Pulse direct current composite electric field bias anti-infiltration turbine blade film hole processing method
By employing a bias-based anti-backflow method using a pulsed DC composite electric field in the machining of film pores in turbine blades, the problems of cation migration from external impurities, improper utilization of passivation film protection, and uneven removal of the remelted layer were solved, achieving high-precision machining of film pores and ensuring machining quality and consistency.
Patent Information
- Application Number
- CN202611655004.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-26
- Publication Date
- 2026-11-24
AI Technical Summary
Existing turbine blade film hole machining processes suffer from problems such as the relocation and enrichment of exogenous impurity cations, the inefficient use of passivation film protection, uneven removal of the remelted layer, and the difficulty in eliminating pre-hole taper and insufficient forming accuracy of the expansion outlet during axial reciprocating machining.
A bias anti-backflow method using a pulsed DC composite electric field is employed. By establishing a dynamic positive bias safety window at different processing stages, and combining electrical discharge pre-holeing with sodium nitrate electrolysis, along with a solid rigid tool electrode and insulation design, axial reciprocating segmented electrolysis and radial hole enlargement are achieved, ensuring the safety and accuracy of the processing.
It effectively prevents the migration of exogenous impurity cations, makes reasonable use of passivation film protection, ensures uniform removal of remelted layer, eliminates pre-hole taper and achieves precise forming of one-sided expansion outlet, thus improving processing quality and consistency.
Smart Images

Figure CN123149502A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of special processing technology, specifically to a method for processing air film holes in turbine blades under biased anti-backflow conditions using a pulsed DC composite electric field. Background Technology
[0002] The film cooling holes of turbine blades are used to guide cooling gas to the blade surface. Their diameter, taper, outlet expansion morphology, and hole wall quality directly affect the coverage effect of the cooling film. Since turbine blades are usually made of difficult-to-machine materials such as high-temperature alloys, and the film cooling holes have small diameters and large depth-to-diameter ratios, machining is prone to tool wear and hole shape deviations. Therefore, electrical discharge machining (EDM) is usually used, or a composite machining method combining EDM pre-machining and electrolytic finishing is used.
[0003] When using integral conductive hollow electrodes in existing electrical discharge machining (EDM), the electrode sidewalls are prone to discharge, causing taper, ripples, remelted layers, and microcracks on the hole walls. Although EDM-electrolysis hybrid machining can remove some of the remelted layer, during the pulse interval, exogenous impurity cations present in the machining environment and working fluid may migrate back to the machined hole walls, accumulate, and form residues due to the combined effects of concentration gradients, working fluid flow, and residual electric fields. Simultaneously, if the corrosion removal products generated during machining are not fully discharged, they may also remain inside the hole, affecting the cleanliness of the hole walls and the quality of subsequent machining. If a fixed positive bias is used to suppress backflow, abnormal discharges may occur due to bubbles, temperature, and conductivity changes within the hole. On the other hand, the stable passivation film formed in sodium nitrate electrolyte is beneficial for suppressing stray corrosion in non-machined areas. If the passivation initiation is simply used as an unfavorable upper limit of the positive bias, the protective effect of the passivation film cannot be fully utilized.
[0004] Furthermore, the remelted layer thickness and electrolytic mass transfer conditions vary at different depths of the film pore. Existing methods, which remove the remelted layer using uniform processing time or charge, are prone to localized under-removal or over-removal. Pre-holes formed by small-diameter machines typically have a residual taper with a large inlet and a small outlet. Relying solely on the tool electrode reciprocating along the hole axis, even if one end reaches the target size, the other end may continue to expand, making it difficult to obtain a near-zero taper, uniform-diameter hole. For film pores with a one-sided expansion outlet section, selective outlet forming is required after the hole body has been precisely finished to a uniform diameter. Therefore, it is necessary to address the coordination issues between positive bias anti-backflow and stable utilization of the passivation film, differentiated removal of the remelted layer, uniform radial expansion after penetration, and precise control of the one-sided expansion outlet. Summary of the Invention
[0005] To address the technical problems in the existing turbine blade film pore composite machining process, such as the migration, enrichment, and deposition of exogenous impurity cations to the machined hole wall during the pulse interval, the unreasonable utilization of the stabilizing passivation film protection effect, uneven removal of the remelted layer, difficulty in eliminating the pre-hole taper during axial reciprocating machining, and insufficient forming accuracy of the expansion outlet, this invention provides a bias-based anti-backflow turbine blade film pore machining method using a pulsed DC composite electric field.
[0006] The technical solution adopted in this invention is: a method for machining film venting holes on turbine blades using a pulsed DC composite electric field to prevent backflow, which is used to machine film venting holes with a hole body and an expansion outlet section on one side on turbine blades, including the following steps:
[0007] S1, acquire the pore geometry data of the film gas pores, the calibration data of the workpiece material and the working fluid, and the inter-electrode state data; establish a dynamic positive bias safety window according to the processing stage, wherein, in the pre-hole stage of electrical discharge machining, characterize the corrosion removal products formed by the local melting, vaporization, peeling, or dispersion of the workpiece material through electrical discharge machining and entering the working fluid, and based on the migration state of exogenous impurity cations in the working fluid and processing environment that are different from the intrinsic elements of the workpiece matrix and do not belong to the current working fluid design components, and the migration state of the exogenous impurity cations into the already processed fluid. The trend of backflow, enrichment, and deposition on the borehole wall is used to determine the lower limit of the positive bias voltage required to prevent backflow. At the same time, the upper limit of the positive bias voltage is determined based on the gas-containing inter-electrode breakdown constraint and the allowable conditions of the anodic reaction at this stage. In the sodium nitrate electrolysis stage, the larger of the positive bias voltage required to prevent backflow and the positive bias voltage required to form and maintain the passivation film is used as the lower limit of the positive bias voltage, and the minimum of the allowable voltage of gas-containing inter-electrode breakdown, the allowable voltage of passivation film destruction, and the allowable voltage of oxygen evolution or excessive anodic reaction is used as the upper limit of the positive bias voltage. The initial processing control parameters are output under the constraint of the dynamic positive bias voltage safety window of the current processing stage.
[0008] S2, perform pre-hole drilling using electrical discharge machining (EDM). A positive bias voltage is superimposed on the EDM pulse, maintaining the positive polarity of the workpiece relative to the tool electrode and preventing it from returning to zero during the pulse interval. The inter-electrode electrical signal and working fluid status are acquired according to the control cycle. Based on the acquisition results, the lower and upper limits of the positive bias voltage for the current stage are updated, limiting the positive bias voltage within the updated dynamic positive bias voltage safety window. When the dynamic positive bias voltage safety window fails, the feed is immediately paused. If the current upper boundary still allows a non-zero protection bias voltage, the positive bias voltage is limited to a non-zero protection value within the upper boundary. If no non-zero allowable value exists, the positive bias voltage source is cut off. At least one of the inter-electrode gap, pulse interval, and working fluid circulation status is adjusted until the dynamic positive bias voltage safety window is restored. The pre-hole discharge history, pre-hole geometry data, and anomaly records are output.
