Method of disassembly of a dual glass photovoltaic module

By using a graded protection method to disassemble double-glass photovoltaic modules, the protective plate absorbs and consolidates the energy from tempered glass breakage. Combined with drilling and softening of the encapsulant film, the problem of cell damage during the disassembly of double-glass photovoltaic modules is solved, ensuring the integrity of the cells and the accuracy of the analysis results.

CN123149228APending Publication Date: 2026-11-24TONGWEI SOLAR ENERGY (CHENGDU) CO LID
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611207159.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-10
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing technologies make it difficult to disassemble double-glass photovoltaic modules without damaging the solar cells, especially double-glass photovoltaic modules with a fully tempered glass structure. This results in the solar cells suffering impact damage when the tempered glass breaks and secondary mechanical damage during drilling.

Method used

A graded protection method is adopted. First, a protective plate is bonded with a first adhesive to absorb the impact energy of tempered glass shattering and form a fracture layer. Then, a second adhesive is used to solidify the glass fragments. Finally, the battery cell is extracted without damage by drilling and softening the adhesive film.

Benefits of technology

This method enables non-destructive extraction of solar cells, ensuring the structural integrity of the cells and the accuracy of subsequent analysis results, while avoiding mechanical damage caused by tempered glass breakage and drilling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149228A_ABST
    Figure CN123149228A_ABST
Patent Text Reader

Abstract

This invention relates to the field of solar cell technology, specifically to a method for disassembling a double-glass photovoltaic module. The provided disassembly method includes: pre-treating the double-glass photovoltaic module to obtain the module body; applying a first adhesive to the tempered glass surface on either side of the module body, bonding a first protective plate to the tempered glass, causing the tempered glass to shatter and form a fractured layer, and removing the first protective plate; applying a second adhesive to the fractured layer, and bonding a second protective plate to the fractured layer to form a composite layer; the composite layer includes a second protective plate, a second adhesive layer, and the fractured layer; drilling a first hole in the composite layer to soften the adhesive film on one side of the solar cell in the module body, twisting the composite layer, removing the adhesive film, and obtaining the solar cell from the double-glass photovoltaic module. This disassembly method enables the non-destructive extraction of the solar cell.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of solar cell technology, and in particular to a method for disassembling a double-glass photovoltaic module. Background Technology

[0002] In recent years, to accurately identify the causes of performance degradation in photovoltaic modules during outdoor use, such as light-induced degradation, damp-heat-induced degradation, and potential-induced degradation, it is usually necessary to disassemble the encapsulation layer of double-glass photovoltaic modules and extract the internal cells without damage. This is to obtain pure samples that meet the requirements for multi-scale characterization, including electroluminescence, photoluminescence, scanning electron microscopy, and energy dispersive spectroscopy. However, because double-glass photovoltaic modules use a symmetrical layered structure formed by laminating two sides of fully tempered glass with encapsulating films, the disassembly process must completely separate the cells from the high-bonding-strength encapsulation system without introducing new mechanical damage, thermal damage, or chemical contamination.

[0003] Currently, existing methods for dismantling double-glass photovoltaic modules mainly include glass-backsheet core extraction technology, thin-film double-glass module core extraction technology, as well as overall violent crushing, manual peeling, and laser cutting. Glass-backsheet core extraction technology removes the backsheet by grinding to expose the cells, but it relies on the assumption that the backsheet can be mechanically removed, making it unsuitable for the structural characteristics of double-glass modules where both sides are fully tempered glass. Thin-film double-glass module core extraction technology utilizes the characteristics of its non-tempered glass substrate for core extraction, eliminating the need to address the problems caused by tempered glass breakage. Overall violent crushing and manual peeling methods primarily serve material recycling after the entire module is scrapped, making it difficult to achieve targeted core extraction from specific areas. The tempered glass in double-glass crystalline silicon modules contains internal pre-stress, which can cause instantaneous high-energy overall breakage. The shock wave and flying fragments can directly lead to structural damage to the cells, such as microcracks, breakage, and grid line detachment.

[0004] Therefore, it is becoming increasingly important to find a method for disassembling double-glass photovoltaic modules that ensures the final obtained solar cells have structural integrity, electrical performance fidelity, and surface cleanliness. Summary of the Invention

[0005] In view of this, the present invention aims to at least partially solve one of the technical problems in the related art. To this end, the present invention provides a method for disassembling a double-glass photovoltaic module, which can achieve non-destructive extraction of the solar cells from the double-glass photovoltaic module, ensuring the integrity of the obtained solar cells and the accuracy of subsequent analysis results.

[0006] To solve the above-mentioned technical problems, the present invention is implemented as follows: According to one aspect of the present invention, a method for disassembling a double-glass photovoltaic module is provided. Pre-processing of double-glass photovoltaic modules yields the module body; Apply the first adhesive to the tempered glass surface on either side of the component body, adhere the first protective plate to the tempered glass, cause the tempered glass to shatter, forming a fracture layer, and remove the first protective plate. A second adhesive is applied to the fractured layer, and a second protective plate is bonded to the fractured layer to form a composite layer; the composite layer includes the second protective plate, the second adhesive layer, and the fractured layer. A first hole is drilled in the composite layer to soften the adhesive film on one side of the solar cell in the module body. The composite layer is then twisted to remove the adhesive film, thereby obtaining the solar cell in the double-glass photovoltaic module.

