Method of manufacturing a composite tobacco sheet, aerosol-generating article and system
By combining aerosols with both sides of the matrix layer to form a matrix layer, the problem of insufficient aroma release in existing aerosol-generated products has been solved, achieving high aerosol concentration and good taste.
Patent Information
- Application Number
- CN202510669717.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-22
- Publication Date
- 2026-11-24
AI Technical Summary
Existing aerosol-generating products take a long time to volatilize and produce aerosols without combustion, resulting in insufficient aroma release and poor aerosol taste.
The method for preparing composite smoke sheets includes a base layer and aerosol-generating matrix layers on both sides. The slurry is bonded to the surface of the base layer through casting, rolling or spraying processes, and the aerosol matrix layers on both sides are formed by casting process. After drying, composite smoke sheets are formed.
It increases the concentration and aroma release of aerosols, improves the taste of aerosols, and reduces user waiting time.
Smart Images

Figure CN123147686A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of heated non-combustible aerosol generation technology, and in particular to a method for preparing composite tobacco sheets, as well as an aerosol generation product and system having the composite tobacco sheets. Background Technology
[0002] Tobacco products (e.g., cigarettes, cigars, etc.) produce tobacco smoke by burning tobacco during use. Efforts are being made to replace these tobacco-burning products by creating products that release compounds without combustion. An example of such a product is an aerosol generating device that releases compounds by heating an aerosol generating product used in conjunction with it. This aerosol generating product may, for example, be tobacco or other non-tobacco products, which may or may not contain nicotine.
[0003] The aerosol generating device is equipped with a heating element that generates heat, which is then transferred to the aerosol generating product. When heated, the aerosol generating product volatilizes to produce aerosols. However, the existing aerosol generating products take a long time to volatilize and produce aerosols, resulting in insufficient aroma release and poor aerosol taste. Summary of the Invention
[0004] This application provides a method for preparing a composite tobacco sheet, as well as an aerosol generating article and system having the composite tobacco sheet, to prepare a composite tobacco sheet capable of increasing aerosol concentration and fully releasing aroma. At least one embodiment of this application provides a method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix layer capable of generating heat, and a first aerosol generating matrix layer and a second aerosol generating matrix layer bonded to both sides of the matrix layer and capable of being heated by the matrix layer to generate aerosols. The method for preparing the composite tobacco sheet includes:
[0005] Provide a matrix layer;
[0006] The slurry used to form the aerosol generation matrix is bonded to one side surface of the matrix layer to form a semi-finished product with an aerosol matrix layer on one side.
[0007] Using a casting process, the slurry is poured onto the other side surface of the substrate layer to form a semi-finished product with aerosol matrix layers on both sides;
[0008] The semi-finished product with aerosol matrix layers on both sides is dried to form composite tobacco sheets.
[0009] In some embodiments, the thickness of the composite tobacco sheet is 0.2 mm to 2 mm.
[0010] In some embodiments, the moisture content of the composite tobacco sheet is 4% to 8%.
[0011] In some embodiments, the slurry comprises at least one of microcrystalline cellulose, silica, kaolin, calcium carbonate, and ceramic beads, and at least one of glycerol, glycerol, propylene glycol, diethylene glycol, triethylene glycol, and tetraethylene glycol.
[0012] In some embodiments, in the step of casting the slurry onto the other side surface of the substrate layer using a casting process to form a semi-finished product with aerosol matrix layers on both sides, the preparation method specifically includes:
[0013] Pour 0.001g to 0.8g of slurry onto the other side surface of the substrate layer;
[0014] The slurry is baked at 60℃ to 105℃ for 1 to 10 minutes, or the slurry is air-dried naturally.
[0015] In some embodiments, the step of bonding the slurry to one side surface of the matrix layer to form a semi-finished product having an aerosol matrix layer on one side specifically includes:
[0016] The slurry is bonded to one side surface of the substrate layer by any of the following processes: casting, rolling, or spraying.
[0017] In some embodiments, when the slurry is bonded to one side surface of the substrate layer using a casting process...
[0018] The slurry is bonded to one side surface of the substrate layer using a casting machine, the casting process comprising:
[0019] The substrate layer is placed on the conveyor belt of the casting machine;
[0020] The slurry used to form the aerosol matrix layer is placed into the feed trough of the casting machine so that the slurry is coated on one side surface of the matrix layer.
[0021] In some embodiments, the casting machine includes heating zones disposed on both sides of the conveyor belt, through which a semi-finished product having an aerosol-generating matrix on one side passes for drying.
[0022] In some embodiments, the heating area includes a first heating area and a second heating area disposed above the conveyor belt, and a third heating area disposed below the conveyor belt; and, along the conveying direction of the conveyor belt, the third heating area has a first end 271 and a second end 272 opposite to each other, the first heating area is located upstream of the second heating area, and both the first heating area and the second heating area are located between the first end 271 and the second end 272.
[0023] In some embodiments, the heating temperature of the first heating zone 250 is 60°C to 80°C, the heating temperature of the second heating zone 260 is 70°C to 90°C, the heating temperature of the third heating zone 270 is 80°C to 120°C, and the total time for the semi-finished product with an aerosol generating matrix on one side in the heating zone is 30 mins to 80 mins.
[0024] In some embodiments, the step of placing the substrate layer on the conveyor belt of the casting machine specifically includes:
[0025] Liquid is sprayed onto the conveyor belt of the casting machine to cover the substrate layer within the liquid spraying area of the conveyor belt.
[0026] In some embodiments, when the slurry is bonded to one side surface of the substrate layer using a casting process, the casting process includes:
[0027] The substrate layer is bonded to the flat plate with water;
[0028] The slurry for forming the aerosol generation matrix is placed in the feed trough of the coating machine, and the coating machine is driven to move between a first position and a second position on a heated plate to coat the slurry onto one side surface of the substrate layer.
[0029] In some embodiments, the plate is a heated plate, and after the steps of covering the substrate layer with slurry and coating one side surface of the substrate layer with slurry using a coating applicator, the casting process further includes:
[0030] The slurry coated on one side of the substrate layer is dried using the heating plate at a temperature of 50°C to 90°C for a time of 35 mins to 90 mins.
