A high performance corrosion protection system and method

The corrosion problem of the desulfurization tower tank was solved by using a high-performance anti-corrosion construction system. The multi-layer anti-corrosion structure and zoned matching materials improved the corrosion resistance and safety of the equipment.

CN123149113APending Publication Date: 2026-11-24BEIXIN BUILDING MATERIALS (JINGGANGSHAN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611226529.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-13
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In wet flue gas desulfurization systems, the desulfurization tower tank is susceptible to severe corrosion due to factors such as high-temperature raw flue gas, strong acidic media, and equipment start-up and shutdown stress. This can lead to pitting corrosion and perforation of the substrate, affecting equipment safety and maintenance costs.

Method used

A high-performance anti-corrosion construction system is adopted, including units such as substrate pretreatment, material mixing, primer coating, flake mortar lining and topcoat protection. Combined with zone-adaptive anti-corrosion materials, a multi-layer anti-corrosion structure is formed to adapt to the corrosion characteristics of different areas.

Benefits of technology

This improved the corrosion resistance of the desulfurization tower tank, reduced the risk of equipment failure and maintenance costs, and ensured the safety and stability of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149113A_ABST
    Figure CN123149113A_ABST
Patent Text Reader

Abstract

This invention relates to the field of equipment corrosion protection construction technology, specifically disclosing a high-performance corrosion protection construction system and method. The system comprises six major units: substrate pretreatment, material mixing, primer coating, flake mortar lining, topcoat protection, and zoned matching of anti-corrosion materials. During construction, the substrate is sandblasted to Sa3 grade with a roughness of 40-70μm; the primer, mortar, and topcoat are all mixed with curing agent at a ratio of 100:2; the mortar is automatically mixed and applied in two coats with a total thickness of 2mm, and then degassed using a solvent roller; finally, special mortar materials are matched according to different corrosion areas such as the high-temperature flue of the desulfurization equipment and the alternating wet and dry zones. This invention combines full-process construction with zoned corrosion protection, improving the impermeability, thermal stability, and durability of the lining, and extending the service life of the equipment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of equipment corrosion protection construction technology, and specifically to a high-performance corrosion protection construction system and method. Background Technology

[0002] Wet flue gas desulfurization (FGD) systems are the core equipment for controlling sulfur dioxide emissions in industrial waste gas. This system works by bringing an alkaline absorbent (such as limestone slurry) into countercurrent contact with high-temperature flue gas within an absorption tower, causing the sulfur dioxide in the flue gas to dissolve and react to form gypsum.

[0003] However, the operating environment of this process is extremely harsh: the highly acidic medium carried by the high-temperature flue gas, the high-velocity scouring during slurry circulation, and the thermal expansion and contraction stress caused by equipment start-up and shutdown all contribute to a complex corrosion system. Especially for carbon steel towers and tanks, once the anti-corrosion coating fails, it can easily lead to pitting corrosion, perforation, or even structural damage, causing companies to face production stoppage risks and high maintenance costs. Therefore, anti-corrosion treatment is necessary for the inner surface of the desulfurization tower tanks. Summary of the Invention

[0004] The purpose of this invention is to provide a high-performance anti-corrosion construction system and method to solve the technical problem of corrosion in desulfurization tower tanks.

[0005] To solve the above-mentioned technical problems, the present invention specifically provides the following technical solution:

[0006] A high-performance anti-corrosion construction system includes a substrate pretreatment unit, a material mixing unit, a primer coating unit, a flake putty lining unit, a topcoat protection unit, and a zoned adaptive anti-corrosion material component.

[0007] The substrate pretreatment unit includes a dry compressed air supply device, a quartz sand / steel shot blasting hopper, grinding tools, and a dust removal device; the compressed air pressure is 0.5~0.6MPa and is oil-free and water-free; the blasting material consists of quartz sand and steel shot, and the overall moisture content of the sand is <1%;

[0008] The material mixing unit is equipped with an independent workstation and a material conveying docking channel. The workstation is used to assemble a glass flake clay mixing device, which can realize automated mixing of flake clay; other materials are mixed manually.

[0009] The primer coating unit is equipped with vinyl ester glass flake primer, organic peroxide curing agent 328E, and brushing tools. The primer to curing agent ratio is 100:2.

[0010] The flake mortar lining unit includes phenolic epoxy vinyl ester flake mortar, curing agent, trowel, wool felt roller, and styrene solvent. The ratio of mortar to curing agent is 100:2, and each batch of mortar must be mixed within 30 minutes for application.

[0011] The topcoat protective unit is equipped with a vinyl ester glass flake topcoat, which contains defoamers, liquid waxes, and thixotropic additives.

