Method for repairing and connecting thin-walled metal parts

By employing powder bed electron beam additive manufacturing technology and utilizing non-uniform energy distribution and path planning, the issues of welding accuracy and cost for thin-walled metal parts have been resolved, enabling efficient and low-cost batch repair.

CN123149418APending Publication Date: 2026-11-24XIAN SAILONG AM TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611663556.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-27
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In the existing technology, the welding and repair of thin-walled metal parts are complicated by high cost, difficulty in achieving precision, and poor versatility of tooling and fixtures. In particular, welding deviation and burn-through are easily caused when welding curved seams.

Method used

By rationally planning the welding path and designing the electron beam energy, powder bed electron beam additive manufacturing is adopted. The angle between the electron beam scanning path and the joint trajectory is controlled to be no less than the preset angle. The area is divided into sub-regions and scanned alternately. The scanning line energy density is non-uniformly distributed and gradually changes with the joint trajectory as the center.

Benefits of technology

It enables efficient batch repair of joints of any shape, ensuring connection quality, preventing burn-through of thin-walled parts, and is simple to operate, low in cost, and suitable for ultra-thin metal parts with a thickness of less than 1mm.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123149418A_ABST
    Figure CN123149418A_ABST
Patent Text Reader

Abstract

This disclosure relates to a method for repairing and joining thin-walled metal parts. The method includes: assembling the thin-walled parts to be repaired to form a joint and placing them on the same horizontal plane; acquiring a two-dimensional trajectory of the joint; and using this trajectory as the center to form a region to be joined; planning an electron beam scanning path within the region, ensuring the angle between the scanning path and the external tangent of the joint trajectory is not less than a preset angle; dividing the region into several sub-regions, with equally spaced parallel scanning lines within each sub-region and overlapping at the boundaries of adjacent sub-regions; placing the workpiece on a powder bed electron beam additive manufacturing equipment forming platform, positioning the joint at the focal plane; and controlling the electron beam to scan and melt line by line in an alternating scanning sequence according to the sub-regions, with the energy density of each scanning line non-uniformly distributed around the joint trajectory, increasing closer to the joint. This invention eliminates the need for complex tooling fixtures, avoids burn-through and weld misalignment in thin-walled parts, supports batch repair of joints of arbitrary shapes, and offers high-quality, efficient, and low-cost connections.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of metal additive manufacturing and repair technology, and in particular to a repair and connection method for thin-walled metal parts. Background Technology

[0002] Thin-walled metal components are widely used in aerospace, automotive, and electronics industries, and the quality of their connection and repair directly affects their performance. While existing technologies have reported on the welding and repair of thin-walled metal components, the following problems are commonly observed: In existing technologies, to address the problem of easily deformed and difficult-to-position drum-shaped thin-walled parts for aero-engines, two halves of the part are manufactured separately using ordinary stamping and stretching forming equipment, and then the two halves are joined and welded together. This method is complex, requires additional assembly and forming processes, and is inefficient and costly. Alternatively, the thin-walled cylindrical part to be welded is inserted into the gap between the outer tire and the inner expansion tire, with the weld seam located at the opening between the outer tire and the inner expansion tire to reduce welding deformation. However, this tooling requires changing the inner and outer tires according to different cylindrical parts, has poor tooling versatility, is only suitable for thin-walled cylindrical parts, and requires changing the fixture according to the cylinder diameter, making operation inconvenient and costly. Another approach is to control the weld depth ≥2mm and the molten pool width ≥1mm by adjusting the focal depth, linear velocity, and beam current during electron beam welding to achieve curved welding. However, the extreme weld depth and molten pool width achieved by electron beam welding exceed the thickness of the thin-walled metal part, causing severe burn-through, and is unsuitable for connecting or repairing thin-walled metal parts. Alternatively, the problem of electron beam weld deviation on the spatial curved surface of hollow blades can be solved through multi-axis control of spatial attitude. The weld width of thin-walled metal components is generally no more than 1 mm, and the accuracy of multi-axis control mechanical alignment methods is difficult to achieve in order to prevent weld deviation.

