dimensional schematic diagram of composite tobacco sheets before rolling;

[0037] Figure 5yes Figure 2 A schematic diagram of the structure of a composite tobacco sheet when it is used in a tubular body;

[0038] Figure 6 This is a schematic diagram of a method for preparing composite tobacco sheets according to an embodiment of this application;

[0039] Figure 7 This is a cross-sectional schematic diagram of a composite tobacco sheet provided in another embodiment of this application;

[0040] Figure 8 yes Figure 7 A three-dimensional schematic diagram of the composite tobacco sheets before rolling. Detailed Implementation

[0041] To facilitate understanding of this application, a more detailed description of this application will be provided below in conjunction with the accompanying drawings and specific embodiments.

[0042] One embodiment of this application provides a composite tobacco sheet 100, such as Figure 1 As shown, the composite tobacco sheet 100 can be wound into a cylindrical shape, the cylindrical structure having a first end 110 and a second end 120 disposed opposite to each other along its length, and a cavity 130 extending between the first end 110 and the first end 120.

[0043] like Figure 2 As shown, the composite tobacco sheet 100 includes a substrate 10 extending between a first end 110 and a second end 120. The substrate 10 is wound to form a hollow columnar shape, thereby creating the aforementioned cavity 130 around a hollow region formed by the substrate 10. The substrate 10 has a thickness direction (see...) Figure 3 The first surface 11 and the second surface 12 (in the X direction indicated by the arrow in the diagram) are positioned opposite each other. An aerosol generating matrix 20 is bonded to the first surface 11 or the second surface 12. The matrix 10 is used to generate heat, which can be used to heat the aerosol generating matrix 20. The aerosol generating matrix 20 volatilizes when heated, thus generating aerosols. It should be noted that the cavity 130 can serve as an airflow channel, allowing airflow carrying aerosols to flow within the cavity 130.

[0044] In the aforementioned composite tobacco sheet 100, the aerosol generating matrix 20 is bonded to the substrate 10, and the aerosol generating matrix 20 and the substrate 10 are in direct contact. Therefore, the heat generated by the substrate 10 can directly heat the aerosol generating matrix 20, allowing it to heat up rapidly and volatilize to generate aerosols, achieving an immediate inhalation effect. In other words, in the aerosol generating device used to heat the composite tobacco sheet 100, there is no need for a preheating stage; smoke can be produced rapidly and instantly upon startup or operation of the heating components, reducing user waiting time. Furthermore, the direct contact between the aerosol generating matrix 20 and the substrate 10 ensures thorough heating, and the substrate 10 heats the aerosol generating matrix 20 uniformly, resulting in a concentrated aerosol with full aroma release and a good aerosol taste.

[0045] In actual preparation, such as Figure 3 and Figure 4 As shown, a sheet-like substrate 10 can be provided first, then the aerosol generating matrix 20 can be bonded to the first surface 11 of the substrate 10, and finally the substrate 10 bonded with the aerosol generating matrix 20 can be rolled up.

[0046] like Figure 3 As shown, the substrate 10 also includes a plurality of through holes 13 connecting the first surface 11 and the second surface 12. When the aerosol generating matrix 20 is heated and volatilizes to generate aerosol, the aerosol will enter the cavity 130 through the through holes 13, and then escape from the port of the first end 110 along the cavity 130.

[0047] In specific usage, such as Figure 5 As shown, the composite tobacco sheet 100 can be assembled in a housing 200. When the composite tobacco sheet 100 is assembled in the housing 200, the composite tobacco sheet 100 and the housing 200 can form an aerosol generating article. The aerosol generating article is used in conjunction with a suitable aerosol generating device (not shown). The aerosol generating device is provided with a receiving chamber for accommodating at least a portion of the aerosol generating article. When the aerosol generating article is accommodated in the receiving chamber, the aerosol generating device and the aerosol generating article cooperate to generate heat in the substrate 10. At this time, the aerosol generating device and the aerosol generating article combine to form an aerosol forming system.