[0007] In some embodiments, drilling the composite layer for the first time includes: Measure the surface of the composite layer away from the solar cell to a predetermined dimension of the solar cell; A first hole is drilled in the core sampling area on the surface of the composite layer, and drilling is stopped when the drilling depth reaches the preset size; wherein, the core sampling area is the area on the composite layer where the battery cell is projected orthogonally.

[0008] In some embodiments, the first drilling of the coring area further includes: A first hole is drilled in the core extraction area, and cooling water is continuously sprayed onto the first hole location.

[0009] In some embodiments, softening the adhesive film on one side of the battery cell in the component body includes: A softening fluid is injected from the drilled hole to soften the adhesive film on one side of the battery cell; wherein the softening fluid includes at least one of trichloroethylene, dichloromethane, trichloromethane, toluene, xylene, tetrahydrofuran, and D-limonene.

[0010] In some of these embodiments, twisting the composite layer includes: A metal rod coated with a third adhesive is inserted into the hole of the first drilled hole in the composite layer, so that the metal rod and the composite layer are bonded together. By twisting the metal rod, the composite layer is removed to obtain the component intermediate; The metal rod coated with the third adhesive is bonded to the battery cell in the component intermediate. The metal rod is twisted to remove the adhesive film and tempered glass on the other side of the battery cell, thus obtaining the battery cell precursor. The third adhesive includes at least one of cyanoacrylate adhesive, cyanoacrylate adhesive, epoxy resin adhesive, acrylate structural adhesive, polyurethane adhesive, UV-curable adhesive, and reactive hot melt adhesive.

[0011] In some embodiments, removing the adhesive film includes: After removing the composite layer, the battery cell precursor is obtained. The softening liquid is coated onto the surface of the battery cell precursor, and then the residual adhesive film on the surface of the battery cell precursor is removed to obtain the battery cell.

[0012] In some embodiments, removing the adhesive film includes: After removing the composite layer, the obtained battery cell precursor is placed at a preset temperature, and then the residual adhesive film on the surface of the battery cell precursor is peeled off to obtain the battery cell. The preset temperature value is less than or equal to -30℃.

[0013] In some embodiments, the step of bonding the first protective plate to the tempered glass, causing the tempered glass to shatter and form a fracture layer, and then removing the first protective plate includes: A second hole is drilled at the edge of the area where the battery cell in the component body is projected onto the first protective plate to induce the tempered glass to shatter and form the shattered layer. An organic solution is added into the hole of the second drilled hole to dissolve the first adhesive and remove the first protective plate; wherein the first adhesive includes at least one of ethyl cyanoacrylate, methyl cyanoacrylate, butyl cyanoacrylate and methoxyethyl cyanoacrylate.

[0014] In some embodiments, the pretreatment of the double-glass photovoltaic module includes: The double-glass photovoltaic module is optically scanned to delineate the core sampling area.

[0015] In some embodiments, after removing the adhesive film, the process further includes: The resulting battery cell after removing the adhesive film is cleaned and dried. In some embodiments, the second adhesive includes at least one of epoxy resin, polyurethane resin, unsaturated polyester resin, UV-curable resin, and acrylate structural resin.

[0016] Implementing the technical solution of the present invention has at least the following beneficial effects: In this invention, a first protective plate is first bonded to tempered glass with a first adhesive before the tempered glass is induced to shatter. The first protective plate absorbs and disperses the impact energy of the shattering, thereby preventing the impact energy from being transmitted to the solar cells below, effectively avoiding impact damage to the solar cells during the tempered glass shattering stage. After removing the first protective plate, a second protective plate is bonded to the shattered layer with a second adhesive, solidifying the loose glass fragments into a unified composite layer. During subsequent drilling of the composite layer, the glass fragments are completely fixed, preventing displacement, scratching, or compression of the solar cells, thus eliminating secondary mechanical damage during the drilling process. Subsequently, the adhesive film on one side of the solar cell is softened and removed by twisting the composite layer. This allows for complete peeling of the solar cell with relatively small mechanical forces, avoiding bending or breakage caused by forceful peeling. This achieves non-destructive extraction of the solar cells in the double-glass photovoltaic module, ensuring the integrity of the obtained solar cells and the accuracy of subsequent analysis results.

[0017] Additional aspects and advantages of the invention will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention. Attached Figure Description

[0018] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.

[0019] Figure 1 The diagram shows the process flow chart of the disassembly method for double-glass photovoltaic modules provided by the present invention.

[0020] Figure 2 The image shows a solar cell obtained by the disassembly method of a double-glass photovoltaic module provided in an embodiment of the present invention.

[0021] The accompanying drawings have illustrated specific embodiments of the invention, which will be described in more detail below. These drawings and descriptions are not intended to limit the scope of the invention in any way, but rather to illustrate the concept of the invention to those skilled in the art through reference to particular embodiments. Detailed Implementation

[0022] The present invention will be further illustrated below with reference to specific embodiments. It should be understood that these embodiments are for illustrative purposes only and are not intended to limit the scope of the invention.

