Metal composite material and manufacturing method, mobile phone middle frame

By forming a lattice structure on a metal substrate and filling it with metal bonding material using high-pressure casting technology, the problem of insufficient bonding strength in steel/aluminum, titanium/aluminum, magnesium/aluminum, and copper/aluminum composite plates during the rolling composite process has been solved, achieving efficient integrated bonding and large-scale production.

CN123149388APending Publication Date: 2026-11-24JIANGYIN KANGRUI MOLDING TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510625480.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-15
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In existing technologies, it is difficult to achieve high bonding strength in the rolling and bonding process of steel/aluminum, titanium/aluminum, magnesium/aluminum, and copper/aluminum composite plates, resulting in unstable quality of composite plates and making it difficult to achieve large-scale production and automation.

Method used

A lattice structure is formed on a metal substrate using 3D printing technology. The support has a bonding layer and hollow holes. Metal bonding material is filled by high-pressure casting. The lattice structure is used to realize the metallurgical reaction between the metal substrate and the bonding material to form a strong bond.

Benefits of technology

It improves the bonding strength of metal composite materials and achieves efficient integrated bonding between metal substrate and bonding material, making it suitable for large-scale production and automated manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149388A_ABST
    Figure CN123149388A_ABST
Patent Text Reader

Abstract

The present application relates to a kind of metal composite material and manufacturing method, cell phone middle frame, a kind of metal composite material, including metal base material, at least one bonding interface is formed on the metal base material, lattice structure body is formed on the bonding interface, the lattice at least includes several support bodies along the bonding interface of the metal base material, several support bodies are formed with bonding layer, several hollow holes are provided on the bonding layer;Metal bonding material is bonded on the metal base material, the metal bonding material also has at least one bonding interface, the bonding interface of the metal bonding material is filled between the lattice structure body, the metal base material and the metal bonding material are bonded by the lattice structure body;Since the metal bonding material fills in the space portion in lattice structure body, therefore, it is firmly bonded and integrated by anchoring effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of metal bonding manufacturing technology, and in particular to a metal composite material and its manufacturing method, and a mobile phone mid-frame. Background Technology

[0002] With the advent of the smart era, people's demand for mobile phones has greatly increased. In order to win the favor of more consumers, mobile phone manufacturers are racking their brains to innovate and design various components. As a component of the mobile phone, the mid-frame and cover glass have undergone many twists and turns in the process of manufacturing. Among them, the processing technology is extremely critical, as the choice of technology directly affects the yield rate and production efficiency.

[0003] Steel / aluminum, titanium / aluminum, magnesium / aluminum, and copper / aluminum composite plates combine the high strength and good plasticity of one metal with the excellent electrical and thermal conductivity, corrosion resistance, and low density of another. Steel / aluminum composite plates are used in subway contact rails in the rail transit sector, as body materials for automobiles and high-speed trains, and as bearing materials for engines. Utilizing the good thermal conductivity of aluminum, various steel / aluminum and titanium / aluminum composite heat sinks and cookware are also available on the market. Furthermore, steel / aluminum, titanium / aluminum, magnesium / aluminum, and copper / aluminum composite plates are widely used in many fields such as machinery, shipbuilding, nuclear energy, and power. Especially with the development of smartphones and 5G technology, steel / aluminum, titanium / aluminum, magnesium / aluminum, and copper / aluminum composite plates, due to their unique properties, are also being used in the production of smartphone frames.

[0004] However, due to significant differences in material properties (deformation resistance, plasticity, thermal conductivity, melting point, etc.) between the two metals, the fabrication of steel / aluminum, titanium / aluminum, magnesium / aluminum, and copper / aluminum composite plates presents certain challenges. Current preparation methods mainly include explosive bonding, brazing bonding, and rolling bonding. Compared to explosive bonding and brazing bonding, rolling bonding offers more stable product quality, simpler equipment, and is easier to scale up and automate. However, during the rolling bonding process of steel / aluminum, titanium / aluminum, magnesium / aluminum, and copper / aluminum composite plates, the combination of two different materials (steel / aluminum, titanium / aluminum, magnesium / aluminum, and copper / aluminum) makes it difficult to achieve high bonding strength in the rolled composite plate. Summary of the Invention

[0005] The purpose of this invention is to overcome the defects existing in the prior art and provide a metal composite material and its manufacturing method, as well as a mobile phone mid-frame.

[0006] To achieve the above objectives, the technical solution of the present invention is to design a metal composite material, characterized in that it includes a metal substrate, the metal substrate having at least one bonding interface, a lattice structure being formed on the bonding interface, the lattice including at least a plurality of supports protruding along the bonding interface of the metal substrate, a bonding layer being formed on the plurality of supports, and a plurality of hollow holes being provided on the bonding layer. A metal bonding material is bonded to the metal substrate, and the metal bonding material also has at least one bonding interface. The bonding interface of the metal bonding material fills the spaces between the crystal structures, and the metal substrate and the metal bonding material are bonded through the crystal structures.