[0003] In summary, current technologies for welding and repairing thin-walled metal parts generally require additional tooling and fixtures for fixation. These tooling and fixtures are complex to design and must be specific to the thin-walled workpiece, making them non-universal, costly to design and manufacture, and complex to operate. For welding thin-walled parts with curved welds, electron beam welding, currently the most precise welding method, is employed. However, its lower current limit remains high, and the minimum energy limit can still cause burn-through in ultra-thin metal components less than 1 mm thick. Furthermore, using multi-axis rotational mechanical motion to center the weld seam is insufficient to meet the accuracy requirements for the weld width of ultra-thin-walled components, leading to weld misalignment, burn-through, and weld defects.

[0004] Therefore, it is necessary to improve one or more of the problems existing in the above-mentioned related technical solutions.

[0005] It should be noted that the information disclosed in the background section above is only used to enhance the understanding of the background of this disclosure, and therefore may include information that does not constitute prior art known to those skilled in the art. Summary of the Invention

[0006] The purpose of this disclosure is to provide a repair and connection method for thin-walled metal parts, applicable to ultra-thin metal parts with a thickness of less than 1 mm. By rationally planning the welding path and designing the beam energy, it solves the problems of burn-through and connection quality caused by welding misalignment due to the difficulty in locating the connection seam during the repair of thin-walled parts. It can support batch repair of connection seams of any shape and improve the efficiency of repairing thin-walled curved connections.

[0007] The objective of this invention is achieved through the following technical solution: This invention provides a method for repairing and connecting thin-walled metal parts, comprising: The thin-walled metal parts to be connected and repaired are spliced ​​together to form a joint, and the joint is placed in the same horizontal plane. Obtain the trajectory of the seam in a two-dimensional plane, and form the area to be connected by offsetting to both sides of the trajectory as the center. Plan an electron beam melting scanning path within the area to be connected, such that the angle between the scanning path and the external tangent of the trajectory of the connecting seam in the two-dimensional plane is not less than a preset angle. Based on the included angle, the scanning path within the area to be connected is divided into several sub-regions, and the scanning lines within each sub-region are parallel straight lines with equal spacing; the scanning paths of adjacent sub-regions overlap at the boundary. The assembled thin-walled metal parts are placed on the forming platform of the powder bed electron beam additive manufacturing equipment, so that the joint is horizontally positioned at the focal plane height of the electron beam. The electron beam is controlled to scan and melt the joint along the scanning path. According to the order of alternating scanning of sub-regions, the first scan line in each sub-region is scanned in turn, and then the second scan line adjacent to the first scan line in each sub-region is scanned in turn. This process is repeated until the scanning and melting of all sub-regions is completed. The energy density of each scan line is non-uniformly distributed, with the energy density being higher closer to the connecting seam trajectory and lower further away from the connecting seam trajectory.

[0008] Optionally, the thickness of the thin-walled metal part is less than 1 mm; the width d of the connecting seam satisfies: 0 < d < min(t1, t2), where t1 and t2 are the thicknesses of the two thin-walled metal parts to be connected and repaired, respectively.

[0009] Optionally, the width W of the region to be connected satisfies: d < W < d + 3 / 4(t1 + t2).

[0010] Optionally, the preset angle is 30°~90°.

[0011] Optionally, the preset angle is 90°, so that the scanning path and the external tangent of the trajectory of the connecting seam intersect perpendicularly in a two-dimensional plane.

[0012] Optionally, the sub-region includes four sub-regions, namely a first sub-region, a second sub-region, a third sub-region, and a fourth sub-region, wherein the scan lines in the first and third sub-regions are horizontal scan lines, and the scan lines in the second and fourth sub-regions are vertical scan lines; The specific order of alternating scanning of sub-regions is as follows: First, scan the first line of the first sub-region, the first line of the second sub-region, the first line of the third sub-region, and the first line of the fourth sub-region in sequence. Then, scan the second line of the first sub-region adjacent to the first line, the second line of the second sub-region adjacent to the first line, the second line of the third sub-region adjacent to the first line, and the second line of the fourth sub-region adjacent to the first line in sequence. Repeat the above order until all sub-regions are scanned and melted.

[0013] Optionally, the spacing between the equally spaced parallel lines is h, satisfying: 0 < h < D, where D is the diameter of the electron beam spot; the distance between the vertices of adjacent scan lines at the outer tangent of the region to be connected is h.

