A soft and chewy texture eye shadow and a method of making the same
By combining magnesium myristate, magnesium palmitate, and zinc stearate as lubricants with oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer, the problems of mold sticking and structural stability in eyeshadow products during the pressing process were solved, achieving a soft and smooth texture while improving heat resistance, deformation resistance, and drop resistance.
Patent Information
- Application Number
- CN202611598958.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-15
- Publication Date
- 2026-11-24
AI Technical Summary
Existing eyeshadow products, in pursuing a soft and smooth texture, struggle to maintain structural stability, resulting in issues such as sticking to the mold, difficulty in demolding, poor heat resistance and deformation, and reduced drop resistance.
A synergistic lubricant of magnesium myristate, magnesium palmitate, and zinc stearate is used, combined with a compound of oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer. Through pre-coating and gradient pressing technology, a powder network that is "soft but not collapsible and can rebound under pressure" is formed, which improves the structural strength and flexibility of the powder.
While maintaining a soft and chewy texture, it effectively solves the problem of sticking to the mold during the pressing process and improves the resistance to heat deformation, edge collapse, and drop.
Smart Images

Figure SMS_1 
Figure SMS_2
Abstract
Description
Technical Field
[0001] This application relates to the field of cosmetic technology, and in particular to a soft, creamy eyeshadow and its preparation method. Background Technology
[0002] With the development of the cosmetics industry, eyeshadow products are now required not only to have rich colors and even application, but also to have a soft and delicate texture and a pleasant feel. The term "soft and smooth texture" typically refers to eyeshadow powder that feels soft to the touch, is easy to pick up, easy to blend, and does not easily break after pressing. However, existing eyeshadow compacts often struggle to maintain structural stability while pursuing a soft and smooth feel: adding oils or softening ingredients can improve the feel, but it can also lead to difficulties in sticking to and unmolding the powder during pressing, easy collapse of the finished product's edges, uncontrollable deformation during storage or use, and a significant decrease in its drop resistance.
[0003] In existing technologies, the pressing and molding properties of eyeshadow are typically improved by adjusting the powder composition and adding lubricants or thickeners. However, these methods often struggle to strike a balance between a soft, smooth feel and structural stability. When oils or softening ingredients are added to achieve a soft, smooth texture, the free oil phase in the powder increases. During pressing, this oil phase easily migrates to the mold surface, leading to sticking and difficulty in demolding. The mechanical stress during demolding can also cause the edges of the powder to collapse. Simultaneously, a high oil content results in insufficient internal bonding of the powder, leading to poor heat resistance, deformation resistance, and reduced drop resistance. Conversely, reducing oils and increasing powder hardness to enhance structural strength results in a dry, inelastic feel, excessive powder fallout, and a significantly diminished user experience.
[0004] Therefore, how to effectively solve the problem of mold sticking during the pressing process while maintaining the soft and smooth texture of eyeshadow, and improve its heat resistance, anti-collapse and anti-drop properties, remains a technical problem that needs to be solved in this field. Summary of the Invention
[0005] This invention provides a soft and smooth eyeshadow and its preparation method, which can effectively solve the problem of sticking to the mold during the pressing process and improve the heat resistance, anti-collapse and anti-drop properties.
[0006] In a first aspect of this application, this application provides a soft and creamy eyeshadow, comprising the following raw materials in parts by weight: 34-45 parts by weight of filler, 2.8-4.2 parts by weight of lubricant, 24-34 parts by weight of emollient, 2-6 parts by weight of thickener, 20-25 parts by weight of colorant, and 0.3-0.7 parts by weight of preservative. The lubricant comprises 0.5 to 1.0 parts by weight of magnesium myristate, 1.0 to 1.5 parts by weight of magnesium palmitate, and 1.3 to 1.7 parts by weight of zinc stearate; The thickener comprises 1.0 to 3.0 parts by weight of oxidized polyethylene wax and 1.0 to 3.0 parts by weight of polydimethylsiloxane crosslinked polymer.