[0012] The partitioned corrosion-resistant material components include high-temperature phenolic epoxy vinyl ester flake mortar, high-temperature wear-resistant flake mortar, medium-temperature wear-resistant flake mortar, and standard medium-temperature flake mortar, which are respectively adapted to the four types of corrosion areas of the desulfurization tower: high-temperature flue, dry-wet alternating zone, spray scouring zone, and clean flue.

[0013] Furthermore, the material mixing unit includes a cylinder, a drive motor, a mixing mechanism disposed inside the cylinder, a storage mechanism located below the cylinder, and a defoaming component disposed between the cylinder and the storage mechanism;

[0014] The stirring mechanism has a gear set located at the top of the cylinder. The gear set consists of a driving gear located at the center and several driven gears arranged around the driving gear. The motor is connected to the driving gear in a transmission connection. The driving gear meshes with the driven gears to transmit power to each driven gear.

[0015] The drive gear is coaxially connected to a first rotating shaft below it, and a second rotating shaft and a third rotating shaft are sequentially connected to the first rotating shaft; wherein, the first rotating shaft is provided with a stirring blade, the second rotating shaft is provided with a frame-type stirring blade, and the third rotating shaft is provided with a spiral blade.

[0016] The driven gear is connected only to the first rotating shaft and the corresponding stirring blade below it;

[0017] The first, second, and third rotating shafts below the driving gear are coaxially arranged in the vertical direction to form a central stirring assembly; the first rotating shaft below the driven gear forms a peripheral stirring assembly; the central stirring assembly and the peripheral stirring assembly operate synchronously in opposite directions within the cylinder.

[0018] Furthermore, the cylinder includes an outer shell and an inner shell, with an insulation interlayer formed between the outer shell and the inner shell; the insulation interlayer is filled with insulation material, or the insulation interlayer is configured as a flow channel that allows heating or cooling media to pass through, so as to regulate the material temperature inside the inner shell.

[0019] Furthermore, the cylinder also includes a top cover with a feed inlet; the inner shell defines an upper cavity for containing materials and a lower cavity located below the upper cavity, the lower cavity having a funnel-shaped contraction structure.

[0020] Furthermore, the bottom of the lower cavity is connected to a discharge port, and an output pipe is connected below the discharge port. The end of the output pipe is provided with an output port. The spiral blades on the third rotating shaft extend to the area of ​​the lower cavity and the output pipe to assist in conveying the material to the discharge port.

[0021] Furthermore, the storage mechanism includes a receiving cavity that communicates with the output port; the bottom inner wall of the receiving cavity is configured as a slope that extends obliquely toward the side away from the output port.

[0022] Furthermore, a sliding cover is provided on one side of the storage mechanism, which is used to close or open the side opening of the receiving cavity.

[0023] A high-performance anti-corrosion construction method, using the high-performance anti-corrosion construction system described in claim 1, includes the following steps:

[0024] S1 Substrate Sandblasting and Rust Removal Pretreatment: Grinding removes weld slag and protruding structures; dry sandblasting treats the steel surface to achieve a rust removal grade of GB8923-88 Sa3, with a substrate roughness of 40~70μm; quartz sand particle size 1~3.2mm, with 1~1.5mm particle size accounting for ≥40%; steel shot particle size 0.63~1.6mm, with 0.63~0.8mm particle size accounting for ≥40%; sand moisture content <1%.

[0025] S2 Anti-corrosion material mixing and preparation: The ratio of primer, flake putty, topcoat and hardener is 100:2; the flake putty is mixed using a glass flake putty mixing device installed in the material mixing unit; other materials are mixed manually.

[0026] S3 Primer Application: Take the mixed primer and apply one coat to seal the substrate.

[0027] S4 flake putty lining construction: Take the mixed flake putty and apply it within 30 minutes. The thickness of a single coat of putty is 1mm. Under normal working conditions, two coats are applied with a total thickness of 2mm. Before the putty initially sets, use styrene solvent to impregnate wool felt and roll it to remove air. For multi-layer construction, use an overlapping process. After sanding the defective areas to create a slope transition, reapply the primer and putty.

[0028] S5 Topcoat Application: After the flake putty has fully cured, take the mixed topcoat and apply a layer to the entire surface.

[0029] Furthermore, the anti-corrosion method adopts differentiated anti-corrosion for different areas: high-temperature flue uses high-temperature phenolic epoxy vinyl ester flake mortar; dry and wet alternating areas use high-temperature wear-resistant flake mortar; spray rinsing areas use medium-temperature wear-resistant flake mortar combined with wear-resistant topcoat; and clean flue uses standard medium-temperature wear-resistant flake mortar lining.

[0030] Furthermore, in step S2, the glass flake putty mixing device can be integrated into the material mixing unit, and the mixed material can be directly transported to the S4 construction station via pipeline.

