Soluble microneedle compositions and microneedle patches based on synergistic penetration enhancement mechanisms

By introducing charge neutralizing and barrier-regulating materials into soluble microneedle compositions, the problems of slow diffusion of macromolecular drugs in the skin and skin barrier damage are solved, achieving efficient transdermal delivery and dynamic ECM repair, improving drug efficacy and reducing the risk of inflammation.

CN123148203APending Publication Date: 2026-11-24CHENGDU BANGMAI MEDICAL CHUANG TECHNOLOGY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202510614823.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-14
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing soluble microneedle technology has difficulty effectively penetrating the skin's extracellular matrix (ECM), causing macromolecular drugs such as smegglutide and apapatide to remain in the epidermal layer of the skin, affecting the drug diffusion rate and bioavailability. At the same time, the use of hyaluronidase may lead to skin barrier damage and inflammation.

Method used

A soluble microneedle composition based on a synergistic permeation-enhancing mechanism is employed. By introducing charge-neutralizing and barrier-regulating materials, including extracellular matrix degrading enzymes, collagen-protecting materials, and osmotic pressure-driving materials, combined with hypertonic solutions and enzymatic factors, the diffusion of macromolecular drugs is promoted, and the structural integrity of the ECM is maintained by MMP inhibitors.

Benefits of technology

It improves the transdermal diffusion rate and bioavailability of macromolecular drugs, shortens the time to peak concentration, reduces skin barrier damage and inflammatory response, and maintains skin integrity and homeostasis.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The present application relates to the technical field of pharmaceutical preparations, and particularly relates to a soluble microneedle composition and a microneedle patch based on a synergistic penetration mechanism, wherein the soluble microneedle composition comprises the following raw materials: 1-10% of a macromolecular drug, 30-55% of a polymer matrix material, 1-5% of a charge neutralization material, 0.1-15% of a barrier regulation material, and 1-5% of an additive, and the barrier regulation material is selected from at least one of an extracellular matrix degradation enzyme / collagen protection composition, an extracellular matrix regeneration promoting material, and an osmotic pressure driving material. The microneedle patch of the present application promotes the penetration and release of a polypeptide or protein macromolecular drug in the intradermis based on a synergistic mechanism of charge neutralization and barrier regulation, solves the problems of low bioavailability and slow peak blood concentration of polypeptide, protein and other macromolecular drugs in the prior art when the drugs are delivered transdermally by microneedles, improves the drug efficacy, avoids secondary damage caused by the penetration mechanism by timely repairing ECM, maintains the integrity of the skin barrier, and avoids inflammation and infection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of pharmaceutical formulation technology, and in particular to soluble microneedle compositions and microneedle patches based on a synergistic permeation-enhancing mechanism. Background Technology

[0002] Soluble microneedle technology, as a novel transdermal drug delivery technology, involves inserting microneedles into the skin to open channels, allowing active ingredients to directly enter the body and exert their effects. This not only improves the infection and pain caused by injection, but also avoids the first-pass effect of the gastrointestinal tract and reduces adverse gastrointestinal reactions. It has advantages such as being painless, highly effective, and easy to operate.

[0003] Soluble microneedles primarily use macromolecular polymers as their framework. When the microneedle enters the skin, the macromolecular material swells and dissolves, allowing the loaded drug to diffuse slowly. While the diffusion of ordinary small-molecule drugs is barely sufficient for skin administration, when the drug is a macromolecular drug such as a protein or peptide, the drug itself has a large molecular weight, resulting in slow diffusion for local delivery. Furthermore, peptides or proteins typically carry a certain electrical charge, making them prone to binding to the epidermis or subcutaneous tissue and thus trapped, hindering diffusion into the bloodstream. This leads to low blood drug concentrations and a long time to peak concentration, thereby affecting the actual therapeutic effect.

[0004] Because the extracellular matrix (ECM) of the skin is a complex macromolecular network, with collagen, hyaluronic acid, and other components forming a dense network, it restricts the free diffusion of macromolecules. Large molecular weight drugs such as semaglutide (approximately 4.1 kDa) cannot completely overcome the physical barrier of the ECM and tend to remain in the epidermis or superficial dermis. Chinese patent CN114470170A discloses a semaglutide-soluble microneedle composition and its preparation method. The soluble microneedle composition includes a needle material and a base material; the needle material includes semaglutide, hyaluronidase, a polymer backbone material, and a pH adjuster, wherein the mass ratio of semaglutide to hyaluronidase is (1-30):1. Hyaluronic acid is a major component of the extracellular matrix of the skin and has high viscoelasticity, which can restrict the diffusion of macromolecules (such as semaglutide). Hyaluronidase breaks down the physical barrier formed by hyaluronic acid (HA) in the extracellular matrix of skin cells, thereby widening the intercellular spaces, promoting drug penetration into the bloodstream, and reducing obstacles to drug diffusion. The soluble microneedle composition of the aforementioned patent combines semaglutide and hyaluronidase, solving the problem that existing semaglutide microneedles are difficult to penetrate into the bloodstream due to the large molecular weight of semaglutide, thus remaining within the epidermal layer.

[0005] However, hyaluronic acid is an important component of the skin barrier, involved in maintaining skin hydration, elasticity, and intercellular signaling. The degradation of hyaluronic acid can lead to temporary dryness or sensitivity. Although the regeneration cycle of hyaluronic acid is relatively short (approximately 24-48 hours), normal skin can recover through its own metabolism. However, frequent use of medications like apapatide, which require daily application, may disrupt skin homeostasis, leading to chronic inflammation or weakened barrier function. Summary of the Invention

[0006] In view of this, the purpose of the present invention is to provide a soluble microneedle composition and microneedle patch based on a synergistic penetration enhancement mechanism, so as to improve drug efficacy while maintaining the integrity of the skin barrier by timely repairing the ECM and avoiding inflammation and infection.

[0007] The present invention solves the above-mentioned technical problems through the following technical means:

[0008] In a first aspect, embodiments of this application provide a soluble microneedle composition based on a synergistic penetration-enhancing mechanism, comprising the following raw materials by mass fraction:

[0009] Macromolecular drugs 1-10%

[0010] Polymer skeleton material 30-55%

[0011] Charge neutralizing materials 1-5%

[0012] Barrier regulation materials 0.1–15%

[0013] Additives 1-5%

[0014] The soluble microneedle composition further includes a solvent, and the total mass fraction of the macromolecular drug, polymer backbone material, charge neutralizing material, barrier regulating material, additives and solvent is 100%.

[0015] The barrier regulation material is selected from at least one of the following: extracellular matrix degrading enzyme / collagen protection composition, extracellular matrix regeneration promoting material, and osmotic pressure driving material.

[0016] In conjunction with the first aspect, in some embodiments, the barrier regulating material is composed of an extracellular matrix degrading enzyme / collagen protective composition and an extracellular matrix regeneration promoting material, wherein the mass ratio of the extracellular matrix degrading enzyme / collagen protective composition to the extracellular matrix regeneration promoting material is 1:(0.5-2);

[0017] Alternatively, the barrier regulating material is composed of an extracellular matrix degrading enzyme / collagen protective composition and an osmotic pressure driving material, wherein the mass ratio of the extracellular matrix degrading enzyme / collagen protective composition to the osmotic pressure driving material is 1:(1-20);

[0018] Alternatively, the barrier regulating material may be composed of an extracellular matrix degrading enzyme / collagen protective composition, an extracellular matrix regeneration promoting material, and an osmotic pressure driving material, wherein the mass ratio of the extracellular matrix degrading enzyme / collagen protective composition, the extracellular matrix regeneration promoting material, and the osmotic pressure driving material is 1:(0.5-2):(1-20).

[0019] In conjunction with the first aspect, in some embodiments, the extracellular matrix degrading enzyme / collagen protective composition comprises an extracellular matrix degrading enzyme and a collagen protective material in a mass ratio of 1:(2-5), wherein the extracellular matrix degrading enzyme is selected from at least one of hyaluronidase, collagenase, elastase, trypsin, deoxyribonuclease, and lipase, and the collagen protective material is selected from at least one of tissue metalloproteinase inhibitor-1, polyethylene glycol-modified tissue metalloproteinase inhibitor-1, MMP inhibitor, vitamin C, α-tocopherol, genipin cross-linked collagen, aminoguanidine, epigallocatechin gallate, arbutin, ferulic acid, quercetin, and doxycycline.

[0020] In conjunction with the first aspect, in some embodiments, the extracellular matrix regeneration promoting material is selected from at least one of N-acetylglucosamine, hyaluronic acid oligosaccharide, transforming growth factor-β, fibroblast growth factor, epidermal growth factor, vascular endothelial growth factor, dipotassium glycyrrhizate, asiaticoside, ginsenoside Rb1, methacrylamide HA, and copper peptide.

[0021] In conjunction with the first aspect, in some embodiments, the osmotic pressure driving material is selected from at least one of sorbitol, mannitol, sodium chloride, magnesium sulfate, propylene glycol, polyethylene glycol, glycine, arginine, and poloxamer.

[0022] In conjunction with the first aspect, in some embodiments, the mass ratio of the macromolecular drug to the charge neutralizing material is 1:(0.5-5), and the charge neutralizing material is selected from at least one of chitosan, polylysine, ε-polylysine, lactoferrin, dopamine-modified cationic polymer, cationic collagen hydrolysate, linear PEI, DOTAP liposomes, poly-β-amino ester, polyarginine, PAMAM low-generation dendritic molecule, cationic cyclodextrin, lecithin, phosphatidylserine, betain, polyacrylic acid, sodium alginate, chondroitin sulfate, polyglutamic acid, phosphatidylcholine, carbomer, polyvinyl alcohol-polyacrylic acid copolymer, and carboxymethyl cellulose.

[0023] In conjunction with the first aspect, in some embodiments, the macromolecular drug is selected from one of peptides, proteins, antibodies, polysaccharides, and nucleic acid drugs.

[0024] In conjunction with the first aspect, in some embodiments, the additive includes a stabilizer and a pH adjuster. The stabilizer is selected from at least one of trehalose, sucrose, glucose, dextran, sulfobutyl ether-β-cyclodextrin, hydroxypropyl cellulose, carboxymethyl cellulose, xanthan gum, polysorbate 80, and glycerol. The pH adjuster is selected from at least one of sodium citrate, Tris buffer, arginine, histidine / hydrochloric acid, glucosamine, potassium bicarbonate, potassium dihydrogen phosphate / dipotassium hydrogen phosphate, NH4HCO3 / NH3, potassium citrate / citric acid, and citric acid / arginine. The solvent is selected from at least one of deionized water, acetic acid solution, phosphoric acid solution, and anhydrous ethanol.

