Aluminum alloy parts for aerospace applications

By introducing a film breaker and chip return cavity structure into the aluminum alloy forging equipment, combined with a multi-stage back pressure variable die cavity mechanism, the problems of oxide film and impurity inclusions were solved, and high-quality aluminum alloy parts forming, especially forging of complex structures, was achieved.

CN123149348APending Publication Date: 2026-11-24CHENGDU JIANJIAN YOUNENG AVIATION EQUIP MFG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610806575.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-06-05
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing aluminum alloy forging equipment is prone to forming oxide films and impurity inclusions during the forging process, and it is difficult to achieve staged compaction, resulting in poor forming quality, especially for aluminum alloy parts with complex structures.

Method used

The oxide film and impurities are scraped off before the main molding by using a film breaker and a chip return cavity structure. The multi-stage back pressure variable mold cavity mechanism achieves step-by-step compaction. Combined with the flash guide, the opening timing of the flash cavity is controlled to ensure uniform material filling.

Benefits of technology

It effectively removes oxide films and impurities, improves the forming quality and cleanliness of aluminum alloy parts, meets the forging requirements of complex structures, and avoids localized incomplete filling and step marks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149348A_ABST
    Figure CN123149348A_ABST
Patent Text Reader

Abstract

The application relates to the technical field of metal plastic forming equipment, and discloses an aluminum alloy part forging forming equipment for aerospace, which comprises a base body and a guide assembly arranged on the base body. The inside of the base body is provided with a forming cavity, a flash cavity and a chip return cavity arranged adjacent to the forming cavity. The forming cavity is used for forming an aluminum alloy part body, the flash cavity is used for accommodating the flash generated in the forming process of an aluminum alloy blank, and the chip return cavity is used for receiving the chips formed after the outer edge of the aluminum alloy blank is broken. Through the arrangement of the breaker and the chip return cavity, the oxidation film, the oxide skin or the corner impurities of the outer edge of the blank are first scraped and peeled off by the breaker before the aluminum alloy blank enters the main forming area of the forming cavity, and the chips are guided into the chip return cavity, so that the risk that the oxide skin or the impurities flow into the forming cavity along with the material is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of metal plastic forming equipment technology, specifically to a forging and forming equipment for aluminum alloy parts used in aerospace. Background Technology

[0002] Aerospace aluminum alloy components typically have complex structures such as high ribs, deep cavities, thin walls, frame beams, and curved transitions, requiring high levels of filling integrity, surface quality, and internal cleanliness during the forging process. Existing aluminum alloy forging equipment usually uses an upper and lower die to press the heated aluminum alloy billet as a whole, causing the billet to plastically flow within the forming cavity and form a predetermined shape.

[0003] However, in the actual forging process, aluminum alloy billets are prone to forming oxide films, scales, or adhering edge impurities on their outer surface during heating, transfer, and placement. Existing equipment typically places the billet directly into the die cavity for pressing, lacking a structure to break the film, remove chips, and isolate the outer edge of the billet before the main forming process. This results in scale or impurities potentially flowing into the forming cavity with the metal material, thereby forming inclusion defects on the surface or inside the forging.

[0004] Meanwhile, even if existing equipment is equipped with chip removal channels, they are mostly simple containment structures, lacking a closed isolation for discharged chips. During subsequent high-pressure forming, oxide scale or chips that have entered the chip removal channels may still flow back into the forming cavity, affecting the forming quality of aluminum alloy parts.

[0005] Furthermore, existing forging equipment mostly uses a single, integral die for pressing, making it difficult to perform staged compaction according to the forming requirements of different areas of complex parts. For deep cavities, high-ribbed or thin-walled transition areas, problems such as insufficient filling, inadequate compaction, or uneven material flow are prone to occur. Moreover, the flash cavity is usually fixedly connected to the forming cavity, and material may enter the flash cavity before the main body area is fully formed, resulting in insufficient material supply to the main body area. Summary of the Invention

[0006] This invention proposes a forging and forming equipment for aerospace aluminum alloy parts that can complete the outer edge chip removal and chip removal of the billet before the main forming process, close the chip return area after chip removal, achieve multi-stage back pressure compaction during the main forming process, and control the timing of flash cavity opening.

[0007] The technical solution of the present invention is as follows: A forging and forming equipment for aluminum alloy parts for aerospace applications includes a base body and a guide assembly disposed on the base body. The base body has a forming cavity, a flash cavity, and a chip return cavity adjacent to the forming cavity. The forming cavity is used to form the main body of the aluminum alloy part, the flash cavity is used to accommodate the flash generated during the forming process of the aluminum alloy billet, and the chip return cavity is used to receive the debris formed after the outer edge of the aluminum alloy billet is broken.

[0008] The base body is equipped with a film-breaking device. This device adheres to the outer edge of the aluminum alloy billet before it enters the main forming area of ​​the forming cavity, scraping and peeling off the oxide film, scale, or edge impurities on the billet's outer edge and guiding them into the chip return cavity. The film-breaking device can exit the final forming contour of the forming cavity before the main forming stage, meaning it only participates in the film-breaking and chip removal process before main forming and does not serve as the forming surface of the final aluminum alloy part's shape.

[0009] The base body is also equipped with a closure. The closure is used to seal the entrance of the chip return chamber after the chip breaker completes chip breaking and chip removal, so as to prevent the oxide scale, debris or edge impurities that enter the chip return chamber from flowing back into the forming chamber during the subsequent main forming process.

[0010] The lifting end of the guide assembly is equipped with a back-pressure variable mold cavity mechanism. The back-pressure variable mold cavity mechanism includes a first forming device, a second forming device, and a third forming device that are sequentially nested together. The first forming device, the second forming device, and the third forming device can perform multi-stage back-pressure forming on the aluminum alloy billet according to different pressing sequences, so that the aluminum alloy billet in the forming cavity is gradually formed from the outer edge restriction and local compaction to the main body forming.

[0011] A positioner is provided between the guide assembly and the back pressure variable mold cavity mechanism, the positioner being used to limit the molding height of the back pressure variable mold cavity mechanism. A flash guide is provided on the top of the base body, the flash guide being used to control the opening or closing of the flash cavity relative to the molding cavity.

[0012] In a preferred embodiment of the present invention, the base body includes a forming base and a supporting base fixedly connected to each other. A chip discharge frame is slidably fitted inside the forming base, and the chip discharge frame communicates with the chip return cavity for collecting debris scraped off by the film-breaking device. The film-breaking device is positioned between the initial positioning area of ​​the aluminum alloy billet and the forming cavity, so that the film-breaking device breaks the outer edge of the aluminum alloy billet during the initial pressing stage, but does not serve as the final forming surface of the forming cavity during the main forming stage.

