Method of manufacturing a composite tobacco sheet, aerosol-generating article and system
By combining a hollow columnar matrix with an aerosol generation matrix in a composite tobacco sheet and drying it with a heated plate, the design of the composite tobacco sheet solves the problems of long aerosol generation time and insufficient aroma release in the existing technology, and achieves an aerosol generation effect with instant smoke and good taste.
Patent Information
- Application Number
- CN202510669498.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-22
- Publication Date
- 2026-11-24
AI Technical Summary
Existing composite tobacco sheets take a long time to volatilize and generate aerosols when not burning, resulting in insufficient aroma release and poor aerosol taste.
The composite tobacco sheet design combines a hollow cylindrical matrix with an aerosol generating matrix. The composite tobacco sheet is formed by heating and coating the slurry with a heating plate and then drying it. The matrix is directly heated to generate aerosols quickly. Combined with a cooling and filtration structure, the aroma release and taste are enhanced.
It achieves instant aerosol generation, full aroma release, good aerosol taste, reduces user waiting time, and improves aerosol concentration and quality through uniform heating.
Smart Images

Figure CN123147684A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of aerosol technology, and in particular to a method for preparing composite tobacco sheets, and an aerosol generating article and system having the composite tobacco sheets. Background Technology
[0002] Tobacco products (e.g., cigarettes, cigars, etc.) produce tobacco smoke by burning tobacco during use. Efforts are being made to replace these tobacco-burning products by creating products that release compounds without combustion. An example of such a product is an aerosol generating device that releases compounds by heating a composite tobacco sheet used with it. This composite tobacco sheet may, for example, be tobacco or other non-tobacco products, which may or may not contain nicotine.
[0003] The aerosol generating device is equipped with a heating element that generates heat, which is then transferred to the composite tobacco sheet. When the composite tobacco sheet is heated, it volatilizes to generate aerosols. However, the existing composite tobacco sheet volatilizes to generate aerosols for a long time, the aroma is not fully released, and the aerosol taste is not good. Summary of the Invention
[0004] This application provides a method for preparing composite tobacco sheets, as well as an aerosol generating article and system having the composite tobacco sheets, to prepare a composite tobacco sheet capable of rapidly generating aerosols.
[0005] At least one embodiment of this application provides a method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix capable of generating heat, the matrix being configured as a hollow column, and the composite tobacco sheet further comprising an aerosol generating matrix bonded to the matrix and capable of being heated by the matrix to generate an aerosol, the method for preparing the composite tobacco sheet comprising:
[0006] The substrate is placed flat on the heating plate;
[0007] The slurry used to form the aerosol generation matrix is poured into the feed trough of the coating device;
[0008] The driving coating device moves between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product;
[0009] The heating plate is activated to heat the slurry coated on the substrate for the first drying process, in order to form composite tobacco sheets.
[0010] In one embodiment, after the step of heating the slurry coated on the substrate with the start-up heating plate to perform a first drying to form composite tobacco sheets, the preparation method further includes:
[0011] Confirm whether the moisture content of the slurry after the first drying is less than the preset value;
[0012] If the size is smaller, the composite tobacco sheet is cut and the cut composite tobacco sheet units are rolled into a cylindrical shape.
[0013] In one embodiment, in the step of confirming whether the moisture content of the slurry after the first drying is less than a preset value, the preset value is less than or equal to 12%.
[0014] In one embodiment, the coating applicator includes a scraper for coating the slurry onto the substrate, the scraper being 0.1 mm to 3 mm away from the surface of the heating plate.
[0015] In one embodiment, prior to the step of moving the driving coating device between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product, the preparation method further includes:
[0016] A liquid is placed between the substrate and the heating plate to keep the substrate and the heating plate in contact.
[0017] In one embodiment, the step of moving the driving coating device between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product specifically includes:
[0018] The coating device is driven to move in a straight line.
[0019] In one embodiment, the step of moving the driving coating device between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product specifically includes:
[0020] The coating device is driven to move between the first position and the second position at a speed of 1 cm to 2 cm per second.