[0009] S3, based on the pre-hole discharge history, pre-hole geometry data, and anomaly records output by S2, and combined with calibration data, determines the unit removal volume discharge energy and remelting layer removal allowance of the pre-hole wall during the pre-hole stage; divides the hole axis into multiple axial processing segments, establishes the minimum removal envelope for each axial processing segment based on the equivalent thickness of the remelting layer, determines the target semi-finished hole profile under the condition that the target semi-finished hole profile is outside the minimum removal envelope and retains a positive processing allowance for subsequent radial hole enlargement, and determines the volume to be removed by the material volume difference between the original measured profile of the pre-hole and the target semi-finished hole profile; when the above two conditions cannot be met simultaneously, automatic processing is stopped or manual verification is initiated; based on the reference volume electrochemical equivalent calibrated under the same material-working fluid reference conditions and the volume removal correction coefficient corresponding to the current processing conditions, the volume to be removed is converted into the effective charge required for electrolytic semi-finishing;
[0010] S4, drain the pre-hole working fluid and replace it with sodium nitrate aqueous solution, and replace it with a solid rigid tool electrode with only the axially locally conductive working section exposed and conductive, and the rest of the non-working surfaces insulated; based on the segmented effective charge output in S3, perform axial reciprocating segmented electrolytic semi-finishing under the constraint of the dynamic positive bias safety window in the updated electrolysis stage, so that the axial locally conductive working section acts on different axial processing sections in sequence, and the working fluid in the hole is periodically replaced with the axial reciprocating motion of the tool electrode. The passivation film formed and maintained by the sodium nitrate system is used to suppress stray corrosion in non-target areas, and the cumulative effective charge is used to control the remelting layer removal and pre-hole taper reduction process, outputting the semi-finished hole profile and segmented volume removal correction coefficient;
[0011] S5: After the bottom end of the solid rigid tool electrode has completely passed through the workpiece exit, based on the semi-finished hole profile, target hole profile, and segmented volume removal correction coefficient output in S4, set the initial safe radial offset, target radial offset, and effective radial reaming charge for each axial segment; align the locally conductive working segments of the axial direction with the corresponding axial segments in sequence; while maintaining the axial position, make the center of the tool electrode approach the target radial offset step by step from the initial safe radial offset according to the preset radial step size and the allocated effective charge, and perform radial-circumferential closed interpolation around the target hole axis at each offset position to maintain the effective machining clearance between the tool electrode and the current hole wall; perform circumferentially uniform segmented radial reaming finishing according to the effective radial reaming charge, and output the corrected hole profile after eliminating residual taper and the charge completion of each axial segment;
[0012] S6, based on the corrected hole contour and charge completion, segmented volume removal correction coefficient, and target surface of the one-sided expansion exit section output by S5, generates segmented pure electrolytic trajectories that only act on the preset expansion angle domain, and assigns effective charge to each trajectory segment; determines the initial safety offset of the exit forming based on the corrected hole radius, the equivalent radius of the axially locally conductive working section, and the exit forming processing gap; determines the target offset of the exit forming based on the target surface radius, the equivalent radius of the axially locally conductive working section, and the exit forming processing gap, so that the axially locally conductive working section is positioned at the exit section and radial-angular interpolation is performed in stages from the initial safety offset to the target offset, forming the one-sided expansion exit section while maintaining the effective processing gap;
[0013] S7 detects the hole geometry, inlet-outlet diameter difference, outlet profile, and pressure-flow characteristics of the completed hole. Based on the detection error, dynamic positive bias safety margin during processing, and abnormal records, it generates the parameter correction amount for the next film gas hole, which is limited by the calibration data. The parameter correction amount is then sent back to S1, S3, S5, and S6 to correct the initial processing control parameters, effective charge for remelting layer removal, radial offset, effective charge for radial hole expansion, and forming parameters of the expansion outlet section on one side for the next film gas hole.
[0014] In one embodiment, in S1, the lower limit of the positive bias voltage in the pre-hole stage of the electric spark is determined according to the anti-backflow requirement corresponding to the trend of the exogenous impurity cations migrating back, enriching and depositing to the processed hole wall. The upper limit of the positive bias voltage is the smaller value between the allowable voltage of the bubble equivalent channel breakdown and the allowable voltage of the anodic reaction in the pre-hole stage. After entering the sodium nitrate electrolysis stage, the lower limit of the positive bias voltage is the larger value between the positive bias voltage required for anti-backflow and the positive bias voltage required for the formation and maintenance of the passivation film. The upper limit of the positive bias voltage is the minimum value among the allowable voltage of the bubble equivalent channel breakdown, the allowable voltage of the passivation film destruction obtained by calibration with the same material and working fluid, and the allowable voltage of oxygen evolution or excessive anodic reaction. When the difference between the upper limit of the positive bias voltage and the lower limit of the positive bias voltage in the current stage is greater than the sum of the preset lower boundary margin and the preset upper boundary margin, the dynamic positive bias voltage safety window is determined to be effective.
[0015] In one embodiment, in S2, the interelectrode current during the pulse interval is attenuated and fitted to obtain the deionization time constant, and the current component higher than the steady-state leakage current is integrated to obtain the backflow characterization charge; the backflow characterization charge is a control characterization quantity that corresponds to the risk of the exogenous impurity cations migrating back, enriching, and depositing to the processed hole wall after calibration with the same material and working fluid, and its allowable limit is obtained by calibration test; when the dynamic positive bias voltage safety window is effective, the positive bias voltage of the next control cycle is updated in a restricted manner according to the difference between the required anti-backflow field strength and the measured positive bias voltage field strength and the deviation of the backflow characterization charge relative to the allowable limit, and the maximum positive bias voltage change in a single control cycle is limited so that the positive bias voltage remains non-zero during the update process and does not exceed the dynamic positive bias voltage safety window; when the dynamic positive bias voltage safety window fails, it is handled according to the abnormal recovery process.
[0016] In one embodiment, in S2, a hollow copper tool electrode with sidewall insulation and only bottom surface conductive is used for EDM pre-holeing. The initial positive bias voltage calibration range during the EDM pre-holeing stage is 3-8V. When at least two of the following conditions are met: inter-electrode voltage drop, peak current exceeding the limit, breakdown delay shortening, and pulse interval current decay slowing down, the corresponding control cycle is marked as an abnormal pulse cycle, and the hole axis position and discharge data of the abnormal pulse cycle are written into the abnormal record.