[0031] In some embodiments, prior to the step of casting the slurry onto the other side surface of the substrate layer using a casting process to form a semi-finished product with aerosol matrix layers on both sides, the preparation method further includes:
[0032] The semi-finished product with an aerosol matrix layer on one side is punched to form a prefabricated composite tobacco sheet;
[0033] The step of casting slurry onto the other side surface of the substrate layer using a casting process to form a semi-finished product with aerosol matrix layers on both sides specifically includes:
[0034] The prefabricated composite smoke sheet is cast using a casting process to form a semi-finished product with aerosol matrix layers on both sides of the matrix layer.
[0035] In some embodiments, the substrate layer has multiple through holes.
[0036] In some embodiments, the sum of the opening areas of the through holes occupies 30-50% of the surface area of the substrate layer.
[0037] In some embodiments, the thickness of the substrate layer is 0.05 mm to 0.15 mm.
[0038] In some embodiments, the combined thickness of the matrix layer and the aerosol-generating matrix layer on either side of the composite tobacco sheet is 0.15 mm to 1.20 mm.
[0039] In some embodiments, the step of using a casting process to pour slurry onto the other side surface of the substrate layer to form a semi-finished product with aerosol matrix layers on both sides specifically includes:
[0040] A mold is provided, the mold including a receiving groove;
[0041] The semi-finished product with an aerosol matrix layer on one side is placed in the receiving tank, with the other side surface of the matrix layer facing the opening of the receiving tank;
[0042] Slurry is poured into the receiving tank to form an aerosol matrix layer on the other side of the substrate layer.
[0043] At least one embodiment of this application also provides an aerosol generating article, comprising:
[0044] Multiple composite tobacco sheets, wherein the composite tobacco sheets are prepared by the preparation method described in the above embodiments;
[0045] A carrier is used to support the composite tobacco sheets, and a plurality of the composite tobacco sheets are held on the carrier.
[0046] In some embodiments, the carrier is configured as a hollow box-shaped body, the hollow region of the box-shaped body being used to receive the aerosol, the box-shaped body having an air inlet for air to enter the hollow region and an air outlet for the aerosol to escape from the box-shaped body.
[0047] At least one embodiment of this application also provides an aerosol generation system, comprising:
[0048] The aerosol-generated products described in the above embodiments;
[0049] An aerosol generating apparatus is provided with a receiving chamber for containing the aerosol generating article. When the aerosol generating article is contained in the receiving chamber, the aerosol generating apparatus and the aerosol generating article cooperate to generate heat in the substrate layer.
[0050] The aerosol generating device further includes a suction nozzle, which defines an outlet for aerosols to escape from the aerosol generating device.
[0051] The preparation method provided in the above embodiments involves bonding the slurry to one side of the substrate layer, and then casting the slurry to the other side of the substrate layer through a casting process, thereby forming a semi-finished product with aerosol generation matrix layers on both sides. The semi-finished product is then dried to form a composite tobacco sheet with aerosol generation matrix layers on both sides. The heat generated by the substrate layer of the composite tobacco sheet can heat both sides of the aerosol generation matrix layers, thereby increasing the concentration of aerosols. Attached Figure Description
[0052] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.
[0053] Figure 1 This is a three-dimensional schematic diagram of a composite tobacco sheet provided in an embodiment of this application;
[0054] Figure 2 Figure 1 A three-dimensional schematic diagram of the matrix layer of composite tobacco sheets in one direction;
[0055] Figure 3 This is a schematic diagram of a method for preparing composite tobacco sheets according to an embodiment of this application;
[0056] Figure 4 This is an embodiment provided by this application. Figure 3 A schematic diagram of the casting machine used in the preparation method; Figure 5 This is an embodiment provided by this application. Figure 3 A schematic diagram of the coating apparatus used in the preparation method at one angle;
[0057] Figure 6 yes Figure 5 A schematic diagram of the intermediate coating device from another angle;
[0058] Figure 7 This is an embodiment provided by this application. Figure 3 A flowchart detailing the steps in step S30 of the preparation method;
[0059] Figure 8 This is an embodiment provided by this application. Figure 3 A schematic diagram of the casting system used in the preparation method at one angle;
[0060] Figure 9This is a schematic diagram of the structure of an aerosol generation system provided in an embodiment of this application;
[0061] Figure 10 This is a schematic diagram of the structure of an aerosol-generated article provided in an embodiment of this application. Detailed Implementation
[0062] To facilitate understanding of this application, a more detailed description of this application will be provided below in conjunction with the accompanying drawings and specific embodiments.
[0063] One embodiment of this application provides a composite tobacco sheet capable of generating an aerosol by heating. In some embodiments, part or all of the composite tobacco sheet is intended to be consumed by a user during use by heating.
[0064] For example Figure 1 A schematic diagram of a composite tobacco sheet 100 according to one embodiment is shown; in this embodiment, the composite tobacco sheet 100 is substantially constructed in a sheet or block shape. For example, in some alternative embodiments, the composite tobacco sheet 100 has a length of approximately 1 to 100 cm, a width of 2 to 30 mm, and a thickness of approximately 0.1 mm to 2 mm. Figure 1 In one embodiment, the composite tobacco sheet 100 is configured as a square shape; or in some other variations, the composite tobacco sheet 100 is configured as a circular, elliptical, trapezoidal, polygonal, or other shapes.
[0065] In some embodiments, the areal density of the composite tobacco sheet 100 is 100–600 g / m³. 2 .
[0066] In some embodiments, the tensile strength of the composite smoke sheet 100 is greater than 1.5 kN / m.
[0067] exist Figure 1 In some embodiments, the composite tobacco sheet 100 has a laminated structure and is configured to include multiple layers formed by lamination. For example, in Figure 1 In this context, the composite tobacco sheet 100 may include:
[0068] A first aerosol generating matrix layer 110, a substrate layer 120, and a second aerosol generating matrix layer 130 are arranged in a stacked or laminated manner, with the substrate layer 120 located between the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 120.