[0021] In one embodiment, the drying time for the first drying is 25 mins to 90 mins, and the drying temperature is 50°C to 120°C.
[0022] In one embodiment, after the step of heating the slurry coated on the substrate with the start-up heating plate to perform a first drying to form composite tobacco sheets, the preparation method further includes:
[0023] The composite tobacco sheet is transferred to a drying oven for drying until the moisture content of the slurry is less than the preset value.
[0024] In one embodiment, in the step of transferring the composite tobacco sheet to a drying oven for drying until the moisture content of the slurry is less than the preset value, the drying time is 5 mins to 45 mins, and the drying temperature is 60°C to 120°C.
[0025] In one embodiment, the thickness of the substrate is 0.005 mm to 0.05 mm.
[0026] In one embodiment, the substrate is a porous and flexible magnetic foil material.
[0027] In one embodiment, the thickness of the composite tobacco sheet is 0.05 mm to 2.95 mm.
[0028] At least one embodiment of this application also provides an aerosol generating article, comprising:
[0029] The shell has a first section, a second section, and a third section arranged sequentially and interconnected along its length;
[0030] The composite tobacco sheet is prepared by the preparation method described in the above embodiments;
[0031] The composite smoke sheet is disposed in the first section, the second section is provided with an air inlet that communicates with the outside, the air inlet allows outside air to enter to cool the aerosol, and the third section is provided with a filter material for filtering the aerosol.
[0032] At least one embodiment of this application also provides an aerosol system, including the aerosol generating article described in the above embodiments, and an aerosol generating apparatus for containing at least a portion of the aerosol generating article;
[0033] When the aerosol generating product is housed in the housing chamber, the aerosol generating product and the aerosol generating device cooperate with each other to generate heat in the substrate.
[0034] The method for preparing composite tobacco sheets provided in the above embodiments involves first placing the substrate flat on a heating plate, then pouring the slurry used to form an aerosol matrix into the feed trough of a coating device, and then driving the coating device to move between a first position and a second position to coat the slurry onto the substrate, thereby forming a semi-finished product. The heating plate is then activated to perform the first drying of the semi-finished product. After the first drying is completed, composite tobacco sheets are formed. Attached Figure Description
[0035] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.
[0036] Figure 1 This is a three-dimensional schematic diagram of a composite tobacco sheet provided in an embodiment of this application.
[0037] Figure 2 yes Figure 1 A cross-sectional schematic diagram of a composite tobacco sheet in one direction.
[0038] Figure 3 yes Figure 2 A three-dimensional schematic diagram of the matrix of composite tobacco sheets before rolling;
[0039] Figure 4 yes Figure 2 A three-dimensional schematic diagram of composite tobacco sheets before rolling;
[0040] Figure 5 yes Figure 2 A schematic diagram of the structure of a composite tobacco sheet when it is used in a tubular body;
[0041] Figure 6 This is a schematic diagram of a method for preparing composite tobacco sheets according to an embodiment of this application;
[0042] Figure 7 yes Figure 6 A schematic diagram of the heating plate and coating apparatus used in the preparation method;
[0043] Figure 8 yes Figure 7 A schematic diagram of the intermediate coating device from another direction. Detailed Implementation
[0044] To facilitate understanding of this application, a more detailed description of this application will be provided below in conjunction with the accompanying drawings and specific embodiments.
[0045] One embodiment of this application provides a composite tobacco sheet 100, such as Figure 1 As shown, after the composite tobacco sheet 100 is rolled into shape, it forms a generally cylindrical structure. The cylindrical structure has a first end 110 and a second end 120 arranged opposite to each other along its length direction, and a cavity 130 extending between the first end 110 and the first end 120.
