Method of manufacturing a composite tobacco sheet, aerosol-generating article and system
By setting aerosol generation matrix layers on both sides of the matrix layer and using thermal conduction or electromagnetic induction heating, the problems of long aerosol volatilization time and insufficient aroma release in existing aerosol generation products are solved, achieving rapid volatilization and sufficient aroma aerosol generation effect.
Patent Information
- Application Number
- CN202510669494.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-22
- Publication Date
- 2026-11-24
AI Technical Summary
Existing aerosol-generated products have long aerosol volatilization time under non-combustion conditions, resulting in insufficient aroma release and poor aerosol taste.
Aerosol generation matrix layers are set on both sides of the matrix layer, and composite tobacco sheets are prepared by double-sided grouting process. The thermal conductivity of the matrix layer is used to heat the aerosol generation matrix layer to rapidly volatilize the aerosol. The matrix layer is heated by thermal conduction or electromagnetic induction.
It shortens the aerosol evaporation time, fully releases the aroma, and provides a good aerosol taste, thus improving the user experience.
Smart Images

Figure CN123147683A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of heated non-combustible aerosol generation technology, and in particular to a method for preparing composite tobacco sheets, as well as an aerosol generation product and system having the composite tobacco sheets. Background Technology
[0002] Tobacco products (e.g., cigarettes, cigars, etc.) produce tobacco smoke by burning tobacco during use. Efforts are being made to replace these tobacco-burning products by creating products that release compounds without combustion. An example of such a product is an aerosol generating device that releases compounds by heating an aerosol generating product used in conjunction with it. This aerosol generating product may, for example, be tobacco or other non-tobacco products, which may or may not contain nicotine.
[0003] The aerosol generating device is equipped with a heating element that generates heat, which is then transferred to the aerosol generating product. When heated, the aerosol generating product volatilizes to produce aerosols. However, the existing aerosol generating products take a long time to volatilize and produce aerosols, resulting in insufficient aroma release and poor aerosol taste. Summary of the Invention
[0004] This application provides a method for preparing composite tobacco sheets, as well as an aerosol generating article and system having the composite tobacco sheets, wherein an aerosol generating matrix layer is provided on both sides of the matrix layer, thereby shortening the volatilization time of the aerosol and making the aroma release of the aerosol generating matrix more complete, thereby improving the taste of the aerosol.
[0005] At least one embodiment of this application provides a method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix layer and an aerosol-generating matrix layer bonded to both sides of the matrix layer and capable of being heated to generate an aerosol, the preparation method comprising:
[0006] A mold is provided, the mold including a receiving groove;
[0007] Slurry is poured into the receiving tank, and the substrate layer is placed on the upper side of the slurry so that the slurry forms an aerosol matrix layer on one side of the substrate layer;
[0008] The mold is placed in a drying oven for the first drying process.
[0009] Continue pouring slurry into the receiving tank to form an aerosol matrix layer on the other side of the substrate layer;
[0010] The mold is placed in the drying oven for a second drying process.
[0011] In some embodiments, after the step of placing the mold in a drying oven for the first drying, the aerosol matrix layer has a moisture content of 50% to 60%.
[0012] In some embodiments, after the step of placing the mold into the drying oven for a second drying, the moisture content of the aerosol matrix layer is 10% to 20%.
[0013] In some embodiments, the thickness of the substrate layer is 0.01 mm to 0.30 mm.
[0014] In some embodiments, the substrate layer has through holes connecting its two sides.
[0015] In some embodiments, there are multiple through holes, and the area ratio of the holes is [missing information]. In some embodiments, the substrate layer is a metal sheet.
[0016] In some embodiments, the metal sheet is made of copper, iron, aluminum, tin, stainless steel, or alloys thereof.
[0017] In some embodiments, the surface of the substrate layer is roughened.
[0018] In some embodiments, the thickness of the composite tobacco sheet is 0.1 mm to 2.0 mm.