[0007] By adopting the above technical solution, this application provides a soft and smooth eyeshadow that effectively solves the problem of sticking to the mold during the pressing process while maintaining a soft and smooth texture, and improves heat resistance, edge collapse resistance, and drop resistance. This may be because, on the one hand, magnesium myristate, magnesium palmitate, and zinc stearate work synergistically through differences in carbon chain length and interfacial interactions: magnesium myristate tends to plasticize the powder interior, making the powder soft and easy to pick up; magnesium palmitate acts as a transitional lubricant; zinc stearate preferentially participates in boron nitride pre-coating, forming a low surface energy lubricating layer on the powder surface and mold interface, and reducing the migration of free oil phase to the mold, thereby reducing sticking to the mold and improving demolding. On the other hand, oxidized polyethylene wax is compounded with polydimethylsiloxane crosslinked polymer: oxidized polyethylene wax provides a heat-resistant skeleton and structural strength, while the crosslinked polymer provides elastic recovery and a soft feel. The two work together to form a powder network that is "soft but not collapsing and can rebound under pressure," which allows for uniform pressure transmission and reduces internal stress, thereby improving heat resistance, edge collapse resistance, and drop resistance.
[0008] Optionally, the weight ratio of magnesium myristate, magnesium palmitate and zinc stearate in the lubricant is (0.6~1.0):(1.0~1.4):1.5.
[0009] By adopting the above technical solution and adjusting the amounts of magnesium myristate, magnesium palmitate, and zinc stearate according to the above weight ratio, the lubrication functions of the three can be complementary. Magnesium myristate provides internal plasticizing, magnesium palmitate provides transitional synergy, and zinc stearate provides surface anti-sticking, thereby maintaining a soft and glutinous texture while avoiding excessive softness that sticks to the mold or excessive hardness that results in insufficient elasticity.
[0010] Optionally, in the thickener, the weight ratio of oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer is (1.5~2.5):(1.5~2.5).
[0011] By adopting the above technical solution and adjusting the amount of oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer according to the above weight ratio, the two can be balanced and synergistically formed into a powder network that is "soft but not collapsing and can rebound under pressure": oxidized polyethylene wax provides a heat-resistant skeleton and structural strength, while crosslinked polymer provides elastic recovery and a soft feel; too high or too low a ratio will result in powder that is too hard, lacks elasticity, or is too soft and sticks to the mold or collapses at the edges. This range can maintain a soft and smooth texture while taking into account anti-sticking to the mold, heat resistance to deformation, anti-collapse at the edges, and anti-drop performance.
[0012] Optionally, the filler includes 10-12 parts by weight of porous spherical silica, 12-16 parts by weight of synthetic fluorophlogopite, 6-8 parts by weight of boron nitride, 5-7 parts by weight of spherical nylon-12 powder, and 1.0-2.0 parts by weight of polymethylsilsesquioxane.
[0013] Optionally, the emollient includes 12-14 parts by weight of isononyl isononanoate, 7-9 parts by weight of phenyl polytrimethylsiloxane, 2-6 parts by weight of hydrogenated polyisobutylene, and 3-5 parts by weight of polydimethylsiloxane.
[0014] In a second aspect, this application provides a method for preparing the soft, creamy eyeshadow described in the first aspect, comprising the following steps: S1. Heat hydrogenated polyisobutylene until completely melted, add oxidized polyethylene wax, stir and mix well, then add isononyl isononate, phenyl polytrimethylsiloxane, and polydimethylsiloxane, mix evenly, then add polydimethylsiloxane crosslinking polymer, disperse, cool down, and obtain a mixed oil phase. S2. Mix boron nitride and zinc stearate to obtain a mixed powder; take 5-20% of the total amount of the mixed oil phase prepared in step S1, add it to the mixed powder, mix, let stand, and sieve to obtain a pre-coated rigid powder. S3. Add porous spherical silica to the remaining mixed oil phase in step S1 in 2 to 4 portions, mix, add synthetic fluorophlogopite and spherical nylon-12 powder, mix, add the pre-coated rigid powder prepared in step S2, mix, add magnesium myristate, magnesium palmitate and polymethylsilsesquioxane, mix, add colorant, mix until the color is uniform, cool down, add preservative, let stand, sieve, and obtain the finished powder. S4. Pre-cool the mold to 10~20℃, preheat the finished powder obtained in step S3 to 50~70℃, then put it into the pre-cooled mold, press, demold, and age to obtain the finished eyeshadow.