[0017] In one embodiment, in S3, the product of the inter-electrode voltage and inter-electrode current of each effective pulse in the pre-hole stage is integrated over time to obtain the single-hole discharge energy; the single-hole discharge energy is divided by the actual material removal volume in the pre-hole stage to obtain the unit removal volume discharge energy; the unit removal volume discharge energy and the abnormal pulse ratio are input together into the remelting layer calibration relationship established with the same material, the same working fluid, and the corresponding pulse energy range to obtain the equivalent thickness of the remelting layer; a minimum removal envelope is established based on the measured profile of the pre-hole, the equivalent thickness of the remelting layer, and the verified delamination safety margin, and the target semi-finished hole is then prepared. When the profile exceeds the minimum removal envelope and a positive radial finishing allowance is reserved for subsequent S5, the volume to be removed by electrolysis is determined by the material volume difference between the original measured profile of the pre-hole and the target semi-finished hole profile. Then, based on the reference volume electrochemical equivalent under the reference working condition and the volume removal correction coefficient corresponding to the current processing conditions, it is converted into the effective charge required for electrolytic semi-finishing. If the requirements for complete removal of the remelted layer and subsequent finishing allowance cannot be met at the same time, automatic processing is stopped or manual verification is initiated. When the discharge energy per unit removal volume or the proportion of abnormal pulses exceeds the calibration range, extrapolation is prohibited and the process is recalibrated or a safe shutdown procedure is initiated.
[0018] In one embodiment, in S4, a sodium nitrate aqueous solution with a mass fraction of 10% to 15% is used as the working fluid, and a solid rigid tool electrode with an aspect ratio of not less than 8 is used. The solid rigid tool electrode only retains an exposed conductive working section with local axial conductivity. The outer peripheral surface, bottom end surface, and other non-working surfaces, excluding the local conductive working section, are provided with an insulating layer, and the axial length of the local conductive working section is less than the length of a single axial machining segment. Electrolytic pulses reaching the calibrated local depassivation threshold are used within the target machining gap. The tool electrode reciprocates axially at a frequency of 10 to 20 Hz and a stroke of 1 to 3 mm. The machining pulses are position-synchronized and gated according to the axial position. The machining pulses are shut off in the boundary transition zone, and only the fluid exchange movement is maintained.
[0019] In one embodiment, in step S5, after the bottom end of the solid rigid tool electrode has completely passed through the workpiece exit, the hole shaft is divided into multiple axial segments, and the axially locally conductive working segment is sequentially aligned with each axial segment. Based on the semi-finished hole profile, the target hole profile, the machining clearance compensation amount, the equivalent radius of the axially locally conductive working segment, and the corresponding segment volume removal correction coefficient, the volume to be removed, the effective electrical charge for radial hole enlargement, the initial safe radial offset, and the target radial offset are determined. The tool electrode maintains its axial position in any axial segment, and starting from the initial safe radial offset, it approaches the target radial offset step by step according to the preset radial step size and the corresponding allocated effective electrical charge, and performs at least one radial-circumferential closed interpolation at each offset position. Finally, when the target radial offset, the accumulated electrical charge meets the requirements, and the profile enters the preset tolerance zone, the process moves to the next segment.
[0020] In one embodiment, in S6, the target radius of the expansion outlet section on one side is determined by the modified hole radius, the axial position of the outlet section, the half-expansion angle, the profile compensation coefficient, and the angular window function. The angular window function continuously decreases from the center of the angular region to both sides within the preset expansion angle region and is zero outside the preset expansion angle region. First, the initial safety bias of the outlet forming is determined based on the modified hole radius, the equivalent radius of the local conductive working section, and the outlet forming processing gap. Then, the target bias of the outlet forming is determined based on the target radius. The effective charge of each trajectory segment is determined based on the segment volume difference, the reference volume electrochemical equivalent, and the segment volume of the corresponding trajectory segment after removing the correction coefficient. The tool electrode only performs radial-angular interpolation in the outlet section from the initial safety bias to the target bias in stages.
[0021] In one embodiment, when the lower limit of the positive bias voltage is not less than the upper limit of the positive bias voltage minus the sum of the preset lower boundary margin and the preset upper boundary margin, the feed is immediately frozen; if the current upper boundary still allows a non-zero protection bias voltage, the positive bias voltage is adjusted to not exceed the non-zero protection value of the upper boundary; if there is no non-zero allowable value, the positive bias voltage source is immediately cut off; then, at least one of the following is executed: tool electrode retraction, increasing pulse interval, increasing working fluid circulation flow rate, and decreasing working fluid temperature; the current stage safety window is resampled and re-established; processing continues only when the safety window is restored to effectiveness; if it is not restored within a preset number of restorations, the main processing power supply is cut off and the corresponding hole position and abnormal data are recorded.
[0022] In one embodiment, in S7, the detection errors include aperture error, inlet-outlet aperture difference, expansion angle error, outlet profile error, and pressure difference-flow coefficient error. Based on the aperture error and inlet-outlet aperture difference, and combined with the taper correction weight corresponding to the axial position, the radial offset and effective radial expansion charge of the next film gas orifice are corrected. In cases where the inlet is already too large, the taper correction weight of the inlet side segment is reset to zero. The profile compensation coefficient and segmented pure electrolytic trajectory of the next film gas orifice are corrected based on the expansion angle error and outlet profile error. Under the constraints of orifice geometry and outlet profile tolerance, the pressure difference-flow coefficient error is used to assist in correcting the profile compensation coefficient or local trajectory dwell time. The initial positive bias, pulse interval, and working fluid circulation parameters of the next film gas orifice are corrected based on the minimum dynamic positive bias safety margin and the number of dynamic positive bias safety window recovery times of each control cycle of the previous film gas orifice. The correction amounts of each parameter are limited within the calibration upper and lower limits of the workpiece material and working fluid.
[0023] The beneficial effects of this invention are:
[0024] I. Compared with the prior art, the present invention uses S1-S7 to form a continuous and mutually restrictive closed-loop processing link. S1 Establishes dynamic positive bias safety windows for the pre-hole stage of EDM and the sodium nitrate electrolysis stage, respectively, so that the constraints on the formation, maintenance and destruction of the passivation film only participate in the control of the corresponding electrolysis stage; S2 Maintains a positive bias voltage that makes the workpiece have positive polarity relative to the tool electrode during the EDM pulse and its interval, and adopts graded protection of frozen feed, non-zero protection bias voltage or cut-off bias voltage when the safety window fails; S3 Determines the remelting layer margin based on the discharge energy per unit removal volume and the proportion of abnormal pulses, and calculates the required charge by using the reference volume electrochemical equivalent under the reference working condition and the volume removal correction coefficient under the current working condition; S4 Uses a solid rigid tool electrode with an axially reciprocating segmented electrolytic semi-finishing and periodic liquid change to implement axial reciprocating segmented electrolysis; S5 After the tool electrode completely penetrates the workpiece, the locally conductive working section is positioned segment by segment and circumferentially uniform radial hole enlargement is implemented; S6 Then, a one-sided expansion outlet section is formed within the preset expansion angle domain; S7 Converts the hole diameter, inlet-outlet hole diameter difference, outlet profile and flow rate detection results into the restricted correction amount for the next hole. This can simultaneously solve the problems of exogenous impurity cation migration, enrichment and deposition, insufficient safety of fixed positive bias voltage, improper use of passivation protection, remelting layer residue, difficulty in performing axial selective machining of the entire conductive electrode, difficulty in obtaining equal diameter holes through axial machining alone, and insufficient consistency of group holes.