[0023] The endpoints and any values ​​of the ranges disclosed herein are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of the various ranges, the endpoint values ​​of the various ranges or individual point values, and individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed herein.

[0024] Unless otherwise specified, all embodiments and optional embodiments of the present invention can be combined with each other to form new technical solutions.

[0025] Unless otherwise specified, all technical features and optional technical features of this invention can be combined to form new technical solutions.

[0026] Unless otherwise specified, all steps of the present invention may be performed sequentially or randomly, preferably sequentially. For example, the method includes steps (a) and (b), indicating that the method may include steps (a) and (b) performed sequentially, or it may include steps (b) and (a) performed sequentially. For example, the mention that the method may also include step (c) indicates that step (c) may be added to the method in any order. For example, the method may include steps (a), (b), and (c), or it may include steps (a), (c), and (b), or it may include steps (c), (a), and (b), etc.

[0027] Unless otherwise specified, the terms "comprising" and "including" as used in this invention can be open-ended or closed-ended. For example, "comprising" and "including" can mean that other components not listed may also be included, or that only the listed components may be included.

[0028] Currently, to extract the solar cells inside double-glass photovoltaic modules for failure analysis, the common methods are overall crushing or direct drilling. This involves mechanically impacting or drilling directly onto the tempered glass and encapsulating film on the module surface, using external force to break the interlayer bonding of the encapsulation layers and expose the solar cells. However, when these methods are used for double-glass crystalline silicon modules with fully tempered glass as the front and rear encapsulation plates, the following problems arise: the outermost tempered glass of the double-glass photovoltaic module contains pre-stress; localized breakage will instantly release high energy and shatter into sharp-edged fragments. Direct drilling or crushing inevitably triggers this energy release and fragmentation during the tempered glass breakage process, thus damaging the solar cells. For example, in the core sampling process of double-glass photovoltaic modules, if the tempered glass is drilled directly, the impact energy from the pre-shattering tempered glass will be transferred to the underlying solar cells through the encapsulant film, causing microcracks, breakage, or grid line detachment in the cells. During subsequent drilling, the broken glass fragments are displaced and scraped by the drill bit, further scratching the surface of the solar cells and the passivation layer. This new damage can mask the original failure characteristics of the module, making failure analysis difficult. In other words, when disassembling double-glass photovoltaic modules, it is impossible to effectively control the energy release when the tempered glass breaks and the state of the fragments after breakage. The energy from the breakage directly affects the cell structure, and the loose glass fragments generated after breakage lack fixation, becoming a continuous source of secondary damage during subsequent drilling operations.

[0029] In view of the technical problems existing in the prior art, this invention proposes a disassembly method for double-glass photovoltaic modules. This method improves the tempered glass breakage and subsequent drilling process through a graded protection and penetration fixation technique, thereby removing the tempered glass layer without damaging the solar cells. Specifically, a two-step protection method is used: First, before inducing tempered glass breakage, a first protective plate is bonded to the tempered glass surface with a first adhesive to absorb and disperse the impact energy of the breakage; second, after removing the first protective plate, a second adhesive penetrates the broken layer and bonds it to the second protective plate, solidifying the broken glass fragments into a single unit before drilling, thus eliminating secondary damage caused by fragment displacement and achieving non-destructive extraction of the solar cells from the double-glass module.

[0030] The specific technical solution of the present invention is as follows: In some embodiments of the present invention, reference is made to Figure 1 A method for disassembling a double-glass photovoltaic module is provided, comprising the following steps: S10. Pre-process the double-glass photovoltaic module to obtain the module body.

[0031] As an example, the structure of a double-glass photovoltaic module, in the thickness direction, consists of tempered glass, encapsulant film, solar cell, encapsulant film, and tempered glass. The encapsulant film can be EVA (polyethylene-polyvinyl acetate copolymer) film, POE (random copolymer elastomer formed by polymerization of ethylene and 1-octene) film, or EPE film (composite film formed by multilayer co-extrusion of EVA and POE materials), etc.; no specific limitation is made.

[0032] Furthermore, the pretreatment is mainly to perform global inspection and positioning of the double-glass photovoltaic module before the formal dismantling operation, and to complete necessary fixing operations, so as to ensure that all subsequent processes can be executed accurately and safely. After the above pretreatment, the module body to be dismantled can be obtained, which still maintains the complete layered structure of front tempered glass / encapsulant film / cell / encapsulant film / back tempered glass.

[0033] S20. Apply the first adhesive to the tempered glass surface on either side of the component body, bond the first protective plate to the tempered glass, cause the tempered glass to shatter, form a fracture layer, and remove the first protective plate.

