An apparatus and process for coating the surface of annealed stainless steel wire

The water-based composite solution coating process controlled by a circulating spraying mechanism and an electric heating box solves the problem of uneven coating on the surface of stainless steel wire, achieving high-performance and environmentally friendly coating generation that meets the needs of take-up and unwinding.

CN123149085APending Publication Date: 2026-11-24ZHEJIANG TENGLONG STAINLESS STEEL BAR & WIRE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611436131.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-16
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing technologies cannot provide a uniform, firm, clean and controllable surface coating for stainless steel wire after annealing, resulting in uneven lubrication, poor controllability, and affecting the tightness of take-up and the smoothness of unwinding.

Method used

A circulating spraying mechanism is used to apply a water-based composite solution to annealed stainless steel wire online. Through the combination of spray holes and sponge blocks, a uniform solid lubricating coating is formed. An electric heating box is used to control the solution temperature and concentration to ensure the stability and consistency of the coating.

Benefits of technology

It achieves the generation of high-performance coatings with strong adhesion, good lubricity, moderate coefficient of friction, environmental friendliness and no pollution, and controllable coating performance to meet the needs of different customers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149085A_ABST
    Figure CN123149085A_ABST
Patent Text Reader

Abstract

This invention provides an apparatus and process for coating the surface of annealed stainless steel wire: It includes a frame and a circulating spraying mechanism mounted on the frame. The circulating spraying mechanism includes a storage tank, a circulating pump, spray pipes, and an electric heating box. First, a water-based composite solution is placed in the heating chamber of the electric heating box for heating and constant temperature control. Then, the circulating pump is started to extract the water-based composite solution from the heating chamber and deliver it to the spray pipes. The water-based composite solution in the spray pipes is sprayed out through spray holes to initially coat the surface of the stainless steel wire. Excess water-based composite solution is returned to the storage tank below for recycling. The initially coated stainless steel wire passes through a sponge block soaked in the water-based composite solution for a secondary coating. Finally, it is taken to the take-up rack after passing through a wire reel. During this process and storage, the water in the water-based composite solution evaporates, and the drawing powder component forms a uniformly adhered, stable solid lubricating coating on the surface of the stainless steel wire.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the technical field of surface coating of stainless steel wire, specifically to an apparatus and process for surface coating of annealed stainless steel wire. Background Technology

[0002] In stainless steel wire production, traditional methods for facilitating take-up and unwinding are mainly divided into two categories: one is to apply lubricating oil before take-up, which easily causes oil drips and environmental pollution, and is not friendly to subsequent processes that require a dry wire surface; the other is to use solid drawing powder for lubrication during drawing, which leaves residual powder after drawing. However, to ensure the surface quality of the wire and prevent contamination, the drawing powder is cleaned by pickling and washing before annealing. The friction coefficient of the cleaned wire surface is unstable, which directly affects the tightness of take-up and the smoothness of unwinding.

[0003] While existing technologies provide powder removal devices, their purpose is solely to remove powder, failing to resolve the conflict between lubrication and cleaning. Furthermore, both oiling and dry powder application suffer from uneven lubrication, poor controllability, and weak adhesion to the wire surface. Therefore, the industry urgently needs a surface treatment solution that provides a uniform, robust, clean, and controllable surface treatment for wires after annealing, while simultaneously optimizing the winding and unwinding process. Summary of the Invention

[0004] The technical problem to be solved by the present invention is to overcome the defects of the prior art and provide an apparatus and process for providing a uniform, firm, clean and controllable coating on the surface of wire after annealing.

[0005] The technical solution of the present invention is to provide an apparatus for coating the surface of annealed stainless steel wire with the following structure: including a frame and a circulating spraying mechanism disposed on the frame; One end of the frame is provided with a wire outlet hole, and the other end is provided with a wire guide wheel. A spray channel for stainless steel wire to pass through is formed between the wire outlet hole and the wire guide wheel. The circulating spraying mechanism includes a storage tank, a circulating pump, and a spray pipe. The spray pipe and the storage tank are located above and below the spraying channel, respectively. One end of the circulating pump is connected to the storage tank, and the other end is connected to the spray pipe. It is used to draw water-based composite solution from the storage tank and transport it to the spray pipe. The bottom of the spray pipe is provided with spray holes for spraying the water-based composite solution from the spray pipe to spray the stainless steel wire in the spraying channel below, and then return to the storage tank.

