A method of preparing a multi-plant component facial mask composition

By forming a composite condensed phase of protein and anionic polysaccharides in the mask, combined with the film-forming method of carbonaceous and layered silicate adsorption components and cross-linked polymers, the problem of insufficient adsorption, cleaning and complete peeling stability of the mask in humid and hot environments is solved, and uniform adsorption and stable peeling of the film layer are achieved.

CN123148200APending Publication Date: 2026-11-24JIANZE (SHENZHEN) BIOTECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611625977.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-20
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing peel-off masks lack sufficient stability in adsorption, cleaning, and complete peeling under humid and polluted environments. After drying, the film layer is uneven in thickness, easily breaks, or leaves residue, resulting in poor user comfort.

Method used

A composite condensed phase is formed by combining protein components and carboxyl-containing anionic polysaccharide components under acidic conditions to coat plant active components. Carbonaceous and layered silicate adsorption components are added, and the composite adsorption powder is formed by vacuum freeze-drying. Combined with acrylic (ester) cross-linked polymers and polyvinyl alcohol film-forming liquid, a stable continuous film layer is formed.

Benefits of technology

It maintains the stability of plant-based active components in humid and polluted environments, improves the continuity and integrity of the membrane layer, uniformly adsorbs sebum and pollutants, improves user comfort, and solves the problems of uneven membrane thickness and breakage during peeling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123148200A_ABST
    Figure CN123148200A_ABST
Patent Text Reader

Abstract

This disclosure relates to the field of biopharmaceutical materials technology, providing a multi-plant component facial mask composition and its preparation method. The steps include: hydrating a protein component and a carboxyl-containing anionic polysaccharide component in an aqueous medium, adjusting the pH to acidic conditions to obtain a composite condensed phase; then adding plant active components to the composite condensed phase for coating to obtain a plant active composite carrier dispersion; adding a drying protection component and a functional auxiliary component to the plant active composite carrier dispersion, followed by vacuum freeze-drying to obtain a composite adsorbent powder; adding a thickening and stabilizing dispersion to a polyvinyl alcohol film-forming solution, continuing to add the composite adsorbent powder, and then degassing and maturing to obtain the multi-plant component facial mask composition. Through the protection of the plant active components by the composite condensed carrier and the synergistic adsorption of the carbonaceous component and the layered silicate component, the facial mask composition can simultaneously adsorb sebum and pollutants, maintain plant activity, and ensure complete film peeling even in humid and polluted environments.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of air filtration materials technology, and more specifically, to a method for preparing a multi-plant component facial mask composition. Background Technology

[0002] Existing peel-off masks typically form a continuous film layer after being applied to the skin, through water evaporation. The film layer adheres to the skin's surface, removing sebum, dust, and impurities from pores. To enhance cleansing power, charcoal powder, mineral powder, or other porous adsorbent materials are often added. These adsorbent materials increase the film layer's ability to adsorb oil and pollutants; however, their particle surfaces have strong water absorption and adsorption properties, which can easily alter the flow state of the slurry and the water migration state within the film layer when added to the film-forming system.

[0003] However, in environments with high temperature, high humidity, and high levels of air pollutants, the secretion of sebum and the adhesion of dust on the skin surface will increase simultaneously. After absorbing moisture from the environment, the adsorbed powder may become wetted, agglomerated, or locally deposited, resulting in inconsistent adsorption capacity and drying shrinkage in different areas of the film. After the film dries, uneven thickness and decreased continuity may occur, making it prone to breakage or residue during peeling. If the film is too sticky or excessively shrunken, it will increase the pulling sensation on the skin, making it difficult to stably remove the adsorbed sebum and pollutants as a whole. Consequently, the mask cannot maintain a stable adsorption, cleaning, and complete peeling state in humid and polluted environments.

[0004] It should be noted that the information disclosed in the background section above is only used to enhance the understanding of the background of this disclosure. Summary of the Invention

[0005] The purpose of this disclosure is to provide a method for preparing a multi-plant component facial mask composition, which solves the problem of insufficient adsorption, cleaning, and complete peeling stability of facial masks in humid and polluted environments.

[0006] Other features and advantages of this disclosure will become apparent from the following detailed description, or may be learned in part from practice of this disclosure.

[0007] According to one aspect of this disclosure, a method for preparing a multi-plant component facial mask composition is provided, comprising the steps of: S1. The protein component and the carboxyl-containing anionic polysaccharide component are added to an aqueous medium for hydration, and the pH is adjusted to acidic conditions to obtain a composite condensed phase. Then, the plant active component is added to the composite condensed phase for coating to obtain a plant active composite carrier dispersion. S2. Add drying protection components and functional auxiliary components to the plant active composite carrier dispersion, and obtain composite adsorption powder after vacuum freeze drying. The functional auxiliary components include carbonaceous adsorption components and layered silicate adsorption components. S3. The acrylic (ester) crosslinked polymer is added to an aqueous medium for dispersion and hydration. After neutralization, a thickened and stable dispersion is obtained. The thickened and stable dispersion is added to a polyvinyl alcohol film-forming solution. Composite adsorbent powder is then added. After stirring, homogenization, degassing, and aging, a multi-plant component facial mask composition is obtained.

[0008] Another aspect of this disclosure provides a multi-plant component facial mask composition, prepared by a method for preparing a multi-plant component facial mask composition.

[0009] As can be seen from the above technical solutions, the exemplary embodiments disclosed herein possess at least the following advantages and positive effects: In some embodiments of this disclosure, the technical solutions provided include, on the one hand, the use of protein components and carboxyl-containing anionic polysaccharide components for hydration in an aqueous medium, forming a composite condensed phase under acidic conditions, followed by the addition of plant active components for coating. Electrostatic association occurs between the protonable amino groups in the protein components and the carboxyl groups in the anionic polysaccharide components, accompanied by hydrogen bonding, thus dispersing and confining the plant active components within the composite condensed phase. Subsequently, the addition of a drying protective component and vacuum freeze-drying reduce moisture migration and thermal damage to the plant active components during the drying process, lowering their direct exposure to the adsorbent powder in subsequent contact. This solves the problems of existing technologies where plant active components are susceptible to humid and hot environments and lack sufficient activity retention during storage and film formation. It also helps the plant active components remain stable and gradually released during mask use, achieving the technical effect of extending the duration of plant-based soothing and antioxidant effects.

[0010] On the other hand, by adding carbonaceous adsorption components and layered silicate adsorption components to the plant-based active composite carrier dispersion, the pore structure of the carbonaceous components and the interlayer structure and surface adsorption sites of the layered silicate components can adsorb sebum, dust, and pore dirt. Simultaneously, the acrylic (ester) crosslinked polymer is dispersed, hydrated, and neutralized in an aqueous medium to form a dispersion with thickening and suspension stabilizing effects. This dispersion is then mixed with a polyvinyl alcohol film-forming solution, ensuring the composite adsorption powder is uniformly dispersed in the continuous film-forming phase. After the water evaporates, the polyvinyl alcohol forms a continuous film layer. The acrylic (ester) crosslinked polymer improves the distribution of powder in the film layer through swelling and network thickening. Stirring and homogenization reduce local agglomeration, while degassing and maturation help reduce internal defects in the film layer. This further overcomes the problems of easy agglomeration of adsorption powder, uneven film thickness, and easy breakage or residue during peeling under humid and hot conditions, achieving more uniform adsorption of sebum and pollutants, and improving the continuity, complete peelability, and user comfort of the film layer.

[0011] In summary, this technical solution utilizes the confined protection of plant active components by the composite coagulation carrier, the preservation of the carrier structure by vacuum freeze-drying, the synergistic adsorption of carbonaceous components and layered silicate components, and the synergistic effect between the continuous and stable film layer formed by polyvinyl alcohol and acrylic (ester) cross-linked polymers. This enables the resulting mask composition to simultaneously adsorb sebum and pollutants, maintain plant activity, and ensure complete film peeling in humid and polluted environments, thereby improving the problems of adsorbed powder agglomeration and tearing irritation.

[0012] It should be understood that the foregoing general description and the following detailed description are exemplary and explanatory only, and are not intended to limit this disclosure. Attached Figure Description

[0013] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this disclosure and, together with the description, serve to explain the principles of this disclosure. It is obvious that the drawings described below are merely some embodiments of this disclosure, and those skilled in the art can obtain other drawings based on these drawings without any inventive effort. In the drawings: Figure 1 This is a schematic flowchart illustrating a method for preparing a multi-plant component facial mask composition in one embodiment; Figure 2 This is a schematic flowchart of step S1 in a method for preparing a multi-plant component facial mask composition in one embodiment; Figure 3 This is a schematic flowchart of step S2 in a method for preparing a multi-plant component facial mask composition in one embodiment; Figure 4 This is a schematic flowchart of step S3 in a method for preparing a multi-plant component facial mask composition in one embodiment. Detailed Implementation

[0014] Exemplary embodiments will now be described more fully with reference to the accompanying drawings. However, these exemplary embodiments can be implemented in many forms and should not be construed as limited to the examples set forth herein; rather, these embodiments are provided so that this disclosure will be more thorough and complete, and will fully convey the concept of the exemplary embodiments to those skilled in the art.