[0014] Optionally, the non-uniform distribution of energy density of each scan line specifically means that it follows a normal distribution centered on the trajectory of the connecting seam, and the energy density in the area to be connected is not less than the half-width at half-maximum of the normal distribution curve.

[0015] Optionally, the electron beam scanning power P and scanning speed V are adjusted according to the material of the thin-walled metal part, with P / V representing the energy input. Materials with higher melting points use a larger P / V, and materials with lower melting points use a smaller P / V.

[0016] Optionally, the connecting seam can be a straight line, a curved line, or an arbitrary shape; the method is used for batch connection repair of thin-walled metal parts; the powder bed electron beam is controlled by a magnetic field deflection system to move the electron beam spot at high speed.

[0017] The technical solutions provided by the embodiments of this disclosure may include the following beneficial effects: In the embodiments of this disclosure, by setting the area to be connected and planning the scanning path, planar connection of seams of arbitrary shapes can be supported, with high connection quality and efficiency; by controlling the non-uniform energy distribution of the electron beam, the connection repair quality is guaranteed, the thin-walled parts are prevented from being burned through, and the connection positioning accuracy is guaranteed; batch connection repair of thin-walled metal parts can be realized with high efficiency; the operation is simple and the cost is low.

[0018] It should be understood that the above general description and the following detailed description are exemplary and explanatory only, and are not intended to limit this disclosure. Attached Figure Description

[0019] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this disclosure and, together with the description, serve to explain the principles of this disclosure. It is obvious that the drawings described below are merely some embodiments of this disclosure, and those skilled in the art can obtain other drawings based on these drawings without any inventive effort.

[0020] Figure 1 This diagram illustrates a process flow of a method for repairing and connecting thin-walled metal parts according to an exemplary embodiment of this disclosure.

[0021] Figure 2 A schematic diagram of the seam trajectory in an exemplary embodiment of this disclosure is shown.

[0022] Figure 3 A schematic diagram of the region to be connected in an exemplary embodiment of this disclosure is shown.

[0023] Figure 4 This diagram illustrates the intersection of the electron beam scanning path and the trajectory line of the connecting seam at an angle θ in an exemplary embodiment of this disclosure.

[0024] Figure 5 A schematic diagram of electron beam scanning path partitioning in an exemplary embodiment of this disclosure is shown.

[0025] Figure 6 This diagram illustrates the distribution of electron beam scanning paths at intervals h within each sub-region in an exemplary embodiment of this disclosure.

[0026] Figure 7 This diagram illustrates the energy density of the connecting melting line in an exemplary embodiment of the present disclosure. Detailed Implementation

[0027] Exemplary embodiments will now be described more fully with reference to the accompanying drawings. However, these exemplary embodiments can be implemented in many forms and should not be construed as limited to the examples set forth herein; rather, they are provided so that this disclosure will be more comprehensive and complete, and will fully convey the concept of the exemplary embodiments to those skilled in the art. The described features, structures, or characteristics may be combined in any suitable manner in one or more embodiments.

[0028] Furthermore, the accompanying drawings are merely illustrative of this disclosure and are not necessarily drawn to scale. The same reference numerals in the drawings denote the same or similar parts, and therefore repeated descriptions of them will be omitted. Some block diagrams shown in the drawings are functional entities and do not necessarily correspond to physically or logically independent entities. These functional entities may be implemented in software, in one or more hardware modules or integrated circuits, or in different network and / or processor devices and / or microcontroller devices.

[0029] This example embodiment first provides a method for repairing and connecting thin-walled metal parts. (See reference...) Figure 1 As shown, it includes: Step S101: Assemble the thin-walled metal parts to be connected and repaired, so that a connecting seam is formed at the joint, and place the connecting seam in the same horizontal plane.

[0030] Step S102: Obtain the trajectory of the connecting seam in a two-dimensional plane, and offset to both sides of the trajectory to form the area to be connected.

[0031] Step S103: Plan an electron beam melting scanning path in the area to be connected, so that the angle between the scanning path and the external tangent of the trajectory of the connecting seam in the two-dimensional plane is not less than a preset angle.

[0032] Step S104: Based on the included angle, the scanning path in the area to be connected is divided into several sub-regions, and the scanning lines in each sub-region are parallel straight lines with equal spacing; the scanning paths of adjacent sub-regions overlap at the boundary.