[0019] In some embodiments, the pulp comprises tobacco or natural plant materials, fibers, adhesives, flavorings, and smoke-generating agents.
[0020] In some embodiments, the two aerosol matrix layers in the composite tobacco sheet have different thicknesses.
[0021] In some embodiments, the concentration of the slurry is 10% to 30%.
[0022] At least one embodiment of this application also provides an aerosol generating article, comprising:
[0023] Multiple composite tobacco sheets, wherein the composite tobacco sheets are prepared by the preparation method described in the above embodiments;
[0024] A carrier is used to support the composite tobacco sheets, and a plurality of the composite tobacco sheets are held on the carrier.
[0025] In some embodiments, the carrier is configured as a hollow box-shaped body, the hollow region of the box-shaped body being used to receive the aerosol, the box-shaped body having an air inlet for air to enter the hollow region and an air outlet for the aerosol to escape from the box-shaped body.
[0026] At least one embodiment of this application also provides an aerosol generation system, comprising:
[0027] The aerosol-generated products described in the above embodiments;
[0028] An aerosol generating apparatus is provided with a receiving chamber for containing the aerosol generating article. When the aerosol generating article is contained in the receiving chamber, the aerosol generating apparatus and the aerosol generating article cooperate to generate heat in the substrate layer.
[0029] The aerosol generating device further includes a suction nozzle, which defines an outlet for aerosols to escape from the aerosol generating device.
[0030] The preparation method of the double-sided grouting process provided in the above embodiments can prepare a sheet-like composite tobacco sheet with aerosol generation matrix layers on both sides of the matrix layer. When the aerosol generation matrix is heated, the aerosol generation matrix can quickly volatilize to generate aerosols, the aroma is fully released, and the generated aerosols have a good taste. Attached Figure Description
[0031] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.
[0032] Figure 1 This is a three-dimensional schematic diagram of a composite tobacco sheet provided in an embodiment of this application;
[0033] Figure 2 yes Figure 1 A three-dimensional schematic diagram of the matrix layer of composite tobacco sheets in one direction;
[0034] Figure 3 This is a schematic diagram of the steps in a method for preparing composite tobacco sheets according to an embodiment of this application;
[0035] Figure 4 This is an embodiment provided by this application. Figure 3 A schematic diagram of the mold and casting equipment used in the preparation method;
[0036] Figure 5 This is a schematic diagram of the structure of an aerosol generation system provided in an embodiment of this application;
[0037] Figure 6 This is a schematic diagram of the structure of an aerosol-generated article provided in an embodiment of this application. Detailed Implementation
[0038] To facilitate understanding of this application, a more detailed description of this application will be provided below in conjunction with the accompanying drawings and specific embodiments.
[0039] One embodiment of this application provides a composite tobacco sheet capable of generating an aerosol by heating. In some embodiments, part or all of the composite tobacco sheet is intended to be consumed by a user during use by heating.
[0040] For example Figure 1 A schematic diagram of a composite tobacco sheet 100 according to one embodiment is shown; in this embodiment, the composite tobacco sheet 100 is substantially constructed in a sheet-like shape. For example, in some alternative embodiments, the composite tobacco sheet 100 has a length of approximately 1 to 100 cm, a width of 2 to 30 mm, and a thickness of approximately 0.1 mm to 2 mm. Figure 1 In one embodiment, the composite tobacco sheet 100 is configured as a square shape; or in some other variations, the composite tobacco sheet 100 is configured as a circular, elliptical, trapezoidal, polygonal, or other shapes.
[0041] In some embodiments, the areal density of the composite tobacco sheet 100 is 100–600 g / m³. 2 .
[0042] In some embodiments, the tensile strength of the composite smoke sheet 100 is greater than 1.5 kN / m.
[0043] exist Figure 1 In some embodiments, the composite tobacco sheet 100 has a laminated structure and is configured to include multiple layers formed by lamination. For example, in Figure 1 In the middle, the composite tobacco sheet 100 includes:
[0044] A first aerosol generating matrix layer 110, a substrate layer 120, and a second aerosol generating matrix layer 130 are arranged in a stacked or laminated manner, with the substrate layer 120 located between the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 120.