[0069] Please continue reading. Figure 1 In conjunction with reference Figure 2 The substrate layer 120 has a thickness direction ( Figure 2(In the direction of the middle arrow X) the first surface 121 and the second surface 122 are set opposite to each other, the first aerosol generating matrix layer 110 is bonded to the first surface 121, and the second aerosol generating matrix is bonded to the second surface 122.
[0070] In this embodiment, the substrate layer 120 is thermally conductive. In one specific embodiment, for example, the substrate layer 120 comprises a metallic or non-metallic material suitable for having a suitable high thermal conductivity; in one specific embodiment, the thermal conductivity of the substrate layer 120 is at least 25 W / m·K, preferably or at least 80 W / m·K; in one specific embodiment, the substrate layer 120 may comprise copper, iron, aluminum, tin, stainless steel, or an alloy containing at least one of these. In use, the substrate layer 130 can be heated directly or indirectly, for example, by thermal conduction or electromagnetic induction, which in turn reheats the first aerosol-generating matrix layer 110 and the second aerosol-generating matrix layer 130 to generate an aerosol.
[0071] Since the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 are both bonded to the matrix layer 120, and both the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 are in direct contact with the matrix layer 120, the heat generated by the matrix layer 120 can directly heat the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130. This allows the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 to be heated quickly and volatilize in time to generate aerosols, achieving an immediate inhalation effect, reducing the user's waiting time, and producing a rich aerosol concentration with full aroma release and good aerosol taste.
[0072] In some embodiments, the substrate layer 120 has a thickness of 0.05 mm to 0.15 mm; and in some embodiments, the substrate layer 120 is rigid or hard, and is not easily bent or rolled. The rigidity of the substrate layer 120 allows the composite tobacco sheet 100 to have a flat sheet structure. In some embodiments, the substrate layer 120 can serve as a carrier structure for the aerosol generation matrix layer, supporting and bearing the aerosol generation matrix layer, which can be attached, bonded, or coated onto the surface of the substrate layer 120.
[0073] In some embodiments, the sum of the thicknesses of the substrate layer 120 and the first aerosol generating layer 110 or the second aerosol generating layer 130 is 0.15 mm to 1.20 mm.
[0074] In some preferred embodiments, the first surface 121 and / or the second surface 122 of the substrate layer 120 are non-smooth; for example, the first surface 121 and / or the second surface 122 are rough; for example, the surface of the substrate layer 120 of the metal or alloy foil is surface-processed by at least one process such as corona, electrochemical etching, indentation, or sanding, thereby forming a rough surface on the surface of the substrate layer 120, such as a sanded surface; the rough surface of the substrate layer 120 is advantageous for maintaining a tight bond with the first aerosol generating matrix layer 110 and / or the second aerosol generating matrix layer 130.
[0075] In some embodiments, the first aerosol generating matrix layer 110 or the second aerosol generating matrix layer 130 can be used to refer to a matrix capable of releasing volatile compounds that can form aerosols. The volatile compounds can be released to generate aerosols by heating the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130. In some embodiments, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 are or may include solids at room temperature.
[0076] In some embodiments, the first aerosol generating matrix layer 110 or the second aerosol generating matrix layer 130 may include one or more of the following: vanilla leaves, tobacco leaves, homogenized tobacco, expanded tobacco, powder, granules, fragments, strips, or flakes; or, the solid first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 may contain additional tobacco or non-tobacco volatile flavor compounds to be released when the matrix is heated.
[0077] In some specific embodiments, the first aerosol generating matrix layer 110 or the second aerosol generating matrix layer 130 may include an active substrate; the active substrate includes or is derived from one or more plant products or components thereof; for example, in some specific embodiments, the active substrate includes plant leaves, bark, fibrous tissue, stems, roots, petals, fruits, etc.; for example, in one specific embodiment, the active substrate includes or is derived from one or more plant varieties or their components, derivatives, or extracts, and the plant variety is tobacco. For example, in one specific embodiment, the active substrate includes a mixture of tobacco and plants such as traditional Chinese medicine. The active substrate may include tobacco or tobacco-containing materials; for example, the active substrate may include any of the following: tobacco leaves, tobacco vein fragments, reconstituted tobacco, homogenized tobacco, extruded tobacco, tobacco slurry, cast tobacco, and expanded tobacco.
[0078] In some alternative embodiments, the first aerosol generating matrix layer 110 or the second aerosol generating matrix layer 130 further includes: a flavoring agent; the flavoring agent may comprise volatile aroma components. For example, in typical embodiments, the flavoring agent may provide an aroma selected from menthol, lemon, vanilla, orange, wintergreen, cherry, and cinnamon; the flavoring agent may include volatile tobacco flavoring compounds released from the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 upon heating.
[0079] In some optional embodiments, the first aerosol-generating matrix layer 110 or the second aerosol-generating matrix layer 130 further includes an aerosol forming agent or a smoke generator; the aerosol forming agent or smoke generator contributes to the densification and stabilization of aerosol formation during use. In some specific embodiments, the aerosol forming agent or smoke generator is or includes at least one of glycerol, glycerol, propylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, etc.
[0080] In some optional embodiments, the first aerosol generating matrix layer 110 or the second aerosol generating matrix layer 130 further includes an adhesive; the adhesive promotes the bonding of the components in the aerosol generating matrix 120 during use; for example, in some specific embodiments, the adhesive is or includes at least one of gum arabic, casein, dextrin, sodium carboxymethyl cellulose, starch, polyvinyl alcohol, guar gum, etc.
[0081] In some optional embodiments, the first aerosol generating matrix layer 110 or the second aerosol generating matrix layer 130 further includes reinforcing fibers; the reinforcing fibers typically have a higher fiber strength than the tobacco plant fibers in the active substrate, thereby enhancing the strength and plasticity of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 during use. For example, in some specific embodiments, the reinforcing fibers include at least one of coniferous wood fibers, broadleaf wood fibers, hemp fibers or flax fibers, bamboo fibers, etc.
[0082] In some embodiments, the thicknesses of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 may be the same or different.
[0083] In one specific embodiment, the substrate layer 120 is heated by electromagnetic induction. When the composite tobacco sheet 100 is placed into the aerosol generating device used with it, the induction coil in the aerosol generating device will generate a changing magnetic field under the action of alternating current. This changing magnetic field will pass through the substrate layer 120, thereby generating induced eddy currents on the substrate layer 120, and then generating heat under the action of the eddy currents.
