A press bending forming die and a press bending forming process
By combining mold design and cooling structure, the problems of uneven stress and frictional heat generation in aluminum alloy profiles during the bending process are solved, achieving high-precision and high-quality bending results.
Patent Information
- Application Number
- CN202611362239.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-03
- Publication Date
- 2026-11-24
AI Technical Summary
In existing bending forming processes, aluminum alloy profiles are prone to local collapse and surface oxidation color difference during bending, mainly due to uneven stress on the workpiece and frictional heat generation.
The mold design adopts a combination of upper movable limiting parts and plastic upper template, and a combination of lower movable limiting parts and plastic lower template. Combined with the internal cavity and internal flow channel cooling structure, the dynamic changes of the cavity and elastic pushing force are used to ensure that the workpiece is subjected to uniform force and reduce frictional heat during the bending process.
It improves the shape accuracy and surface quality of the workpiece, avoids local collapse and surface oxidation color difference, and improves the surface protection effect after molding.
Smart Images

Figure CN123149318A_ABST
Abstract
Description
Technical Field
[0001] This application belongs to the field of profile processing technology, and more specifically, it relates to a bending forming mold and a bending forming process. Background Technology
[0002] Aluminum alloy profiles are commonly used structural components in current vehicles. They are typically long, thin-walled, hollow structures that need to be bent into shape according to the design. Existing bending processes mostly use rigid molds matched to the forming structure. The workpiece is bent under pressure in the mold cavity, rubbing against the cavity wall. Therefore, oil spraying is required in the mold cavity during the bending process for lubrication and cooling. On the one hand, the rigid bending process can easily lead to local collapse due to uneven stress on the workpiece, affecting the shape accuracy. On the other hand, oil spraying in the mold cavity can easily cause oxidation color difference defects on the workpiece surface. Summary of the Invention
[0003] The purpose of this application is to provide a bending die, which aims to improve the shape accuracy and surface quality of workpiece bending.
[0004] To achieve the above objectives, the technical solution adopted in this application is as follows: Firstly, embodiments of this application provide a bending forming mold, comprising: The upper mold assembly includes an upper mold base, an upper movable limiting member and a plastic upper template connected to the upper mold base, wherein the movable end of the upper movable limiting member faces downward and is connected to the plastic upper template; The lower mold assembly includes a lower mold base, a lower movable limiting member and a plastic lower template connected to the lower mold base, the movable end of the lower movable limiting member facing upward and connected to the plastic lower template, and a cavity for bending the workpiece is formed between the plastic lower template and the plastic upper template. During the process of the upper mold base and the lower mold base gradually closing as they approach each other, the cavity gradually changes from an initial straight shape to a curved shape based on the limited movement of the upper and lower movable limiting parts. The curved shape matches the target forming shape of the workpiece.
[0005] Compared with the prior art, the solution shown in this application embodiment adopts a combination of upper movable limiting component and plastic upper template for the upper mold assembly, and a combination of lower movable limiting component and plastic lower template for the lower mold assembly. When the workpiece is bent, the upper mold assembly and the lower mold assembly are in the open mold state, and the upper movable limiting component and the lower movable limiting component are in the initial position. At this time, a straight cavity is formed between the plastic upper template and the plastic lower template, and the workpiece to be bent can be directly placed into the straight cavity.
[0006] After the workpiece to be bent is placed in the straight cavity, the mold closes based on the downward pressing motion of the upper mold base or the upward pushing motion of the lower mold base. During the mold closing process, the top surface of the workpiece abuts against the plastic upper mold plate and the bottom surface abuts against the plastic lower mold plate. As the upper and lower mold bases approach each other, the workpiece gradually generates a reaction force on the plastic upper and lower mold plates. At this time, the plastic upper and lower mold plates gradually deform into a bent shape based on the movement of the upper and lower movable limiting parts. When the upper and lower movable limiting parts reach the limited amount of movement, the mold closes. At this time, the cavity forms a bent shape that perfectly matches the target forming shape of the workpiece, thereby realizing the bending forming of the workpiece.
[0007] By utilizing the dynamic changes of the cavity during the mold closing process, the upper and lower plastic mold plates can maintain a stable contact with the workpiece at all times. This reduces the sliding friction between the workpiece and the cavity wall, which helps to uniform the stress on the workpiece during bending, thereby improving the problem of local overpressure collapse and improving the shape accuracy of the workpiece during bending. At the same time, using the upper and lower plastic mold plates as the cavity walls not only results in a lower coefficient of friction with the workpiece surface and lower frictional heat generation, eliminating the need for oil spraying for lubrication and cooling, but also improves the surface oxidation and color difference problems caused by lubricating oil and high frictional temperatures. Furthermore, the plastic material can also protect the workpiece surface, improve the problem of surface scratches, and further improve the surface quality of the workpiece after forming.
[0008] In conjunction with the first aspect, in one possible implementation, at least one of the plastic upper template and the plastic lower template is provided with an inner cavity and / or an inner flow channel for circulating cooling medium.
[0009] Specifically, the upper plastic mold has an inner cavity, which is connected to the refrigerant circulation loop through the liquid inlet and outlet. This allows the low-temperature cooling medium to continuously enter the upper plastic mold and the cooling medium that has increased in temperature after heat exchange to continuously flow out. This cooling medium helps to cool the upper plastic mold. During the bending process, the heat dissipated by the friction of the workpiece in the cavity is transferred to the cooling medium through the upper plastic mold and discharged. This helps to avoid the problem of surface oxidation color difference caused by overheating of the workpiece during the bending process.
[0010] Optionally, the interior of the plastic upper template can be equipped with an internal flow channel instead of an inner cavity connected to the refrigerant circulation loop. The internal flow channel can be arranged in a serpentine or spiral path. The heat can also be carried away by the continuous flow of the cooling medium in the internal flow channel. In addition, compared with opening an inner cavity inside the plastic upper template, the method of setting an internal flow channel can reduce the impact on the structural strength of the plastic upper template itself, thereby reducing the risk of crushing of the plastic upper template during bending.
[0011] Optionally, the interior of the plastic upper template can also be configured as a combination structure of an inner cavity and an inner flow channel, with the inner cavity and the inner flow channel connected. The inner cavity is located in the area of the plastic upper template with a larger wall thickness, while the inner flow channel is located in the area of the plastic upper template with a smaller wall thickness and is connected to the refrigerant circulation loop, thereby improving the cooling effect of the cooling medium on the plastic upper template.
[0012] For example, the lower plastic mold is provided with an internal cavity or internal flow channel connected to a refrigerant circulation loop, or a combination of an internal cavity and an internal flow channel, thereby enabling the lower plastic mold to be cooled by a cooling medium, and thus carrying away the heat generated by friction between the workpiece and the cavity.
