Method of manufacturing a composite tobacco sheet, aerosol-generating article and system
By coating and drying aerosols onto a substrate to generate a matrix slurry, composite tobacco sheets are formed, solving the problem of insufficient aroma release in existing aerosol-generated products and achieving instant evaporation of aerosols and a good taste.
Patent Information
- Application Number
- CN202510669516.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-22
- Publication Date
- 2026-11-24
AI Technical Summary
Existing aerosol-generating products take a long time to volatilize and produce aerosols under non-combustible conditions, resulting in insufficient aroma release and poor aerosol taste.
An aerosol-generating matrix slurry is coated onto a substrate using a casting process and then dried in a heated zone to form a composite smoke sheet. The substrate and the aerosol-generating matrix are in direct contact, and the heat generated by the substrate directly heats the aerosol-generating matrix to rapidly generate aerosols.
It achieves instant evaporation of aerosols, fully releases aroma, provides a good aerosol taste, reduces user waiting time, and ensures even heating.
Smart Images

Figure CN123147685A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of heated non-combustible aerosol generation technology, and in particular to a method for preparing composite tobacco sheets, and an aerosol generation product and system having the composite tobacco sheets. Background Technology
[0002] Tobacco products (e.g., cigarettes, cigars, etc.) produce tobacco smoke by burning tobacco during use. Efforts are being made to replace these tobacco-burning products by creating products that release compounds without combustion. An example of such a product is an aerosol generating device that releases compounds by heating an aerosol generating product used in conjunction with it. This aerosol generating product may, for example, be tobacco or other non-tobacco products, which may or may not contain nicotine.
[0003] The aerosol generating device is equipped with a heating element that generates heat, which is then transferred to the aerosol generating product. When heated, the aerosol generating product volatilizes to produce aerosols. However, the existing aerosol generating products take a long time to volatilize and produce aerosols, resulting in insufficient aroma release and poor aerosol taste. Summary of the Invention
[0004] This application provides a method for preparing composite tobacco sheets, as well as an aerosol generating product and system having the composite tobacco sheets, to prepare a composite tobacco sheet capable of rapidly generating aerosols.
[0005] At least one embodiment of this application provides a method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix capable of generating heat, the matrix being constructed as a hollow column, and the composite tobacco sheet further comprising an aerosol generating matrix bonded to the matrix and capable of being heated by the matrix to generate aerosols, the method for preparing the composite tobacco sheet comprising:
[0006] The substrate is placed on the conveyor belt of the casting machine;
[0007] The slurry used to form the aerosol generation matrix is placed in the feed trough of the casting machine;
[0008] The casting machine is started so that the substrate passes through the feed trough, and the slurry is coated on the surface of the substrate to form a semi-finished product;
[0009] The semi-finished product is dried to form composite tobacco sheets;
[0010] The composite tobacco sheet is cut and rolled into a cylindrical shape.
[0011] In one embodiment, the step of starting the casting machine to allow the substrate to pass through the feed trough, thereby coating the substrate surface with the slurry to form a semi-finished product, specifically includes:
[0012] The slurry is applied to the substrate surface using a scraper.
[0013] In one embodiment, the distance between the scraper and the conveyor belt is 0.10 mm to 3.00 mm.
[0014] In one embodiment, a baffle plate is provided at the location of the scraper, and the baffle plate and the scraper enclose the feed trough to the scraper. The baffle plate surrounds the slurry to the scraper.
[0015] In one embodiment, the step of placing the substrate on the conveyor belt of the casting machine specifically includes:
[0016] The substrate is bonded to the conveyor belt using a liquid.
[0017] In one embodiment, during the step of drying the semi-finished product to form composite tobacco sheets,
[0018] Heating zones are provided on both sides of the conveyor belt, and the heating zones are used to dry the slurry coated on the substrate.
[0019] In one embodiment, the transmission belt has a first side and a second side disposed opposite to each other, the first side being provided with a first heating area and the second side being provided with a second heating area, the first heating area and the second heating area having the same extension length along the transmission direction of the transmission belt.