[0031] Compared with the prior art, this application has the following advantages:

[0032] In this invention, the system utilizes a dry and clean sandblasting medium to ensure the stability of the substrate surface. Automated mixing ensures uniform mixing and consistent application of the mortar. Combined with a labyrinthine barrier structure formed by glass flakes and a high-temperature resistant resin matrix, the lining's impermeability and thermal stability are enhanced, creating a multi-layered anti-corrosion structure. Simultaneously, specialized materials are matched according to the corrosion characteristics of different areas to achieve compatibility between the anti-corrosion layer and the desulfurization environment. By integrating substrate pretreatment, material mixing, primer coating, flake mortar lining, and topcoat protection with zoned anti-corrosion measures, the entire process of the desulfurization tower, from surface treatment to anti-corrosion layer formation, is fully controlled. Attached Figure Description

[0033] To more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are merely exemplary, and those skilled in the art can derive other embodiments based on the provided drawings without creative effort.

[0034] Figure 1 This is a schematic diagram of the anti-corrosion construction method according to an embodiment of the present invention.

[0035] Figure 2 This is a schematic diagram of the anti-corrosion construction system according to an embodiment of the present invention.

[0036] Figure 3 This is a schematic diagram of the partitioned adaptation anti-corrosion material according to an embodiment of the present invention.

[0037] Figure 4 This is a schematic diagram of the desulfurization tower partitioning according to an embodiment of the present invention.

[0038] Figure 5 This is a schematic diagram of the overall structure of an embodiment of the present invention.

[0039] Figure 6 This is a top view of the structure according to an embodiment of the present invention.

[0040] Figure 7 Embodiments of the present invention Figure 3 A schematic diagram of the AA cross-section.

[0041] Figure 8 This is a schematic diagram of the cylinder and stirring mechanism according to an embodiment of the present invention.

[0042] Figure 9 This is a schematic diagram of the overall stirring mechanism according to an embodiment of the present invention.

[0043] Figure 10 This is a schematic diagram of the top cover flushing hole structure according to an embodiment of the present invention.

[0044] Figure 11 Embodiments of the present invention Figure 4 Enlarged view of section A.

[0045] Figure 12 Embodiments of the present invention Figure 5 Enlarged view of section B in the middle.

[0046] The labels in the diagram represent the following:

[0047] 1. Substrate pretreatment unit; 2. Material mixing unit; 3. Primer coating unit; 4. Flake putty lining unit; 5. Topcoat protection unit; 6. Zoned adaptive anti-corrosion material components;

[0048] 21. Cylinder body; 22. Motor; 23. Stirring mechanism; 24. Storage mechanism; 25. Defoaming component;

[0049] 211. Outer shell; 212. Inner shell; 213. Insulation layer; 214. Upper cavity; 215. Lower cavity; 216. Discharge port; 217. Output pipe; 218. Output port; 219. Top cover; 2110. Flushing hole; 2111. Feed inlet; 231. Gear set; 232. First rotating shaft; 233. Stirring blade; 234. Second rotating shaft; 235. Frame-type stirring blade; 236. Third rotating shaft; 237. Spiral blade; 241. Inclined ramp; 242. Receiving cavity; 243. Sliding cover; 251. Through hole.

[0050] 601. High-temperature flue; 602. Dry and wet alternation zone; 603. Spray flushing zone; 604. Clean flue. Detailed Implementation

[0051] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0052] This invention discloses a high-performance anti-corrosion construction system, such as... Figures 1 to 4As shown, it includes a substrate pretreatment unit 1, a material mixing unit 2, a primer coating unit 3, a flake mortar lining unit 4, a topcoat protection unit 5, and a zoned adaptive anti-corrosion material component 6. Each unit is structurally independent but functionally connected, forming a complete anti-corrosion construction system that can achieve standardized management and control of the entire anti-corrosion construction process of the desulfurization tower.

[0053] Currently, most gypsum board production lines use coal-fired heat sources and are equipped with limestone-gypsum wet desulfurization processes, which account for about 85% of applications. The desulfurization towers are mostly made of iron tanks, which are exposed to strong acid and alkali environments for a long time, making them prone to corrosion and damage, leading to equipment failures, production stoppages, and safety hazards. This system solves the corrosion problem of desulfurization tower tanks by relying on the cooperation of various functional units.

[0054] The substrate pretreatment unit 1 includes a dry compressed air supply device, a quartz sand / steel shot blasting hopper, grinding tools, and a dust cleaning device; the compressed air pressure is 0.5~0.6MPa and is oil-free and water-free; the blasting material is divided into quartz sand and steel shot, and the overall moisture content of the sand is <1%.