[0015] By adopting the above technical solution, in step S2 of this application, boron nitride and zinc stearate are first dry-mixed, and then pre-coated with a portion of the mixed oil phase, so that zinc stearate and a portion of the oil phase are preferentially enriched on the surface of boron nitride, resulting in pre-coated rigid powder. This pretreatment improves the interfacial compatibility between boron nitride and the oil phase and subsequent powder, avoiding direct exposure of the rigid powder, which would lead to a hard and brittle powder. On the other hand, it allows zinc stearate to preferentially contact the mold interface during pressing, forming a low surface energy lubricating layer and reducing the migration of free oil phase to the mold surface, thereby reducing mold sticking and improving demolding.
[0016] Optionally, the spherical nylon-12 powder has an average particle size of 5 μm.
[0017] Optionally, the colorant comprises 15-18 parts by weight of CI 77891 / triethoxyoctylsilane / aluminum hydroxide and 5-7 parts by weight of CI 77492 / CI 77499 / CI 77491 / triethoxyoctylsilane.
[0018] Optionally, the preservative is phenoxyethanol.
[0019] Optionally, in step S1, the heating temperature of the hydrogenated polyisobutylene is 95~105℃.
[0020] Optionally, in step S2, 8-12% of the total amount of the mixed oil phase prepared in step S1 is added to the mixed powder for coating.
[0021] Optionally, in step S4, the pressing procedure is: pre-compression of 30~50 kgf / cm³. 2 Hold for 1-3 seconds, then increase to 60-100 kgf / cm² 2 Maintain for 8-12 seconds, then reduce to 20-40 kgf / cm² within 6-10 seconds. 2 Hold the pressure for 4-6 seconds, then release the pressure completely.
[0022] Optionally, in step S4, the aging temperature is 23~25℃, the relative humidity is 45~55%, and the aging time is 24~48h.
[0023] In summary, this application includes at least one of the following beneficial technical effects: 1. This application provides a soft, creamy eyeshadow that effectively solves the problem of sticking to the mold during the pressing process while maintaining a soft, creamy texture, and improves heat resistance, edge collapse resistance, and drop resistance. On one hand, magnesium myristate, magnesium palmitate, and zinc stearate work synergistically through differences in carbon chain length and interfacial interactions: magnesium myristate tends to plasticize the powder interior, making the powder soft and easy to pick up; magnesium palmitate acts as a transitional lubricant; zinc stearate preferentially participates in boron nitride pre-coating, forming a low surface energy lubricating layer on the powder surface and at the mold interface, and reducing the migration of free oil phases to the mold, thereby reducing sticking and improving demolding. On the other hand, oxidized polyethylene wax is compounded with a polydimethylsiloxane crosslinked polymer: oxidized polyethylene wax provides a heat-resistant skeleton and structural strength, while the crosslinked polymer provides elastic recovery and a supple feel. Together, they form a powder network that is "soft but not collapsing, and can rebound under pressure," allowing for uniform pressure transmission and reducing internal stress, thereby improving heat resistance, edge collapse resistance, and drop resistance.
[0024] 2. This application provides a method for preparing a soft and smooth eyeshadow. Through stepwise mixing, pre-coating and gradient pressing aging, the oil phase, powder and lubricant are evenly dispersed, the powder density is uniform and the internal stress is reduced, thereby improving the drop resistance. Detailed Implementation
[0025] The embodiments of the present invention will be described in detail below with reference to the examples. However, those skilled in the art will understand that the following examples are only for illustrating the present invention and should not be regarded as limiting the scope of the present invention. Specific conditions not specified in the examples shall be carried out according to conventional conditions or conditions recommended by the manufacturer. Reagents or instruments whose manufacturers are not specified are all conventional products that can be purchased commercially.
[0026] Porous spherical silica was purchased from Xuancheng Jingrui New Materials Co., Ltd. (VK-SQ80), and polymethylsilsesquioxane was purchased from Momentive (Shanghai) Trading Co., Ltd. TM 145A), phenyl polytrimethylsiloxane was purchased from Hunan Jiahang Pharmaceutical Technology Co., Ltd. (CF702014), polydimethylsiloxane crosslinking polymer was purchased from Shanghai Dingfen Chemical Technology Co., Ltd. (P36198), polydimethylsiloxane was purchased from Dow Chemical, CI 77891 / triethoxyoctylsilane / aluminum hydroxide was purchased from Shanghai Kefeng Biotechnology Co., Ltd. (605055), CI 77492 / CI 77499 / CI 77491 / triethoxyoctylsilane was purchased from Shanghai Kefeng Biotechnology Co., Ltd. (609389).