[0007] A further preferred technical solution is that the lattice structure includes a plurality of supports protruding in the direction perpendicular to the bonding interface, the supports being cylindrical in shape, and the diameter of the cylinders being between 0.8mm and 1.2mm.

[0008] In a further preferred embodiment, a bonding layer is provided on several of the supports, and the distance between the bonding layer and the bonding interface of the metal substrate is 0.25-0.35 mm.

[0009] A method for manufacturing a metal composite material, characterized by comprising at least the following steps: forming a metal lattice structure on a metal substrate using a 3D printer, wherein the lattice comprises at least a plurality of supports protruding along the bonding interface of the metal substrate, a bonding layer is formed on the plurality of supports, and the bonding layer is provided with a plurality of hollow holes. Metal bonding material is filled into the space within the lattice structure by high-pressure casting; the metal substrate and the metal bonding material are bonded through the lattice structure.

[0010] A further preferred technical solution is to perform surface treatment on the surface of the crystal structure before filling the metal bonding material into the crystal structure; and to perform heat treatment to relieve stress or temper the crystal structure after the crystal structure is formed.

[0011] A mobile phone frame includes a phone border, which includes at least a first border, a second border, a third border, and a fourth border. The first border and the third border are symmetrically arranged, as are the second border and the fourth border. The phone border is composed of a metal substrate. The mobile phone frame also includes a middle plate disposed within the phone border and formed by a metal bonding material. The middle plate is characterized in that a bonding interface is formed on the inner surface of the phone border, and a lattice structure is formed on the bonding interface. The lattice structure includes at least a plurality of supports protruding along the bonding interface of the phone border, and a bonding layer is formed on the plurality of supports. The bonding layer has a plurality of perforations. The middle plate fills the spaces between the lattice structures, and the phone border and the middle plate are bonded through the lattice structures.

[0012] In a further preferred embodiment, the hollow holes are shaped like the number 8, and a plurality of figure-eight hollow holes are evenly arranged in the first direction (width) of the mobile phone frame joining interface, and evenly arranged in the opposite direction to the adjacent hollow holes in the second direction (length) of the mobile phone frame joining interface, and the hollow holes are arranged in a ring around the support body in the joining interface of the mobile phone frame.

[0013] In a further preferred technical solution, figure-eight shaped perforations are arranged in a ring around the support body in the bonding layer, forming a mesh-like bonding layer. The mesh-like bonding layer is formed by arc-shaped connecting parts centered on the support body. Any two adjacent support bodies are connected by arc-shaped connecting parts. The arc-shaped connecting parts gradually narrow from the support body to the middle of the two adjacent support bodies. Taking a single support body and the arc-shaped connecting parts around it as a unit, the periphery of the support body has four ring-shaped connecting parts arranged in a ring, and the whole is similar to the shape of a fan blade.

[0014] In a further preferred embodiment, the mobile phone frame is made of titanium and titanium alloy, the crystal structure is made of titanium and titanium alloy, and the intermediate plate is made of aluminum and aluminum alloy.

[0015] In a further preferred embodiment, the support body is cylindrical with a diameter of 1 mm, the distance between the bonding layer and the bonding interface of the mobile phone frame is 0.3 mm, and the thickness of the bonding layer is 0.2 mm.

[0016] The advantages and beneficial effects of this invention are as follows: Since the metal bonding material fills the space within the lattice structure, it is firmly bonded and integrated through an anchoring effect; the figure-eight shaped perforated bonding layer guides the intermediate plate to fill the lattice structure on the mobile phone frame bonding interface, causing the intermediate plate to be anchored to the bonding layer and the arc-shaped connection formed by the perforated holes in the bonding layer within the space around the support, thus improving the bonding strength due to the shear force between them. Attached Figure Description

[0017] Figure 1 This is a front view of the metal bonding material of the present invention; Figure 2 Metal bonding material of the present invention Figure 1 A sectional view; Figure 3 This is an axonometric view of the metal substrate and lattice structure of the present invention; Figure 4 This is an isometric view of the mobile phone frame of the present invention; Figure 5 This is an axonometric view of a lattice structure according to another embodiment of the present invention; Figure 6 This is a top view of a lattice structure according to another embodiment of the present invention; In the figure: 10, metal substrate; 20, metal bonding material; 30, crystal structure; 31, bonding layer; 32, support; 33, hollow hole; 34, arc-shaped connection; 40, mobile phone frame; 50, middle plate. Detailed Implementation

[0018] The specific embodiments of the present invention will be further described below with reference to the accompanying drawings and examples. The following examples are only used to more clearly illustrate the technical solutions of the present invention and should not be construed as limiting the scope of protection of the present invention.