[0025] II. Compared with existing technologies, this invention no longer applies the same positive bias boundary to different processing stages. Instead, it establishes a phased dynamic safety window based on the actual medium and reaction state. In the pre-hole stage of electrical discharge machining, the lower limit is determined by the need to prevent backflow, and the upper limit is limited by the allowable conditions for gas-containing inter-electrode breakdown and anodic reaction in the pre-hole stage. After entering the sodium nitrate electrolysis stage, the bias required for passivation film formation and maintenance is used as a candidate lower limit, and the allowable bias for passivation film damage obtained through calibration with the same material and working fluid is included in the upper limit. The controller updates the safety window for the current stage based on the deionization time constant, calibrated backflow characterization charge, temperature, conductivity, and pressure. This ensures that the positive bias meets the requirements for backflow prevention and stable passivation protection while preventing the entry into the gas-containing channel breakdown, film instability, or excessive anodic reaction range. When the safety window does not have a non-zero allowable value, the positive bias source is directly cut off, avoiding the contradiction between "safety window failure" and "continuing to maintain a safe bias," thereby improving the physical rationality of the dynamic adjustment mechanism and processing safety.
[0026] Third, compared with the prior art, this invention divides the effective discharge energy of a single hole by the actual material removal volume in the pre-hole stage to form the unit removal volume discharge energy, which is used together with the abnormal pulse ratio to estimate the equivalent thickness of the remelted layer. The equivalent thickness of the remelted layer is used to establish the minimum removal envelope, and the actual volume to be removed is determined by the material volume difference between the original measured profile of the pre-hole and the target semi-finished hole profile that meets the minimum removal envelope and retains the subsequent radial finishing allowance, thereby avoiding the omission of the amount of remelted layer body removed. This volume to be removed is then converted into the required charge through the reference volume electrochemical equivalent and volume removal correction coefficient under the reference working condition. The solid rigid tool electrode of S4 retains only the axially locally conductive working section, and the rest of the non-working surface is insulated. Selective semi-finishing of different hole axis positions is achieved by axial movement of the locally conductive working section, position synchronous pulse gating, and accumulated effective charge, and the axial reciprocating motion generates periodic liquid exchange, thereby enabling controlled reduction of the taper of the pre-hole with a large inlet and a small outlet while removing the remelted layer.
[0027] IV. Compared with the prior art, this invention sets up an independent segmented radial hole enlargement step after axial semi-finishing. Only after the bottom end of the solid rigid tool electrode has completely passed through the workpiece outlet is the axially localized conductive working section sequentially aligned with each hole shaft segment and maintaining the corresponding axial position. The center of the tool electrode determines the radial offset based on the target hole radius, the equivalent radius of the localized conductive working section, and the machining clearance compensation amount, and then performs radial-circumferential closed interpolation around the target hole shaft. In this way, the electrolytic effect is limited to the vicinity of the current segment, avoiding the simultaneous change of the machining clearance of multiple hole segments when the entire conductive electrode is eccentric. After the hole finishing is completed, S6 converts the target outlet profile into the radial-angular trajectory of the tool electrode center, and selectively expands only the preset angular region of the outlet. S7 then corrects S5 with the hole diameter and the difference between the inlet and outlet hole diameters, and corrects S6 with the expansion angle, outlet profile error, and flow coefficient error constrained by geometric tolerances, which helps to improve the consistency of the hole size, outlet profile, and pressure-flow characteristics of the group of holes. Attached Figure Description
[0028] Figure 1 This is a flowchart of the overall method of the present invention;
[0029] Figure 2 This is a closed-loop topology diagram of the composite power supply sampling control in this invention;
[0030] Figure 3 This is a timing diagram of the pulsed DC composite electric field in this invention;
[0031] Figure 4 This is a graph showing the change in the dynamic positive bias safety window in this invention.
[0032] Figure 5 This is a diagram showing the positive bias anti-backflow mechanism and ion concentration distribution in this invention;
[0033] Figure 6 This is a diagram showing the effective electrical charge distribution of the piston-type fluid exchanger and the orifice shaft in this invention.
[0034] Figure 7 This is a target profile view of the one-sided expansion outlet section in this invention;
[0035] Figure 8 This is the closed-loop diagram of the current hole final inspection driving the next hole constraint correction in this invention;
[0036] Figure 9 This is a schematic diagram of the positive bias pre-hole principle of the sidewall insulated hollow electrode in this invention;
[0037] Figure 10 This is a schematic diagram of the solid rigid tool electrode piston-type fluid changing and electrolytic semi-finishing principle in this invention;
[0038] Figure 11 This is a schematic diagram of the axial reciprocating segmented electrolytic semi-finishing principle in this invention;
[0039] Figure 12 This is a schematic diagram illustrating the radial enlargement and finishing principle after the tool electrode has penetrated the hole in this invention.
[0040] Figure 13 This is a schematic diagram illustrating the principle of selective pure electrolytic forming of the expansion outlet section on one side in this invention. Detailed Implementation
[0041] Reference Figures 1 to 13 To address the problems existing in the background art, this application proposes a method for machining film gas holes on turbine blades using a pulsed DC composite electric field bias to prevent backflow. This method is used to machine film gas holes with a hole body and an expanded outlet section on one side on turbine blades, and includes the following steps:
[0042] S1, acquire the pore geometry data of the film gas pores, the calibration data of the workpiece material and the working fluid, and the inter-electrode state data; establish a dynamic positive bias safety window according to the processing stage, wherein, in the pre-hole stage of electrical discharge machining, characterize the corrosion removal products formed by the local melting, vaporization, peeling, or dispersion of the workpiece material through electrical discharge machining and entering the working fluid, and based on the migration state of exogenous impurity cations in the working fluid and processing environment that are different from the intrinsic elements of the workpiece matrix and do not belong to the current working fluid design components, and the migration state of the exogenous impurity cations into the already processed fluid. The trend of backflow, enrichment, and deposition on the borehole wall is used to determine the lower limit of the positive bias voltage required to prevent backflow. At the same time, the upper limit of the positive bias voltage is determined based on the gas-containing inter-electrode breakdown constraint and the allowable conditions of the anodic reaction at this stage. In the sodium nitrate electrolysis stage, the larger of the positive bias voltage required to prevent backflow and the positive bias voltage required to form and maintain the passivation film is used as the lower limit of the positive bias voltage, and the minimum of the allowable voltage of gas-containing inter-electrode breakdown, the allowable voltage of passivation film destruction, and the allowable voltage of oxygen evolution or excessive anodic reaction is used as the upper limit of the positive bias voltage. The initial processing control parameters are output under the constraint of the dynamic positive bias voltage safety window of the current processing stage.