[0046] like Figure 2As shown, the composite tobacco sheet 100 includes a substrate 10 extending between a first end 110 and a second end 120. The substrate 10 is wound and constructed into a hollow cylindrical shape, thereby defining the aforementioned cavity 130 within the hollow region formed by the substrate 10. The substrate 10 has a thickness direction (see...) Figure 3 The first surface 11 and the second surface 12 (in the X direction indicated by the arrow in the diagram) are positioned opposite each other. An aerosol generating matrix 20 is bonded to the first surface 11 or the second surface 12. The matrix 10 is used to generate heat, which can be used to heat the aerosol generating matrix 20. The aerosol generating matrix 20 volatilizes when heated, thus generating aerosols. It should be noted that the cavity 130 can serve as an airflow channel, allowing airflow carrying aerosols to flow within the cavity 130.
[0047] In the aforementioned composite tobacco sheet 100, the aerosol generating matrix 20 is bonded to the substrate 10, and the aerosol generating matrix 20 and the substrate 10 are in direct contact. Therefore, the heat generated by the substrate 10 can directly heat the aerosol generating matrix 20, allowing it to heat up rapidly and volatilize to generate aerosols, achieving an immediate inhalation effect. In other words, in the aerosol generating device used to heat the composite tobacco sheet 100, there is no need for a preheating stage; smoke can be produced rapidly and instantly upon startup or operation of the heating components, reducing user waiting time. Furthermore, the direct contact between the aerosol generating matrix 20 and the substrate 10 ensures thorough heating, and the substrate 10 heats the aerosol generating matrix 20 uniformly, resulting in a concentrated aerosol with full aroma release and a good aerosol taste.
[0048] In actual preparation, such as Figure 3 and Figure 4 As shown, a sheet-like substrate 10 can be provided first, then the first aerosol generating matrix 20 can be bonded to the first surface 11 of the substrate 10, and finally the substrate 10 bonded with the aerosol generating matrix 20 can be rolled up.
[0049] like Figure 3 As shown, the substrate 10 also includes a plurality of through holes 13 connecting the first surface 11 and the second surface 12. When the first aerosol generating matrix 20 is heated and volatilizes to generate aerosol, the aerosol will enter the cavity 130 through the through holes 13, and then escape from the port of the first end 110 along the cavity 130.
[0050] In specific usage, such as Figure 5As shown, the composite tobacco sheet 100 can be assembled in a housing 200. When the composite tobacco sheet 100 is assembled in the housing 200, the composite tobacco sheet 100 and the housing 200 can form an aerosol generating article. The aerosol generating article is used in conjunction with a suitable aerosol generating device (not shown). The aerosol generating device is provided with a receiving chamber for accommodating at least a portion of the aerosol generating article. When the aerosol generating article is accommodated in the receiving chamber, the aerosol generating device and the aerosol generating article cooperate to generate heat in the substrate 10. At this time, the aerosol generating device and the aerosol generating article combine to form an aerosol forming system.
[0051] For example, a magnetic field generator can be provided in the aerosol generating device 100. The magnetic field generator can be an induction coil, and the substrate 10 is made of a conductive material, such as aluminum foil, copper foil, silver foil, etc., as described below, or any one of nickel-iron alloy, high-nickel alloy, stainless steel, or pure iron. When the aerosol-generated product is contained in the containing chamber, the controller of the aerosol generating device controls the flow of alternating current to the induction coil, thereby causing the induction coil to generate an alternating magnetic field. The alternating magnetic field penetrates the substrate 10, inducing eddy currents on the substrate 10, and then the substrate 10 generates heat under the action of the eddy currents.
[0052] The housing 200 includes a first section 210, a second section 220, and a third section 230 arranged sequentially and connected along its length. The first section 210 is used to hold the composite tobacco sheet 100. The second section 220 is a cooling section for allowing external cold air to enter the housing 200 through the air inlet 221. The third section 230 is used to contain a filtering substance 240 and is also provided with a filter nozzle for the user to inhale.
[0053] When the user inhales through the filter nozzle in the third section 230, the aerosol generated by the volatilization of the first aerosol generating matrix 20 can enter the cavity 130 through the through hole 13, and then flow further along the cavity 130 to the second section 220, where it mixes with the external cold air for cooling. Finally, the cooled aerosol enters the third section 230 for filtration to remove some unwanted particles. The user can then inhale the cooled and filtered aerosol by inhaling through the filter nozzle in the third section 230.
