Lithium battery slurry high temperature coating die with built-in heating tube
By incorporating a built-in heating element and a micrometer adjustment mechanism, the problems of uneven heating and unstable material output in traditional lithium battery coating dies have been solved, achieving uniform coating and stable output of high-solids slurry.
Patent Information
- Application Number
- CN202611301871.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-24
AI Technical Summary
Traditional lithium battery coating dies cannot be adapted to high solids content slurries. External heating methods result in uneven temperature control, leading to low heating efficiency, uneven coating, and high discharge resistance, making it difficult to meet the stable coating requirements of high viscosity slurries.
The lithium battery slurry high-temperature coating die head with built-in heating tubes achieves precise control of heating uniformity and slurry thickness by setting multiple heating holes and thermocouple sensors on the rear side of the lower die, combined with a micrometer adjustment mechanism.
It significantly improves coating uniformity and stability, reduces slurry viscosity, ensures consistent coating thickness, and solves the problems of uneven heating and unstable material output of traditional dies.
Smart Images

Figure CN123149108A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of coating die technology, and in particular to a high-temperature coating die for lithium battery slurry with a built-in heating tube. Background Technology
[0002] Traditional lithium battery coating dies lack heating structures and are only suitable for low-to-medium solids content slurries applied at room temperature. These slurries have high solvent content, and heating the die can easily cause the solvent to evaporate rapidly, leading to slurry drying, blockage, particle formation, and coating defects. Therefore, the industry generally uses room temperature dies.
[0003] In contrast, high-solids lithium-ion battery slurries have an extremely low solvent content, and trace amounts of solvent evaporation will not cause the slurry to dry out. The die head can be directly heated at a constant temperature (around 80°C to improve fluidity). Existing room-temperature dies (around 25°C) and externally heated dies have low heating efficiency and uneven temperature control, making it difficult to reduce the viscosity of high-viscosity slurries and easily leading to problems such as high discharge resistance, uneven coating thickness, and numerous electrode particles. Therefore, it is necessary to use an internal heating tube close to the flow channel for heating, to stably reduce the slurry viscosity throughout the process, and to ensure uniform lateral discharge from the die lip. Based on the shortcomings of existing technologies, this invention proposes a high-temperature coating die head for lithium-ion battery slurries with an internal heating tube. Summary of the Invention
[0004] To address the aforementioned issues, this invention aims to provide a high-temperature coating die for lithium battery slurry with a built-in heating tube, which is suitable for slurries with high solids content, provides uniform heating, and can significantly improve coating uniformity and stability.
[0005] The technical solution of this invention is a high-temperature coating die head for lithium battery slurry with a built-in heating tube, including an upper die and a lower die, with a gasket between the upper die and the lower die, and the upper die and the lower die are locked by a locking screw. The lower die has a feeding channel in the middle of its rear side, a main cavity and a secondary cavity arranged along the width direction on the top surface of the middle part of the lower die, the secondary cavity being located in front of the main cavity, the feeding channel being connected to the main cavity, and a material extrusion channel being formed between the upper die and the lower die in front of the secondary cavity under the guidance of the gasket. The lower die has multiple heating holes and thermocouple sensors arranged in the front-rear direction on its rear side, the heating holes being located below the main cavity and containing heating tubes. A junction box is connected to the rear side of the lower die, and the junction box has a heating tube connector electrically connected to the heating tube and a thermocouple wire connector electrically connected to the thermocouple sensor.
[0006] Preferably, multiple heating tubes are arranged at intervals along the width direction at the same height of the lower mold; multiple thermocouple sensors are arranged at intervals along the width direction, and the thermocouple sensors are arranged on the lower mold at a position between the heating tubes and the main cavity.
[0007] Preferably, the width and depth of the main cavity are both greater than the depth and width of the secondary cavity.
[0008] Preferably, the junction box is connected to the junction box mounting block, and the junction box mounting block is connected to the rear side of the lower mold.
[0009] Preferably, the upper mold and the lower mold are connected to a back plate on their rear sides. The upper part of the back plate is connected to the rear side of the upper mold by screws, and the lower part of the back plate is connected to the rear side of the lower mold by screws.
[0010] Preferably, the bottom surface of the front area of the upper die is provided with an elongated adjustment groove along the width direction. The elongated adjustment groove is located above the material extrusion channel in front of the secondary cavity. The elongated adjustment groove is provided with a series of T-shaped adjustment blocks connected end to end. The top of the T-shaped adjustment block extends into a connecting rod. The connecting rod passes through the mounting hole of the upper die and is connected to a micrometer adjustment mechanism. The micrometer adjustment mechanism adjusts the lifting and lowering of the connecting rod to achieve fine adjustment of the T-shaped adjustment block up and down.
[0011] Preferably, the micrometer adjustment mechanism includes a micrometer screw lifting mechanism, wherein the lower end of the lifting screw of the micrometer screw lifting mechanism is connected to a coupling, the top of the connecting rod is connected inside the coupling, and the micrometer screw lifting mechanism is connected to the top surface of the upper mold through a fixing frame.