[0013] In a preferred embodiment of the present invention, the film-breaking device includes a sliding plate, a guide rail, a film-breaking side plate, and a telescopic drive component. The sliding plate is slidably mounted within the forming base via the guide rail, and the film-breaking side plate is connected to the side of the sliding plate near the forming cavity. The telescopic drive component drives the sliding plate to move the film-breaking side plate between a film-breaking position and a clearance position. When the film-breaking side plate is in the film-breaking position, it scrapes and breaks the outer edge of the aluminum alloy billet and guides the debris to the chip return cavity; when the film-breaking side plate is in the clearance position, it exits the final forming contour of the forming cavity.

[0014] In a preferred embodiment of the present invention, the closure includes a rotating shaft, a circular plate, a servo motor, a transmission chain, a hinge rod, a closing plate, and a limiting slider. The servo motor drives the rotating shaft and the circular plate to rotate via the transmission chain, and the circular plate drives the closing plate to slide via the hinge rod, thereby opening or closing the corresponding chip return cavity inlet.

[0015] In a preferred embodiment of the present invention, the guide assembly includes a main guide post, a secondary guide post, a top fixing plate, a molding cylinder, and a molding frame. The molding frame is slidably engaged with the main guide post via a main guide frame and with the secondary guide post via a secondary guide frame, so that the molding frame can stably rise and fall along the main guide post and the secondary guide post.

[0016] In a preferred embodiment of the present invention, the back-pressure variable mold cavity mechanism includes a power assembly, a first molding unit, a second molding unit, a third molding unit, and a molding guide. The power assembly is installed inside the mold frame, and the first molding unit, the second molding unit, and the third molding unit are sequentially sleeved from the outside to the inside and can slide relative to each other. The molding guide is used to control the pressing sequence of the first molding unit, the second molding unit, and the third molding unit, and to drive the first molding unit, the second molding unit, and the third molding unit to reset after molding is completed.

[0017] In a preferred embodiment of the present invention, the power assembly includes a power mounting bracket, a telescopic plate, a limiting guide shaft, and at least two back pressure units. Each back pressure unit includes a stepper motor, a worm gear drive shaft, a universal joint arm, a pressure block, a hinged top block, a worm gear shaft, and an encoder. The stepper motor drives the pressure block to move via the worm gear drive shaft, the worm gear shaft, and the universal joint arm. The pressure block transmits back pressure to the telescopic plate via the hinged top block.

[0018] In a preferred embodiment of the present invention, the first forming device includes a main template, a shielding frame, a first inner guide groove, a first forming top block, a flash forming top block, a side mounting plate, and a guide slider. The second forming device includes a second forming top block, a second inner guide groove, and a first limiting guide plate. The third forming device includes a third forming top block and a second limiting guide plate. The specific forming contours of the first forming top block, the second forming top block, and the third forming top block can be set according to the actual shape of aerospace aluminum alloy parts to adapt to the forging of high-rib, deep-cavity, frame beam, curved surface, thin-walled, or irregularly shaped complex structures.

[0019] In a preferred embodiment of the present invention, the molding guide includes a connecting guide frame, a limiting guide frame, a guide rod, and a springback assembly. The guide rod is connected to the second molding top block and the third molding top block respectively, and the guide rod corresponding to the second molding top block and the guide rod corresponding to the third molding top block have different effective lengths, so that the second molding top block and the third molding top block form different pressing strokes and resetting strokes after the first molding top block.

[0020] In a preferred embodiment of the present invention, the positioner includes a grating sensor and a grating guide post for detecting the downward pressure position of the main template relative to the forming base. The flash guide includes a flash baffle, a guide block, and a telescopic device. The telescopic device is used to drive the flash baffle to switch between a state of blocking the flash cavity and a state of opening the flash cavity.

[0021] The working principle and beneficial effects of this invention are as follows:

[0022] 1. By setting up a film-breaking device and a chip return cavity, the present invention enables the aluminum alloy billet to have its oxide film, oxide scale, or edge impurities scraped and peeled off by the film-breaking side plate before entering the main forming area of ​​the forming cavity, and guides the debris into the chip return cavity, thereby reducing the risk of oxide scale or impurities entering the forming cavity with the material flow.

[0023] 2. By switching between the breaking position and the avoidance position of the breaking side plate, the present invention enables the breaking side plate to play the role of breaking the film and guiding the chip only before the main forming stage, and to exit the final forming contour of the forming cavity before the main forming stage, so as to avoid the breaking side plate becoming the final forming surface, thereby reducing the outer edge indentation, step marks or local deflection defects of the forging.

[0024] 3. The present invention seals the inlet of the chip return chamber with a sealer, so that the oxide scale, debris or edge impurities that enter the chip return chamber after the film breaks are less likely to flow back into the forming chamber in the subsequent high-pressure forming stage, thereby improving the cleanliness and stability of the forging forming area.

[0025] 4. The present invention enables aluminum alloy billets to be formed in multiple stages of back pressure in the forming cavity according to different pressing sequences by sequentially connecting the first forming device, the second forming device and the third forming device. This realizes a step-by-step forging process from outer edge restriction, local compaction to main body forming, which helps to improve the problems of insufficient material filling and insufficient local compaction in complex cavities.

[0026] 5. The present invention uses guide rods of different effective lengths in the forming guide to enable the second forming top block and the third forming top block to form different pressing strokes and reset strokes after the first forming top block, thereby realizing multi-segment forming sequence control from a structural point of view, rather than simply relying on the overall mold to press down once.

[0027] 6. The present invention controls the opening or blocking of the flash cavity relative to the forming cavity by using a flash guide, so that the aluminum alloy material fills the forming cavity first in the early stage of the main body forming, and then enters the flash cavity to form flash after the main body forming is completed, thereby reducing the risk of insufficient filling of the main body area caused by the material entering the flash cavity too early.

[0028] 7. The specific shapes of the forming cavity, flash cavity, chip return cavity, and the first forming top block, the second forming top block, and the third forming top block of the present invention can be adapted to the actual structure of aerospace aluminum alloy parts, so it can be applied to the forging and forming of aluminum alloy parts with high ribs, deep cavities, frame beams, thin walls, curved surfaces, and irregular complex shapes. Attached Figure Description

[0029] The present invention will now be described in further detail with reference to the accompanying drawings and specific embodiments.