[0033] Step S105: Place the assembled thin-walled metal part on the forming platform of the powder bed electron beam additive manufacturing equipment, so that the joint is horizontally positioned at the focal plane height of the electron beam.

[0034] Step S106: Control the electron beam to scan and melt the seam along the scanning path. According to the order of alternating scanning of sub-regions, first scan the first scan line in each sub-region, then scan the second scan line adjacent to the first scan line in each sub-region, and repeat until the scanning and melting of all sub-regions is completed.

[0035] The energy density of each scan line is non-uniformly distributed, with the energy density being higher closer to the connecting seam trajectory and lower further away from the connecting seam trajectory.

[0036] It is important to understand that a method for repairing and joining thin-walled metal parts is provided. This method first involves assembling the thin-walled metal parts to be repaired, forming a seam at the joint, and placing the seam within the same horizontal plane. Specifically, two thin-walled metal parts to be repaired are assembled according to their target shapes, ensuring the seam is within the same horizontal plane so that it is at the focal plane height of the electron beam during subsequent scanning. Then, the trajectory of the seam in a two-dimensional plane is acquired, and the area to be joined is formed by offsetting to both sides of this trajectory. The seam can be a straight line, a curve, or any shape. In the two-dimensional plane, its trajectory line is generated along the seam, and a certain distance is offset to both sides from this trajectory line, forming a strip-shaped area of ​​a certain width W, i.e., the area to be joined. This area to be joined covers the seam and the adjacent base material areas on both sides, ensuring that the metal on both sides of the seam can be fully melted and self-fused during electron beam scanning.

[0037] It is also important to understand that the electron beam melting scanning path is planned within the area to be joined, ensuring that the angle between the scanning path and the external tangent of the connecting seam trajectory in the two-dimensional plane is not less than a preset angle. The preset angle refers to the minimum angle between the scanning path and the external tangent of the connecting seam trajectory. When the connecting seam is curved, the external tangent directions at different points on the connecting seam trajectory are different, and the tangents at the intersection of the scanning path and the connecting seam trajectory form an angle. This angle, not less than the preset angle, ensures that the scanning path crosses the connecting seam, rather than being parallel to it, thus allowing the electron beam energy to effectively act on both sides of the connecting seam, forming a sufficient molten pool for self-fusion welding. If the angle is too small, the scanning path and the connecting seam trajectory tend to be parallel, resulting in less beam current acting on the parts to be joined, and insufficient molten pool for self-fusion welding. Therefore, the angle needs to be controlled within a range not less than the preset angle.

[0038] It is also important to understand that, based on the aforementioned angle, the scanning path within the area to be connected is divided into several sub-regions. Within each sub-region, the scanning lines are equally spaced parallel straight lines; the scanning paths of adjacent sub-regions overlap at their boundaries. Since the connecting seam may be curved, its external tangent direction varies along the trajectory. To ensure that the angle requirement between the scanning path and the external tangent of the connecting seam trajectory is met throughout the entire area to be connected, the area to be connected needs to be divided into several sub-regions along the connecting seam trajectory. Within each sub-region, the external tangent direction of the connecting seam trajectory changes less, and equally spaced parallel straight lines can be planned as scanning lines within this sub-region. At the boundaries of adjacent sub-regions, the scanning paths overlap to ensure the connection effect at the boundaries and avoid incomplete fusion defects.

[0039] It's also important to understand that the assembled thin-walled metal parts are placed on the forming platform of the powder bed electron beam additive manufacturing equipment, with the joint horizontally positioned at the focal plane height of the electron beam. Powder bed electron beam additive manufacturing equipment typically includes a vacuum chamber, electron gun, magnetic field deflection system, forming platform, and powder supply system. The electron beam is generated by the electron gun, focused and deflected by the magnetic field deflection system, forming an electron beam spot on the forming platform. Placing the assembled thin-walled metal parts on the forming platform and adjusting their height so that the joint is located at the focal plane of the electron beam ensures the highest electron beam energy density and the smallest beam spot, thereby achieving precise scanning melting. Placing the joint horizontally facilitates vertical electron beam incidence, ensuring the accuracy of the scanning path.