[0054] In some embodiments, the through holes 13 are arranged in an array.
[0055] In some embodiments, the plurality of through holes 13 may be arranged in a circular, elliptical, racetrack-shaped, rectangular, triangular-hexagonal or other shapes.
[0056] In some embodiments, the plurality of through holes 13 may be arranged in a centrally symmetrical or axisymmetric pattern.
[0057] Furthermore, in some embodiments, the porosity of the plurality of through holes 13 on the substrate 10 is 20%-50%. In some preferred embodiments, the porosity of the plurality of through holes 13 on the substrate 10 is 20%, 25%, 30%, 35%, 40%, 45%, or 50%. This allows aerosols to pass smoothly through the through holes 13 so that the aerosols can flow into the cavity 130.
[0058] In some embodiments, the through-hole 13 is formed by machining or chemical etching. Further in some embodiments, machining includes drilling or laser processing.
[0059] In some embodiments, the thermal conductivity of the substrate 10 is at least 25 W / m·K. In one embodiment of this application, the thermal conductivity of the substrate 10 is 25 W / m·K, 30 W / m·K, 32 W / m·K, 35 W / m·K, 40 W / m·K, or 45 W / m·K.
[0060] In some embodiments, the thickness of the substrate 10 is between 0.005 mm and 0.05 mm. Preferably, the thickness of the substrate 10 is 0.006 mm, 0.01 mm, 0.012 mm, 0.015 mm, 0.020 mm, 0.018 mm, 0.02 mm, 0.025 mm, or 0.03 mm. Within this range, the substrate 10 can maintain a certain structural strength to support the first aerosol generation matrix layer 20 coated thereon, while the thickness of the substrate 10 also allows it to maintain a certain degree of flexibility, enabling it to be rolled from a sheet into a column shape.
[0061] In some embodiments, the substrate 10 may include a sensitive metal or alloy that can be penetrated by a magnetic field and generate heat. When the substrate 10 is in a changing magnetic field, according to the law of electromagnetic induction, the magnetic flux through the substrate 10 changes, generating an induced electromotive force (EMF) within the substrate 10. Since the substrate 10 is a conductor with relatively low resistance, a closed loop is formed inside the substrate 10 under the influence of the induced EMF, generating induced eddy currents. As the eddy currents flow inside the substrate 10, electrical energy is converted into heat energy, causing the temperature of the substrate 10 to rise. This heat then heats the aerosol-forming matrix layer 12.
[0062] In some embodiments, the substrate 10 may include a soft magnetic alloy. Soft magnetic alloys, with their core advantages of high electromagnetic response, low loss, and high saturation magnetization, are widely used in energy conversion and signal processing.
[0063] In some specific embodiments, the substrate 10 includes magnetic foil materials such as aluminum foil, copper foil, and silver foil, or any one of nickel-iron alloy, high-nickel alloy, stainless steel, or pure iron.
[0064] In some embodiments, the aerosol generating matrix 20 includes tobacco extract. The tobacco extract can be obtained by extracting extracts from tobacco leaves and flowers using a solvent, then extracting the extracts with ethanol, followed by drying, dehydration, desalting, and cooking of the raw materials, adding an extract with a special aroma, and performing ultrasonic-assisted extraction to finally obtain a tobacco extract with a specific flavor. In one embodiment of this application, the tobacco extract is mainly used for tobacco flavoring, which can enhance the aroma, reduce off-flavors, and improve cigarette quality. Its aroma is realistic and natural, making it an excellent raw material for cigarette flavoring. Furthermore, tobacco extract can also be used in daily-use fragrances to provide unique aromas and flavors.
[0065] In some embodiments, the main components of tobacco extract include furfuryl alcohol, benzyl alcohol, phytol, solanone, β-turfayne, β-ionone, hexahydrofarnesone, diene, daidzeinone, dihydroactinolone, isopentenone, indole, etc.