[0045] Please continue reading. Figure 1 In conjunction with reference Figure 2 The substrate layer 120 has a thickness direction ( Figure 2 (In the direction of the middle arrow X) the first surface 121 and the second surface 122 are set opposite to each other, the first aerosol generating matrix layer 110 is bonded to the first surface 121, and the second aerosol generating matrix is bonded to the second surface 122.
[0046] In some embodiments, the substrate layer 120 is thermally conductive. In one specific embodiment, for example, the substrate layer 120 comprises a metallic or non-metallic material suitable for having a suitable high thermal conductivity; in one specific embodiment, the thermal conductivity of the substrate layer 120 is at least 25 W / m·K, preferably or at least 80 W / m·K;
[0047] In some embodiments, the substrate layer 120 may be in the form of a metal sheet, and the material of the substrate layer 120 may include copper, iron, aluminum, tin, stainless steel, or an alloy containing at least one of them. In use, the substrate layer 130 may be heated directly or indirectly, for example, by means of thermal conduction or electromagnetic induction, in turn heating the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 to generate aerosols.
[0048] Since the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 are both bonded to the matrix layer 120, and both the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 are in direct contact with the matrix layer 120, the heat on the matrix layer 120 can directly heat the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130. This allows the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 to be heated quickly and volatilize in time to generate aerosols, achieving an immediate inhalation effect, reducing the user's waiting time, and producing a rich aerosol concentration with full aroma release and good aerosol taste.
[0049] In some embodiments, the substrate layer 120 has a thickness of 0.01 mm to 0.3 mm; and in some embodiments, the substrate layer 120 is rigid or hard, and is not easily bent or rolled. The rigidity of the substrate layer 120 allows the composite tobacco sheet 100 to have a flat sheet structure. In some embodiments, the substrate layer 120 can serve as a carrier structure for the aerosol generation matrix layer, supporting and bearing the aerosol generation matrix layer, which can be attached, bonded, or coated onto the surface of the substrate layer 120.
[0050] In some embodiments, the substrate layer 120 is made of any one of the following materials: metal sheet, aluminum foil, magnetic foil, paper, non-woven fabric, and nylon fabric.
[0051] When the substrate layer 120 is made of metal sheet, aluminum foil or magnetic foil, the substrate layer 120 can generate eddy currents through electromagnetic induction, thereby generating heat on the substrate layer 120.
[0052] Specifically, the aerosol generating device used in conjunction with the composite tobacco sheet 100 is equipped with a magnetic field generator, which can be an induction coil. An alternating current is passed through the induction coil, thereby generating a changing magnetic field. When the composite tobacco sheet 100 is placed in the aerosol generating device, the magnetic field generated by the induction coil can pass through the substrate layer 120, thereby inducing eddy currents on the substrate layer 120.
[0053] When the substrate layer 120 is made of paper, non-woven fabric, or nylon fabric, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 can generate aerosols through microwave heating, light heating, or infrared heating. Specifically, an element for generating microwaves, infrared rays, or light can be provided in the aerosol generating device used in conjunction with the composite tobacco sheet 100. The generated microwaves, light, or infrared rays irradiate the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130. Since the composite tobacco sheet 100 has a relatively thin thickness, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 can quickly volatilize and generate aerosols under the irradiation of microwaves, infrared rays, or light. Furthermore, since aerosol generating matrix layers are provided on both sides of the substrate layer 120, the aroma of the aerosol generating matrix is fully released, resulting in a better taste of the generated aerosol.
[0054] In some embodiments, the first surface 121 and / or the second surface 122 of the substrate layer 120 are non-smooth; for example, the first surface 121 and / or the second surface 122 are rough; for example, the surface of the substrate layer 120 of the metal or alloy foil is surface-processed by at least one process such as corona, electrochemical etching, indentation, or sanding, thereby forming a rough surface on the surface of the substrate layer 120, such as a sanded surface; the rough surface of the substrate layer 120 is advantageous for maintaining a tight bond with the first aerosol generating matrix layer 110 and / or the second aerosol generating matrix layer 130.
