Preparation device and preparation process of large-size high-thermal-conductivity aluminum-based composite material

By employing a dual negative pressure design and radial constraint force, the problems of uneven shrinkage and pressure in the preparation of large-size aluminum-based composite materials were solved, achieving high-quality billet forming and cost-effective preparation.

CN123149409APending Publication Date: 2026-11-24HENAN HANYIN OPTOELECTRONICS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611379403.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-07
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing technologies struggle to effectively suppress uneven shrinkage of the cladding and ensure uniform pressure transmission when preparing large-size aluminum-based composite materials, leading to a decrease in billet forming quality and cylindricity, as well as high equipment costs.

Method used

The design employs a dual negative pressure system. By setting independent negative pressure channels inside the casing and in the cylindrical cavity, the negative pressure value in the cylindrical cavity is controlled to be greater than that inside the casing, thus creating a pressure difference and applying pre-pressure. Combined with radial constraint force, this ensures uniform pressure transmission during the vacuuming and hot-pressing stages.

Benefits of technology

It significantly improves the molding quality of large-size aluminum-based composite materials, increases cylindricity, reduces equipment investment and production costs, and improves process efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149409A_ABST
    Figure CN123149409A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of powder metallurgy technology, specifically relating to an apparatus and its preparation process for large-size high thermal conductivity aluminum-based composite materials. The preparation process includes: loading mixed powder into a sleeve and placing it in a cylindrical cavity of a mold, with a pressure plate guiding and fitting at the top of the cylindrical cavity; placing the entire mold in a heating furnace for heating; evacuating the inside of the sleeve and simultaneously evacuating the space below the pressure plate in the cylindrical cavity, with the negative pressure value inside the cylindrical cavity greater than that inside the sleeve, creating a pressure difference between the upper and lower parts of the pressure plate and applying pre-pressure to the sleeve, while the sidewalls of the cylindrical cavity simultaneously apply radial constraint force to the sleeve; after heating and heat preservation, applying pressure to the pressure plate using a press to densify and shape the powder. This invention achieves the synergistic effect of axial pre-pressure and radial constraint during the vacuuming stage through differentiated negative pressure design, effectively suppressing uneven shrinkage of the sleeve, significantly improving the forming quality of large-size billets, and eliminating the need for expensive vacuum equipment, making it suitable for the industrial production of large-size billets.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of aluminum-based composite material preparation technology, and in particular to a preparation apparatus and process for large-size high thermal conductivity aluminum-based composite materials. Background Technology

[0002] Particle-reinforced aluminum matrix composites have broad application prospects in high-end fields such as aerospace, electronic packaging, and nuclear power due to their high specific strength, high specific stiffness, low coefficient of thermal expansion, and good thermal conductivity. With the increasing demands for lightweighting and integration in major engineering equipment in these fields, the need for large-size aluminum matrix composite ingots is becoming increasingly urgent.

[0003] Powder metallurgy is considered an ideal method for preparing aluminum-based composite materials with low, medium and high particle content due to its advantages such as a wide range of matrix alloy selection, a large adjustable range and uniform distribution of reinforcing body content, and relatively low manufacturing temperature.

[0004] The mainstream process routes for preparing large-size aluminum-based composite ingots using powder metallurgy mainly include vacuum hot pressing and hot isostatic pressing. However, existing technologies have many shortcomings. On the one hand, traditional vacuum hot pressing or hot isostatic pressing processes rely on expensive specialized equipment such as vacuum hot pressing furnaces or hot isostatic pressing furnaces, resulting in large equipment investments, high production costs, and limitations in the size of the equipment cavity, making it difficult to prepare extra-large ingots with diameters greater than 400 mm. On the other hand, even when using ordinary air-fired electric furnaces with external vacuum to reduce reliance on expensive equipment, the problem of uneven shrinkage of the cladding under vacuum negative pressure still exists, leading to a decrease in the cylindricity of the ingot.

[0005] To address the aforementioned issues, existing patents have explored ways to improve the situation.

[0006] Patent CN112410598B (Powder Metallurgical Preparation Method of Large-Size Ingots of Particle-Reinforced Aluminum Matrix Composites) proposes a method of loading mixed powder into a metal sheath and placing it in a steel mold. The mixture is then heated in a conventional resistance furnace, with degassing performed using an external vacuum pump. The mold is then moved to a press for hot pressing. While this method can prepare large-size ingots with diameters ranging from Φ400mm to Φ2000mm, eliminating reliance on a vacuum hot press furnace, it still has the following shortcomings in practical applications: During the vacuum stage, the powder inside the sheath causes uneven shrinkage of the sheath wall under negative pressure, reducing the cylindricity of the ingot; during the hot pressing stage, ingots with insufficient cylindricity experience uneven stress under unidirectional pressure, easily leading to localized density differences and deformation, affecting the forming quality and subsequent processing performance of the ingot.

[0007] Patent CN115383115A (A powder metallurgy process for a non-continuously reinforced aluminum matrix composite billet) proposes to transfer the heated and heat-insulated cladding to a low-temperature metal mold on a press platform for pressure bonding in order to solve the problem of lateral deformation of the mold in the hot pressing process. However, the problem of uneven shrinkage of the cladding during the vacuuming stage has not been effectively solved, and the fitting accuracy between the cladding and the mold is difficult to guarantee during the transfer process, which increases the complexity of operation and the uncertainty of quality.