[0055] This unit serves as the front-end foundation structure of the entire anti-corrosion construction system. By configuring specialized equipment and defining specific media parameters, it provides a qualified substrate surface for the subsequent adhesion of the anti-corrosion layer.

[0056] Based on the structural configuration of substrate pretreatment unit 1, this system performs step S1 substrate sandblasting and rust removal pretreatment: grinding to remove weld slag and protruding structures, dry sandblasting treatment of the steel surface, achieving a rust removal grade of GB8923-88 Sa3, substrate roughness 40~70μm; quartz sand particle size 1~3.2mm, 1~1.5mm particle size ≥40%; steel shot particle size 0.63~1.6mm, 0.63~0.8mm particle size ≥40%, sand moisture content <1%; after sandblasting, in any 100mm×100mm area on the substrate surface, the residual rust spots and oxide scale discoloration area does not exceed 5%.

[0057] During the pretreatment process, it is necessary to thoroughly grind and remove weld beads, weld slag, and spatter from the substrate surface, smooth the weld seam and uneven structure, and ensure that the construction base surface is regular.

[0058] The material mixing unit 2 is equipped with an independent workstation and a material conveying docking channel. The workstation is used to assemble a glass flake mortar mixing device, which can realize automated mixing of flake mortar; other materials are mixed manually.

[0059] This unit adopts a zoned mixing structure design, which distinguishes the mixing mode of flake mortar from that of ordinary materials. The unit is reserved with a material conveying docking channel to enable the linkage between the mixing station and the construction station.

[0060] Specifically, such as Figures 5 to 12As shown, the material mixing unit 2 includes a cylinder 21, a drive motor 22, a mixing mechanism 23 disposed inside the cylinder 21, a storage mechanism 24 located below the cylinder 21, and a defoaming component 25 disposed between the cylinder 21 and the storage mechanism 24.

[0061] To adapt to the temperature control requirements under different operating conditions, such as Figure 7 and Figure 11 The cylinder 21 adopts a double-layer structure. The cylinder 21 includes an outer shell 211 and an inner shell 212, with an insulation interlayer 213 formed between the outer shell 211 and the inner shell 212. Both the outer shell 211 and the inner shell 212 are made of corrosion-resistant stainless steel, and the insulation interlayer 213 has a radial thickness set according to the insulation requirements.

[0062] Furthermore, the insulation jacket 213 is filled with insulation material, or the insulation jacket 213 is configured as a flow channel that allows the heating medium or cooling medium to pass through, thereby regulating the material temperature inside the inner shell 212.

[0063] Specifically, when the insulation interlayer 213 is filled with insulation material, polyurethane foam or rock wool is selected as the insulation material; when the insulation interlayer 213 is constructed as a medium flow channel, a spiral guide plate is provided inside, hot water or heat transfer oil is used as the heating medium, and cold water or ethylene glycol solution is used as the cooling medium. The inlet and outlet of the insulation interlayer 213 are connected to the external constant temperature circulation unit through flanges and pipelines, respectively. By controlling the medium temperature, the temperature of the mortar material in the inner shell 212 is kept within the temperature range suitable for construction, preventing the mortar from prematurely gelling and curing due to excessive temperature.

[0064] Meanwhile, the cylinder 21 also includes a top cover 219, on which a feed inlet 2111 is provided for material to be added. The feed inlet 2111 is equipped with a flip-up locking sealing cap, which is closed during the stirring process to prevent material from splashing out and solvent from evaporating.

[0065] Specifically, the inner shell 212 defines an upper cavity 214 for containing materials and a lower cavity 215 located below the upper cavity 214. The cylindrical section of the upper cavity 214 and the conical section of the lower cavity 215 have a smooth arc transition, with no dead angles for flow.

[0066] To guide the material to be discharged in a concentrated manner, the lower cavity 215 has a funnel-shaped converging structure. The bottom of the lower cavity 215 is connected to the discharge port 216, and the discharge pipe 217 is connected below the discharge port 216. The end of the discharge pipe 217 is provided with an discharge port 218.

[0067] In order to achieve multi-stage compound mixing and ensure that all mixing components work together, the mixing mechanism 23 has a gear set 231 set on the top of the cylinder 21.

[0068] like Figure 8 and Figure 9 As shown, the gear set 231 consists of a centrally located driving gear and several driven gears arranged around the driving gear. The motor 22 is connected to the driving gear, and the driving gear meshes with the driven gears to transmit power to each driven gear. Thus, the first rotating shaft 232 below the driving gear and the first rotating shaft 232 below the driven gears receive power.

[0069] In this embodiment, there are multiple driven gears arranged symmetrically, and the gear ratio between the driving gear and the driven gear is set so that the central stirring component and the peripheral stirring components run synchronously at the same speed but in opposite directions. The drive motor 22 is a variable frequency geared motor, and the output speed can be steplessly adjusted within a certain range to adapt to the stirring requirements of mortars of different viscosities.