[0055] In some embodiments, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 can be used to refer to a matrix capable of releasing volatile compounds that can form aerosols. The volatile compounds can be released to generate the aerosol by heating the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130. In some general embodiments, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 are or may include solids at room temperature.
[0056] In some embodiments, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 may include one or more of the following: vanilla leaves, tobacco leaves, homogenized tobacco, expanded tobacco, powder, granules, fragments, strips, or flakes; or, the solid first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 may contain additional tobacco or non-tobacco volatile flavor compounds to be released when the matrix is heated.
[0057] In some specific embodiments, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 may include an active substrate; the active substrate includes or is derived from one or more plant products or components thereof; for example, in some specific embodiments, the active substrate includes plant leaves, bark, fibrous tissue, stems, roots, petals, fruits, etc.; for example, in one specific embodiment, the active substrate includes or is derived from one or more plant varieties or their components, derivatives, or extracts, and the plant variety is tobacco. For example, in one specific embodiment, the active substrate includes a mixture of tobacco and plants such as traditional Chinese medicine. The active substrate may include tobacco or tobacco-containing materials; for example, the active substrate may include any of the following: tobacco leaves, tobacco vein fragments, reconstituted tobacco, homogenized tobacco, extruded tobacco, tobacco slurry, cast tobacco, and expanded tobacco.
[0058] In some optional embodiments, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 further include: a flavoring agent; the flavoring agent may comprise volatile aroma components. For example, in typical embodiments, the flavoring agent may provide an aroma selected from menthol, lemon, vanilla, orange, wintergreen, cherry, and cinnamon; the flavoring agent may include volatile tobacco flavoring compounds released from the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 upon heating.
[0059] In some optional embodiments, the first aerosol-generating matrix layer 110 and the second aerosol-generating matrix layer 130 further include an aerosol forming agent or a smoke generator; the aerosol forming agent or smoke generator contributes to the densification and stabilization of aerosol formation during use. In some specific embodiments, the aerosol forming agent or smoke generator is or includes at least one of glycerol, glycerol, propylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, etc.
[0060] In some optional embodiments, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 further include: an adhesive; the adhesive promotes the bonding of the components in the aerosol generating matrix 120 during use; for example, in some specific embodiments, the adhesive is or includes at least one of gum arabic, casein, dextrin, sodium carboxymethyl cellulose, starch, polyvinyl alcohol, guar gum, etc.
[0061] In some optional embodiments, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 further include reinforcing fibers; the reinforcing fibers typically have a higher fiber strength than the tobacco plant fibers in the active substrate, thereby enhancing the strength and plasticity of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 during use. For example, in some specific embodiments, the reinforcing fibers include at least one of coniferous wood fibers, broadleaf wood fibers, hemp fibers or flax fibers, bamboo fibers, etc.
[0062] In some embodiments, the thicknesses of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 may be the same or different.
[0063] In one specific embodiment, the substrate layer 120 is heated by electromagnetic induction. When the composite tobacco sheet 100 is placed into the aerosol generating device used with it, the induction coil in the aerosol generating device will generate a changing magnetic field under the action of alternating current. This changing magnetic field will pass through the substrate layer 120, thereby generating induced eddy currents on the substrate layer 120, and then generating heat under the action of the eddy currents.
[0064] At this time, when the composite tobacco sheet 100 is placed into the aerosol generating device, if the second surface 122 of the substrate layer 120 faces the induction coil, the thickness of the second aerosol generating matrix layer 130 bonded to the second surface 122 is not greater than the thickness of the first aerosol generating matrix layer 110 bonded to the first surface 121, so as to avoid the first aerosol generating matrix layer 110 being overheated and producing a burnt taste.