[0034] As an example, a first adhesive is applied to the tempered glass surface on either side of the component body obtained in step S10. Then, a first protective plate is bonded to the tempered glass, causing the tempered glass to shatter, forming a fracture layer. The first protective plate is then removed. The first protective plate can be a piece of ordinary non-tempered glass of a certain thickness, or it can be a metal plate. It is understood that the first adhesive is an adhesive that provides sufficient bonding strength to absorb impact energy upon shattering, while also being easily soluble in a specific solvent for removal. For example, the first adhesive can be a cyanoacrylate-based instant adhesive. It is also understood that the first protective plate completely covers the tempered glass with the first adhesive. Optionally, the first protective plate can also cover the core sampling area, which can be the area where the solar cell is projected onto the tempered glass, and its bonding area is preferably several times the area of ​​the core sampling area.

[0035] Furthermore, after the first protective plate and tempered glass are bonded and cured, a hole can be drilled using a magnetic drill at the edge of the area where the solar cell projects onto the first protective plate within the module body. The localized stress concentration generated by the drilling precisely induces the tempered glass beneath it to shatter uniformly within the core extraction area, rather than experiencing uncontrollable large-area shattering. When the tempered glass shatters, the pre-stress stored within it is released instantaneously as a high-energy impact. At this point, the first protective plate, firmly bonded to the surface of the tempered glass, acts like a car windshield, absorbing and dispersing the impact energy, effectively preventing the energy from propagating to the encapsulation film and solar cell below. This avoids structural damage to the solar cell, such as microcracks, shattering, or grid line detachment, during the tempered glass shattering process.

[0036] Furthermore, after the tempered glass shatters, a fractured layer is formed. When removing the first protective plate, an organic solvent can be added to the drilled hole to dissolve the first adhesive. For example, acetone can be added to allow the acetone to penetrate along the drill hole and dissolve the bonding interface of the first adhesive, thereby enabling the first protective plate to be completely peeled off without damage, exposing a fractured layer composed of a large number of glass fragments for subsequent processing.

[0037] S30. Apply the second adhesive to the fractured layer and bond the second protective plate to the fractured layer to form a composite layer; the composite layer includes the second protective plate, the second adhesive layer and the fractured layer.

[0038] As an example, after steps S10 and S20, a fractured layer has formed on one side of the component body's tempered glass. A second adhesive is then applied to this fractured layer, and a second protective plate is bonded to it, forming a composite layer. The composite layer includes the second protective plate, the second adhesive layer, and the fractured layer. It is understood that the second protective plate can be a standard non-tempered glass plate of a certain thickness. The second adhesive is an adhesive with high curing strength and excellent permeability, such as epoxy resin. The second adhesive is evenly applied to the surface of the fractured layer, allowing it to fully penetrate every crack and crevice, initially bonding the loose glass fragments into a single unit. Then, the second protective plate is pressed flat onto the second adhesive, ensuring no air bubbles or gaps. It can then be left to cure at room temperature for a specific time to allow the second adhesive to reach its maximum bonding strength.

[0039] Furthermore, step S30, through the penetration and curing of the second adhesive and its bonding with the second protective plate, forms a composite rigid structure consisting of the second protective plate, the second adhesive layer, and the fragmentation layer. This composite layer completely fixes the originally loose glass fragments into a single, immobile unit, completely eliminating the possibility of displacement, scraping, or compression of the underlying battery cells and adhesive film by the high-speed rotating drill bit during subsequent drilling operations on the composite layer. This fundamentally prevents secondary mechanical damage during the drilling process.

[0040] S40. Drill a first hole in the composite layer to soften the adhesive film on one side of the cell in the module body, twist the composite layer, remove the adhesive film, and obtain the cell in the double-glass photovoltaic module.

[0041] As an example, a first drill hole is further made on the surface of the composite layer. Preferably, the first drill hole can be made in the core-taking area of ​​the composite layer surface, which is the area where the solar cell is projected onto the composite layer. When the drill bit travels to a certain position, in the preferred embodiment, the drill bit can reach the solar cell precisely without touching the surface of the solar cell, thereby precisely controlling the drilling endpoint and avoiding damage to the tempered glass on the opposite side or the solar cell due to excessive drill bit feed. This ensures the integrity of the non-core-taking area of ​​the module, enabling multi-point local targeted core taking of the same module without affecting the rest. The above-mentioned twisting of the composite layer, and then removing the composite layer, involves applying shear force to gently break the initial strong bond between the solar cell and the adhesive film, avoiding the solar cell from breaking due to direct vertical pulling. This creates a more easily separable interface for subsequent vertical pulling, reducing the required pulling force, thereby achieving "non-damaging peeling".

[0042] In some embodiments, drilling a first hole in the composite layer includes: S101. Measure the preset dimension from the surface of the composite layer away from the solar cell to the solar cell.

[0043] S102. Drill a first hole in the core sampling area on the surface of the composite layer, and stop drilling when the drilling depth reaches a preset size; wherein, the core sampling area is the area on the composite layer where the solar cell is projected orthogonally.