[0048] For example, a magnetic field generator can be provided in the aerosol generating device 100. The magnetic field generator can be an induction coil, and the substrate 10 is made of a conductive material, such as aluminum foil, copper foil, silver foil, etc., as described below, or any one of nickel-iron alloy, high-nickel alloy, stainless steel, or pure iron. When the aerosol-generated product is contained in the containing chamber, the controller of the aerosol generating device controls the flow of alternating current to the induction coil, thereby causing the induction coil to generate an alternating magnetic field. The alternating magnetic field penetrates the substrate 10, inducing eddy currents on the substrate 10, and then the substrate 10 generates heat under the action of the eddy currents.

[0049] The housing 200 includes a first section 210, a second section 220, and a third section 230 arranged sequentially and in fluid communication along its length. The first section 210 is used to hold the composite smoke sheet 100. The second section 220 is a cooling section for allowing external cold air to enter the housing 200 through the air inlet 221. The third section 230 is used to contain a substance 240 with a filtering function. The third section 230 is also provided with a filter nozzle for the user to inhale.

[0050] When the user inhales through the filter nozzle in the third section 230, the aerosol generated by the volatilization of the aerosol generating matrix 20 can enter the cavity 130 through the through hole 13, and then flow further along the cavity 130 to the second section 220, where it mixes with the external cold air for cooling. Finally, the cooled aerosol enters the third section 230 for filtration to remove some unwanted particles. The user can then inhale the cooled and filtered aerosol by inhaling through the filter nozzle in the third section 230.

[0051] In some embodiments, the through holes 13 are arranged in an array.

[0052] In some embodiments, the plurality of through holes 13 may be arranged in a circular, elliptical, racetrack-shaped, rectangular, triangular-hexagonal or other shapes.

[0053] In some embodiments, the plurality of through holes 13 may be arranged in a centrally symmetrical or axisymmetric pattern.

[0054] Furthermore, in some embodiments, the porosity of the plurality of through holes 13 on the substrate 10 is 20%-50%. In some preferred embodiments, the porosity of the plurality of through holes 13 on the substrate 10 is 20%, 25%, 30%, 35%, 40%, 45%, or 50%. This allows aerosols to pass smoothly through the through holes 13 so that the aerosols can flow into the cavity 130.

[0055] In some embodiments, the through-hole 13 is formed by machining or chemical etching. Further in some embodiments, machining includes drilling or laser processing.

[0056] In some embodiments, the thermal conductivity of the substrate 10 is at least 25 W / m·K. In one embodiment of this application, the thermal conductivity of the substrate 10 is 25 W / m·K, 30 W / m·K, 32 W / m·K, 35 W / m·K, 40 W / m·K, or 45 W / m·K.

[0057] In some embodiments, the thickness of the substrate 10 is between 0.005 mm and 0.05 mm. Preferably, the thickness of the substrate 10 is 0.006 mm, 0.01 mm, 0.012 mm, 0.015 mm, 0.020 mm, 0.018 mm, 0.02 mm, 0.025 mm, or 0.03 mm. Within this range, the substrate 10 can maintain a certain structural strength to support the aerosol-forming matrix layer 20 bonded thereto, while the thickness of the substrate 10 also allows it to maintain a certain degree of flexibility, enabling it to be rolled from a sheet into a column shape.

[0058] In some embodiments, the substrate 10 may include a sensitive metal or alloy that can be penetrated by a magnetic field and generate heat. When the substrate 10 is in a changing magnetic field, according to the law of electromagnetic induction, the magnetic flux through the substrate 10 changes, generating an induced electromotive force (EMF) within the substrate 10. Since the substrate 10 is a conductor with relatively low resistance, a closed loop is formed inside the substrate 10 under the influence of the induced EMF, generating induced eddy currents. As the eddy currents flow inside the substrate 10, electrical energy is converted into heat energy, causing the temperature of the substrate 10 to rise. This heat then heats the aerosol-forming matrix layer 12.

[0059] In some embodiments, the substrate 10 may include a soft magnetic alloy. Soft magnetic alloys, with their core advantages of high electromagnetic response, low loss, and high saturation magnetization, are widely used in energy conversion and signal processing.