[0065] It is easy to understand that when the composite tobacco sheet 100 is placed into the aerosol generating device, if the first surface 121 of the substrate layer 120 faces the induction coil, the thickness of the first aerosol generating matrix layer 110 bonded to the first surface 121 is not greater than the thickness of the second aerosol generating matrix layer 120 bonded to the second surface 121, so as to avoid the second aerosol generating matrix layer 120 being overheated and producing a burnt taste.
[0066] In some embodiments, such as Figure 2 As shown, the substrate layer 120 also includes a plurality of through holes 123 connecting the first surface 121 and the second surface 122. By providing the through holes 123, aerosols generated by the heating and volatilization of the first aerosol generating matrix layer 110 or the second aerosol generating matrix layer 130 can escape through the through holes 123. In this embodiment, the substrate layer 120 is square, so the plurality of through holes 123 can be arranged in a rectangular array. In some other embodiments, the substrate layer 120 is circular, so the plurality of through holes 123 can be arranged in a ring array.
[0067] In some embodiments, the sum of the opening areas of the plurality of through holes 123 occupies 30-50% of the surface area of the first surface 121 or the second surface 122. Furthermore, it should be noted that the design of the porosity on the substrate layer 120 and the distribution of the through holes 123 can also adjust the temperature field distribution on the substrate layer 120. For example, providing through holes 123 in high-temperature regions can effectively prevent heat concentration in the substrate layer 120 in those regions; furthermore, by adjusting the porosity in high-temperature regions, the amount of heat generation and transfer can also be controlled.
[0068] Furthermore, in some embodiments, the through-hole 123 has a diameter of 0.5 mm to 3 mm, which is advantageous for the smooth passage of aerosols through the through-hole 123.
[0069] Figure 3 A schematic diagram of a method for preparing a composite tobacco sheet 100 with a laminated structure is shown in one embodiment; according to Figure 3 As shown, the preparation method includes:
[0070] S10, providing a mold, the mold including a receiving groove;
[0071] S20, pour slurry into the receiving tank and place the substrate layer on the upper side of the slurry so that the slurry forms an aerosol matrix layer on one side of the substrate layer;
[0072] S30, the mold is placed in a drying oven for the first drying;
[0073] S40, continue pouring slurry into the receiving tank to form an aerosol matrix layer on the other side of the substrate layer;
[0074] S50, the mold is placed in the drying oven for a second drying.
[0075] Specifically, such as Figure 4 As shown, a mold 200 is provided in advance, which includes a plurality of receiving grooves 210. A slurry for forming an aerosol generating matrix is poured into the receiving grooves 210 using a casting device 300. Then, a matrix layer 120 is placed on top of the slurry, so that the first surface 121 of the matrix layer 120 contacts the slurry, while the second surface 122 faces the opening of the receiving groove 210. At this time, the slurry will form a first aerosol generating matrix layer 110 on the first surface 121.
[0076] In some embodiments, the casting device 300 may be any one of a disposable dropper, a dropper tip, a pipette, a pipette gun, a syringe, a dispensing machine, etc.
[0077] In some embodiments, the concentration of the slurry being poured is 10% to 30%.
[0078] After the slurry forms the first aerosol generating matrix layer 110 on the first surface 121, the mold 200 is transferred to a drying environment for the first drying process, so as to dry the first aerosol generating matrix layer 110 and thus make the first aerosol generating matrix layer 110 tightly bonded to the first surface 121.
[0079] After the first drying is completed, the mold is removed from the drying oven, and slurry is poured into the receiving tank 210 again, thereby forming a second aerosol generating matrix layer 120 on the second surface 122 of the substrate layer 120. At this time, aerosol generating matrix layers are formed on both sides of the substrate layer 120. The mold 200 is then placed back into the drying oven for a second drying process to dry the first aerosol generating matrix layer 110, thereby ensuring that the second aerosol generating matrix layer 120 is tightly bonded to the first surface 122. It is easy to understand that during the second drying process, the first aerosol generating matrix layer 110 is dried simultaneously with the second aerosol generating matrix layer 120.