[0070] A first rotating shaft 232 is coaxially connected below the drive gear, and a second rotating shaft 234 and a third rotating shaft 236 are sequentially connected to the first rotating shaft 232. The first rotating shaft 232 is provided with a stirring blade 233, the second rotating shaft 234 is provided with a frame-type stirring blade 235, and the third rotating shaft 236 is provided with a spiral blade 237.

[0071] The first rotating shaft 232, the second rotating shaft 234 and the third rotating shaft 236 below the drive gear are coaxially arranged in the vertical direction to form a central stirring assembly.

[0072] The driven gear is connected only to the first rotating shaft 232 and the corresponding stirring blade 233.

[0073] The first rotating shaft 232 below the driven gear constitutes the peripheral stirring assembly.

[0074] Through the meshing transmission of the driving gear and the driven gear, the central stirring component and the peripheral stirring component operate synchronously in opposite directions inside the cylinder 21, thereby forming a stirring field that combines shearing and wall sweeping inside the cylinder.

[0075] To prevent material from adhering to the cylinder wall, the outer contour of the frame-type stirring blade 235 is adapted to the inner wall contour of the inner shell 212 and is positioned close to the inner wall of the inner shell 212. This structure continuously scrapes the inner wall during operation, reducing material adhesion. A small operating gap is maintained between the scraper blades on the frame-type stirring blade 235 and the inner wall of the inner shell 212, ensuring that the adhering sludge is effectively scraped off without damaging the inner wall of the cylinder.

[0076] To overcome the difficulty in feeding the viscous mortar, the spiral blades 237 on the third rotating shaft 236 extend to the area of ​​the lower cavity 215 and the output pipe 217 to assist in conveying the material to the discharge port 216. This spiral pushing structure can directly force the material towards the discharge port, avoiding blockage.

[0077] During the material discharge process, in order to eliminate air bubbles entrained by the agitation, such as Figure 8 and Figure 12 The defoaming component 25 is disposed inside the discharge port 216. The defoaming component 25 includes a plate body, each plate body having several through holes 251. The plate body is a detachable multi-layer sieve plate structure, with the through holes 251 of adjacent sieve plates staggered. When the material flows through the through holes 251, it is subjected to repeated shearing and compression, causing the internal bubble walls to rupture and the gas to escape, thus completing the defoaming process.

[0078] The discharged material enters storage mechanism 24. For example... Figure 6 and Figure 4 The storage mechanism 24 includes a receiving cavity 242, which communicates with the output port 218. To facilitate the accumulation and retrieval of materials within the receiving cavity, the bottom inner wall of the receiving cavity 242 is configured as a ramp 241, which extends inclinedly towards the side away from the output port 216. Furthermore, a sliding cover 243 is provided on one side of the storage mechanism 24, which is used to close or open the side opening of the receiving cavity 242 to facilitate material output or temporary storage.

[0079] To prevent material from prematurely flowing out of the outlet 218 without being fully mixed during the mixing process, an openable and closable sealing structure (such as a gate valve or sealing cap, not shown in the figure) can be provided at the outlet 218. During the mixing process, the sealing structure remains closed to prevent material from flowing out prematurely; after the mixing is completed, the sealing structure opens, and the material is discharged through the outlet 218 to the storage mechanism 24.

[0080] Because the putty is sticky, it is difficult to clean the inside. Figure 10 A flushing hole 2110 is also provided on the top cover 219 for injecting cleaning fluid into the upper cavity 214. A rotating spray head is provided at the inner end of the flushing hole 2110, and the outer end is connected to the high-pressure cleaning fluid supply system through a pipeline.

[0081] After the stirring device is used, the inside of the cylinder 21 can be rinsed with high-pressure cleaning fluid. Rotating the spray head can expand the spray range of the cleaning fluid and improve the cleaning effect.

[0082] Based on the structural characteristics of the material mixing unit 2, this system performs step S2, mixing and preparing anti-corrosion materials: the ratio of primer, flake putty, topcoat and curing agent is 100:2; the flake putty is mixed using a glass flake putty mixing device assembled in the material mixing unit; other materials are mixed manually.

[0083] In step S2, the glass flake putty mixing device can be integrated into the material mixing unit, and the mixed material is directly transported to the S4 construction station through pipeline.

[0084] The primer coating unit 3 is equipped with vinyl ester glass flake primer, organic peroxide curing agent 328E, and a brush tool. The primer to curing agent ratio is 100:2. The primer uses vinyl ester resin as the base, fills with mica powder, and adds coupling agents and accelerators to wet the substrate, seal and prevent rust, and improve the adhesion of the putty.