[0013] For example, both the upper and lower plastic molds can be equipped with internal cavities or internal flow channels, or a combination of internal cavities and internal flow channels, thereby enabling the cooling medium to simultaneously cool the upper and lower plastic molds, which is beneficial to further improve the cooling effect on the workpiece.
[0014] In some embodiments, the upper surface of the plastic upper template is provided with an elastic top plate, and the movable end of the upper movable limiting member abuts against the surface of the elastic top plate; the lower surface of the plastic lower template is provided with an elastic bottom plate, and the movable end of the lower movable limiting member abuts against the surface of the elastic bottom plate.
[0015] In the above technical solution, considering that the plastic upper mold and plastic lower mold will deform with the bending deformation of the workpiece during the bending process, elastic top plates and elastic bottom plates are set to form deformation guides on the surfaces of the two molds that are away from the cavity. At the same time, by means of the contact between the elastic top plate and the movable end of the upper movable limiting member, and the abutment between the elastic bottom plate and the movable end of the lower movable limiting member, the pressure can be evenly distributed to the plastic upper mold and plastic lower mold, thereby avoiding the problem of stress concentration on the plastic upper mold and plastic lower mold.
[0016] For example, the upper mold base has a plurality of upper limit stations distributed horizontally at intervals, and the trajectory of the bottom center line of each upper limit station matches the target forming shape of the top surface of the workpiece. The upper movable limiting component includes: Several upper pressure blocks are slidably connected to the upper mold base in the vertical direction, and each upper pressure block corresponds one-to-one with each upper limit platform. Several upper elastic elements are connected to the upper mold base and are respectively connected to each of the upper pressure blocks, for applying a downward elastic pushing force to each of the upper pressure blocks independently; During the mold closing process, each of the upper pressure blocks slides upward against the elastic pushing force based on the reaction force of the elastic top plate until it abuts against its respective upper limit position platform.
[0017] In the above technical solution, the structure and size of each upper pressure block are completely consistent. Based on this, by setting a height difference at the bottom of each upper limit platform of the upper mold base, or the lower end face used to cooperate with the upper pressure block, it is possible to make the elastic top plate that abuts against each upper pressure block form a bending state that perfectly matches the boundary trajectory of the top surface of the workpiece when the mold is closed and each upper pressure block abuts against the corresponding upper limit platform. This allows the plastic upper mold plate to change according to the bending deformation of the elastic top plate, thereby enabling the top surface area of the workpiece to obtain the target forming shape under the constraint of the plastic upper mold plate.
[0018] Throughout the bending process, the continuous elastic pushing force applied to the upper pressure block by the upper elastic element ensures that the stress on various parts of the workpiece becomes more uniform, thus mitigating the problem of localized stress concentration and collapse during bending. Furthermore, when opening the mold for the bent workpiece, the upper elastic element can release the elastic pushing force to restore the elastic top plate to its initial state, thereby restoring the plastic upper mold to its original shape and facilitating rapid demolding of the workpiece from the plastic upper mold.
[0019] For example, the upper pressure block is slidably connected to the upper mold base via an upper sliding rod. The upper sliding rod slides through an upper sliding hole in the upper mold base. One end of the upper sliding rod is screwed to the upper pressure block, and the other end extends upward through the upper sliding hole and is provided with an upper limit head. The upper sliding rod is fitted with an upper adjusting block, which is located between the upper pressure block and the upper limit platform.
[0020] In the above technical solution, the upper sliding rod and the upper sliding hole opened in the upper mold base form a sliding fit. The upper adjusting block is sleeved on the upper sliding rod and located between the upper pressure block and the upper limit station. Thus, the distance between the upper adjusting block and the upper limit station is the limited range of motion of the upper pressure block. Since the upper sliding rod and the upper pressure block adopt a detachable connection method with threaded fit, the upper adjusting block of different thickness can be replaced by removing the upper sliding rod, thereby realizing the adjustment of the limited range of motion of the upper pressure block. This can adapt to the bending requirements of different target forming shapes of the workpiece.
[0021] In one possible implementation, the lower mold base has a plurality of lower limiting platforms that are horizontally spaced apart, and the trajectory of the line connecting the top centers of each of the lower limiting platforms matches the target forming shape of the bottom surface of the workpiece. The lower movable limiting component includes: Several lower ejector blocks are slidably connected to the lower mold base in the vertical direction, and each lower ejector block corresponds one-to-one with each lower limit platform. Several lower elastic elements are connected to the lower mold base and are respectively connected to each of the lower top blocks, for applying an upward elastic pushing force to each of the lower top blocks independently; During the mold closing process, each of the lower ejector blocks slides downward against the elastic thrust based on the reaction force of the elastic base plate until it abuts against its respective lower limit platform.
[0022] In the above technical solution, during the bending process, the continuous elastic pushing force applied by the lower elastic element to the lower top block can make the stress on various positions of the workpiece more uniform, thereby improving the problem of localized stress concentration and collapse of the workpiece during bending. Furthermore, when opening the mold of the bent workpiece, the lower elastic element can release the elastic pushing force to restore the elastic base plate to its initial state, thus restoring the plastic lower mold plate to its original shape, which is beneficial for the rapid demolding of the workpiece from the plastic lower mold plate.
[0023] In some embodiments, the lower top block is slidably connected to the lower mold base via a sliding rod. The sliding rod slides through a sliding hole in the lower mold base. One end of the sliding rod is screwed to the lower top block, and the other end extends downward through the sliding hole and is provided with a lower limit head. The sliding rod is fitted with a lower adjusting block, which is located between the lower top block and the lower limit platform.
[0024] In the above technical solution, the sliding rod and the sliding hole opened in the lower mold base form a sliding fit. The lower adjusting block is sleeved on the sliding rod and located between the lower top block and the lower limit stage. Thus, the distance between the lower adjusting block and the lower limit stage is the limited movement of the lower top block. Since the sliding rod and the lower top block adopt a detachable connection method with threaded fit, the lower adjusting block of different thickness can be replaced by removing the sliding rod, thereby realizing the adjustment of the limited movement of the lower top block. This can adapt to the bending requirements of different target forming shapes of the workpiece.
[0025] In some embodiments, the upper mold base is provided with a plurality of upper limit stages, and the lower mold base is provided with a plurality of lower limit stages. The mating connection structure between the upper movable limit member and the upper mold base is the same as the mating connection structure between the lower movable limit member and the lower mold base.
[0026] In the above technical solution, both the upper and lower movable limiting parts have elastic pushing function and the ability to adjust the amount of movement. This enables the workpiece to obtain bidirectional elastic buffer during the bending process, which is beneficial to further improve the uniformity of the workpiece's stress and also facilitates the demolding of the formed workpiece.