[0080] After the second drying is completed, the substrate layer 120 with aerosol generation matrix layers on both sides is removed from the mold to form the composite tobacco sheet 100 described above.
[0081] It should be noted that, in the specific preparation process, a substrate layer 120 with a large surface area is usually provided first. Then, multiple substrate layer 120 units with smaller surface areas are punched from the substrate layer 120. The multiple substrate layer 120 units are then placed into the receiving grooves 210 of the module 200 respectively. Then, slurry is poured into each receiving groove 210. After pouring, the mold 200 is transferred to a drying oven for drying, so that multiple composite tobacco sheets 100 can be prepared at one time.
[0082] In some embodiments, after the first drying, the moisture content of the first aerosol generating matrix layer 110 is measured to ensure that the moisture content of the first aerosol generating matrix layer 110 is within a threshold range. If, after measurement, the moisture content of the first aerosol generating matrix layer 110 exceeds the threshold range, the first aerosol generating matrix layer 110 needs to be dried further until the moisture content is within the threshold range.
[0083] In some embodiments, after the first drying, the moisture content of the first aerosol-generated matrix layer 110 is 50% to 60%.
[0084] In some embodiments, after the second drying, the moisture content of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 120 as a whole is measured to ensure that the moisture content of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 120 as a whole is within a threshold range. Similarly, if, after measurement, the moisture content of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 120 as a whole exceeds the threshold range, drying needs to continue until the moisture content is within the threshold range.
[0085] In some embodiments, after the second drying, the overall moisture content of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 120 is 10% to 20%.
[0086] Specifically, when measuring the moisture content, the matrix layer 120 with the aerosol matrix layer can be removed from the mold 200, and then the moisture content of the aerosol matrix layer can be measured using a moisture measuring instrument, which can be a rapid moisture analyzer. Since multiple composite tobacco sheets 100 can be prepared at one time, a batch sampling method can be used for moisture measurement, eliminating the need to measure the moisture content of each composite tobacco sheet 100 individually.
[0087] In some embodiments, the thickness of the composite tobacco sheet 100 obtained after the second drying is 0.1 mm to 2.0 mm. If the thickness is too thick, the aerosol generation matrix layer will not be heated sufficiently, resulting in a poor aerosol taste; while if the thickness is too thin, the aerosol generation matrix layer will be easily over-baked, resulting in a poor aerosol taste as well.
[0088] In some embodiments, the pulp composition includes tobacco or natural plant materials, fibers, adhesives, flavorings, and smoke-generating agents.
[0089] In some specific embodiments, the pulp composition includes 45%-80% tobacco or natural plant materials, 3%-20% fiber, 0-5% adhesive, 10-35% flavoring, and 15%-40% smoke-generating agent.
[0090] One embodiment of this application also provides an aerosol generation system, such as Figure 5 As shown, the aerosol generation system includes an aerosol generation product 2000 and an aerosol generation device 3000. The aerosol generation product 2000 includes a composite smoke sheet 100. The aerosol generation device 3000 is used to house the aerosol generation product 2000. When the aerosol generation product 2000 is housed in the aerosol generation device 3000, the aerosol generation device 3000 and the aerosol generation product 2000 cooperate to generate heat in the substrate layer 12.
[0091] For example, a magnetic field generator can be installed in the aerosol generating device 3000. The magnetic field generator can be an induction coil, and the substrate layer 120 is made of a conductive material. Suitable conductive materials can be any of iron, aluminum, nickel, nickel-iron alloy, or stainless steel. When the aerosol generated product 2000 is housed in the aerosol generating device 3000, the controller of the aerosol generating device 3000 controls the supply of alternating current to the induction coil, thereby causing the induction coil to generate an alternating magnetic field. The alternating magnetic field penetrates the substrate layer 120, inducing eddy currents on the substrate layer 120, and then the substrate layer 120 generates heat under the action of the eddy currents.