[0008] Therefore, how to effectively suppress uneven shrinkage of the cladding during the vacuuming stage, ensure uniform pressure transmission during the hot pressing stage to improve the billet forming quality, and at the same time take into account equipment cost and process efficiency, remains a technical challenge in this field. Summary of the Invention

[0009] The purpose of this invention is to solve the above-mentioned problems by providing a preparation device and process for large-size high thermal conductivity aluminum-based composite materials.

[0010] To achieve the above objectives, the technical solution of the present invention is as follows: a preparation process for large-size high thermal conductivity aluminum-based composite materials, comprising the following steps: Step 1: Pack the uniformly mixed aluminum matrix powder and reinforcing phase particles into a sleeve, place the sleeve in the cylindrical cavity of the mold, and guide the pressure plate to fit the top of the cylindrical cavity; Step 2: Place the entire mold in a heating furnace for heating; Step 3: Vacuum the inside of the casing and simultaneously vacuum the space below the pressure plate of the columnar cavity. The negative pressure value inside the columnar cavity is greater than the negative pressure value inside the casing, so that a pressure difference is formed on the upper and lower sides of the pressure plate and a pre-pressure is applied to the casing. The inner wall of the columnar cavity applies a radial constraint force to the outer circumference of the casing. Step 4: After heating and heat preservation, place the mold, sleeve and pressure plate as a whole in the press. Apply pressure to the pressure plate through the press and transfer the pressure to the sleeve to densify and form the mixed powder.

[0011] On the other hand, this application also provides an apparatus for preparing large-size high thermal conductivity aluminum-based composite materials, comprising: The mold has a cylindrical cavity with an open top for placing the package, an insertion groove at the bottom of the cylindrical cavity, and a suction port on the side wall; The pressure plate and guide plate are fitted to the top of the columnar cavity and can slide up and down along the axial direction of the columnar cavity; The outer wall of the mold is provided with a first interface and a second interface, which are respectively connected to the insertion slot and the suction port. The insertion slot is used to insert and cooperate with the suction pipe that is built into the cylindrical cavity. During operation, the negative pressure value of the first interface is less than that of the second interface, so that a pressure difference is formed simultaneously on the upper and lower sides of the pressure plate and the inner and outer sides of the casing.

[0012] The present invention discloses a preparation apparatus and process for large-size high thermal conductivity aluminum-based composite materials, which have the following advantages compared with the prior art: First, the present invention sets up two independent negative pressure channels for vacuuming the inside of the casing and the cylindrical cavity, and controls the negative pressure value in the cylindrical cavity to be greater than that in the casing, so that a pressure difference is formed on the upper and lower sides of the pressure plate. During the vacuuming stage, axial pre-pressure is applied to the casing to initially compact the mixed powder inside the casing, thereby improving the initial density of the billet.

[0013] Secondly, the inner wall of the cylindrical cavity applies a radial constraint force to the outer circumferential surface of the casing, which effectively suppresses the uneven shrinkage of the casing under negative pressure, ensuring the cylindricity of the billet during the vacuuming stage, and laying the foundation for uniform pressure transmission in the subsequent hot pressing stage.

[0014] Third, after the heating and heat preservation are completed, the mold, sleeve and pressure plate are placed in the press for hot pressing. The columnar cavity continuously provides radial constraint during the hot pressing stage, so that the unidirectional pressure applied by the press can be evenly transmitted, avoiding local stress concentration and density difference caused by uneven billet shape, and significantly improving the forming quality of large-size billets. Attached Figure Description

[0015] Figure 1 This is a schematic diagram of the overall structure of the apparatus for preparing large-size high thermal conductivity aluminum-based composite materials according to the present invention. Figure 1 .

[0016] Figure 2 This is a schematic diagram of the overall structure of the apparatus for preparing large-size high thermal conductivity aluminum-based composite materials according to the present invention. Figure 2 .

[0017] Figure 3 This is a side view of the apparatus for preparing a large-size, high thermal conductivity aluminum-based composite material according to the present invention.

[0018] Figure 4 This is a bottom view schematic diagram of the apparatus for preparing a large-size, high thermal conductivity aluminum-based composite material according to the present invention.

[0019] Figure 5 This is a top view schematic diagram of the preparation device for a large-size, high thermal conductivity aluminum-based composite material according to the present invention.

[0020] Figure 6 This is a schematic diagram of the mold structure in the preparation device of a large-size high thermal conductivity aluminum-based composite material according to the present invention.

[0021] Figure 7for Figure 6 The diagram shows a cross-sectional view of the present invention at point AA.

[0022] Figure 8 for Figure 6 The diagram shows a cross-sectional view of the present invention at point BB.

[0023] Figure 9 for Figure 7 The diagram shows a partially enlarged structural schematic of the present invention at point C.

[0024] Figure 10 for Figure 8 The diagram shows a partially enlarged structural schematic of the present invention at point D.

[0025] Figure 11 for Figure 7 The diagram shows a cross-sectional view of the mold and heating furnace of the present invention at point EE.

[0026] Figure 12 This is a bottom view of the mold structure in this invention.

[0027] Figure 13 This is a schematic diagram of the pressure plate in the present invention.

[0028] Figure 14 This is a schematic diagram of the internal structure of the mold in this invention.