[0085] Specifically, the primer contains no glass flake components, has low viscosity, and can deeply wet steel substrates. Its internal coupling agents, accelerators, and other additives, combined with mica powder fillers, can fill the capillary pores of the substrate and form a tightly sealed bottom layer.

[0086] Based on the supporting structure of primer coating unit 3, this system performs step S3 primer application: taking the stirred primer, one coat of primer is applied to seal the substrate. This step relies on the standardized mixing ratio and material structure of the primer coating unit to form a sealed bottom layer on the substrate surface, providing an adhesion base for the flake mortar lining construction.

[0087] Unit 4, the flake mortar lining unit, comprises phenolic epoxy vinyl ester flake mortar, a hardener, a trowel, a felt roller, and styrene solvent. The mortar and hardener are mixed in a 100:2 ratio, and each batch of mixed slurry must be applied within 30 minutes. The flake mortar is filled with multiple layers of parallel glass flakes, forming a labyrinthine barrier structure. The phenolic epoxy vinyl ester matrix can withstand high temperatures of 90~180℃ for extended periods, and the lining layer possesses toughness to offset thermal stress caused by temperature changes in the equipment.

[0088] During the operation of the desulfurization tower, the flue gas contains acidic corrosive media such as SO2 and HCl, and there are temperature alternation conditions. The glass flakes arranged in parallel and overlapping manner inside the mortar can form a multi-level physical barrier, prolong the penetration path of the corrosive media, form a labyrinth effect, and prevent the acidic media from penetrating the substrate.

[0089] This unit integrates the main material of the putty, curing agent, construction tools and auxiliary solvents to form an integrated lining construction structure. The filler and resin matrix structure of the putty itself can improve the impermeability and thermal stability of the lining, and build the core barrier protection structure of the anti-corrosion system, undertaking the main anti-corrosion defense function.

[0090] Based on the structural configuration of the flake mortar lining unit 4, this system performs step S4 flake mortar lining construction: take the mixed flake mortar, complete the application within 30 minutes, with a single coat thickness of 1mm, and two coats for a total thickness of 2mm under normal working conditions; before the mortar initially sets, use styrene solvent to impregnate wool felt and roll it to remove air; for multi-layer construction, use an overlapping process, and after sanding the slope transition at the defective areas, reapply the primer and mortar.

[0091] The lining repair method in step S4 is as follows: When the lining contains impurities, grind it with a grinding wheel to create a sloped transition, clean it with solvent, and then apply primer and putty. For areas where the lining is missed or the thickness is insufficient, clean it with solvent, dry it, and then apply putty to the designed thickness. During construction, the surface must be kept clean, and protrusions and drips must be removed by grinding in a timely manner. When applying multiple layers, end joints are strictly prohibited; overlapping is required to ensure the overall continuity of the lining.

[0092] The labyrinth barrier structure formed by glass flakes and the high-temperature resistant resin matrix further optimize the protective performance of the lining, enhance the overall anti-corrosion structure's resistance to penetration and temperature changes, and adapt to the complex acid and alkali corrosion and temperature alternation conditions of the desulfurization tower.

[0093] The topcoat protection unit 5 is equipped with a vinyl ester glass flake topcoat, which contains defoamer, liquid wax, and thixotropic agent. The topcoat uses vinyl ester resin as the base and adds mica powder, color paste, defoamer, thixotropic agent, liquid wax, and accelerator as functional fillers and additives. The curing agent is an organic peroxide.

[0094] As the surface protective structure of the anti-corrosion system, the topcoat comes into direct contact with the corrosive flue gas medium inside the desulfurization tower. Liquid wax additives can give the topcoat air-drying properties, resulting in a smooth and dense surface after molding. Defoamers and thixotropic agents can optimize the topcoat's application and molding effect, preventing surface defects such as pores and sagging. Mica powder and color paste can improve the topcoat's weather resistance and structural density.

[0095] This unit uses a special topcoat and multiple additives to form a surface protection structure. The resin matrix and functional filler combination structure of the topcoat can provide full coverage protection for the internal mortar lining, preventing external corrosive media from directly scouring and eroding the mortar lining.

[0096] Based on the structural configuration of the topcoat protection unit 5, this system performs step S5 topcoat application: after the flake mortar has fully cured, a layer of the mixed topcoat is applied to the entire surface. This step forms a surface protective structure after the mortar core lining has cured, forming a hierarchical combination with the bottom primer and the middle mortar lining to construct a multi-layered anti-corrosion structure that seals the substrate, blocks the medium, and protects the surface.