[0092] In some embodiments, such as Figure 5 As shown, the aerosol generating product 2000 includes a carrier 1000, which has multiple receiving slots 1400. Each receiving slot 1400 contains one composite smoke sheet 100. The composite smoke sheet 100 is held in the receiving slot 1400 by fitting tightly with it, thereby holding it on the carrier 1000. For example, if the aerosol generating product 2000 includes five composite smoke sheets 100, then the carrier 1000 has five corresponding receiving slots 1400, each holding one composite smoke sheet 100. Thus, through the support of the carrier 1000, the aerosol generating product 2000 can carry multiple composite smoke sheets 100 and place them into the aerosol generating device 3000 at one time.
[0093] In some embodiments, such as Figure 6 As shown, the carrier 1000 can also be constructed as a box-shaped body, which is hollow. The aforementioned receiving groove 1400 can be provided on the inner surface of the box-shaped body, thereby holding the composite tobacco sheet 100 inside the box-shaped body. After the composite tobacco sheet is prepared by the above-described preparation method, multiple composite tobacco sheets are then placed into the box-shaped body to form the shape shown in the aerosol generating article 2000a provided in this embodiment.
[0094] The hollow region 1100 of the box-shaped body is used to receive the aerosol generated by the volatilization of the aerosol matrix layer after being heated, and the box-shaped body also has an air inlet 1200 for air to enter the hollow region 1100, and an air outlet 1300 disposed opposite to the air inlet for aerosol to escape from the box-shaped body.
[0095] Please continue reading. Figure 5The aerosol generating device 3000 includes a housing 3100, and a battery cell 3200 and a main board 3300 disposed within the housing 3100. The battery cell 3200 and the main board 3300 are electrically connected, and the main board 3300 is equipped with a controller for the aerosol generating device 300. The housing 3100 also includes a receiving section defining a receiving chamber 3400 for receiving the aerosol generating article 2000. Specifically, the aerosol generating article 2000 can be... Figure 5 The object is housed in the containment chamber 3400 in the direction of the middle arrow X, or along... Figure 5 The middle arrow Y direction is contained within the containment chamber 3400.
[0096] In some embodiments, the receiving chamber 3400 may be provided with a plurality of induction coils 3410. When the aerosol generating article 2000 is received in the receiving chamber 3400, the plurality of induction coils 3410 correspond to each composite smoke sheet 100 respectively. The controller controls the supply of alternating current to each induction coil 3410, so that each induction coil 3410 can induce an alternating magnetic field. The induced alternating magnetic field penetrates each substrate layer 120, thereby generating eddy currents in the substrate layer 120, and then generating heat under the action of the eddy currents.
[0097] It is easy to understand that the aerosol generating device can also use other methods well known to those skilled in the art to generate heat in the substrate layer 120, and is not limited to the electromagnetic method in the above embodiments.
[0098] In some embodiments, the controller may be configured to simultaneously provide alternating current to multiple induction coils 3410, thereby causing multiple composite tobacco sheets 100 to volatilize simultaneously and generate aerosols.
[0099] Alternatively, in some embodiments, the controller may be configured to provide alternating current to the induction coil 3410 in a certain order, so that multiple composite tobacco sheets 100 evaporate in a certain order to generate aerosols. After the last composite tobacco sheet 100 evaporates to generate aerosols, the aerosol generating product 2000 can be removed from the aerosol generating device 3000 and a new aerosol generating product 2000 can be placed in the aerosol generating device 3000.
[0100] like Figure 5 As shown, the aerosol generating device 3000 is also provided with a suction nozzle 3500, which has a defined outlet 3510 for the aerosol to escape from the aerosol generating device 300, so that the user can inhale the aerosol when sucking on the suction nozzle 3500.
[0101] In some embodiments, the nozzle 3500 is in communication with the receiving chamber 3400, when the aerosol generating article 2000 is manufactured according to... Figure 5When the composite tobacco sheet 100 in the aerosol generating device 3000 is placed in the aerosol generating product 2000, the aerosol generated by the heating and volatilization of the composite tobacco sheet 100 is directly released into the receiving chamber 3400 so that the aerosol can further flow to the mouthpiece 3500.