[0066] In some embodiments, the aerosol generating matrix 20 comprises at least one of tobacco-based and tea-based materials; or at least one of carbon powder and ceramic beads.
[0067] One embodiment of this application also provides a method for preparing composite tobacco sheet 100, such as... Figure 6 As shown, the preparation method includes:
[0068] S10, the substrate is placed flat on the heating plate;
[0069] S20, the slurry used to form the aerosol generation matrix is poured into the feed trough of the coating machine;
[0070] S30, drive the coating device to move between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product;
[0071] S40, the heating plate is activated to heat the slurry coated on the substrate for the first drying to form composite tobacco sheets;
[0072] like Figure 7 As shown, the heating plate 200 includes a first surface 210 and a second surface 220 disposed opposite to each other. The first surface 210 is used to place the substrate 10. A heating element (not shown) is disposed between the first surface 210 and the second surface 220. The heating element generates heat when it is powered on, and the heat is further conducted to the first surface 210, thereby raising the temperature of the first surface 210.
[0073] In some embodiments, the heating plate 200 is made of a material with high thermal conductivity, so that the heat generated by the heating element can be quickly conducted to the first surface 210, and the temperature of the first surface 210 can rise rapidly. The material with high thermal conductivity can be any of the following: a metallic material such as silver, copper, aluminum, or pure iron, or a non-metallic material such as diamond or graphene.
[0074] A coating applicator 300 is a device or tool used to uniformly apply paint, ink, adhesive, or other liquid materials to the surface of an object. For example... Figure 7 He Ru Figure 8 As shown, the coating applicator 300 includes a scraper 310, an adjustment section 320, and a feed trough 330. The feed trough 330 is used to hold the slurry for forming the aerosol generating matrix 20. The scraper 310 is used to coat the slurry onto the substrate 10. The adjustment section 320 is used to adjust the distance between the scraper 310 and the first surface 210 of the heating plate 200, that is, to adjust the height of the scraper 310. Figure 8 The mid-distance d is shown.
[0075] Specifically, in the preparation process, the substrate 10 is first placed flat on the first surface 210 of the heating plate 200, then the slurry is poured into the feed trough 330, and the scraper 320 is adjusted to the preset height. Then, the coating device 300 is driven along... Figure 7 The middle arrow moves from the first position to the second position. During the movement, the scraper 320 can coat the slurry onto the substrate 10.
[0076] After the coating applicator 300 moves to the second position, the slurry coated on the substrate 10 is inspected. If the slurry coating is uneven, the coating applicator 300 is driven to move from the second position to the first position until the slurry is evenly coated on the surface of the substrate 10. If the slurry coating is even, it is not necessary to drive the coating applicator 300 from the second position to the first position again. After the slurry is evenly coated on the substrate 10, a semi-finished product is formed. The semi-finished product has a high water content, meaning there is a lot of water in the slurry. High water content means the aerosol generation matrix 20 is not fully heated, resulting in a poor-tasting aerosol.
[0077] Therefore, the heating plate 200 is then activated to perform the first drying of the semi-finished product, so that some of the moisture in the slurry evaporates. The dried slurry then forms an aerosol matrix 20 and tightly bonds to the substrate 10, thereby forming a composite tobacco sheet. Specifically, the first drying can be performed by controlling the heating temperature and heating time of the heating plate 200. Once the heating time is reached, the first drying is complete.
[0078] In some embodiments, the above preparation method further includes: after forming the composite tobacco sheet, detecting the moisture content of the composite tobacco sheet to confirm whether the moisture content of the slurry is less than a preset value; if it is less, cutting the matrix 10 and rolling the cut matrix units into a column shape, thereby obtaining a single composite tobacco sheet 100.
[0079] In some embodiments, the substrate 10 can be cut into multiple substrate units of arbitrary shape (e.g., square), and then rolled up by each substrate unit to form a composite tobacco sheet 100.