[0020] In one embodiment, the conveyor belt has a first side and a second side arranged opposite to each other. The first side is provided with a first heating area and a second heating area arranged sequentially along the conveying direction. The second side is provided with a third heating area. The third heating area has a first end and a second end arranged opposite to each other along the conveying direction. The first heating area and the second heating area are both located between the first end and the second end.
[0021] In one embodiment, along the conveying direction of the conveyor belt, the first heating area is located upstream of the second heating area, the heating temperature of the second heating area is not less than the heating temperature of the first heating area, and the heating temperature of the third heating area is not less than the heating temperature of the second heating area.
[0022] In one embodiment, the substrate is located on the first side of the conveyor belt.
[0023] In one embodiment, the first heating zone has a heating temperature of 50°C to 80°C, the second heating zone has a heating temperature of 60°C to 90°C, the third heating zone has a heating temperature of 70°C to 120°C, and the heating time is 25 mins to 90 mins.
[0024] In one embodiment, the thickness of the composite tobacco sheet is 0.05 mm to 2.95 mm.
[0025] At least one embodiment of this application also provides an aerosol generating article, comprising:
[0026] The shell has a first section, a second section, and a third section arranged sequentially and interconnected along its length;
[0027] The composite tobacco sheet is prepared by the preparation method described in the above embodiments;
[0028] The composite smoke sheet is disposed in the first section, the second section is provided with an air inlet that communicates with the outside, the air inlet allows outside air to enter to cool the aerosol, and the third section is provided with a filter material for filtering the aerosol.
[0029] At least one embodiment of this application also provides an aerosol system, including the aerosol generating article described in the above embodiments, and an aerosol generating apparatus for containing at least a portion of the aerosol generating article;
[0030] When the aerosol generating product is housed in the housing chamber, the aerosol generating product and the aerosol generating device cooperate with each other to generate heat in the substrate.
[0031] In one embodiment, the substrate is a porous and flexible magnetic foil material.
[0032] The method for preparing composite tobacco sheets provided in the above embodiments involves coating a slurry used to form an aerosol generation matrix onto a substrate using a casting process. The substrate is then heated and dried to evaporate at least part of the water in the slurry, thereby tightly bonding the slurry to the substrate. The substrate is then cut, and finally, the cut substrate is rolled up to form a hollow cylindrical composite tobacco sheet. Attached Figure Description
[0033] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.
[0034] Figure 1This is a three-dimensional schematic diagram of a composite tobacco sheet provided in an embodiment of this application.
[0035] Figure 2 yes Figure 1 A cross-sectional schematic diagram of a composite tobacco sheet in one direction.
[0036] Figure 3 yes Figure 2 A three-dimensional schematic diagram of the matrix of composite tobacco sheets before rolling;
[0037] Figure 4 yes Figure 2 A three-dimensional schematic diagram of composite tobacco sheets before rolling;
[0038] Figure 5 yes Figure 2 A schematic diagram of the structure of a composite tobacco sheet when it is used in a tubular body;
[0039] Figure 6 This is a schematic diagram of a method for preparing composite tobacco sheets according to an embodiment of this application;
[0040] Figure 7 This is a schematic diagram of the structure of a casting machine provided in one embodiment of this application;
[0041] Figure 8 This is a schematic diagram of the structure of a casting machine provided in another embodiment of this application.
[0042] Figure 9 This is a schematic diagram of the feed trough of a casting machine provided in another embodiment of this application. Detailed Implementation
[0043] To facilitate understanding of this application, a more detailed description of this application will be provided below in conjunction with the accompanying drawings and specific embodiments.
[0044] One embodiment of this application provides a composite tobacco sheet 100, such as Figure 1 As shown, after the composite tobacco sheet 100 is rolled into shape, it forms a generally cylindrical structure. The cylindrical structure has a first end 110 and a second end 120 arranged opposite to each other along its length direction, and a cavity 130 extending between the first end 110 and the first end 120.
[0045] like Figure 2 As shown, the composite tobacco sheet 100 includes a substrate 10 extending between a first end 110 and a second end 120. The substrate 10 is wound and constructed into a hollow cylindrical shape, thereby defining the aforementioned cavity 130 within the hollow region formed by the substrate 10. The substrate 10 has a thickness direction (see...) Figure 3The first surface 11 and the second surface 12 (in the X direction indicated by the arrow in the diagram) are positioned opposite each other. An aerosol generating matrix 20 is bonded to the first surface 11 or the second surface 12. The matrix 10 is used to generate heat, which can be used to heat the aerosol generating matrix 20. The aerosol generating matrix 20 volatilizes when heated, thus generating aerosols. It should be noted that the cavity 130 can serve as an airflow channel, allowing airflow carrying aerosols to flow within the cavity 130.