[0025] Secondly, embodiments of this application also provide a microneedle patch, including a substrate and a needle formed on the substrate, the needle being made of the soluble microneedle composition as described above.

[0026] In conjunction with the second aspect, in some embodiments, the material of the substrate is selected from at least one of hyaluronic acid or its sodium salt, polyvinyl alcohol, polyvinylpyrrolidone, hydroxypropyl methylcellulose, sodium carboxymethyl cellulose, gelatin, dextran, sodium alginate, silk fibroin, biodegradable polylactic acid, polycaprolactone, polylactic-glycolic acid copolymer, polyaspartic acid, lactoferrin, carbomer, hydroxypropyl chitosan, elastin peptide, polylactic-glycolic acid copolymer / polyethylene glycol / polyvinyl alcohol, polyester, polyethersulfone, polypropylene, polyimide, polyethylene naphthalate, polyurethane, polydimethylsiloxane, thermoplastic polyurethane, polytetrafluoroethylene, polycarbonate, poly(lactic-glycolic acid), poly(glycolic acid), poly-L-lactide, polystyrene-block-poly(ethylene-cyclobutene)-block-polystyrene, silicone, paper, medical nonwoven fabric, and textile materials.

[0027] The soluble microneedle composition of this invention, based on a synergistic penetration-enhancing mechanism, involves charge neutralization and barrier regulation mechanisms during its use as a microneedle patch. Specifically, the charge neutralization mechanism is as follows: The extracellular matrix (ECM) and stratum corneum of the skin contain a large number of negatively charged groups (such as chondroitin sulfate, hyaluronic acid, and phospholipids), which repel negatively charged macromolecules (such as semaglutide), forming an "electrostatic barrier" and reducing penetration. This invention introduces a cationic charge neutralizer to form a complex or surface coating with semaglutide, shielding its inherent negative charge and reducing its repulsion to negatively charged sites in skin tissue. Similarly, for positively charged macromolecules (such as apapatide), upon contact with the skin's ECM (negatively charged), they bind tightly due to charge attraction, easily confining them to the epidermal-dermal junction, reducing the deep diffusion rate and increasing the risk of local degradation. By introducing an anionic charge neutralizer, the positive charge of abapapeptide is partially shielded by forming an abapapeptide-anionic complex (electrostatic complex or complex micelles), reducing its affinity for the negative charge of the ECM, decreasing surface binding, and promoting drug diffusion into the dermis and around capillaries.

[0028] The soluble microneedle composition of this invention releases macromolecular drugs upon entering the skin due to changes in skin pH (7.4) / ionic strength or protein dissociation. The charge-neutralizing material and the macromolecular drug complex are weakly positive / electroneutral, facilitating passage through the intercellular lipid bilayer and increasing lipophilicity; reducing binding to skin anionic sites and preventing drug "stuck" in the superficial epidermis. The soluble microneedle composition containing charge-neutralizing materials can protect the smegglutinin structure, preventing its degradation due to proteases or oxidative stress in the epidermis. Some charge-neutralizing materials (such as lactoferrin and PAMAM) have antioxidant / anti-inflammatory effects, further reducing skin barrier reactions. After entering the dermis, the soluble microneedle composition releases macromolecular drugs due to changes in environmental pH and ionic strength (e.g., Na+). + Ca 2+ Increased plasma concentration triggers charge imbalance, causing the soluble microneedle composition to dissociate and release smegglutinin, which then penetrates into the capillary network or lymphatic system.

[0029] The barrier regulation mechanism is as follows:

[0030] (I) Osmotic pressure-driven temporary ECM regulation mechanism

[0031] On one hand, this invention introduces osmotic pressure-driven materials such as sorbitol, mannitol, sodium chloride, magnesium sulfate, propylene glycol, polyethylene glycol, glycine, arginine, and poloxamer to locally apply a hypertonic solution, inducing skin cells (such as keratinocytes and fibroblasts) to dehydrate and shrink, thereby expanding the intercellular space and reducing ECM density, and enhancing drug diffusion efficiency. The specific steps are as follows:

[0032] (1) Formation of hyperosmotic environment: Osmotic pressure drives the material to form a high osmotic pressure gradient in the skin, resulting in an imbalance of osmotic pressure inside and outside the cells;

[0033] (2) Cell dehydration and shrinkage: Water flows out of the cell, the cell volume shrinks, and the intercellular connections (such as tight junctions and desmosomes) temporarily loosen;

[0034] (3) ECM gap expansion: After cell contraction, the gap between dermal fibroblasts increases, and the porosity of the collagen / HA network increases (pore size increases from 20nm to 50-100nm);

[0035] (4) Enhanced drug diffusion: The enlarged gap provides diffusion channels for macromolecules such as smegglutinin (4.1kDa), reducing retention in the dermis.

[0036] The osmotic pressure-driven material of this invention is reversible and non-invasive in use. Reversible means that after the osmotic pressure-driven material is removed, the cells reabsorb water and return to their original state (approximately 1-2 hours). Non-invasive means that it does not damage the cell membrane or ECM structure, thus having a high degree of safety.

[0037] (II) ECM Dynamic Regulation Mechanism

[0038] The extracellular matrix (ECM) of the epidermis and superficial dermis mainly includes hyaluronic acid (HA), collagen, elastin, DNA / nucleic acid residues, and lipid barrier components. This invention introduces materials such as hyaluronidase, collagenase, elastase, trypsin, deoxyribonuclease, and lipase to selectively degrade key components of the ECM, thereby breaking the natural barrier structure and providing a more unobstructed diffusion and penetration channel for drug molecules.

[0039] Hyaluronidase specifically degrades HA (rather than collagen or elastin), a major hydrated macromolecule in the ECM. Its degradation significantly increases the ECM pore size (from 20 nm to 100 nm), promoting the diffusion of macromolecular drugs. While HA clearance does not directly disrupt the collagen fiber or elastin network, HA degradation triggers secondary reactions such as inflammatory signal activation and upregulation of matrix metalloproteinase (MMP) expression. Low-molecular-weight fragments produced by HA degradation (such as oligo-HA) can activate keratinocytes and fibroblasts via CD44 receptors or TLR-4, triggering the release of inflammatory factors (such as IL-6 and TNF-α). These inflammatory factors stimulate fibroblasts to secrete MMPs (such as MMP-3 and MMP-9), which degrade collagen (types I / III) and elastin, leading to ECM structural damage. Damage to the collagen network results in weakened skin barrier function (risk of erythema and edema); ECM collapse, in turn, hinders sustained drug diffusion (due to excessively large pores and loss of directionality). This invention introduces collagen-protective materials such as MMP inhibitors to suppress MMP activity, thereby maintaining the integrity of collagen fibers in the ECM and preventing skin barrier damage. The combined use of hyaluronidase and collagen-protective materials allows hyaluronidase to target and clear HA, opening physical diffusion channels; the MMP inhibitors suppress MMP overactivation caused by HA degradation, protecting the collagen / elastin network. While expanding the pore size of the ECM, this invention maintains the structural stability of the ECM, avoiding the contradiction of "channel expansion but structural collapse"; it also reduces inflammatory responses and lowers skin irritation.

[0040] Furthermore, long-term and frequent HA deficiency may lead to decreased skin hydration (dryness, flaking), loosened ECM structure, weakened barrier function, and the accumulation of low molecular weight HA fragments may trigger inflammation (via TLR-4 / CD44 signaling). The introduction of cross-linked hyaluronic acid, peptide-based ECM repair factors (such as collagen peptides and elastin peptides), human-like collagen, epidermal growth factor (EGF), basic fibroblast growth factor (bFGF), and anti-inflammatory factors (such as lactoferrin and PAMAM-G3) to achieve dynamic balance regulation enhances permeability while promptly repairing the ECM structure, preventing barrier function loss, reducing inflammatory responses and tissue damage, and maintaining tissue homeostasis. Simultaneously, a time-sequential release mechanism is introduced, employing a control strategy of rapid release of enzymatic hydrolysis factors (immediate activation upon skin puncture) and delayed / continuous release of repair factors (delayed intervention after enzymatic hydrolysis) to prevent premature clearance of repair factors during the peak of enzymatic activity, ensuring a dynamic balance between ECM degradation and regeneration.

[0041] The "charge neutralization + barrier regulation" synergistic mechanism of this invention can improve the diffusion rate and penetration of macromolecular drugs in skin tissue, increase the amount of drug entering the bloodstream per unit time, shorten the time to peak drug concentration, and improve drug efficacy. While enhancing efficacy, it also prevents secondary damage caused by excessive activation of hyaluronidase / collagenase by timely repairing the ECM; reduces the upregulation of matrix-degrading enzymes such as MMPs, thus reducing further ECM damage; and maintains the integrity of the skin barrier, preventing inflammation and infection. pH adjusters can promote the solubility of macromolecular drugs in water and ensure a constant pH range, improving drug stability and bioactivity. Stabilizers ensure the stereostructural stability of the drug during the drying process, thereby ensuring its activity. Specific types of polymer backbone materials enhance the mechanical strength of the microneedles, ensuring effective penetration into the skin and rapid dissolution to release the drug after opening the skin's drug delivery channels.

[0042] The microneedle patch of this invention promotes the penetration and release of large molecular drugs such as peptides or proteins into the skin through a synergistic mechanism of "charge neutralization + barrier regulation," solving the problems of low bioavailability and slow peak blood concentration in existing technologies for transdermal delivery of large molecular drugs such as peptides and proteins using microneedles. While improving efficacy, it also promptly repairs the ECM, avoiding secondary damage caused by the penetration-enhancing mechanism, maintaining the integrity of the skin barrier, and preventing inflammation and infection. Detailed Implementation

[0043] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions in the embodiments of this application will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0044] In the embodiments of this application, the terms "exemplary" or "for example" are used to indicate that something is an example, illustration, or description. Any embodiment or design that is described as "exemplary" or "for example" in the embodiments of this application should not be construed as being more preferred or advantageous than other embodiments or designs. Specifically, the use of the terms "exemplary" or "for example" is intended to present the relevant concepts in a specific manner.