[0060] In some specific embodiments, the substrate 10 may include magnetic foil materials such as aluminum foil, copper foil, and silver foil, or any one of nickel-iron alloy, high-nickel alloy, stainless steel, or pure iron.

[0061] In some embodiments, the aerosol-generating matrix layer 20 includes tobacco extract. The tobacco extract can be obtained by extracting extracts from tobacco leaves and flowers using a solvent, then extracting the extracts with ethanol, followed by drying, dehydration, desalting, and cooking of the raw materials, adding an extract with a special aroma, and performing ultrasonic-assisted extraction to finally obtain a tobacco extract with a specific flavor. In one embodiment of this application, the tobacco extract is mainly used for tobacco flavoring, which can enhance the aroma, reduce off-flavors, and improve cigarette quality. Its aroma is realistic and natural, making it an excellent raw material for cigarette flavoring. Furthermore, tobacco extract can also be used in daily-use fragrances to provide unique aromas and flavors.

[0062] In some embodiments, the main components of tobacco extract include furfuryl alcohol, benzyl alcohol, phytol, solanone, β-turfayne, β-ionone, hexahydrofarnesone, diene, daidzeinone, dihydroactinolone, isopentenone, indole, etc.

[0063] In some embodiments, the aerosol generating matrix 20 comprises at least one of tobacco-based and tea-based materials; or at least one of carbon powder and ceramic beads.

[0064] One embodiment of this application also provides a method for preparing the composite tobacco sheet 100 described in the above embodiment, such as... Figure 6 As shown, the preparation method includes:

[0065] S10, the solid slurry is first rolled to form a sheet;

[0066] S20, the sheet-shaped separator, the sheet-shaped substrate, and the sheet-shaped body are stacked and then rolled a second time to form a semi-finished product;

[0067] S30, the semi-finished product is dried to obtain composite tobacco sheets;

[0068] S40, the composite tobacco sheet is rolled into a hollow cylindrical shape.

[0069] Specifically, the components used to form the aerosol generation matrix 20 are first prepared into a solid slurry. A solid slurry is a mixture with a certain degree of fluidity, consisting of solid particles and a suitable amount of liquid. However, the solid slurry also needs to maintain a certain level of stability to ensure that the solid particles remain relatively stably dispersed in the liquid, avoiding sedimentation, agglomeration, or stratification. The stability of the slurry can be improved by adding appropriate dispersants, stabilizers, and other additives.

[0070] Then, a roller press is used to perform a first roller press on the solid slurry to compress it into a sheet. During the roller press, the roller spacing of the roller press is first adjusted to a preset spacing so that the sheet formed after the solid slurry is rolled is within a preset thickness range.

[0071] A sheet-like substrate 10 of a predetermined thickness is placed in the feed trough of a roller press, and then a sheet-like solid slurry is applied to the first surface 11 or the second surface 12 of the substrate 10. The substrate 10 will subsequently be rolled into a cylindrical shape. To facilitate subsequent processing of the substrate 10, its thickness can be determined based on its subsequent processes. Furthermore, the substrate 10 may also possess a certain degree of flexibility. To prevent breakage of the substrate 10 during the roller pressing process, a sheet-like separator of a predetermined thickness is also required. Before placing the substrate 10 into the feed trough of the roller press, the sheet-like separator is placed in the feed trough, and then the substrate 10 is applied to the sheet-like separator, thereby preventing breakage of the substrate 10 during the roller pressing process. Additionally, it also prevents the solid slurry from sticking to the rollers of the roller press during the roller pressing process.

[0072] Specifically, if a solid slurry is rolled onto the first surface 11 of the substrate 10, the spacer and the second surface 12 of the substrate 10 are stacked together, that is, the second surface 12 of the substrate 10 and the spacer are in contact with each other. If a solid slurry is rolled onto the second surface 12 of the substrate 10, the spacer and the first surface 11 of the substrate 10 are stacked together.