[0029] Figure 15 This is a schematic diagram of the connection structure of the heating furnace, lifting frame and docking assembly in this invention.

[0030] Figure 16 This is a schematic flowchart illustrating the preparation process of a large-size, high thermal conductivity aluminum-based composite material according to the present invention.

[0031] In the diagram: 1. Mold; 1a. Cylinder; 1a-1. Guide rib; 10. Interface 1; 100. Insertion groove; 101. Conical self-sealing component; 11. Interface 2; 110. Air passage; 12. Thermal insulation seal; 13. Top connection; 15. Pressure plate; 150. Rigid component; 2. Heating furnace; 2a. Balance port; 20. Frame; 21. Linear power drive component; 3. Press; 30. Lifting component; 31. Pressing component; 4. Docking assembly; 40. Guide rail; 41. Support component; 42. Insertion pipe; 5. Conveying unit; 50. Drive device; 51. Drive belt; 9. Sheath; 90. Air extraction pipe. Detailed Implementation

[0032] The present invention will now be described in further detail with reference to the accompanying drawings. The drawings are simplified schematic diagrams, illustrating only the basic structure of the invention, and therefore only show the components relevant to the invention.

[0033] Example 1 refer to Figures 1 to 15 This invention application provides a preparation apparatus for large-size, high thermal conductivity aluminum-based composite materials. It is mainly applicable to the powder metallurgy preparation of large-size ingots of particle-reinforced aluminum-based composite materials, particularly suitable for vacuum hot pressing sintering of large-size ingots with silicon carbide, boron carbide, or other ceramic particles as reinforcing phases and pure aluminum or aluminum alloy powder as the matrix. The prepared ingots can reach diameters of 400mm to 2000mm and have a density of over 99.5%. They can be directly used for subsequent forging, extrusion, rolling, and other deformation processing, or directly cut into target parts, applicable to aerospace, aviation, electronics, nuclear power, and other fields.

[0034] In this invention, the aluminum matrix powder can be pure aluminum powder or various aluminum alloy powders, such as 6061 aluminum alloy, 2029 aluminum alloy, 2009 aluminum alloy, 6092 aluminum alloy, etc. The reinforcing phase particles can be one or more of silicon carbide, boron carbide, alumina, silicon, tungsten carbide, and titanium diboride, with a particle volume content of 10%–75%. Powder mixing can be performed using ordinary mechanical mixing or high-energy ball milling, with a mixing time of 0.5–24 hours. The sheath 9 can be made of aluminum, aluminum alloy, iron, or steel, with a wall thickness generally of 3–10 mm and a cylindrical shape. The sheath 9 is sealed using argon arc welding or similar methods, and a suction pipe 90 is welded to it. The suction pipe 90 is made of the same material as the sheath 9, and its inner diameter is generally not less than 10 mm.

[0035] The mold 1 used in this invention includes a cylindrical body 1a, which is a thick-walled steel mold 1, and can be made of a material suitable for high-temperature environments up to 600℃. A columnar cavity is formed inside the cylindrical body 1a. The outer circumferential surface of the pressure plate 15 is guided and sealed to the inner wall of the columnar cavity; both are precision-machined and have a clearance fit. The wall thickness of the mold 1 and the thickness of the upper and lower pressure heads are generally not less than 40mm to ensure that the mold 1 has sufficient rigidity and resistance to deformation under high temperature and high pressure.

[0036] The bottom of the cylindrical cavity is provided with a insertion groove 100, which is used to insert and mate with the suction tube 90 built into the sleeve 9 inside the cylindrical cavity. The bottom of the insertion groove 100 is connected to the interface 10 through an air passage. (See reference...) Figure 9In specific implementation, the insertion groove 100 is coaxially arranged with the cylindrical cavity and has a conical surface at the bottom. The suction pipe 90 is coaxially arranged with the sleeve 9. When the sleeve 9 is set in the cylindrical cavity, the suction pipe 90 is inserted into the insertion groove 100, and a conical self-sealing element 101 is sleeved on the outside of the suction pipe 90. It can be made of steel or copper, and its outer circumference has a conical structure that matches the conical surface of the insertion groove 100. With this arrangement, when negative pressure is provided to the insertion groove 100 for suction, a pressure difference will be generated on both sides of the conical self-sealing element 101. Under the action of the pressure difference, the conical self-sealing element 101 can be pushed downward to form a seal, ensuring the sealing effect.

[0037] The inner wall of the cylindrical cavity is provided with a suction port, which is used to evacuate the space of the cylindrical cavity located below the pressure plate 15. The outer wall of the mold 1 is provided with a first interface 10 and a second interface 11 that communicate with the insertion groove 100 and the suction port, respectively.

[0038] As a preferred embodiment, refer to Figure 1 , Figure 6 Interface 10 and interface 21 are located on the side wall of the mold base away from the press 3, which facilitates docking with the docking assembly 4 located at the end of the conveying unit 5.

[0039] refer to Figures 1 to 3 , Figure 15 The docking component 4 includes a horizontally arranged guide rail 40 and a support member 41 that is guided on the guide rail 40. The support member 41 can be driven by a cylinder or other driving component. The support member 41 is provided with a plug tube 42 corresponding to the first docking interface 10 and the second docking interface 11. When the support member 41 moves horizontally, the plug tube 42 can be plugged and inserted with the first docking interface 10 and the second docking interface 11.