[0006] Preferably, there are multiple outlet holes, which are evenly spaced along the width of the frame; there are also multiple wire guide wheels, which are coaxially arranged and correspond one-to-one with each outlet hole.

[0007] Preferably, there are multiple spray holes, which are evenly spaced along the length of the spray pipe; a sponge plate is provided on the frame below the spray pipe, and the lower end face of the sponge plate abuts against the stainless steel wire on the spray channel.

[0008] Preferably, the frame is provided with multiple sponge blocks corresponding to the spray channels one by one at the position behind the spray pipe. Each sponge block has a through groove extending through its front and rear ends. The through groove is used for the stainless steel wire on the corresponding spray channel to pass through. The inner diameter of the through groove is smaller than the outer diameter of the stainless steel wire so that the sponge block fits against the outer peripheral wall of the stainless steel wire. The sponge block is wetted with a water-based composite solution to evenly coat the surface of the stainless steel wire.

[0009] Preferably, the circulating spray mechanism further includes an electric heating box, which is installed on the pipeline between the liquid storage tank and the circulating pump. The electric heating box is equipped with a heating chamber and a controller. The heating chamber is equipped with an electric heating unit and a temperature control unit, which are electrically connected to the controller. The electric heating unit is used to heat the water-based composite solution in the heating chamber, and the temperature control unit is used to detect the temperature of the water-based composite solution in the heating chamber and transmit the detection signal to the controller. The controller is used to control the switching of the electric heating unit.

[0010] This invention also provides a process for coating the surface of annealed stainless steel wire, comprising the following steps: S1. The water-based composite solution is placed in the heating chamber of the electric heating box for heating and constant temperature control; S2. After annealing, the stainless steel wire passes through the outlet hole and spray channel. The circulation pump is started to draw water-based composite solution from the heating chamber and deliver it to the spray pipe. The water-based composite solution in the spray pipe is sprayed out through the spray hole and wets and penetrates the sponge plate below to preliminarily coat the surface of the stainless steel wire. Excess water-based composite solution flows back to the storage tank below and is then recycled. S3. The stainless steel wire with initial coating is coated a second time by a sponge block soaked in water-based composite solution to make the water-based composite solution on its surface more uniform. S4. The stainless steel wire coated with the water-based composite solution twice is taken to the take-up rack after passing through the wire reel. During this process and storage, the water in the water-based composite solution evaporates, and the wire drawing powder component forms a uniformly adhered and stable solid lubricating coating on the surface of the stainless steel wire. The core of this invention is that by preparing and coating the water-based composite solution online, the wire drawing powder adheres in the optimal state and is finally transformed into a brand-new, in-situ generated composite coating.

[0011] Preferably, in step S1, the water-based composite solution is a stable suspension solution formed by mixing drawing powder and water in a specific ratio, heating and controlling the temperature.

[0012] Preferably, the heating temperature of the water-based composite solution is 80-90℃.

[0013] Preferably, the heating temperature of the water-based composite solution is 90°C.

[0014] Preferably, the concentration of the water-based composite solution is 0.5 as characterized by refractive index.

[0015] With the above structure, the apparatus and process for coating the surface of annealed stainless steel wire in this invention have the following advantages compared with the prior art: 1. Achieved the generation of high-performance coatings: By applying a warm solution online, the wire drawing powder particles can adhere more evenly and tightly to the wire surface, and the resulting coating has a much stronger adhesion than simply applying dry powder or oil film, resulting in more stable performance.

[0016] 2. Perfectly balances take-up and unwinding needs: The coating provides excellent lubrication during take-up to ensure a tight roll shape; after curing, it provides a moderate and consistent coefficient of friction to ensure uniform tension and no dust shedding during unwinding for downstream customers.

[0017] 3. Clean and environmentally friendly process: Water is used as the medium, eliminating the risk of oil pollution; the solution can be recycled, minimizing waste and making it environmentally friendly.