[0084] At this time, when the composite tobacco sheet 100 is placed into the aerosol generating device, if the second surface 122 of the substrate layer 120 faces the induction coil, the thickness of the second aerosol generating matrix layer 130 bonded to the second surface 122 is not greater than the thickness of the first aerosol generating matrix layer 110 bonded to the first surface 121, so as to avoid the first aerosol generating matrix layer 110 being overheated and producing a burnt taste.
[0085] It is easy to understand that when the composite tobacco sheet 100 is placed into the aerosol generating device, if the first surface 121 of the substrate layer 120 faces the induction coil, the thickness of the first aerosol generating matrix layer 110 bonded to the first surface 121 is not greater than the thickness of the second aerosol generating matrix layer 120 bonded to the second surface 121, so as to avoid the second aerosol generating matrix layer 120 being overheated and producing a burnt taste.
[0086] In some embodiments, such as Figure 2 As shown, the substrate layer 120 also includes a plurality of through holes 123 connecting the first surface 121 and the second surface 122. By providing the through holes 123, aerosols generated by the heating and volatilization of the first aerosol generating matrix layer 110 or the second aerosol generating matrix layer 130 can escape through the through holes 123. In this embodiment, the substrate layer 120 is square, so the plurality of through holes 123 can be arranged in a rectangular array. In some other embodiments, the substrate layer 120 is circular, so the plurality of through holes 123 can be arranged in a ring array.
[0087] In some embodiments, the sum of the opening areas of the plurality of through holes 123 occupies 30-50% of the surface area of the first surface 121 or the second surface 122. Furthermore, it should be noted that the design of the porosity on the substrate layer 120 and the distribution of the through holes 123 can also adjust the temperature field distribution on the substrate layer 120. For example, providing through holes 123 in high-temperature regions can effectively prevent heat concentration in the substrate layer 120 in those regions; furthermore, by adjusting the porosity in high-temperature regions, the amount of heat generation and transfer can also be controlled.
[0088] Furthermore, in some embodiments, the through-hole 123 has a diameter of 0.5 mm to 3 mm, which is advantageous for the smooth passage of aerosols through the through-hole 123.
[0089] Figure 3 A schematic diagram of a method for preparing a composite tobacco sheet 100 with a laminated structure is shown in one embodiment; according to Figure 3 As shown, the preparation method includes:
[0090] S10 provides a substrate layer 120;
[0091] S20, the slurry used to form the aerosol generation matrix is bonded to one side surface of the matrix layer to form a semi-finished product with an aerosol matrix layer on one side;
[0092] In some embodiments, the slurry used to form the aerosol generation matrix can be bonded to one side surface of the substrate layer 120, that is, bonded to the first surface 121 or the second surface 122 of the substrate layer 120, by processes such as rolling, casting, and spraying.
[0093] In some embodiments, when a casting process is employed, a casting machine can be used to deposit the first aerosol generation matrix 110 onto the first surface 121. For example... Figure 4 As shown, the casting machine 200 includes a conveyor belt 210 and a drive wheel 220. The drive wheel 220 rotates, thereby driving the conveyor belt along... Figure 4 Moving in the direction of the middle arrow, the conveyor belt 210 has a loading end 211 and a unloading end 212 arranged opposite to each other. The casting machine 200 also includes a feed trough 230, a scraper 240, a first heating zone 250, a second heating zone 260 and a third heating zone 270. The feed trough 230 is used to place the slurry that forms the aerosol generation matrix, and the loading end 211 is used to place the matrix layer 120.
[0094] In the specific preparation process, firstly, the height of the doctor blade 240 of the casting machine is adjusted. The substrate layer 120 is placed at the feeding end 211 of the conveyor belt 210, and then the prepared slurry is placed into the feed trough 230. The casting machine is started, and the rotating wheel 220 begins to rotate, thereby driving the conveyor belt 210 to begin conveying. The substrate layer 120 can then move along the conveyor belt. When the substrate layer 120 moves into the feed trough 230, the slurry in the feed trough 230 can be coated onto the first surface 121 of the substrate layer 120. As the conveyor belt 210 continues to convey, the substrate layer 120 continues to move to the doctor blade 240. There is a certain distance between the doctor blade 240 and the conveyor belt 210, that is, the doctor blade 240 has a certain height. This height is set according to the thickness of the composite tobacco sheet to be prepared.
[0095] When the substrate moves to the scraper 240, the scraper 240 can scrape the slurry coated on the substrate layer 120, so that the slurry is evenly coated on the first surface 121 of the substrate layer 120, that is, the thickness of the slurry coated on the substrate layer 120 is basically the same. At this time, a semi-finished product with an aerosol generation matrix layer on one side surface of the substrate layer 120 is formed.
[0096] like Figure 4As shown, the first heating region 250 and the second heating region 260 are located on one side of the conveyor belt 210, that is, above the conveyor belt 210, while the third heating region 270 is located on the other side of the conveyor belt 210, that is, below the conveyor belt 210. The first heating region 250 and the second heating region 260 are arranged sequentially along the conveying direction of the conveyor belt 210, meaning the first heating region 250 is upstream of the second heating region 260. Along the conveying direction of the conveyor belt 210, the third heating region 270 has a first end 271 and a second end 272 that are oppositely disposed, with both the first heating region 250 and the second heating region 260 located between the first end 271 and the second end 272.
[0097] When the conveyor belt 210 transports the substrate layer 120 to the heating zone, the heating zone heats the semi-finished product formed above, that is, it dries the slurry on the first surface 121 of the substrate layer 120, causing some of the water in the slurry to evaporate, thereby making the dried slurry tightly bonded to the first surface 121 of the substrate layer 120. In this embodiment, when the conveyor belt 210 transports the substrate layer 120 to the heating zone, the substrate layer 120 can be heated from below by the third heating zone 270, and simultaneously heated from above by the first heating zone 250 or the second heating zone 260, thereby heating the substrate layer 120 from both sides to improve the drying efficiency of the slurry.