[0046] In the aforementioned composite tobacco sheet 100, the aerosol generating matrix 20 is bonded to the substrate 10, and the aerosol generating matrix 20 and the substrate 10 are in direct contact. Therefore, the heat generated by the substrate 10 can directly heat the aerosol generating matrix 20, allowing it to heat up rapidly and volatilize to generate aerosols, achieving an immediate inhalation effect. In other words, in the aerosol generating device used to heat the composite tobacco sheet 100, there is no need for a preheating stage; smoke can be produced rapidly and instantly upon startup or operation of the heating components, reducing user waiting time. Furthermore, the direct contact between the aerosol generating matrix 20 and the substrate 10 ensures thorough heating, and the substrate 10 heats the aerosol generating matrix 20 uniformly, resulting in a concentrated aerosol with full aroma release and a good aerosol taste.
[0047] In actual preparation, such as Figure 3 and Figure 4 As shown, a sheet-like substrate 10 can be provided first, then the first aerosol generating matrix 20 can be bonded to the first surface 11 of the substrate 10, and finally the substrate 10 bonded with the aerosol generating matrix 20 can be rolled up.
[0048] like Figure 3 As shown, the substrate 10 also includes a plurality of through holes 13 connecting the first surface 11 and the second surface 12. When the first aerosol generating matrix 20 is heated and volatilizes to generate aerosol, the aerosol will enter the cavity 130 through the through holes 13, and then escape from the port of the first end 110 along the cavity 130.
[0049] In specific usage, such as Figure 5 As shown, the composite tobacco sheet 100 can be assembled in a tube 200. When the composite tobacco sheet 100 is assembled in the shell 200, the composite tobacco sheet 100 and the shell 200 can form an aerosol generating product. The aerosol generating product is used in conjunction with a suitable aerosol generating device (not shown). The aerosol generating device is provided with a receiving chamber for containing at least part of the aerosol generating product. When the aerosol generating product is contained in the receiving chamber, the aerosol generating device and the aerosol generating product cooperate to generate heat in the substrate 10. At this time, the aerosol generating device and the aerosol generating product are combined to form an aerosol forming system.
[0050] For example, a magnetic field generator can be provided in the aerosol generating device 100. The magnetic field generator can be an induction coil, and the substrate 10 is made of a conductive material, such as aluminum foil, copper foil, silver foil, etc., as described below, or any one of nickel-iron alloy, high-nickel alloy, stainless steel, or pure iron. When the aerosol-generated product is contained in the containing chamber, the controller of the aerosol generating device controls the flow of alternating current to the induction coil, thereby causing the induction coil to generate an alternating magnetic field. The alternating magnetic field penetrates the substrate 10, inducing eddy currents on the substrate 10, and then the substrate 10 generates heat under the action of the eddy currents.
[0051] The housing 200 includes a first section 210, a second section 220, and a third section 230 arranged sequentially and connected along its length. The first section 210 is used to hold the composite tobacco sheet 100. The second section 220 is a cooling section for allowing external cold air to enter the housing 200 through the air inlet 221. The third section 230 is used to contain a filtering substance 240 and is also provided with a filter nozzle for the user to inhale.
[0052] When the user inhales through the filter nozzle in the third section 230, the aerosol generated by the volatilization of the first aerosol generating matrix 20 can enter the cavity 130 through the through hole 13, and then flow further along the cavity 130 to the second section 220, where it mixes with the external cold air for cooling. Finally, the cooled aerosol enters the third section 230 for filtration to remove some unwanted particles. The user can then inhale the cooled and filtered aerosol by inhaling through the filter nozzle in the third section 230.
[0053] In some embodiments, the through holes 13 are arranged in an array.
[0054] In some embodiments, the plurality of through holes 13 may be arranged in a circular, elliptical, racetrack-shaped, rectangular, triangular-hexagonal or other shapes.