[0040] In practice, the connectors 42 corresponding to interface 10 and interface 2 can be connected to different vacuum pumping devices; or they can be connected to different branches of the same vacuum pumping device, and the negative pressure values ​​of the two branches can be controlled by adjusting the valves.

[0041] Furthermore, it is understandable that the sleeve 9 will undergo certain deformation under the negative pressure and pressure of the pressure plate 15 inside the cylindrical cavity. Therefore, the outer peripheral surface of the sleeve 9 may be tightly fitted to the inner sidewall of the cylindrical cavity, making it inconvenient for the sleeve 9 to separate from the mold 1.

[0042] As a more preferred option, refer to Figure 7 , Figure 8 , Figure 10 , Figure 11 , Figure 13The edge of the pressure plate 15 is provided with a plurality of rigid members 150 spaced apart around its own axis. The inner circumferential surfaces of the plurality of rigid members 150 are all on the same cylindrical surface, which is coaxial with the pressure plate 15, and the radial dimension of the cylindrical surface is smaller than the radial dimension of the inner circumferential surface of the cylindrical cavity.

[0043] The rigid component 150 is formed as follows: a rigid cylinder is fixedly installed around the axis at the lower end edge of the pressure plate 15. The rigid cylinder is coaxial with the pressure plate 15. Then, multiple cutting slits are made along the axial direction of the rigid cylinder to divide the rigid cylinder into multiple independent rigid components 150 in the circumferential direction. The inner circumferential surface of the rigid cylinder is adapted to the outer circumferential surface of the sleeve 9. When the pressure plate 15 is installed in the cylinder 1a, the rigid component 150 is inserted between the inner circumferential surface of the cylindrical cavity and the outer circumferential surface of the sleeve 9. The outer circumferential surface of the rigid component 150 is inserted and fitted with the inner circumferential surface of the cylinder 1a for guiding and fitting. The inner circumferential surfaces of multiple rigid components 150 together form a cylindrical constraint space. The radial dimension of this constraint space is smaller than the radial dimension of the cylindrical cavity, which is used to radially limit the outer circumferential surface of the sleeve 9. Since the inner circumferential surface of the rigid member 150 is in direct contact with the outer circumferential surface of the sleeve 9, the radial shrinkage tendency of the sleeve 9 under vacuum negative pressure is constrained by the inner circumferential surface of the rigid member 150, thereby effectively suppressing the uneven shrinkage of the sleeve 9. Furthermore, because the rigid members 150 are spaced apart, gaps exist between adjacent rigid members 150. These gaps allow gas in the columnar cavity to flow between the space below the pressure plate 15 and the space above the pressure plate 15, which is beneficial for the rapid entry of gas into the space below the pressure plate 15 during subsequent demolding by introducing positive air pressure into the columnar cavity. Simultaneously, the gaps between the rigid members 150 also facilitate the uniform extraction of gas from various areas of the columnar cavity during vacuuming, improving vacuuming efficiency.

[0044] More preferably, a plurality of guide ribs 1a-1 are evenly spaced around the axis on the inner circumferential surface of the cylindrical cavity. The guide ribs 1a-1 extend axially from the bottom of the cylindrical cavity to the middle or top region of the cylindrical cavity. The guide ribs 1a-1 are strip-shaped structures that protrude radially inward, and their width and height are determined according to the size of the mold 1 and the process requirements. A plurality of rigid members 150 of the pressure plate 15 are inserted between two adjacent guide ribs 1a-1, that is, each rigid member 150 is located in the region enclosed by two adjacent guide ribs 1a-1. The guide ribs 1a-1 are located outside the cylindrical surface enclosed by the inner circumferential surface of the rigid member 150, that is, there is a gap between the radial inner end of the guide rib 1a-1 and the inner circumferential surface of the rigid member 150. The guide ribs 1a-1 do not directly contact the outer circumferential surface of the sleeve 9, but rather cooperate with the rigid member 150. When the pressure plate 15 slides along the axial direction of the cylindrical cavity, the guide rib 1a-1 guides and limits the rigid component 150, preventing the pressure plate 15 from deflecting or tilting during the sliding process and ensuring that the pressure plate 15 always moves smoothly along the axial direction of the cylindrical cavity. At the same time, the guide rib 1a-1 also enhances the structural strength of the cylindrical cavity. During the hot pressing of large-sized billets, the cylindrical cavity needs to withstand large radial pressure and lateral force. The setting of the guide rib 1a-1 significantly improves the deformation resistance of the mold 1.

[0045] More preferably, the suction port is located on the side wall of the guide rib 1a-1 near the axis of the pressure plate 15.

[0046] As a protruding structure on the inner wall of the cylindrical cavity, the guide rib 1a-1's surface near the axis of the pressure plate 15 is less likely to be blocked by the pressure plate 15 or the sleeve 9 during the vacuuming process of the cylindrical cavity. If the suction port is directly set on the smooth inner circumferential surface of the cylindrical cavity, when the pressure plate 15 descends to a lower position, the edge of the pressure plate 15 or the outer circumferential surface of the rigid member 150 may cover the suction port, resulting in blockage of the suction port or a significant reduction in pumping efficiency. However, by setting the suction port on the side wall of the guide rib 1a-1, since the guide rib 1a-1 protrudes radially inward, even if the edge of the pressure plate 15 or the outer circumferential surface of the rigid member 150 is close to the inner circumferential surface of the cylindrical cavity, the side wall of the guide rib 1a-1 near the axis still leaves a gap with the pressure plate 15 or the rigid member 150, ensuring that the suction port remains unobstructed at all times. In addition, the suction ports on the side wall of the guide rib 1a-1 are evenly distributed along the circumference of the columnar cavity, which can achieve uniform air extraction in the internal space of the columnar cavity, avoid local pressure differences caused by uneven air extraction, and thus ensure that the air pressure difference on the upper and lower sides of the pressure plate 15 is evenly distributed, improving the uniformity of the pre-pressure.