[0044] For example, before drilling the composite layer for the first time, a step of measuring and calibrating the drilling depth is included; that is, measuring a preset dimension from the surface of the composite layer away from the solar cell to the solar cell, which is the total thickness of all material layers between the upper surface of the second protective plate and the upper surface of the solar cell. This preset dimension is marked on the drill bit to establish a clear and observable drilling depth reference. Then, the first drilling is performed in the core area on the surface of the composite layer, and drilling is stopped when the drilling depth reaches the preset dimension. In this way, since the depth reference corresponding to the solar cell position has been pre-calibrated on the drill bit, when the drill bit travels to the marked position, it can be accurately determined that the drill bit has just penetrated the solar cell without touching the tempered glass on the opposite side, thereby precisely controlling the drilling endpoint and avoiding damage to the tempered glass on the opposite side or damage to the solar cell in the non-target area due to excessive feed of the drill bit. This ensures the integrity of the non-core area of ​​the module and enables multi-point local targeted core sampling of the same module without affecting the rest.

[0045] In some embodiments, when drilling the first hole in the coring area, the method further includes: drilling the first hole in the coring area and continuously spraying cooling water at the first hole location.

[0046] For example, during the first drilling of the core sampling area, cooling water can be continuously sprayed onto the first drill hole location. In this way, the high-speed rotating drill bit generates a large amount of frictional heat due to friction with the composite material layer composed of glass, adhesive layers, etc. If this heat accumulates and is conducted to the solar cell, it may cause thermal degradation of the passivation layer and crystal structure of the solar cell. By continuously spraying cooling water onto the drill hole location, the convective heat transfer effect of the cooling water instantly absorbs and removes the frictional heat, effectively suppressing the local temperature rise in the drilled area and the solar cell below, preventing thermal damage. Simultaneously, the cooling water flow can also wash away glass powder and other debris generated during drilling, preventing the powder from scratching the sample surface under the influence of the drill bit, further improving the reliability of non-destructive coring.

[0047] In some embodiments, softening the adhesive film on one side of the battery cell in the component body includes: injecting a softening liquid from a drilled hole to soften the adhesive film on one side of the battery cell; wherein the softening liquid includes at least one of trichloroethylene, dichloromethane, trichloromethane, toluene, xylene, tetrahydrofuran, and D-limonene.

[0048] For example, after completing the first drilling, the encapsulating film on one side of the solar cell in the module body is softened. Optionally, a softening liquid is injected from the drilling location to soften the encapsulating film on the solar cell side. The softening liquid includes, but is not limited to, one or more of trichloroethylene, dichloromethane, chloroform, toluene, xylene, tetrahydrofuran, and D-limonene. More specifically, the first drilling forms a channel in the composite layer that extends to the surface of the solar cell. Through this drilling channel, a softening liquid, such as trichloroethylene, is injected into the encapsulating film area between the solar cell and the back tempered glass, and the area is allowed to stand for a sufficient amount of time to allow the softening liquid to penetrate and swell the encapsulating film. Under the action of the softening liquid, the volume of the encapsulating film expands, the intermolecular forces weaken, and the adhesion between the film and the back glass is significantly reduced, thereby forming a peeling gap between the encapsulating film and the solar cell; thus preventing the solar cell from bending or breaking when subsequently peeled off by twisting with minimal mechanical force.

[0049] In some embodiments, the torsion composite layer includes: S201. Insert the metal rod coated with the third adhesive into the hole of the first drilled hole of the composite layer to bond the metal rod and the composite layer.

[0050] S202. By twisting the metal rod, the composite layer is removed to obtain the component intermediate.

[0051] S203. A metal rod coated with a third adhesive is bonded to a solar cell in the intermediate body of the module. The metal rod is twisted to remove the adhesive film and tempered glass on the other side of the solar cell, thus obtaining the solar cell precursor. The third adhesive includes at least one of cyanoacrylate adhesive, cyanoacrylate adhesive, epoxy resin adhesive, acrylic structural adhesive, polyurethane adhesive, UV-curable adhesive, and reactive hot melt adhesive.

[0052] For example, after the adhesive film has softened, a process of twisting to remove the composite layer and adhesive film is performed. For instance, a metal rod coated with a third adhesive is inserted into the first drilled hole in the composite layer, bonding the metal rod to the composite layer. The third adhesive includes, but is not limited to, one or more of cyanoacrylate adhesive, epoxy resin adhesive, acrylic structural adhesive, polyurethane adhesive, UV-curable adhesive, and reactive hot melt adhesive. By twisting the metal rod, the entire composite layer is removed, yielding the module intermediate. During this process, the metal rod provides a reliable rigid handle, and the torque is evenly transmitted to the entire bonding surface, allowing the composite layer to be smoothly removed as a whole, avoiding secondary disturbance to the broken glass layer caused by localized prying. After removing the composite layer, the upper adhesive film that detaches with the glass is gently peeled off with a tool, exposing one side of the solar cell. Then, the metal rod coated with the third adhesive is bonded to the solar cell in the module intermediate again. The metal rod is gently twisted to remove the adhesive film and tempered glass on the other side of the solar cell, yielding the solar cell precursor. Since the adhesive film on the other side of the battery cell has had its adhesion force sufficiently reduced by the softening liquid, the gentle torque acting on the metal rod can be evenly distributed on the surface of the battery cell through the bonding surface, allowing the battery cell to be completely separated from the adhesive film under controlled minimal shear force, thus completely avoiding local stress concentration and breakage caused by clamping with sharp tools such as tweezers.

