A high-grade non-oriented electrical steel slab casting method and slab

By controlling the differentiated settings of slab casting speed, crystallizer cooling water temperature, and electromagnetic stirring power, a slab structure with primary columnar crystals, secondary columnar crystals, and fine equiaxed crystal layers is formed, solving the problem of balancing surface quality and magnetic properties in high-grade non-oriented electrical steel slabs, and achieving a high-efficiency balance between quality and performance.

CN123149378APending Publication Date: 2026-11-24SHOUGANG ZHIXIN QIAN AN ELECTROMAGNETIC MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611278801.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-21
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In the existing technology, it is difficult to achieve both surface quality and magnetic properties in high-grade non-oriented electrical steel slabs. Existing solutions result in an excessively high proportion of columnar crystals or equiaxed crystals, which respectively lead to surface defects or deterioration of magnetic properties.

Method used

By controlling the slab casting speed, crystallizer cooling water temperature, electromagnetic stirring power, and cooling intensity with differentiated settings, a slab structure with primary columnar crystals, secondary columnar crystals, and fine equiaxed crystal layers is formed. Combined with slow cooling treatment, a precise spatial distribution of columnar and equiaxed crystals is achieved.

Benefits of technology

It achieves a balance between surface quality and magnetic properties of high-grade non-oriented electrical steel slabs, reducing the risk of surface defects and improving magnetic properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149378A_ABST
    Figure CN123149378A_ABST
Patent Text Reader

Abstract

The application belongs to the technical field of steel smelting continuous casting, and particularly relates to a high-grade non-oriented electrical steel slab casting method and a slab. The prior art adopts a one-size-fits-all mode, that is, only a controlled cooling system is adopted or full electromagnetic stirring is adopted, resulting in that the proportion of columnar crystals is too high to deteriorate surface quality or the proportion of equiaxed crystals is too high to deteriorate magnetic properties; the scheme differentiates the electromagnetic stirring power and the cooling intensity in different cooling sections, adopts small-power first electromagnetic stirring treatment to hinder the extension of coarse columnar crystals in the 2nd cooling section to the 3rd cooling section, adopts large-power second electromagnetic stirring treatment to form secondary columnar crystals in cooperation with strong water spray cooling in the 4th cooling section to the 5th cooling section, and adopts slow cooling treatment to form equiaxed crystals in the 6th cooling section to the 8th cooling section, so that the precise spatial distribution control of columnar crystals and equiaxed crystals is realized, and thus the technical bottleneck that surface quality and magnetic properties cannot be considered simultaneously in the prior art is broken through.