[0043] In this embodiment, "corrosion removal products" does not refer only to chemical corrosion products in the usual sense, but rather to the general term used in this application for the special processing of film pore composites. Specifically, it refers to the substances that enter the working fluid after the workpiece material is removed from the workpiece substrate under the action of electric spark discharge, electrothermal action, electrochemical reaction, or their coupling effect. For the pre-hole stage of electric spark discharge, the corrosion removal products mainly originate from the transient high temperature within the discharge channel, causing localized melting, vaporization, thermal stripping, and rapid solidification of the workpiece surface material, thereby forming fine metal particles, melted and re-solidified particles, oxidation or reaction products, and some ionic components. For the subsequent electrolysis stage, the corrosion removal products may also include metal ions, hydroxides, or other reaction products formed by the anodic dissolution of the workpiece. Therefore, this application uses "corrosion removal products" to uniformly describe the workpiece material removal products directly caused by the processing behavior, to distinguish them from exogenous impurity components introduced by the processing environment, working fluid impurities, or external system anomalies.
[0044] It should be further clarified that corrosion removal products are not the same concept as the exogenous impurity cations that this application focuses on suppressing. Corrosion removal products originate directly from the workpiece itself. For example, intrinsic elements such as nickel, chromium, cobalt, and iron in nickel-based superalloys enter the working fluid during processing and are considered removal products of the workpiece material itself. Even if these intrinsic elements exist in particulate, ionic, or other dispersed states, they are not directly defined as contaminants introduced from the outside. Exogenous impurity cations, on the other hand, refer to cations that enter the processing system from processing water, working fluid raw materials, circulation pipelines, storage devices, fixtures, environmental media, or other external sources, and are distinct from the intrinsic composition of the workpiece material and the normal design composition of the current working fluid.
[0045] When using deionized water or low-conductivity working fluid in the pre-hole stage of EDM, if sodium, potassium, calcium, or other impurity cations not inherent to the workpiece matrix are present in the working fluid or circulation system, these ions may migrate towards the machined hole wall during the pulse interval due to the combined effects of concentration gradient, working fluid flow, and inter-electrode electric field, forming local enrichment, adsorption, or residue near the hole wall. For film pores in nickel-based superalloys, such external impurity residues may affect the cleanliness of the hole wall and subsequent service reliability. Therefore, this application utilizes a positive bias voltage that maintains the positive polarity of the workpiece relative to the tool electrode to establish a directional electric field near the hole wall that repels positive ions, thereby weakening the tendency of external impurity cations to migrate back towards the hole wall.
[0046] In this invention, positive bias refers to a non-zero DC bias voltage applied between the workpiece and the tool electrode, which keeps the workpiece relatively positive relative to the tool electrode; the polarity of the positive bias voltage remains unchanged during both the on-time and off-time of the electrical discharge pulse. This positive bias voltage differs from the negative bias voltage that keeps the workpiece relatively negative relative to the tool electrode, and from the zero bias voltage when no DC bias voltage is applied.
[0047] In S1, the dynamic positive bias safety window is established according to the current processing stage: the lower limit of the positive bias in the pre-hole stage is determined based on the anti-backflow requirement corresponding to the tendency of exogenous impurity cations to migrate back, enrich, and deposit to the processed hole wall, and the upper limit of the positive bias is determined by the allowable conditions for gas-containing inter-electrode breakdown and the allowable conditions for anodic reaction in the pre-hole stage; the lower limit of the positive bias in the sodium nitrate electrolysis stage is the larger value between the positive bias required for anti-backflow and the positive bias required for the formation and maintenance of the passivation film, and the upper limit of the positive bias is the minimum value among the allowable voltage for gas-containing inter-electrode breakdown, the allowable voltage for passivation film destruction, and the allowable voltage for oxygen evolution or excessive anodic reaction; when the difference between the upper limit and the lower limit of the positive bias in the current stage is greater than the sum of the preset lower boundary margin and the preset upper boundary margin, the dynamic positive bias safety window in the current stage is determined to be effective.
[0048] Further implementation details for S1 are as follows:
[0049] The hole geometry data is obtained from the blade 3D model, the clamping datum measured by the coordinate measuring machine, and the blade profile measured by the in-machine probe, and is uniformly transformed into a local coordinate system with the gas film hole axis as the z-axis and the outlet expansion center direction as the angular zero position. Workpiece material-working fluid calibration data are established for the deionized water or low-conductivity working fluid used in the EDM pre-hole stage and the sodium nitrate aqueous solution used in the electrolysis stage. The calibration data includes at least the generation and discharge characteristics of corrosion removal products, the type, valence, diffusion coefficient, effective concentration range, concentration gradient, and residual risk range of exogenous impurity cations included in the anti-backflow control, as well as the reference volume electrochemical equivalent, volume removal correction relationship, passivation film formation and maintenance potential range, allowable bias voltage for passivation film damage, oxygen evolution or excessive anodic reaction initiation potential, allowable bias voltage for anodic reaction in the pre-hole stage, and gas-containing inter-electrode breakdown parameters. Online inter-electrode status data is obtained by a voltage / current sampling unit, a servo position encoder, a temperature sensor, a conductivity sensor, and an inlet / outlet pressure sensor. Each data point is written into the same process record using the orifice number, processing stage, control cycle number, sampling time, and orifice shaft position as an index, so that each stage can call the calibration data corresponding to the current working fluid and processing stage.
[0050] Online estimation and calibration mapping: For the concentration of exogenous impurity cations and their normal concentration gradient in the near-zone of the orifice wall, which are difficult to measure directly cycle by cycle, a calibration mapping is established in advance using test holes with the same material, working fluid, and corresponding impurity ion conditions. This mapping includes "working fluid conductivity, cumulative effective processing charge, circulation flow rate, orifice axis position, and processing stage—exogenous impurity cation concentration and concentration gradient." The controller obtains estimated values in each control cycle based on online conductivity, cumulative charge, circulation flow rate, and position index. The local liquid velocity component towards the orifice wall is obtained by the calibration flow field mapping of the inlet-outlet pressure difference, circulation flow rate, and corresponding orifice depth. The equivalent pressure and equivalent channel length of the bubble do not require direct online measurement but are obtained from calibration lookup values corresponding to pressure, temperature, conductivity, interelectrode gap, and discharge waveform characteristics. If the current state exceeds the effective range of the calibration mapping, the analytical extrapolation is stopped, and the process enters recalibration or a safe recovery procedure.