[0018] 4. Highly controllable coating performance: By precisely controlling the solution concentration (refractive index), temperature and coating amount, the thickness and performance of the final coating can be precisely controlled to meet the needs of different customers and with good reproducibility.

[0019] The core of this invention lies in the fact that by preparing and coating a water-based composite solution online, the drawing powder adheres in an optimal state, ultimately transforming into a completely new, in-situ generated composite coating. Attached Figure Description

[0020] Figure 1 This is a schematic diagram of the structure in the first axial view direction of the present invention.

[0021] Figure 2 This is a schematic diagram of the structure in the second axial view direction of the present invention.

[0022] Figure 3 This is a top-view structural diagram of the present invention.

[0023] Figure 4 for Figure 1 A magnified view of a portion of the image.

[0024] Explanation of reference numerals in the attached figures: 1. Frame; 11. Cable outlet; 12. Cable guide wheel; 2. Circulating spray mechanism; 21. Liquid storage tank; 22. Circulating pump; 23. Spray pipe; 24. Sponge board; 25. Sponge block; 26. Electric heating box. Detailed Implementation

[0025] The present invention will now be described in further detail with reference to the accompanying drawings and specific embodiments.

[0026] In the description of this invention, it should be understood that the terms "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention. At the same time, the terms "first," "second," etc., are only used to distinguish the names of various components and do not have a primary or secondary relationship. Therefore, they should not be construed as limitations on this invention.

[0027] like Figures 1-4 As shown, the present invention discloses an apparatus for coating the surface of annealed stainless steel wire with the following structure: including a frame 1 and a circulating spraying mechanism 2 disposed on the frame 1.

[0028] The frame 1 is located between the annealing furnace cooling tank and the take-up device. One end of the frame is provided with a wire outlet 11 (i.e. the wire outlet of the annealing furnace cooling tank), and the other end is provided with a wire guide wheel 12. A spray channel for stainless steel wire to pass through is formed between the wire outlet 11 and the wire guide wheel 12.

[0029] There are multiple outlet holes 11, which are evenly spaced along the width of the frame 1; there are also multiple wire guide wheels 12, which correspond one-to-one with the outlet holes 11; the multiple wire guide wheels 12 are coaxially arranged and rotatably connected to the frame 1.

[0030] The circulating spray mechanism 2 includes a liquid storage tank 21, a circulating pump 22, a spray pipe 23, and an electric heating box 26. The spray pipe 23 and the liquid storage tank 21 are located above and below the spray channel, respectively. One end of the circulating pump 22 is connected to the liquid storage tank 21, and the other end is connected to the spray pipe 23. The electric heating box 26 is installed on the pipeline between the liquid storage tank 21 and the circulating pump 22 and is used to heat and maintain the temperature of the water-based composite solution. The circulating pump 22 is used to draw the water-based composite solution heated at a constant temperature in the electric heating box 26 and deliver it to the spray pipe 23. The bottom of the spray pipe 23 is provided with spray holes, which are used to spray the water-based composite solution in the spray pipe 23 to spray the stainless steel wire in the spray channel below, and then return to the liquid storage tank 21.

[0031] There are multiple spray holes, which are evenly spaced along the length of the spray pipe 23; a sponge plate 24 is provided on the frame 1 below the spray pipe 23, and the lower end face of the sponge plate 24 abuts against the stainless steel wire on the spray channel.

[0032] On the frame 1, a plurality of sponge blocks 25 corresponding to the spray channels are provided behind the spray pipe 23. The sponge blocks 25 can be pre-wetted with a water-based composite solution. The sponge blocks 25 are provided with through grooves that run through their front and rear ends. The through grooves are used for the stainless steel wires on the corresponding spray channels to pass through. The inner diameter of the through grooves is smaller than the outer diameter of the stainless steel wires so that the sponge blocks 25 fit against the outer peripheral wall of the stainless steel wires.