[0027] Example 1 Example 1 provides a soft, creamy eyeshadow, comprising the following raw materials in parts by weight, as shown in Table 1: Table 1
[0028] Preparation method S1. Preparation of oil phase: 4.0 parts by weight of hydrogenated polyisobutylene were heated to 100°C until completely melted. 2.0 parts by weight of oxidized polyethylene wax were added and stirred at 300 rpm until homogeneous. Then, 13.0 parts by weight of isononyl isononanoate, 8.5 parts by weight of phenyl polytrimethylsiloxane, and 4.0 parts by weight of polydimethylsiloxane were added and mixed evenly. Then, 2.0 parts by weight of polydimethylsiloxane crosslinking polymer were added and dispersed at 1500 rpm for 10 min under high shear. The mixture was then cooled to 70°C to obtain the mixed oil phase. S2. Rigid powder pretreatment: 7.0 parts by weight of boron nitride and 1.5 parts by weight of zinc stearate are placed in a planetary mixer and dry-mixed at 200 rpm for 3 min to obtain a mixed powder; 3.5 parts by weight of the mixed oil phase prepared in step S1 are added to the mixed powder and mixed at 200 rpm for 8 min at 55℃. After standing for 30 min, the mixture is passed through a 100-mesh sieve to obtain a pre-coated rigid powder. S3. Powder Mixing: Place the remaining mixed oil phase from step S1 in a planetary mixer, maintaining the temperature at 50°C. Add 11.0 parts by weight of porous spherical silica in three portions, mixing for 3 minutes after each addition. Add 14.0 parts by weight of synthetic fluorophlogopite and 6.0 parts by weight of spherical nylon-12 powder, mixing at 500 rpm for 5 minutes. Add the pre-coated rigid powder prepared in step S2, mixing at 300 rpm for 5 minutes. Add 0.8 parts by weight of magnesium myristate, 1.2 parts by weight of magnesium palmitate, and 2.0 parts by weight of polymethyl silsesquioxane, mixing for 3 minutes. Add 16.5 parts by weight of CI 77891 / triethoxyoctylsilane / aluminum hydroxide and 6.0 parts by weight of CI 77492 / CI 77499 / CI 77491 / triethoxyoctylsilane was mixed at 300 rpm for 8 min until the color was uniform. After the temperature dropped to below 40℃, 0.5 parts by weight of phenoxyethanol were added and mixed at 300 rpm for 3 min. After standing for 6 h, the mixture was passed through an 80-mesh sieve to obtain the finished powder. S4. Pressing: Pre-cool the metal mold to 15℃, and blow dry air onto the mold surface to obtain a pre-cooled mold. Place the finished powder obtained in step S3 in an oven and preheat it at 60℃ for 10 minutes. Then, load it into the pre-cooled mold and press it. The pressing procedure is: pre-press 40 kgf / cm². 2 Hold for 2 seconds at 15 kgf / cm 2 / s rises to 80kgf / cm 2 Hold for 10 seconds, then slowly reduce to 30 kgf / cm² within 8 seconds. 2 Hold the pressure for 5 seconds, then release the pressure completely. After demolding, let it stand and age for 36 hours in an environment with a temperature of 24℃ and a relative humidity of 50% to obtain the finished eyeshadow.
[0029] Example 2
[0030] Example 2 provides a soft and smooth eyeshadow. The difference from Example 1 is that in step S3, the total weight of magnesium myristate and magnesium palmitate remains unchanged, and the weight ratio of magnesium myristate to magnesium palmitate is 1:1.
[0031] Specifically, step S3 is different, and is as follows: S3, Powder Mixing: Place the remaining mixed oil phase from step S1 in a planetary mixer, maintain the temperature at 50°C, add 11.0 parts by weight of porous spherical silica in 3 portions, mixing for 3 minutes after each addition, add 14.0 parts by weight of synthetic fluorophlogopite and 6.0 parts by weight of spherical nylon-12 powder, mix at 500 rpm for 5 minutes, add the pre-coated rigid powder prepared in step S2, mix at 300 rpm for 5 minutes, add 1.0 parts by weight of magnesium myristate, 1.0 parts by weight of magnesium palmitate, and 2.0 parts by weight of polymethyl silsesquioxane, mix for 3 minutes, add 16.5 parts by weight of CI77891 / triethoxyoctylsilane / aluminum hydroxide and 6.0 parts by weight of CI 77492 / CI 77499 / CI 77491 / triethoxyoctylsilane was mixed at 300 rpm for 8 min until the color was uniform. After the temperature dropped below 40℃, 0.5 parts by weight of phenoxyethanol were added and mixed at 300 rpm for 3 min. After standing for 6 h, the mixture was passed through an 80-mesh sieve to obtain the finished powder.