[0045] The soluble microneedle composition based on a synergistic permeation-enhancing mechanism of this application comprises the following raw materials in the following mass fractions: 1-10% macromolecular drug, 30-55% polymer backbone material, 1-5% charge neutralizing material, 0.1-15% barrier regulating material, and 1-5% additives. The soluble microneedle composition also includes a solvent. The total mass fraction of the macromolecular drug, polymer backbone material, charge neutralizing material, barrier regulating material, additives, and solvent is 100%. The barrier regulating material is selected from at least one of extracellular matrix degrading enzyme / collagen protective composition, extracellular matrix regeneration promoting material, and osmotic pressure driving material.

[0046] In some embodiments, the barrier regulation material is composed of an extracellular matrix degrading enzyme / collagen protective composition and an extracellular matrix regeneration promoting material, wherein the mass ratio of the extracellular matrix degrading enzyme / collagen protective composition to the extracellular matrix regeneration promoting material is 1:(0.5-2).

[0047] In other embodiments, the barrier regulating material consists of an extracellular matrix degrading enzyme / collagen protective composition and an osmotic pressure driving material, wherein the mass ratio of the extracellular matrix degrading enzyme / collagen protective composition to the osmotic pressure driving material is 1:(1-20).

[0048] In other embodiments, the barrier regulating material is composed of an extracellular matrix degrading enzyme / collagen protective composition, an extracellular matrix regeneration promoting material, and an osmotic pressure driving material, wherein the mass ratio of the extracellular matrix degrading enzyme / collagen protective composition, the extracellular matrix regeneration promoting material, and the osmotic pressure driving material is 1:(0.5-2):(1-20).

[0049] In some embodiments, the extracellular matrix degrading enzyme / collagen protective composition comprises an extracellular matrix degrading enzyme and a collagen protective material in a mass ratio of 1:(2-5). The extracellular matrix degrading enzyme is selected from at least one of hyaluronidase, collagenase, elastase, trypsin, deoxyribonuclease, and lipase. The collagen protective material is selected from at least one of tissue metalloproteinase inhibitor-1 (TIMP-1), polyethylene glycol-modified tissue metalloproteinase inhibitor-1 (PEG-TIMP-1), chemically synthesized MMP inhibitors (such as Marimastat), vitamin C, α-tocopherol, genipin cross-linked collagen, aminoguanidine, epigallocatechin gallate, arbutin, ferulic acid, quercetin, and doxycycline.

[0050] In some embodiments, the extracellular matrix regeneration promoting material is selected from at least one of N-acetylglucosamine (GlcNAc), hyaluronic acid oligosaccharide (HAOligos), transforming growth factor-β (TGF-β), fibroblast growth factor (FGF-2), epidermal growth factor (EGF), vascular endothelial growth factor, dipotassium glycyrrhizate, GlcNAc, TGF-β, Asiaticoside, ginsenoside Rb1, methacrylamide HA (MethHA), and copper peptide (GHK-Cu).

[0051] In some embodiments, the osmotic pressure driving material is selected from at least one of sorbitol, mannitol, sodium chloride, magnesium sulfate, propylene glycol, polyethylene glycol, glycine, arginine, and poloxamer.

[0052] In some embodiments, the mass ratio of the macromolecular drug to the charge neutralizing material is 1:(0.5-5), and the charge neutralizing material is selected from at least one of chitosan (degree of deacetylation ≥85%), polylysine (molecular weight <10kDa), ε-polylysine, lactoferrin, dopamine-modified cationic polymer, cationic collagen hydrolysate, linear PEI (low molecular weight), DOTAP liposomes (PEG modified), polyβ-amino ester, polyarginine, PAMAM low-generation dendritic molecule (G3), cationic cyclodextrin (HP-β-CD-N+), lecithin, phosphatidylserine, betain, polyacrylic acid, sodium alginate, chondroitin sulfate, polyglutamic acid, phosphatidylcholine, carbomer, polyvinyl alcohol-polyacrylic acid (PVA-PAA) copolymer, and carboxymethyl cellulose.

[0053] In some embodiments, the macromolecular drug is selected from one of the following: peptides, proteins, antibodies, polysaccharides, and nucleic acid drugs, such as smegglutide and apapatide.

[0054] In some embodiments, the additives include stabilizers and pH adjusters. The stabilizers are selected from at least one of trehalose, sucrose, glucose, dextran, sulfobutyl ether-β-cyclodextrin, hydroxypropyl cellulose, carboxymethyl cellulose, xanthan gum, polysorbate 80, and glycerol. The pH adjusters are selected from at least one of sodium citrate, Tris buffer, arginine, histidine / hydrochloric acid, glucosamine, potassium bicarbonate, potassium dihydrogen phosphate / dipoctyl hydrogen phosphate, NH4HCO3 / NH3, potassium citrate / citric acid, and citric acid / arginine. The solvent is selected from at least one of deionized water, acetic acid solution, phosphoric acid solution, and anhydrous ethanol.

[0055] This application also discloses a microneedle patch, comprising a substrate and needles formed on the substrate, the needles being made of the soluble microneedle composition described above. The substrate is selected from at least one of the following: hyaluronic acid or its sodium salt, polyvinyl alcohol, polyvinylpyrrolidone, hydroxypropyl methylcellulose, sodium carboxymethyl cellulose, gelatin, dextran, sodium alginate, silk fibroin, biodegradable polylactic acid, polycaprolactone, polylactic-glycolic acid copolymer, polyaspartic acid, lactoferrin, carbomer, hydroxypropyl chitosan, elastin peptide, polylactic-glycolic acid copolymer / polyethylene glycol / polyvinyl alcohol, polyester, polyethersulfone, polypropylene, polyimide, polyethylene naphthalate, polyurethane, polydimethylsiloxane, thermoplastic polyurethane, polytetrafluoroethylene, polycarbonate, poly(lactic-glycolic acid), poly(glycolic acid), poly-L-lactide, polystyrene-block-poly(ethylene-cyclobutene)-block-polystyrene, silicone, paper, medical nonwoven fabric, and textile materials.

[0056] In this application, the barrier regulating material can be uniformly mixed in a soluble microneedle composition to form a needle, or the needle can be first prepared by using macromolecular drugs, polymer backbone materials, charge neutralizing materials and additives to form a needle, and then the barrier regulating material can be coated on the surface of the formed needle.

[0057] In some embodiments, when a barrier-regulating material is uniformly mixed in a soluble microneedle composition to form a needle, the method for preparing a microneedle patch includes the following steps:

[0058] S1. Dissolve the macromolecular drug in a solution containing stabilizers and pH adjusters, then add charge neutralizing materials and barrier regulating materials, stir and mix to form a homogeneous solution, then add polymer backbone materials, stir and mix evenly to obtain the needle solution;

[0059] S2. Take an appropriate amount of needle solution, inject it into the microneedle negative mold, spread it evenly, centrifuge, and remove the excess needle solution from the surface of the microneedle negative mold.

[0060] S3. After drying the microneedle negative mold containing the needle body solution, take an appropriate amount of base material and place it in the dried microneedle negative mold, spread it evenly, centrifuge, dry, and demold to obtain the microneedle patch.

[0061] Alternatively, step S3 can also involve placing the finished substrate (such as medical nonwoven fabric) into the microneedle mold that has not been dried in step S2, drying it, demolding it, and obtaining the microneedle patch.

[0062] In some embodiments, when a barrier-regulating material is coated on the surface of the needle, the method for preparing the microneedle patch includes the following steps:

[0063] (1) Dissolve the macromolecular drug in a solution containing stabilizer and pH adjuster, then add charge neutralizing material, stir and mix to form a homogeneous solution, then add polymer skeleton material, stir and mix evenly to obtain the needle solution.

[0064] (2) Take an appropriate amount of needle solution, inject it into the microneedle negative mold, spread it evenly, centrifuge, and remove the excess needle solution from the surface of the microneedle negative mold.

[0065] (3) After the microneedle negative mold containing the needle body solution is dried, take an appropriate amount of base material and place it in the dried microneedle negative mold, spread it evenly, centrifuge, dry, and demold.

[0066] Alternatively, step (3) can also be to place the finished substrate (such as medical nonwoven fabric) in the microneedle mold that has not been dried in step (2), dry it, and demold it.

[0067] (4) The microsphere-shaped barrier control material is uniformly sprayed onto the outer layer of the needle using a spraying method and dried to obtain the microneedle patch.

[0068] To better understand the above technical solutions, the following will provide a detailed explanation of the specific implementation methods described in the specification.

[0069] Example 1

[0070] This embodiment verifies the protective effect of TIMP-1 inhibitors on the ECM in a microneedle delivery system, evaluates their efficacy and safety in reducing collagen degradation, and clarifies the necessity of introducing MMP inhibitors. Details are as follows:

[0071] (1) Experimental Design

[0072] (A) Group Design

[0073] Control group: Contains only hyaluronidase (HAase, 50 U / mL), without TIMP-1;

[0074] Experimental group: HAase (50 U / mL) + TIMP-1 (0.2 mg / mL);

[0075] Blank group: No HAase and TIMP-1 (only charge neutralizer and framework material).

[0076] (B) Drugs and Materials

[0077] Macromolecular drug: Smegglutide (1 mg / mL);

[0078] Charge neutralizing material: glycine, with a molar ratio of glycine to smegglutinin of 6:1;

[0079] Polymer backbone material: polylactic acid-glycolic acid copolymer (50% w / w), wherein the molar ratio of lactic acid to glycolic acid is 50:50;

[0080] Stabilizer: Trehalose (5% w / w);

[0081] pH adjuster: Histidine buffer (pH 5.0);

[0082] Substrate: Sodium hyaluronate (8% w / w).

[0083] (2) Experimental methods

[0084] ① Preparation of microneedle patches in the experimental group

[0085] Trehalose was added to deionized water, and the pH was adjusted to 5.0 with histidine buffer to obtain an additive solution. Smegglutinin was dissolved in the additive solution, and then hyaluronidase and TIMP-1 were added. The mixture was stirred and mixed to form a homogeneous solution. Polylactic acid-glycolic acid copolymer was then added and stirred until homogeneous. After vacuum degassing, a needle solution was obtained. An appropriate amount of needle solution was injected into a microneedle PDMS mold, coated evenly, centrifuged, and excess needle solution was removed from the surface of the microneedle negative mold. The microneedle PDMS mold containing the needle solution was freeze-dried (-40℃, 24h). Sodium hyaluronate was then coated onto the dried microneedle PDMS mold, coated evenly, centrifuged, dried, and demolded to obtain a microneedle patch.

[0086] ② Preparation of control group microneedle patches

[0087] The only difference between the control group and the experimental group was that the control group did not have IMP-1 added; the rest of the steps were exactly the same as those of the experimental group.