[0015] Furthermore, the described features or characteristics may be combined in any suitable manner in one or more embodiments. Numerous specific details are provided in the following description to give a thorough understanding of embodiments of this disclosure. However, those skilled in the art will recognize that the technical solutions of this disclosure may be practiced without one or more of the specific details, or other methods, steps, etc. may be employed. In other instances, well-known methods, implementations, or operations are not shown or described in detail to avoid obscuring various aspects of this disclosure.

[0016] The flowcharts shown in the accompanying drawings are merely illustrative and do not necessarily include all content and operations / steps, nor do they necessarily have to be performed in the described order. For example, some operations / steps can be broken down, while others can be combined or partially combined; therefore, the actual execution order may change depending on the specific circumstances.

[0017] like Figure 1 and Figure 2 As shown, this invention proposes a method for preparing a multi-plant component facial mask composition, the steps of which include: S1. The protein component and the carboxyl-containing anionic polysaccharide component are added to an aqueous medium for hydration, and the pH is adjusted to acidic conditions to obtain a composite condensed phase. Then, the plant active component is added to the composite condensed phase for coating to obtain a plant active composite carrier dispersion.

[0018] Step S1 includes: S1.1. Add at least two of the following extracts: camellia flower extract, scutellaria root extract, polygonum cuspidatum root extract, tea extract, and rosemary leaf extract to an aqueous medium and stir at 20–35°C for 20–40 min to obtain the plant extract to be coated. Add at least two of the following extracts: aloe vera leaf extract, witch hazel extract, centella asiatica extract, licorice root extract, and chamomile flower extract to another aqueous medium and stir at 35°C for 10–30 min to obtain the hydrophilic plant extract. S1.2 Add the biopolymer component containing protonable amino groups to an aqueous medium for hydration, stir and dissolve at 50-60°C and cool to 35-45°C to obtain a biopolymer dispersion. Add the anionic polysaccharide component containing carboxyl groups to another portion of the aqueous medium, stir and hydrate at 35-45°C to obtain anionic polysaccharide dispersion. S1.3 Add the plant extract to be coated to the biopolymer dispersion and stir at 35-45℃ for 10-20 min. Then add the anionic polysaccharide dispersion and adjust the pH to 3.8-4.5 using the acidity adjustment component. Continue stirring for 20-40 min to obtain the composite coagulated dispersion. S1.4 Cool the composite coagulated dispersion to 8-15℃, add hydrophilic plant extract, stir gently for 10-20 min, and then let it stand at 5-10℃ for 1-3 h to obtain the plant active composite carrier dispersion.

[0019] The biopolymer component containing protonable amino groups includes at least one of type A gelatin and type B gelatin; the anionic polysaccharide component containing carboxyl groups includes at least one of gum arabic and pectin; the acidity regulating component includes at least one of citric acid and lactic acid; the dry basis mass ratio of the biopolymer component to the anionic polysaccharide component is 1.5:1 to 2.5:1; the mass fractions of the biopolymer dispersion and the anionic polysaccharide dispersion are 4% to 8% respectively; the dry basis mass ratio of the plant extract to be coated to the total dry basis mass of the biopolymer component and the anionic polysaccharide component is 1:2 to 1:5; and the mass ratio of the plant extract to be coated to the hydrophilic plant extract is 1:0.5 to 1:3.

[0020] Gelatin and gum arabic or pectin are dissolved and hydrated separately in an aqueous medium, allowing the polymer chains to fully contact the water and reducing clumping caused by localized water absorption during direct mixing. This provides conditions for subsequent contact between plant extracts and carrier components. Citric acid or lactic acid is used to adjust the pH of the system. Under conditions where gelatin has a net positive charge and the anionic polysaccharide retains sufficient negative charge, the protonated amino groups in gelatin can electrostatically attract the dissociated carboxyl groups in the polysaccharide, promoting the combination of the two types of polymers and forming an enriched complex condensed phase, providing loading space for some plant active ingredients.

[0021] First, the plant extract to be coated is mixed with a gelatin dispersion to ensure sufficient contact between some polyphenols, flavonoids, and other components in the selected plant extract and the gelatin. The phenolic hydroxyl groups and other groups in these components can form hydrogen bonds with the polar groups on the gelatin peptide chains, and some hydrophobic structures can also interact with the hydrophobic regions of the gelatin. Subsequently, anionic polysaccharides are added and the pH is adjusted, allowing the portion of the plant components already bound to the gelatin to be enriched along with the composite condensed phase, thereby reducing the proportion completely free in the aqueous phase and providing conditions for the retention of plant active ingredients in subsequent formulations. This process involves physical binding and encapsulation; it does not mean that all extracts enter the carrier, nor does it necessarily mean that the water solubility of poorly soluble components will increase.

[0022] Cooling and allowing the composite condensed dispersion to stand at low temperatures promotes the formation of physical bonds between gelatin segments, causing the gelatin-rich condensed phase to gradually gel and helping to limit the migration of bound plant components. Adding another portion of the plant extract after cooling avoids the aforementioned high-temperature mixing process, reducing heating time. Gentle stirring ensures that the water-soluble components are mainly distributed in the continuous aqueous phase and can further contact the carrier surface. This results in a compound system where some plant components are bound to the carrier, while others are dispersed in the aqueous phase, providing a foundation for the formulation of subsequent mask compositions. The physical bonds formed at low temperatures are temperature-dependent; the actual dispersion state and storage stability still need to be verified based on the final concentration and subsequent formulation.

[0023] S2. Add drying protection components and functional auxiliary components to the plant active composite carrier dispersion, and obtain composite adsorption powder after vacuum freeze drying. The functional auxiliary components include carbon adsorption components and layered silicate adsorption components.

[0024] Please refer to Figure 3 Step S2 includes: S2.1 Add the layered silicate adsorbent component to water, stir at 20-35℃ and let it stand to swell for 2-6 h to obtain a layered silicate dispersion; S2.2 Add the carbonaceous adsorption component and the coloring component to the layered silicate dispersion, and stir and disperse at 20-35℃ for 20-40 min to obtain the adsorption dispersion; S2.3 Add the drying and protection components to the plant active composite carrier dispersion, stir and dissolve at 5-20℃, then add the adsorption dispersion and mix to obtain the composite dispersion to be freeze-dried. S2.4 Pre-freeze the composite dispersion to be freeze-dried, and then freeze-dry it under vacuum for 18 to 30 hours at a cold trap temperature not higher than -60℃ and a chamber pressure of 3 to 15 Pa. Crush and sieve the freeze-dried material to obtain the composite adsorption powder.

[0025] The layered silicate adsorption component includes at least one of bentonite, kaolin, and montmorillonite; the carbonaceous adsorption component includes at least one of carbon powder and activated carbon; the drying and protection component includes at least one of maltodextrin and trehalose; and the coloring component includes at least one of CI 77266 and iron oxide black. Based on 100 parts by weight of the dry basis of the layered silicate adsorption component, the carbonaceous adsorption component is 10-50 parts by weight, the drying and protection component is 20-80 parts by weight, and the coloring component is 1-10 parts by weight. The mass fraction of the layered silicate adsorption component in water is 1%-5%.

[0026] Functional auxiliary components also include plant mucilage components; The preparation steps for plant mucilage components are as follows: Plant mucilage raw materials are added to an aqueous extraction medium and extracted at 40–60°C for 30–120 min to obtain plant mucilage extract. The plant mucilage raw materials include at least one of the flowers of the genus Althaea and the genus Hibiscus. The aqueous extraction medium includes at least one of water and aqueous ethanol. The plant mucilage extract was filtered or centrifuged to separate the solid and liquid phases, and the liquid phase was concentrated and the solid content was adjusted to 2% to 6% to obtain the plant mucilage component. Between step S2.1 and step S2.2, step S2 further includes: The plant mucilage component was added to the layered silicate dispersion and stirred at 20–35°C for 20–40 min to distribute the plant mucilage component at the hydration interface of the layered silicate particles. Based on 100 parts by weight of the dry basis of the layered silicate adsorbed component, the solids in the plant mucilage component were 1–10 parts by weight, and the mass ratio of the plant mucilage raw material to the aqueous extraction medium was 1:5–1:20.

[0027] The layered silicate adsorbent components are pre-stirred and allowed to stand in water, which facilitates the wetting of the particle surface and reduces clumping when the dry powder is directly mixed with the plant-based active composite carrier. Specifically, montmorillonite in bentonite and montmorillonite added alone undergo a certain degree of interlayer hydration and swelling, while kaolinite mainly undergoes surface wetting and hydration. This pretreatment ensures sufficient contact between the mineral particles and the aqueous medium, providing conditions for the subsequent dispersion of plant mucilage, carbonaceous adsorbent components, and coloring components.

[0028] Filtration or centrifugation of plant mucilage extracts can reduce the introduction of insoluble plant residues, while concentration and solids content adjustment facilitate control over the amount added. The polysaccharides in mucilage contain hydroxyl groups, and some also contain carboxyl groups, giving them the ability to bind water and bind to mineral surfaces through interactions such as hydrogen bonds. Adding plant mucilage to the pre-hydrated mineral dispersion promotes sufficient contact between the mucilage and mineral particles; when the dosage and system conditions are appropriate, the increased viscosity of the aqueous phase and the presence of hydrated polymer chains on the particle surface can slow down particle sedimentation, providing conditions for subsequent mixing.