[0030] Figure 1 This is a schematic diagram of the overall structure of the present invention;

[0031] Figure 2 This is a schematic diagram of the overall structure of the base body of the present invention;

[0032] Figure 3 This is a schematic diagram of the internal structure of the base body of the present invention;

[0033] Figure 4 This is a bottom view of the internal structure of the base body of the present invention;

[0034] Figure 5 This is a schematic diagram of the overall structure of the membrane rupture device of the present invention;

[0035] Figure 6 This is a side view of the overall structure of the membrane rupture device of the present invention;

[0036] Figure 7 This is a schematic diagram of the overall structure of the closure device of the present invention;

[0037] Figure 8 This is a schematic diagram of the overall structure of the flash guide of the present invention;

[0038] Figure 9 This is a schematic diagram of the cylinder transmission structure for the molding die of the present invention;

[0039] Figure 10 This is a bottom view of the cylinder transmission structure for the molding die of the present invention;

[0040] Figure 11 This is a schematic diagram of the transmission structure of the side mounting plate of the present invention;

[0041] Figure 12 This is a schematic diagram of the internal structure of the back pressure variable mold cavity mechanism of the present invention;

[0042] Figure 13 This is a schematic diagram of the transmission structure of the back pressure variable mold cavity mechanism of the present invention;

[0043] Figure 14 This is a side view of the overall structure of the back pressure variable mold cavity mechanism of the present invention;

[0044] Figure 15 This is a schematic diagram of the overall structure of the power component of the present invention;

[0045] Figure 16 This is a schematic diagram of the overall structure of the back pressure device of the present invention;

[0046] Figure 17 This is a schematic diagram of the back pressure drive structure of the present invention;

[0047] Figure 18 This is an exploded structural diagram of the molding device of the present invention;

[0048] Figure 19 This is an exploded bottom view of the molding device of the present invention.

[0049] In the diagram: 1. Base body; 11. Molding base; 12. Support base; 13. Chip ejection frame; 14. Molding cavity; 15. Flash cavity;

[0050] 16. Collapse cavity;

[0051] 2. Film rupture device; 21. Sliding plate; 22. Guide rail; 23. Film rupture side plate;

[0052] 3. Enclosure; 31. Rotating shaft; 32. Circular plate; 33. Servo motor; 34. Transmission chain; 35. Hinge rod; 36. Enclosure plate; 37. Limit slider.

[0053] 4. Guide components; 41. Main guide column; 42. Secondary guide column; 43. Top fixing plate; 44. Pressing cylinder; 45. Pressing frame; 46. Main column guide frame; 47. Secondary column guide frame.

[0054] 5. Positioner; 51. Grating sensor; 52. Grating guide post.

[0055] 6. Back pressure variable mold cavity mechanism;

[0056] 61. Power assembly; 611. Power mounting bracket; 612. Telescopic plate; 613. Limiting guide shaft; 614. Back pressure unit; 6141. Stepper motor; 6142. Worm gear drive shaft; 6143. Universal joint drive arm; 6144. Top pressure block; 6145. Hinge top block; 6146. Worm gear shaft; 6147. Encoder;

[0057] 62. First forming device; 621. Main template; 622. Covering frame; 623. First inner guide groove; 624. First forming top block; 625. Flash forming top block; 626. Side mounting plate; 627. Guide slider;

[0058] 63. Second forming device; 631. Second forming top block; 632. Second inner guide groove; 633. First limiting guide plate;

[0059] 64. Third forming device; 641. Third forming top block; 642. Second limiting guide plate;

[0060] 65. Molding guide; 651. Connecting guide frame; 652. Limiting guide frame; 653. Guide rod; 654. Springback assembly;

[0061] 7. Flash guide; 71. Flash cover; 72. Guide block; 73. Expansion joint. Detailed Implementation

[0062] The technical solutions of the present invention will be clearly and completely described below with reference to the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.

[0063] Example

[0064] It should be noted that the forming cavity 14, flash cavity 15, and chip return cavity 16 shown in the attached drawings are merely schematic structures to facilitate understanding of the working principle of the present invention. In practical applications, the forming cavity 14 can be configured as a high-rib cavity, deep cavity, frame beam cavity, curved surface cavity, stepped cavity, thin-walled transition cavity, or a complex cavity formed by a combination of the above cavities, depending on the specific shape of the aerospace aluminum alloy parts; the flash cavity 15 can be configured as an annular, segmented, partially expanded, or irregularly shaped flash cavity, depending on the outer contour of the parts; the chip return cavity 16 can also be configured as a single cavity, multi-cavity, annular cavity, or segmented chip return channel, depending on the chip removal location. The cavity shapes in the attached drawings should not be construed as limitations on the actual structure of forged parts.

[0065] Example 1

[0066] like Figure 1 - Figure 19 As shown, this embodiment provides a forging and forming equipment for aluminum alloy parts for aerospace applications, including a base body 1, a mold breaker 2, a sealer 3, a guide assembly 4, a positioner 5, a back pressure variable mold cavity mechanism 6, and a flash guide 7.

[0067] The base body 1 includes a forming base 11 and a supporting base 12, with the forming base 11 fixedly mounted on the supporting base 12. The supporting base 12 is used to support the forming base 11 and the upper forging structure. The forming base 11 is used to install the forming cavity 14, the flash cavity 15, the chip return cavity 16, the film breaker 2, the closure device 3, and the flash guide 7.

[0068] The forming base 11 has a forming cavity 14, a flash cavity 15, and a chip return cavity 16 inside. The forming cavity 14 is used to form the body of the aluminum alloy part. The flash cavity 15 is located outside the forming cavity 14 and is used to accommodate the flash generated during the forging process of the aluminum alloy billet. The chip return cavity 16 is located in the adjacent area of ​​the forming cavity 14 and is used to receive the oxide scale, debris, or edge impurities formed by the scratching and peeling of the outer edge of the aluminum alloy billet during the film breaking process.

[0069] A chip discharge frame 13 is slidably fitted inside the forming base 11, and the chip discharge frame 13 is connected to the chip return chamber 16. After the chips are peeled off by the film breaker 2, they enter the chip return chamber 16 and can then continue to enter the chip discharge frame 13 for centralized collection. After a period of use, the chip discharge frame 13 can be pulled out from the forming base 11 to clean the oxide scale and chips, preventing chips from remaining in the forming base 11 for a long time and affecting subsequent forging.