[0088] ③ Preparation of blank group microneedle patches

[0089] The only difference between the blank control group and the experimental group is that the blank control group did not contain hyaluronidase and TIMP-1; the rest of the steps were exactly the same as those of the experimental group.

[0090] (3) In vitro experiments (pig ear skin model)

[0091] (I) HA and collagen degradation detection: HA content was detected by ELISA 6 hours after microneedle patch application, and collagen density was quantified by Masson staining.

[0092] (II) Transdermal efficiency: The cumulative release rate of smegglutinin and transdermal flow rate were determined using a Franz diffusion cell.

[0093] (4) In vivo experiments (SD rats, n=6)

[0094] (I) Pharmacokinetics: After microneedle application, blood drug concentration was detected by ELISA (0-24h), and AUC and bioavailability were calculated.

[0095] (II) Skin safety: Draize score (0-4 points), HE staining to observe inflammatory cell infiltration.

[0096] (III) ECM regeneration: Immunohistochemical detection of HA and type I collagen expression 24 hours after application.

[0097] (5) Experimental Results

[0098] Please refer to Table 1 for data on the protective effect of extracorporeal ECM:

[0099]

[0100] Table 1

[0101] The data in Table 1 show that HAase significantly degraded HA (68.3%), but TIMP-1 did not affect the HA degradation efficiency (65.1% vs 68.3%). The collagen retention rate in the control group was only 54.7%, while that in the experimental group increased to 85.6%, proving that TIMP-1 effectively inhibited MMP activity and protected collagen.

[0102] Please refer to Table 2 for in vivo pharmacokinetic and safety data:

[0103]

[0104]

[0105] Table 2

[0106] The data in Table 2 show that the transdermal efficiency of the experimental group and the control group was similar (AUC 238.9 vs 240.6), and TIMP-1 did not affect drug release. The control group suffered from inflammation due to excessive collagen degradation (IL-6↑, Draize score 2.8), while the experimental group showed significant improvement (IL-6↓45%, Draize score 1.5).

[0107] Please refer to Table 3 for relevant data on ECM regeneration capacity:

[0108] index Experimental group (HAase + TIMP-1) Control group (HAase) HA regeneration rate (24h, %) 82.3±4.1 58.4±3.7 Collagen regeneration rate (24h, %) 88.9±3.8 61.2±4.5

[0109] Table 3

[0110] The data in Table 3 show that Masson staining in the control group revealed broken and disordered collagen fibers, while the experimental group showed intact collagen structure and uniform HA distribution.

[0111] The data in Tables 1-3 indicate that while HAase effectively degrades HA and improves transdermal efficiency, it activates MMPs, leading to excessive collagen degradation (retention rate of only 54.7%). TIMP-1 inhibits MMP activity, increasing collagen retention to 85.6% without interfering with the penetration-enhancing effect of HAase. TIMP-1 significantly reduces the inflammatory response (IL-6 ↓ 45%), lowers the Draize score from 2.8 to 1.5, promotes ECM regeneration (HA and collagen regeneration rates > 80%), and maintains skin barrier integrity. Introducing MMP inhibitors (such as TIMP-1) can balance enzymatic penetration enhancement and ECM protection, avoiding the risk of skin damage from long-term medication.

[0112] Example 2

[0113] This embodiment verifies the promoting effect of ECM regeneration promoting material on HA and collagen regeneration in a microneedle delivery system, evaluates its safety, and clarifies the necessity of introducing regenerative materials.

[0114] (1) Experimental Design

[0115] (A) Group Design

[0116] Control group: Contains only hyaluronidase (HAase, 50 U / mL) and charge neutralizer (glycine), without regeneration promoter;

[0117] Experimental group: HAase (50 U / mL) + glycine + N-acetylglucosamine (GlcNAc, 5% w / w) + transforming growth factor-β (TGF-β, 1 ng / mL) + cross-linked HA microspheres (10% w / w);

[0118] Blank group: No HAase and regeneration accelerator (only charge neutralizer and framework material).

[0119] (B) Drugs and Materials

[0120] Macromolecular drug: Smegglutide (1 mg / mL);

[0121] Charge neutralizing material: glycine, with a molar ratio of glycine to smegglutinin of 6:1;

[0122] Polymer backbone material: Polyvinyl alcohol (PVA, 15% w / w);

[0123] Stabilizer: Mannitol (4% w / w);

[0124] pH adjuster: Histidine buffer (pH 5.0);

[0125] Substrate: Sodium hyaluronate (8% w / w).

[0126] (2) Experimental methods

[0127] ① Preparation of microneedle patches in the experimental group

[0128] Mannitol was added to deionized water, and the pH was adjusted to 5.0 with histidine buffer to obtain an additive solution. Smegglutinin was dissolved in the additive solution, and then hyaluronidase, GlcNAc, TGF-β and cross-linked HA microspheres were added. The mixture was stirred and mixed to form a homogeneous solution. Polyvinyl alcohol was then added and stirred until homogeneous. After vacuum degassing, the needle solution was obtained. An appropriate amount of the needle solution was injected into a microneedle PDMS mold, coated evenly, centrifuged, and excess needle solution was removed from the surface of the microneedle negative mold. The microneedle PDMS mold containing the needle solution was freeze-dried (-40℃, 24h). Sodium hyaluronate was then coated onto the dried microneedle PDMS mold, coated evenly, centrifuged, dried, and demolded to obtain a microneedle patch.

[0129] ② Preparation of control group microneedle patches

[0130] The only difference between the control group and the experimental group was that the control group did not contain GlcNAc, TGF-β and cross-linked HA microspheres; the rest of the steps were exactly the same as those in the experimental group.

[0131] ③ Preparation of blank group microneedle patches

[0132] The only difference between the blank group and the experimental group is that the blank group did not contain hyaluronidase, GlcNAc, TGF-β and cross-linked HA microspheres; the rest of the steps were exactly the same as those of the experimental group.

[0133] (3) In vitro experiments (pig ear skin model)

[0134] (I) HA and collagen degradation detection: HA content was detected by ELISA 24 hours after microneedle patch application, and collagen density was quantified by Sirius red staining.

[0135] (II) Transdermal efficiency: The cumulative release rate of smegglutinin and transdermal flow rate were determined using a Franz diffusion cell.

[0136] (4) In vivo experiments (SD rats, n=6)

[0137] (I) Pharmacokinetics: After microneedle application, blood drug concentration was detected by ELISA (0-24h), and AUC and bioavailability were calculated.

[0138] (II) Skin safety: Draize score (0-4 points), HE staining to observe inflammatory cell infiltration, and detection of IL-6 and TNF-α levels.

[0139] (III) ECM regeneration: Immunohistochemical detection of HA and type I collagen expression 72 hours after application.

[0140] (5) Experimental Results

[0141] Please refer to Table 4 for data on the protective effect of in vitro ECM:

[0142] index Blank group Control group (HAase) Experimental group (regeneration accelerator) HA regeneration rate (%) 8.3±1.2 32.5±3.1 84.7±4.3 Collagen density (μg / mg) 85.6±4.2 58.3±3.8 92.1±4.5 <![CDATA[Transdermal flux (μg / cm 2 / h)]]> 0.6±0.1 2.4±0.3 3.8±0.4

[0143] Table 4

[0144] The data in Table 4 show that the HA regeneration rate in the control group was only 32.5%, while that in the experimental group it increased to 84.7%, indicating that GlcNAc and TGF-β significantly promoted HA synthesis. The collagen density in the experimental group recovered to 92.1 μg / mg (close to the blank group's 85.6 μg / mg), proving that the cross-linked HA microspheres guided the orderly regeneration.

[0145] Please refer to Table 5 for in vivo pharmacokinetic and safety data:

[0146] index Blank group Control group (HAase) Experimental group (regeneration accelerator) AUC0-24h (ng·h / mL) 98.5±8.7 245.6±15.3 498.3±24.1 Bioavailability (%) 18.2±1.6 45.3±2.8 61.5±3.2 Draize rating 1.0 (Non-irritating) 2.5 (Moderate erythema) 1.2 (Mild erythema) IL-6 (pg / mL) 15.2±2.3 48.6±5.1 22.4±3.5

[0147] Table 5

[0148] The data in Table 5 show that the bioavailability of the experimental group was 61.5%, which was significantly higher than that of the control group (45.3%). The regeneration promoter maintained continuous permeation channels by repairing the ECM. The inflammatory factor IL-6 in the experimental group decreased by 54% (48.6→22.4 pg / mL), and the Draize score improved (2.5→1.2).

[0149] Please refer to Table 6 for relevant data on ECM regeneration capacity:

[0150] index Experimental group (regeneration accelerator) Control group (HAase) HA regeneration rate (72h, %) 89.2±3.8 35.6±3.2 Collagen regeneration rate (72h, %) 90.5±4.1 55.4±4.7

[0151] Table 6

[0152] The data in Table 6 show that in the control group, HA was sparsely distributed and collagen fibers were broken; in the experimental group, HA was evenly distributed, collagen was tightly arranged, and fibroblast activity was enhanced.

[0153] The data in Tables 4-6 indicate that while HAase can improve transdermal efficiency in the short term, it leads to irreversible damage to HA and collagen (regeneration rate <35%). The combination of GlcNAc + TGF-β + cross-linked HA microspheres increased the HA regeneration rate to 84.7%, and restored collagen density to normal levels (92.1 μg / mg). The experimental group showed a significant reduction in inflammatory response (IL-6 ↓ 54%) and improved skin irritation (Draize score 1.2). The regeneration promoter dynamically repairs the ECM, avoiding the decline in barrier function caused by long-term medication. Introducing an ECM regeneration promoter can balance penetration enhancement with skin health, making it particularly suitable for chronic diseases requiring multiple doses (such as diabetes and obesity).

[0154] Example 3

[0155] The soluble microneedle composition based on the synergistic permeation-enhancing mechanism in this embodiment includes a macromolecular drug, a polymeric framework material, a charge-neutralizing material, an extracellular matrix degrading enzyme / collagen protective composition, additives, and a solvent. The solvent used is deionized water. The total mass fraction of the macromolecular drug, polymeric framework material, charge-neutralizing material, extracellular matrix degrading enzyme / collagen protective composition, additives, and solvent is 100%.