[0080] Moisture content is an important parameter in composite tobacco sheet 100. If the moisture content is too high, the aerosol generating matrix 20 will not be heated sufficiently, meaning that the matrix 10 will not bake the aerosol generating matrix 20 sufficiently, which will result in the aerosol generated by the volatilization of the aerosol generating matrix 20 after heating having an unpleasant taste.
[0081] In some embodiments, if the moisture content of the slurry is less than 12% after the first drying, the requirement can be confirmed, and the substrate 10 can be cut.
[0082] In some embodiments, the moisture content of the slurry can be measured using a rapid moisture analyzer.
[0083] In some embodiments, the above preparation method further includes: before placing the substrate 10 on the heating plate 200, coating an appropriate amount of liquid on the heating plate 200, or coating an appropriate amount of liquid on the surface of the substrate 10 facing the heating plate 200, so that the substrate 10 can be flatly attached to the heating plate 200 under the action of liquid tension and adhesion, avoiding the substrate 10 from lifting, so that the coating device 300 can uniformly coat the slurry on the substrate 10.
[0084] In some embodiments, the liquid can be any of water, oil, emulsion, etc.
[0085] In some embodiments, the drying temperature for the first drying using the heating plate 200 is 25 mins to 90 mins, and the drying time is 50°C to 120°C.
[0086] In some embodiments, if the moisture content of the slurry coated on the substrate 10 after the first drying is greater than a preset value, the slurry needs to be dried a second time until the moisture content of the slurry is less than the preset value after the second drying. This is because the temperature of the heating plate 200 may be unevenly distributed, which may cause the moisture content of the slurry on some substrates 10 to be less than the preset value after the first drying, while the moisture content of the slurry on some substrates 10 may be greater than the preset value.
[0087] In some specific embodiments, if the moisture content of the slurry after the first drying is greater than a preset value, the composite tobacco sheet formed after the first drying is transferred to a drying oven for a second drying until the moisture content of the slurry is less than the preset value.
[0088] In some embodiments, during the second drying in the drying oven, the drying time is 5 mins to 45 mins, and the drying temperature is 60°C to 120°C. That is, the first drying is performed using a heating plate 200 at a drying temperature of 25 mins to 90 mins and a drying time of 50°C to 120°C. If the moisture content of the slurry is greater than 12% after the first drying, the matrix 10 is placed in the aforementioned drying oven for a second drying until the moisture content of the slurry is less than 12%.
[0089] In some embodiments, the thickness of the composite tobacco sheet 100 is 0.05 mm to 2.95 mm, so that the aerosol generating matrix 20 can be sufficiently heated to produce an aerosol with better taste, while avoiding over-baking of the aerosol generating matrix 20 and the resulting burnt taste. Therefore, in some embodiments, the distance between the scraper 320 and the first surface 210 of the heating plate 200 can be set between 0.10 mm and 3.00 mm, that is, the height of the scraper 320 can be set between 0.10 mm and 3.00 mm, so that the thickness of the composite tobacco sheet 100 formed after drying is between 0.05 mm and 2.95 mm.
[0090] In some embodiments, the coating applicator 300 moves along a straight line between a first position and a second position, thereby facilitating the uniform coating of the slurry onto the substrate 10. Therefore, in some embodiments, a linear guide rail (not shown) may be provided on the heating plate 200, along which the coating applicator 300 moves, thereby enabling the coating applicator 300 to move along a straight line between the first and second positions.
[0091] In some embodiments, a driving mechanism may be provided on the heating plate, which drives the coating applicator 300 to move along a straight line between a first position and a second position. Alternatively, in some embodiments, the coating applicator 300 may be manually driven to move along a straight line between the first position and the second position.
[0092] The coating applicator 300 needs to move at a certain speed between the first and second positions to ensure rapid movement and improve the uniformity of the slurry coating on the substrate 10. In some embodiments, the coating applicator 300 is driven to move between the first and second positions at a speed of 1 cm to 2 cm per second to ensure uniform coating of the slurry on the substrate 10.