[0073] Start the roller pressing equipment for a second roller pressing to press the sheet-like solid slurry onto the substrate 10 to form a semi-finished product.

[0074] The first and second rolling processes can use the same rolling equipment or different rolling equipment. For example, a simpler rolling equipment can be used for the first rolling to roll the solid slurry into sheets, while the rolling equipment used in mass production can be used for the second rolling to prepare the aforementioned semi-finished product.

[0075] In the semi-finished product formed after the second rolling process, the solid slurry can be bonded to one of the first surface 11 and the second surface 12 of the matrix 10. At this time, the solid slurry contains a large amount of moisture, and the aerosol generating matrix 20 is not heated sufficiently, resulting in a poor-tasting aerosol. Therefore, the semi-finished product needs to be dried to evaporate some of the moisture in the solid slurry, so that the moisture content in the solid slurry reaches a preset value, thereby forming composite tobacco sheets. This allows the aerosol generating matrix 20 to be fully heated to produce aerosols with a better taste.

[0076] The resulting composite tobacco sheet 100 is then rolled into a hollow cylindrical shape, at which point the composite tobacco sheet 100 resembles the shape of a traditional cigarette.

[0077] It should be noted that if the provided substrate 10 is a whole sheet, then there are multiple substrate units on the substrate 10. The composite tobacco sheet formed after drying is also a whole. In this case, the composite tobacco sheet needs to be cut along the shape of the substrate unit, and then the cut composite tobacco sheet is rolled up to form the above-mentioned single composite tobacco sheet 100.

[0078] It should be noted that the composite tobacco sheet formed after the second rolling is a single-sided composite tobacco sheet, that is, the aerosol generating matrix 20 is bonded to one of the first surface 11 and the second surface 12 of the substrate 10.

[0079] In some embodiments, the single-sided composite tobacco sheet formed by the above preparation steps has a thickness of 0.1 mm to 3.95 mm.

[0080] In some embodiments, the separator is removed before drying the semi-finished product to avoid the separator affecting the evaporation of moisture in the solid slurry during drying.

[0081] In some embodiments of the composite tobacco sheet, the roller spacing of the rolling mill is between 0.05 mm and 4.00 mm during the first rolling process to control the thickness of the composite tobacco sheet 100 within a certain range. For example, if the roller spacing of the rolling mill is set to 2 mm, the thickness of the final composite tobacco sheet 100 will not exceed 2 mm. In some embodiments, in the above-described preparation method, before the first rolling process, the roller spacing of the rolling mill is set between 0.05 mm and 4.00 mm.

[0082] In some embodiments, the single-sided composite tobacco sheet has a thickness of 0.1 mm to 3.95 mm.

[0083] One embodiment of this application provides a composite tobacco sheet 100a, such as Figure 7 and Figure 8 As shown, compared to the composite tobacco sheet 100 in the above embodiments, the composite tobacco sheet 100a provided in this embodiment has a first aerosol generating matrix 20a bonded to the first surface 11 of the substrate 10, and a second aerosol generating matrix 20b bonded to the second surface 12. When the substrate 10 generates heat, both the first aerosol generating matrix 20a and the second aerosol generating matrix 20b can be heated and volatilized to generate aerosols, thereby increasing the aerosol concentration.

[0084] In practical use, when the user inhales, the aerosol generated by the first aerosol generating matrix 20a enters the cavity 130 through the through hole 13; while the aerosol generated by the second aerosol generating matrix 20b evaporates directly into the cavity 130; after the aerosol generated by the first aerosol generating matrix 20a and the aerosol generated by the second aerosol generating matrix 20b are mixed, they flow together along the airflow channel in the shell 200 to the filter nozzle in the third section 230.

[0085] Since both sides of the substrate 10 are bonded with aerosol generating matrix, the substrate 10 can simultaneously heat the aerosol generating matrix on both sides to generate aerosol, and the resulting composite tobacco sheet is a double-sided composite tobacco sheet.

[0086] In some embodiments, the composition of the first aerosol generating matrix 20a may be the same as or different from the composition of the second aerosol generating matrix 20b.