[0156] In this embodiment, the macromolecular drug is smegglutide, with a mass percentage of 2.0 W%. The polymer backbone material is a mixture of polyvinyl alcohol and polyvinylpyrrolidone. Polyvinyl alcohol acts as a film-forming and mechanical support, ensuring that the microneedle can effectively penetrate the skin; the mass percentage of polyvinyl alcohol is 25.0 W. Polyvinylpyrrolidone is used to improve the uniformity and rapid solubility of the needle; the mass percentage of polyvinylpyrrolidone is 10.0 W. The charge neutralizing material is a mixture of chitosan and ε-polylysine. Chitosan with a degree of deacetylation ≥85% is selected. It is positively charged and forms a complex with the negatively charged component at an appropriate pH to regulate local charge balance and reduce electrostatic repulsion; the mass percentage of chitosan is 1.5 W. ε-polylysine is used to assist in regulating charge balance; the mass percentage of ε-polylysine is 2.0 W.

[0157] The extracellular matrix (ECM) degrading enzyme in the ECM / collagen protection composition is hyaluronidase. This hyaluronidase is encapsulated in polylactic-co-glycolic acid copolymer (lactic acid to glycolic acid mass ratio of 1:1) using a double emulsification-solvent evaporation method to achieve enzyme activity protection and controlled release. The microsphere encapsulation process here uses a conventional double emulsification-solvent evaporation method, which will not be described in detail. The collagen protection material is quercetin, used to prevent excessive collagen degradation during enzymatic hydrolysis and protect the ECM structure. The concentration of hyaluronidase is 200 U / mL, and the mass percentage of quercetin is 0.1 W%. Hyaluronidase is released within 5–10 minutes after the needle is inserted into the skin tissue, locally degrading hyaluronic acid in the ECM and forming diffusion channels. Hyaluronidase is encapsulated in a polylactic acid-glycolic acid copolymer slow-release carrier to slowly release enzyme molecules, maintaining its activity at an effective but controllable level, and avoiding excessive degradation of HA caused by instantaneous high enzyme concentration (such as inflammation or structural collapse caused by excessively large ECM pore size).

[0158] The additives include glycerol, polysorbate 80, EDTA, and a pH adjuster. Glycerol acts as a plasticizer to prevent the needle from drying and cracking; the mass percentage of glycerol is 3.0 W%. Polysorbate 80 acts as a dispersant to maintain the homogeneity of the system; the mass percentage of polysorbate 80 is 0.3 W%. EDTA is used to chelate metal ions and enhance stability; the mass percentage of EDTA is 0.1 W. The pH adjuster is a mixture of potassium dihydrogen phosphate and dipotassium hydrogen phosphate; the mass percentage of the pH adjuster is 0.1 W, adjusting the pH of the needle solution to 6.8-7.0 to facilitate the stable formation of the complex.

[0159] In this embodiment, the microneedle patch uses medical nonwoven fabric and a PVA / PVP composite layer (the same as the polymer skeleton material) as the patch base to ensure that the needle adheres firmly to the skin.

[0160] The preparation method of the microneedle patch in this embodiment is as follows:

[0161] (1) Preparation of PVA / PVP composite

[0162] PVA and PVP are dissolved separately in deionized water at 60–80°C, stirred and mixed, and then glycerol, polysorbate 80 and EDTA are added and mixed evenly. Part of the resulting solution is used as a polymer skeleton material solution and the other part is used as a base PVA / PVP composite layer solution.

[0163] (2) Preparation of charge neutralization solution

[0164] Chitosan and ε-polylysine were first dissolved in a 0.1% potassium dihydrogen phosphate / dipotassium hydrogen phosphate solution. After adjusting the pH to 6.8-7.0, smegglutinin was added and stirred for 1 hour to form a charge-neutralized solution.

[0165] (3) Preparation of needle solution and injection molding

[0166] The charge neutralization solution, microsphere-treated hyaluronidase, and quercetin were added to the polymer backbone material solution, then injected into the PDMS microneedle mold, vacuum degassed (about 10 minutes), left to stand at room temperature for 12 hours, and then cured into a needle array by drying at 25°C for 24 hours.

[0167] (4) Substrate preparation

[0168] The aforementioned PVA / PVP composite layer solution is cast into a base mold on the needle array and covered with medical nonwoven fabric to form a base layer. After curing at room temperature, the mold is removed and air-dried to obtain the microneedle patch.

[0169] In this embodiment, chitosan and ε-polylysine form a complex with smegglutide, regulating the surface charge of the drug and reducing the binding force between smegglutide and the negative charge of the skin ECM; after the release of hyaluronidase, it locally degrades hyaluronic acid in the ECM, rapidly forming diffusion channels and improving the transdermal drug penetration rate; quercetin inhibits collagen degradation caused by enzymatic hydrolysis, protecting tissue safety.

[0170] Example 4

[0171] The soluble microneedle composition based on the synergistic permeation-enhancing mechanism in this embodiment includes a macromolecular drug, a polymer backbone material, a charge neutralizing material, an extracellular matrix degrading enzyme / collagen protective composition, an extracellular matrix regeneration promoting material, additives, and a solvent. The solvent is deionized water, and the total mass fraction of the macromolecular drug, polymer backbone material, charge neutralizing material, extracellular matrix degrading enzyme / collagen protective composition, extracellular matrix regeneration promoting material, additives, and solvent is 100%.

[0172] In this embodiment, the macromolecular drug is smegglutide, with a mass percentage of 2.5 wt%. The polymer backbone material is a mixture of hydroxypropyl methylcellulose, gelatin, and polyvinyl alcohol. Hydroxypropyl methylcellulose, with good film-forming properties and biocompatibility, is used to form a soft and uniform needle body, and its mass percentage is 10.0 wt%. Gelatin, with a mass percentage of 15.0 wt, is used to impart appropriate flexibility and biodegradability to the microneedle body. Polyvinyl alcohol, with a mass percentage of 20.0 wt%, is used to provide good mechanical strength to the needle body.

[0173] The charge neutralizing material is a mixture of polylysine and polyβ-amino ester, with polylysine being positively charged and having a mass percentage of 1.5 W; polyβ-amino ester is used to further optimize the charge balance of the composite and has a mass percentage of 0.5 W.

[0174] The extracellular matrix degrading enzyme in the extracellular matrix degrading enzyme / collagen protection composition is hyaluronidase. Similar to Example 3, the hyaluronidase is still microsphere-encapsulated using polylactic-co-glycolic acid copolymer. The hyaluronidase is dispersed in deionized water at a concentration of 200 U / mL and uniformly coated onto the outer layer of the needle body by spraying. The collagen protection material is tissue metalloproteinase inhibitor-1, used to prevent excessive collagen degradation during enzymatic hydrolysis and protect the ECM structure. The collagen protection material has a mass percentage of 0.2 W.

[0175] The extracellular matrix regeneration promoting materials include cross-linked hyaluronic acid, N-acetylglucosamine, and epidermal growth factor. Cross-linked hyaluronic acid is used to promote ECM regeneration, with a mass percentage of 1.5 W. N-acetylglucosamine is used to promote HA regeneration, with a mass percentage of 0.5 W. The dosage of epidermal growth factor is 20 ng / injection.

[0176] The additives include glycerol, polysorbate 80, EDTA, and a pH adjuster. Glycerol is 3.0 W% by mass; polysorbate 80 is 0.3 W% by mass; EDTA is 0.1 W% by mass; and the pH adjuster is a mixed solution of histidine and hydrochloric acid, with a pH adjuster mass percentage of 0.1 W%.

[0177] In this embodiment, the base of the microneedle patch is made of medical nonwoven fabric mixed with HPMC / gelatin to form a film for adhering to the skin.

[0178] The preparation method of the microneedle patch in this embodiment is as follows:

[0179] (1) Preparation of needle skeleton

[0180] HPMC, gelatin and PVA were dissolved in deionized water at 50°C. Glycerin, polysorbate 80 and EDTA were added and mixed evenly to prepare a base solution.

[0181] (2) Formation of charge neutralization complex

[0182] Polylysine and polyβ-amino ester were pre-dissolved in 0.1% histidine / hydrochloric acid solution and adjusted to pH 6.8–7.0. Smeglucopyne was then added and stirred to form a complex.

[0183] (3) Injection molding and degassing

[0184] The mixed solution was injected into the PDMS microneedle mold, vacuum degassed for 10 minutes, and then dried and cured after standing at room temperature for 12 hours.

[0185] (4) Substrate preparation

[0186] A repair solution containing cross-linked HA, NAG, and EGF is poured into a needle base mold and covered with medical nonwoven fabric to form a base layer. After curing at room temperature, the microneedle patch is demolded.

[0187] (5) Enzyme encapsulation

[0188] Microsphere-based hyaluronidase and tissue metalloproteinase inhibitor-1 (TIMP-1) were uniformly coated onto the outer layer of the needle using a spraying method, and the final microneedle patch was obtained after drying.

[0189] In this embodiment, the charge neutralization complex reduces the adsorption of smegglutinin to the negative charge of the skin ECM, hyaluronidase degrades hyaluronic acid in the ECM, opens drug diffusion channels, and the backing repair layer releases cross-linked HA, NAG and EGF, promoting skin ECM regeneration and repairing the barrier damaged by enzymatic hydrolysis, thereby improving safety and sustained release effect.

[0190] Example 5

[0191] The soluble microneedle composition based on the synergistic permeation-enhancing mechanism in this embodiment includes a macromolecular drug, a polymer backbone material, a charge neutralizing material, an extracellular matrix degrading enzyme / collagen protective composition, an extracellular matrix regeneration promoting material, additives, a solvent, and an osmotic pressure driving material. The solvent used is deionized water. The total mass fraction of the macromolecular drug, polymer backbone material, charge neutralizing material, extracellular matrix degrading enzyme / collagen protective composition, extracellular matrix regeneration promoting material, additives, solvent, and osmotic pressure driving material is 100%.

[0192] In this embodiment, the macromolecular drug is semaglutide, with a mass percentage of 3.0 wt%. The polymer backbone material is a mixture of silk fibroin, polylactic acid-glycolic acid copolymer, and polyvinyl alcohol. Silk fibroin has excellent mechanical strength and good biocompatibility, making it suitable for long-term punctures; the mass percentage of silk fibroin is 10 wt%. Polylactic acid-glycolic acid copolymer is used to provide controlled-release performance and enhance needle rigidity; the mass percentage of polylactic acid-glycolic acid copolymer is 10 wt%. Polyvinyl alcohol is used to ensure the overall film formation and puncture capability of the needle; the mass percentage of polyvinyl alcohol is 20 wt%.