[0055] In some embodiments, the plurality of through holes 13 may be arranged in a centrally symmetrical or axisymmetric pattern.
[0056] Furthermore, in some embodiments, the porosity of the plurality of through holes 13 on the substrate 10 is 20%-50%. In some preferred embodiments, the porosity of the plurality of through holes 13 on the substrate 10 is 20%, 25%, 30%, 35%, 40%, 45%, or 50%. This allows aerosols to pass smoothly through the through holes 13 so that the aerosols can flow into the cavity 130.
[0057] In some embodiments, the through-hole 13 is formed by machining or chemical etching. Further in some embodiments, machining includes drilling or laser processing.
[0058] In some embodiments, the thermal conductivity of the substrate 10 is at least 25 W / m·K. In one embodiment of this application, the thermal conductivity of the substrate 10 is 25 W / m·K, 30 W / m·K, 32 W / m·K, 35 W / m·K, 40 W / m·K, or 45 W / m·K.
[0059] In some embodiments, the thickness of the substrate 10 is between 0.005 mm and 0.05 mm. Preferably, the thickness of the substrate 10 is 0.006 mm, 0.01 mm, 0.012 mm, 0.015 mm, 0.020 mm, 0.018 mm, 0.02 mm, 0.025 mm, or 0.03 mm. Within this range, the substrate 10 can maintain a certain structural strength to support the first aerosol generation matrix layer 20 coated thereon, while the thickness of the substrate 10 also allows it to maintain a certain degree of flexibility, enabling it to be rolled from a sheet into a column shape.
[0060] In some embodiments, the substrate 10 may include a sensitive metal or alloy that can be penetrated by a magnetic field and generate heat. When the substrate 10 is in a changing magnetic field, according to the law of electromagnetic induction, the magnetic flux through the substrate 10 changes, generating an induced electromotive force (EMF) within the substrate 10. Since the substrate 10 is a conductor with relatively low resistance, a closed loop is formed inside the substrate 10 under the influence of the induced EMF, generating induced eddy currents. As the eddy currents flow inside the substrate 10, electrical energy is converted into heat energy, causing the temperature of the substrate 10 to rise. This heat then heats the aerosol-forming matrix layer 12.
[0061] In some embodiments, the substrate 10 may include a soft magnetic alloy. Soft magnetic alloys, with their core advantages of high electromagnetic response, low loss, and high saturation magnetization, are widely used in energy conversion and signal processing.
[0062] In some specific embodiments, the substrate 10 includes magnetic foil materials such as aluminum foil, copper foil, and silver foil, or any one of nickel-iron alloy, high-nickel alloy, stainless steel, or pure iron.
[0063] In some embodiments, the first aerosol generating matrix layer 20 includes tobacco extract. The tobacco extract can be obtained by extracting extracts from tobacco leaves and flowers using a solvent, then extracting the extracts with ethanol, followed by drying, dehydration, desalting, and cooking of the raw materials, adding an extract with a special aroma, and performing ultrasonic-assisted extraction to finally obtain a tobacco extract with a specific flavor. In one embodiment of this application, the tobacco extract is mainly used for tobacco flavoring, which can enhance the aroma, reduce off-flavors, and improve cigarette quality. Its aroma is realistic and natural, making it an excellent raw material for cigarette flavoring. Furthermore, tobacco extract can also be used in daily-use fragrances to provide unique aromas and flavors.
[0064] In some embodiments, the main components of tobacco extract include furfuryl alcohol, benzyl alcohol, phytol, solanone, β-turfayne, β-ionone, hexahydrofarnesone, diene, daidzeinone, dihydroactinolone, isopentenone, indole, etc.
[0065] In some embodiments, the components of the first aerosol generating matrix 20 include at least one of tobacco-based and tea-based materials; or at least one of carbon powder and ceramic beads.