[0070] In this embodiment, a non-forming transition area is formed between the initial positioning area of ​​the aluminum alloy billet and the forming cavity 14. This non-forming transition area is used to arrange the film-breaking device 2 and guide the outer edge of the billet into the forming cavity 14. It is not part of the final shaping area of ​​the aluminum alloy part. The film-breaking device 2 is located in this non-forming transition area and is used to break the film and remove chips from the outer edge of the aluminum alloy billet before it enters the main forming area of ​​the forming cavity 14.

[0071] The film-breaking device 2 includes a sliding plate 21, a guide rail 22, a film-breaking side plate 23, and a telescopic drive component. The guide rail 22 is disposed inside the molding base 11, and the sliding plate 21 is slidably mounted inside the molding base 11 via the guide rail 22. The film-breaking side plate 23 is connected to the side of the sliding plate 21 near the molding cavity 14. The telescopic drive component is connected to the sliding plate 21 and is used to drive the sliding plate 21 to slide back and forth along the guide rail 22, thereby causing the film-breaking side plate 23 to switch between the film-breaking position and the avoidance position.

[0072] When the rupture plate 23 is in the rupture position, it extends into the non-forming transition area between the initial positioning area of ​​the aluminum alloy billet and the forming cavity 14. After being subjected to initial downward pressure, the outer edge of the aluminum alloy billet expands slightly and adheres to the rupture plate 23. The rupture plate 23 scrapes and peels off the oxide film, scale, or edge impurities on the outer edge of the billet. The peeled scale and debris enter the chip return cavity 16 under the pressure of the outer edge of the billet and can further enter the chip discharge frame 13.

[0073] After the rupture side plate 23 completes rupture and chip removal, the telescopic drive drives the sliding plate 21 to retract along the guide rail 22, moving the rupture side plate 23 to a clearance position. When the rupture side plate 23 is in the clearance position, it exits the final forming contour of the forming cavity 14, so that it no longer serves as the forming boundary of the forming cavity 14. This avoids the rupture side plate 23 from continuing to compress the aluminum alloy billet during the main forming stage, thereby preventing the formation of step marks, annular indentations, or local deflection defects on the outer edge of the forging.

[0074] To ensure that the ruptured side plate 23 can reliably exit the final molded contour, its retraction stroke can satisfy the following relationship:

[0075] S23≥W23+C23

[0076] Wherein, S23 is the actual retraction stroke of the rupture side plate 23 from the rupture position to the avoidance position, W23 is the effective width of the rupture side plate 23 extending into the non-forming transition area, and C23 is the safety clearance of the rupture side plate 23 after it exits the final formed contour of the forming cavity 14. Through the above relationship, it can be ensured that the rupture side plate 23 does not participate in the final contour forming of the part during the main forming stage.

[0077] The volume of the chip return cavity 16 can be designed based on the area of ​​the oxide film breaking region on the outer edge of the aluminum alloy billet and the equivalent thickness of the oxide scale. Its effective volume can satisfy the following relationship:

[0078] V16≥K×Ap×δp

[0079] Where V16 is the effective volume of the chip return cavity 16, Ap is the equivalent area of ​​the contact between the outer edge of the aluminum alloy billet and the film breaking side plate 23, δp is the equivalent thickness of the scratched and peeled oxide film, oxide scale, or surface impurities, and K is the chip loosening correction coefficient. This relationship is used to illustrate that the chip return cavity 16 should have sufficient accommodating space, without limiting specific values.

[0080] The closure 3 is disposed inside the molding base 11 and is arranged correspondingly to the chip return cavity 16. The closure 3 includes a rotating shaft 31, a circular plate 32, a servo motor 33, a transmission chain 34, a hinge rod 35, a closing plate 36, and a limiting slider 37.

[0081] A rotating shaft 31 is rotatably mounted inside the forming base 11, and a circular plate 32 is fixedly connected to the top of the rotating shaft 31. A servo motor 33 is mounted inside the forming base 11, and the output end of the servo motor 33 is connected to the rotating shaft 31 via a transmission chain 34. Several sealing plates 36 are slidably assembled inside the forming base 11 along the circumference of the circular plate 32, and the sealing plates 36 are respectively set to different chip return cavity 16 inlets. A limiting slider 37 is provided at the bottom of the sealing plate 36, which is used to limit the sliding direction of the sealing plate 36, so that the sealing plate 36 can open or close the chip return cavity 16 inlet in a predetermined direction.

[0082] One end of the hinge rod 35 is movably hinged to the circular plate 32, and the other end is movably hinged to the closing plate 36. When the servo motor 33 drives the rotating shaft 31 and the circular plate 32 to rotate through the transmission chain 34, the circular plate 32 drives the closing plate 36 to slide through the hinge rod 35, thereby realizing the opening or closing of the inlet of the chip return cavity 16.

[0083] During the film breaking and chip removal process of the film breaker 2, the sealing plate 36 is in the open state, allowing oxide scale and debris to smoothly enter the chip return chamber 16. After the film breaker 2 completes the film breaking and chip removal and retracts to the avoidance position, the servo motor 33 drives the circular plate 32 to rotate, and the circular plate 32 pushes the sealing plate 36 to the closed position via the hinge rod 35. After the sealing plate 36 closes the entrance to the chip return chamber 16, even if the pressure inside the forming chamber 14 increases in the subsequent main forming stage, the oxide scale and debris in the chip return chamber 16 are unlikely to reverse into the forming chamber 14.

[0084] The sliding amount of the closed plate 36 can satisfy the following relationship:

[0085] S36≥B16+C36

[0086] Where S36 is the actual sliding amount of the sealing plate 36, B16 is the effective width of the inlet of the chip return cavity 16, and C36 is the sealing allowance. Through the above relationship, it can be ensured that the sealing plate 36 completely blocks the inlet of the chip return cavity 16.

[0087] The guide assembly 4 includes a main guide post 41, a secondary guide post 42, a top fixing plate 43, a molding drive cylinder 44, and a molding frame 45. The main guide post 41 and the secondary guide post 42 are mounted on the base body 1, and the top fixing plate 43 is fixedly connected to the top of the main guide post 41 and the secondary guide post 42. The molding drive cylinder 44 is mounted on the top fixing plate 43, and the molding frame 45 is mounted on the output end of the molding drive cylinder 44. The molding frame 45 slides with the main guide post 41 through the main guide frame 46 and slides with the secondary guide post 42 through the secondary guide frame 47, enabling the molding frame 45 to move stably up and down along the main guide post 41 and the secondary guide post 42.