[0027] For example, both ends of the cavity are provided with positioning clamps, which are used to block and clamp the ends of the workpiece.
[0028] In the above technical solution, by setting positioning chucks to clamp both ends of the workpiece, the axial position accuracy of the workpiece during the bending process can be improved, and the risk of axial dislocation affecting the forming dimensional accuracy when the workpiece is subjected to bending force can be reduced. On this basis, by using positioning chucks to seal the ends of the workpiece, a sealed space can be formed inside the workpiece, thereby reducing the risk of collapse during the bending process.
[0029] For example, the positioning clamp is provided with a pressure injection tube, which is used to inject pressure medium into the core cavity of the workpiece.
[0030] In the above technical solution, a pressure medium is injected into the core cavity of the workpiece through the injection pipe before mold closing. The pressure medium can improve the support of the core cavity of the workpiece, thereby reducing the risk of local collapse when the workpiece is bent, which is beneficial to improving the bending quality of the workpiece.
[0031] Secondly, this application also provides a bending forming process using the aforementioned bending forming mold, comprising the following steps: Adjust the upper mold assembly and lower mold assembly according to the target forming shape of the workpiece so that the bending shape of the cavity matches the target forming shape of the workpiece. Cooling medium is circulated into the interior of the plastic upper mold and the plastic lower mold to pre-cool the cavity and maintain the temperature of the cavity within a set range. In the open mold state, the workpiece to be bent is placed into the straight cavity, the positioning chucks on both sides of the cavity are used to clamp the workpiece, and pressure medium is injected into the core cavity of the workpiece. The upper mold base moves downwards and approaches the lower mold base to close the mold. The plastic upper mold plate drives each upper pressure block to slide upwards against the elastic pushing force of the upper elastic element. At the same time, the plastic lower mold plate drives each lower ejector block to slide downwards against the elastic pushing force of the lower elastic element. Finally, when the upper pressure block abuts against the upper limit station and the lower ejector block abuts against the lower limit station, the cavity with the bending shape is formed. The cavity is opened after being held under pressure for a set time in the bent state. The opening process is driven by the elastic pushing force of the upper and lower elastic elements to restore the cavity from the bent state to the straight state. The positioning chuck releases the formed workpiece and removes the workpiece from the cavity in the through-hole configuration.
[0032] Compared with the prior art, the solution shown in this application uses the above-mentioned bending die to perform bending operations on the workpiece to be bent. It can utilize the dynamic changes of the cavity during the mold closing process to ensure that the upper and lower plastic molds maintain a stable contact with the workpiece based on the elastic pushing force. This reduces the sliding friction between the workpiece and the cavity wall, which helps to uniform the force on the workpiece during the bending process, thereby improving the problem of local overpressure collapse of the workpiece and improving the shape accuracy of the workpiece bending. At the same time, using the upper and lower plastic molds as the cavity walls not only results in a lower coefficient of friction with the workpiece surface and lower frictional heat generation, but also allows for cooling through the water-cooling structure inside the upper and lower plastic molds. Compared with the traditional oil spraying lubrication cooling solution, this can improve the surface oxidation color difference problem caused by lubricating oil and high frictional temperature. In addition, the plastic material can also protect the workpiece surface, improve the workpiece surface scratch problem, and further improve the surface quality of the workpiece after forming. Attached Figure Description
[0033] To more clearly illustrate the technical solutions in the embodiments of this application, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0034] Figure 1 This is a three-dimensional structural diagram of the bending forming mold provided in the embodiments of this application; Figure 2 A cross-sectional view of the bending die provided in an embodiment of this application; Figure 3 The bending die provided in this application embodiment moves along the direction of the die closing process at the beginning. Figure 2 Schematic diagram of the cross-section of line AA in the middle; Figure 4 The bending die provided in this application, after being closed, follows the... Figure 2 Schematic diagram of the cross-section of line AA in the middle; Figure 5 This is a flowchart illustrating the bending forming process provided in an embodiment of this application.
[0035] In the diagram: 10. Upper mold assembly; 11. Upper mold base; 111. Upper limit stop; 12. Upper movable limit component; 121. Upper pressure block; 122. Upper elastic element; 123. Upper slide rod; 1231. Upper limit head; 124. Upper adjusting block; 13. Plastic upper mold plate; 131. Inner cavity; 132. Inner flow channel; 14. Elastic top plate; 20. Lower mold assembly; 21. Lower mold base; 211. Lower limit stop; 22. Lower movable limit component; 221. Lower top block; 222. Lower elastic element; 223. Lower slide rod; 2231. Lower limit head; 224. Lower adjusting block; 23. Plastic lower mold plate; 24. Elastic base plate; 30. Cavity; 40. Positioning chuck; 41. Injection tube; 50. Workpiece. Detailed Implementation
[0036] To make the technical problems, technical solutions, and beneficial effects to be solved by this application clearer, the following detailed description is provided in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and are not intended to limit the scope of this application.
[0037] It should be noted that when an element is referred to as being "set on" another element, it can be directly on the other element or indirectly on the other element. It should be understood that the terms "length," "height," "thickness," "upper," "lower," "front," "rear," "top," "bottom," "inner," and "outer," etc., indicating orientation or positional relationships, are based on the orientation or positional relationships shown in the accompanying drawings and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application.
[0038] It should be understood that current vehicles have increasingly higher requirements for structural strength and lightweight performance, therefore, aluminum alloy profiles are being used more and more widely as structural components in vehicles. For example, roof racks typically use thin-walled, hollow aluminum alloy profiles, which are usually made from straight blanks and processed into the designed shape through a bending process.
[0039] In related technologies, the bending forming process relies on a bending forming die structure designed to match the shape and size of the product. The bending forming die typically consists of two parts, upper and lower, which are pressed together by a hydraulic mechanism to achieve the bending forming of the workpiece. Because the die is made entirely of high-rigidity metal, many problems affecting the forming quality exist during the bending process: On the one hand, due to the difference between the cavity structure and the shape of the workpiece before bending, the bent section of the workpiece is stressed earlier than the straight section during the bending process. During this process, the workpiece often does not deform according to the target forming shape, but rather adapts to the actual stress conditions. Only after the mold is fully closed can the workpiece achieve the target forming shape based on the constraints of the cavity. Based on this bending deformation pattern, stress concentration easily forms at the bent parts of the workpiece, leading to defects such as localized collapse in hollow workpieces.