[0193] The charge-neutralizing materials include PAMAM low-generation dendritic molecules (G3) and cationic cyclodextrin (HP-β-CD-N+). PAMAM low-generation dendritic molecules (G3) are positively charged materials, forming a stable nanocomposite with high charge density and excellent controlled release effect. The mass percentage of PAMAM low-generation dendritic molecules (G3) is 1.0 W. The cationic cyclodextrin is used to further optimize the charge balance of the composite, and the mass percentage of cationic cyclodextrin is 0.5 W.

[0194] The extracellular matrix degrading enzymes in the extracellular matrix degrading enzyme / collagen protective composition are hyaluronidase and deoxyribonuclease. Similar to Example 3, the hyaluronidase is microsphere-encapsulated using polylactic-co-glycolic acid copolymer. The hyaluronidase is dispersed in deionized water at a concentration of 200 U / mL and uniformly coated onto the outer layer of the needle body using a spray method. The deoxyribonuclease concentration is 5 U / mL, which helps with local ECM adjustment. The collagen protective material is PEG-TIMP-1, with a mass percentage of 0.1 W%.

[0195] The osmotic pressure driving materials include sorbitol, mannitol, and sodium chloride (NaCl). Sorbitol is used to create a high osmotic pressure environment to induce skin cell dehydration and shrinkage. The mass percentage of sorbitol in the needle solution is 5.0 W, the mass percentage of mannitol in the needle solution is 3.0 W, and the mass percentage of sodium chloride (NaCl) in the needle solution is 0.9 W.

[0196] The extracellular matrix regeneration promoting material includes cross-linked hyaluronic acid, N-acetylglucosamine, and epidermal growth factor. The mass percentage of cross-linked hyaluronic acid is 1.5W, the mass percentage of N-acetylglucosamine is 0.5W, and the dosage of epidermal growth factor is 20ng / injection.

[0197] The additives include glycerol, polysorbate 80, EDTA, and a pH adjuster. The glycerol content is 3.0 W% by mass; the polysorbate 80 content is 0.3 W% by mass; the EDTA content is 0.1 W% by mass; and the pH adjuster is a mixed solution of potassium citrate and citric acid, with a pH adjuster content of 0.2 W% by mass in the injection solution.

[0198] In this embodiment, the base of the microneedle patch is a mixture of medical nonwoven fabric and polylactic acid-glycolic acid copolymer / polyethylene glycol (PEG) film, ensuring that the needle adheres firmly to the skin.

[0199] The preparation method of the microneedle patch in this embodiment is as follows:

[0200] (1) Preparation of needle solution

[0201] Dissolve and mix silk fibroin, PVA, and glycerol, then add charge neutralizing material and stir thoroughly. Prepare an osmotic pressure regulating solution containing sorbitol, mannitol, and NaCl beforehand and mix thoroughly.

[0202] (2) Injection molding and degassing

[0203] Needle tip layer (enzymatic barrier): Microsphere-modified hyaluronidase, deoxyribonuclease and PEG-TIMP-1 are added to a mixture of silk fibroin, PVA and glycerol to fill the needle tip part of the microneedle mold. After vacuum degassing for 10 minutes, the mixture is freeze-dried to form the needle tip layer.

[0204] Intermediate layer (charge neutralization complex sustained release): Silk fibroin, PVA, glycerol, charge neutralization components, sorbitol, mannitol and NaCl are mixed evenly and then filled into the middle section of the microneedle mold body. After vacuum degassing for 10 minutes, the mixture is freeze-dried to form the microneedle intermediate layer.

[0205] Needle base layer (barrier repair): A repair solution containing cross-linked HA, NAG and EGF is filled into the bottom of the microneedle mold by casting. After vacuum degassing for 10 minutes, it is freeze-dried to form the needle base layer.

[0206] (3) Substrate preparation

[0207] PLGA and PEG were dissolved together in DMSO and water, poured onto the bottom layer of the microneedle, and covered with medical nonwoven fabric to form a base layer. After curing, the microneedle patch was demolded.

[0208] In this embodiment, the charge neutralization complex reduces the adhesion of semaglutide to the negative charge in the skin ECM, the hyaluronidase in the needle tip layer degrades hyaluronic acid in the ECM to form diffusion channels, and the osmotic pressure regulating material in the middle layer forms a hyperosmotic gradient in the skin, inducing cell dehydration and shrinkage, expanding the intercellular space, and making the drug complex diffuse more rapidly. The cross-linked HA, NAG and EGF released at the needle bottom promote ECM regeneration and ensure that the skin barrier recovers rapidly after permeation enhancement, thereby ensuring long-term safety and efficacy.

[0209] Example 6

[0210] The soluble microneedle composition based on the synergistic permeation-enhancing mechanism in this embodiment includes a macromolecular drug, a polymer framework material, a charge neutralizing material, and an extracellular matrix degrading enzyme / collagen protective composition. The solvent used is deionized water, and the total mass fraction of the macromolecular drug, polymer framework material, charge neutralizing material, and extracellular matrix degrading enzyme / collagen protective composition is 100%.

[0211] In this embodiment, the macromolecular drug is abapatide, with a mass percentage of 1.0 W. The polymer backbone materials include polyvinyl alcohol, polyvinylpyrrolidone, gelatin, and HPMC, with a mass percentage of 25 W for polyvinyl alcohol, 10 W for polyvinylpyrrolidone, 10 W for gelatin in the injection solution, and 10 W for HPMC.

[0212] The charge neutralizing material is composed of sodium alginate, with a mass percentage of 5.0 W. As an anionic material, sodium alginate binds to the positive charge of apapatide, shielding the positive charge of the drug and reducing its electrostatic force with the negative charge in the skin's ECM.

[0213] The extracellular matrix degrading enzyme in the extracellular matrix degrading enzyme / collagen protection composition is hyaluronidase. Similar to Example 3, the hyaluronidase is still microsphere-encapsulated using polylactic-co-glycolic acid copolymer. The collagen protection material is quercetin, with a mass percentage of 0.1 W%. Hyaluronidase and quercetin are dispersed in deionized water, with the hyaluronidase concentration at 200 U / mL.

[0214] The additives include glycerol, polysorbate 80, EDTA, and a pH adjuster. The glycerol content is 3.0% by weight; the polysorbate 80 content is 0.3% by weight; the EDTA content is 0.1% by weight; and the pH adjuster uses Tris buffer.

[0215] In this embodiment, the microneedle patch uses a substrate made of medical nonwoven fabric and a PVA / PVP composite layer.

[0216] The preparation method of the microneedle patch in this embodiment is as follows:

[0217] (1) Preparation of needle substrate

[0218] PVA, PVP, HPMC, and gelatin were dissolved in deionized water at 50°C, stirred and mixed, and then glycerin, polysorbate 80, and EDTA were added. After the mixture was adjusted to be uniform, it was cast onto a pre-prepared medical nonwoven fabric substrate to form a base layer.

[0219] (2) Preparation of charge neutralization complex

[0220] Sodium alginate was first dissolved in Tris buffer, and the pH was adjusted to 6.8-7.0. Then, apapatide was added and stirred for 1 hour to form a complex.

[0221] (3) Preparation of needle solution and injection molding

[0222] The charge neutralizing complex was uniformly mixed into the aforementioned framework solution, then injected into the PDMS microneedle mold, vacuum degassed (about 10 minutes), left to stand at room temperature for 12 hours, and then dried at 25°C for 24 hours to solidify into a needle array.

[0223] (4) Enzyme encapsulation

[0224] The microsphere-treated hyaluronidase and quercetin solution were uniformly sprayed onto the surface of the needle using a spraying method, and the final patch was obtained after air drying.

[0225] In this embodiment, sodium alginate and abapapeptide form a stable complex, reducing the non-specific adsorption between the drug and the negative charge of the skin ECM, and hyaluronidase locally degrades hyaluronic acid in the ECM, forming diffusion channels.

[0226] Example 7

[0227] The soluble microneedle composition based on the synergistic permeation-enhancing mechanism in this embodiment includes a macromolecular drug, a polymer backbone material, a charge neutralizing material, an extracellular matrix degrading enzyme / collagen protective composition, an extracellular matrix regeneration promoting material, additives, and an osmotic pressure driving material. The solvent used is deionized water, and the total mass fraction of the macromolecular drug, polymer backbone material, charge neutralizing material, extracellular matrix degrading enzyme / collagen protective composition, extracellular matrix regeneration promoting material, additives, and osmotic pressure driving material is 100%.

[0228] In this embodiment, the macromolecular drug is abapatide, with a mass percentage of 1.2 W. The polymer backbone materials include sodium carboxymethyl cellulose (CMC-Na), gelatin, and PVP, with a mass percentage of 10 W for sodium carboxymethyl cellulose (CMC-Na), 15 W for gelatin, and 10 W for PVP.

[0229] The charge neutralizing agent is chondroitin sulfate, with a mass percentage of 2.0 W%. The extracellular matrix degrading enzyme in the extracellular matrix degrading enzyme / collagen protecting composition is hyaluronidase, with a concentration of 200 U / mL. The collagen protecting agent is TIMP-1, with a mass percentage of 0.1 W.

[0230] The extracellular matrix regeneration promoting materials include cross-linked hyaluronic acid, N-acetylglucosamine, and epidermal growth factor. Cross-linked hyaluronic acid is used to promote ECM regeneration, with a mass percentage of 1.5 W. N-acetylglucosamine is used to promote HA regeneration, with a mass percentage of 0.5 W. The dosage of epidermal growth factor is 20 ng / injection.

[0231] The additives include glycerol, polysorbate 80, EDTA, and a pH adjuster. The glycerol is 3.0% by weight; the polysorbate 80 is 0.3% by weight; the EDTA is 0.1% by weight; and the pH adjuster is a potassium dihydrogen phosphate / dipotassium hydrogen phosphate buffer.

[0232] In this embodiment, the substrate of the microneedle patch is a substrate formed by medical nonwoven fabric and CMC-Na / gelatin mixed film.

[0233] The preparation method of the microneedle patch in this embodiment is similar to that in Embodiment 4 above. However, after injection molding, a solution containing repair factors is applied to the backing of the needle body by casting to form a repair layer, and then the patch is cured and demolded at room temperature.

[0234] In this embodiment, based on charge neutralization and enzymatic barrier dissolution, the repair layer releases cross-linked HA, NAG, and EGF to promote ECM regeneration, further improving penetration while ensuring skin safety.