[0051] Calculation of the lower limit of positive bias voltage: For various exogenous impurity cations that may migrate back, accumulate, and deposit on the walls of the processed holes during the current processing stage, the required electric field strength for preventing backflow is calculated, and the most unfavorable value is taken as the required anti-backflow electric field strength for the current control cycle. These exogenous impurity cations are distinct from the intrinsic elements of the workpiece matrix and are not part of the normal design components of the current working fluid. For exogenous impurity cations below the reliable detection range, to avoid the denominator approaching zero in the initial processing stage or at low concentrations, the lowest effective concentration or detection limit obtained from calibration is used to constrain the calculated concentration. For the electrolysis stage using sodium nitrate aqueous solution, the positive bias voltage required for passivation film formation and maintenance is also determined based on the polarization curve of the same material and working fluid. The controller takes the larger of the anti-backflow requirement and the passivation film formation and maintenance requirement as the lower limit of the positive bias voltage for the electrolysis stage. In the EDM pre-hole stage, the positive bias voltage term required for passivation film formation and maintenance is zero. The required anti-backflow field strength is calculated according to the following formula:
[0052] ;
[0053] ;
[0054] ;
[0055] In the formula, For the first The control cycle is used to calculate the first... Effective molar concentration of exogenous impurity cations included in anti-backflow control, in mol / m³; The estimated or measured molar concentration of the exogenous impurity cation in the near-pore wall region, in mol / m³; The lowest effective concentration or detection limit obtained under the same material-working solution and corresponding exogenous impurity cation conditions, in mol / m³; when Below At that time, concentration-related items were uniformly adopted. To avoid using different concentration calibers for the numerator and denominator. For the first The electric field strength required to prevent backflow for each type of exogenous impurity cation. The electric field strength required for the current control cycle to prevent backflow is the result of taking the most unfavorable value for all types of exogenous impurity cations currently under control. The unit is V / m. is the molar gas constant, in J / (mol·K); The absolute temperature of the working fluid is expressed in Kelvin (K). For the first The valence of the exogenous impurity cation; C is the Faraday constant, expressed in C / mol. The diffusion coefficient is expressed in m² / s. The coordinates are the normal coordinates pointing from the borehole wall to the working fluid inside the borehole; This represents the magnitude of the concentration gradient along the normal direction, in mol / m³. 4 ; The component of the liquid velocity toward the orifice wall is expressed in m / s. The field strength margin is used to cover model errors, expressed in V / m. In the formula... Indicates taking only The non-negative part.
[0056] ;
[0057] In the formula, For the first The lower limit of the positive bias voltage for each control cycle, in V; The equivalent inter-electrode gap between the tool electrode and the hole wall, in meters; The meaning and units are the same as before; This is the total compensation for electrode polarization voltage, contact voltage drop, and lead voltage drop, expressed in V. For the first Each control cycle is calculated from the polarization curve of the same material—sodium nitrate—and the positive bias voltage required for the formation and maintenance of the passivation film, in units of V, which is zero during the pre-hole stage of electrical discharge machining.
[0058] Calculation of the upper limit of positive bias voltage: The bubble pressure and equivalent channel length between the gas electrodes are corrected using discharge calibration data from this machine tool, this working fluid, and the actual pressure range. The bubble equivalent channel breakdown voltage is estimated using the calibrated Paschen / Townsend type equivalent relationship. This relationship is only obtained from the calibration of this machine tool and working fluid. Use this method when the formula is within the valid range and the denominator is positive. When the range is exceeded, use the experimentally calibrated breakdown boundary interpolation instead of theoretical extrapolation. After obtaining the allowable breakdown value, select the corresponding upper boundary constraint according to the current processing stage.
[0059] ;
[0060] In the formula, For the first Bubble equivalent channel breakdown voltage per control cycle, in V; The first Tangen ionization correlation coefficient is given in units of 1 / (Pa·m). The second Thomson ionization correlation coefficient is given in V / (Pa·m). The equivalent pressure inside the bubble is expressed in Pa. The equivalent channel length of the bubble is expressed in meters (m). The equivalent secondary electron emission coefficient is dimensionless. , and Calibration is performed by discharge tests under the conditions of this machine tool and its working fluid.
[0061] ;
[0062] ;
[0063] In the formula, For the pre-hole stage of electrical discharge machining The upper limit of the positive bias voltage for each control cycle The first stage of sodium nitrate electrolysis The upper limit of the positive bias voltage for each control cycle, in V; A breakdown safety factor of less than 1; This is the breakdown voltage of the bubble's equivalent channel. The allowable bias voltage for the anodic reaction in the pre-hole stage is obtained by calibration using the same material—pre-hole working fluid and corresponding pulse conditions. Its calibration upper limit is the value that is reached first under the limiting conditions such as continuous electrolytic leakage current, obvious gas evolution, unacceptable surface oxidation or abnormal discharge. The allowable bias voltage for passivation film destruction is obtained by directly calibrating the same material—sodium nitrate working solution—through anodic polarization curves and repeated pulse tests. This sets the allowable voltage for oxygen evolution or excessive anodic reaction. The controller selects the appropriate upper limit according to the processing stage, thereby avoiding the introduction of passivation film destruction constraints during the pre-pore stage before a passivation film is established.
[0064] It should be noted that the controller can be implemented using a PLC, DSP, or industrial motion control card, and its control logic is programmed and implemented by the steps described in S1 to S7.
[0065] Judgment, output, and subsequent uses: In the current processing stage, when - Greater than the preset lower boundary margin With preset upper boundary margin When the sum is equal to the sum, the dynamic positive bias safety window is deemed valid, and the allowable positive bias range for the k-th control cycle is expressed by the following formula:
[0066] ;
[0067] S1 outputs the current stage dynamic positive bias safety window, initial positive bias, pulse peak / width / interval, initial feed rate, and flushing pressure. This control package serves as the direct input for the first control cycle of S2. When entering the subsequent electrolysis stage, the dynamic positive bias safety window for the electrolysis stage is re-established based on the calibration data corresponding to the sodium nitrate working solution.
[0068] In the formula, For the first The dynamic positive bias safety window allowed per control cycle; and These represent the lower and upper limits of the current positive bias, respectively. and These are the lower boundary safety margin and the upper boundary safety margin, respectively, both in units of V. Only when... hour, The effective interval is non-empty; the first control period. for A special case at that time.
[0069] Upon entering the sodium nitrate electrolysis stage, the passivation film formation and maintenance bias, the allowable bias for passivation film destruction, the oxygen evolution or excessive anode reaction threshold, the volumetric electrochemical equivalent, and the volumetric removal correction relationship corresponding to the working solution are recalculated to establish a new dynamic positive bias safety window for the electrolysis stage. If the safety window is invalid, the electrode feed is not allowed to continue, and the calculation is repeated by lowering the working solution temperature, increasing the circulation flow rate, or increasing the inter-electrode gap; if there is no non-zero allowable bias, the positive bias source is kept off until the safety window is restored.
[0070] S2, perform pre-hole drilling using electrical discharge machining (EDM). A positive bias voltage is superimposed on the EDM pulse, maintaining the positive polarity of the workpiece relative to the tool electrode and preventing it from returning to zero during the pulse interval. The inter-electrode electrical signal and working fluid status are acquired according to the control cycle. Based on the acquisition results, the lower and upper limits of the positive bias voltage for the current stage are updated, limiting the positive bias voltage within the updated dynamic positive bias voltage safety window. When the dynamic positive bias voltage safety window fails, the feed is immediately paused. If the current upper boundary still allows a non-zero protection bias voltage, the positive bias voltage is limited to a non-zero protection value within the upper boundary. If no non-zero allowable value exists, the positive bias voltage source is cut off. At least one of the inter-electrode gap, pulse interval, and working fluid circulation status is adjusted until the dynamic positive bias voltage safety window is restored. The pre-hole discharge history, pre-hole geometry data, and anomaly records are output.