[0032] The other preparation steps are the same as in Example 1.
[0033] Example 3
[0034] Example 3 provides a soft and smooth eyeshadow. The difference from Example 1 is that in step S3, the total weight of magnesium myristate and magnesium palmitate remains unchanged, and the weight ratio of magnesium myristate to magnesium palmitate is 0.6:1.4.
[0035] Specifically, step S3 is different, and is as follows: S3, Powder Mixing: Place the remaining mixed oil phase from step S1 in a planetary mixer, maintain the temperature at 50°C, add 11.0 parts by weight of porous spherical silica in 3 portions, mixing for 3 minutes after each addition, add 14.0 parts by weight of synthetic fluorophlogopite and 6.0 parts by weight of spherical nylon-12 powder, mix at 500 rpm for 5 minutes, add the pre-coated rigid powder prepared in step S2, mix at 300 rpm for 5 minutes, add 0.6 parts by weight of magnesium myristate, 1.4 parts by weight of magnesium palmitate, and 2.0 parts by weight of polymethyl silsesquioxane, mix for 3 minutes, add 16.5 parts by weight of CI77891 / triethoxyoctylsilane / aluminum hydroxide and 6.0 parts by weight of CI 77492 / CI 77499 / CI 77491 / triethoxyoctylsilane was mixed at 300 rpm for 8 min until the color was uniform. After the temperature dropped below 40℃, 0.5 parts by weight of phenoxyethanol were added and mixed at 300 rpm for 3 min. After standing for 6 h, the mixture was passed through an 80-mesh sieve to obtain the finished powder.
[0036] The other preparation steps are the same as in Example 1.
[0037] Example 4
[0038] Example 4 provides a soft and smooth eyeshadow. The difference from Example 1 is that in step S1, the total weight of oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer remains unchanged, and the weight ratio of oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer is 1.5:2.5.
[0039] Specifically, step S1 is different, specifically: S1, oil phase preparation: 4.0 parts by weight of hydrogenated polyisobutylene are heated to 100°C until completely melted, 1.5 parts by weight of oxidized polyethylene wax are added, and the mixture is stirred at 300 rpm. Then, 13.0 parts by weight of isononyl isononanoate, 8.5 parts by weight of phenyl polytrimethylsiloxane, and 4.0 parts by weight of polydimethylsiloxane are added and mixed evenly. Then, 2.5 parts by weight of polydimethylsiloxane crosslinking polymer are added and dispersed at 1500 rpm for 10 min under high shear. The mixture is then cooled to 70°C to obtain a mixed oil phase.
[0040] The other preparation steps are the same as in Example 1.
[0041] Example 5
[0042] Example 5 provides a soft and smooth eyeshadow, which differs from Example 1 in that, in step S1, the total weight of oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer remains unchanged, and the weight ratio of oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer is 2.5:1.5.
[0043] Specifically, step S1 is different, specifically: S1, oil phase preparation: 4.0 parts by weight of hydrogenated polyisobutylene are heated to 100°C until completely melted, 2.5 parts by weight of oxidized polyethylene wax are added, and the mixture is stirred at 300 rpm. Then, 13.0 parts by weight of isononyl isononanoate, 8.5 parts by weight of phenyl polytrimethylsiloxane, and 4.0 parts by weight of polydimethylsiloxane are added and mixed evenly. Then, 1.5 parts by weight of polydimethylsiloxane crosslinking polymer are added and dispersed at 1500 rpm for 10 min under high shear. The mixture is then cooled to 70°C to obtain a mixed oil phase.
[0044] The other preparation steps are the same as in Example 1.
[0045] Comparative Example 1 Comparative Example 1 provides a soft and creamy eyeshadow, which differs from Example 1 in that, in step S3, magnesium myristate is replaced by magnesium palmitate in equal parts by weight.
[0046] The preparation method is the same as in Example 1.
[0047] Comparative Example 2 Comparative Example 2 provides a soft and creamy eyeshadow, which differs from Example 1 in that, in step S3, magnesium palmitate is replaced by magnesium myristate in equal parts by weight.
[0048] The preparation method is the same as in Example 1.