[0040] On the other hand, because relative sliding occurs between the workpiece surface and the cavity wall during bending, an oil spraying system is used to address the heat generation caused by sliding friction and the frictional damage to the workpiece surface. This system sprays lubricating oil into the cavity, lubricating the workpiece surface and reducing frictional resistance between the workpiece and the cavity wall. The lubricating oil also carries away the heat generated by friction. However, the problem with oil-lubricated cooling is that the heat generated during the instant the workpiece slides relative to the cavity wall can cause the lubricating oil adhering to the workpiece surface to burn off, resulting in color differences on the workpiece surface.
[0041] To improve the shape accuracy and surface quality of workpiece bending, please refer to the following: Figures 1 to 4 The present application provides a bending forming die. The bending forming die includes an upper die assembly 10 and a lower die assembly 20.
[0042] The upper mold assembly 10 includes an upper mold base 11, and an upper movable limiting member 12 and a plastic upper template 13 connected to the upper mold base 11. The movable end of the upper movable limiting member 12 faces downward and is connected to the plastic upper template 13. The lower mold assembly 20 includes a lower mold base 21, and a lower movable limiting member 22 and a plastic lower template 23 connected to the lower mold base 21. The movable end of the lower movable limiting member 22 faces upward and is connected to the plastic lower template 23. A cavity 30 for bending the workpiece 50 is formed between the plastic lower template 23 and the plastic upper template 13.
[0043] During the process of the upper mold base 11 and the lower mold base 21 gradually closing as they approach each other, the cavity 30 gradually changes from an initial straight shape to a curved shape based on the limited movement of the upper movable limit member 12 and the lower movable limit member 22. The curved shape matches the target forming shape of the workpiece 50.
[0044] The bending die provided in this application, compared with the prior art, has an upper die assembly 10 consisting of an upper movable limiting member 12 and a plastic upper template 13, and a lower die assembly 20 consisting of a lower movable limiting member 22 and a plastic lower template 23. When bending the workpiece 50, the upper die assembly 10 and the lower die assembly 20 are in the open state, and the upper movable limiting member 12 and the lower movable limiting member 22 are both in the initial position. At this time, a straight cavity 30 is formed between the plastic upper template 13 and the plastic lower template 23, and the workpiece 50 to be bent can be directly placed into the straight cavity 30.
[0045] After the workpiece 50 to be bent is placed in the straight cavity 30, the mold closes based on the downward pressing motion of the upper mold base 11 or the upward pushing motion of the lower mold base 21. During the mold closing process, the top surface area of the workpiece 50 abuts against the plastic upper mold plate 13, and the bottom surface area abuts against the plastic lower mold plate 23. As the upper mold base 11 and the lower mold base 21 approach each other, the workpiece 50 gradually generates a reaction force on the plastic upper mold plate 13 and the plastic lower mold plate 23. At this time, the plastic upper mold plate 13 and the plastic lower mold plate 23 gradually transform into a bent shape based on the movement of the upper movable limit member 12 and the lower movable limit member 22. When the upper movable limit member 12 and the lower movable limit member 22 reach the limited amount of movement, the mold closes. At this time, the cavity 30 forms a bent shape that perfectly matches the target forming shape of the workpiece 50, thereby realizing the bending forming of the workpiece 50.
[0046] By utilizing the dynamic changes of the cavity 30 during the mold closing process, the upper plastic template 13 and the lower plastic template 23 can maintain a stable contact with the workpiece 50 at all times. This reduces the sliding friction between the workpiece 50 and the cavity wall of the cavity 30, which helps to uniform the stress on the workpiece 50 during the bending process, thereby improving the problem of local overpressure collapse of the workpiece 50 and improving the shape accuracy of the workpiece 50 during bending. At the same time, using the upper plastic template 13 and the lower plastic template 23 as the cavity wall of the cavity 30 not only results in a smaller coefficient of friction with the surface of the workpiece 50 and lower frictional heat generation, eliminating the need for oil spraying for lubrication and cooling, but also improves the surface oxidation color difference problem caused by lubricating oil and high frictional temperature. Furthermore, the plastic material can also protect the surface of the workpiece 50, improve the surface scratch problem of the workpiece 50, and further improve the surface quality of the workpiece 50 after forming.
[0047] It should be noted that in this embodiment, the plastic upper template 13 and the plastic lower template 23 can be made of heat-conducting materials that are resistant to high temperature and have shaping ability, such as PVC, modified polytetrafluoroethylene and other heat-conducting modified materials with fixed structural form. They also have a certain ability to bend under pressure and have good processing performance, and can be processed to form a contact surface that is completely matched with the cross-section of the workpiece 50.
[0048] It should be understood that, in this embodiment, in the initial unstressed state, a straight-through cavity 30 is formed between the plastic upper mold plate 13 and the plastic lower mold plate 23, matching the straight shape of the workpiece 50 blank. During the mold closing process, the plastic upper mold plate 13 and the plastic lower mold plate 23 undergo bending deformation synchronously with the workpiece 50. Therefore, the relative sliding amount between the plastic upper mold plate 13 and the plastic lower mold plate 23 and the workpiece 50 during the bending process is almost non-existent, resulting in very little heat generated by friction. Furthermore, the plastic materials used in both molds inherently possess a low coefficient of friction, thus eliminating the need for additional lubricating oil. This avoids the problem of color difference on the surface of the workpiece 50 caused by the burning of the oil-soaked surface.
[0049] In some embodiments, to reduce the temperature between the cavity wall of the cavity 30 and the workpiece 50, please refer to... Figure 2 At least one of the plastic upper template 13 and the plastic lower template 23 is provided with an inner cavity 131 and / or an inner flow channel 132, the inner cavity 131 and / or the inner flow channel 132 for circulating cooling medium.
[0050] Here, the cooling medium can be powered by an external pumping circulation system, thereby achieving a continuous circulation state of entering and exiting the inner cavity 131 or the inner flow channel 132. The cooling medium can be oil, water, or coolant, and there is no limitation thereto.
[0051] Optionally, in this embodiment, the plastic upper template 13 is provided with an inner cavity 131. The inner cavity 131 is connected to the refrigerant circulation loop based on the liquid inlet and liquid outlet, thereby realizing that the low-temperature cooling medium continuously enters the plastic upper template 13 and the cooling medium with increased temperature after heat exchange continuously flows out. In this way, the plastic upper template 13 is cooled down by means of the cooling medium. During the bending process, the heat dissipated by the friction between the workpiece 50 and the cavity 30 is transferred to the cooling medium through the plastic upper template 13 and discharged. This helps to avoid the problem of surface oxidation color difference caused by the overheating of the workpiece 50 during the bending process.