[0012] Preferably, a feeding pipe is connected to the middle of the rear side of the lower mold, and the feeding pipe is connected to the feeding channel.
[0013] This invention solves the technical problems of traditional room temperature dies being difficult to adapt to coating high solids content and high viscosity slurries, uneven temperature control of external heating methods, and low heating efficiency. It can adapt to high solids content slurries, and the heating method is uniform, which can significantly improve coating uniformity and coating stability. At the same time, the extrusion thickness of the slurry can be finely adjusted. Attached Figure Description
[0014] Figure 1 This is a schematic diagram of the structure of the present invention; Figure 2 for Figure 1 A structural diagram from another perspective; Figure 3 for Figure 1 Exploded view; Figure 4 for Figure 3 A structural diagram from another perspective; Figure 5 This is a cross-sectional view of the flow channel in this invention; Figure 6 This is a cross-sectional view of the center of the connecting rod in this invention; Wherein: 1—Upper mold; 1a—Long strip adjustment groove; 1b—Mounting hole; 2—Lower mold; 21—Feeding channel; 22—Main cavity; 23—Secondary cavity; 24—Heating hole; 25—Thermocouple sensor; 3—Gasket; 4—Mold locking screw; 5—Material extrusion channel; 6—Heating tube; 7—Gateway box; 71—Heating tube connector; 72—Thermocouple connector; 8—Gateway box mounting block; 9—Back plate; 10—T-type adjustment block; 12—Micrometer adjustment mechanism; 121—Micrometer screw lifting mechanism; 122—Lifting screw; 123—Coupling; 13—Fixed frame; 14—Feeding pipe. Detailed Implementation
[0015] The present invention will now be described in further detail with reference to the accompanying drawings.
[0016] like Figures 1 to 6 As shown, this invention provides a high-temperature coating die head for lithium battery slurry with a built-in heating tube, including an upper die 1 and a lower die 2. A gasket 3 is provided between the upper die 1 and the lower die 2. The upper die 1 and the lower die 2 are locked by a locking screw 4. The lower die 2 has a feeding channel 21 in the middle of its rear side. The top surface of the lower die 2 has a main cavity 22 and a secondary cavity 23 arranged along its width direction. The secondary cavity 23 is located in front of the main cavity 22. The feeding channel 21 and the main cavity 22 are connected. A material extrusion channel 5 is formed between the upper mold 1 and the lower mold 2 in front of the secondary cavity 23 under the guidance of the gasket 3. The lower mold 2 has multiple heating holes 24 and thermocouple sensors 25 arranged in the front-back direction on its rear side. The heating holes 24 are located below the main cavity 22 and have heating tubes 6 inside. A junction box 7 is connected to the rear side of the lower mold 2. The junction box 7 is provided with a heating tube connector 71 electrically connected to the heating tube 6 and a thermocouple wire connector 72 electrically connected to the thermocouple sensor 25.
[0017] In the above scheme, multiple heating tubes 6 are arranged at intervals along the width direction at the same height of the lower mold 2; multiple thermocouple sensors 25 are arranged at intervals along the width direction, and the thermocouple sensors 25 are arranged on the lower mold 2 between the heating tubes 6 and the main cavity 22. The interval arrangement of the heating tubes 6 achieves uniform heating of the entire lower mold 2, ensuring that the slurry can maintain a basically the same temperature in different areas inside the lower mold 2.
[0018] Specifically, the width and depth of the main cavity 22 are both greater than the depth and width of the secondary cavity 23.
[0019] Specifically, the junction box 7 is connected to the junction box mounting block 8, and the junction box mounting block 8 is connected to the rear side of the lower mold 2.
[0020] Specifically, the upper mold 1 and the lower mold 2 are connected to the rear side of a back plate 9. The upper part of the back plate 9 is connected to the rear side of the upper mold 1 by screws, and the lower part of the back plate 9 is connected to the rear side of the lower mold 2 by screws.
[0021] Specifically, the bottom surface of the front area of the upper mold 1 is provided with a long strip-shaped adjustment groove 1a along the width direction. The long strip-shaped adjustment groove 1a is located above the material extrusion channel 5 in front of the secondary cavity 23. The long strip-shaped adjustment groove 1a is provided with a series of T-shaped adjustment blocks 10 connected end to end. The top of the T-shaped adjustment block 10 extends out of the connecting rod. The connecting rod passes through the mounting hole 1b of the upper mold 1 and is connected to a micrometer adjustment mechanism 12. The micrometer adjustment mechanism 12 adjusts the connecting rod to achieve fine up and down adjustment of the T-shaped adjustment block 10.
[0022] Specifically, the micrometer adjustment mechanism 12 includes a micrometer screw lifting mechanism 121. The lower end of the lifting screw 122 of the micrometer screw lifting mechanism 121 is connected to a coupling 123. The top of the connecting rod is connected inside the coupling 123. The micrometer screw lifting mechanism 121 is connected to the top surface of the upper mold 1 through a fixing frame 13.