[0066] One embodiment of this application provides a method for preparing the composite tobacco sheet 100 described in the above embodiment using a casting process, such as... Figure 6 As shown, the preparation method includes:
[0067] S10, the substrate is placed on the conveyor belt of the casting machine;
[0068] S20, the slurry for forming the aerosol generation matrix is placed in the feed trough of the casting machine;
[0069] S30, start the casting machine so that the substrate passes through the feed trough, and then the slurry is coated on the surface of the substrate to form a semi-finished product;
[0070] S40, the semi-finished product is dried to form composite tobacco sheets;
[0071] S50, the composite tobacco sheet is cut and rolled into a cylindrical shape.
[0072] like Figure 7 As shown, the casting machine 300 includes a conveyor belt 340 and a drive wheel 380. The drive wheel 380 rotates, thereby driving the conveyor belt along... Figure 7 Moving in the direction of the middle arrow, the conveyor belt 340 has a loading end 310 and a unloading end 370 arranged opposite to each other. The casting machine 300 also includes a feed trough 320, a scraper 330, a first heating zone 350 and a second heating zone 360. The feed trough 320 is used to hold the slurry for forming the aerosol generating matrix 20, and the loading end 310 is used to hold the substrate 10.
[0073] Specifically, the substrate 10 can be placed at the loading end 310 manually or through automated equipment, and then the slurry for forming the aerosol generation matrix 20 is placed in the feeding tank 320. The casting machine 300 is started, and the rotating wheel 380 begins to rotate, thereby driving the conveyor belt 340 to move the substrate 10 along the conveying direction of the conveyor belt 340 into the feeding tank 320. The slurry in the feeding tank 320 can then be coated onto the first surface 11 or the second surface 12 of the substrate 10. The substrate 10 coated with slurry further passes through a doctor blade 330, which is used to uniformly coat the slurry onto the surface of the substrate 10 to form a semi-finished product. The distance between the doctor blade 330 and the conveyor belt 340 can also be adjusted to control the thickness of the slurry coating on the substrate 10.
[0074] As the conveyor belt 340 continues to move, the substrate 10 moves further into the first heating zone 350 and the second heating zone 360. The first heating zone 350 and the second heating zone 360 can heat and dry the substrate 10 coated with slurry to evaporate some of the moisture in the slurry coated on the substrate 10, thereby allowing the slurry to bond to the substrate 10 to form a composite tobacco sheet. The composite tobacco sheet formed at this time has a low moisture content, that is, less moisture in the aerosol generating matrix 20. The aerosol generating matrix 20 can be fully heated to volatilize and produce aerosols with better taste.
[0075] After drying, the resulting composite tobacco sheet can be fed from the feeding end 370, and then cut into multiple basic units. The shape of the basic units is not specifically limited; for example, they can be square. Rolling each basic unit together forms the aforementioned hollow cylindrical composite tobacco sheet 100. Rolling the composite tobacco sheet into a hollow cylindrical shape allows the composite tobacco sheet 100 to resemble the shape of a traditional cigarette, without requiring a change in the user's smoking habits.
[0076] In some embodiments, the thickness of the composite tobacco sheet 100 is 0.05 mm to 2.95 mm. This allows the aerosol generating matrix 20 to be sufficiently heated to produce an aerosol with a better taste; it also prevents the aerosol generating matrix 20 from being over-baked and developing a burnt taste. In some embodiments, the distance between the scraper 330 and the conveyor belt 340 can be set between 0.10 mm and 3.00 mm, that is, the height of the scraper 330 can be set between 0.10 mm and 3.00 mm, so that the thickness of the composite tobacco sheet 100 formed after the slurry is dried is between 0.05 mm and 2.95 mm.
[0077] In some embodiments, before placing the substrate 10 on the conveyor belt 340, an appropriate amount of liquid is applied to the conveyor belt 340, or an appropriate amount of liquid is applied to the surface of the substrate 10 facing the conveyor belt 340. Under the action of the liquid, the substrate 10 can fully adhere to the conveyor belt 340, so as to maintain stability during the conveying process and avoid displacement of the substrate 10 during the conveying process. This is beneficial for the uniform coating of the slurry on the substrate 10.
[0078] In some embodiments, the liquid can be any of water, oil, emulsion, etc.
[0079] In some embodiments, at least one heating zone is provided on both sides of the conveyor belt 340. When the substrate 10 moves along the conveyor belt 340 to these heating zones, these heating zones can heat and dry the slurry of the substrate 10 to evaporate at least part of the moisture in the slurry. Since the heating zones are provided on both sides of the conveyor belt 340, these heating zones can dry the slurry from above and below the substrate 10 to improve drying efficiency.