[0040] It's also important to understand that the electron beam is controlled to scan and melt the joint along the scanning path. Following an alternating scanning sequence of sub-regions, the first scan line of each sub-region is scanned sequentially, followed by the second scan line adjacent to the first scan line, and so on, until all sub-regions are scanned and melted. Specifically, under the control of the magnetic field deflection system, the electron beam moves at high speed along a pre-planned scanning path. During scanning, instead of completing all scan lines of one sub-region before scanning the next, an alternating scanning method is used: first scanning the first scan line of each sub-region, then the second scan line, and so on, until all scan lines are completed. This scanning sequence ensures that the melting of each sub-region occurs almost simultaneously, resulting in a more uniform distribution of welding thermal stress and significantly reducing deformation problems in thin-walled parts caused by thermal stress concentration. The powder bed electron beam, controlled by the magnetic field deflection system, moves the electron beam spot at high speed, enabling rapid and tailless movement of the weld point, ensuring a uniform distribution of the weld point at the weld seam, making it more suitable for welding easily deformable thin-walled workpieces.

[0041] It is also important to understand that the energy density of each scan line is non-uniformly distributed. Centered on the seam track, the energy density is higher closer to the seam track and lower further away. Specifically, the energy density of the electron beam is not uniformly distributed along each scan line, but gradually decreases towards both sides of the seam track. Regions closer to the seam track require higher energy densities to ensure sufficient melting of the metal on both sides of the seam, forming a dense connection; regions farther from the seam track have lower energy densities to prevent overheating, deformation, or burn-through of the base material. This non-uniform energy distribution can be achieved by controlling the scanning speed, beam current intensity, or residence time of the electron beam. For example, the scanning speed can be reduced or the beam current increased in the portion of the scan line close to the seam track, while the scanning speed can be increased or the beam current decreased in the portion farther from the seam track.

[0042] Based on the above-mentioned repair and connection method for thin-walled metal parts, by setting the area to be connected and planning the scanning path, planar connection of seams of arbitrary shapes can be supported, with high connection quality and efficiency; by controlling the non-uniform energy distribution of the electron beam, the connection repair quality is guaranteed, the thin-walled parts are prevented from being burned through, and the connection positioning accuracy is guaranteed; batch connection repair of thin-walled metal parts can be realized with high efficiency; the operation is simple and the cost is low.

[0043] The following will describe in more detail each step of the repair and connection method for the thin-walled metal parts described in this example embodiment.

[0044] In one embodiment, reference Figures 2 to 6 As shown, the thickness of the thin-walled metal part is less than 1 mm; the width d of the connecting seam satisfies: 0 < d < min(t1, t2), where t1 and t2 are the thicknesses of the two thin-walled metal parts to be connected and repaired, respectively. This embodiment is applicable to the connection and repair of ultra-thin metal parts. The thicknesses of the two thin-walled metal parts to be connected can be the same or different, denoted as t1 and t2 respectively. To ensure the connection and repair effect, the smaller the connecting seam width, the better. Ideally, d should approach 0, indicating that the two connecting parts are closely adjacent. In actual operation, d is difficult to reach 0, and d is generally between 0.1 and 0.3 mm. To ensure sufficient molten material filling in the connecting seam, the connecting seam width d cannot exceed the thickness of the parts to be connected, therefore 0 < d < min(t1, t2). If the connecting seam width is too large, the molten material filling will be insufficient, which may easily lead to incomplete fusion or void defects; if the connecting seam width is too small, the two parts to be connected may directly contact each other without filling, but this is difficult to achieve in actual assembly. Therefore, this range ensures that the joint has enough space to fill the molten material without causing poor connection due to excessive gaps.

[0045] In one embodiment, reference Figures 2 to 6 As shown, the width W of the area to be connected satisfies: d < W < d + 3 / 4(t1 + t2). The span of the width W of the area to be connected must at least exceed the width d of the connecting seam, i.e., W > d, to ensure that the parts to be connected achieve self-fusion welding. To ensure the connection effect, the span of the connection path, in addition to crossing the connecting seam, must reach at least half the thickness of each connecting part at both ends of the path, and the maximum should not exceed 3 / 4 of the distance from the edge of the connecting seam towards the connecting part. If W is too large, too much molten material will be produced after the connecting parts are melted, which will cause deformation or burn-through of the connecting parts; if W is too small, the area to be connected will not completely cover the area on both sides of the connecting seam, resulting in a weak connection. Therefore, W satisfies d < W < d + 3 / 4(t1 + t2). This range ensures that the area to be connected can cover the connecting seam, and that the base material on both sides of the connecting seam can be partially melted to form a metallurgical bond, while avoiding excessive melting of the base material that could lead to deformation or burn-through.