[0019] like Figure 1-3 As shown, a metal composite material includes a metal substrate 10, the metal substrate 10 having at least one bonding interface, a lattice structure 30 formed on the bonding interface, the lattice structure 30 including at least a plurality of supports 32 protruding along the bonding interface of the metal substrate 10, a bonding layer 31 formed on the plurality of supports 32, and a plurality of perforated holes 33 provided on the bonding layer 31.

[0020] The metal substrate 10 is made of metal and formed into a predetermined shape. The metal substrate 10 can be a plate shape, a strip shape, a strip shape, a U shape, or a frame shape. The material of the metal substrate 10 is not particularly limited, such as steel, titanium, aluminum, magnesium, etc.

[0021] Furthermore, the forming method of the metal substrate 10 is not particularly limited, and can be any of the following methods: rolling, extrusion, casting, forging, or machining. Additionally, in the example shown in Figure 1, for simplicity, an example of a quadrilateral shape for the metal substrate 10 structure is depicted, but the shape of the metal substrate 10 structure can be arbitrary, and the shape of the metal substrate 10 structure is determined according to the final shape.

[0022] A lattice structure 30 is formed on the metal substrate 10. The lattice structure 30 is made of metal, and the material is not particularly limited; it can be steel, titanium, aluminum, magnesium, etc. The metal substrate 10 and the lattice structure 30 can be made of different materials, but materials with similar coefficients of thermal expansion are preferred. The lattice structure 30 is formed by a 3D printer or similar means. That is, the lattice structures 30 are stacked and bonded to the bonding interface of the metal substrate 10. Furthermore, the bonding interface does not necessarily have to be planar.

[0023] As a 3D printer, known methods can be applied, such as powder bed deposition, directed energy deposition, and thermomelting. Powder bed deposition involves spreading metal powder and then irradiating only the desired areas with a laser to melt and solidify it. Directed energy deposition involves spraying molten metal for deposition and solidification. Thermomelting involves using thermoplastic resin as a binder to deposit metal powder and then removing the binder to form the final shape. The method of forming the lattice structure 30 is not limited to these methods, but by using a 3D printer, the bonding strength can be designed by setting the desired morphology (porosity, area ratio, described later). In this embodiment, the lattice structure 30 includes a plurality of supports 32 protruding perpendicular to the bonding interface, and a bonding layer 31 is formed on each of the supports 32. The bonding layer 31 has a plurality of perforations 33. Furthermore, in the following description, the portion surrounding the bonding interface between the bonding layer and the metal substrate 10 is referred to as the spatial portion. Furthermore, the shape of the lattice structure 30 is not limited to the shape shown in the figure; it can also be a square lattice, a triangular lattice, or a honeycomb shape, etc. In addition, the lattice structure 30 has at least a support, a bonding layer, and a space between the bonding layer and the metal substrate 10, and the bonding layer has a perforation 33 to communicate with the outside, so its shape is not limited.

[0024] The lattice structure 30 includes a plurality of supports 32 perpendicular to the interface of the metal substrate 10, and the plurality of supports 32 are arranged at equal intervals along the length and width directions of the interface of the metal substrate 10.

[0025] The shape of the support 32 is not limited to a cylinder. The support 32 can be designed according to the joint strength. When the joint interface is a continuous plane or a continuous curved surface, the support 32 is preferably a cylinder.

[0026] The diameter of the cylinder can be designed according to the joint strength. The diameter of the cylinder satisfies the support of the joint interface, and at the same time, realizes the anchoring strength between the joint interface and the metal substrate 10.

[0027] The diameter of the cylinder is between 0.8mm and 1.2mm, and can be 0.8mm, 0.85mm, 0.9mm, 0.95mm, 1.0mm, 1.05mm, or 1.1mm.

[0028] A plurality of the supports 32 are provided with a bonding layer 31. The distance between the bonding layer 31 and the bonding interface of the metal substrate 10 is 0.25-0.35 mm. The distance between the bonding layer 31 and the bonding interface of the metal substrate 10 can be equal. The distance between the bonding layer 31 and the bonding interface is 0.25 mm, 0.26 mm, 0.27 mm, 0.28 mm, 0.29 mm, 0.30 mm, 0.31 mm, 0.32 mm, 0.33 mm, 0.34 mm, and 0.35 mm.

[0029] The bonding layer 31 and the bonding interface may have unequal spacing. In this case, the bonding interface of the metal substrate 10 is formed with an uneven surface, or the bonding layer 31 is formed with an uneven surface, or both the bonding interface of the metal substrate 10 and the bonding layer 31 are formed with uneven surfaces, so that the bonding layer 31 and the bonding interface have unequal spacing.