[0049] Comparative Example 3 Comparative Example 3 provides a soft, creamy eyeshadow, which differs from Example 1 in that zinc stearate is not added in step S2.
[0050] Specifically, step S2 is different, specifically: S2, rigid powder pretreatment: take 3.5 parts by weight of the mixed oil phase prepared in step S1, add it to 7.0 parts by weight of boron nitride, mix at 200 rpm for 5 min at 55℃, let stand for 20 min, and then pass it through a 100-mesh sieve to obtain pre-coated rigid powder.
[0051] The other preparation steps are the same as in Example 1.
[0052] Comparative Example 4 Comparative Example 4 provides a soft and creamy eyeshadow, which differs from Example 1 in that, in step S1, an equal part by weight of oxidized polyethylene wax is replaced with a polydimethylsiloxane crosslinked polymer.
[0053] The preparation method is the same as in Example 1.
[0054] Comparative Example 5 Comparative Example 5 provides a soft and creamy eyeshadow, which differs from Example 1 in that, in step S1, an equal part by weight of polydimethylsiloxane crosslinked polymer is replaced with oxidized polyethylene wax.
[0055] The preparation method is the same as in Example 1.
[0056] Comparative Example 6 Comparative Example 6 provides a soft and smooth eyeshadow, which differs from Example 1 in that, in step S1, an equal part by weight of oxidized polyethylene wax is replaced with microcrystalline wax.
[0057] The preparation method is the same as in Example 1.
[0058] Comparative Example 7 Comparative Example 7 provides a soft, creamy eyeshadow. The difference from Example 1 is that boron nitride and zinc stearate are not pretreated. The specific preparation steps are as follows: S1. Preparation of oil phase: 4.0 parts by weight of hydrogenated polyisobutylene were heated to 100°C until completely melted. 2.0 parts by weight of oxidized polyethylene wax were added and stirred at 300 rpm until homogeneous. Then, 13.0 parts by weight of isononyl isononanoate, 8.5 parts by weight of phenyl polytrimethylsiloxane, and 4.0 parts by weight of polydimethylsiloxane were added and mixed evenly. Then, 2.0 parts by weight of polydimethylsiloxane crosslinking polymer were added and dispersed at 1500 rpm for 10 min under high shear. The mixture was then cooled to 70°C to obtain the mixed oil phase. S2. Powder Mixing: Place the mixed oil phase obtained in step S1 in a planetary mixer and maintain the temperature at 55℃. Add 11.0 parts by weight of porous spherical silica in three portions, mixing for 3 minutes after each addition. Add 14.0 parts by weight of synthetic fluorophlogopite and 6.0 parts by weight of spherical nylon-12 powder, mixing at 500 rpm for 5 minutes. Add 7.0 parts by weight of boron nitride and 1.5 parts by weight of zinc stearate, mixing at 300 rpm for 5 minutes. Add 0.8 parts by weight of magnesium myristate, 1.2 parts by weight of magnesium palmitate, and 2.0 parts by weight of polymethyl silsesquioxane, mixing for 3 minutes. Add 16.5 parts by weight of CI 77891 / triethoxyoctylsilane / aluminum hydroxide and 6.0 parts by weight of CI 77492 / CI 77499 / CI 77491 / triethoxyoctylsilane was mixed at 300 rpm for 8 min until the color was uniform. After the temperature dropped to below 40℃, 0.5 parts by weight of phenoxyethanol were added and mixed at 300 rpm for 3 min. After standing for 6 h, the mixture was passed through an 80-mesh sieve to obtain the finished powder. S3. Pressing: Pre-cool the metal mold to 15℃, and blow dry air onto the mold surface to obtain a pre-cooled mold. Place the finished powder obtained in step S2 in an oven and preheat it at 60℃ for 10 minutes. Then, load it into the pre-cooled mold and press it. The pressing procedure is: pre-press 40 kgf / cm². 2 Hold for 2 seconds at 15 kgf / cm 2 / s rises to 80kgf / cm 2 Hold for 10 seconds, then slowly reduce to 30 kgf / cm² within 8 seconds. 2 Hold the pressure for 5 seconds, then release the pressure completely. After demolding, let it stand and age for 36 hours in an environment with a temperature of 24℃ and a relative humidity of 50% to obtain the finished eyeshadow.
[0059] Performance testing The eyeshadows prepared in Examples 1-5 and Comparative Examples 1-7 were subjected to heat deformation resistance, compression deformation, mold adhesion, and drop resistance tests.