[0033] The electric heating chamber 26 contains a heating cavity and a controller. The height of the heating cavity is lower than that of the storage tank 21 to facilitate the return flow of the water-based composite solution into the heating cavity (the height of the water-based composite solution in the heating cavity is no higher than 80% of the height of the heating cavity). The heating cavity contains an electric heating unit and a temperature control unit, both electrically connected to the controller. The electric heating unit heats the water-based composite solution in the heating cavity, while the temperature control unit detects the temperature of the water-based composite solution in the heating cavity and transmits the detection signal to the controller. The controller controls the switching of the electric heating unit. The electric heating unit can be an electric heating element powered by an external power source, while the temperature control unit can be a temperature sensor to monitor the temperature of the water-based composite solution in the heating cavity in real time.

[0034] This invention also provides a process for coating the surface of annealed stainless steel wire, comprising the following steps: First, the drawing powder and water are mixed in a specific ratio, placed in the heating chamber of an electric heating box, heated and kept at a constant temperature to form a stable suspension solution (i.e., a water-based composite solution); the concentration of the water-based composite solution is 0.5 as characterized by refractive index; the heating temperature of the water-based composite solution is 80-90℃, with 90℃ being the optimal constant temperature heating temperature.

[0035] Then, the annealed stainless steel wire passes through the outlet hole and spray channel. The circulation pump is started to draw water-based composite solution from the heating chamber and deliver it to the spray pipe. The water-based composite solution in the spray pipe is sprayed out through the spray hole and wets and penetrates the sponge plate below, performing a preliminary coating on the surface of the stainless steel wire. Excess water-based composite solution flows back to the storage tank below and is then recycled.

[0036] Next, the initially coated stainless steel wire is coated a second time by a sponge block soaked in a water-based composite solution, making the water-based composite solution on its surface more uniform.

[0037] Finally, the stainless steel wire, after being uniformly coated with the water-based composite solution twice, is taken to the take-up rack after passing through the wire reel. During this process and storage, the water in the water-based composite solution evaporates, and the wire drawing powder component forms a uniformly adhered and stable solid lubricating coating on the surface of the stainless steel wire.

[0038] The core of this invention lies in the online preparation and coating of a water-based composite solution, which allows the wire drawing powder to adhere in an optimal state, ultimately transforming it into a novel, in-situ generated composite coating. The wire drawing powder is a dry lubricant used when drawing stainless steel wire, also called wire drawing powder. Common components include calcium hydroxide, sodium hydroxide, stearic acid, animal and vegetable oils, paraffin wax, talc, industrial soap, and industrial alkali, and are generally classified into calcium-based and sodium-based types. The wire drawing powder in this invention can be a dry wire drawing lubricant produced by Kyoei Chemical Co., Ltd., or a commercially available stainless steel wire drawing powder.

[0039] The present invention provides an apparatus and process for coating the surface of annealed stainless steel wire, which realizes the generation of high-performance coating. By applying a warm solution online, the wire drawing powder particles can adhere more evenly and tightly to the surface of the wire. The resulting coating has a much stronger adhesion than that of simply applying dry powder or oil film, and its performance is more stable.

[0040] The coating of this invention provides excellent lubricity during take-up, ensuring a tight roll shape; after curing, it provides a moderate and consistent coefficient of friction, ensuring uniform tension and no dust shedding during the unwinding process for downstream customers, perfectly balancing the needs of take-up and unwinding.

[0041] This invention uses water as a medium, eliminating the risk of oil pollution. The solution can be recycled, minimizing waste and being environmentally friendly, with a clean and environmentally friendly process. By precisely controlling the solution concentration (refractive index), temperature, and coating amount, this invention can accurately regulate the thickness and performance of the final coating, meeting the needs of different customers. It offers good reproducibility and highly controllable coating performance.

[0042] The above description is merely a specific embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in the present invention should be included within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be determined by the scope of the claims.