[0098] After the slurry has dried, the conveyor belt 210 can transport the substrate layer 120 to the discharge end 212.
[0099] In some embodiments, the heating temperature of the first heating region 250 is 60°C to 80°C, the heating temperature of the second heating region 260 is 70°C to 90°C, the heating temperature of the third heating region 270 is 80°C to 120°C, and the total duration of the substrate layer 120 in the heating region is 30 mins to 80 mins.
[0100] In some embodiments, before placing the substrate layer 120 on the conveyor belt 210, liquid is sprayed onto the conveyor belt 210 of the casting machine 200, covering the substrate layer 120 within the liquid spraying area. This allows the substrate layer 100 to fully adhere to the conveyor belt 210 under the action of the liquid's tension and adsorption force, thus maintaining stability during conveying and preventing displacement of the substrate layer 120 during conveying. This is beneficial for the uniform coating of the slurry onto the substrate layer 120.
[0101] The liquid can be any of the following: water, oil, emulsion, etc.
[0102] In some embodiments, when a casting process is used to bond the slurry for forming an aerosol generation matrix to one side surface of the substrate layer 120, a combination of a heated plate 300 and a coating device 400 can also be used.
[0103] like Figure 5 As shown, the heating plate 300 includes a first surface 310 and a second surface 320 disposed opposite to each other. The first surface 310 is used to place the substrate layer 120. A heating element (not shown) is disposed between the first surface 310 and the second surface 320. The heating element generates heat when it is powered on, and the heat is further conducted to the first surface 310, thereby raising the temperature of the first surface 310.
[0104] In some embodiments, the heating plate 300 is made of a material with high thermal conductivity, so that the heat generated by the heating element can be quickly conducted to the first surface 310, and the temperature of the first surface 310 can rise rapidly. The material with high thermal conductivity can be any of the following: a metallic material such as silver, copper, aluminum, or pure iron, or a non-metallic material such as diamond or graphene.
[0105] A coating applicator 400 is a device or tool used to uniformly apply paint, ink, adhesive, or other liquid materials to the surface of an object, such as... Figure 5 and Figure 6 As shown, the coating applicator 400 includes a doctor blade 410, an adjustment section 420, and a feed trough 430. The feed trough 430 is used to hold the slurry that forms the aerosol generation matrix. The doctor blade 410 is used to coat the slurry onto the substrate layer 120, and the adjustment section 420 is used to adjust the distance between the doctor blade 410 and the first surface 310 of the heating plate 300, that is, to adjust the height of the doctor blade 410. Figure 6 The mid-distance d is shown.
[0106] Specifically, in the preparation process, the substrate layer 120 is first bonded to the heating plate 300 with water to ensure full adhesion. Then, the slurry is poured into the feed trough 430, and the scraper 420 is adjusted to the preset height. Finally, the coating device 400 is driven along... Figure 5 and Figure 6 The middle arrow moves from the first position to the second position. During the movement, the scraper 420 can coat the slurry onto the substrate layer 120.
[0107] After the coating applicator 400 moves to the second position, the slurry coated on the substrate layer 120 is inspected. If the slurry coating is uneven, the coating applicator 400 is driven to move from the second position to the first position until the slurry is evenly coated on one side surface of the substrate layer 120. At this point, a semi-finished product with an aerosol-generating matrix layer on one side surface of the substrate layer 120 is formed. If the slurry coating is uniform, it is not necessary to drive the coating applicator 400 from the second position to the first position again.
[0108] In some embodiments, after coating is completed, the heating plate 400 is activated to heat and dry the semi-finished product, so that some of the moisture in the slurry evaporates, and the dried slurry can then be tightly bonded to the surface of a layer of the substrate layer 120. Specifically, heating and drying can be carried out by controlling the heating temperature and heating time of the heating plate 400. Once the heating time is reached, drying is complete.
[0109] In some embodiments, the drying temperature of the heating plate 400 is 50°C to 90°C, and the drying time is 35 mins to 90 mins.
[0110] It should be noted that when applying the slurry to one side surface of the substrate layer 120 using the coating applicator 400, a flat plate without heating function can also be used. After coating, the substrate layer 120 is then transferred to a drying oven for drying.
[0111] S30, using a casting process, the slurry is poured onto the other side surface of the substrate layer to form a semi-finished product with aerosol matrix layers on both sides;
[0112] S40, the semi-finished product with aerosol matrix layers on both sides is dried to form a composite smoke sheet. After obtaining a semi-finished product with an aerosol generating matrix layer bonded to one side surface of the substrate layer 120 through the above-mentioned processes such as casting, rolling, or spraying, the slurry can be poured onto the other side surface of the substrate layer 120 using any of the following: disposable dropper, dropper tip, pipette, pipette gun, syringe, dispensing machine, etc., thereby forming a semi-finished product with aerosol generating matrix layers on both sides of the substrate layer 120. Then, the semi-finished product with aerosol generating matrix layers on both sides is dried to form a composite smoke sheet.
[0113] It should be noted that after forming a semi-finished product with an aerosol generating matrix layer on one side of the substrate layer 120, drying of the semi-finished product is not necessary. Drying can be carried out after forming a semi-finished product with aerosol generating matrix layers on both sides. Through the preparation method of steps S10 to S40 above, a composite tobacco sheet 100 with aerosol generating matrix layers bonded to both the first surface 121 and the second surface 122 of the substrate layer 120 can be prepared. Thus, the heat generated by the substrate layer 120 can heat both sides of the aerosol generating matrix layer, thereby increasing the concentration of aerosols, fully releasing the aroma, and improving the aerosol taste. In some embodiments, the composite tobacco sheet 100 needs to have a suitable thickness. If the thickness is too thin, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 are easily overheated and produce a burnt taste; while if the thickness is too thick, the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 are not heated sufficiently, affecting the taste. Therefore, in some embodiments, after the slurry is dried, the composite tobacco sheet 100 has a thickness of 0.2 mm to 2 mm.