[0029] Pre-mixing the carbonaceous adsorption component and the layered silicate adsorption component in the aqueous phase facilitates a more uniform distribution of the two types of particles before freeze-drying. The surface and accessible pores of activated carbon can adsorb some organic matter, while mineral particles provide corresponding surface adsorption and liquid absorption, together forming the adsorption basis of the composite powder. The adsorption capacity of ordinary carbon powder depends on its pore structure and surface properties and cannot be directly equated with activated carbon. Carbon black or iron oxide black is mainly used for color adjustment; pre-dispersion helps reduce localized color spots caused by pigment agglomeration during subsequent formulation.

[0030] Maltodextrin and trehalose contain numerous hydroxyl groups, which can form hydrogen bonds with polar groups in plant bioactive carriers. Under suitable freeze-drying conditions, they form a sugar-rich drying matrix, restricting the molecular movement of some components and mitigating structural changes caused by freezing and water loss. Maltodextrin serves both as a filler and a drying matrix former, while trehalose provides freeze-drying protection; both contribute to the retention of some plant bioactive components during the drying process.

[0031] Pre-freezing and vacuum freeze-drying remove ice primarily through sublimation, reducing the thermal impact of continuous high-temperature drying. Under conditions where the material does not experience significant collapse, the pores left after ice crystal removal provide pathways for subsequent moisture entry, facilitating the wetting of the freeze-dried product. Plant-based active carriers, sugars, and adsorbent particles are retained in the drying matrix, and after pulverization and sieving, they form a powder that is easy to measure and blend, providing a raw material basis for the subsequent preparation of facial mask compositions.

[0032] S3. The acrylic (ester) crosslinked polymer is added to an aqueous medium for dispersion and hydration. After neutralization, a thickened and stable dispersion is obtained. The thickened and stable dispersion is added to a polyvinyl alcohol film-forming solution. Composite adsorbent powder is then added. After stirring, homogenization, degassing, and aging, a multi-plant component facial mask composition is obtained.

[0033] Please refer to Figure 4 Step S3 includes: S3.1. Add polyvinyl alcohol to water for hydration, stir at 80-90℃ until dissolved to obtain polyvinyl alcohol film-forming solution. Add acrylic (ester) crosslinking polymer to another part of water for dispersion and hydration, add alkaline regulator to neutralize, and obtain thickened and stable dispersion. S3.2 Cool the polyvinyl alcohol film-forming solution to no higher than 45°C, add the thickening and stabilizing dispersion, and add the moisturizing component, skin conditioning component and chelating component. Stir evenly to obtain the composite film-forming base material. S3.3 Cool the composite film-forming base material to no higher than 35°C, add the composite adsorption powder and stir to disperse, then add ethanol, preservative auxiliary components and fragrance components, and adjust the pH to 5.2-6.2 to obtain a multi-plant component film-forming slurry; S3.4. The multi-plant component film-forming slurry is vacuum degassed at 20-30℃ for 10-30 min, allowed to stand and mature for 30-120 min, and then filled to obtain a multi-plant component facial mask composition.

[0034] The acrylate crosspolymer includes at least one of carbomer and acrylate / C10-30 alkanol acrylate crosspolymers; the alkalinity regulator includes at least one of sodium hydroxide and aminomethylpropanol; the moisturizing component includes at least two of glycerin, propylene glycol, and butylene glycol; the skin conditioning component includes at least one of allantoin and dipotassium glycyrrhizate; the chelating component includes at least one of disodium EDTA and sodium citrate; and the preservative auxiliary component includes methylparaben, 1,2-hexanediol, ethylhexylglycerin, capryloyl hydroxamic acid, phenoxyethanol, and p-hydroxypropyl hydroxypropyl ester. The composition contains at least two of the following: acetophenone; fragrance components include at least one of the following: fragrance and plant fragrance; and based on the total mass of the multi-plant component mask composition, the composition comprises: 8%–18% polyvinyl alcohol, 0.2%–1.0% acrylate cross-linked polymer, 5%–20% composite adsorbent powder, 3%–15% ethanol, 3%–12% moisturizing components, 0.1%–2% skin conditioning components, 0.05%–0.5% chelating components, 0.5%–1.0% preservative auxiliary components, 0.02%–0.10% fragrance components, and the balance being water.

[0035] Polyvinyl alcohol (PVA) is fully hydrated and dissolved by heating to form a film-forming solution, reducing the impact of undissolved particles on coating uniformity and film continuity. After the mask is applied, as water and ethanol gradually evaporate, the PVA molecular chains approach each other, forming a film with a certain cohesive force through chain segment entanglement and hydrogen bonding. This allows the dispersed composite adsorbent powder to be removed along with the film, providing conditions for removing some of the dirt adhering to the skin surface.

[0036] The separate dispersion and hydration of acrylic crosslinked polymers help reduce clumping when directly added to viscous film-forming solutions. After neutralization, some carboxyl groups in the polymer are converted into negatively charged carboxylate groups. The electrostatic repulsion and hydration between chain segments promote the swelling of the original crosslinked network, increase the viscosity of the base material, and form a certain yield stress under suitable conditions. This helps to slow down the sedimentation of adsorbed particles and reduce flow after coating.

[0037] Glycerin, propylene glycol, and butylene glycol contain hydroxyl groups, which can form hydrogen bonds with water and polyvinyl alcohol, thus providing both moisturizing and plasticizing effects. Adding appropriate amounts can regulate the interactions between polymer chains in the film, reducing excessive brittleness and breakage during removal after drying. Ethanol is used to adjust the volatility of the mixed solvents, and when the ratio is appropriate, it helps to shorten the drying time. Both types of components need to be matched with the film-forming agent and powder dosage to balance spreading, drying, and removal performance, avoiding excessive moisturizing components that can cause slow drying or a sticky film.

[0038] The film-forming solution is cooled in stages before the addition of the plant-based active complex carrier and other auxiliary components. This avoids the plant ingredients undergoing the high-temperature dissolution process of polyvinyl alcohol, reducing the heating time. Allantoin and dipotassium glycyrrhizate, as skin conditioning components, provide the basis for the formula's soothing and caring effects; chelating components bind some metal ions, helping to reduce oxidation or color changes caused by metal ions. Preservatives and preservative auxiliary components are used to inhibit microbial growth during storage and use, while fragrance components are used to adjust the product's scent.

[0039] In one embodiment, between step S3.2 and step S3.3, step S3 further includes: A film-forming polysaccharide component is added to a composite film-forming matrix and stirred and dispersed at 20–40°C to obtain a composite film-forming matrix containing film-forming polysaccharides. Subsequently, a sizing ion source and a slow-release stabilizing component are added and stirred continuously to allow the divalent metal ions released by the sizing ion source to undergo ionic cross-linking with the carboxyl groups in the film-forming polysaccharides. The film-forming polysaccharide component includes at least one of sodium alginate and sodium carboxymethyl cellulose; the shaping ion source includes at least one of calcium sulfate and calcium lactate; and the sustained-release stabilizing component includes at least one of tetrasodium pyrophosphate and sodium citrate. Based on 100 parts by mass of polyvinyl alcohol, the film-forming polysaccharide component comprises 5 to 30 parts by mass, the shaping ion source comprises 1 to 10 parts by mass, and the sustained-release stabilizing component comprises 0.5 to 5 parts by mass. The mass ratio of the film-forming polysaccharide component to the shaping ion source is 3:1 to 15:1.

[0040] This disclosure discloses a multi-plant component facial mask composition, which is prepared by a method for preparing a multi-plant component facial mask composition.

[0041] Common raw materials and operating conditions for the following embodiments: All embodiments used the same batch of corresponding raw materials. Tea extract, Scutellaria baicalensis root extract, Aloe vera leaf extract, and Centella asiatica extract were all water-dispersible powder raw materials; polyvinyl alcohol was a grade with a degree of alcoholysis of 88% and an average degree of polymerization of 500; type A gelatin was a grade with a gel strength of 200; calcium sulfate was dihydrate, calcium lactate was pentahydrate, and sodium citrate was anhydrous. The water used in all embodiments was purified water, and the ethanol was anhydrous ethanol. All raw material amounts were by weight.

[0042] 20g of citric acid was added to 180g of water and stirred at 25°C for 10 minutes to obtain a 10% (w / w) citric acid aqueous solution. 20g of sodium hydroxide was added to 180g of water and stirred for 10 minutes, then cooled to 25°C to obtain a 10% (w / w) sodium hydroxide aqueous solution. The specified mass was weighed from the above solutions for each embodiment, and the water carried over from the solutions was not counted again in the separately added purified water.

[0043] The composite adsorbent powders in all embodiments were processed using the same freeze-drying procedure. The composite dispersion to be freeze-dried was dispensed into trays with a thickness of 5 mm and pre-frozen at -40°C for 8 hours. Subsequently, the cold trap temperature was set to -65°C, the chamber pressure to 10 Pa, and the shelf temperatures were sequentially set to -25°C for 10 hours, -10°C for 8 hours, and 20°C for 6 hours, for a total vacuum freeze-drying time of 24 hours. The freeze-dried material was then pulverized using a blade grinder at 3000 rpm for 30 seconds, and then passed through a 100-mesh sieve to collect the undersize powder. This fixed freeze-drying, pulverizing, and sieving procedure was used in all the following embodiments.