[0030] The thickness of the bonding layer 31 is between 0.18 mm and 0.22 mm, and can be 0.18 mm, 0.185 mm, 0.19 mm, 0.195 mm, 0.2 mm, 0.205 mm, 0.21 mm, 0.215 mm, or 0.22 mm. The thickness of the bonding layer and the spacing between the bonding layers are controlled between 0.48 mm and 0.52 mm.

[0031] The bonding layer 31 is provided with a plurality of perforated holes 33 to connect the space to the outside. The perforated holes 33 are arranged in a regular pattern on the bonding layer. Generally, the perforated holes 33 are located around the joint between the support body 32 and the bonding layer 31 to avoid the support body 32 and prevent the perforated holes 33 from affecting the strength of the support body 32. The plurality of perforated holes 33 can be evenly arranged in the first direction of the bonding interface of the metal substrate 10, and evenly arranged in the opposite direction to the adjacent perforated holes 32 in the second direction of the bonding interface of the metal substrate 10. The first direction and the second direction of the bonding interface of the metal substrate 10 are perpendicular.

[0032] Furthermore, the perforated holes 33 may be unevenly arranged at the joint interface of the metal substrate 10, or they may be arranged in a ring around the support 32 at the joint interface of the metal substrate 10.

[0033] The shape of the perforated hole 32 can be a regular shape, such as a circle, an ellipse, or a figure-eight shape. In some embodiments, a figure-eight shaped perforated hole 32, compared to a circular perforated hole 32, helps the metal bonding material 20 to enter the space within the lattice structure 30, allowing the metal bonding material 20 to fill the space within the lattice structure 30 and forming a firm anchoring effect around the support 32 within the space. In addition, the shape of the perforated hole 33 can be an irregular shape.

[0034] A metal bonding material 20 is bonded to the metal substrate 10. The metal bonding material 20 also has at least one bonding interface. The bonding interface of the metal bonding material 20 fills the spaces between the crystal structures. The metal substrate 10 and the metal bonding material 20 are bonded through the crystal structure 30.

[0035] The metal bonding material 20 fills the space within the lattice structure 30 and is integrated with the lattice structure 30. That is, the entire space is connected to the outside of the lattice structure 30 and is not an independent space. The metal bonding material 20 is made of metal, and is a non-ferrous metal different from the metal substrate 10, such as aluminum, copper, or magnesium. As described above, the lattice structure 30 is bonded to the metal substrate 10 via a bonding interface. Furthermore, the metal bonding material 20 fills the spaces within the lattice structure 30, thus achieving integration. Therefore, the metal substrate 10 and the metal bonding material 20 are bonded through the lattice structure 30. Since the metal bonding material 20 fills the spaces within the lattice structure 30, they are firmly bonded and integrated through an anchoring effect. Moreover, since the metal bonding material 20 is metal, a more robust bond can be achieved by causing a metallurgical reaction between the metal substrate 10 and the metal bonding material 20 during the manufacturing process.

[0036] Next, the manufacturing method of the metal bonding material will be explained. First, as... Figure 2As shown, a lattice structure 30 is formed at the inner bonding interface of the metal substrate 10 using a 3D printer or similar means. The lattice structure 30 can be made of the same material as the metal substrate 10 or a different material. Before constructing the lattice structure 30, the inner surface of the metal substrate 10 (corresponding to the bonding interface surface) can be pre-treated. For example, an uneven or porous shape can be formed on the inner surface of the metal substrate 10, or an oxide coating removal process or a bonding agent (such as flux) can be applied. Alternatively, surface treatments such as electroplating, PVD, or CVD coating can be performed. For example, by forming a metal layer on the surface of the lattice structure 30 that reacts metallurgically with or promotes a metallurgical reaction with the metal bonding material 20, or by attaching fine metal powder to the surface of the lattice structure 30, the bonding strength can be further improved.

[0037] Furthermore, in this embodiment, the lattice structure 30 includes a plurality of supports 32 protruding in a direction perpendicular to the bonding interface. A bonding layer 31 is formed on the plurality of supports 32. The bonding layer 31 is provided with a plurality of perforated holes 33. The orientation of the supports 32 is composed of a direction perpendicular to the bonding interface and a direction orthogonal to it. The direction perpendicular to the plane of the paper is omitted. The same applies below.

[0038] Next, as Figure 3 As shown, a metal bonding material 20 is filled into the space within the lattice structure 30. Furthermore, when filling the space within the lattice structure 30 with the metal bonding material 20, this manufacturing method utilizes necessary molds, etc., but these are not shown in the diagram.

[0039] The method for filling the space within the lattice structure 30 with the metal bonding material 20 is not particularly limited; for example, common casting methods such as melt forging, high-pressure casting, die casting, and gravity casting can be used. However, to improve quality by fully filling every corner of the space with the metal bonding material 20, melt forging, high-pressure casting, and die casting are particularly preferred. Furthermore, to achieve a stronger bond through the metallurgical reaction between the lattice structure 30 and the metal bonding material 20, melt forging and high-pressure casting, which maintain the interface between the metal bonding material and the lattice structure 30 at high temperatures for extended periods and facilitate reaction, are preferred.