[0052] As a modified embodiment of the aforementioned plastic upper template 13, an inner flow channel 132 can be provided inside the plastic upper template 13 to replace the inner cavity 131 and connect to the refrigerant circulation loop. The inner flow channel 132 can be arranged in a serpentine path or a spiral path. The heat can also be carried away by the continuous flow of the cooling medium in the inner flow channel 132. In addition, compared with the method of opening the inner cavity 131 inside the plastic upper template 13, the method of setting the inner flow channel 132 can reduce the impact on the structural strength of the plastic upper template 13 itself, thereby reducing the risk of crushing of the plastic upper template 13 during bending.
[0053] As another modified embodiment of the above-mentioned plastic upper template 13, the interior of the plastic upper template 13 can also be configured as a combination structure of inner cavity 131 and inner flow channel 132. The inner cavity 131 and the inner flow channel 132 are connected. The inner cavity 131 is arranged in the area with a larger wall thickness of the plastic upper template 13, while the inner flow channel 132 is arranged in the area with a smaller wall thickness of the plastic upper template 13 and is connected to the refrigerant circulation loop, thereby improving the cooling effect of the cooling medium on the plastic upper template 13.
[0054] In some embodiments, the interior of the plastic lower template 23 is provided with an inner cavity 131 or an inner flow channel 132 connected to the refrigerant circulation loop, or a combination of the inner cavity 131 and the inner flow channel 132, thereby enabling the cooling of the plastic lower template 23 by the cooling medium, and thus carrying away the heat generated by friction between the workpiece 50 and the cavity 30.
[0055] It should be noted that in this embodiment, both the plastic upper template 13 and the plastic lower template 23 can be provided with an inner cavity 131 or an inner flow channel 132, or a combination of the inner cavity 131 and the inner flow channel 132, thereby realizing the synchronous cooling of the plastic upper template 13 and the plastic lower template 23 by the cooling medium, which is beneficial to further improve the cooling effect on the workpiece 50.
[0056] For some possible implementations, please refer to [link / reference]. Figures 2 to 4 The upper surface of the plastic upper template 13 is provided with an elastic top plate 14, and the movable end of the upper movable limiting member 12 presses against the surface of the elastic top plate 14; the lower surface of the plastic lower template 23 is provided with an elastic bottom plate 24, and the movable end of the lower movable limiting member 22 presses against the surface of the elastic bottom plate 24.
[0057] Both the elastic top plate 14 and the elastic bottom plate 24 can be made of spring steel plates. By utilizing the elastic bending deformation and elastic recovery capabilities of the spring steel plates under stress, not only can the stress be evenly distributed, but the adaptability of conformal bending can also be improved. This avoids the plastic upper template 13 directly bearing the force of the upper movable limiting member 12 and the plastic lower template 23 directly bearing the force of the lower movable limiting member 22. This avoids the problem of bending shape size difference caused by abnormal deformation of the plastic upper template 13 and the plastic lower template 23, thereby ensuring the dimensional accuracy of the cavity 30 in the bending shape, which is beneficial to improving the shape accuracy of the workpiece 50 in the pressure bending process.
[0058] Considering that the plastic upper mold 13 and plastic lower mold 23 will deform during the bending process due to the bending deformation of the workpiece 50, elastic top plate 14 and elastic bottom plate 24 are provided to form deformation guides on the surfaces of the two away from the cavity 30, respectively. At the same time, by means of the contact between the elastic top plate 14 and the movable end of the upper movable limiting member 12, and the abutment between the elastic bottom plate 24 and the movable end of the lower movable limiting member 22, the pressure can be evenly distributed to the plastic upper mold 13 and plastic lower mold 23, thereby avoiding the problem of stress concentration on the plastic upper mold 13 and plastic lower mold 23.
[0059] For example, please refer to Figure 3 and Figure 4 The upper mold base 11 has several upper limit stations 111 distributed horizontally at intervals, and the trajectory of the bottom center line of each upper limit station 111 matches the target forming shape of the top surface of the workpiece 50.
[0060] The upper limit platform 111 can be a stepped structure with a height difference formed along the length of the cavity 30. Each upper limit platform 111 limits the upward movement of the upper pressure block 121. Therefore, by setting the bottom height of each upper limit platform 111, the bottom center point of each upper limit platform 111 is located on the equidistant line of the top surface outline of the workpiece 50. This allows the plastic upper template 13, which forms a curved shape after mold closing, to match the target forming shape of the top surface of the workpiece 50.
[0061] Specifically, the upper movable limiting member 12 includes several upper pressure blocks 121 and several upper elastic elements 122; the upper pressure blocks 121 are slidably connected to the upper mold base 11 in the vertical direction, and each upper pressure block 121 corresponds one-to-one with each upper limit platform 111; the upper elastic elements 122 are connected to the upper mold base 11, and each upper elastic element 122 is connected one-to-one with each upper pressure block 121, for applying a downward elastic pushing force independently to each upper pressure block 121.
[0062] During the mold closing process, each upper pressure block 121 slides upward against the elastic pushing force based on the reaction force of the elastic top plate 14 until it abuts against its corresponding upper limit position 111.
[0063] Here, the upper elastic element 122 can be a helical spring or a nitrogen spring. The sliding fit between the upper pressure block 121 and the upper mold base 11 can be achieved by using a guide groove or guide rail provided on the upper mold base 11. During the mold closing process, the upper pressure block 121 compresses the upper elastic element 122 until it abuts against the upper limit platform 111 and reaches the limit position. When the mold opens, the upper elastic element 122 releases its elastic potential energy and drives the upper pressure block 121 to slide in the opposite direction, so that the plastic upper mold plate 13 returns to its initial state based on the self-resetting ability of the elastic top plate 14.
[0064] The structure and dimensions of each upper pressure block 121 are completely identical. Based on this, by setting a height difference at the bottom of each upper limit platform 111 of the upper mold base 11, or the lower end face used to cooperate with the upper pressure block 121, the elastic top plate 14 that abuts against each upper pressure block 121 forms a bending state that perfectly matches the boundary trajectory of the top surface of the workpiece 50 when the mold is closed and each upper pressure block 121 abuts against the corresponding upper limit platform 111. This allows the plastic upper mold plate 13 to change shape according to the bending deformation of the elastic top plate 14, thereby allowing the top surface area of the workpiece 50 to obtain the target forming shape under the constraint of the plastic upper mold plate 13.
[0065] Throughout the bending process, the elastic pushing force continuously applied by the upper elastic element 122 to the upper pressure block 121 ensures that the stress on various positions of the workpiece 50 becomes more uniform, thereby improving the problem of localized stress concentration and collapse of the workpiece 50 during bending. Furthermore, when opening the mold for the bent workpiece 50, the upper elastic element 122 can release the elastic pushing force to restore the elastic top plate 14 to its initial state, thus restoring the plastic upper mold plate 13 to its original shape, which facilitates rapid demolding of the workpiece 50 from the plastic upper mold plate 13.