[0044] Example 1: Add 3g of tea extract and 3g of Scutellaria baicalensis root extract to 54g of water and stir at 300 rpm for 30 minutes at 30℃ to obtain 60g of plant extract to be coated. Separately, add 3g of Aloe vera leaf extract and 3g of Centella asiatica extract to 54g of water and stir at 300 rpm for 20 minutes at 25℃ to obtain 60g of hydrophilic plant extract. The mass fraction of plant extracts in both extracts is 10%. The mass ratio of tea extract to Scutellaria baicalensis root extract is 1:1, the mass ratio of Aloe vera leaf extract to Centella asiatica extract is 1:1, and the mass ratio of the plant extract to be coated to the hydrophilic plant extract is 1:1.

[0045] 16g of type A gelatin was added to 250.67g of water and hydrated at 25°C for 30 minutes. The temperature was then raised to 55°C and stirred at 300 rpm for 30 minutes, followed by cooling to 40°C to obtain a biopolymer dispersion. 8g of gum arabic was added to 125.33g of water and stirred at 300 rpm for 40 minutes at 40°C to obtain an anionic polysaccharide dispersion. The mass ratio of type A gelatin to gum arabic was 2:1, and the mass fraction of both polymer dispersions was approximately 6%.

[0046] Add 60g of the plant extract to be coated to the biopolymer dispersion and stir at 300 rpm for 15 minutes at 40℃. Then, add the entire anionic polysaccharide dispersion within 5 minutes. Subsequently, add 4g of a 10% citric acid aqueous solution within 4 minutes and continue stirring at 40℃ for 30 minutes to obtain a composite coagulated dispersion. In this stage, 0.4g of citric acid was added, bringing the total amount of the plant extract to be coated to 6g, and the total amount of type A gelatin and gum arabic to 24g, with a mass ratio of 1:4.

[0047] The composite coagulated dispersion was cooled to 12°C, 60g of hydrophilic plant extract was added, and the mixture was stirred at 150 rpm for 15 minutes. Then it was allowed to stand at 8°C for 2 hours to obtain the plant active composite carrier dispersion.

[0048] Add 40g of bentonite to 1293.33g of water, stir at 500 rpm for 30 minutes at 25℃, and then let stand to swell for 4 hours to obtain a layered silicate dispersion with a bentonite mass fraction of approximately 3%. Add 12g of activated carbon and 0.8g of iron oxide black, stir at 500 rpm for 30 minutes at 25℃ to obtain an adsorption dispersion. The composition is: 100 parts by mass of bentonite, 30 parts by mass of activated carbon, and 2 parts by mass of iron oxide black.

[0049] The entire plant-based active composite carrier dispersion was placed at 20°C, and 20g of maltodextrin was added. The mixture was stirred at 300 rpm for 20 minutes, followed by the addition of the entire adsorption dispersion over 10 minutes. Stirring continued for another 20 minutes to obtain the composite dispersion to be freeze-dried. The mixture consisted of 100 parts by weight of bentonite and 50 parts by weight of maltodextrin. Pre-freezing, vacuum freeze-drying, pulverizing, and sieving were performed under common operating conditions to obtain the composite adsorption powder. 100g of this powder was weighed for subsequent mask preparation.

[0050] The final mask's fixed ingredients are: 120g polyvinyl alcohol, 3g carbomer, 100g composite adsorbent powder, 30g glycerin, 20g propylene glycol, 2g allantoin, 2g dipotassium glycyrrhizate, 0.5g disodium EDTA, 80g ethanol, 7.2g phenoxyethanol, 0.8g ethylhexylglycerin, 0.5g fragrance, 12g of a 10% sodium hydroxide aqueous solution, 2g of a 10% citric acid aqueous solution, and 620g of water added separately, for a total weight of 1000g. The above-mentioned acid-base adjusting solution is an additional ingredient added during the finished product preparation stage and does not include the citric acid used in the composite adsorbent powder preparation stage.

[0051] Slowly add 120g of polyvinyl alcohol to 400g of water, hydrate at 25°C and 300 rpm for 30 minutes, then stir at 90°C and 400 rpm for 120 minutes to obtain a polyvinyl alcohol film-forming solution. Cover the dissolving container and connect it to a reflux condenser to reduce water loss during heating.

[0052] Slowly add 3g of carbomer to 150g of water, stir at 300 rpm for 20 minutes at 25°C, and then let stand for hydration for 40 minutes. Add 12g of 10% sodium hydroxide aqueous solution within 5 minutes, and stir at 200 rpm for 15 minutes to obtain a thickened and stable dispersion.

[0053] Add 2g of allantoin to 30g of glycerol and stir at 25℃ for 10 minutes to obtain an allantoin pre-dispersion. Add 2g of dipotassium glycyrrhizate and 0.5g of disodium EDTA to 20g of water and stir at 35℃ for 15 minutes to obtain an auxiliary component solution. Cool the polyvinyl alcohol film-forming solution to 40℃, add all the thickening and stabilizing dispersion, allantoin pre-dispersion, and auxiliary component solution, and stir at 300 rpm for 20 minutes to obtain a composite film-forming base.

[0054] Cool the composite film-forming base material to 30°C, and add 100g of composite adsorption powder in batches over 10 minutes, stirring at 400 rpm for 20 minutes. Use a rotor-stator homogenizing head with a rotor diameter of 20mm to homogenize at 3000 rpm for 2 minutes, with the jacket temperature set at 30°C.

[0055] 7.2g of phenoxyethanol, 0.8g of ethylhexylglycerin, and 20g of propylene glycol were stirred at 25°C for 10 minutes, and then the above base material was added. 0.5g of fragrance and 80g of ethanol were stirred at 25°C for 5 minutes, and then the base material was slowly added over 10 minutes. Subsequently, 2g of a 10% citric acid aqueous solution and 50g of the remaining water were added, and the mixture was stirred at 250 rpm for 15 minutes to obtain a multi-plant component film-forming slurry.

[0056] The film-forming slurry was placed at 25°C, and the absolute pressure inside the container was reduced to 30 kPa within 5 minutes. Then, it was stirred at 60 rpm for 20 minutes to degas. After restoring to normal pressure, it was sealed and allowed to stand at 25°C for 60 minutes. It was then filled into bottles of 100g each to obtain a multi-plant component facial mask composition.

[0057] In this embodiment, the finished product contains 12% polyvinyl alcohol, 0.3% carbomer, 10% composite adsorbent powder, 8% ethanol, 3% glycerol, 2% propylene glycol, 0.2% allantoin, 0.2% dipotassium glycyrrhizate, 0.05% disodium EDTA, 0.72% phenoxyethanol, 0.08% ethylhexylglycerin, and 0.05% fragrance. The mass ratio of glycerol to propylene glycol is 3:2, and the mass ratio of phenoxyethanol to ethylhexylglycerin is 9:1. In the final product formulation stage, 1.2g of sodium hydroxide and 0.2g of citric acid are added.

[0058] Example 2: This embodiment adds the preparation of plant mucilage components and the premixing step with bentonite to the original embodiment. The other raw material types and the fixed addition of the final mask are the same as in embodiment 1.

[0059] 100g of hollyhock flowers (dried flowers) were added to 1000g of water and extracted at 50℃ with stirring at 300 rpm for 60 minutes. After extraction, the mixture was centrifuged at 4000 rpm for 10 minutes, and the supernatant was collected. The supernatant was concentrated at 40℃ and 10 kPa absolute pressure for 60 minutes, and then pre-frozen and freeze-dried under common operating conditions to obtain the dried plant mucilage extract. 2g of the dried plant mucilage extract was weighed and added to 48g of water. The mixture was stirred at 25℃ with stirring at 300 rpm for 30 minutes to obtain 50g of plant mucilage fraction with a solid content of 4%. The mass ratio of plant mucilage extract to extraction medium was 1:10.

[0060] 3g of tea extract, 3g of Scutellaria baicalensis root extract, and 54g of water were stirred at 30°C for 30 minutes to obtain 60g of plant extract to be coated; 3g of Aloe vera leaf extract, 3g of Centella asiatica extract, and 54g of water were stirred at 25°C for 20 minutes to obtain 60g of hydrophilic plant extract. A biopolymer dispersion was prepared using 16g of type A gelatin and 250.67g of water, and an anionic polysaccharide dispersion was prepared using 8g of gum arabic and 125.33g of water. The hydration, dissolution, and cooling conditions were the same as in Example 1.

[0061] The plant extract to be coated was added to the biopolymer dispersion and stirred at 40°C for 15 minutes. Then, all the anionic polysaccharide dispersion and 4g of a 10% citric acid aqueous solution were added, and stirring was continued at 40°C for 30 minutes. After cooling to 12°C, the hydrophilic plant extract was added, and the mixture was gently stirred for 15 minutes. Finally, it was allowed to stand at 8°C for 2 hours to obtain the plant active composite carrier dispersion. The stirring speed and feeding time were the same as in Example 1.

[0062] Add 40g of bentonite to 1293.33g of water, stir at 500 rpm for 30 minutes at 25℃, and let stand to swell for 4 hours. Then add 50g of plant mucilage component, stir at 300 rpm for 30 minutes at 25℃, then add 12g of activated carbon and 0.8g of iron oxide black, and stir at 500 rpm for 30 minutes to obtain an adsorption dispersion containing plant mucilage component.

[0063] The entire plant-based active composite carrier dispersion was placed at 20°C, and 20g of maltodextrin was added. The mixture was stirred at 300 rpm for 20 minutes, followed by the addition of the entire adsorption dispersion over 10 minutes, and stirring continued for another 20 minutes. The powder was then pre-frozen, vacuum freeze-dried, pulverized, and sieved under the same operating conditions to obtain the composite adsorption powder. The composition consisted of 5 parts by weight of dried plant mucilage extract (100 parts by weight), 30 parts by weight of activated carbon, 50 parts by weight of maltodextrin, and 2 parts by weight of iron oxide black.