[0040] The formation of a reaction layer at the interface between the metal bonding material 20 and the lattice structure 30 is promoted by prolonged close contact between the molten metal bonding material 20 and the lattice structure 30 at high temperature. The reaction layer is an intermetallic compound formed at the interface between the metal bonding material 20 and the lattice structure 30. For example, if the lattice structure 30 is an iron-based material such as maraging steel and the metal bonding material 20 is an aluminum alloy, the reaction layer is formed by intermetallic compounds such as FeAl3 and Fe2Al3. If the lattice structure is a titanium alloy and the metal bonding material 20 is an aluminum alloy, the reaction layer is formed by intermetallic compounds such as Gamma TiAl, Alloferrin 2-TiAl, and TiAl3. Thus, it is preferable that a reaction layer is formed at the interface between the lattice structure 30 and the metal bonding material 20. Furthermore, the reaction layer (intermetallic compound) is not limited to these; the presence of a certain degree of intermetallic compound (reaction layer) can improve the bonding strength between dissimilar metals, as the types of metals used in the lattice structure 30 and the metal bonding material 20 can be composed of various intermetallic compounds.

[0041] As described above, the longer the molten metal bonding material 20 and the lattice structure 30 are in close contact at high temperature, the easier it is for the reaction layer to form and grow. Therefore, the formation state of the reaction layer can be controlled by casting conditions such as the melting temperature (solution temperature) of the metal bonding material 20, the contact time in the molten state (solidification time), and the preheating temperature of the lattice structure 30. For example, it is preferable to maintain an intermetallic compound formation holding time for forming an intermetallic compound at the interface between the lattice structure 30 and the metal bonding material 20 after the metal bonding material 20 is filled into the mold and before the mold is opened. By appropriately setting the intermetallic compound formation holding time, the intermetallic compound bonding with respect to the interface between the lattice structure 30 and the metal bonding material can be adjusted.

[0042] Furthermore, generally speaking, in metal casting, increasing the cooling rate can refine the grains, stabilize quality, and shorten cycle time, thus reducing manufacturing costs. For example, in aluminum die casting, multiple internal cooling mechanisms are incorporated into the mold, and the mold temperature is low at the start of casting. Therefore, the solidification time is very short, ranging from a few seconds to tens of seconds, and even for large products, it rarely exceeds one minute, making it difficult to form a reaction layer. Conversely, in gravity mold casting and low-pressure casting, the solidification time is extended by about 10 minutes, but the casting pressure is reduced to 0.1 MPa. This insufficient pressure to bring the molten metal into close contact with the crystal lattice structure makes it difficult to form a reaction layer.

[0043] On the other hand, molten metal forging or high-pressure casting methods involve a long contact time (solidification time) in the molten state and a casting pressure as high as about 100 MPa, which can pressurize the molten metal and maintain close contact with the crystal structure 30, thus easily forming a reaction layer, making them preferred casting methods. Thus, after filling the molten metal under high pressure (e.g., 50 MPa or more, more preferably 80 MPa or more), extending the holding time until mold opening (at least 1 minute, more preferably 2 minutes or more, more preferably 4 minutes or more) allows the desired intermetallic compound to be obtained.

[0044] Furthermore, the surface of the lattice structure 30 can be subjected to the surface treatment described above before the metal bonding material 20 is filled into the lattice structure 30. Additionally, after the lattice structure 30 is formed, a heat treatment to relieve stress in the lattice structure 30 or a tempering treatment can be performed. Through these methods, a metal bonding material can be obtained.

[0045] As described above, according to the embodiment, the metal substrate 10 and the metal bonding material 20 are joined by the lattice structure 30, thus enabling a strong bond between the two materials. For example, when the metal bonding material 20 is formed directly on the surface of the metal substrate 10 by casting or the like, it is sometimes impossible to sufficiently ensure the bond strength at the interface between the two materials. In this case, by integrating the lattice structure 30 and the metal bonding material 20 together, the two materials can be joined with high bond strength. That is, in this embodiment, it is effective when the bond strength between the metal substrate 10 and the lattice structure 30 is greater than the bond strength between the metal substrate 10 and the metal bonding material 20.

[0046] Furthermore, the bonding strength between the lattice structure 30 and the metal bonding material 20 can be adjusted by considering the shape of the structure (the shape and volume fraction of the support, bonding layer, and space portion 9b). At this time, by constructing the lattice structure 30 using a 3D printer, the lattice structure 30 can be designed in any shape. Therefore, by designing the desired shape of the lattice structure 30 based on the material of either the lattice structure 30 or the metal bonding material 20, sufficient bonding strength can be ensured.