[0093] It should be noted that the preferred embodiments of this application are given in the specification and accompanying drawings, but are not limited to the embodiments described in this specification. Furthermore, those skilled in the art can make improvements or modifications based on the above description, and all such improvements and modifications should fall within the protection scope of the appended claims.
Claims
1. A method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix capable of generating heat, the matrix being constructed as a hollow column, the composite tobacco sheet further comprising an aerosol generating matrix bonded to the matrix and capable of being heated by the matrix to generate aerosols, characterized in that, The method for preparing the composite tobacco sheet includes: The substrate is placed flat on the heating plate; The slurry used to form the aerosol generation matrix is poured into the feed trough of the coating device; The driving coating device moves between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product; The heating plate is activated to heat the slurry coated on the substrate for the first drying process, in order to form composite tobacco sheets.
2. The preparation method according to claim 1, characterized in that, After the step of heating the slurry coated on the substrate with the starting heating plate to perform a first drying to form composite tobacco sheets, the preparation method further includes: Confirm whether the moisture content of the slurry after the first drying is less than the preset value; If the size is smaller, the composite tobacco sheet is cut and the cut composite tobacco sheet units are rolled into a cylindrical shape.
3. The preparation method according to claim 2, characterized in that, In the step of confirming whether the moisture content of the slurry after the first drying is less than a preset value, the preset value is less than or equal to 12%.
4. The preparation method according to claim 1, characterized in that, The coating apparatus includes a scraper for coating the slurry onto the substrate, the scraper being 0.1 mm to 3 mm away from the surface of the heating plate.
5. The preparation method according to claim 1, characterized in that, Prior to the step of moving the driving coating device between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product, the preparation method further includes: A liquid is placed between the substrate and the heating plate to keep the substrate and the heating plate in contact.
6. The preparation method according to claim 1, characterized in that, The step of moving the driving coating device between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product specifically includes: The coating device is driven to move in a straight line.
7. The preparation method according to claim 6, characterized in that, The step of moving the driving coating device between a first position and a second position on the heating plate to coat the slurry onto the substrate to form a semi-finished product specifically includes: The coating device is driven to move between the first position and the second position at a speed of 1 cm to 2 cm per second.
8. The preparation method according to claim 1, characterized in that, The drying time for the first drying is 25 mins to 90 mins, and the drying temperature is 50℃ to 120℃.
9. The preparation method according to claim 8, characterized in that, After the step of heating the slurry coated on the substrate with the starting heating plate to perform a first drying to form composite tobacco sheets, the preparation method further includes: The composite tobacco sheet is transferred to a drying oven for drying until the moisture content of the slurry is less than the preset value.
10. The preparation method according to claim 8, characterized in that, In the step of transferring the composite tobacco sheet to a drying oven for drying until the moisture content of the slurry is less than the preset value, the drying time is 5 mins to 45 mins and the drying temperature is 60℃ to 120℃.
11. The preparation method according to any one of claims 1 to 10, characterized in that, The thickness of the substrate is 0.005 mm to 0.05 mm.
12. The preparation method according to any one of claims 1 to 10, characterized in that, The substrate is a porous and flexible magnetic foil material.
13. The preparation method according to any one of claims 1 to 10, characterized in that, The thickness of the composite tobacco sheet is 0.05mm to 2.95mm.
14. An aerosol-generating product, characterized in that, include: The shell has a first section, a second section, and a third section arranged sequentially and interconnected along its length; The composite tobacco sheet is prepared by the preparation method according to any one of claims 1-13; The composite smoke sheet is disposed in the first section, the second section is provided with an air inlet that communicates with the outside, the air inlet allows outside air to enter to cool the aerosol, and the third section is provided with a filter material for filtering the aerosol.
15. An aerosol generation system, characterized in that, Includes the aerosol generating article as described in claim 14, and an aerosol generating apparatus for containing at least a portion of the aerosol generating article; When the aerosol generating product is housed in the housing chamber, the aerosol generating product and the aerosol generating device cooperate with each other to generate heat in the substrate.