[0087] Based on the aforementioned composite tobacco sheet 100a, the above preparation method further includes:

[0088] After the step of stacking the sheet-like separator, the sheet-like substrate, and the sheet-like body, and performing a second rolling press to form a semi-finished product, the method further includes:

[0089] Remove the separator that is in contact with the substrate, stack another sheet onto the other surface of the substrate, stack two more separators onto the two sheets respectively, and perform a third roll press to bond the two sheets to both sides of the substrate.

[0090] Specifically, after the second rolling, a semi-finished product of single-sided composite tobacco sheet can be obtained.

[0091] Then, another sheet-like solid slurry is rolled onto the other surface of the substrate 10. For example, after the second rolling, if the single-sided composite tobacco sheet is prepared by rolling solid slurry on the first surface 11 of the substrate 10, then another sheet-like solid slurry is laminated onto the second surface 12 of the substrate 10. Similarly, if the single-sided composite tobacco sheet is prepared by rolling solid slurry on the second surface 12 of the substrate 10, then another sheet-like solid slurry is laminated onto the first surface of the substrate 10.

[0092] Simultaneously, the separators on the single-sided composite tobacco sheet obtained after the second rolling are removed, and two other new separators are respectively laminated onto the solid slurry on both sides of the substrate 10, that is, the solid slurry on both sides of the substrate 10 is located between the two new separators. After lamination, a third rolling is performed. After the rolling is completed, a semi-finished double-sided composite tobacco sheet is obtained. At this time, the solid slurry on both sides of the substrate is bonded to the first surface 11 and the second surface 12 of the substrate 10, respectively. However, since it has not been dried yet, the semi-finished double-sided composite tobacco sheet is obtained, and the water content will be relatively high.

[0093] Next, remove the separators on both sides and put the semi-finished double-sided composite tobacco sheet into a drying oven for drying, so that at least part of the moisture in the semi-finished product evaporates to reach the preset moisture content requirement. After drying, the double-sided composite tobacco sheet can be obtained. Finally, roll the double-sided composite tobacco sheet into a hollow cylindrical shape to obtain the above-mentioned composite tobacco sheet 100a.

[0094] In some embodiments, before drying, the two spacers on both sides of the substrate 10 are removed to prevent the spacers from affecting the evaporation of moisture during drying.

[0095] In some embodiments, the above preparation method further includes:

[0096] The roller spacing during the second rolling process is greater than the roller spacing during the third rolling process.

[0097] Roller spacing refers to the distance between the two rollers of a rolling mill. The smaller the roller spacing, the thinner the final composite tobacco sheet; conversely, the larger the roller spacing, the thicker the final composite tobacco sheet. Therefore, shortening the roller spacing during the third rolling process can result in a thinner double-sided composite tobacco sheet.

[0098] In some specific embodiments, when the rolling equipment performs the second rolling, the roller spacing of the rolling equipment is between 0.05mm and 4.00mm, and when the rolling equipment performs the third rolling, the roller spacing of the rolling equipment is between 0.15mm and 3.90mm.

[0099] In some embodiments, the double-sided composite tobacco sheet prepared by the above embodiments has a thickness of 0.2 mm to 3.85 mm. Within this thickness range, the volatilization of the first aerosol generating matrix 20a and the second aerosol generating matrix 20b can produce aerosols with better taste.

[0100] In some embodiments, when drying the semi-finished composite tobacco sheet, the drying temperature is 60°C to 120°C and the drying time is 1 min to 30 mins, so that the composite tobacco sheet has a suitable moisture content.

[0101] In some embodiments, the sheet-like separator in the above embodiments may be made of non-adhesive materials such as aluminum foil, PI film, or cling film.

[0102] In some embodiments, the sheet-like separator in the above embodiments needs to have a suitable thickness. If the thickness is too thin, damage to the substrate 10 cannot be avoided during the rolling process; while if the thickness of the separator is too thick, the separator is prone to displacement during rolling, resulting in uneven distribution of the slurry after rolling. Therefore, in some embodiments, the thickness of the separator is between 0.01 mm and 0.1 mm.