[0047] Furthermore, the lattice structure 30 is disposed not only near the bonding interface of the metal substrate 10, but also inside the metal bonding material 20. Therefore, the lattice structure 20 can mitigate the effects of differences in mechanical properties such as rigidity and hardness, and differences in thermal expansion coefficients between the metal substrate 10 and the metal bonding material 20. For example, by appropriately designing the shape and structure of the lattice structure 30 and the filling depth of the metal bonding material 20, damage at the bonding interface can be suppressed and prevented, and the mechanical and thermal properties of the dissimilar metal bonding can be freely designed and controlled.

[0048] Furthermore, by forming a reaction layer at the interface between the lattice structure 30 and the metal bonding material 20, a higher bonding strength can be obtained. Next, as... Figure 4 As shown, the manufacturing and application of metal bonding materials in conjunction with a titanium-aluminum mobile phone frame are further explained. The mobile phone frame includes a mobile phone bezel 40, which includes at least a first bezel, a second bezel, a third bezel, and a fourth bezel. The first bezel and the third bezel are symmetrically arranged, as are the second bezel and the fourth bezel. The mobile phone bezel 40 may have two component assemblies, consisting of a U-shaped component and a long strip component, or it may consist of four components, consisting of two U-shaped components and two long strip components, as shown below. Figure 3 As shown, the mobile phone frame 40 can of course be composed of other components, but no matter how the mobile phone frame 40 is composed, it includes at least a first frame, a second frame, a third frame and a fourth frame. The mobile phone frame 40 is composed of the metal substrate, which is titanium or titanium alloy material.

[0049] A bonding interface is formed on the inner side of the mobile phone frame 40. A lattice structure 30 is formed on the bonding interface. The lattice structure 30 includes at least a plurality of supports 32 protruding along the bonding interface on the inner side of the mobile phone frame 40. A bonding layer 31 is formed on the plurality of supports 32. A plurality of hollow holes 33 are provided on the bonding layer 31.

[0050] The lattice structure 30 includes a plurality of supports 32 perpendicular to the inner bonding interface of the mobile phone frame 40, and the plurality of supports 32 are arranged at equal intervals along the length and width directions of the inner bonding interface of the mobile phone frame 40.

[0051] The support 32 is cylindrical in shape, and the diameter of the cylinder is 1 mm.

[0052] A plurality of the support bodies 32 are provided with a bonding layer 31. The distance between the bonding layer 31 and the bonding interface on the inner side of the mobile phone frame 40 is 0.3 mm, and the distance between the bonding layer 31 and the bonding interface on the inner side of the mobile phone frame 40 is equal. The distance between the bonding layer and the bonding interface on the inner side of the mobile phone frame 40 can be controlled by the height of the support body 32. The support body 32 is formed on the bonding interface on the inner side of the mobile phone frame 40 with a height of 0.3 mm, and the bonding layer 31 is formed on the top of the support body 32, so that the distance between the bonding layer 31 and the bonding interface on the inner side of the mobile phone frame 40 can be 0.3 mm.

[0053] The thickness of the bonding layer 31 is 0.2mm. The bonding layer 31 is provided with a plurality of hollow holes 33 to connect the space to the outside. The plurality of hollow holes 33 can be evenly arranged in a first direction on the inner bonding interface of the mobile phone frame 40, and evenly arranged in the opposite direction to the adjacent hollow holes 33 in a second direction on the inner bonding interface of the mobile phone frame 40. The first direction and the second direction of the inner bonding interface of the mobile phone frame 40 are perpendicular, and the hollow holes 33 are arranged in a ring around the support 32 on the inner bonding interface of the mobile phone frame 40.

[0054] The hollow holes 32 are in the shape of an 8. Several figure-eight shaped hollow holes 32 are evenly arranged in the first direction (width) of the inner bonding interface of the mobile phone frame 40. In the second direction (length) of the inner bonding interface of the mobile phone frame 40, they are evenly arranged in the opposite direction to the adjacent hollow holes 32. The hollow holes 32 are arranged in a ring around the support body 32 on the inner bonding interface of the mobile phone frame 40. Compared with circular hollow holes 32, this helps the metal bonding material 20 to enter the space within the lattice structure 30, so that the metal bonding material 20 fills the space within the lattice structure 20, and forms a firm anchoring effect around the support body 32 in the space.

[0055] The mobile phone frame also includes a middle plate 50, which is disposed within the mobile phone frame 40. The middle plate 50 is formed by the metal bonding material 20. The middle plate 50 has a bonding interface corresponding to the first frame, second frame, third frame and fourth frame of the mobile phone frame 40. The bonding interface of the middle plate 50 is filled between the lattice structure 30. The mobile phone frame 40 and the middle plate 50 are joined by the lattice structure 30 to form the mobile phone frame.