[0053] In some embodiments, removing the adhesive film includes: after removing the composite layer to obtain a battery cell precursor, applying a softening liquid to the surface of the battery cell precursor, and then removing the adhesive film remaining on the surface of the battery cell precursor to obtain a battery cell.

[0054] For example, a softening solution can be applied to the surface of the pre-cell battery obtained after peeling, causing the residual adhesive film to swell and soften again, further reducing its adhesive strength and cohesive strength. Subsequently, the fully softened residual adhesive film can be removed by gentle wiping or rinsing, completely separating the adhesive film residue from the cell surface without introducing shearing or scraping forces. This further ensures that the final cell surface is free of adhesive film and organic residues, meeting the high standards of sample cleanliness required for subsequent precise characterization.

[0055] In some embodiments, removing the adhesive film includes: after removing the composite layer, placing the obtained battery cell precursor at a preset temperature, and then peeling off the adhesive film remaining on the surface of the battery cell precursor to obtain the battery cell; wherein the preset temperature is less than or equal to -30°C.

[0056] For example, the removal of residual adhesive film can also be achieved through a physical low-temperature method; that is, the solar cell precursor obtained after removing the composite layer is placed at a preset temperature, and then the residual adhesive film on the surface of the solar cell precursor is peeled off to obtain the solar cell; wherein, the preset temperature is set to a range of less than or equal to -30°C. Optionally, the preset temperature can be any value among -31°C, -33°C, -35°C, -37°C, -39°C, -42°C, -45°C, -48°C, -50°C, and -100°C. If the preset temperature is greater than -30°C, the adhesive film cannot undergo a complete glass transition, and it still retains high viscosity. The adhesion force to the solar cell cannot be sufficiently attenuated, resulting in a large mechanical force still required for peeling, which poses a risk of causing bending deformation and microcracks in the solar cell. By placing the solar cell precursor in an ultra-low temperature environment below or equal to -30°C, the temperature of the encapsulating film drops below its glass transition temperature. This freezes the chain movement of the film molecules, transforming them from a soft rubber state to a hard and brittle glass state. The adhesive force decreases sharply, generating shrinkage stress, which naturally creates microcracks and peeling gaps at the interface between the encapsulating film and the solar cell / glass. At this point, only slight assisted peeling from the edges is required to completely separate the solar cell from the encapsulating film, without the need for any organic solvents, thus eliminating the potential contamination of the solar cell surface by residual chemical reagents.

[0057] In some embodiments, the first protective plate is bonded to the tempered glass, causing the tempered glass to shatter and form a fractured layer. Removing the first protective plate includes: S301. A second hole is drilled at the edge of the area where the solar cell in the module body is projected onto the first protective plate to induce the tempered glass to shatter and form a fracture layer.

[0058] S302. Add an organic solution into the hole of the second drilled hole to dissolve the first adhesive and remove the first protective plate; wherein the first adhesive includes, but is not limited to, one or more of ethyl cyanoacrylate, methyl cyanoacrylate, butyl cyanoacrylate and methoxyethyl cyanoacrylate.

[0059] For example, after the first protective plate and tempered glass are bonded and cured with, for example, cyanoacrylate-based instant adhesive, the first protective plate is completely bonded to cover the core sampling area with a first adhesive. The bonded area can be one, two, or several times the area of ​​the core sampling area. Then, a second hole is drilled using a magnetic drill at the edge of the area where the solar cell is projected onto the first protective plate in the module body. The purpose of the second hole is to utilize the localized stress concentration generated by the drilling to precisely induce uniform, overall fragmentation of the tempered glass beneath it within the core sampling area, rather than uncontrollable large-area shattering. When the tempered glass shatters, the pre-stress stored within it is released instantaneously in the form of a high-energy impact. Further, an organic solvent is added to the drilled second hole to dissolve the first adhesive. For example, acetone is added, allowing it to penetrate along the drill hole and dissolve the bonding interface of the first adhesive, thus enabling the first protective plate to be peeled off completely without damage.

[0060] In some embodiments, the double-glass photovoltaic module is preprocessed, including: optically scanning the double-glass photovoltaic module to delineate the core sampling area.

[0061] For example, optical scanning is performed on double-glass photovoltaic modules to delineate core sampling areas. Specifically, non-destructive testing methods such as electroluminescence imaging, photoluminescence imaging, or high-resolution optical imaging can be used to perform a global scan on aged modules that have been in outdoor service for many years or on brand-new modules to identify and locate target analysis defects such as hot spots, microcracks, and performance degradation areas inside the modules. Based on the analysis results of the scanned images, one or more circular or square core sampling areas are delineated on the surface of the module. Optionally, the size of the core sampling area can be arbitrarily determined within the range of diameter from 10mm to 200mm according to the actual needs of subsequent characterization. The module with the delineated area is horizontally fixed on the operating platform to ensure that the delineated area is in a completely horizontal state to avoid introducing lateral shear stress during drilling.