[0066] For details, please refer to Figure 2 The upper pressure block 121 is slidably connected to the upper mold base 11 via the upper slide rod 123. The upper slide rod 123 is slidably inserted into the upper sliding hole opened in the upper mold base 11. One end of the upper slide rod 123 is screwed to the upper pressure block 121, and the other end extends upward through the upper sliding hole and is provided with an upper limit head 1231. The upper slide rod 123 is fitted with an upper adjusting block 124, which is located between the upper pressure block 121 and the upper limit platform 111.
[0067] The upper sliding rod 123 can have a connecting thread at one end and an upper limit head 1231 with a diameter larger than the rod body at the other end. The rod body of the upper sliding rod 123 passes through the upper sliding hole. In the initial state, based on the elastic force of the upper elastic element 122, the upper limit head 1231 abuts against the top surface of the upper mold base 11 (the outer peripheral edge area of the top of the upper sliding hole), thereby constraining the upper pressure block 121 to slide downward to its limit position. During the mold closing process, the upper pressure block 121 is continuously subjected to force and overcomes the elastic force of the upper elastic element 122 to slide upward. When the upper adjusting block 124 abuts against the upper limit platform 111, it reaches the limit position of upward sliding. Therefore, the thickness of the upper adjusting block 124 determines the limited range of motion of the upper pressure block 121 in the vertical direction. By replacing the upper adjusting block 124 with different thicknesses, the limited range of motion of the upper pressure block 121 can be adjusted.
[0068] The upper slide rod 123 and the upper sliding hole opened in the upper mold base 11 form a sliding fit. The upper adjusting block 124 is sleeved on the upper slide rod 123 and located between the upper pressure block 121 and the upper limit stage 111. Thus, the distance between the upper adjusting block 124 and the upper limit stage 111 is the limited range of motion of the upper pressure block 121. Since the upper slide rod 123 and the upper pressure block 121 adopt a detachable connection with a threaded fit, the upper adjusting block 124 of different thicknesses can be replaced by removing the upper slide rod 123, thereby realizing the adjustment of the limited range of motion of the upper pressure block 121. This can adapt to the bending requirements of different target forming shapes of the workpiece 50.
[0069] For example, please refer to Figure 3 and Figure 4 The lower mold base 21 has several lower limit platforms 211 that are horizontally spaced apart, and the trajectory of the line connecting the top centers of each lower limit platform 211 matches the target forming shape of the bottom surface of the workpiece 50.
[0070] The lower limit platform 211 can be a stepped structure with a height difference formed along the length of the cavity 30. Each lower limit platform 211 forms a limit position for the downward movement of the lower top block 221. Therefore, by setting the top surface height of each lower limit platform 211, the top center point of each lower limit platform 211 is located on the equidistant line of the bottom contour line of the workpiece 50. This allows the plastic lower template 23, which forms a curved shape after mold closing, to match the target forming shape of the bottom surface of the workpiece 50.
[0071] Specifically, the lower movable limit member 22 includes several lower push blocks 221 and several lower elastic elements 222; the lower push blocks 221 are slidably connected to the lower mold base 21 in the vertical direction, and each lower push block 221 corresponds one-to-one with each lower limit platform 211; the lower elastic elements 222 are connected to the lower mold base 21, and each lower elastic element 222 is connected one-to-one with each lower push block 221, for applying an upward elastic pushing force independently to each lower push block 221.
[0072] During the mold closing process, each lower ejector block 221 slides downward against the elastic push force based on the reaction force of the elastic base plate 24 until it abuts against its corresponding lower limit platform 211.
[0073] Here, the lower elastic element 222 can be a helical spring or a nitrogen spring. The sliding fit between the lower ejector block 221 and the lower mold base 21 can be achieved by using a guide groove or guide rail provided on the lower mold base 21. During the mold closing process, the lower ejector block 221 compresses the lower elastic element 222 until it abuts against the lower limit platform 211 and reaches the limit position. When the mold opens, the lower elastic element 222 releases its elastic potential energy and drives the lower ejector block 221 to slide in the opposite direction, so that the plastic lower mold plate 23 returns to its initial state based on the self-resetting ability of the elastic base plate 24.
[0074] The structures and dimensions of each lower ejector block 221 are completely identical. Based on this, by setting a height difference on the top of each lower limit platform 211 of the lower mold base 21, or the upper end surface used to cooperate with the lower ejector block 221, the elastic base plate 24 that abuts against each lower ejector block 221 forms a bending state that perfectly matches the bottom boundary trajectory of the workpiece 50 when the mold is closed and each lower ejector block 221 abuts against the corresponding lower limit platform 211. This allows the plastic lower mold plate 23 to change shape according to the bending deformation of the elastic base plate 24, thereby allowing the bottom area of the workpiece 50 to obtain the target molding shape under the constraint of the plastic lower mold plate 23.
[0075] During the bending process, the elastic pushing force continuously applied by the lower elastic element 222 to the lower top block 221 can make the stress on various positions of the workpiece 50 more uniform, thereby improving the problem of local stress concentration and collapse of the workpiece 50 during bending. In addition, when the workpiece 50 is opened after bending, the lower elastic element 222 can release the elastic pushing force to restore the elastic base plate 24 to its initial state, thereby restoring the plastic lower template 23 to its original shape, which is beneficial for the rapid demolding of the workpiece 50 and the plastic lower template 23.
[0076] Specifically, such as Figure 2 As shown, the lower top block 221 is slidably connected to the lower mold base 21 via the lower sliding rod 223. The lower sliding rod 223 is slidably inserted into the lower sliding hole opened in the lower mold base 21. One end of the lower sliding rod 223 is screwed to the lower top block 221, and the other end extends downward out of the lower sliding hole and is provided with a lower limit head 2231. The lower sliding rod 223 is fitted with a lower adjusting block 224, which is located between the lower top block 221 and the lower limit platform 211.
[0077] The sliding rod 223 can have a connecting thread at one end and a lower limit head 2231 with a diameter larger than the rod body at the other end. The rod body of the sliding rod 223 passes through the sliding hole. In the initial state, based on the elastic force of the lower elastic element 222, the lower limit head 2231 abuts against the bottom surface of the lower mold base 21 (the outer peripheral edge area of the bottom end of the sliding hole). This can constrain the lower ejector block 221 to the limit position of upward sliding under the action of the elastic force of the lower elastic element 222. During the mold closing process, the lower ejector block 221 is continuously subjected to force and overcomes the elastic force of the lower elastic element 222 to slide downward. When the lower adjusting block 224 abuts against the lower limit platform 211, it reaches the limit position of downward sliding. Therefore, the thickness of the lower adjusting block 224 determines the limited range of motion of the lower ejector block 221 in the vertical direction. By replacing the lower adjusting block 224 with a different thickness, the limited range of motion of the lower ejector block 221 can be adjusted.