[0056] The intermediate plate 50 fills the space within the lattice structure 30 and is integrated with the lattice structure 30. That is, the entire space is connected to the outside of the lattice structure 30 and is not an independent space. The intermediate plate 50 is made of metal, and it is a non-ferrous metal different from the mobile phone frame 40; the intermediate plate 50 is made of aluminum.

[0057] The figure-eight shaped perforations 33 are arranged in a ring around the support 32 in the bonding layer 31, thus forming a mesh-like bonding layer 31. The mesh-like bonding layer 31 is formed by arc-shaped connecting portions 34 centered on the support 32. Any two adjacent support bodies 32 are connected by the arc-shaped connecting portions 34. The arc-shaped connecting portions 34 gradually narrow from the support body 32 to the middle of the two adjacent support bodies 32. Taking a single support body 32 and the surrounding arc-shaped connecting portions 34 as units, the periphery of the support body 32 has a ring arrangement. The four annular connecting parts 34 are generally fan-shaped. The middle plate 50 is filled by the hollow holes 32 into the middle part between the bonding interface layer and the bonding layer 31 on the inner side of the mobile phone frame 40. The middle plate 50 forms an intermetallic compound in the middle part around the support part 32. The bonding strength between the middle plate 50 and the mobile phone frame 40 is mainly obtained by the tensile strength of the lattice structure 30 and the middle plate 50 themselves, as well as the anchoring effect brought about by the integration of the middle plate 50 and the lattice structure 30.

[0058] Therefore, the figure-eight shaped perforated hole 33 of the bonding layer can guide the intermediate plate 50 to fill into the lattice structure 30 on the bonding interface of the mobile phone frame 40, so that the intermediate plate 50 in the space around the support 32 is anchored to the bonding layer 31 and the arc-shaped connection portion 34 formed by the perforated hole 33 in the bonding layer 31, and the shear force between them can be applied to improve the bonding strength.

[0059] Therefore, the design of the anchoring effect of the lattice structure 30 is crucial in the bonding strength between the phone frame 40 and the middle plate 50. Taking a single support 32 and its surrounding arc-shaped connecting parts 34 as units, the support 32 has four annular connecting parts 34 arranged in a ring around its perimeter. The lattice structure 30, composed of the bonding layer 3 and the support 32, which is shaped like a fan blade, can achieve a more efficient anchoring effect. Therefore, the bonding strength between the phone frame 40 and the middle plate 50 can be improved.

[0060] In addition, by forming figure-eight shaped perforations 32 in the bonding layer 31 of the lattice structure 30 and adjusting the spacing between the bonding interface of the mobile phone frame 40 and the bonding layer 31, the anchoring effect can be achieved more efficiently.

[0061] An initial 3D model is obtained by performing 3D modeling on the mobile phone frame 40 to be printed. The mobile phone frame 40 to be printed is a large thin-walled titanium alloy part. The initial 3D model is then modified by adding allowance, adding infill structure, shaping and placement, model repair, adding support structure and adding lattice structure 30 to obtain a test 3D model. Based on the test 3D model, the lattice structure 30 is generated by 3D printing. The lattice structure 30 includes a plurality of support bodies 32 perpendicular to the joint interface of the mobile phone frame 40. The plurality of support bodies 32 are arranged at equal intervals along the length and width directions of the joint interface of the mobile phone frame 40. The support 32 is cylindrical in shape, and the diameter of the cylinder is 1 mm; A plurality of the supports 32 are provided with a bonding layer 31. The distance between the bonding layer 31 and the bonding interface of the mobile phone frame 40 is 0.3 mm. The thickness of the bonding layer 31 is 0.2 mm. The bonding layer 31 is provided with a plurality of hollow holes 33 to connect the space to the outside. The plurality of hollow holes 33 can be evenly arranged in a first direction of the bonding interface of the mobile phone frame 40, and evenly arranged in the opposite direction to the adjacent hollow holes 33 in a second direction of the bonding interface of the mobile phone frame 40. The first direction and the second direction of the bonding interface of the mobile phone frame 40 are perpendicular, and the hollow holes 33 are arranged in a ring around the support 32 in the bonding interface of the mobile phone frame 40.

[0062] An intermediate plate 50, which is molten aluminum, is filled into the space within the lattice structure 30 of the phone frame 40. Furthermore, when filling the space within the lattice structure 30 with the intermediate plate 50, this manufacturing method utilizes necessary molds (not shown), pressurizes the molten aluminum to maintain continuous contact with the lattice structure 30, generating a reaction layer. By bonding the phone frame 40 and the intermediate plate 50 through the lattice structure 30, the two materials are firmly bonded to form the phone's mid-frame.