[0080] In some embodiments, each heating zone is configured to be heated independently, so that each heating zone can be set to a corresponding temperature for heating, thereby achieving the optimal heating state by adjusting the temperature of each heating zone, thereby improving drying efficiency.
[0081] In some embodiments, heating areas may be provided only on the first side 341 or the second side 342 of the conveyor belt 340, without the need to provide heating areas on both sides of the conveyor belt 340.
[0082] Specifically, in some embodiments, such as Figure 7 As shown, the conveyor belt 340 has a first side 341 and a second side 342 arranged opposite to each other. The first side 341 is provided with a first heating area 350, and the second side 342 is provided with a second heating area 360. Along the conveying direction of the conveyor belt 340, the first heating area 350 and the second heating area 360 have the same extension length so that the slurry on the substrate 10 can be heated evenly.
[0083] Alternatively, in some embodiments, such as Figure 8As shown, the casting machine 300 includes a first heating region 351a and a second heating region 352a arranged sequentially on the first side 341 of the conveyor belt 340 along the conveying direction of the conveyor belt 340, and a third heating region 360a arranged on the second side 342 of the conveyor belt 340. Along the conveying direction of the conveyor belt 340, the third heating region 360a has a first end 361a and a second end 362a arranged opposite to each other. The first heating region 351a and the second heating region 352a are both located between the first end 361a and the second end 362a.
[0084] Thus, during the movement of the heating region, the substrate 10 can be heated from below by the third heating region 360a, and simultaneously heated from above by the first heating region 351a or the second heating region 352a.
[0085] The first heating region 351a and the second heating region 352a can be as follows: Figure 8 The arrangement shown can be either spaced apart or arranged sequentially adjacent to each other.
[0086] And, in some embodiments, such as Figure 8 As shown, along the conveying direction of the conveyor belt 340, the first heating zone 351a is located upstream of the second heating zone 352a. That is, the substrate 10 first passes through the first heating zone 351a and then through the second heating zone 352a. The heating temperature of the second heating zone 352a is not less than the heating temperature of the first heating zone 351a, and the heating temperature of the third heating zone 360a is not less than the heating temperature of the second heating zone 352a. This method achieves a better drying effect.
[0087] In some specific embodiments, the heating temperatures of the first heating region 351a, the second heating region 352a, and the third heating region 360a are the same.
[0088] Alternatively, in some specific embodiments, the heating temperature of the first heating region 351a is lower than the heating temperature of the second heating region 352a, and the heating temperature of the second heating region 352a is lower than the heating temperature of the third heating region 360a.
[0089] And, in some embodiments, such as Figure 8As shown, the substrate 10 is disposed on the first side 341 of the conveyor belt 340, that is, the substrate 10, the first heating area 351a and the second heating area 352a are located on the same side, while the third heating area 360a is located separately on the second side 342 of the conveyor belt 340. Thus, the second heating area 360a and the substrate 10 are separated by the conveyor belt 340. In other words, the third heating area 360a heats and bakes the substrate 10 through the conveyor belt 340. This method can improve the uniformity of heating and baking the substrate 10.
[0090] In some embodiments, the first heating zone 351a has a heating temperature of 50°C to 80°C, the second heating zone 352a has a heating temperature of 60°C to 90°C, and the third heating zone 360a has a heating temperature of 70°C to 120°C, and the heating time is 25 mins to 90 mins. The heating temperature and heating time are set as described above in the through hole so that the slurry of the substrate 10 has a suitable moisture content after drying. The suitable moisture content allows the aerosol generating matrix 20 to volatilize and generate aerosol with a better taste after being heated.
[0091] In some embodiments, such as Figure 9 As shown, three baffles 390 are also provided at the scraper 330. The baffles 390 and the scraper 330 together form a feed trough 320. The slurry is placed in the feed trough 320 in the direction indicated by arrow A. So when the slurry enters the feed trough 320, the baffles 390 can surround the slurry to the scraper 320, which is beneficial for the scraper 320 to evenly coat the slurry on the surface of the substrate 10.