[0071] In S2, the interelectrode current during the pulse interval is attenuated and fitted to obtain the deionization time constant, and the current component higher than the steady-state leakage current is integrated to obtain the backflow characterization charge. The backflow characterization charge is not used as a direct measurement of the actual migration charge of exogenous impurity cations, but is established through calibration tests under the same material, working fluid, and corresponding pulse parameters to establish its correspondence with the risk of exogenous impurity cations migrating back to the processed hole wall, enriching, and depositing. The calibration test gives the allowable limit value. When the dynamic positive bias safety window is effective, the positive bias of the next control cycle is updated in a limited manner according to the difference between the required anti-backflow field strength and the measured positive bias field strength, as well as the deviation of the backflow characterization charge relative to the allowable limit value, and the maximum allowable positive bias change in a single control cycle is limited. When the safety window fails, the abnormal recovery process is initiated.
[0072] In S2, a hollow copper tool electrode with sidewall insulation and only bottom surface conductivity is used for EDM pre-holeing. The initial positive bias voltage calibration range during the EDM pre-holeing stage is 3-8V. When at least two of the following conditions are met: inter-electrode voltage drop, peak current exceeding the limit, breakdown delay shortening, and pulse interval current decay slowing down, the corresponding control cycle is marked as an abnormal pulse cycle, and the hole shaft position and discharge data of the abnormal pulse cycle are written into the abnormal record.
[0073] When the lower limit of the positive bias voltage is not less than the upper limit of the positive bias voltage minus the sum of the preset lower boundary margin and the preset upper boundary margin, the feed is immediately frozen; if the current upper boundary still allows a non-zero protection bias voltage, the positive bias voltage is adjusted to not exceed the non-zero protection value of the upper boundary; if there is no non-zero allowable value, the positive bias voltage source is immediately cut off; then, at least one of the following is executed: tool electrode retraction, increasing pulse interval, increasing working fluid circulation flow rate, and decreasing working fluid temperature, to resample and re-establish the current stage safety window, and processing continues only when the safety window is restored to effectiveness; if it is not restored within the preset number of restorations, the main processing power is cut off and the corresponding hole position and abnormal data are recorded.
[0074] Further implementation details for S2 are as follows:
[0075] Equipment Operation and Sampling: The EDM pre-hole uses a hollow tool electrode made of copper or brass, with a 20-40 μm insulating layer formed on its sidewalls, exposing only the bottom surface for conductivity. After coaxial alignment, the electrode is rotated and fed, and deionized water or a low-conductivity working fluid is flushed in through the inner hole. During the EDM pulse conduction period, a positive bias voltage is superimposed by a power combining unit, and the non-zero output of the positive bias voltage source is retained during the pulse interval. The sampling frequency should be sufficient to distinguish the pulse rise edge, breakdown delay, peak current, and the interval decay process. In this embodiment, 100 consecutive pulses constitute a control cycle, and each sampling record is simultaneously associated with the electrode axial position, gap, temperature, conductivity, and inlet / outlet pressure. The number of pulses in the control cycle can be adjusted according to the power supply repetition frequency, but it should ensure that the interval decay can be stably fitted within one cycle and that the control delay is less than the time of significant changes in the state inside the hole.
[0076] Deionization state extraction: For the current during the interval after each effective pulse turn-off, first remove the sampling zero drift and steady-state leakage current, then fit it using the following formula:
[0077] ;
[0078] In the formula, The interval current is measured in amperes (A) from the moment the pulse is turned off. The amplitude of the decaying current at the moment of turn-off, in amperes (A). The time elapsed since the switch was turned off, in seconds (s). The deionization time constant is expressed in seconds (s). This is the steady-state leakage current, in amperes (A). An increase indicates that the dissipation of the inter-electrode conductive channel is slower, which results in a longer pulse interval in the next control cycle or triggers fluid recovery.
[0079] ;
[0080] In the formula, For the first The average backflow charge of each effective pulse within a control cycle is represented by C; The number of valid pulses included in the statistics; The valid pulse number; For the first The interval duration of each effective pulse, in seconds; This is the current during the pulse interval, in amperes (A). The value corresponds to the steady-state leakage current, in A; the maximum value calculation in the formula only retains the non-negative part of the difference. This is a calibrated characteristic quantity for backflow risk control, and its allowable limit is uniformly denoted as... The value is determined by calibration tests using the same materials, working fluid, and corresponding pulse conditions.
[0081] Positive bias update: When the dynamic positive bias safety window is active, the controller recalculates using formula S1 based on the latest gap, temperature, pressure, and ion concentration. , and And generate the positive bias command for the next control cycle according to the following formula:
[0082] ;
[0083] In the formula, and These are the positive bias voltages for the current and next control cycles, respectively, in V; Indicates will Restricted to closed intervals Inside; To prevent errors in the backflow field strength, the gain is corrected; This is the equivalent interelectrode gap; To achieve the required backflow prevention field strength; To measure the positive bias voltage field strength; To correct the gain for the refluxing charge; and These represent the current recirculation characteristic electricity and the allowable limit, respectively; This is the equivalent capacitance used to convert the charge deviation into a voltage correction. The formula output also accepts the maximum positive bias voltage change in a single control cycle. limit, The unit is V, representing the value within a single control cycle. The maximum allowable amplitude. This update will not be executed if the dynamic positive bias safety window fails; instead, the abnormal recovery process will be initiated.
[0084] Anomaly handling, output, and subsequent applications: When inter-electrode voltage sag, peak current exceeds limits, breakdown delay shortens, and When at least two of the increasing parameters reach the calibrated threshold, the cycle is recorded as an abnormal pulse cycle and written to the hole axis position. When the safety window is active, priority is given to reducing feed, increasing pulse interval, and increasing flushing fluid; when the safety window fails, feed is immediately frozen. If the current upper boundary still allows a non-zero protection bias, the positive bias source is adjusted to not exceed the non-zero protection value of the upper boundary; if no non-zero allowable value exists, the positive bias source is immediately cut off. Subsequently, the tool electrode is retracted 20–50 μm, the pulse interval is increased by 10%–20%, the circulation flow rate is increased by 10%–20%, and at least two sampling cycles are waited before recalculating the safety window. If no effective safety window is found within three recovery attempts, the positive bias source remains off and the main machining power supply is cut off. Pre-hole penetration is cross-confirmed by servo displacement, sudden changes in outlet pressure, and changes in inter-electrode waveform. S2 outputs pulse-by-pulse waveform, effective discharge energy sequence, abnormal pulse ratio, minimum safety margin, pre-hole inlet / outlet profile, and penetration position; among which, discharge history, abnormal ratio, and pre-hole geometry serve as inputs for S3 remelting layer estimation and removal volume calculation, and minimum safety margin serves as constraints for S4 initial positive bias and flushing parameters.