[0064] Weigh 100g of the composite adsorbent powder of this embodiment, and prepare a face mask using 120g of polyvinyl alcohol, 3g of carbomer, 30g of glycerin, 20g of propylene glycol, 2g of allantoin, 2g of dipotassium glycyrrhizate, 0.5g of disodium EDTA, 80g of ethanol, 7.2g of phenoxyethanol, 0.8g of ethylhexylglycerin, 0.5g of fragrance, 12g of a 10% sodium hydroxide aqueous solution, 2g of a 10% citric acid aqueous solution, and 620g of water, following the fixed temperature, time, rotation speed, water distribution, and ingredient addition sequence of Example 1.

[0065] The obtained slurry was defoamed for 20 minutes at 60 revolutions per minute under an absolute pressure of 30 kPa at 25°C. After returning to normal pressure, it was sealed and allowed to stand for 60 minutes at 25°C before being filled into bottles with the nominal amount of 100g each.

[0066] Example 3: This embodiment further adds the steps of adding sodium alginate, calcium sulfate, and sodium citrate to the process described in Example 2. The plant mucilage component, the plant active composite carrier dispersion, and the composite adsorbent powder are all prepared according to the fixed raw material amounts and process conditions of Example 2.

[0067] The fixed ingredients of the mask in this embodiment are: 120g polyvinyl alcohol, 3g carbomer, 100g composite adsorbent powder prepared in Example 2, 30g glycerin, 20g propylene glycol, 2g allantoin, 2g dipotassium glycyrrhizate, 0.5g disodium EDTA, 80g ethanol, 7.2g phenoxyethanol, 0.8g ethylhexylglycerin, 0.5g fragrance, 6g sodium alginate, 1.2g calcium sulfate, 0.6g sodium citrate, 12g of 10% sodium hydroxide aqueous solution, 2g of 10% citric acid aqueous solution, and 612.2g water, with a total mass of 1000g.

[0068] 120g of polyvinyl alcohol was added to 400g of water and hydrated at 25°C for 30 minutes and stirred at 90°C for 120 minutes according to the conditions of Example 1 to obtain a film-forming solution. 3g of carbomer was added to 150g of water and dispersed and hydrated according to the conditions of Example 1. Then, 12g of a 10% sodium hydroxide aqueous solution was added to obtain a thickened and stabilized dispersion.

[0069] 2g of allantoin and 30g of glycerin were premixed, and 2g of dipotassium glycyrrhizate and 0.5g of disodium EDTA were dissolved in 20g of water. The above components and the thickening and stabilizing dispersion were added to a polyvinyl alcohol film-forming solution cooled to 40°C, and stirred at 300 rpm for 20 minutes to obtain the composite film-forming base. The premixing and pre-dissolving conditions were the same as in Example 1.

[0070] Cool the composite film-forming base material to 35℃, and slowly sprinkle 6g of sodium alginate over 10 minutes, stirring at 300 rpm for 60 minutes. Add 0.6g of sodium citrate to 5g of water, stir at 25℃ for 10 minutes, then add the base material, and stir for another 10 minutes. Add 1.2g of calcium sulfate to 10g of water, stir at 500 rpm for 10 minutes at 25℃ to form a calcium salt dispersion, add the base material over 10 minutes, and then stir at 300 rpm for 20 minutes at 35℃.

[0071] Based on 100 parts by weight of polyvinyl alcohol, sodium alginate comprises 5 parts by weight, calcium sulfate comprises 1 part by weight, and sodium citrate comprises 0.5 parts by weight; the mass ratio of sodium alginate to calcium sulfate is 5:1. Sodium citrate is added before calcium sulfate to regulate the initial process of calcium ions participating in the binding of sodium alginate.

[0072] Cool the base material to 30°C, add 100g of composite adsorption powder within 10 minutes, stir at 400 rpm for 20 minutes, then use a homogenizing head with a rotor diameter of 20mm to homogenize at 3000 rpm for 2 minutes, with the jacket temperature at 30°C.

[0073] Add 20g of propylene glycol, 7.2g of phenoxyethanol, and 0.8g of ethylhexylglycerin after premixing for 10 minutes; add 80g of ethanol and 0.5g of fragrance after premixing for 5 minutes, and then add them within 10 minutes. Then add 2g of 10% citric acid aqueous solution and the remaining 27.2g of water, and stir at 250 rpm for 15 minutes to obtain the film-forming slurry.

[0074] The film-forming slurry was degassed for 20 minutes at 60 rpm under 25°C and 30 kPa absolute pressure. After returning to normal pressure, it was sealed and allowed to stand for 60 minutes at 25°C before being bottled in 100g bottles. Sodium alginate, calcium sulfate, and sodium citrate accounted for 0.6%, 0.12%, and 0.06% of the total mass of the finished product, respectively.

[0075] Example 4: This embodiment adds a hydroxypropyl betacyclodextrin pre-encapsulation treatment to the original embodiment 2, and adjusts the amount of maltodextrin added. Sodium alginate, calcium sulfate and sodium citrate as in the original embodiment 3 are not added.

[0076] 9g of hydroxypropyl beta-cyclodextrin was added to 54g of water and stirred at 300 rpm for 15 minutes at 30°C. Then, 3g of tea extract and 3g of Scutellaria baicalensis root extract were added, and the mixture was stirred at 30°C for another 60 minutes to obtain 69g of pre-encapsulated plant extract dispersion. The mass ratio of hydroxypropyl beta-cyclodextrin to the total amount of tea extract and Scutellaria baicalensis root extract was 1.5:1, and the mass ratio of tea extract to Scutellaria baicalensis root extract was 1:1.

[0077] Add 3g of Aloe vera leaf extract and 3g of Centella asiatica extract to 54g of water, and stir at 300 rpm for 20 minutes at 25°C to obtain 60g of hydrophilic plant extract. The mass ratio of the pre-encapsulated plant extract dispersion to the hydrophilic plant extract is 69:60.

[0078] Add 16g of type A gelatin to 250.67g of water, hydrate and dissolve according to the conditions of Example 1, and cool to 40°C; add 8g of gum arabic to 125.33g of water, and stir at 300 rpm for 40 minutes at 40°C. Add 69g of the pre-encapsulated plant extract dispersion to the biopolymer dispersion, stir at 40°C for 15 minutes, and then add the entire anionic polysaccharide dispersion within 5 minutes.

[0079] Add 4g of a 10% citric acid aqueous solution within 4 minutes, and continue stirring at 40℃ for 30 minutes. After cooling to 12℃, add 60g of hydrophilic plant extract, stir at 150 rpm for 15 minutes, and then let stand at 8℃ for 2 hours to obtain a plant active composite carrier dispersion. The mass ratio of type A gelatin to gum arabic is 2:1, and the mass ratio of the total amount of plant extract to be coated to the total amount of type A gelatin and gum arabic is 1:4.

[0080] The plant mucilage extract was prepared under the fixed conditions of Example 2. 2g of the extract was added to 48g of water and stirred at 300 rpm for 30 minutes at 25°C to obtain 50g of the plant mucilage component. 40g of bentonite was added to 1293.33g of water and stirred at 500 rpm for 30 minutes at 25°C, then allowed to stand for 4 hours. Next, 50g of the plant mucilage component was added, and the mixture was stirred at 300 rpm for 30 minutes. Subsequently, 12g of activated carbon and 0.8g of iron oxide black were added, and the mixture was stirred at 500 rpm for 30 minutes to obtain an adsorption dispersion.

[0081] The entire plant-based active composite carrier dispersion was placed at 20°C, and 11g of maltodextrin was added. The mixture was stirred at 300 rpm for 20 minutes, and then the entire adsorption dispersion was added within 10 minutes. The mixture was stirred for another 20 minutes. The mixture was then pre-frozen, vacuum freeze-dried, pulverized, and sieved under the same operating conditions to obtain the composite adsorption powder.

[0082] Based on 100 parts by weight of bentonite, the composition includes 27.5 parts by weight of maltodextrin, 22.5 parts by weight of hydroxypropyl beta-cyclodextrin, 5 parts by weight of dried plant mucilage extract, 30 parts by weight of activated carbon, and 2 parts by weight of iron oxide black. The total amount of hydroxypropyl beta-cyclodextrin and maltodextrin added is 20g, which is the same as the amount of maltodextrin added in Example 2.

[0083] Weigh 100g of the composite adsorbent powder prepared in this embodiment, and use 120g of polyvinyl alcohol, 3g of carbomer, 30g of glycerin, 20g of propylene glycol, 2g of allantoin, 2g of dipotassium glycyrrhizate, 0.5g of disodium EDTA, 80g of ethanol, 7.2g of phenoxyethanol, 0.8g of ethylhexylglycerin, 0.5g of fragrance, 12g of a 10% sodium hydroxide aqueous solution, 2g of a 10% citric acid aqueous solution, and 620g of water to prepare a face mask. The total mass of the materials used is 1000g.

[0084] The preparation of the film-forming solution, the preparation of the thickening dispersion, the addition of auxiliary components, the dispersion of powder, and the homogenization all followed the fixed temperature, time, rotation speed, and water distribution as in Example 1. The resulting slurry was degassed for 20 minutes at 60 rpm under 25°C and an absolute pressure of 30 kPa. After returning to normal pressure, it was sealed and allowed to stand for 60 minutes at 25°C before being filled into bottles with a nominal volume of 100 g each.