[0092] It should be noted that the preferred embodiments of this application are given in the specification and accompanying drawings, but are not limited to the embodiments described in this specification. Furthermore, those skilled in the art can make improvements or modifications based on the above description, and all such improvements and modifications should fall within the protection scope of the appended claims.
Claims
1. A method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix capable of generating heat, the matrix being constructed as a hollow column, the composite tobacco sheet further comprising an aerosol generating matrix bonded to the matrix and capable of being heated by the matrix to generate aerosols, characterized in that, The method for preparing the composite tobacco sheet includes: The substrate is placed on the conveyor belt of the casting machine; The slurry used to form the aerosol generation matrix is placed in the feed trough of the casting machine; The casting machine is started so that the substrate passes through the feed trough, and the slurry is coated on the surface of the substrate to form a semi-finished product; The semi-finished product is dried to form composite tobacco sheets; The composite tobacco sheet is cut and rolled into a cylindrical shape.
2. The preparation method according to claim 1, characterized in that, The step of starting the casting machine to allow the substrate to pass through the feed trough, thereby coating the substrate surface with the slurry to form a semi-finished product, specifically includes: The slurry is applied to the substrate surface using a scraper.
3. The preparation method according to claim 2, characterized in that, The distance between the scraper and the conveyor belt is 0.10mm to 3.00mm.
4. The preparation method according to claim 2, characterized in that, A baffle plate is provided at the scraper position, and the baffle plate and the scraper together form the feed trough, and the baffle plate surrounds the slurry to the scraper.
5. The preparation method according to claim 1, characterized in that, The step of placing the substrate on the conveyor belt of the casting machine specifically includes: The substrate is bonded to the conveyor belt using a liquid.
6. The preparation method according to claim 1, characterized in that, In the step of drying the semi-finished product to form composite tobacco sheets, Heating zones are provided on both sides of the conveyor belt, and the heating zones are used to dry the slurry coated on the substrate.
7. The preparation method according to claim 6, characterized in that, The transmission belt has a first side and a second side arranged opposite to each other. The first side is provided with a first heating area, and the second side is provided with a second heating area. Along the transmission direction of the transmission belt, the first heating area and the second heating area have the same extension length.
8. The preparation method according to claim 6, characterized in that, The conveyor belt has a first side and a second side arranged opposite to each other. The first side is provided with a first heating area and a second heating area arranged sequentially along the conveying direction. The second side is provided with a third heating area. The third heating area has a first end and a second end arranged opposite to each other along the conveying direction. The first heating area and the second heating area are both located between the first end and the second end.
9. The preparation method according to claim 8, characterized in that, Along the conveying direction of the conveyor belt, the first heating area is located upstream of the second heating area, the heating temperature of the second heating area is not less than the heating temperature of the first heating area, and the heating temperature of the third heating area is not less than the heating temperature of the second heating area.
10. The preparation method according to claim 9, characterized in that, The substrate is located on the first side of the conveyor belt.
11. The preparation method according to claim 9, characterized in that, The first heating zone has a heating temperature of 50℃ to 80℃, the second heating zone has a heating temperature of 60℃ to 90℃, the third heating zone has a heating temperature of 70℃ to 120℃, and the heating time is 25 mins to 90 mins.
12. The preparation method according to claim 1, characterized in that, The thickness of the composite tobacco sheet is 0.05mm to 2.95mm.
13. The preparation method according to claim 1, characterized in that, The substrate is a porous and flexible magnetic foil material.
14. An aerosol-generating product, characterized in that, include: The shell has a first section, a second section, and a third section arranged sequentially and interconnected along its length; The composite tobacco sheet is prepared by the preparation method according to any one of claims 1-13; The composite smoke sheet is disposed in the first section, the second section is provided with an air inlet that communicates with the outside, the air inlet allows outside air to enter to cool the aerosol, and the third section is provided with a filter material for filtering the aerosol.
15. An aerosol generation system, characterized in that, Includes the aerosol generating article as described in claim 14, and an aerosol generating apparatus for containing at least a portion of the aerosol generating article; When the aerosol generating product is housed in the housing chamber, the aerosol generating product and the aerosol generating device cooperate with each other to generate heat in the substrate.