[0114] In some embodiments, the composite tobacco sheet 100 has a moisture content of 4% to 8%, so that the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130 can be heated and volatilized into an aerosol that produces a better taste. Too high a moisture content can lead to insufficient heating, while too low a moisture content can lead to over-baking, both of which result in a poor taste of the aerosol. When specifically measuring the moisture content, a rapid moisture meter can be used to measure the moisture content of the composite tobacco sheet 100.
[0115] In some embodiments, the slurry comprises at least one of microcrystalline cellulose, silica, kaolin, calcium carbonate, and ceramic beads, and at least one of glycerol, glycerol, propylene glycol, diethylene glycol, triethylene glycol, and tetraethylene glycol. Glycerol, glycerol, propylene glycol, diethylene glycol, triethylene glycol, and tetraethylene glycol are volatile upon heating to generate aerosols, while microcrystalline cellulose, silica, kaolin, calcium carbonate, and ceramic beads are used to adsorb glycerol, glycerol, propylene glycol, diethylene glycol, triethylene glycol, and tetraethylene glycol.
[0116] In some embodiments, the slurry also includes at least one of sodium alginate and konjac gum, which can increase the viscosity of the slurry and facilitate its adhesion to the substrate layer 120.
[0117] In some embodiments, steps S30 and S40 specifically include:
[0118] S31, pour 0.001g to 0.8g of slurry onto the other side surface;
[0119] S41, the slurry is baked at a temperature of 60℃~105℃ for 1~10 minutes.
[0120] If too much slurry is poured and dried, the composite tobacco sheet 100 will be too thick, which will result in insufficient heating of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130. If too little slurry is poured and dried, the composite tobacco sheet 100 will be too thin, which will result in over-baking of the first aerosol generating matrix layer 110 and the second aerosol generating matrix layer 130, resulting in a burnt taste.
[0121] Once the amount of slurry poured is determined, the temperature and duration of the subsequent drying process will also affect the thickness of the composite tobacco sheet 100. A higher drying temperature and longer drying time will result in a thinner final thickness of the composite tobacco sheet 100; conversely, a lower drying temperature and shorter drying time will result in a thicker final thickness of the composite tobacco sheet 100.
[0122] In this embodiment, by pouring 0.001g to 0.8g of slurry onto the second surface and then baking the slurry at a temperature of 60℃ to 105℃ for 1 to 10 minutes, the final composite tobacco sheet 100 can have a suitable thickness, for example, between 0.2mm and 2mm.
[0123] In some embodiments, after pouring 0.001g to 0.8g of slurry onto the second surface, the slurry can be naturally air-dried to bond the second aerosol generation matrix layer 130 to the second surface 122 of the substrate layer 120.
[0124] In some embodiments, prior to the step of casting the slurry onto the other side surface of the substrate layer using a casting process to form a semi-finished product with aerosol matrix layers on both sides, the preparation method further includes:
[0125] The semi-finished product with an aerosol matrix layer on one side is punched to form a prefabricated composite tobacco sheet;
[0126] In the step of casting slurry onto the other side of the substrate layer to form a semi-finished product with aerosol matrix layers on both sides using a casting process, the prefabricated composite tobacco sheet is cast using a casting process to form a semi-finished product with aerosol matrix layers on both sides of the substrate layer.
[0127] In some embodiments, step S30 specifically includes:
[0128] S31a, providing a mold, the mold including a receiving groove;
[0129] S32a, the semi-finished product with an aerosol matrix layer on one side is placed in the receiving tank, and the other side surface of the matrix layer faces the opening of the receiving tank;
[0130] S33a, pour slurry into the receiving tank to form an aerosol matrix layer on the other side of the substrate layer.
[0131] Specifically, such as Figure 8 As shown, a mold 140 is provided in advance, which includes several receiving grooves 141. After a semi-finished product with an aerosol generation matrix layer on one side is obtained by the above-mentioned processes such as casting, rolling or spraying, the semi-finished product is placed in the receiving groove 141, with the other side surface of the semi-finished product facing the opening of the receiving groove 141. Then, slurry is poured into the receiving groove 141 by the casting equipment 150, thereby forming an aerosol generation matrix layer on the other side of the substrate layer 120.
[0132] After casting, the mold 140 can be transferred to a drying oven for drying. Once drying is complete, the resulting composite tobacco sheet can be removed.
[0133] In some embodiments, the mold 140 can be a packaging box for composite tobacco sheets, with several receiving slots 141 provided in the packaging box. After casting, the packaging box is transferred together to a drying oven for drying, which can save steps.
[0134] In some embodiments, prior to step S30, the above-described preparation method further includes:
[0135] The semi-finished product with an aerosol matrix layer on one side is punched to form a prefabricated composite tobacco sheet;
[0136] Meanwhile, step S30 specifically includes:
[0137] The prefabricated composite smoke sheet is cast using a casting process to form a semi-finished product with aerosol matrix layers on both sides of the matrix layer.
[0138] During the preparation process, a substrate layer 120 with a large surface area can be provided first. Multiple substrate units are provided on the substrate layer 120. After the aerosol generating matrix is bonded to one side surface of the substrate layer 120 through the above-mentioned processes such as casting, rolling or spraying, the semi-finished product with an aerosol generating matrix layer on one side is punched.
[0139] Specifically, each base unit can be cut off from the semi-finished product using a punching device, and the cut-off tobacco sheet is the pre-made composite tobacco sheet. Thus, in step S40, each pre-made composite tobacco sheet can be placed in the receiving groove 141 of the mold 140, and slurry can be poured onto the other side of each pre-made composite tobacco sheet using a casting device, thereby forming an aerosol generation matrix layer on both sides of the pre-made composite tobacco sheet.
[0140] One embodiment of this application also provides an aerosol generation system, such as Figure 9As shown, the aerosol generation system includes an aerosol generation product 2000 and an aerosol generation device 3000. The aerosol generation product 2000 includes a composite smoke sheet 100. The aerosol generation device 3000 is used to house the aerosol generation product 2000. When the aerosol generation product 2000 is housed in the aerosol generation device 3000, the aerosol generation device 3000 and the aerosol generation product 2000 cooperate to generate heat in the substrate layer 12.