[0047] The mold 1 includes a base and a cylindrical body 1a disposed on the top of the base, the base and the cylindrical body 1a together forming a cylindrical cavity. The base is provided with an insertion groove 100 that is fitted into the suction pipe 90 of the sleeve 9, and the side wall of the cylindrical body 1a is provided with a suction port.

[0048] In this invention, a common air resistance furnace can be used for the heating furnace 2, eliminating the need for expensive vacuum hot press furnaces or hot isostatic pressing furnaces. The heating furnace 2 can be a detachable cylindrical structure, fitted over the outside of the cylindrical body 1a from top to bottom. A heat-insulating seal 12 is provided between the lower end of the heating furnace 2 and the outer periphery of the cylindrical body 1a. This heat-insulating seal 12 is used to reduce heat loss from the inside of the heating furnace 2 and prevent outside air from entering the heating furnace 2 and affecting heating efficiency. A balancing port 2a is provided on the side wall of the heating furnace 2. This balancing port 2a is used to balance the air pressure inside and outside the heating furnace 2 when it is fitted over the cylindrical body 1a, facilitating the installation and removal of the heating furnace 2.

[0049] In practical operation, the base of mold 1 with sleeve 9 and cylinder 1a are first assembled. Then, the heating furnace 2 is fitted over the cylinder 1a from above, with a gap between the inner circumference of the heating furnace 2 and the outer circumference of the cylinder 1a. The lower end of the heating furnace 2 is sealed to the outer periphery of the cylinder 1a through a heat-insulating seal 12, reducing heat loss from the bottom of the furnace. The heating furnace 2 uses resistance heating, with resistance heating elements embedded in the furnace wall, which heat the cylinder 1a after being energized. Because the heating furnace 2 is a separable cylindrical structure, heating furnaces of different specifications can be replaced according to the size of mold 1, improving the versatility and flexibility of the equipment. At the same time, the heating furnace 2 is set separately from mold 1, which facilitates the rapid transfer of mold 1 to the press for hot pressing after heating, reducing heat loss and improving process efficiency.

[0050] refer to Figure 11 In specific implementation, the pressure plate 15 and the cylinder 1a are in clearance fit. The gap between the two allows a small amount of airflow to pass through. With this setting, when suction is carried out through the negative pressure port, the high-temperature airflow in the heating furnace 2 can also enter the columnar cavity through the tiny gap between the pressure plate 15 and the side wall of the columnar cavity. The high-temperature airflow can improve the heating uniformity of the inner sleeve 9. At this time, the balance port 2a can replenish the gas in the heating furnace 2.

[0051] As a preferred embodiment, refer to Figures 1 to 5 The preparation apparatus may further include a conveying unit 5, a press, and a vertical drive component. The conveying unit 5 includes a guide rail frame, on which the mold 1 is guided and mounted. The guide rail frame is equipped with a drive belt 51, which is driven by a drive device 50. The drive device 50 adopts a structure commonly used in the prior art, such as a servo motor. The bottom of the mold 1 is connected to the drive belt 51 by a connector, thereby achieving the effect of horizontally driving the mold 1.

[0052] The press is located at one end of the conveying unit 5 and includes a top pressing component and a bottom pressing component 31 respectively disposed on the upper and lower sides of the conveying unit 5. The top pressing component is fixedly disposed below the conveying unit 5, serving as the worktable of the press and used to support the base of the mold 1. (Refer to...) Figure 7The bottom of the mold 1 is provided with a top contact part 13 that cooperates with the top pressing part; the lower pressing part 31 is provided above the conveying unit 5 and can move in the vertical direction to apply pressure to the pressure plate 15.

[0053] The conveying unit 5 can horizontally convey the mold 1 from the heating position to between the top pressing member and the bottom pressing member 31. The other end of the conveying unit 5 is provided with a vertical drive member, which includes a frame 20 and a linear power drive member 21 provided at the end of the frame 20. The heating furnace 2 is provided at the lower end of the linear power drive member. The linear power drive member can be any type of cylinder or electric telescopic rod, used to drive the heating furnace 2 to move in the vertical direction, that is, to drive the heating furnace 2 to rise and fall in the vertical direction, so as to realize that the heating furnace 2 is sleeved on the outside of the mold 1 cylinder 1a or removed from the outside of the mold 1 cylinder 1a.