[0060] Heat resistance deformation test: Open the eyeshadow sample box, place it in a constant temperature chamber at 50±1℃ for 24 hours, then remove it and allow it to return to room temperature; visually observe the edge and surface morphology of the powder compact under a D65 standard light source, and score it from 0 to 4 points (0 points: no deformation; 1 point: slight deformation; 2 points: local collapse ≤1 / 4; 3 points: obvious collapse or cracks; 4 points: overall deformation); a score ≤1 is considered qualified. Compression deformation and compression hardness tests: A texture analyzer (TA.XT Plus, Stable Micro Systems) was used. A 20mm diameter cylindrical flat-bottomed pressure plate was used to compress the eyeshadow powder to a deformation of 1mm at a speed of 0.3mm / s. The maximum force F2 during compression and the height L2 after unloading were recorded. The compression deformation L1 was 1mm. The compression deformation rate was calculated as L2 / L1×100%. F2 was used as the compression hardness index, with the unit being N. The smaller the F2, the softer the powder. Five points were measured for each sample, and the average value was taken. Adhesion Test: The degree of adhesion of eyeshadow powder to the mold during the molding process was evaluated using the mold residue method. Before the test, the metal mold was cleaned and dried with anhydrous ethanol, and placed in an environment of 23±1℃ and 50±5%RH for 30 min to equilibrate. The initial mass m0 of the mold was weighed, accurate to 0.1 mg. A fixed mass m was then weighed. p The finished powder is preheated, molded, and pressed according to the conditions in step S4; after pressing, it is demolded under the same environment, and the mass m1 of the mold (including residual powder) is immediately weighed; the amount of sticking Δm = m1 - m0, and the formula for calculating the sticking rate is as follows: Adhesion rate (%) = (m1 - m0) / m p ×100%; Each group of samples was pressed in parallel three times, and the average value was taken. The lower the sticking rate, the less the powder adheres to the mold surface, and the better the demolding performance. Drop Resistance Test: The eyeshadow compact was placed in its matching packaging tray, the lid was opened, and it was dropped freely from a height of 80cm onto a marble tile surface. One experimenter performed the drop test, while another scored the results. Scoring criteria (0-10 points, lower scores indicate better drop resistance): 0 points: No significant change; 1-2 points: Linear cracks; 3-4 points: Mesh cracks; 5-6 points: Broken area not exceeding 1 / 3 of the eyeshadow compact's volume; 7-8 points: Broken area exceeding 1 / 3 of the eyeshadow compact's volume, but the eyeshadow was not completely shattered; 9-10 points: The eyeshadow shattered completely. The test results are shown in Table 2.
[0061] Table 2
[0062] Results Analysis and Summary Based on Examples 1-3 and Table 2, it can be seen that the combined use of magnesium myristate and magnesium palmitate is beneficial in balancing the soft and smooth texture of the eyeshadow with its resistance to deformation, sticking, and drop. Changes in the ratio of the two will affect the powder properties, and the overall effect of Example 1 is better.
[0063] Based on Examples 1, 4-5, and Table 2, it can be seen that when oxidized polyethylene wax is compounded with polydimethylsiloxane crosslinked polymer, the ratio of the two can affect heat resistance deformation, compression deformation rate, compression hardness, sticking rate, and drop resistance. Too much crosslinked polymer or too much oxidized polyethylene wax will reduce the performance. The ratio in Example 1 has the best overall effect.
[0064] Based on Examples 1, Comparative Examples 1-3 and Table 2, it can be seen that the combination of magnesium myristate, magnesium palmitate and zinc stearate, as well as the participation of zinc stearate in pre-coating, has a synergistic effect on improving compression set, reducing mold sticking, improving heat resistance and drop resistance; replacing or omitting zinc stearate alone will result in poor performance.
[0065] Based on Examples 1, Comparative Examples 4-6 and Table 2, it can be seen that oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer cannot be substituted for each other, and microcrystalline wax cannot replace oxidized polyethylene wax. The absence or substitution of any component significantly reduces the eyeshadow's resistance to deformation, adhesion, and drop. Although Comparative Example 4 has a lower F2 and a softer feel, its adhesion rate and drop resistance are worse.
[0066] As can be seen from Example 1, Comparative Example 7 and Table 2, pre-coating boron nitride and zinc stearate can improve powder dispersibility and flexibility, thereby improving the eyeshadow's resistance to deformation, sticking, and drop; without pre-coating, the performance decreases.