[0085] Example 5: This embodiment, based on Example 4, adopts a method of separately preparing and storing the film-forming base material and the shaping dispersion, and does not add calcium salt to the film-forming base material containing sodium alginate before filling. The plant active composite carrier, plant mucilage component, and composite adsorbent powder are all prepared according to the fixed dosage and process conditions of Example 4.

[0086] The total mass of the two materials was 1000g, of which the first film-forming base was 950g and the second shaping dispersion was 50g. The total input consisted of 120g polyvinyl alcohol, 3g carbomer, 100g of the composite adsorbent powder prepared in Example 4, 30g glycerol, 20g propylene glycol, 2g allantoin, 2g dipotassium glycyrrhizate, 80g ethanol, 7.2g phenoxyethanol, 0.8g ethylhexylglycerin, 0.5g fragrance, 9g sodium alginate, 2g calcium lactate, 0.6g sodium citrate, 0.15g hydroxyethyl cellulose, 12g of a 10% sodium hydroxide aqueous solution, 2g of a 10% citric acid aqueous solution, and 608.75g of water. Disodium EDTA was not added in this example.

[0087] The first batch of film-forming base material consists of 120g polyvinyl alcohol, 3g carbomer, 100g composite adsorbent powder, 30g glycerin, 18g propylene glycol, 2g allantoin, 2g dipotassium glycyrrhizate, 80g ethanol, 6.84g phenoxyethanol, 0.76g ethylhexylglycerin, 0.5g fragrance, 9g sodium alginate, 0.6g sodium citrate, 12g of 10% sodium hydroxide aqueous solution, 2g of 10% citric acid aqueous solution, and 563.3g water, totaling 950g.

[0088] Add 120g of polyvinyl alcohol to 400g of water and hydrate at 300 rpm for 30 minutes at 25°C, then stir at 400 rpm for 120 minutes at 90°C. Add 3g of carbomer to 120g of water and stir at 300 rpm for 20 minutes at 25°C, then let it stand to hydrate for 40 minutes. Then, add 12g of a 10% sodium hydroxide aqueous solution within 5 minutes and stir at 200 rpm for 15 minutes.

[0089] Add 2g of allantoin to 30g of glycerol and stir at 25°C for 10 minutes; add 2g of dipotassium glycyrrhizate to 20g of water and stir at 35°C for 15 minutes. Cool the polyvinyl alcohol film-forming solution to 40°C, add carbomer thickening and stabilizing dispersion, allantoin pre-dispersion, and dipotassium glycyrrhizate solution, and stir at 300 rpm for 20 minutes.

[0090] Cool the base material to 35℃, then slowly add 9g of sodium alginate over 10 minutes, stirring at 300 rpm for 60 minutes. Add 0.6g of sodium citrate to 5g of water, stir at 25℃ for 10 minutes, then add the base material and stir for another 10 minutes. Cool the base material to 30℃, then add 100g of composite adsorption powder over 10 minutes, stirring at 400 rpm for 20 minutes. Then, use a homogenizing head with a 20mm rotor diameter to homogenize at 3000 rpm for 2 minutes, with the jacket temperature set to 30℃.

[0091] 6.84 g of phenoxyethanol, 0.76 g of ethylhexylglycerin, and 18 g of propylene glycol were premixed at 25°C for 10 minutes and then added to the base material. 0.5 g of fragrance and 80 g of ethanol were premixed for 5 minutes and then added within 10 minutes. Subsequently, 2 g of a 10% citric acid aqueous solution and 18.3 g of the remaining water were added, and the mixture was stirred at 250 rpm for 15 minutes. Following the pressure change program of Example 1, the mixture was degassed at 60 rpm for 20 minutes at 25°C and an absolute pressure of 30 kPa. After returning to normal pressure, the mixture was sealed and allowed to stand at 25°C for 60 minutes to obtain the first film-forming base material.

[0092] The fixed feed for the second shaping dispersion consisted of 2g calcium lactate, 0.15g hydroxyethyl cellulose, 2g propylene glycol, 0.36g phenoxyethanol, 0.04g ethylhexylglycerin, and 45.45g water, totaling 50g.

[0093] Add 0.15g of hydroxyethyl cellulose to 1g of propylene glycol and stir at 25°C for 5 minutes. Then add 30g of water and hydrate by stirring at 300 rpm for 40 minutes. Add 2g of calcium lactate to 15.45g of water and stir at 300 rpm for 20 minutes at 30°C. Then add the hydroxyethyl cellulose dispersion within 5 minutes and continue stirring for 15 minutes.

[0094] Premix 0.36g of phenoxyethanol, 0.04g of ethylhexylglycerin, and the remaining 1g of propylene glycol at 25°C for 10 minutes. Add the second part of the mixture and stir at 200 rpm for 10 minutes. Keep the mixture at 25°C and degas at an absolute pressure of 30kPa for 15 minutes. After restoring to normal pressure, seal and let stand for 30 minutes to obtain the second fixed dispersion.

[0095] The first portion of film-forming base material is packaged in 19g bags, and the second portion of setting dispersion is packaged in 1g bags. The two bags form a set and should be stored separately in sealed containers. When using, take one bag of film-forming base material and one bag of setting dispersion, and stir in a mixing container at 200 rpm for 30 seconds. After mixing, complete the coating process within 60 seconds. The mass ratio of the first portion of film-forming base material to the second portion of setting dispersion is 19:1.

[0096] Based on 100 parts by weight of the mixed polyvinyl alcohol, sodium alginate comprises 7.5 parts by weight, calcium lactate 1.67 parts by weight, and sodium citrate 0.5 parts by weight; the mass ratio of sodium alginate to calcium lactate is 4.5:1. The mass ratio of phenoxyethanol to ethylhexylglycerin in both materials is 9:1, and the preservative auxiliary components each account for 0.8% of their respective material feed weights. After mixing, sodium alginate comprises 0.9%, calcium lactate 0.2%, sodium citrate 0.06%, and hydroxyethyl cellulose 0.015%.

[0097] Experiment 1: Microbiological tests were performed on the multi-plant component facial mask compositions prepared in Examples 1-5 and Comparative Examples 1-3, with three independent preparation batches for each group. Example 5 included a first film-forming base and a second shaping dispersion stored separately, so the two materials were tested separately, and the mixture was further tested after mixing the two materials at a mass ratio of 19:1.

[0098] Microbiological testing was conducted according to the microbiological testing methods specified in the "Cosmetic Safety Technical Specifications". The total bacterial count, total mold and yeast counts of each sample were determined, and thermotolerant coliforms, Staphylococcus aureus, and Pseudomonas aeruginosa were also tested. Method suitability validation was performed before testing by serially diluting the samples using sterile diluent containing a preservative neutralizer to minimize interference from phenoxyethanol, ethylhexylglycerin, and other preservative auxiliary components on microbial culture.

[0099] Total bacterial count, mold count, and yeast count were determined using the culture counting method, and the results were expressed as the number of colonies formed per unit mass of sample. Thermotolerant coliforms, Staphylococcus aureus, and Pseudomonas aeruginosa were detected using qualitative testing methods. The test results are shown in Table 1.

[0100] Table 1: As shown in Table 1, the total bacterial count, mold count, and yeast count in all examples and comparative examples were below the corresponding limit values. Thermotolerant coliforms, Staphylococcus aureus, and Pseudomonas aeruginosa were not detected, indicating that the preservative auxiliary components used, along with the corresponding preparation, degassing, and filling conditions, provided a basis for the microbial control of the mask composition. In Example 5, both the first film-forming base and the second shaping dispersion showed good microbial control results when stored separately, indicating that independently configuring the shaping ion source did not cause an increase in the microbial indicators of the second material.

[0101] Experiment 2: The physicochemical safety of the multi-plant component facial mask compositions prepared in Examples 1-5 and Comparative Examples 1-3 were tested. In Example 5, the first film-forming base and the second shaping dispersion were mixed at a mass ratio of 19:1, and the mixed sample was tested. Three independent preparation batches were set up for each sample.

[0102] Mercury and arsenic were determined by hydride atomic fluorescence spectrometry, lead and cadmium were determined by flame atomic absorption spectrometry, methanol was determined by direct gas chromatography, dioxane was determined by gas chromatography-mass spectrometry, and diethylene glycol was determined according to the method specified in the "Cosmetic Safety Technical Specifications".

[0103] The method detection concentrations for mercury, lead, arsenic, and cadmium were 0.002 mg / kg, 1.5 mg / kg, 0.01 mg / kg, and 0.18 mg / kg, respectively; the method detection concentration for dioxane was 1 mg / kg; the method detection concentration for diethylene glycol was 0.003%; and the method detection concentration for methanol was 25 mg / kg, with a quantitative concentration of 100 mg / kg. Results below the method detection concentration were expressed as "less than the corresponding detection concentration"; when methanol was detected but below the quantitative concentration, it was expressed as "detected and less than 100 mg / kg". The detection results are shown in Table 2.