[0062] In some embodiments, after removing the adhesive film, the process further includes cleaning and drying the resulting battery cell. For example, cleaning can be performed using organic solvents such as acetone and ethanol. Immersion and sonication are used to sequentially dissolve and remove adhesive residues such as cyanoacrylate glue introduced during the peeling process, as well as to thoroughly remove swollen film precipitates and small-molecule organic impurities. After cleaning, the solar cells are dried using nitrogen gas and stored in a desiccator to provide solar cell samples with no chemical contamination or foreign impurities on their surface for subsequent characterization.

[0063] In some embodiments, the second adhesive includes, but is not limited to, one or more of epoxy resin, polyurethane resin, unsaturated polyester resin, UV-curable resin, and acrylate structural resin.

[0064] In some embodiments, a 2400mm×1200mm commercial perovskite module was used for verification. The module structure is a symmetrical layered structure of "front tempered glass / EVA film / battery cell / EVA film / back tempered glass".

[0065] Furthermore, the following disassembly method is adopted, including the following steps: S1. Perform a global scan of the component using EL imaging, PL imaging, and optical imaging to identify target analysis areas such as hot spots, cracks, and performance degradation within the component. A circular core sampling area with a recommended diameter of 10-200 mm is defined; this size meets all subsequent characterization requirements, including SEM, EDS, and minority carrier lifetime measurements. Fix the component under test horizontally on the operating platform, ensuring the core sampling area is completely horizontal to avoid lateral stress during drilling.

[0066] S2. Take a piece of ordinary non-tempered glass with a recommended size of 10cm × 10cm (±5cm) × 5 (±2)mm. Adhere it completely to the tempered glass surface of the core sampling area using instant adhesive. The adhesive area should cover the entire core sampling area and be several times its size to ensure protection. Use a magnetic drill to drill small holes at the corners of the core sampling area to induce uniform shattering of the tempered glass on that side. Immediately stop drilling and let it stand for several minutes until the tempered glass completely shatters. In this step, the protective glass can completely absorb the impact energy from the tempered glass shattering, preventing the impact from being transmitted to the underlying battery cells and causing damage. Apply acetone locally to the adhesive area to dissolve the instant adhesive, then completely remove the protective glass to expose the shattered tempered glass surface.

[0067] S3. Apply high-curing-strength epoxy resin evenly to the surface of the shattered tempered glass, ensuring that the epoxy resin fully penetrates into all the cracks in the glass, and initially bond the loose glass fragments together.

[0068] S4. Bonding the second layer of protective glass: Take a piece of ordinary non-tempered glass (protective glass #2) of the same size as the protective glass and press it flat onto the epoxy resin surface to ensure that there are no air bubbles or gaps between the glass and the broken tempered glass, forming a composite rigid structure of ordinary glass-epoxy resin-broken tempered glass.

[0069] S5. Allow to stand at room temperature for 2 hours to ensure the epoxy resin is fully cured and reaches maximum bonding strength, so that the broken tempered glass is completely fixed into a whole, preventing glass fragments from shifting or falling off during subsequent drilling.

[0070] S6. Measure the total thickness of "protective glass #2 + epoxy resin layer + tempered glass + EVA film + battery cell" in advance, and mark the corresponding depth on the drill bit of the magnetic drill to avoid over-drilling and damaging the tempered glass and battery cell on the opposite side. Use the magnetic drill to drill vertically along the target core area, continuously circulating cooling water into the core area during drilling. When the drill bit reaches the marked depth, reduce the drilling feed speed and observe the drilling status in real time; when the battery cell is penetrated, a transparent edge will appear on the opposite side of the core area. At this point, stop drilling immediately to ensure that the tempered glass on the opposite side remains intact, providing stable mechanical support for subsequent battery cell peeling.

[0071] S7. After removing the magnetic drill, bond the metal rod to the center of the core sample using cyanoacrylate adhesive. By twisting the metal rod, remove the protective glass #2, the epoxy resin layer, and the broken tempered glass as a whole. Then, gently peel off the upper EVA film bonded to the glass using tweezers. Add trichloroethylene (TCE) solution to the core area and let it stand for 12 hours to allow TCE to fully penetrate and soften the lower EVA film, significantly reducing the adhesion between EVA and the cell, creating a peeling gap between the cell and EVA. Bond the metal rod to the cell surface again using cyanoacrylate adhesive. The adhesive strength of this adhesive is greater than the adhesion between the softened EVA and the cell. By gently twisting the metal rod, peel the cell completely off the opposite glass and EVA film, obtaining the desired result. Figure 2 The battery cells shown.

[0072] The parts of this invention not described in detail are techniques known to those skilled in the art.

[0073] The basic principles of the present invention have been described above with reference to specific embodiments. However, it should be noted that the advantages, benefits, and effects mentioned in the present invention are merely examples and not limitations, and should not be considered as essential features of each embodiment of the present invention. Furthermore, the specific details disclosed above are for illustrative and facilitative purposes only, and are not limitations. These details do not limit the present invention to the necessity of employing the aforementioned specific details.

[0074] It should be noted that the terms "and / or" or " / " used herein are merely descriptions of the relationship between related objects, indicating that three relationships can exist. For example, A and / or B can represent: A existing alone, A and B existing simultaneously, or B existing alone. The singular forms "a," "described," and "the" used in the embodiments of the invention and the appended claims are also intended to include the plural forms, unless the context clearly indicates otherwise.