[0063] Furthermore, in some embodiments, the lattice structure 30 is designed as a mesh structure, such as... Figure 5 and Figure 6 As shown, the lattice structure 30 includes a support body, which is composed of several support units. Each support unit includes four inclined prisms. The bottoms of the four adjacent prisms are formed on the substrate 10, and the ends of the four prisms are joined together to form a square pyramid shape. The lattice structure 30 is composed of several support units forming a grid-like structure, and the four prisms in the support unit are respectively joined to one of the adjacent prisms in the four surrounding support units on the substrate 10.

[0064] The prism is a cylinder or a polygonal prism.

[0065] The diameter of the cylinder is between 0.8mm and 1.2mm, and can be 0.8mm, 0.85mm, 0.9mm, 0.95mm, 1.0mm, 1.05mm, or 1.1mm.

[0066] By filling the space within the lattice structure 30 with the metal bonding material 20 in a grid-like lattice, a strong anchoring effect is formed in the space.

[0067] The above description is only a preferred embodiment of the present invention. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the technical principles of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.

Claims

1. A metal composite material, characterized in that, The invention includes a metal substrate having at least one bonding interface, a lattice structure formed on the bonding interface, the lattice including at least a plurality of supports protruding along the bonding interface of the metal substrate, a bonding layer formed on the plurality of supports, and a plurality of perforations provided on the bonding layer. A metal bonding material is bonded to the metal substrate, and the metal bonding material also has at least one bonding interface. The bonding interface of the metal bonding material fills the space between the crystal structures, and the metal substrate and the metal bonding material are bonded through the crystal structures.

2. The metal composite material according to claim 1, characterized in that, The lattice structure includes several supports protruding vertically along the bonding interface. The supports are cylindrical in shape, with a diameter of 0.8 mm to 1.2 mm.

3. The metal composite material according to claim 1, characterized in that, A bonding layer is provided on several of the supports, and the distance between the bonding layer and the bonding interface of the metal substrate is 0.25-0.35 mm.

4. A method for manufacturing a metal composite material, characterized in that, The method includes at least the following steps: forming a metal lattice structure on a metal substrate by 3D printing; the lattice structure includes at least a plurality of supports protruding along the bonding interface of the metal substrate; a bonding layer is formed on the plurality of supports; and a plurality of hollow holes are provided on the bonding layer. Metal bonding material is filled into the space within the lattice structure by high-pressure casting; the metal substrate and the metal bonding material are bonded through the lattice structure.

5. The method for manufacturing a metal composite material according to claim 4, characterized in that, Before filling the lattice structure with metal bonding material, the surface of the lattice structure is surface treated; after the lattice structure is formed, heat treatment can be performed to relieve stress or temper the lattice structure.

6. A mobile phone frame, the mobile phone frame including a mobile phone border, the mobile phone border including at least a first border, a second border, a third border and a fourth border, the first border and the third border being symmetrically arranged, the second border and the fourth border being symmetrically arranged, the mobile phone border being composed of the metal substrate, the mobile phone frame further including a middle plate, the middle plate being disposed within the mobile phone border, the middle plate being formed by the metal bonding material, characterized in that, A bonding interface is formed on the inner side of the mobile phone frame. A lattice structure is formed on the bonding interface. The lattice structure includes at least a plurality of supports protruding along the bonding interface of the mobile phone frame. A bonding layer is formed on the plurality of supports. The bonding layer has a plurality of hollow holes. The middle plate is filled between the lattice structures. The mobile phone frame and the middle plate are bonded through the lattice structures.

7. A mobile phone mid-frame according to claim 6, characterized in that, The hollow holes are shaped like the number 8. Several figure-eight hollow holes are evenly arranged in the first direction (width) of the mobile phone frame joint interface, and evenly arranged in the opposite direction to the adjacent hollow holes in the second direction (length) of the mobile phone frame joint interface. The hollow holes are arranged in a ring around the support body in the joint interface of the mobile phone frame.

8. A mobile phone mid-frame according to claim 7, characterized in that, The figure-eight shaped perforations are arranged in a ring around the support body in the bonding layer, forming a mesh-like bonding layer. The mesh-like bonding layer is formed by arc-shaped connecting parts centered on the support body. Any two adjacent support bodies are connected by arc-shaped connecting parts. The arc-shaped connecting parts gradually narrow from the support body to the middle of the two adjacent support bodies. Taking a single support body and the arc-shaped connecting parts around it as a unit, the support body has four ring-shaped connecting parts arranged in a ring around its perimeter, and the whole is similar to the shape of a fan blade.

9. A mobile phone mid-frame according to any one of claims 6-8, characterized in that, The phone frame is made of titanium or titanium alloy, the lattice structure is made of titanium or titanium alloy, and the middle plate is made of aluminum or aluminum alloy.

10. A mobile phone frame according to any one of claims 6-8, characterized in that, The support body is cylindrical in shape with a diameter of 1 mm. The distance between the bonding layer and the bonding interface of the mobile phone frame is 0.3 mm, and the thickness of the bonding layer is 0.2 mm.