[0235] Example 8

[0236] The soluble microneedle composition based on the synergistic permeation-enhancing mechanism in this embodiment includes a macromolecular drug, a polymer backbone material, a charge neutralizing material, an extracellular matrix degrading enzyme / collagen protective composition, an extracellular matrix regeneration promoting material, additives, a solvent, and an osmotic pressure driving material. The solvent used is deionized water. The total mass fraction of the macromolecular drug, polymer backbone material, charge neutralizing material, extracellular matrix degrading enzyme / collagen protective composition, extracellular matrix regeneration promoting material, additives, solvent, and osmotic pressure driving material is 100%.

[0237] In this embodiment, the macromolecular drug is abapapeptide, with a mass percentage of 1.5 W. The polymer backbone material is a mixture of polylactic-co-glycolic acid copolymer (PLGA), polyethylene glycol (PEG), and gelatin, with a mass percentage of 15 W for PLGA, 5 W for PEG, and 10 W for gelatin.

[0238] The charge neutralizing material is carbomer 940, a synthetic anionic polymer whose carboxyl groups are highly deprotonated in neutral or weakly acidic environments, forming a strong electrostatic complex with the positive charge of apapatide, thus achieving neutralization. The mass percentage of carbomer is 1.0 W%.

[0239] The extracellular matrix degrading enzymes in the extracellular matrix degrading enzyme / collagen protective composition are hyaluronidase and deoxyribonuclease. Similar to Example 3, the hyaluronidase is microsphere-encapsulated using polylactic-co-glycolic acid copolymer. The hyaluronidase is dispersed in deionized water at a concentration of 200 U / mL and uniformly coated onto the outer layer of the needle body using a spray method. The deoxyribonuclease concentration is 5 U / mL, which helps with local ECM adjustment. The collagen protective material is PEG-TIMP-1, with a mass percentage of 0.1 W%.

[0240] The osmotic pressure driving materials include sorbitol, mannitol, and sodium chloride (NaCl). Sorbitol is used to create a high osmotic pressure environment to induce skin cell dehydration and shrinkage. The mass percentage of sorbitol is 5.0 W, mannitol is 3.0 W, and sodium chloride (NaCl) is 0.9 W.

[0241] The extracellular matrix regeneration promoting material includes cross-linked hyaluronic acid, N-acetylglucosamine, and epidermal growth factor. The mass percentage of cross-linked hyaluronic acid is 1.5W, the mass percentage of N-acetylglucosamine is 0.5W, and the dosage of epidermal growth factor is 20ng / injection.

[0242] The additives include glycerol, polysorbate 80, EDTA, and a pH adjuster. Glycerol is 3.0 W% by mass; polysorbate 80 is 0.3 W% by mass; EDTA is 0.1 W% by mass; and the pH adjuster is a mixed solution of potassium citrate / citric acid, with a pH adjuster mass percentage of 0.2 W%.

[0243] In this embodiment, the substrate of the microneedle patch is formed by blending medical nonwoven fabric with PLGA / PEG to enhance mechanical support and biodegradability.

[0244] The preparation method of the microneedle patch in this embodiment is as follows:

[0245] (1) Dissolve PLGA and PEG in a suitable organic solvent in proportion, mix them and then coat them onto non-woven fabric to make a base film.

[0246] (2) The needle solution is prepared according to the above formula, and the charge neutralizing component, enzymatic hydrolysis material and osmotic pressure driving material are added. The solution is injected into the mold, vacuum degassed, and dried and solidified after standing at room temperature.

[0247] (3) Use a spraying method to evenly coat the outer layer of the needle with microspheres of hyaluronidase and quercetin;

[0248] (4) The repair solution containing cross-linked HA, NAG and EGF is poured into the needle backing, and after curing, it is demolded to obtain the final patch.

[0249] In this embodiment, charge neutralization regulation causes apapain to exist in the form of a complex, reducing its negative charge adsorption to the ECM. Hyaluronidase degrades HA in the ECM, forming diffusion channels. Osmotic pressure drives the material to generate a hypertonic gradient in the skin, inducing local cell dehydration and shrinkage, and expanding the intercellular space. The repair layer promotes ECM regeneration after drug release, restores the skin barrier, and ensures safety.

[0250] Example 9

[0251] The soluble microneedle composition based on the synergistic permeation-enhancing mechanism in this embodiment includes a macromolecular drug, a polymer backbone material, a charge neutralizing material, an extracellular matrix degrading enzyme / collagen protective composition, an extracellular matrix regeneration promoting material, and additives and osmotic pressure driving materials. The solvent used in the additives is deionized water.

[0252] In this embodiment, the macromolecular drug is semaglutide, with a mass percentage of 1.0 W. The polymer backbone material is a mixture of silk fibroin, polylactic acid-glycolic acid copolymer, and polyvinyl alcohol, with a mass percentage of 10 W for silk fibroin, polylactic acid-glycolic acid copolymer, and polyvinyl alcohol.

[0253] The charge neutralizing materials include PAMAM low-generation dendritic molecules (G3) and cationic cyclodextrin (HP-β-CD-N+), with the mass percentage of PAMAM low-generation dendritic molecules (G3) being 0.5 W and the mass percentage of cationic cyclodextrin being 0.5 W.

[0254] The extracellular matrix degrading enzymes in the extracellular matrix degrading enzyme / collagen protective composition are hyaluronidase and deoxyribonuclease. Similar to Example 3, the hyaluronidase is microsphere-encapsulated using polylactic-co-glycolic acid copolymer. The hyaluronidase is dispersed in deionized water at a concentration of 200 U / mL and uniformly coated onto the outer layer of the needle body using a spray method. The deoxyribonuclease concentration is 5 U / mL, which helps with local ECM adjustment. The collagen protective material is PEG-TIMP-1, with a mass percentage of 0.1 W%.

[0255] The osmotic pressure driving materials include sorbitol, mannitol, and sodium chloride (NaCl). Sorbitol is used to create a high osmotic pressure environment to induce skin cell dehydration and shrinkage. The mass percentage of sorbitol in the needle solution is 5.0 W, the mass percentage of mannitol in the needle solution is 3.0 W, and the mass percentage of sodium chloride (NaCl) in the needle solution is 0.9 W.

[0256] The extracellular matrix regeneration promoting material includes cross-linked hyaluronic acid, N-acetylglucosamine, and epidermal growth factor. The mass percentage of cross-linked hyaluronic acid is 1.5W, the mass percentage of N-acetylglucosamine is 0.5W, and the dosage of epidermal growth factor is 20ng / injection.

[0257] The additives include glycerin, polysorbate 80, EDTA, and a pH adjuster. Glycerin is 0.5% by mass; polysorbate 80 is 0.2% by mass; EDTA is 0.1% by mass; and the pH adjuster is a mixed solution of potassium citrate / citric acid, with the pH adjuster accounting for 0.2% by mass in the injection solution.

[0258] In this embodiment, the base of the microneedle patch is a mixture of medical nonwoven fabric and polylactic acid-glycolic acid copolymer / polyethylene glycol (PEG) film, ensuring that the needle adheres firmly to the skin.

[0259] The preparation method of the microneedle patch in this embodiment is exactly the same as that in Example 5.

[0260] Example 10

[0261] The soluble microneedle composition based on the synergistic permeation-enhancing mechanism in this embodiment includes a macromolecular drug, a polymer backbone material, a charge neutralizing material, an extracellular matrix degrading enzyme / collagen protective composition, an extracellular matrix regeneration promoting material, and additives and osmotic pressure driving materials. The solvent used in the additives is deionized water.

[0262] In this embodiment, the macromolecular drug is smegglutide, with a mass percentage of 10.0 W. The polymer backbone material is a mixture of silk fibroin, polylactic acid-glycolic acid copolymer, and polyvinyl alcohol, with a mass percentage of 20 W for silk fibroin, 20 W for polylactic acid-glycolic acid copolymer, and 15 W for polyvinyl alcohol.

[0263] The charge neutralizing materials include PAMAM low-generation dendritic molecules (G3) and cationic cyclodextrin (HP-β-CD-N+), with PAMAM low-generation dendritic molecules (G3) comprising 3.0 W by mass and cationic cyclodextrin comprising 2.0 W by mass.

[0264] The extracellular matrix degrading enzymes in the extracellular matrix degrading enzyme / collagen protective composition are hyaluronidase and deoxyribonuclease. Similar to Example 3, the hyaluronidase is microsphere-encapsulated using polylactic-co-glycolic acid copolymer. The hyaluronidase is dispersed in deionized water at a concentration of 200 U / mL and uniformly coated onto the outer layer of the needle body using a spray method. The deoxyribonuclease concentration is 5 U / mL, which helps with local ECM adjustment. The collagen protective material is PEG-TIMP-1, with a mass percentage of 0.1 W%.

[0265] The osmotic pressure driving materials include sorbitol, mannitol, and sodium chloride (NaCl). Sorbitol is used to create a high osmotic pressure environment to induce skin cell dehydration and shrinkage. The mass percentage of sorbitol in the needle solution is 5.0 W, the mass percentage of mannitol in the needle solution is 3.0 W, and the mass percentage of sodium chloride (NaCl) in the needle solution is 0.9 W.

[0266] The extracellular matrix regeneration promoting material includes cross-linked hyaluronic acid, N-acetylglucosamine, and epidermal growth factor. The mass percentage of cross-linked hyaluronic acid is 1.5W, the mass percentage of N-acetylglucosamine is 0.5W, and the dosage of epidermal growth factor is 20ng / injection.

[0267] The additives include glycerin, polysorbate 80, EDTA, and a pH adjuster. Glycerin is 3.0 W% by mass; polysorbate 80 is 1.2 W% by mass; EDTA is 0.6 W% by mass; and the pH adjuster is a mixed solution of potassium citrate / citric acid, with a pH adjuster content of 0.2 W% in the injection solution.

[0268] In this embodiment, the base of the microneedle patch is a mixture of medical nonwoven fabric and polylactic acid-glycolic acid copolymer / polyethylene glycol (PEG) film, ensuring that the needle adheres firmly to the skin.

[0269] The preparation method of the microneedle patch in this embodiment is exactly the same as that in Example 5.

[0270] Animal experiments

[0271] In accordance with ethical requirements, six male SD rats weighing between 180-200g were selected. After 3 days of quarantine, they were randomly divided into two groups of three rats each: the Smegglutide Example 1 group and the Abapatide Example 1 group.