[0103] In some embodiments, the sheet formed after the first roll pressing of the solid slurry has a thickness of 0.05 mm to 4.00 mm.

[0104] In some embodiments, the composite tobacco sheet has a moisture content of less than 12%, specifically, it may be 5%, 8%, or 10%, and the moisture content can be measured by a rapid moisture analyzer.

[0105] It should be noted that the preferred embodiments of this application are given in the specification and accompanying drawings, but are not limited to the embodiments described in this specification. Furthermore, those skilled in the art can make improvements or modifications based on the above description, and all such improvements and modifications should fall within the protection scope of the appended claims.

Claims

1. A method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix capable of generating heat, the matrix being constructed as a hollow column, the composite tobacco sheet further comprising an aerosol generating matrix bonded to the matrix and capable of being heated by the matrix to generate aerosols, characterized in that, The method for preparing the composite tobacco sheet includes: The solid slurry is first rolled to form a sheet-like structure; The sheet-shaped separator, the sheet-shaped substrate, and the sheet-shaped body are stacked and then subjected to a second roll forming to form a semi-finished product. The semi-finished product is dried to obtain composite tobacco sheets; The composite tobacco sheet is rolled into a hollow cylindrical shape.

2. The preparation method according to claim 1, characterized in that, In the step of first rolling the solid slurry to form a sheet, the roller spacing ranges from 0.05 mm to 4.00 mm.

3. The preparation method according to claim 1, characterized in that, After the step of stacking the sheet-like separator, the sheet-like substrate, and the sheet-like body, and performing a second rolling press to form a semi-finished product, the method further includes: Remove the separator that is in contact with the substrate, stack another sheet onto the other surface of the substrate, stack two more separators onto the two sheets respectively, and perform a third roll press to bond the two sheets to both sides of the substrate.

4. The preparation method according to claim 3, characterized in that, The roller spacing during the second rolling process is greater than the roller spacing during the third rolling process.

5. The preparation method according to claim 1, characterized in that, The step of drying the semi-finished product to obtain composite tobacco sheets specifically includes: Before drying the semi-finished product, the separator is removed and then the drying process begins.

6. The preparation method according to claim 1, characterized in that, The step of drying the semi-finished product to obtain composite tobacco sheets specifically includes: The drying temperature of the semi-finished product is 60℃~120℃, and the drying time is 1min~30mins.

7. The preparation method according to claim 1, characterized in that, The thickness of the sheet-like body is 0.05 mm to 4.00 mm.

8. The preparation method according to claim 1, characterized in that, The thickness of the substrate is 0.005 mm to 0.05 mm.

9. The preparation method according to claim 1, characterized in that, The thickness of the isolation element is 0.01mm to 0.1mm.

10. The preparation method according to claim 1, characterized in that, The thickness of the composite tobacco sheet is 0.1 mm to 3.95 mm.

11. The preparation method according to claim 1, characterized in that, The insulating material is aluminum foil, PI film, or cling film.

12. The preparation method according to claim 3, characterized in that, The thickness of the composite tobacco sheet is 0.2mm to 3.85mm.

13. The preparation method according to claim 1, characterized in that, The substrate is a porous and flexible magnetic foil material.

14. An aerosol-generating product, characterized in that, include: The shell has a first section, a second section, and a third section arranged sequentially and interconnected along its length; The composite tobacco sheet is prepared by the preparation method according to any one of claims 1-13; The composite smoke sheet is disposed in the first section, the second section is provided with an air inlet that communicates with the outside, the air inlet allows outside air to enter to cool the aerosol, and the third section is provided with a filter material for filtering the aerosol.

15. An aerosol generation system, characterized in that, Includes the aerosol generating article as described in claim 14, and an aerosol generating apparatus for containing at least a portion of the aerosol generating article; When the aerosol generating product is housed in the housing chamber, the aerosol generating product and the aerosol generating device cooperate with each other to generate heat in the substrate.