[0088] The back pressure variable mold cavity mechanism 6 is located at the lifting end of the guide assembly 4. The back pressure variable mold cavity mechanism 6 includes a power assembly 61, a first molder 62, a second molder 63, a third molder 64, and a molding guide 65.

[0089] The power assembly 61 is installed inside the compression mold frame 45. The first molding unit 62, the second molding unit 63, and the third molding unit 64 are sequentially sleeved from the outside to the inside and can slide relative to each other. The molding guide 65 is disposed between the first molding unit 62 and the compression mold frame 45, and cooperates with the second molding unit 63 and the third molding unit 64. It is used to control the pressing sequence of the first molding unit 62, the second molding unit 63, and the third molding unit 64, and to drive each molding unit to reset after molding is completed.

[0090] The power assembly 61 includes a power mounting bracket 611, a telescopic plate 612, a limiting guide shaft 613, and at least two back pressure units 614. The power mounting bracket 611 is fixedly connected to the inside of the molding frame 45, and the telescopic plate 612 is slidably mounted inside the power mounting bracket 611. Several limiting guide shafts 613 are disposed on the top of the telescopic plate 612 and slidably pass through the power mounting bracket 611. The back pressure units 614 are mounted on the power mounting bracket 611, and the output end of the back pressure units 614 is connected to the telescopic plate 612 for driving the telescopic plate 612 to move and transmitting back pressure from the telescopic plate 612 to the first molding unit 62, the second molding unit 63, or the third molding unit 64.

[0091] The back pressure unit 614 includes a stepper motor 6141, at least two worm gear drive shafts 6142, at least two universal joint arms 6143, a top pressure block 6144, a hinged top block 6145, at least two worm wheel shafts 6146, and an encoder 6147. The worm wheel shafts 6146 are rotatably mounted on the mold frame 45, and the worm gear drive shafts 6142 are driven by their corresponding worm wheel shafts 6146 via a worm gear structure. The stepper motor 6141 is connected to one of the worm gear drive shafts 6142, and the encoder 6147 is mounted on the other worm gear drive shaft 6142. The universal joint arm 6143 is connected to the worm gear drive shaft 6142, the top pressure block 6144 is connected to the output end of the universal joint arm 6143, and the hinged top block 6145 is movably hinged to the bottom of the top pressure block 6144 and connected to the telescopic plate 612.

[0092] Through the above structure, the rotation output by the stepper motor 6141 is transmitted to the top pressure block 6144 via the worm gear drive shaft 6142, worm wheel shaft 6146, and universal drive arm 6143. The top pressure block 6144 transmits downward pressure to the telescopic plate 612 through the hinged top block 6145. The telescopic plate 612 then transmits back pressure to the first forming unit 62, the second forming unit 63, or the third forming unit 64. The encoder 6147 can detect the rotational position of the worm gear drive shaft 6142 to assist in determining the output state of the back pressure unit 614.

[0093] The first molding device 62 includes a main template 621, a shielding frame 622, a first inner guide groove 623, a first molding top block 624, a flash molding top block 625, a side mounting plate 626, and a guide slider 627. The side mounting plates 626 are respectively installed on both sides of the main template 621, and the guide slider 627 is disposed between the side mounting plates 626 and the main column guide frame 46. The shielding frame 622 is disposed on the top of the main template 621 and is inserted into the molding frame 45. The first inner guide groove 623 is disposed on the inner wall of the main template 621, and the first molding top block 624 and the flash molding top block 625 are disposed on the bottom of the main template 621.

[0094] The second molding device 63 includes a second molding top block 631, a second inner guide groove 632, and a first limiting guide plate 633. The second molding top block 631 is slidably assembled inside the main template 621 and slidably engaged with the first inner guide groove 623. The first limiting guide plate 633 is fixedly connected to the top of the second molding top block 631.

[0095] The third molding device 64 includes a third molding top block 641 and a second limiting guide plate 642. The third molding top block 641 is slidably assembled inside the second molding top block 631 and slidably engaged with the second inner guide groove 632. The second limiting guide plate 642 is disposed on the top of the third molding top block 641.

[0096] The bottom shapes of the first forming top block 624, the second forming top block 631, and the third forming top block 641 can be set according to the specific structure of the aerospace aluminum alloy parts. When the part has a high-rib structure, the first forming top block 624, the second forming top block 631, or the third forming top block 641 can be set as a compaction structure corresponding to the high-rib area; when the part has a deep cavity structure, it can be set as a forming structure corresponding to the bottom or sidewall transition area of ​​the deep cavity; when the part has a curved thin-wall structure, it can be set as a curved compaction structure matching the curved thin-wall area. Therefore, the specific shape of the forming top block can be replaced according to the complex cavity of the actual part.

[0097] The molding guide 65 includes a connecting guide frame 651, a limiting guide frame 652, guide rods 653, and a springback assembly 654. The connecting guide frame 651 is connected to the main template 621, and the limiting guide frame 652 is connected to the power mounting bracket 611. Several guide rods 653 are disposed between the connecting guide frame 651 and the limiting guide frame 652. The springback assembly 654 is sleeved on the guide rods 653, and its two ends are connected to the connecting guide frame 651 and the limiting guide frame 652, respectively. The guide rods 653 are connected to the second molding top block 631 and the third molding top block 641, respectively, and the guide rods 653 corresponding to the second molding top block 631 and the third molding top block 641 have different effective lengths. Through the difference in the effective length of the guide rods 653, the second molding top block 631 and the third molding top block 641 can form different pressing strokes and reset strokes after the first molding top block 624.

[0098] To illustrate the pressing sequence of the first forming unit 62, the second forming unit 63, and the third forming unit 64, we can assume that the pressing displacement of the first forming unit 62 when it begins to contact the aluminum alloy blank is H1, the pressing displacement of the second forming unit 63 when it begins to participate in forming is H2, and the pressing displacement of the third forming unit 64 when it begins to participate in forming is H3. This will satisfy the following conditions:

[0099] H1 < H2 < H3

[0100] Through this relationship, the first forming device 62 first restricts the outer edge and initially compacts the blank, the second forming device 63 then further compacts the local area, and the third forming device 64 finally compacts the main area, the central area, the deep cavity area or the final forming area.