[0046] In one embodiment, the preset angle is 30° to 90°. Connection repair is equivalent to stitching two parts together. The more perpendicular (90°) the stitching path is to the seam, the better the effect; the more parallel (0°) it is, the worse the effect. The minimum 30° limit is an empirically determined value. In actual operation, the angle is generally controlled at no less than 45° to ensure a 100% yield rate. When the angle is less than 30°, the scanning path is too parallel to the seam trajectory, the electron beam energy is dispersed, and a sufficiently deep molten pool cannot be formed, resulting in insufficient connection strength. Therefore, setting the preset angle to 30° to 90° ensures that the scanning path can effectively cross the seam while also providing process flexibility.

[0047] In one embodiment, reference Figure 6 As shown, the preset angle is 90°, ensuring that the scanning path intersects the external tangent of the connecting seam trajectory perpendicularly in a two-dimensional plane. This is the most preferred embodiment. When the scanning path is perpendicular to the external tangent of the connecting seam trajectory, the electron beam energy acts on both sides of the connecting seam to the maximum extent, forming a symmetrical molten pool, resulting in the best connection quality. Furthermore, the path planning is simple and suitable for connecting seams of various shapes. For straight connecting seams, the scanning path only needs to be perpendicular to the connecting seam; for curved connecting seams, in each sub-region, the scanning path is perpendicular to the average tangent direction of the connecting seam trajectory within that sub-region, thereby ensuring the connection quality throughout the entire connecting region.

[0048] In one embodiment, reference Figure 5 As shown, the sub-regions include four: a first sub-region, a second sub-region, a third sub-region, and a fourth sub-region. The scan lines in the first and third sub-regions are horizontal scan lines, while the scan lines in the second and fourth sub-regions are vertical scan lines. Specifically, in... Figure 5 In the diagram, sub-region ① represents the first sub-region, sub-region ② represents the second sub-region, sub-region ③ represents the third sub-region, and sub-region ④ represents the fourth sub-region. The specific order of alternating sub-region scanning is as follows: first, scan the first line of the first sub-region, the first line of the second sub-region, the first line of the third sub-region, and the first line of the fourth sub-region in sequence; then, scan the second line of the first sub-region adjacent to the first line, the second line of the second sub-region adjacent to the first line, the second line of the third sub-region adjacent to the first line, and the second line of the fourth sub-region adjacent to the first line in sequence. Repeat this sequence until all sub-regions have been scanned and melted. For example... Figure 5As shown, the scanning path at the joint is divided into four sub-regions. The first and third sub-regions are located on opposite sides of the joint, with their scanning lines being horizontal; the second and fourth sub-regions are located on the other two sides, with their scanning lines being vertical. This partitioning method ensures that the scanning lines within each sub-region meet the angle requirement with the external tangent of the joint trajectory. The alternating scanning sequence ensures that the melting of the four sub-regions occurs almost simultaneously, resulting in uniform thermal stress distribution and preventing localized overheating that could lead to deformation of the thin-walled part. For example, the first line of the first sub-region is scanned first, then the electron beam is moved to scan the first line of the second sub-region, then the first line of the third sub-region, then the first line of the fourth sub-region; then the second line of each sub-region is scanned, and so on. This scanning sequence disperses heat spatially, which is beneficial for controlling the heat-affected zone.

[0049] In one embodiment, reference Figure 6 As shown, the spacing between the equally spaced parallel lines is h, satisfying: 0 < h < D, where D is the electron beam spot diameter. At the outer tangent of the region to be connected, the vertex spacing of adjacent scan lines is h. The path spacing h, where h = 0 (path overlap), indicates that the energy source is repeatedly scanning the same path, which is ineffective and could cause burn-through of the component. Therefore, adjacent paths need to be spaced a certain distance, i.e., h > 0. The electron beam spot diameter is D. Scanning one path will cover an area of ​​width D. The next path scans immediately after the first path, i.e., h = D. To ensure the quality of the adjacent paths, there needs to be a certain amount of overlap between the two adjacent paths, i.e., h < D. In summary, 0 < h < D. This range ensures that there is sufficient overlap between adjacent scan lines to avoid unfused areas, while also preventing excessive energy input and burn-through due to excessive overlap. At the outer tangent of the connecting region, the vertex spacing of adjacent scan lines is h, where vertex refers to the endpoint of the scan line, and vertex spacing is the distance between the endpoints of adjacent scan lines at the boundary of adjacent sub-regions, ensuring that the scan lines at the boundary of sub-regions are evenly distributed and the connection quality is consistent.