[0272] The administration method was as follows: Hair was removed from the back of rats beforehand. Microneedles were fixed to the probe of a tension gauge and applied to the rat's back with a force of 150 N at a speed of 1000 mm / min for 5 minutes. The microneedles were removed 2 hours after administration. At 6, 12, and 24 hours post-administration, 0.5 mL of blood was collected and placed in centrifuge tubes coated with sodium heparin. The plasma was separated by centrifugation at 5000 rpm for 10 minutes and then stored at -20°C. The plasma concentrations of semaglutide and abapatide were detected by LC / MS. The following are example data from in vivo pharmacokinetic (PK) and in vitro transdermal release experiments using rats as a model (n=6, mean ± SD for each group):

[0273]

[0274]

[0275] Table 7

[0276] In vitro transdermal release assay results (Franz diffusion cell, 24-hour cumulative release).

[0277]

[0278] Table 8

[0279] In vivo pharmacokinetic results for both semaglutide and abapatide showed that with the increase of the permeation-enhancing mechanism (from charge neutralization + enzymatic barrier degradation alone, to the addition of barrier repair, and then to the simultaneous addition of osmotic pressure-driven and barrier repair), Cmax (maximum plasma concentration) was significantly increased, Tmax (time to reach maximum concentration) was significantly shortened, and AUC0–24h (area under the curve from 0 to 24 hours) was significantly increased. For example, in Example 5, semaglutide achieved a Cmax of 180 ng / mL and an AUC of approximately 1500 ng·h / mL, while abapatide achieved a Cmax of 150 ng / mL and an AUC of approximately 1200 ng·h / mL in Example 8, both indicating that the synergistic permeation-enhancing mechanism significantly improved drug absorption efficiency.

[0280] In vitro transdermal release results showed that the cumulative release over 24 hours increased with increasing system complexity. In Examples 5 and 8, the release amounts of smegglutinin and abapatide reached approximately 98 μg / cm³, respectively. 2 and 96 μg / cm 2 This is significantly higher than the example using only charge neutralization + enzymatic barrier (approximately 55 μg / cm³). 2 and 50 μg / cm 2 This indicates that osmotic pressure-driven materials induce skin cell dehydration, widening the intercellular spaces and further promoting drug penetration. Simultaneously, barrier repair ensures the skin rapidly recovers its integrity after release, guaranteeing safety.

[0281] Comprehensive validation showed that both drugs exhibited the best permeation-enhancing effect in the embodiment of "charge neutralization + enzymatic barrier degradation + osmotic pressure-driven temporary ECM regulation + barrier repair," demonstrating that the synergistic mechanism of "charge neutralization + enzymatic barrier degradation + osmotic pressure-driven temporary ECM regulation + barrier repair" can achieve efficient, rapid, and safe transdermal delivery. Data indicate that this synergistic permeation-enhancing system not only significantly improves drug bioavailability but also takes into account skin barrier repair, reducing the potential inflammatory risk caused by ECM degradation.

[0282] The soluble microneedle patch described in this invention is based on a synergistic permeation-enhancing mechanism of "charge neutralization + enzymatic barrier hydrolysis + osmotic pressure-driven ECM temporary regulation + barrier repair". By using different polymer backbone materials, various charge neutralizing materials and different combinations selected from a variety of barrier regulation materials, three embodiments were designed for smegglutide and abapatide respectively.

[0283] Examples 3 and 6 (charge neutralization + enzymatic barrier decomposition only) are suitable for basic permeation enhancement requirements; Examples 4 and 7 (barrier repair added) further ensure local tissue safety and are suitable for long-term delivery; Examples 5 and 8 (osmotic pressure driven) expand diffusion channels by inducing cell dehydration, and are most effective in improving drug delivery efficiency.

[0284] Both in vivo and in vitro experimental data show that:

[0285] With the upgrade of the penetration-enhancing system, drug absorption is accelerated, Cmax and AUC are significantly improved, and transdermal release is also greatly increased. The synergistic penetration-enhancing mechanism enables rapid and sustained drug penetration, while simultaneously utilizing barrier repair strategies to maintain skin integrity, demonstrating significant clinical translational potential. The above examples and experimental data fully validate the technical solution of this invention, which can meet the requirements of efficient, safe, and controllable release for transdermal delivery of macromolecular drugs.

[0286] The above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit it. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the present invention without departing from the spirit and scope of the present invention, and all such modifications and substitutions should be covered within the scope of the claims of the present invention. Technical aspects, shapes, and structures not described in detail in this invention are all well-known technologies.

Claims

1. A soluble microneedle composition based on synergistic penetration enhancing mechanism characterized in that, The raw materials include the following mass fractions: The soluble microneedle composition further includes a solvent, and the total mass fraction of the macromolecular drug, the polymer skeleton material, the charge neutralization material, the barrier regulation material, the additive, and the solvent is 100%. The barrier regulation material is selected from at least one of an extracellular matrix degradation enzyme / collagen protection composition, an extracellular matrix regeneration promotion material, and an osmotic pressure driving material.

2. The synergistically penetration enhancing mechanism based dissolvable microneedle composition according to claim 1, wherein, The barrier regulation material is composed of the extracellular matrix degradation enzyme / collagen protection composition and the extracellular matrix regeneration promotion material, and the mass ratio of the extracellular matrix degradation enzyme / collagen protection composition to the extracellular matrix regeneration promotion material is 1:(0.5-2). Alternatively, the barrier regulation material is composed of the extracellular matrix degradation enzyme / collagen protection composition and the osmotic pressure driving material, and the mass ratio of the extracellular matrix degradation enzyme / collagen protection composition to the osmotic pressure driving material is 1:(1-20). Alternatively, the barrier regulation material is composed of the extracellular matrix degradation enzyme / collagen protection composition, the extracellular matrix regeneration promotion material, and the osmotic pressure driving material, and the mass ratio of the extracellular matrix degradation enzyme / collagen protection composition to the extracellular matrix regeneration promotion material to the osmotic pressure driving material is 1:(0.5-2):(1-20).

3. The synergistically penetration enhancing mechanism based dissolvable microneedle composition as claimed in claim 2, wherein, The extracellular matrix degradation enzyme / collagen protection composition is composed of an extracellular matrix degradation enzyme and a collagen protection material, and the mass ratio of the extracellular matrix degradation enzyme to the collagen protection material is 1:(2-5), the extracellular matrix degradation enzyme is selected from at least one of hyaluronidase, collagenase, elastase, trypsin, deoxyribonuclease, and lipase, and the collagen protection material is selected from at least one of tissue inhibitor of metalloproteinase-1, PEGylated tissue inhibitor of metalloproteinase-1, MMP inhibitor, vitamin C, alpha-tocopherol, genipin cross-linked collagen, aminoguanidine, epigallocatechin gallate, arbutin, ferulic acid, quercetin, and doxycycline.

4. The synergistically penetration enhancing mechanism based dissolvable microneedle composition as claimed in claim 2, wherein, The extracellular matrix regeneration promotion material is selected from at least one of N-acetylglucosamine, hyaluronic acid oligosaccharide, transforming growth factor-β, fibroblast growth factor, epidermal growth factor, vascular endothelial growth factor, dipotassium glycyrrhizinate, asiaticoside, ginsenoside Rb1, methacrylated HA, and copper peptide.

5. The synergistically penetration enhancing mechanism based dissolvable microneedle composition as claimed in claim 2, wherein, The osmotic pressure driving material is selected from at least one of sorbitol, mannitol, sodium chloride, magnesium sulfate, propylene glycol, polyethylene glycol, glycine, arginine, and poloxamer.

6. The synergistically penetration enhancing mechanism based dissolvable microneedle composition as claimed in claim 1, wherein, The mass ratio of the macromolecular drug to the charge neutralization material is 1:(0.5-5), and the charge neutralization material is selected from at least one of chitosan, polylysine, ε-polylysine, lactoferrin, dopamine-modified cationic polymer, cationic collagen hydrolysate, linear PEI, DOTAP liposome, poly-β-amino ester, poly-arginine, PAMAM low-generation dendrimer, cationic cyclodextrin, lecithin, phosphatidylserine, betaine, polyacrylic acid, sodium alginate, chondroitin sulfate, polyglutamic acid, phosphatidylcholine, carbomer, polyvinyl alcohol-polyacrylic acid copolymer, and carboxymethyl cellulose.

7. The synergistically penetration enhancing mechanism based dissolvable microneedle composition as claimed in claim 1 wherein, The macromolecular drug is selected from one of the following: polypeptide, protein, antibody, polysaccharide, and nucleic acid drugs.

8. The synergistically penetration enhancing mechanism based dissolvable microneedle composition as claimed in claim 1, wherein, The additives include stabilizers and pH adjusters. The stabilizers are selected from at least one of trehalose, sucrose, glucose, dextran, sulfobutyl ether-β-cyclodextrin, hydroxypropyl cellulose, carboxymethyl cellulose, xanthan gum, polysorbate 80, and glycerol. The pH adjusters are selected from at least one of sodium citrate, Tris buffer, arginine, histidine / hydrochloric acid, glucosamine, potassium bicarbonate, potassium dihydrogen phosphate / dipotassium hydrogen phosphate, NH4HCO3 / NH3, potassium citrate / citric acid, and citric acid / arginine. The solvents are selected from at least one of deionized water, acetic acid solution, phosphoric acid solution, and anhydrous ethanol.

9. A microneedle patch characterized by, It includes a substrate and a needle formed on the substrate, said needle being made of a soluble microneedle composition as described in any one of claims 1-8.

10. The microneedle patch of claim 1, wherein, The substrate material is selected from at least one of the following: hyaluronic acid or its sodium salt, polyvinyl alcohol, polyvinylpyrrolidone, hydroxypropyl methylcellulose, sodium carboxymethyl cellulose, gelatin, dextran, sodium alginate, silk fibroin, biodegradable polylactic acid, polycaprolactone, polylactic-glycolic acid copolymer, polyaspartic acid, lactoferrin, carbomer, hydroxypropyl chitosan, elastin peptide, polylactic-glycolic acid copolymer / polyethylene glycol / polyvinyl alcohol, polyester, polyethersulfone, polypropylene, polyimide, polyethylene naphthalate, polyurethane, polydimethylsiloxane, thermoplastic polyurethane, polytetrafluoroethylene, polycarbonate, poly(lactic-glycolic acid), poly(glycolic acid), poly-L-lactide, polystyrene-block-poly(ethylene-cyclobutene)-block-polystyrene, silicone, paper, medical nonwoven fabric, and textile materials.

Citation Information

Patent Citations

  • Soluble semeglutide microneedle composition and preparation method thereof