[0104] Table 2: As shown in Table 2, the concentrations of mercury, lead, arsenic, cadmium, and dioxane in all examples and comparative examples were below the corresponding method detection concentrations. Diethylene glycol was not detected, and although methanol was detected, it was below the quantification concentration and below the corresponding limit. These results indicate that, under the stated raw material and preparation conditions, the introduction of plant extracts, bentonite, activated carbon, iron oxide black, polymeric film-forming components, and other auxiliary components did not cause the tested substances to exceed the limits.

[0105] Experiment 3: The rehydration dispersibility of the composite adsorbent powders prepared in Examples 1-4 and Comparative Examples 1-3 was tested. Example 5 used the same composite adsorbent powder as Example 4, therefore the rehydration dispersibility of the powder in Example 5 was measured using the same batch of composite adsorbent powder.

[0106] Weigh 1.00 g of the composite adsorbent powder and add 20.00 g of purified water at 25°C. Stir at 300 rpm for 5 minutes. Pour the resulting dispersion into a 250 μm sieve and rinse three times with 50.00 g of purified water. Dry the residue on the sieve, along with the sieve mesh, at 50°C until constant weight. Subtract the mass of the sieve mesh to obtain the dry mass of the coarse agglomerates on the sieve. The residual rate of the rehydrated coarse agglomerates is calculated as the ratio of the dry mass of the coarse agglomerates on the sieve to the mass of the composite adsorbent powder fed into the sieve.

[0107] The finished products from each embodiment and comparative example were placed in sealed containers of the same material and stored at 40°C in the dark for 28 days. In Example 5, the first film-forming base and the second sizing dispersion were stored separately. Viscosity testing was performed using the first film-forming base. For plant component testing, the two materials were mixed at a mass ratio of 19:1. Samples before and after storage were equilibrated at 25°C for 24 hours, and the apparent viscosity at a shear rate of 10 sec was measured using a rotational rheometer. The apparent viscosity change rate was calculated as the percentage difference between the apparent viscosity after storage and the initial apparent viscosity relative to the initial apparent viscosity.

[0108] Baicalin was selected as a representative plant component. 1.00 g of the sample before and after storage was weighed and added to 50 mL of 70% methanol aqueous solution. The mixture was extracted by sonication for 30 minutes and centrifuged at 10,000 rpm for 10 minutes. The supernatant was filtered through a microporous membrane, and the baicalin content was determined by high-performance liquid chromatography (HPLC). The baicalin retention rate was calculated as the ratio of the baicalin content after storage to the baicalin content before storage. Three independent batches were prepared for each sample, and the results are expressed as mean ± standard deviation.

[0109] Table 3: As shown in Table 3, the powder obtained after freeze-drying the plant-based active composite carrier formed in Example 1 with the adsorption dispersion had a low rehydration coarse agglomeration residue rate. In Comparative Example 1, the plant extract to be coated was added after freeze-drying, resulting in a decrease in the storage retention of baicalin. This indicates that the plant extract participates in the composite coagulation process of gelatin and gum arabic, which helps to reduce the loss of plant components after entering the system containing activated carbon, mineral particles, and ethanol.

[0110] In Example 2, the addition of plant mucilage after bentonite hydration resulted in less coarse agglomeration residue in the powder after rehydration, and less viscosity change during storage. The hydrophilic polysaccharides in the plant mucilage can contact the hydrated mineral surface, improving the wetting state of mineral particles during co-freeze-drying and subsequent rehydration, and reducing the possibility of direct particle contact leading to the formation of large agglomerates.

[0111] In Comparative Example 2, maltodextrin was added only after freeze-drying. Since the maltodextrin did not participate in the freezing and sublimation drying process, it was difficult to form a continuous dry protective matrix around the plant carrier and adsorbent particles. Therefore, more coarse aggregates remained after rehydration, and the retention of baicalin was relatively low. In Comparative Example 3, the plant-based active composite carrier and the adsorbent dispersion were freeze-dried separately before mixing. The lack of a common dispersion process between the different components before freezing made it more prone to the formation of large aggregates after rehydration.

[0112] In Example 3, sodium alginate, calcium sulfate, and sodium citrate were added before storage. After storage, the apparent viscosity increased significantly, indicating that the binding between calcium ions and sodium alginate can continue during storage, and the slow-release stabilizing component can delay the initial gel formation.

[0113] In Example 4, the storage retention of baicalin was improved after pre-encapsulation treatment with hydroxypropyl beta-cyclodextrin, indicating that pre-encapsulation can provide additional binding space for some plant components. In Example 5, the film-forming base containing sodium alginate and the calcium lactate shaping dispersion were stored separately. The viscosity change of the film-forming base was less than that in the example where calcium salt was added in advance, indicating that separate storage can reduce premature gelation caused by added calcium ions.

[0114] Experiment 4: The mask compositions prepared in each example and comparative example were equilibrated at 25°C for 24 hours. In Example 5, the first part of the film-forming base material and the second part of the shaping dispersion were mixed at a mass ratio of 19:1, stirred at 200 rpm for 30 seconds, and tested immediately.

[0115] Using a coater with a gap of 0.50 mm, each sample was evenly coated onto the surface of a horizontally placed polytetrafluoroethylene (PTFE) plate and dried at 25°C and 50% relative humidity. Timing began immediately after coating completion, with one independent parallel sample taken every minute for inspection. The time when no obvious wet slurry transfer was observed on the film surface and the film could be continuously peeled off from the plate was recorded as the peelable film time.

[0116] Another film layer prepared under the same conditions was placed at 25℃ and 50% relative humidity for 48 hours and cut into strips 10mm wide and 60mm long. Tensile testing was performed using a tensile testing machine with an initial clamping distance of 30mm and a tensile speed of 50mm per minute. Tensile strength was calculated based on the actual film thickness and breaking load, and elongation at break was calculated based on the elongation at break of the strip. Five strips were tested in each independent batch.

[0117] The complete peel-off rate was determined using polyurethane skin dummy sheets. The sample was applied at a rate of 20 mg / cm² to the surface of a 25 cm² dummy sheet and dried at 25°C and 50% relative humidity. Once the film was peelable, it was peeled off in the same direction and at similar speeds. A complete peel was defined as when the entire film could be peeled off without leaving more than one-tenth of the coated area. Ten sheets were tested per independent batch, for a total of 30 sheets. The complete peel-off rate was calculated as the percentage of sheets with complete peel-offs out of the total number of sheets tested.

[0118] The model oil was prepared by mixing trioleic acid glyceride and squalane in a mass ratio of 7:3. 0.100 g of the model oil was uniformly applied to the surface of a 25 square centimeter polyurethane skin simulation sheet and left at 25°C for 30 minutes. Subsequently, 0.500 g of a mask composition was applied to the surface of the simulation sheet, and after the film layer reached a removable state, it was peeled off in the same direction.

[0119] Residual squalane was extracted from the surface of the simulation sheet using n-hexane, and its content was determined by gas chromatography. A blank simulation sheet was also prepared, coated only with model oil without the mask composition. The model oil carryover rate was calculated as the percentage difference between the residual squalane content of the blank simulation sheet and the treated simulation sheet relative to the residual squalane content of the blank simulation sheet. Three independent batches were prepared for each sample, and the test results are shown in Table 4.

[0120] Table 4: As shown in Table 4, Example 1 can form a continuous film layer with certain tensile strength and deformation capacity, and the composite adsorbed powder can be removed along with the film layer. In Example 2, the addition of plant mucilage improved the complete removal capability of the film layer, indicating that the regulation of the mineral particle hydration interface by plant mucilage helps reduce local film defects caused by particle aggregation. The plant mucilage has a certain water retention capacity, which prolongs the time required for the film layer to reach a removable state.

[0121] In Example 3, calcium ions formed ionic bonds with sodium alginate, restricting the movement of some polysaccharide segments and increasing the tensile strength of the film, but reducing the elongation at break and the complete film peeling rate. In Example 4, after adding plant-based pre-encapsulation treatment, good film integrity and model oil removal ability were still maintained, indicating that the addition of hydroxypropyl betacyclodextrin did not significantly disrupt the polyvinyl alcohol film-forming system. In Example 5, the calcium lactate-based dispersion was mixed with the sodium alginate-containing film-forming base material only before use, ensuring that ionic bonding mainly occurred during the use and drying film-forming stages. This method reduced the problem of premature thickening during storage and combined the continuous film-forming effect of polyvinyl alcohol with the ionic bonding of sodium alginate, which is beneficial for forming a film with certain strength and the ability to be peeled off completely.

[0122] The powders in Comparative Examples 2 and 3 exhibited poor rehydration and dispersibility. After the addition of the film-forming matrix, they were more prone to localized particle aggregation, leading to weak areas in the film and a decrease in tensile strength, elongation at break, and complete film removal rate. The inadequate dispersion of adsorbed particles within the continuous film layer also reduced their contact with the model oil contaminants and their ability to be removed along with the film. These results indicate that the addition of maltodextrin before freeze-drying and the co-freezing of the plant-based active composite carrier and the adsorption dispersion are beneficial for improving powder rehydration and dispersion, continuous film formation, and the removal of surface model oil contaminants.

[0123] It should be understood that this disclosure is not limited to the precise structures described above and shown in the accompanying drawings, and various modifications and changes can be made without departing from its scope. The scope of this disclosure is limited only by the appended claims.