[0050] In one embodiment, reference Figure 7 As shown, the energy density of each scan line is non-uniformly distributed specifically: it follows a normal distribution centered on the trajectory of the connecting seam, and the energy density within the region to be connected is not less than the half-width at half-maximum (WHM) of the normal distribution curve. Figure 7As shown, the energy density of the melting line follows a normal distribution centered on the connection line. The half-width at half-maximum (WHM) of the normal distribution curve refers to the width at which the energy density drops to half its maximum value. Ensuring that the energy density within the region to be joined is not less than the WHM of the normal distribution curve guarantees a dense connection without burning through the thin-walled metal component, while also ensuring accurate connection positioning. Specifically, the energy density is highest at the center of the scanning line, i.e., at the connection seam trajectory, ensuring sufficient melting of the metal on both sides of the seam; it gradually decreases towards both sides, reaching a lower level at the edge of the region to be joined. This non-uniform energy distribution can be achieved by controlling the scanning parameters of the electron beam, such as beam current, scanning speed, and focusing current. This implementation further ensures that the thin-walled component is not burned through while guaranteeing connection quality.

[0051] In one embodiment, the electron beam scanning power P and scanning speed V are adjusted according to the material of the thin-walled metal part, with P / V representing the energy input. Materials with higher melting points use a larger P / V, and materials with lower melting points use a smaller P / V. The above steps apply to thin-walled metal materials of different compositions. The difference lies in the electron beam scanning power P and scanning speed V. Generally, the P / V ratio represents the energy input; a larger ratio indicates a larger energy input, and vice versa. For metals with higher melting points, such as titanium alloys and nickel-based superalloys, a higher energy input (i.e., a larger P / V) is used to ensure melting; for metals with lower melting points, such as aluminum alloys and copper alloys, a lower energy input (i.e., a smaller P / V) is used. By adjusting P / V, the connection and repair needs of different materials can be met, ensuring connection quality and avoiding burn-through or lack of fusion.

[0052] In one embodiment, the joint seam is a straight line, a curve, or an arbitrary shape; the method is used for batch joint repair of thin-walled metal parts; the powder bed electron beam is controlled by a magnetic field deflection system to move the electron beam spot at high speed. The repair joint method of the present invention is not limited by the shape of the joint seam. Whether it is a straight line, a curve, or any complex shape, joint repair can be achieved by acquiring the joint seam trajectory, planning the area to be joined, and the scanning path. Because powder bed electron beam additive manufacturing equipment is used, the electron beam is controlled by a magnetic field deflection system, eliminating the need for mechanically moving the workpiece or electron gun, enabling high-speed scanning at speeds of several meters per second or even higher. Therefore, this method is particularly suitable for batch repair, allowing multiple thin-walled metal parts to be repaired to be placed on a forming platform and scanned and melted sequentially or simultaneously, significantly improving repair efficiency. Simultaneously, it is simple to operate, low in cost, and requires no complex tooling fixtures, possessing significant industrial application value.

[0053] It should be noted that although several modules or units for the device used to perform actions have been mentioned in the detailed description above, this division is not mandatory. In fact, according to embodiments of this disclosure, the features and functions of two or more modules or units described above can be embodied in one module or unit. Conversely, the features and functions of one module or unit described above can be further divided and embodied by multiple modules or units. Components shown as modules or units may or may not be physical units; that is, they may be located in one place or distributed across multiple network units. Some or all of the modules can be selected to achieve the purpose of this disclosure according to actual needs. Those skilled in the art can understand and implement this without any inventive effort.

[0054] Other embodiments of this disclosure will readily occur to those skilled in the art upon consideration of the specification and practice of the invention. This application is intended to cover any variations, uses, or adaptations of this disclosure that follow the general principles of this disclosure and include common knowledge or customary techniques in the art not disclosed herein. The specification and examples are to be considered exemplary only, and the true scope and spirit of this disclosure are indicated by the appended claims.