[0078] The sliding rod 223 and the sliding hole in the lower mold base 21 form a sliding fit. The lower adjusting block 224 is sleeved on the sliding rod 223 and located between the lower top block 221 and the lower limit stage 211. Thus, the distance between the lower adjusting block 224 and the lower limit stage 211 is the limited range of motion of the lower top block 221. Since the sliding rod 223 and the lower top block 221 adopt a detachable connection with a threaded fit, the lower adjusting block 224 of different thicknesses can be replaced by removing the sliding rod 223, thereby realizing the adjustment of the limited range of motion of the lower top block 221. This can adapt to the bending requirements of different target forming shapes of the workpiece 50.
[0079] It should be noted that, in order to further improve the bending forming effect, such as Figure 2 As shown, in this embodiment, the upper mold base 11 is provided with a plurality of upper limit platforms 111, and the lower mold base 21 is provided with a plurality of lower limit platforms 211. The mating connection structure between the upper movable limit member 12 and the upper mold base 11 is the same as the mating connection structure between the lower movable limit member 22 and the lower mold base 21.
[0080] In this embodiment, both the upper movable limiting member 12 and the lower movable limiting member 22 have elastic pushing function and the ability to adjust the amount of movement. This allows the workpiece 50 to obtain bidirectional elastic buffer during the bending process, which is beneficial to further improve the uniformity of the force on the workpiece 50 and also makes it easier to demold the workpiece 50 after molding.
[0081] In some embodiments, please refer to Figure 3 and Figure 4 Both ends of the cavity 30 are provided with positioning clamps 40, which are used to block and clamp the ends of the workpiece 50.
[0082] It should be noted that the positioning chuck 40 can be structurally based on a common hydraulic gripper, with an additional plug for sealing the end of the workpiece 50. The positioning chuck 40 serves two purposes: firstly, it provides radial clamping force to the end of the workpiece 50; secondly, it limits the length of the workpiece 50, preventing axial movement during bending deformation. When installing the workpiece 50 to be bent, the core cavity can be sealed first by inserting the plug into the core cavity end of the workpiece 50, and then clamping force can be applied to the workpiece 50.
[0083] By setting the positioning chuck 40 to clamp both ends of the workpiece 50, the axial position accuracy of the workpiece 50 during the bending process can be improved, and the risk of axial dislocation affecting the forming dimensional accuracy when the workpiece 50 is subjected to bending force can be reduced. On this basis, by using the positioning chuck 40 to seal the ends of the workpiece 50, a closed space can be formed inside the workpiece 50, thereby reducing the risk of collapse during the bending process of the workpiece 50.
[0084] For example, such as Figure 3As shown, in this embodiment, the positioning chuck 40 is provided with a pressure injection tube 41, which is used to inject pressure medium toward the core cavity of the workpiece 50.
[0085] The pressure medium can be a liquid or quicksand with fine particles. After the pressure medium is injected into the core cavity of the workpiece 50, the supporting effect of the core cavity formed by air pressure is greatly improved, which helps to reduce the risk of local collapse of the surface of the workpiece 50 due to core cavity collapse.
[0086] Before mold closing, pressure medium is injected into the core cavity of workpiece 50 through injection pipe 41. This pressure medium can improve the support of the core cavity of workpiece 50, thereby reducing the risk of local collapse during bending and improving the bending quality of workpiece 50. During demolding, the pressure medium in the core cavity can be extracted through injection pipe 41, thus avoiding loss and waste of pressure medium.
[0087] Here, the pressure medium can be a liquid. Both ends of the workpiece 50 are equipped with pressure injection pipes 41, and the pressure injection pipes 41 are equipped with switching valves. When bending is performed, one of the switching valves is opened, and the pressure medium is injected into the core cavity through the pressure injection pipe 41 by a pressurization system such as a pressurized water pump. When demolding is performed after bending is completed, the other switching valve is opened, and the pressure medium in the core cavity is extracted by a suction device such as a negative pressure pump, thereby preventing the pressure medium from dripping or spilling.
[0088] Based on the same inventive concept, please combine Figures 1 to 5 It is understood that this application also provides a bending forming process, which uses the above-mentioned bending forming mold and includes the following steps: S1. Adjust the upper mold assembly 10 and the lower mold assembly 20 based on the target forming shape of the workpiece 50 so that the bending shape of the cavity 30 matches the target forming shape of the workpiece 50. S2. Cooling medium is circulated into the interior of the plastic upper mold plate 13 and the plastic lower mold plate 23 to pre-cool the cavity 30 and maintain the temperature of the cavity 30 within the set range. S3. In the mold-open state, the workpiece 50 to be bent is placed into the straight cavity 30, and the workpiece 50 is clamped by the positioning chucks 40 on both sides of the cavity 30, and pressure medium is injected into the core cavity of the workpiece 50. S4. The upper mold base 11 moves down and approaches the lower mold base 21 to close the mold. The plastic upper mold plate 13 drives each upper pressure block 121 to slide upward against the elastic pushing force of the upper elastic element 122. At the same time, the plastic lower mold plate 23 drives each lower ejector block 221 to slide downward against the elastic pushing force of the lower elastic element 222. Finally, when the upper pressure block 121 abuts against the upper limit platform 111 and the lower ejector block 221 abuts against the lower limit platform 211, a curved cavity 30 is formed. S5. After the cavity 30 is held under pressure for a set time in the bent state, the mold opens. The mold opening process is driven by the elastic pushing force of the upper elastic element 122 and the lower elastic element 222 to restore the cavity 30 from the bent state to the straight state. S6. The positioning chuck 40 releases the formed workpiece 50 and removes the workpiece 50 from the cavity 30 in the through-hole configuration.
[0089] This application provides a bending forming process. Compared with the prior art, the bending forming mold described above is used to perform the bending operation on the workpiece 50 to be bent. By utilizing the dynamic changes of the cavity 30 during the mold closing process, the upper plastic template 13 and the lower plastic template 23 maintain a stable contact with the workpiece 50 based on the elastic pushing force. This reduces the sliding friction between the workpiece 50 and the cavity wall of the cavity 30, which helps to uniform the stress on the workpiece 50 during the bending process, thereby improving the problem of local overpressure collapse of the workpiece 50 and enhancing the overall appearance of the bent workpiece 50. The molding accuracy is improved. At the same time, the upper plastic template 13 and the lower plastic template 23 are used as the cavity walls of the cavity 30. This not only reduces the coefficient of friction with the surface of the workpiece 50 and reduces the heat generated by friction, but also allows for cooling through the internal cooling structure of the upper plastic template 13 and the lower plastic template 23. Compared with the traditional oil spraying lubrication cooling scheme, this can improve the surface oxidation color difference caused by lubricating oil and high friction temperature. In addition, the plastic material can also protect the surface of the workpiece 50, improve the surface scratch problem of the workpiece 50, and further improve the surface quality of the workpiece 50 after molding.