[0101] The molding pressure at each stage can be checked according to the following relationship:

[0102] Pi = Fi / Ai

[0103] Where Pi is the equivalent forming pressure of the i-th stage, Fi is the downward pressure of the forming device corresponding to the i-th stage, and Ai is the effective contact area between the forming device and the aluminum alloy blank corresponding to the i-th stage. i corresponds to the first forming device 62, the second forming device 63, and the third forming device 64, respectively. In order to achieve a step-by-step process from outer edge restriction and local compaction to main body forming, the pressure relationship can be made to satisfy:

[0104] P1≤P2≤P3

[0105] Wherein, P1 is the equivalent pressure during the operation of the first forming device 62, P2 is the equivalent pressure during the operation of the second forming device 63, and P3 is the equivalent pressure during the operation of the third forming device 64. This relationship is used to illustrate the design principle of progressively increasing pressure in each stage of multi-stage back pressure forming, and does not limit specific pressure values.

[0106] The positioner 5 includes a grating sensor 51 and a grating guide post 52. The grating guide post 52 is disposed on both sides of the back pressure variable molding cavity mechanism 6 and is connected to the molding base 11 and the top fixing plate 43, respectively. The grating sensor 51 is disposed on both sides of the main template 621 and cooperates with the grating guide post 52 to detect the downward pressure position of the main template 621 relative to the molding base 11. Through the positioner 5, it is possible to determine whether the back pressure variable molding cavity mechanism 6 has reached the end position of the film breaking stage, the first molding stage position, the second molding stage position, the third molding stage position, and the molding termination position, thereby ensuring the stability of the molding height.

[0107] The flash guide 7 includes a flash baffle 71, a guide block 72, and a telescopic device 73. The flash baffle 71 is slidably mounted in the molding base 11 and is correspondingly positioned between the flash cavity 15 and the molding cavity 14. The telescopic device 73 is installed on one side of the molding base 11, and its output end is connected to the flash baffle 71. The guide block 72 is located at the bottom of the flash baffle 71 and is slidably mounted in the molding base 11 to limit the sliding direction of the flash baffle 71.

[0108] During the initial pressing, film breaking, and early stage of main body forming of aluminum alloy billet, the flash baffle 71 is in a state of blocking the flash cavity 15, so that the aluminum alloy billet does not enter the flash cavity 15 too early. After the first forming device 62, the second forming device 63, and the third forming device 64 complete the forming action in sequence, the telescopic device 73 drives the flash baffle 71 to open the flash cavity 15, allowing excess aluminum alloy material to enter the flash cavity 15 to form flash.

[0109] The opening stroke of the burr cover 71 can satisfy the following relationship:

[0110] S71≥B15+C71

[0111] Wherein, S71 is the actual opening stroke of the flash baffle 71, B15 is the effective width of the inlet of the flash cavity 15, and C71 is the safety margin for opening the flash cavity 15. Through this relationship, it can be ensured that the flash cavity 15 is fully opened when material discharge is required.

[0112] The complete working process of this equipment is as follows: First, the heated aerospace-grade aluminum alloy billet is placed into the initial positioning area of ​​the billet on the base body 1. At this time, the rupture side plate 23 is in the rupture position, the sealing plate 36 is in the position where the inlet of the chip return chamber 16 is opened, and the flash baffle plate 71 is in the position where the flash baffle chamber 15 is blocked. Subsequently, the die drive cylinder 44 drives the die frame 45 to descend along the main guide column 41 and the auxiliary guide column 42. After the aluminum alloy billet is subjected to initial pressure, the outer edge expands slightly and comes into contact with the rupture side plate 23. The rupture side plate 23 scrapes and peels off the oxide film, oxide scale, or edge impurities on the outer edge of the billet, and the debris enters the chip return chamber 16 and further enters the chip discharge frame 13.

[0113] After the film breaking is completed, the telescopic drive drives the sliding plate 21 to retract along the guide rail 22, causing the film-breaking side plate 23 to exit the final molding contour of the molding cavity 14. Subsequently, the closure 3 is activated, and the servo motor 33 drives the rotating shaft 31 and the circular plate 32 to rotate through the transmission chain 34. The circular plate 32 pushes the closure plate 36 to the closed position through the hinge rod 35, thereby closing the entrance of the chip return cavity 16 and preventing debris from flowing back into the molding cavity 14 in the subsequent main molding stage.

[0114] After the mold-breaking side plate 23 is cleared and the inlet of the chip return cavity 16 is closed, the back pressure variable mold cavity mechanism 6 enters the main forming stage. The first forming device 62 first presses down, and the first forming top block 624 restricts the outer edge of the aluminum alloy billet and initially compacts it; then, the second forming device 63 presses down further under the action of the forming guide 65, and the second forming top block 631 compacts the local area; then, the third forming device 64 presses down further, and the third forming top block 641 compacts the main body area, the central area, the deep cavity area or the final forming area, so that the aluminum alloy billet completes the main body forming step by step in the forming cavity 14.

[0115] During the main body forming process, the flash baffle 71 keeps the flash cavity 15 blocked, allowing the aluminum alloy material to fill the main body first within the forming cavity 14. After the main body forming is completed, the telescopic device 73 drives the flash baffle 71 to open the flash cavity 15, allowing excess aluminum alloy material to enter the flash cavity 15 and form flash. After forming is completed, the mold drive cylinder 44 drives the mold frame 45 to rise, and the springback component 654 drives the corresponding forming device to reset, restoring the equipment to its initial state.

[0116] Example 2

[0117] Based on Embodiment 1, the film-breaking side plate 23 can be configured as a segmented structure, with multiple film-breaking side plates 23 arranged at intervals along the outer edge of the aluminum alloy billet, forming a chip-guiding gap between adjacent film-breaking side plates 23. This structure is suitable for film breaking at the outer edge of round, elliptical, rectangular, or irregularly shaped billets. The segmented film-breaking side plate 23 can reduce the overall film-scraping resistance and allow the peeled oxide scale to enter the corresponding chip return cavity 16 along each chip-guiding gap.

[0118] In this embodiment, each film-breaking side plate 23 can be individually retracted by the corresponding sliding plate 21 and guide rail 22, or it can be synchronously driven by the same telescopic drive member through the linkage plate. As long as it can enter the film-breaking position during the film-breaking stage and exit the final molding contour of the molding cavity 14 before the main molding stage, the purpose of the present invention can be achieved.

[0119] Example 3

[0120] Based on Embodiment 1 or Embodiment 2, the forming cavity 14 can be configured as a cavity for complex aerospace structural parts. For example, the forming cavity 14 may include a high-rib forming area, a deep cavity forming area, a thin-walled forming area, and a curved surface transition forming area. Correspondingly, the first forming top block 624 can be used for outer edge restriction and large-area initial pressing, the second forming top block 631 can be used for compaction of the high-rib root or thin-walled transition area, and the third forming top block 641 can be used for compaction of the deep cavity bottom, central area, or final forming area.