[0097] like Figure 3 and Figure 4 The partitioned adaptive anti-corrosion material component 6 includes high-temperature phenolic epoxy vinyl ester flake mortar, high-temperature wear-resistant flake mortar, medium-temperature wear-resistant flake mortar, and standard medium-temperature wear-resistant flake mortar, respectively adapted to four types of corrosion zones in the desulfurization tower: high-temperature flue 601, wet-dry alternating zone 602, spray scouring zone 603, and clean flue 604. This component adopts a partitioned matching material structure design, differing from the traditional construction structure of uniform anti-corrosion materials. It can be specifically adapted to the corrosion conditions of different areas of the desulfurization tower, achieving adaptation of the anti-corrosion layer to the desulfurization environment.

[0098] Furthermore, this system employs differentiated anti-corrosion methods for different zones: high-temperature flue 601 uses high-temperature phenolic epoxy vinyl ester flake mortar; the alternating wet and dry zone 602 uses high-temperature wear-resistant flake mortar; the spray scouring zone 603 uses medium-temperature wear-resistant flake mortar combined with a wear-resistant topcoat; and the clean flue 604 uses standard medium-temperature wear-resistant flake mortar lining. Based on the actual operating principle of the desulfurization tower, the high-temperature raw flue gas from the boiler enters the absorption tower after dust removal and heat exchange pretreatment, where it reacts counter-currently with limestone slurry. During this process, different operating conditions exist, including high-temperature scouring, alternating wet and dry conditions, and acidic medium spray corrosion. The corrosion mechanisms and intensity vary in each zone.

[0099] By combining the anti-corrosion material components with the structure of each construction unit in a zoned manner, and specifically matching the working conditions of each area, the unit of substrate pretreatment, material mixing, primer coating, flake mortar lining and topcoat protection is combined with zoned anti-corrosion, realizing full-process control of the desulfurization tower from surface treatment to anti-corrosion layer formation, completing the construction of a multi-level and differentiated anti-corrosion construction system for all working conditions, and adapting to the anti-corrosion protection needs of the overall reaction working conditions of the desulfurization tower.

[0100] The above embodiments are merely exemplary embodiments of the present invention and are not intended to limit the present invention. The scope of protection of the present invention is defined by the claims. Those skilled in the art can make various modifications or equivalent substitutions to the present invention within its spirit and scope of protection, and such modifications or equivalent substitutions should also be considered as falling within the scope of protection of the embodiments of the present invention.

Claims

1. A high-performance anti-corrosion construction system, characterized in that, It includes a substrate pretreatment unit (1), a material mixing unit (2), a primer coating unit (3), a flake putty lining unit (4), a topcoat protection unit (5), and a zoned adaptive anti-corrosion material assembly (6). The substrate pretreatment unit (1) includes a dry compressed air supply device, a quartz sand / steel shot blasting hopper, grinding tools, and a dust removal device; the compressed air pressure is 0.5~0.6MPa and is oil-free and water-free; the blasting material is divided into quartz sand and steel shot, and the overall moisture content of the sand is <1%; The material mixing unit (2) is equipped with an independent workstation and a material conveying docking channel. The workstation is used to assemble a glass flake clay mixing device, which can automatically mix the flake clay; other materials are mixed manually. The primer coating unit (3) is equipped with vinyl ester glass flake primer, organic peroxide curing agent 328E, and brushing tools. The ratio of primer to curing agent is 100:

2. The flake mortar lining unit (4) includes phenolic epoxy vinyl ester flake mortar, curing agent, trowel, wool felt roller, and styrene solvent. The ratio of mortar to curing agent is 100:

2. Each batch of mortar needs to be mixed within 30 minutes for construction. The topcoat protective unit (5) is equipped with vinyl ester glass flake topcoat, and the topcoat contains defoamer, liquid wax, thixotropic agent and other additives. The partitioned anti-corrosion material components (6) include high-temperature phenolic epoxy vinyl ester flake mortar, high-temperature wear-resistant flake mortar, medium-temperature wear-resistant flake mortar, and standard medium-temperature wear-resistant flake mortar, which are respectively adapted to the four types of corrosion areas of the desulfurization tower: high-temperature flue (601), dry and wet alternation zone (602), spray scouring zone (603), and clean flue (604).