Claims

1. A method for preparing a multi-plant component facial mask composition, characterized in that the steps include... include: S1. The protein component and the carboxyl-containing anionic polysaccharide component are added to an aqueous medium for hydration, and the pH is adjusted to acidic conditions to obtain a composite condensed phase. Then, the plant active component is added to the composite condensed phase for coating to obtain a plant active composite carrier dispersion. S2. Add drying protection components and functional auxiliary components to the plant active composite carrier dispersion, and obtain composite adsorption powder after vacuum freeze drying. The functional auxiliary components include carbonaceous adsorption components and layered silicate adsorption components. S3. The acrylic (ester) crosslinked polymer is added to an aqueous medium for dispersion and hydration. After neutralization, a thickened and stable dispersion is obtained. The thickened and stable dispersion is added to a polyvinyl alcohol film-forming solution. Composite adsorbent powder is then added. After stirring, homogenization, degassing, and aging, a multi-plant component facial mask composition is obtained.

2. The method for preparing a multi-plant component facial mask composition according to claim 1, characterized in that, Step S1 includes: S1.

1. Add at least two of the following extracts to an aqueous medium: camellia flower extract, scutellaria root extract, polygonum cuspidatum root extract, tea extract, and rosemary leaf extract. Stir at 20–35°C for 20–40 min to obtain the plant extract to be coated. Add at least two of the following extracts to another aqueous medium: aloe vera leaf extract, witch hazel extract, centella asiatica extract, licorice root extract, and chamomile flower extract. Stir at 35°C for 10–30 min to obtain the hydrophilic plant extract. S1.2 Add the biopolymer component containing protonable amino groups to an aqueous medium for hydration, stir and dissolve at 50-60°C and cool to 35-45°C to obtain a biopolymer dispersion. Add the anionic polysaccharide component containing carboxyl groups to another portion of the aqueous medium, stir and hydrate at 35-45°C to obtain anionic polysaccharide dispersion. S1.3 Add the plant extract to be coated to the biopolymer dispersion and stir at 35-45℃ for 10-20 min. Then add the anionic polysaccharide dispersion and adjust the pH to 3.8-4.5 using the acidity adjustment component. Continue stirring for 20-40 min to obtain the composite coagulated dispersion. S1.4 Cool the composite coagulated dispersion to 8-15℃, add hydrophilic plant extract, stir gently for 10-20 min, and then let it stand at 5-10℃ for 1-3 h to obtain the plant active composite carrier dispersion.

3. The method for preparing a multi-plant component facial mask composition according to claim 2, characterized in that, The biopolymer component containing protonable amino groups includes at least one of type A gelatin and type B gelatin; the anionic polysaccharide component containing carboxyl groups includes at least one of gum arabic and pectin; the acidity regulating component includes at least one of citric acid and lactic acid; the dry basis mass ratio of the biopolymer component to the anionic polysaccharide component is 1.5:1 to 2.5:1; the mass fractions of the biopolymer dispersion and the anionic polysaccharide dispersion are 4% to 8% respectively; the dry basis mass ratio of the plant extract to be coated to the total dry basis mass of the biopolymer component and the anionic polysaccharide component is 1:2 to 1:5; and the mass ratio of the plant extract to be coated to the hydrophilic plant extract is 1:0.5 to 1:

3.

4. The method for preparing a multi-plant component facial mask composition according to claim 1, characterized in that, Step S2 includes: S2.1 Add the layered silicate adsorbent component to water, stir at 20-35℃ and let it stand to swell for 2-6 h to obtain a layered silicate dispersion; S2.2 Add the carbonaceous adsorption component and the coloring component to the layered silicate dispersion, and stir and disperse at 20-35℃ for 20-40 min to obtain the adsorption dispersion; S2.3 Add the drying and protection components to the plant active composite carrier dispersion, stir and dissolve at 5-20℃, then add the adsorption dispersion and mix to obtain the composite dispersion to be freeze-dried. S2.4 Pre-freeze the composite dispersion to be freeze-dried, and then freeze-dry it under vacuum for 18 to 30 hours at a cold trap temperature not higher than -60℃ and a chamber pressure of 3 to 15 Pa. Crush and sieve the freeze-dried material to obtain the composite adsorbent powder.

5. The method for preparing a multi-plant component facial mask composition according to claim 4, characterized in that, The layered silicate adsorption component includes at least one of bentonite, kaolin, and montmorillonite; the carbonaceous adsorption component includes at least one of carbon powder and activated carbon; the drying and protection component includes at least one of maltodextrin and trehalose; and the coloring component includes at least one of CI77266 and iron oxide black. Based on 100 parts by weight of the dry basis of the layered silicate adsorption component, the carbonaceous adsorption component is 10-50 parts by weight, the drying and protection component is 20-80 parts by weight, and the coloring component is 1-10 parts by weight. The mass fraction of the layered silicate adsorption component in water is 1%-5%.

6. The method for preparing a multi-plant component facial mask composition according to claim 4, characterized in that, Functional auxiliary components also include plant mucilage components; The preparation steps for plant mucilage components are as follows: Plant mucilage raw materials are added to an aqueous extraction medium and extracted at 40–60°C for 30–120 min to obtain plant mucilage extract. The plant mucilage raw materials include at least one of the flowers of the genus Althaea and the genus Hibiscus. The aqueous extraction medium includes at least one of water and aqueous ethanol. The plant mucilage extract was filtered or centrifuged to separate the solid and liquid phases, and the liquid phase was concentrated and the solid content was adjusted to 2% to 6% to obtain the plant mucilage component. Between step S2.1 and step S2.2, step S2 further includes: The plant mucilage component was added to the layered silicate dispersion and stirred at 20–35°C for 20–40 min to distribute the plant mucilage component at the hydration interface of the layered silicate particles. Based on 100 parts by weight of the dry basis of the layered silicate adsorbed component, the solids in the plant mucilage component were 1–10 parts by weight, and the mass ratio of the plant mucilage raw material to the aqueous extraction medium was 1:5–1:

20.

7. The method for preparing a multi-plant component facial mask composition according to claim 1, characterized in that, Step S3 includes: S3.

1. Add polyvinyl alcohol to water for hydration, stir at 80-90℃ until dissolved to obtain polyvinyl alcohol film-forming solution. Add acrylic (ester) crosslinking polymer to another part of water for dispersion and hydration, add alkaline regulator to neutralize, and obtain thickened and stable dispersion. S3.2 Cool the polyvinyl alcohol film-forming solution to no higher than 45°C, add the thickening and stabilizing dispersion, and add the moisturizing component, skin conditioning component and chelating component. Stir evenly to obtain the composite film-forming base material. S3.3 Cool the composite film-forming base material to no higher than 35°C, add the composite adsorption powder and stir to disperse, then add ethanol, preservative auxiliary components and fragrance components, and adjust the pH to 5.2-6.2 to obtain a multi-plant component film-forming slurry; S3.

4. The multi-plant component film-forming slurry is vacuum degassed at 20-30℃ for 10-30 min, allowed to stand and mature for 30-120 min, and then filled to obtain a multi-plant component facial mask composition.

8. The method for preparing a multi-plant component facial mask composition according to claim 7, characterized in that, The acrylate crosspolymer includes at least one of carbomer and acrylate / C10-30 alkanol acrylate crosspolymers; the alkalinity regulator includes at least one of sodium hydroxide and aminomethylpropanol; the moisturizing component includes at least two of glycerin, propylene glycol, and butylene glycol; the skin conditioning component includes at least one of allantoin and dipotassium glycyrrhizate; the chelating component includes at least one of disodium EDTA and sodium citrate; and the preservative auxiliary component includes methylparaben, 1,2-hexanediol, ethylhexylglycerin, capryloyl hydroxamic acid, phenoxyethanol, and p-hydroxypropyl hydroxypropyl ester. The composition contains at least two of the following: acetophenone; fragrance components include at least one of the following: fragrance and plant fragrance; and based on the total mass of the multi-plant component mask composition, the composition comprises: 8%–18% polyvinyl alcohol, 0.2%–1.0% acrylate cross-linked polymer, 5%–20% composite adsorbent powder, 3%–15% ethanol, 3%–12% moisturizing components, 0.1%–2% skin conditioning components, 0.05%–0.5% chelating components, 0.5%–1.0% preservative auxiliary components, 0.02%–0.10% fragrance components, and the balance being water.

9. The method for preparing a multi-plant component facial mask composition according to claim 7, characterized in that, Between step S3.2 and step S3.3, step S3 further includes: A film-forming polysaccharide component is added to a composite film-forming matrix and stirred and dispersed at 20–40°C to obtain a composite film-forming matrix containing film-forming polysaccharides. Subsequently, a sizing ion source and a slow-release stabilizing component are added and stirred continuously to allow the divalent metal ions released by the sizing ion source to undergo ionic cross-linking with the carboxyl groups in the film-forming polysaccharides. The film-forming polysaccharide component includes at least one of sodium alginate and sodium carboxymethyl cellulose; the shaping ion source includes at least one of calcium sulfate and calcium lactate; and the sustained-release stabilizing component includes at least one of tetrasodium pyrophosphate and sodium citrate. Based on 100 parts by mass of polyvinyl alcohol, the film-forming polysaccharide component comprises 5 to 30 parts by mass, the shaping ion source comprises 1 to 10 parts by mass, and the sustained-release stabilizing component comprises 0.5 to 5 parts by mass. The mass ratio of the film-forming polysaccharide component to the shaping ion source is 3:1 to 15:

1.

10. A multi-plant component facial mask composition, characterized in that, This is prepared by the method of any one of claims 1 to 9 for the preparation of a multi-plant component facial mask composition.