[0121] With this arrangement, the back pressure variable mold cavity mechanism 6 can adapt to more complex aerospace aluminum alloy component structures, and is not limited to the simple cavity shape shown in the attached figure.

[0122] Example 4

[0123] Based on the above embodiments, the flash cavity 15 can adopt a segmented flash cavity structure. The flash baffle 71 can also be correspondingly configured as a segmented baffle. Multiple flash baffles 71 can be synchronously driven by the same telescopic member 73, or they can be driven separately by multiple telescopic members 73 in sections. For aerospace aluminum alloy parts with irregular outer contours, the opening timing of different flash baffles 71 can be selected according to the material flow state at different flash positions to improve the stability of flash formation.

[0124] Through the above specific embodiments, the present invention can complete the outer edge film breaking, chip removal, and chip sealing before the aluminum alloy billet enters the main forming area of ​​the forming cavity 14. During the main forming process, multi-stage back pressure compaction is achieved through the first forming device 62, the second forming device 63, and the third forming device 64. After the main body is formed, the flash guide 7 controls the opening of the flash cavity 15. This process can reduce the risk of oxide scale inclusions and chip backflow, while improving the step-by-step forming effect of complex aluminum alloy forgings.

[0125] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. A forging and forming equipment for aluminum alloy parts for aerospace applications, comprising a base body (1) and a guide assembly (4) disposed on the base body (1), characterized in that: The base body (1) is provided with a forming cavity (14), a flash cavity (15), and a chip return cavity (16) adjacent to the forming cavity (14). The forming cavity (14) is used to form the main body of the aluminum alloy parts, the flash cavity (15) is used to accommodate the flash generated during the forming process of the aluminum alloy blank, and the chip return cavity (16) is used to receive the chips formed after the outer edge of the aluminum alloy blank is broken. The base body (1) is provided with a film-breaking device (2). The film-breaking device (2) can fit against the outer edge of the aluminum alloy blank before the aluminum alloy blank enters the main forming area of ​​the forming cavity (14) to scrape and peel off the oxide film, oxide scale or corner impurities on the outer edge of the aluminum alloy blank and introduce them into the chip return cavity (16). The film-breaking device (2) can exit the final forming contour of the forming cavity (14) before the main forming stage. The base body (1) is provided with a closure (3) inside. The closure (3) is used to close the entrance of the chip return chamber (16) after the film breaker (2) completes the film breaking and chip removal, so as to prevent the chips from flowing back to the molding chamber (14). The lifting end of the guide component (4) is provided with a back pressure variable mold cavity mechanism (6). The back pressure variable mold cavity mechanism (6) includes a first forming device (62), a second forming device (63), and a third forming device (64) that are sequentially fitted together. The first forming device (62), the second forming device (63), and the third forming device (64) can perform multi-stage back pressure forming on the aluminum alloy billet according to different pressing sequences, so that the aluminum alloy billet in the forming cavity (14) is gradually formed from the outer edge restriction and local compaction to the main body forming. A positioner (5) is provided between the guide component (4) and the back pressure variable mold cavity mechanism (6), and the positioner (5) is used to limit the molding height of the back pressure variable mold cavity mechanism (6); The top of the base body (1) is provided with a flash guide (7), which is used to control the opening or blocking of the flash cavity (15) relative to the molding cavity (14).

2. The forging equipment for aerospace aluminum alloy parts according to claim 1, characterized in that: The base body (1) includes a molded base (11) and a support base (12) that are fixedly connected to each other. The support base (12) is used to support the molded base (11). The molding base (11) is slidably fitted with a chip discharge frame (13), which is connected to the chip return chamber (16) and is used to collect the debris scraped off by the film breaker (2). The molding cavity (14) is located inside the molding base (11), and the flash cavity (15) is located outside the molding cavity (14); The film-breaking device (2) is positioned between the initial positioning area of ​​the aluminum alloy billet and the forming cavity (14), so that the film-breaking device (2) breaks the outer edge of the aluminum alloy billet in the initial pressing stage, and does not serve as the final forming surface of the forming cavity (14) in the main forming stage.

3. The forging equipment for aerospace aluminum alloy parts according to claim 2, characterized in that: The membrane rupture device (2) includes a sliding plate (21), a guide rail (22), a membrane rupture side plate (23), and a telescopic drive component; The guide rail (22) is disposed inside the molding base (11), the sliding plate (21) is slidably assembled inside the molding base (11) through the guide rail (22), and the film breaking side plate (23) is connected to the side of the sliding plate (21) near the molding cavity (14). The telescopic drive is connected to the sliding plate (21) and is used to drive the sliding plate (21) to move the membrane breaking side plate (23) between the membrane breaking position and the avoidance position; When the film-breaking side plate (23) is in the film-breaking position, it extends between the initial positioning area of ​​the aluminum alloy billet and the forming cavity (14) to scrape and break the film on the outer edge of the aluminum alloy billet and guide the debris to the chip return cavity (16). When the membrane-breaking side plate (23) is in the avoidance position, it exits the final forming contour of the forming cavity (14) so ​​that the aluminum alloy blank can enter the forming cavity (14) to complete the main forming.

4. The forging equipment for aerospace aluminum alloy parts according to claim 2, characterized in that: The closure (3) includes a rotating shaft (31), a circular plate (32), a servo motor (33), a transmission chain (34), a hinge rod (35), a closing plate (36), and a limiting slider (37). The rotating shaft (31) is rotatably mounted inside the molding base (11), and the circular plate (32) is fixedly connected to the top of the rotating shaft (31); The servo motor (33) is installed inside the molding base (11), and the output end of the servo motor (33) is connected to the rotating shaft (31) through the transmission chain (34). Several of the closed plates (36) are slidably assembled in the molding base (11) along the circumference of the circular plate (32), and the limiting slider (37) is disposed at the bottom of the closed plate (36) and is used to limit the sliding direction of the closed plate (36); One end of the hinge rod (35) is movably hinged to the circular plate (32), and the other end is movably hinged to the closing plate (36), so that when the circular plate (32) rotates, it can drive several of the closing plates (36) to slide synchronously, so as to open or close the corresponding chip return cavity (16) inlet.