[0141] For example, a magnetic field generator can be installed in the aerosol generating device 3000. The magnetic field generator can be an induction coil, and the substrate layer 120 is made of a conductive material. Suitable conductive materials can be any of iron, aluminum, nickel, nickel-iron alloy, or stainless steel. When the aerosol generated product 2000 is housed in the aerosol generating device 3000, the controller of the aerosol generating device 3000 controls the supply of alternating current to the induction coil, thereby causing the induction coil to generate an alternating magnetic field. The alternating magnetic field penetrates the substrate layer 120, inducing eddy currents on the substrate layer 120, and then the substrate layer 120 generates heat under the action of the eddy currents.
[0142] In some embodiments, such as Figure 9 As shown, the aerosol generating product 2000 includes a carrier 1000, which has multiple receiving slots 1400. Each receiving slot 1400 contains one composite smoke sheet 100. The composite smoke sheet 100 is held in the receiving slot 1400 by fitting tightly with it, thereby holding it on the carrier 1000. For example, if the aerosol generating product 2000 includes five composite smoke sheets 100, then the carrier 1000 has five corresponding receiving slots 1400, each holding one composite smoke sheet 100. Thus, through the support of the carrier 1000, the aerosol generating product 2000 can carry multiple composite smoke sheets 100 and place them into the aerosol generating device 3000 at one time.
[0143] In some embodiments, such as Figure 10 As shown, the carrier 1000 can also be constructed as a box-shaped body, which is hollow. The aforementioned receiving groove 1400 can be provided on the inner surface of the box-shaped body, thereby holding the composite tobacco sheet 100 inside the box-shaped body. After the composite tobacco sheet is prepared by the above-described preparation method, multiple composite tobacco sheets are then placed into the box-shaped body to form the shape shown in the aerosol generating article 2000a provided in this embodiment.
[0144] The hollow region 1100 of the box-shaped body is used to receive the aerosol generated by the volatilization of the aerosol matrix layer after being heated, and the box-shaped body also has an air inlet 1200 for air to enter the hollow region 1100, and an air outlet 1300 disposed opposite to the air inlet for aerosol to escape from the box-shaped body.
[0145] Please continue reading. Figure 9 The aerosol generating device 3000 includes a housing 3100, and a battery cell 3200 and a main board 3300 disposed within the housing 3100. The battery cell 3200 and the main board 3300 are electrically connected, and the main board 3300 is equipped with a controller for the aerosol generating device 300. The housing 3100 also includes a receiving section defining a receiving chamber 3400 for receiving the aerosol generating article 2000. Specifically, the aerosol generating article 2000 can be... Figure 9 The object is housed in the containment chamber 3400 in the direction of the middle arrow X, or along... Figure 9 The middle arrow Y direction is contained within the containment chamber 3400.
[0146] In some embodiments, the receiving chamber 3400 may be provided with a plurality of induction coils 3410. When the aerosol generating article 2000 is received in the receiving chamber 3400, the plurality of induction coils 3410 correspond to each composite smoke sheet 100 respectively. The controller controls the supply of alternating current to each induction coil 3410, so that each induction coil 3410 can induce an alternating magnetic field. The induced alternating magnetic field penetrates each substrate layer 120, thereby generating eddy currents in the substrate layer 120, and then generating heat under the action of the eddy currents.
[0147] It is easy to understand that the aerosol generating device can also use other methods well known to those skilled in the art to generate heat in the substrate layer 120, and is not limited to the electromagnetic method in the above embodiments.
[0148] In some embodiments, the controller may be configured to simultaneously provide alternating current to multiple induction coils 3410, thereby causing multiple composite tobacco sheets 100 to volatilize simultaneously and generate aerosols.
[0149] Alternatively, in some embodiments, the controller may be configured to provide alternating current to the induction coil 3410 in a certain order, so that multiple composite tobacco sheets 100 evaporate in a certain order to generate aerosols. After the last composite tobacco sheet 100 evaporates to generate aerosols, the aerosol generating product 2000 can be removed from the aerosol generating device 3000 and a new aerosol generating product 2000 can be placed in the aerosol generating device 3000.
[0150] like Figure 9 As shown, the aerosol generating device 3000 is also provided with a suction nozzle 3500, which has a defined outlet 3510 for the aerosol to escape from the aerosol generating device 300, so that the user can inhale the aerosol when sucking on the suction nozzle 3500.
[0151] In some embodiments, the nozzle 3500 is in communication with the receiving chamber 3400, when the aerosol generating article 2000 is manufactured according to... Figure 9 When the composite tobacco sheet 100 in the aerosol generating device 3000 is placed in the aerosol generating product 2000, the aerosol generated by the heating and volatilization of the composite tobacco sheet 100 is directly released into the receiving chamber 3400 so that the aerosol can further flow to the mouthpiece 3500.
[0152] Alternatively, in some embodiments, when the aerosol-generating article is in accordance with Figure 10 When the aerosol generating product 2000a shown is housed in the aerosol generating device 3000, the aerosol generated by the heating and volatilization of the composite tobacco sheet 100 is released into the hollow region 1100 of the box-shaped body, and then escapes from the aerosol generating product 2000 through the gas outlet 1300 of the box-shaped body and further enters the mouthpiece 3500 for the user to inhale.
[0153] It should be noted that the preferred embodiments of this application are given in the specification and accompanying drawings, but are not limited to the embodiments described in this specification. Furthermore, those skilled in the art can make improvements or modifications based on the above description, and all such improvements and modifications should fall within the protection scope of the appended claims.
Claims
1. A method for preparing a composite tobacco sheet, the composite tobacco sheet comprising a matrix layer capable of generating heat, and a first aerosol-generating matrix layer and a second aerosol-generating matrix layer bonded to both sides of the matrix layer and capable of being heated by the matrix layer to generate aerosols, characterized in that, The method for preparing the composite tobacco sheet includes: Provide a matrix layer; The slurry used to form the aerosol generation matrix is bonded to one side surface of the matrix layer to form a semi-finished product with an aerosol matrix layer on one side. Using a casting process, the slurry is poured onto the other side surface of the substrate layer to form a semi-finished product with aerosol matrix layers on both sides; The semi-finished product with aerosol matrix layers on both sides is dried to form composite tobacco sheets.