Claims

1. An apparatus for coating the surface of annealed stainless steel wire, characterized in that: Includes a frame (1) and a circulating spraying mechanism (2) mounted on the frame (1); The frame (1) has a wire outlet hole (11) at one end and a wire guide wheel (12) at the other end. A spray channel for stainless steel wires to pass through is formed between the wire outlet hole (11) and the wire guide wheel (12). The circulating spray mechanism (2) includes a storage tank (21), a circulating pump (22), and a spray pipe (23). The spray pipe (23) and the storage tank (21) are located above and below the spray channel, respectively. One end of the circulating pump (22) is connected to the storage tank (21), and the other end is connected to the spray pipe (23). It is used to extract the water-based composite solution in the storage tank (21) and transport it to the spray pipe (23). The bottom of the spray pipe (23) is provided with a spray hole. The spray hole is used to spray the water-based composite solution in the spray pipe (23) to spray the stainless steel wire in the spray channel below, and then return it to the storage tank (21).

2. The apparatus for coating the surface of annealed stainless steel wire according to claim 1, characterized in that: There are multiple outlet holes (11), which are evenly spaced along the width direction of the frame (1); there are also multiple wire guide wheels (12), which are coaxially arranged and correspond one-to-one with the outlet holes (11).

3. The apparatus for coating the surface of annealed stainless steel wire according to claim 2, characterized in that: The spray holes are multiple and are evenly spaced along the length of the spray pipe (23); a sponge plate (24) is provided on the frame (1) below the spray pipe (23), and the lower end face of the sponge plate (24) abuts against the stainless steel wire on the spray channel.

4. The apparatus for coating the surface of annealed stainless steel wire according to claim 3, characterized in that: The frame (1) is provided with a plurality of sponge blocks (25) corresponding to the spray channels one by one at the position behind the spray pipe (23). The sponge blocks (25) are provided with through grooves that penetrate through their front and rear ends. The through grooves are used for the stainless steel wires on the corresponding spray channels to pass through. The inner diameter of the through grooves is smaller than the outer diameter of the stainless steel wires so that the sponge blocks (25) fit against the outer peripheral wall of the stainless steel wires.

5. The apparatus for coating the surface of annealed stainless steel wire according to claim 1, characterized in that: The circulating spray mechanism (2) also includes an electric heating box (26), which is installed on the pipeline between the liquid storage tank (21) and the circulating pump (22). The electric heating box (26) is provided with a heating chamber and a controller. The heating chamber is provided with an electric heating unit and a temperature control unit. The electric heating unit and the temperature control unit are electrically connected to the controller. The electric heating unit is used to heat the water-based composite solution in the heating chamber. The temperature control unit is used to detect the temperature of the water-based composite solution in the heating chamber and transmit the detection signal to the controller. The controller is used to control the switching of the electric heating unit.

6. A process for coating the surface of annealed stainless steel wire using the apparatus described in any one of claims 1-5, characterized in that: Includes the following steps, S1. The water-based composite solution is placed in the heating chamber of the electric heating box for heating and constant temperature control; S2. After annealing, the stainless steel wire passes through the outlet hole and spray channel. The circulation pump is started to draw water-based composite solution from the heating chamber and deliver it to the spray pipe. The water-based composite solution in the spray pipe is sprayed out through the spray hole and wets and penetrates the sponge plate below to preliminarily coat the surface of the stainless steel wire. Excess water-based composite solution flows back to the storage tank below and is then recycled. S3. The stainless steel wire with initial coating is coated a second time by a sponge block soaked in water-based composite solution to make the water-based composite solution on its surface more uniform. S4. The stainless steel wire coated with a water-based composite solution twice is taken to the take-up rack after passing through the wire reel. During this process and storage, the water in the water-based composite solution evaporates, and the wire drawing powder component forms a uniformly adhered and stable solid lubricating coating on the surface of the stainless steel wire.

7. The process for coating the surface of annealed stainless steel wire according to claim 6, characterized in that: In step S1, the water-based composite solution is a stable suspension solution formed by mixing drawing powder and water in a specific ratio, heating and controlling the temperature.

8. The process for coating the surface of annealed stainless steel wire according to claim 7, characterized in that: The heating temperature of the water-based composite solution is 80-90℃.

9. A process for coating the surface of annealed stainless steel wire according to claim 8, characterized in that: The heating temperature of the water-based composite solution is 90℃.

10. A process for coating the surface of annealed stainless steel wire according to claim 9, characterized in that: The concentration of the water-based composite solution, expressed as refractive index, is 0.5.