[0054] The specific workflow is as follows: First, at the loading station, the sleeve 9 containing the mixed powder is loaded into the cylindrical cavity of the mold 1, and the pressure plate 15 is installed on top of the cylindrical cavity; then, the heating furnace 2 is driven downward by the vertical drive component, so that the heating furnace 2 is fitted outside the cylinder 1a of the mold 1, the heating furnace 2 is started to heat the mold 1, and at the same time the support component 41 is driven to move horizontally, so that the insertion pipe 42 is inserted into the first interface 10 and the second interface 11, and a negative pressure suction force is applied to the insertion pipe 42 to evacuate the inside of the sleeve 9 and the cylindrical cavity respectively; after the heating and heat preservation is completed, the heating furnace 2 is driven upward by the vertical drive component to remove the heating furnace 2 from the outside of the cylinder 1a; then the mold 1 is transported horizontally to the top and bottom pressure components 31 of the press by the conveying unit 5; the press is started, the top pressure component moves downward, and pressure is applied to the pressure plate 15 to complete the hot pressing densification molding. The combination of the aforementioned automated conveying and heating systems enables continuous operation in the preparation of large-sized billets, significantly improving production efficiency and reducing quality instability caused by manual operation.

[0055] Example 2 refer to Figure 16 This application also provides a preparation process for large-size high thermal conductivity aluminum-based composite materials, which includes the following steps: First, the uniformly mixed aluminum matrix powder and reinforcing phase particles are loaded into the sleeve 9. The powder mixing can be carried out by mechanical mixing or high-energy ball milling. The sleeve 9 containing the mixed powder is placed in the cylindrical cavity of the mold 1, and the pressure plate 15 is guided and fitted to the top of the cylindrical cavity.

[0056] The mold 1 is placed entirely in the heating furnace 2 for heating. During the heating process, the temperature of the mold 1 gradually increases and is transferred to the sleeve 9 and the mixed powder inside, so that the mixed powder reaches a temperature suitable for hot pressing and sintering. The heating temperature is generally 550℃~650℃, the heating rate is 10℃ / h~50℃ / h, and the holding time is 3h~20h.

[0057] A vacuum is evacuated inside the casing 9 to remove gas from the gaps between the mixed powders and from the powder surface, thus preventing residual pores in the sintered body. The vacuum level inside the casing 9 is 110 Pa to 120 Pa. Simultaneously, a vacuum is evacuated from the space below the pressure plate 15 in the columnar cavity. During evacuation, the negative pressure inside the columnar cavity is greater than the negative pressure inside the casing 9; specifically, the vacuum level inside the columnar cavity is 1 / 10 to 1 / 2 of the vacuum level inside the casing 9. Thus, the upper side of the pressure plate 15 bears atmospheric pressure, and the lower side of the pressure plate 15 bears the negative pressure from the columnar cavity, creating a pressure difference between the upper and lower sides of the pressure plate 15. This pressure difference applies a downward preload to the pressure plate 15, which is then transmitted to the casing 9, initially compacting the mixed powder inside the casing 9. Simultaneously, a pressure difference is also generated within the columnar cavity and the casing 9.

[0058] Meanwhile, the inner wall of the cylindrical cavity applies a radial constraint force to the outer circumferential surface of the sleeve 9, effectively suppressing the uneven shrinkage of the sleeve 9 wall under negative pressure. Through the above-mentioned dual pressure difference design, the axial pre-compression and radial constraint of the sleeve 9 are achieved during the vacuuming stage, ensuring the shape regularity of the billet during the vacuuming stage.

[0059] After heating and heat preservation, the mold 1, sleeve 9, and pressure plate 15 are placed as a whole on the working platform of the press. Pressure is applied to the pressure plate 15 by the press, and this pressure is evenly transmitted to the sleeve 9 through the pressure plate 15, causing the mixed powder inside the sleeve 9 to densify and form under the combined action of high temperature and high pressure. The pressure applied by the press is generally 20MPa to 150MPa, and the holding time is 2min to 20min. Since the sleeve 9 has maintained good cylindricity during the vacuum stage, the unidirectional pressure applied by the press can be evenly transmitted, avoiding local stress concentration and density differences caused by uneven billet shape, thereby ensuring the forming quality of large-sized billets. In addition, the cylindrical cavity of the mold 1 continuously provides radial constraint during the hot pressing stage, further ensuring the dimensional accuracy of the billet.

[0060] After hot pressing and densification is completed, the mold 1, the sleeve 9 and the billet are cooled to an appropriate temperature as a whole, and then the sleeve 9 is separated from the mold 1.

[0061] During separation, mold 1 is driven directly below heating furnace 2, and then insertion pipe 42 is inserted into the interface. Positive air pressure (i.e., gas pressure higher than atmospheric pressure) is then introduced into the negative pressure port. This positive air pressure acts on the lower side of pressure plate 15, pushing it upwards out of the cylindrical cavity. During the hot pressing stage, pressure plate 15 may undergo slight elastic deformation or develop adhesion with the inner wall of the cylindrical cavity under the high pressure of the press, causing it to become stuck and difficult to remove. By introducing compressed gas through positive pressure ports located at the bottom or side wall of the cylindrical cavity, the upward thrust of the air pressure smoothly pushes pressure plate 15 out, avoiding damage to mold 1 or billet caused by mechanical hammering or prying. This design significantly improves the convenience and safety of demolding, and is especially suitable for the preparation of large-sized billets, as the pressure plate 15 corresponding to large-sized billets is larger in size and weight, making mechanical demolding more difficult. The pneumatic-assisted demolding method effectively solves this problem. Finally, the cladding 9 is removed by machining (such as turning or milling) to obtain the final composite material billet. Cooling can be achieved by furnace cooling or air cooling, and the cooling rate is selected according to the material system and billet size to avoid thermal stress caused by excessive cooling rate, which could lead to billet cracking.