Claims

1. A method for repairing and connecting thin-walled metal parts, characterized in that, include: The thin-walled metal parts to be connected and repaired are spliced ​​together to form a joint, and the joint is placed in the same horizontal plane. Obtain the trajectory of the seam in a two-dimensional plane, and form the area to be connected by offsetting to both sides of the trajectory as the center. Plan an electron beam melting scanning path within the area to be connected, such that the angle between the scanning path and the external tangent of the trajectory of the connecting seam in the two-dimensional plane is not less than a preset angle. Based on the included angle, the scanning path within the area to be connected is divided into several sub-regions, and the scanning lines within each sub-region are parallel straight lines with equal spacing; the scanning paths of adjacent sub-regions overlap at the boundary. The assembled thin-walled metal parts are placed on the forming platform of the powder bed electron beam additive manufacturing equipment, so that the joint is horizontally positioned at the focal plane height of the electron beam. The electron beam is controlled to scan and melt the joint along the scanning path. According to the order of alternating scanning of sub-regions, the first scan line in each sub-region is scanned in turn, and then the second scan line adjacent to the first scan line in each sub-region is scanned in turn. This process is repeated until the scanning and melting of all sub-regions is completed. The energy density of each scan line is non-uniformly distributed, with the energy density being higher closer to the connecting seam trajectory and lower further away from the connecting seam trajectory.

2. The repair and connection method for thin-walled metal parts according to claim 1, characterized in that, The thickness of the thin-walled metal part is less than 1 mm; the width d of the connecting seam satisfies: 0 < d < min(t1, t2), where t1 and t2 are the thicknesses of the two thin-walled metal parts to be connected and repaired, respectively.

3. The repair and connection method for thin-walled metal parts according to claim 2, characterized in that, The width W of the region to be connected satisfies: d < W < d + 3 / 4(t1 + t2).

4. The repair and connection method for thin-walled metal parts according to claim 1, characterized in that, The preset angle is 30°~90°.

5. The repair and connection method for thin-walled metal parts according to claim 4, characterized in that, The preset angle is 90°, so that the scanning path and the external tangent of the trajectory of the connecting seam intersect perpendicularly in a two-dimensional plane.

6. The repair and connection method for thin-walled metal parts according to claim 1, characterized in that, The sub-regions include four sub-regions, namely the first sub-region, the second sub-region, the third sub-region, and the fourth sub-region. The scan lines in the first and third sub-regions are horizontal scan lines, and the scan lines in the second and fourth sub-regions are vertical scan lines. The specific order of alternating scanning of sub-regions is as follows: First, scan the first line of the first sub-region, the first line of the second sub-region, the first line of the third sub-region, and the first line of the fourth sub-region in sequence. Then, scan the second line of the first sub-region adjacent to the first line, the second line of the second sub-region adjacent to the first line, the second line of the third sub-region adjacent to the first line, and the second line of the fourth sub-region adjacent to the first line in sequence. Repeat the above order until all sub-regions are scanned and melted.

7. The repair and connection method for thin-walled metal parts according to claim 1, characterized in that, The spacing between the equally spaced parallel lines is h, satisfying: 0 < h < D, where D is the diameter of the electron beam spot; the distance between the vertices of adjacent scan lines at the outer tangent of the region to be connected is h.

8. The repair and connection method for thin-walled metal parts according to claim 1, characterized in that, The non-uniform distribution of energy density of each scan line specifically means that it follows a normal distribution centered on the trajectory of the connecting seam, and the energy density in the area to be connected is not less than the half-width at half-maximum of the normal distribution curve.

9. The repair and connection method for thin-walled metal parts according to claim 1, characterized in that, Based on the material of the thin-walled metal part, the electron beam scanning power P and scanning speed V are adjusted, with P / V representing the energy input. Materials with higher melting points use a larger P / V, and materials with lower melting points use a smaller P / V.

10. The method for repairing and connecting thin-walled metal parts according to any one of claims 1-9, characterized in that, The connecting seam can be straight, curved, or of any shape; the method is used for batch connection and repair of thin-walled metal parts; the powder bed electron beam is controlled by a magnetic field deflection system to move the electron beam spot at high speed.