[0067] The above are all preferred embodiments of this application and are not intended to limit the scope of protection of this application. Therefore, all equivalent changes made to the products, methods and principles of this application should be covered within the scope of protection of this application.
Claims
1. A soft, creamy eyeshadow, characterized in that, It includes the following raw materials in parts by weight: 34-45 parts by weight of filler, 2.8-4.2 parts by weight of lubricant, 24-34 parts by weight of emollient, 2-6 parts by weight of thickener, 20-25 parts by weight of colorant, and 0.3-0.7 parts by weight of preservative; The lubricant comprises 0.5 to 1.0 parts by weight of magnesium myristate, 1.0 to 1.5 parts by weight of magnesium palmitate, and 1.3 to 1.7 parts by weight of zinc stearate; The thickener comprises 1.0 to 3.0 parts by weight of oxidized polyethylene wax and 1.0 to 3.0 parts by weight of polydimethylsiloxane crosslinked polymer.
2. The soft, creamy eyeshadow according to claim 1, characterized in that, In the lubricant, the weight ratio of magnesium myristate, magnesium palmitate, and zinc stearate is (0.6~1.0):(1.0~1.4):1.
5.
3. The soft, creamy eyeshadow according to claim 1, characterized in that, In the thickener, the weight ratio of oxidized polyethylene wax and polydimethylsiloxane crosslinked polymer is (1.5~2.5):(1.5~2.5).
4. The soft, creamy eyeshadow according to claim 1, characterized in that, The filler comprises 10-12 parts by weight of porous spherical silica, 12-16 parts by weight of synthetic fluorophlogopite, 6-8 parts by weight of boron nitride, 5-7 parts by weight of spherical nylon-12 powder, and 1.0-2.0 parts by weight of polymethylsilsesquioxane.
5. The soft, creamy eyeshadow according to claim 4, characterized in that, The emollient comprises 12-14 parts by weight of isononyl isononanoate, 7-9 parts by weight of phenyl polytrimethylsiloxane, 2-6 parts by weight of hydrogenated polyisobutylene, and 3-5 parts by weight of polydimethylsiloxane.
6. A method for preparing the soft, creamy eyeshadow according to claim 5, characterized in that, Includes the following steps: S1. Heat hydrogenated polyisobutylene until completely melted, add oxidized polyethylene wax, stir and mix well, then add isononyl isononate, phenyl polytrimethylsiloxane, and polydimethylsiloxane, mix evenly, then add polydimethylsiloxane crosslinking polymer, disperse, cool down, and obtain a mixed oil phase. S2. Mix boron nitride and zinc stearate to obtain a mixed powder; take 5-20% of the total amount of the mixed oil phase prepared in step S1, add it to the mixed powder, mix, let stand, and sieve to obtain a pre-coated rigid powder. S3. Add porous spherical silica to the remaining mixed oil phase in step S1 in 2 to 4 portions, mix, add synthetic fluorophlogopite and spherical nylon-12 powder, mix, add the pre-coated rigid powder prepared in step S2, mix, add magnesium myristate, magnesium palmitate and polymethylsilsesquioxane, mix, add colorant, mix until the color is uniform, cool down, add preservative, let stand, sieve, and obtain the finished powder. S4. Pre-cool the mold to 10~20℃, preheat the finished powder obtained in step S3 to 50~70℃, then put it into the pre-cooled mold, press, demold, and age to obtain the finished eyeshadow.
7. The preparation method according to claim 6, characterized in that, In step S1, the heating temperature of hydrogenated polyisobutylene is 95~105℃.
8. The preparation method according to claim 6, characterized in that, In step S2, 8-12% of the total amount of the mixed oil phase prepared in step S1 is added to the mixed powder for coating.
9. The preparation method according to claim 6, characterized in that, In step S4, the pressing procedure is as follows: pre-compression of 30~50 kgf / cm³. 2 Hold for 1-3 seconds, then increase to 60-100 kgf / cm² 2 Maintain for 8-12 seconds, then reduce to 20-40 kgf / cm² within 6-10 seconds. 2 Hold the pressure for 4-6 seconds, then release the pressure completely.
10. The preparation method according to claim 6, characterized in that, In step S4, the aging temperature is 23~25℃, the relative humidity is 45~55%, and the aging time is 24~48h.