[0062] Through the above steps, this preparation process not only eliminates the reliance on expensive vacuum hot press furnaces or hot isostatic pressing furnaces, reducing equipment investment and production costs, but also achieves axial pre-compression and radial constraint on the sleeve 9 during the vacuuming stage through the differentiated negative pressure design of the vacuuming inside the sleeve 9 and the vacuuming in the cylindrical cavity. This effectively suppresses uneven shrinkage of the sleeve 9 and simultaneously creates a pressure difference between the upper and lower sides of the pressure plate 15, providing pre-pressure to the sleeve 9 before hot pressing. The comprehensive application of the above technical means significantly improves the forming quality of the billet and enables the stable preparation of large-size, high thermal conductivity aluminum-based composite material billets with diameters greater than 400 mm and even reaching 2000 mm.

[0063] In practice, SiC powder with an average particle size of 50 micrometers and 6061 aluminum alloy powder with an average particle size of 40 micrometers are selected and mixed according to a 55 vol.% SiC / 6061 composition. The mixture is then loaded into a mixer at a ball-to-powder ratio of 1:1 and mixed for 4 hours. A total of 3000 kg of the mixed powder is then packed into an 1100 aluminum sheath with an inner diameter of 1500 mm, a height of 1000 mm, and a wall thickness of 5 mm. The loose packing density is approximately 56%. The aluminum sheath is sealed using argon arc welding, and a vacuum pipe is simultaneously welded in place. The sheath containing the mixed powder is then placed into a cylindrical cavity in a steel mold with an inner diameter of 1520 mm, a height of 1300 mm, and a wall thickness of 70 mm.

[0064] First, evacuate the cylindrical cavity until the vacuum level reaches 50 Pa. Then, evacuate the inside of the casing. Control the pumping rates of the first and second vacuum units to maintain the vacuum level inside the casing between 110 Pa and 120 Pa, and the vacuum level inside the cylindrical cavity between 10 Pa and 50 Pa.

[0065] Heating was performed under the aforementioned vacuum conditions at a rate of 30°C / hour until a temperature of 620°C was maintained for 10 hours, with the vacuum level inside the casing maintained at 115 Pa and the vacuum level inside the cylindrical cavity maintained at 30 Pa. After the holding period, the mold was transferred to the hydraulic press table within 3 minutes, and hot-pressing was performed at a pressure of 60 MPa for 15 minutes. After the mold cooled to room temperature, positive air pressure was introduced into the cylindrical cavity, and the pressure plate was ejected under the pressure. The casing was then removed by machining to obtain a dense ingot with a diameter of 1500 mm and a height of 550 mm.

[0066] The 55 vol.% SiC / 6061Al composite material prepared in this embodiment has a three-point flexural strength of 425 MPa in the annealed state, a thermal conductivity of 202 W / m·K, and a coefficient of thermal expansion of 9.2 × 10⁻⁶. -6 / K. The cylindricity test results of the billet show that the radial runout error of the billet is less than 0.5 mm, which is significantly better than the forming accuracy of the existing technology.

[0067] Comparative Example The same raw material ratio and mixing process as in the previous example were used: SiC powder with an average particle size of 50 micrometers and 6061 aluminum alloy powder with an average particle size of 40 micrometers were selected and mixed according to a 55 vol.% SiC / 6061 composition. The mixture was then loaded into a mixer at a ball-to-powder ratio of 1:1 and mixed for 4 hours. A total of 3000 kg of the mixed powder was packed into an 1100 aluminum sheath with an inner diameter of 1500 mm, a height of 1000 mm, and a wall thickness of 5 mm. The loose packing density was approximately 56%. The aluminum sheath was sealed using argon arc welding, and a 1100 aluminum tube with a wall thickness of 4 mm and an inner diameter of 12 mm was welded in as a vacuum pipe. The sheath containing the mixed powder was then placed into a steel mold with an inner diameter of 1520 mm, a height of 1300 mm, and a wall thickness of 70 mm. 100 mm thick steel pads were placed at the top and bottom of the mold. The mold with the sheath is hoisted into the resistance furnace, the evacuation pipe is extended outside the furnace, and a vacuum unit is used to evacuate the air. Once the vacuum is better than 1.0 Pa, heating begins at a rate of 30℃ / hour until it reaches 620℃ and is held for 10 hours at a vacuum level of 1.0 Pa. The evacuation system is then shut off, and the mold is removed from the furnace within 3 minutes and hoisted onto the press table. Hot pressing is performed at 60 MPa pressure for 15 minutes. After the mold cools to room temperature, the mold and sheath are removed by machining to obtain a dense ingot with a diameter of 1500 mm and a height of 550 mm.

[0068] The 55 vol.% SiC / 6061Al composite material prepared using this comparative example exhibits a three-point flexural strength of 420 MPa in the annealed state, a thermal conductivity of 200 W / m·K, and a coefficient of thermal expansion of 9.2 × 10⁻⁶. -6 / K. The cylindricity test results of the billet show that the radial runout error of the billet is about 3mm, and there are obvious local depressions and protrusions on the surface of the billet. This is due to the uneven shrinkage of the cladding under negative pressure during the vacuuming stage.