5. The forging equipment for aerospace aluminum alloy parts according to claim 1, characterized in that: The guide assembly (4) includes a main guide post (41), a secondary guide post (42), a top fixing plate (43), a molding cylinder (44), and a molding frame (45). The main guide post (41) and the auxiliary guide post (42) are disposed on the base body (1), and the top fixing plate (43) is fixedly connected to the top of the main guide post (41) and the auxiliary guide post (42); The molding cylinder (44) is mounted on the top fixing plate (43), and the molding frame (45) is mounted on the output end of the molding cylinder (44); The molding frame (45) slides with the main guide frame (46) and the main guide column (41), and slides with the auxiliary guide frame (47) and the auxiliary guide column (42), so that the molding frame (45) can move stably up and down along the main guide column (41) and the auxiliary guide column (42).

6. The forging equipment for aerospace aluminum alloy parts according to claim 5, characterized in that: The back pressure variable mold cavity mechanism (6) includes a power assembly (61), a first molding unit (62), a second molding unit (63), a third molding unit (64), and a molding guide (65). The power assembly (61) is installed inside the molding frame (45), and the first molding unit (62), the second molding unit (63) and the third molding unit (64) are sequentially sleeved from the outside to the inside and can slide relative to each other; The molding guide (65) is disposed between the first molding device (62) and the molding frame (45), and cooperates with the second molding device (63) and the third molding device (64); The power assembly (61) is used to provide back pressure to the first molding machine (62), the second molding machine (63) and the third molding machine (64); The molding guide (65) is used to control the order of pressing down the first molding device (62), the second molding device (63) and the third molding device (64), and to drive the first molding device (62), the second molding device (63) and the third molding device (64) to reset after molding is completed.

7. The forging equipment for aerospace aluminum alloy parts according to claim 6, characterized in that: The power assembly (61) includes a power mounting bracket (611), a telescopic plate (612), a limiting guide shaft (613), and at least two back pressure units (614). The power mounting bracket (611) is fixedly connected to the inside of the molding frame (45), and the telescopic plate (612) is slidably assembled inside the power mounting bracket (611); Several of the aforementioned limiting guide shafts (613) are disposed on the top of the telescopic plate (612) and are slidably inserted into the power mounting frame (611); The back pressure unit (614) is mounted on the power mounting bracket (611), and the output end of the back pressure unit (614) is connected to the telescopic plate (612) to drive the telescopic plate (612) to transmit back pressure to the first molding machine (62), the second molding machine (63) or the third molding machine (64); The back pressure unit (614) includes a stepper motor (6141), a worm gear drive shaft (6142), a universal drive arm (6143), a top pressure block (6144), a hinged top block (6145), a worm gear shaft (6146), and an encoder (6147). The worm gear shaft (6146) is rotatably mounted on the mold frame (45), and the worm drive shaft (6142) is in transmission cooperation with the worm gear shaft (6146) through the worm gear structure; The stepper motor (6141) is connected to one of the worm gear drive shafts (6142), and the encoder (6147) is mounted on the other worm gear drive shaft (6142). The universal drive arm (6143) is connected to the worm gear drive shaft (6142), the top pressure block (6144) is connected to the output end of the universal drive arm (6143), and the hinged top block (6145) is movably hinged to the bottom of the top pressure block (6144) and connected to the telescopic plate (612).

8. The forging equipment for aerospace aluminum alloy parts according to claim 6, characterized in that: The first molding device (62) includes a main template (621), a shielding frame (622), a first inner guide groove (623), a first molding top block (624), a flash molding top block (625), a side mounting plate (626), and a guide slider (627). The side mounting plates (626) are respectively installed on both sides of the main template (621), and the guide slider (627) is disposed between the side mounting plates (626) and the main column guide frame (46); The shielding frame (622) is disposed on the top of the main template (621) and is inserted into the molding frame (45); The first inner guide groove (623) is disposed on the inner wall of the main template (621), and the first forming top block (624) and the flash forming top block (625) are disposed on the bottom of the main template (621); The second molding device (63) includes a second molding top block (631), a second inner guide groove (632), and a first limiting guide plate (633). The second molding top block (631) is slidably assembled inside the main template (621) and slidably engaged with the first inner guide groove (623). The first limiting guide plate (633) is fixedly connected to the top of the second molding top block (631). The third molding device (64) includes a third molding top block (641) and a second limiting guide plate (642). The third molding top block (641) is slidably assembled inside the second molding top block (631) and slidably cooperates with the second inner guide groove (632). The second limiting guide plate (642) is disposed on the top of the third molding top block (641).

9. A forging and forming equipment for aerospace aluminum alloy parts according to claim 8, characterized in that: The molding guide (65) includes a connecting guide frame (651), a limiting guide frame (652), a guide rod (653), and a springback assembly (654). The connecting guide frame (651) is connected to the main template (621), and the limiting guide frame (652) is connected to the power mounting frame (611); A plurality of guide rods (653) are disposed between the connecting guide frame (651) and the limiting guide frame (652), and the spring-loaded assembly (654) is sleeved on the guide rods (653), and the two ends of the spring-loaded assembly (654) are respectively connected to the connecting guide frame (651) and the limiting guide frame (652). The guide rod (653) is connected to the second molding top block (631) and the third molding top block (641) respectively, and the guide rod (653) corresponding to the second molding top block (631) and the guide rod (653) corresponding to the third molding top block (641) have different effective lengths, so that the second molding top block (631) and the third molding top block (641) form different pressing strokes and reset strokes after the first molding top block (624).

10. A forging and forming equipment for aerospace aluminum alloy parts according to claim 2, characterized in that: The positioner (5) includes a grating sensor (51) and a grating guide post (52). The grating guide post (52) is disposed on both sides of the back pressure variable mold cavity mechanism (6) and is connected to the molding base (11) and the top fixing plate (43) respectively. The grating sensor (51) is disposed on both sides of the main template (621) and cooperates with the grating guide post (52) to detect the downward pressure position of the main template (621) relative to the molding base (11); The flash guide (7) includes a flash cover (71), a guide block (72), and a telescopic device (73). The flash cover (71) is slidably mounted in the molding base (11) and is correspondingly disposed between the flash cavity (15) and the molding cavity (14). The telescopic device (73) is installed on one side of the molding base (11), and the output end of the telescopic device (73) is connected to the flash cover (71). The guide block (72) is disposed at the bottom of the flash cover (71) and slidably mounted in the molding base (11) so that the flash cover (71) can switch between blocking the flash cavity (15) and opening the flash cavity (15).