2. The high-performance anti-corrosion construction system according to claim 1, characterized in that, The material mixing unit (2) includes a cylinder (21), a drive motor (22), a mixing mechanism (23) disposed in the cylinder (21), a storage mechanism (24) located below the cylinder (21), and a defoaming component (25) disposed between the cylinder (21) and the storage mechanism (24). The stirring mechanism (23) has a gear set (231) set on the top of the cylinder (21). The gear set (231) consists of a driving gear located at the center and a plurality of driven gears arranged around the driving gear. The motor (22) is connected to the driving gear in a transmission connection. The driving gear is meshed with the driven gears to transmit power to each driven gear. A first rotating shaft (232) is coaxially connected below the drive gear, and a second rotating shaft (234) and a third rotating shaft (236) are sequentially connected to the first rotating shaft (232); wherein, a stirring blade (233) is provided on the first rotating shaft (232), a frame-type stirring blade (235) is provided on the second rotating shaft (234), and a spiral blade (237) is provided on the third rotating shaft (236); The driven gear is connected only to the first rotating shaft (232) and the corresponding stirring blade (233). The first rotating shaft (232), the second rotating shaft (234), and the third rotating shaft (236) below the driving gear are coaxially arranged in the vertical direction to form a central stirring assembly; the first rotating shaft (232) below the driven gear forms a peripheral stirring assembly; the central stirring assembly and the peripheral stirring assembly operate synchronously in opposite directions within the cylinder (21).

3. The high-performance anti-corrosion construction system according to claim 2, characterized in that, The cylinder (21) includes an outer shell (211) and an inner shell (212), and an insulation interlayer (213) is formed between the outer shell (211) and the inner shell (212); the insulation interlayer (213) is filled with insulation material, or the insulation interlayer (213) is configured to have a flow channel for passing through a heating medium or a cooling medium, so as to regulate the material temperature inside the inner shell (212).

4. The high-performance anti-corrosion construction system according to claim 2, characterized in that, The cylinder (21) also includes a top cover (219), on which a feed inlet (2111) is provided; the inner shell (212) defines an upper cavity (214) for containing materials and a lower cavity (215) located below the upper cavity (214), the lower cavity (215) having a funnel-shaped contraction structure.

5. The high-performance anti-corrosion construction system according to claim 4, characterized in that, The bottom of the lower cavity (215) is connected to a discharge port (216), and an output pipe (217) is connected below the discharge port (216). The end of the output pipe (217) is provided with an output port (218). The spiral blades (237) on the third rotating shaft (236) extend to the area of ​​the lower cavity (215) and the output pipe (217) to assist in conveying materials to the discharge port (216).

6. The high-performance anti-corrosion construction system according to claim 5, characterized in that, The storage mechanism (24) includes a receiving cavity (242) which is connected to the output port (218); the bottom inner wall of the receiving cavity (242) is configured as a ramp (241) which extends inclinedly toward the side away from the discharge port (216).

7. The high-performance anti-corrosion construction system according to claim 6, characterized in that, The storage mechanism (24) is also provided with a sliding cover (243) on one side, which is used to close or open the side opening of the receiving cavity (242).

8. A high-performance anti-corrosion construction method, characterized in that, The high-performance anti-corrosion construction system according to claim 1 includes the following steps: S1 Substrate Sandblasting and Rust Removal Pretreatment: Grinding removes weld slag and protruding structures; dry sandblasting treats the steel surface to achieve a rust removal grade of GB8923-88 Sa3, with a substrate roughness of 40~70μm; quartz sand particle size 1~3.2mm, with 1~1.5mm particle size accounting for ≥40%; steel shot particle size 0.63~1.6mm, with 0.63~0.8mm particle size accounting for ≥40%; sand moisture content <1%. S2 Anti-corrosion material mixing and preparation: The ratio of primer, flake putty, topcoat and hardener is 100:2; the flake putty is mixed using a glass flake putty mixing device installed in the material mixing unit; other materials are mixed manually. S3 Primer Application: Take the mixed primer and apply one coat to seal the substrate. S4 flake putty lining construction: Take the mixed flake putty and apply it within 30 minutes. The thickness of a single coat of putty is 1mm. Under normal working conditions, two coats are applied with a total thickness of 2mm. Before the putty initially sets, use styrene solvent to impregnate wool felt and roll it to remove air. For multi-layer construction, use an overlapping process. After sanding the defective areas to create a slope transition, reapply the primer and putty. S5 Topcoat Application: After the flake putty has fully cured, take the mixed topcoat and apply a layer to the entire surface.

9. The high-performance anti-corrosion construction method according to claim 8, characterized in that, The anti-corrosion method adopts differentiated anti-corrosion in different areas: the high-temperature flue (601) uses high-temperature phenolic epoxy vinyl ester flake mortar; the dry and wet alternation zone (602) uses high-temperature wear-resistant flake mortar; the spray scouring zone (603) uses medium-temperature wear-resistant flake mortar combined with wear-resistant topcoat; and the clean flue (604) uses standard medium-temperature wear-resistant flake mortar lining.

10. The high-performance anti-corrosion construction method according to claim 28, characterized in that, In step S2, the glass flake putty mixing device can be integrated into the material mixing unit, and the mixed material is directly transported to the S4 construction station through pipeline.