[0090] The above description is merely a preferred embodiment of this application and is not intended to limit this application. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this application should be included within the protection scope of this application.
Claims
1. A bending forming die, characterized in that, include: The upper mold assembly (10) includes an upper mold base (11), an upper movable limiting member (12) and a plastic upper template (13) connected to the upper mold base (11), wherein the movable end of the upper movable limiting member (12) faces downward and is connected to the plastic upper template (13); The lower mold assembly (20) includes a lower mold base (21), a lower movable limiting member (22) and a plastic lower template (23) connected to the lower mold base (21). The movable end of the lower movable limiting member (22) faces upward and is connected to the plastic lower template (23). A cavity (30) for bending the workpiece (50) is formed between the plastic lower template (23) and the plastic upper template (13). As the upper mold base (11) and the lower mold base (21) approach each other and gradually close, the cavity (30) gradually changes from an initial straight shape to a curved shape based on the limited movement of the upper movable limit member (12) and the lower movable limit member (22), and the curved shape matches the target forming shape of the workpiece (50).
2. The bending forming die as described in claim 1, characterized in that, At least one of the plastic upper template (13) and the plastic lower template (23) is provided with an inner cavity (131) and / or an inner flow channel (132), the inner cavity (131) and / or the inner flow channel (132) for circulating cooling medium.
3. The bending forming die as described in claim 1, characterized in that, The upper surface of the plastic upper template (13) is provided with an elastic top plate (14), and the movable end of the upper movable limiting member (12) abuts against the plate surface of the elastic top plate (14); the lower surface of the plastic lower template (23) is provided with an elastic bottom plate (24), and the movable end of the lower movable limiting member (22) abuts against the plate surface of the elastic bottom plate (24).
4. The bending forming die as described in claim 3, characterized in that, The upper mold base (11) has a plurality of upper limit platforms (111) distributed horizontally at intervals, and the trajectory of the bottom center line of each upper limit platform (111) matches the target forming shape of the top surface of the workpiece (50); the upper movable limiting member (12) includes: Several upper pressure blocks (121) are slidably connected to the upper mold base (11) in the vertical direction, and each upper pressure block (121) corresponds one-to-one with each upper limit station (111); Several upper elastic elements (122) are connected to the upper mold base (11) and are respectively connected to each of the upper pressure blocks (121) to apply a downward elastic pushing force to each of the upper pressure blocks (121) independently. During the mold closing process, each of the upper pressure blocks (121) slides upward against the elastic pushing force based on the reaction force of the elastic top plate (14) until it abuts against its respective upper limit position platform (111).
5. A bending forming die as described in claim 4, characterized in that, The upper pressure block (121) is slidably connected to the upper mold base (11) via an upper sliding rod (123). The upper sliding rod (123) is slidably inserted into the upper sliding hole opened in the upper mold base (11). One end of the upper sliding rod (123) is screwed to the upper pressure block (121), and the other end extends upward through the upper sliding hole and is provided with an upper limit head (1231). The upper sliding rod (123) is fitted with an upper adjusting block (124), which is located between the upper pressure block (121) and the upper limit platform (111).
6. A bending forming die as described in claim 3, characterized in that, The lower mold base (21) has a plurality of horizontally spaced lower limiting platforms (211), and the trajectory of the line connecting the top centers of each lower limiting platform (211) matches the target forming shape of the bottom surface of the workpiece (50); the lower movable limiting member (22) includes: Several lower top blocks (221) are slidably connected to the lower mold base (21) in the vertical direction, and each lower top block (221) corresponds one-to-one with each lower limit platform (211); Several lower elastic elements (222) are connected to the lower mold base (21) and are respectively connected to each of the lower top blocks (221) to apply an upward elastic pushing force to each of the lower top blocks (221) independently. During the mold closing process, each of the lower push blocks (221) slides downward against the elastic push force based on the reaction force of the elastic base plate (24) until it abuts against its respective lower limit platform (211).
7. A bending forming die as described in claim 6, characterized in that, The lower top block (221) is slidably connected to the lower mold base (21) via a sliding rod (223). The sliding rod (223) slides through the sliding hole opened in the lower mold base (21). One end of the sliding rod (223) is screwed to the lower top block (221), and the other end extends downward through the sliding hole and is provided with a lower limit head (2231). The sliding rod (223) is fitted with a lower adjusting block (224), which is located between the lower top block (221) and the lower limit platform (211).
8. A bending forming die as described in any one of claims 1-7, characterized in that, Both ends of the cavity (30) are provided with positioning clamps (40), which are used to block and clamp the ends of the workpiece (50).
9. A bending forming die as described in claim 8, characterized in that, The positioning chuck (40) is provided with a pressure injection tube (41), which is used to inject pressure medium into the core cavity of the workpiece (50).
10. A bending forming process, characterized in that, The bending forming die as described in any one of claims 1-9 includes the following steps: Adjust the upper mold assembly (10) and lower mold assembly (20) based on the target forming shape of the workpiece (50) so that the bending shape of the cavity (30) matches the target forming shape of the workpiece (50); Cooling medium is circulated into the interior of the plastic upper template (13) and the plastic lower template (23) to pre-cool the cavity (30) and maintain the temperature of the cavity (30) within a set range. In the open mold state, the workpiece (50) to be bent is placed into the straight cavity (30), and the workpiece (50) is clamped by the positioning chucks (40) on both sides of the cavity (30), and pressure medium is injected into the core cavity of the workpiece (50). The upper mold base (11) moves down and approaches the lower mold base (21) to close the mold. The plastic upper mold plate (13) drives each upper pressure block (121) to slide upward against the elastic pushing force of the upper elastic element (122). At the same time, the plastic lower mold plate (23) drives each lower ejector block (221) to slide downward against the elastic pushing force of the lower elastic element (222). Finally, when the upper pressure block (121) abuts against the upper limit platform (111) and the lower ejector block (221) abuts against the lower limit platform (211), the cavity (30) with the bending shape is formed. The cavity (30) is opened after holding pressure for a set time in the bent state. The opening process is driven by the elastic pushing force of the upper elastic element (122) and the lower elastic element (222) to restore the cavity (30) from the bent state to the straight state. The positioning chuck (40) releases the formed workpiece (50) and removes the workpiece (50) from the cavity (30) in the through-hole configuration.