[0069] A comparison between the embodiments and the comparative examples shows that their mechanical and thermophysical properties are basically equivalent, but the billet forming quality of the embodiments is significantly better than that of the comparative examples. The embodiments, by simultaneously evacuating the cylindrical cavity and controlling differentiated negative pressure during the vacuuming stage, generate pre-pressure on the pressure plate and apply radial constraint to the sheath, effectively suppressing uneven shrinkage of the sheath. The radial runout error of the billet is reduced from 3 mm in the comparative example to below 0.5 mm, and the forming accuracy is improved by 6 times. This indicates that the differentiated negative pressure design of the present invention significantly improves the forming quality of large-size billets while ensuring material properties, providing higher-precision billets for subsequent forging, extrusion, rolling, and other deformation processes.

[0070] Obviously, the above embodiments are merely illustrative examples for clear explanation and are not intended to limit the implementation. Those skilled in the art will recognize that other variations or modifications can be made based on the above description. It is neither necessary nor possible to exhaustively list all possible implementations here. However, obvious variations or modifications derived therefrom are still within the scope of protection of this invention.

Claims

1. A preparation process for a large-size, high thermal conductivity aluminum-based composite material, characterized in that, Includes the following steps: Step 1: Pack the uniformly mixed aluminum matrix powder and reinforcing phase particles into a sleeve, place the sleeve in the cylindrical cavity of the mold, and guide the pressure plate to fit the top of the cylindrical cavity; Step 2: Place the entire mold in a heating furnace for heating; Step 3: Vacuum the inside of the casing and simultaneously vacuum the space below the pressure plate of the columnar cavity. The negative pressure value inside the columnar cavity is greater than the negative pressure value inside the casing, so that a pressure difference is formed on the upper and lower sides of the pressure plate and a pre-pressure is applied to the casing. The inner wall of the columnar cavity applies a radial constraint force to the outer circumference of the casing. Step 4: After heating and heat preservation, place the mold, sleeve and pressure plate as a whole in the press. Apply pressure to the pressure plate through the press and transfer the pressure to the sleeve to densify and form the mixed powder.

2. The preparation process of a large-size high thermal conductivity aluminum-based composite material according to claim 1, characterized in that, Also includes: Step 5: After cooling, separate the sleeve from the mold and remove the sleeve.

3. The preparation process of a large-size high thermal conductivity aluminum-based composite material according to claim 1, characterized in that, The vacuum level inside the sheath is 110 Pa to 120 Pa, and the vacuum level inside the cylindrical cavity is 1 / 10 to 1 / 2 of the vacuum level inside the sheath.

4. The preparation process of a large-size high thermal conductivity aluminum-based composite material according to claim 2, characterized in that, When separating the sleeve from the mold, positive air pressure is introduced into the cylindrical cavity, and the pressure plate is pushed out of the cylindrical cavity by the air pressure.

5. A device for preparing large-size, high thermal conductivity aluminum-based composite materials, characterized in that, include: The mold has a cylindrical cavity with an open top for placing the package, an insertion groove at the bottom of the cylindrical cavity, and a suction port on the side wall; The pressure plate and guide plate are fitted to the top of the columnar cavity and can slide up and down along the axial direction of the columnar cavity; The outer wall of the mold is provided with a first interface and a second interface, which are respectively connected to the insertion slot and the suction port. The insertion slot is used to insert and cooperate with the suction pipe that is built into the cylindrical cavity. During operation, the negative pressure value of the first interface is less than that of the second interface, so that a pressure difference is formed simultaneously on the upper and lower sides of the pressure plate and the inner and outer sides of the casing.

6. The apparatus for preparing large-size high thermal conductivity aluminum-based composite materials according to claim 5, characterized in that, The edge of the pressure plate is provided with a plurality of rigid members arranged at intervals around its own axis. The inner circumferential surfaces of the plurality of rigid members are all on the same columnar surface, which is coaxial with the pressure plate. The radial dimension of the columnar surface is smaller than the radial dimension of the inner circumferential surface of the columnar cavity.

7. The apparatus for preparing large-size high thermal conductivity aluminum-based composite materials according to claim 6, characterized in that, Multiple guide ribs are evenly spaced around the axis on the inner circumferential surface of the cylindrical cavity. The rigid member is inserted between two adjacent guide ribs, and the guide ribs are located outside the cylindrical surface.

8. The apparatus for preparing large-size high thermal conductivity aluminum-based composite materials according to claim 6, characterized in that, The suction port is located on the side wall of the guide rib near the axis of the pressure plate.

9. The apparatus for preparing large-size high thermal conductivity aluminum-based composite materials according to claim 5, characterized in that, The mold includes a base and a cylindrical body disposed on top of the base; The heating furnace has a cylindrical structure and is fitted around the outside of the cylinder from top to bottom. A heat-insulating sealing element is provided between the lower end and the outer periphery of the cylinder, and a balance port is provided on the side wall.

10. The apparatus for preparing large-size high thermal conductivity aluminum-based composite materials according to claim 9, characterized in that, Also includes: A conveying unit is used to transport the mold horizontally; A press is located at one end of a conveying unit and includes a top pressing component and a bottom pressing component disposed on the upper and lower sides of the conveying unit. The conveying unit is capable of conveying the mold between the top pressing component and the bottom pressing component. A vertical drive unit is located at the other end of the conveying unit and is used to drive the heating furnace to move vertically.