[0102] Alternatively, in some embodiments, when the aerosol-generating article is in accordance with Figure 6 The aerosol generating product 2000a shown is housed in the aerosol generating device 3000. The aerosol generated by the heating and volatilization of the composite tobacco sheet 100 is released into the hollow region 1100 of the box-shaped body, and then escapes from the aerosol generating product 2000 through the air outlet 1300 of the box-shaped body and further enters the mouthpiece 3500 for the user to inhale.
[0103] It should be noted that the preferred embodiments of this application are given in the specification and accompanying drawings, but are not limited to the embodiments described in this specification. Furthermore, those skilled in the art can make improvements or modifications based on the above description, and all such improvements and modifications should fall within the protection scope of the appended claims.
Claims
1. A method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix layer and an aerosol-generating matrix layer bonded to both sides of the matrix layer and capable of being heated to generate an aerosol, characterized in that, The preparation method includes: A mold is provided, the mold including a receiving groove; Slurry is poured into the receiving tank, and the substrate layer is placed on the upper side of the slurry so that the slurry forms an aerosol matrix layer on one side of the substrate layer; The mold is placed in a drying oven for the first drying process. Continue pouring slurry into the receiving tank to form an aerosol matrix layer on the other side of the substrate layer; The mold is placed in the drying oven for a second drying process.
2. The preparation method according to claim 1, characterized in that, After the step of placing the mold in a drying oven for the first drying, the moisture content of the aerosol matrix layer is 50% to 60%.
3. The preparation method according to claim 1, characterized in that, After the step of placing the mold into the drying oven for a second drying, the moisture content of the aerosol matrix layer is 10% to 20%.
4. The preparation method according to claim 1, characterized in that, The thickness of the substrate layer is 0.01mm-0.30mm.
5. The preparation method according to claim 1, characterized in that, The substrate layer has through holes connecting its two sides.
6. The preparation method according to claim 5, characterized in that, The number of through holes is multiple, and the area of the holes accounts for 30%-50%.
7. The preparation method according to claim 1, characterized in that, The substrate layer is a metal sheet.
8. The preparation method according to claim 7, characterized in that, The metal sheet is made of copper, iron, aluminum, tin, stainless steel, or their alloys.
9. The preparation method according to claim 1, characterized in that, The surface of the substrate layer is roughened.
10. The preparation method according to claim 1, characterized in that, The thickness of the composite tobacco sheet is 0.1mm-2.0mm.
11. The preparation method according to claim 1, characterized in that, The pulp composition includes tobacco or natural plant materials, fibers, adhesives, flavorings, and smoke-generating agents.
12. The preparation method according to claim 1, characterized in that, In the composite tobacco sheet, the two aerosol matrix layers have different thicknesses.
13. The preparation method according to claim 1, characterized in that, The concentration of the slurry is 10% to 30%.
14. An aerosol-generating product, characterized in that... include: Multiple composite tobacco sheets, wherein the composite tobacco sheets are prepared by the preparation method according to any one of claims 1-13; A carrier is used to support the composite tobacco sheets, and a plurality of the composite tobacco sheets are held on the carrier.
15. The aerosol-generating article according to claim 14, characterized in that, The carrier is constructed as a hollow box-shaped body, the hollow area of which is used to receive the aerosol. The box-shaped body has an air inlet for air to enter the hollow area and an air outlet for the aerosol to escape from the box-shaped body.
16. An aerosol generation system, characterized in that, include: The aerosol-generating article according to claim 14 or 15; An aerosol generating apparatus is provided with a receiving chamber for containing the aerosol generating article. When the aerosol generating article is contained in the receiving chamber, the aerosol generating apparatus and the aerosol generating article cooperate to generate heat in the substrate layer. The aerosol generating device further includes a suction nozzle, which defines an outlet for aerosols to escape from the aerosol generating device.