[0023] Specifically, a feed pipe 14 is connected to the middle of the rear side of the lower mold 2, and the feed pipe 14 is connected to the feed channel 21.
[0024] In this invention, the structure of the micrometer screw lifting mechanism 121 is consistent with the screw lifting structure of a micrometer in the prior art, and the detailed structure will not be described again here. Input is obtained by rotating the knob at the tail end, which is then transmitted through the internal screw and nut mechanism to convert the screw at the front end into a micrometer-level precise linear motion. This ultimately achieves a 10-micrometer-level lifting adjustment for each T-shaped adjusting block, thereby adjusting the thickness of the slurry in the corresponding area.
[0025] The slurry enters the feed channel 21 through the feed pipe 14, enters the main cavity 22 for buffering and pressure adjustment, and enters the secondary cavity 23 for further buffering under the guidance of the gasket 3. It continues to enter the material extrusion channel 5 under the guidance of the gasket 3, and the slurry thickness at the corresponding width position is adjusted by the T-shaped adjusting block 10 and the micrometer adjusting mechanism 12, and finally shaped and extruded from the die lip.
[0026] The above description is merely a preferred embodiment of the present invention and is not intended to limit the invention in any way. Any simple modifications, equivalent changes, or alterations made to the above embodiments based on the technical principles of the present invention shall still fall within the scope of the technical solution of the present invention.
Claims
1. A high-temperature coating die head for lithium battery slurry with a built-in heating tube, comprising an upper die (1) and a lower die (2), wherein a gasket (3) is provided between the upper die (1) and the lower die (2), and the upper die (1) and the lower die (2) are locked by a locking screw (4), characterized in that: The lower die (2) has a feeding channel (21) in the middle of its rear side. The top surface of the lower die (2) has a main cavity (22) and a secondary cavity (23) in the width direction. The secondary cavity (23) is located in front of the main cavity (22). The feeding channel (21) and the main cavity (22) are connected. The upper die (1) and the lower die (2) in front of the secondary cavity (23) form a material extrusion channel (5) under the guidance of the gasket (3). The lower die (2) has multiple heating holes (24) and thermocouple sensors (25) arranged in the front-back direction on its rear side. The heating holes (24) are located below the main cavity (22) and have heating tubes (6) inside. The lower die (2) is connected to a junction box (7). The junction box (7) has a heating tube connector (71) electrically connected to the heating tube (6) and a thermocouple wire connector (72) electrically connected to the thermocouple sensor (25).
2. The lithium battery slurry high-temperature coating die head with built-in heating tube according to claim 1, characterized in that: Multiple heating tubes (6) are arranged at intervals along the width direction at the same height of the lower mold (2); multiple thermocouple sensors (25) are arranged at intervals along the width direction, and the thermocouple sensors (25) are arranged on the lower mold (2) at the position between the heating tubes (6) and the main cavity (22).
3. A high-temperature coating die for lithium battery slurry with a built-in heating tube according to claim 1, characterized in that: The width and depth of the main cavity (22) are both greater than the depth and width of the secondary cavity (23).
4. A high-temperature coating die for lithium battery slurry with a built-in heating tube according to claim 1, characterized in that: The junction box (7) is connected to the junction box mounting block (8), which is connected to the rear side of the lower mold (2).
5. A high-temperature coating die for lithium battery slurry with a built-in heating tube according to claim 1, characterized in that: The upper mold (1) and the lower mold (2) are connected to a back plate (9) on their rear sides. The upper part of the back plate (9) is connected to the rear side of the upper mold (1) by screws, and the lower part of the back plate (9) is connected to the rear side of the lower mold (2) by screws.
6. A high-temperature coating die for lithium battery slurry with a built-in heating tube according to claim 1, characterized in that: The bottom surface of the front area of the upper mold (1) is provided with a long strip-shaped adjustment groove (1a) along the width direction. The long strip-shaped adjustment groove (1a) is located above the material extrusion channel (5) in front of the secondary cavity (23). The long strip-shaped adjustment groove (1a) is provided with a series of T-shaped adjustment blocks (10) connected end to end. The top of the T-shaped adjustment block (10) extends out of the connecting rod. The connecting rod passes through the mounting hole (1b) of the upper mold (1) and is connected to a micrometer adjustment mechanism (12). The micrometer adjustment mechanism (12) adjusts the connecting rod to achieve fine adjustment of the T-shaped adjustment block (10) up and down.
7. A high-temperature coating die for lithium battery slurry with a built-in heating tube according to claim 6, characterized in that: The micrometer adjustment mechanism (12) includes a micrometer screw lifting mechanism (121). The lower end of the lifting screw (122) of the micrometer screw lifting mechanism (121) is connected to a coupling (123). The top of the connecting rod is connected inside the coupling (123). The micrometer screw lifting mechanism (121) is connected to the top surface of the upper mold (1) through a fixing frame (13).
8. A high-temperature coating die for lithium battery slurry with a built-in heating tube according to claim 1, characterized in that: The lower mold (2) is connected to the middle of the rear side of the feed pipe (14), and the feed pipe (14) is connected to the feed channel (21).