[0075] In the detailed description and claims, a list of items connected by the terms "at least one of," "at least one of," "at least one of," or other similar terms may mean any combination of the listed items. For example, if items A and B are listed, then the phrase "at least one of A and B" means only A; only B; or A and B. In another example, if items A, B, and C are listed, then the phrase "at least one of A, B, and C" means only A; or only B; only C; A and B (excluding C); A and C (excluding B); B and C (excluding A); or all of A, B, and C. Item A may contain a single element or multiple elements. Item B may contain a single element or multiple elements. Item C may contain a single element or multiple elements.

[0076] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for disassembling a double-glass photovoltaic module, characterized in that, include: Pre-processing of double-glass photovoltaic modules yields the module body; Apply the first adhesive to the tempered glass surface on either side of the component body, adhere the first protective plate to the tempered glass, cause the tempered glass to shatter, forming a fracture layer, and remove the first protective plate. A second adhesive is applied to the fractured layer, and a second protective plate is bonded to the fractured layer to form a composite layer; the composite layer includes the second protective plate, the second adhesive layer, and the fractured layer. A first hole is drilled in the composite layer to soften the adhesive film on one side of the solar cell in the module body. The composite layer is then twisted to remove the adhesive film, thereby obtaining the solar cell in the double-glass photovoltaic module.

2. The method for disassembling a double-glass photovoltaic module according to claim 1, characterized in that, The first drilling of the composite layer includes: Measure the surface of the composite layer away from the solar cell to a predetermined dimension of the solar cell; A first hole is drilled in the core sampling area on the surface of the composite layer, and drilling is stopped when the drilling depth reaches the preset size; wherein, the core sampling area is the area on the composite layer where the battery cell is projected orthogonally.

3. The method for disassembling a double-glass photovoltaic module according to claim 2, characterized in that, The first drilling of the coring area also includes: A first hole is drilled in the core extraction area, and cooling water is continuously sprayed onto the first hole location.

4. The method for disassembling a double-glass photovoltaic module according to claim 1, characterized in that, The softening of the adhesive film on one side of the battery cell in the component body includes: A softening fluid is injected from the drilled hole to soften the adhesive film on one side of the battery cell; wherein the softening fluid includes at least one of trichloroethylene, dichloromethane, trichloromethane, toluene, xylene, tetrahydrofuran, and D-limonene.

5. The method for disassembling a double-glass photovoltaic module according to claim 1, characterized in that, The twisting of the composite layer includes: A metal rod coated with a third adhesive is inserted into the hole of the first drilled hole in the composite layer, so that the metal rod and the composite layer are bonded together. By twisting the metal rod, the composite layer is removed to obtain the component intermediate; The metal rod coated with the third adhesive is bonded to the battery cell in the component intermediate. The metal rod is twisted to remove the adhesive film and tempered glass on the other side of the battery cell, thus obtaining the battery cell precursor. The third adhesive includes at least one of cyanoacrylate adhesive, cyanoacrylate adhesive, epoxy resin adhesive, acrylate structural adhesive, polyurethane adhesive, UV-curable adhesive, and reactive hot melt adhesive.

6. The method for disassembling a double-glass photovoltaic module according to claim 1 or 5, characterized in that, The removal of the adhesive film includes: After removing the composite layer, the battery cell precursor is obtained. The softening liquid is coated onto the surface of the battery cell precursor, and then the residual adhesive film on the surface of the battery cell precursor is removed to obtain the battery cell.

7. The method for disassembling a double-glass photovoltaic module according to claim 1 or 5, characterized in that, The removal of the adhesive film includes: After removing the composite layer, the obtained battery cell precursor is placed at a preset temperature, and then the residual adhesive film on the surface of the battery cell precursor is peeled off to obtain the battery cell. The preset temperature value is less than or equal to -30℃.

8. The method for disassembling a double-glass photovoltaic module according to claim 1, characterized in that, The step of bonding the first protective plate to the tempered glass, causing the tempered glass to shatter and form a fractured layer, and then removing the first protective plate includes: A second hole is drilled at the edge of the area where the battery cell in the component body is projected onto the first protective plate to induce the tempered glass to shatter and form the shattered layer. An organic solution is added into the hole of the second drilled hole to dissolve the first adhesive and remove the first protective plate; wherein the first adhesive includes at least one of ethyl cyanoacrylate, methyl cyanoacrylate, butyl cyanoacrylate and methoxyethyl cyanoacrylate.

9. The method for disassembling a double-glass photovoltaic module according to claim 1, characterized in that, The pretreatment of the double-glass photovoltaic module includes: The double-glass photovoltaic module is optically scanned to delineate the core sampling area.

10. The method for disassembling a double-glass photovoltaic module according to claim 1, characterized in that, After removing the adhesive film, the process further includes: The resulting battery cell after removing the adhesive film is cleaned and dried. And / or, the second adhesive comprises at least one of epoxy resin, polyurethane resin, unsaturated polyester resin, UV-curable resin, and acrylate structured resin.