2. The preparation method according to claim 1, characterized in that, The thickness of the composite tobacco sheet is 0.2 mm to 2 mm.
3. The preparation method according to claim 1, characterized in that, The moisture content of the composite tobacco sheet is 4% to 8%.
4. The preparation method according to claim 1, characterized in that, The slurry comprises at least one of microcrystalline cellulose, silica, kaolin, calcium carbonate, and ceramic beads, and at least one of glycerol, glycerol, propylene glycol, diethylene glycol, triethylene glycol, and tetraethylene glycol.
5. The preparation method according to claim 1, characterized in that, In the step of casting slurry onto the other side surface of the substrate layer using a casting process to form a semi-finished product with aerosol matrix layers on both sides, the preparation method specifically includes: Pour 0.001g to 0.8g of slurry onto the other side surface of the substrate layer; The slurry is baked at 60℃ to 105℃ for 1 to 10 minutes, or the slurry is air-dried naturally.
6. The preparation method according to claim 1, characterized in that, The step of bonding the slurry to one side surface of the matrix layer to form a semi-finished product having an aerosol matrix layer on one side specifically includes: The slurry is bonded to one side surface of the substrate layer by any of the following processes: casting, rolling, or spraying.
7. The preparation method according to claim 6, characterized in that, When the slurry is bonded to one side surface of the substrate layer using a casting process... The slurry is bonded to one side surface of the substrate layer using a casting machine, the casting process comprising: The substrate layer is placed on the conveyor belt of the casting machine; The slurry used to form the aerosol matrix layer is placed into the feed trough of the casting machine so that the slurry is coated on one side surface of the matrix layer.
8. The preparation method according to claim 7, characterized in that, The casting machine includes heating zones located on both sides of the conveyor belt, through which a semi-finished product with an aerosol-generating matrix on one side passes for drying.
9. The preparation method according to claim 8, characterized in that, The heating area includes a first heating area and a second heating area disposed above the conveyor belt, and a third heating area disposed below the conveyor belt; and, along the conveying direction of the conveyor belt, the third heating area has a first end 271 and a second end 272 opposite to each other, the first heating area is located upstream of the second heating area, and both the first heating area and the second heating area are located between the first end 271 and the second end 272.
10. The preparation method according to claim 9, characterized in that, The heating temperature of the first heating zone 250 is 60℃~80℃, the heating temperature of the second heating zone 260 is 70℃~90℃, the heating temperature of the third heating zone 270 is 80℃~120℃, and the total time of the semi-finished product with an aerosol generating matrix on one side in the heating zone is 30mins~80mins.
11. The preparation method according to claim 7, characterized in that, The step of placing the substrate layer on the conveyor belt of the casting machine specifically includes: Liquid is sprayed onto the conveyor belt of the casting machine to cover the substrate layer within the liquid spraying area of the conveyor belt.
12. The preparation method according to claim 6, characterized in that, When the slurry is bonded to one side surface of the substrate layer using a casting process, the casting process includes: The substrate layer is bonded to the flat plate with water; The slurry for forming the aerosol generation matrix is placed in the feed trough of the coating machine, and the coating machine is driven to move between a first position and a second position on a heated plate to coat the slurry onto one side surface of the substrate layer.
13. The preparation method according to claim 12, characterized in that, The plate is a heated plate. After the steps of covering the substrate layer with slurry and coating one side surface of the substrate layer with slurry using a coating device, the casting process further includes: The slurry coated on one side of the substrate layer is dried using the heating plate at a temperature of 50°C to 90°C for a time of 35 mins to 90 mins.
14. The preparation method according to claim 1, characterized in that, Before the step of casting the slurry onto the other side surface of the substrate layer using a casting process to form a semi-finished product with aerosol matrix layers on both sides, the preparation method further includes: The semi-finished product with an aerosol matrix layer on one side is punched to form a prefabricated composite tobacco sheet; The step of casting slurry onto the other side surface of the substrate layer using a casting process to form a semi-finished product with aerosol matrix layers on both sides specifically includes: The prefabricated composite smoke sheet is cast using a casting process to form a semi-finished product with aerosol matrix layers on both sides of the matrix layer.
15. The preparation method according to claim 1, characterized in that, The substrate layer has multiple through holes.
16. The preparation method according to claim 15, characterized in that, The sum of the opening areas of the through holes occupies 30-50% of the surface area of the substrate layer.
17. The preparation method according to claim 1, characterized in that, The thickness of the substrate layer is 0.05 mm to 0.15 mm.
18. The preparation method according to claim 1, characterized in that, In the composite tobacco sheet, the sum of the thickness of the matrix layer and the aerosol-generating matrix layer on either side is 0.15mm-1.20mm.
19. The preparation method according to claim 1, characterized in that, The step of using a casting process to pour slurry onto the other side surface of the substrate layer to form a semi-finished product with aerosol matrix layers on both sides specifically includes: A mold is provided, the mold including a receiving groove; The semi-finished product with an aerosol matrix layer on one side is placed in the receiving tank, with the other side surface of the matrix layer facing the opening of the receiving tank; Slurry is poured into the receiving tank to form an aerosol matrix layer on the other side of the substrate layer.
20. An aerosol-generating product, characterized in that, include: Multiple composite tobacco sheets, wherein the composite tobacco sheets are prepared by the preparation method according to any one of claims 1-19; A carrier is used to support the composite tobacco sheets, and a plurality of the composite tobacco sheets are held on the carrier.
21. The aerosol-generating article according to claim 20, characterized in that, The carrier is constructed as a hollow box-shaped body, the hollow area of which is used to receive the aerosol. The box-shaped body has an air inlet for air to enter the hollow area and an air outlet for the aerosol to escape from the box-shaped body.
22. An aerosol generation system, characterized in that, include: The aerosol-generating article according to claim 20 or 21; An aerosol generating apparatus is provided with a receiving chamber for containing the aerosol generating article. When the aerosol generating article is contained in the receiving chamber, the aerosol generating apparatus and the aerosol generating article cooperate to generate heat in the substrate layer. The aerosol generating device further includes a suction nozzle, which defines an outlet for aerosols to escape from the aerosol generating device.