[0085] It should also be noted that the remelted layer is formed when the material is melted and resolidified after electrical discharge machining.
[0086] S3, based on the pre-hole discharge history, pre-hole geometry data, and anomaly records output by S2, and combined with calibration data, determines the unit removal volume discharge energy and remelting layer removal allowance of the pre-hole wall during the pre-hole stage; divides the hole axis into multiple axial machining segments, establishes a minimum removal envelope based on the equivalent thickness of the remelting layer and the verified safety margin, and determines the target semi-finished hole profile under the condition that the target semi-finished hole profile is outside the minimum removal envelope and retains a positive radial finishing allowance relative to the target final hole body; the volume to be electrolyzed is determined by the actual material volume difference between the original measured profile of the pre-hole and the target semi-finished hole profile, and then based on the reference volume electrochemical equivalent calibrated under the same material and working fluid reference conditions. Volume removal correction factor corresponding to the current processing conditions The volume to be removed by electrolysis is converted into the effective amount of electricity required for semi-finished electrolysis.
[0087] In S3, the instantaneous effective power of the inter-electrode voltage and inter-electrode current of each effective pulse in the pre-hole stage is integrated over time to obtain the single-hole effective discharge energy. The sampling polarity is uniformly agreed upon with the effective discharge power being positive. In the calculation, the absolute value of the product of instantaneous voltage and current is taken to avoid energy sign reversal caused by different sampling polarities. The single-hole effective discharge energy is divided by the actual material removal volume in the pre-hole stage to obtain the discharge energy per unit removal volume. This energy, along with the abnormal pulse ratio, is input into the remelting layer calibration relationship established with the same material, working fluid, and corresponding pulse energy range to obtain the equivalent thickness of the remelting layer. The equivalent thickness of the remelting layer is not directly deducted from the volume to be removed, but is used to determine the minimum removal envelope that the target semi-finished hole contour must cross.
[0088] Further implementation details for S3 are as follows:
[0089] Data preparation and spatial mapping: The effective pulse waveforms output by S2 are mapped to the hole shaft segments according to the encoder position along the electrode axis, and short-circuit, arcing, and sampling saturation pulses are removed; the pre-hole measured profile can be obtained through in-machine low-voltage impedance scanning, film replication measurement, or offline three-dimensional measurement, and the actual material removal volume during the pre-hole stage is determined. The result is obtained from the difference in geometric volume before and after pre-holeing. The remelted layer calibration relationship established with the same material grade, pulse energy range, and working fluid as the blade is used, along with the reference volume electrochemical equivalent obtained under the same material—sodium nitrate working fluid—reference calibration conditions. The remelted layer calibration relationship is tied to the material grade, working fluid, pulse energy range, and temperature range; different combinations use independent calibration groups. The delamination safety margin is determined based on the upper confidence boundary of the fitted residual or a verified safety margin. The minimum envelope removal is denoted as Target semi-finished hole radius Must meet > It should also be smaller than the final target hole radius. A radial finishing allowance greater than zero (S5) is retained. If both requirements cannot be met simultaneously, the pre-hole condition is judged to be out of tolerance and automatic processing is stopped or manual verification is initiated.
[0090] ;
[0091] ;
[0092] In the formula, The effective discharge energy of a single aperture is expressed in J. The total number of effective pulses, dimensionless; The valid pulse number; For the first The conduction start time of each effective pulse, in seconds; For the first The conduction duration of each effective pulse, in seconds; Inter-electrode voltage, in volts (V). Inter-electrode current, in amperes (A); The variable is time, in seconds (s). This represents the actual material removal volume during the pre-hole stage, in m³. Energy removed per unit volume of discharge, in J / m³; Equivalent remelted layer thickness, in meters (m); This represents the proportion of abnormal pulses to the total number of pulses, and is dimensionless; if axial segmented calibration is used, then... , , and All are calculated using the same segment. Only when... , The remelting layer calibration relationship is only applicable when the working fluid state is within the corresponding calibration sample range; thus, the obtained... It must not be less than zero; if any input exceeds the calibration range, extrapolation is prohibited, and recalibration should be initiated, a verified safety margin should be adopted, or the automatic closed-loop process should be suspended.
[0093] Envelope Removal, Volume Removal, and Effective Charge: Minimum envelope removal is determined by the original measured radius of the pre-hole. Equivalent remelted layer thickness and verified delamination safety margin The feasibility criteria were jointly determined. After meeting these criteria, the total material volume difference between the original measured profile of the pre-hole and the finally determined target semi-finished hole profile was used as the volume to be removed. Instead of only calculating the volume between the outer boundary of the remelted layer and the target semi-finished hole profile, this ensures that the remelted layer body is also included in the removal volume. Abnormal pulse concentration areas can be addressed by increasing... Increase the minimum removal envelope, but the target semi-finished hole profile must not exceed the tolerance on the target hole diameter, and a positive radial finishing allowance must be reserved for S5. The volume to be removed is converted into the effective charge required for electrolytic semi-finishing based on the reference volume electrochemical equivalent and the volume removal correction factor, and the actual effective charge is accumulated in S4:
[0094] ;
[0095] ;
[0096] ;
[0097] ;
[0098] In the formula, The estimated effective charge required for semi-finished electrolysis, in C; The volume of material to be removed from the original measured profile of the pre-hole to the target semi-finished hole profile, in m³. The reference volume electrochemical equivalent under the same material and working fluid reference calibration conditions represents the material removal volume corresponding to a unit reference charge under the reference conditions, in m³ / C. The volume of the current processing conditions relative to the reference calibration conditions is adjusted by a correction factor and is dimensionless; therefore, the actual effective volume equivalent is... ; Deadline Cumulative effective processed charge after deducting stray reactions or baseline current, in C; For integration time; This represents the total processing current. This refers to stray reactions or baseline current. Indicates taking only The non-negative part. It is only used for converting demanded electricity and will not be counted repeatedly on the cumulative effective electricity side.
[0099] Outputs and subsequent uses: S3 outputs the minimum removal envelope, target semi-finished hole profile, total volume to be removed, total power required, allowance / power distribution along the hole axis, and permissible axial reciprocating envelope, serving as the main control input for S4 axial reciprocating segmented electrolytic semi-finishing; the segmented allowance is used for the local conductive working segment dwell distribution in S4, and the motion envelope allows the solid rigid tool electrode to pass through the workpiece exit in S4 so that it can directly enter S5 radial reaming after confirming complete penetration.
[0100] S4, drain the pre-hole working fluid and replace it with sodium nitrate aqueous solution, and replace it with a solid rigid tool electrode with only the axially locally conductive working section exposed and conductive, and the rest of the non-working surfaces insulated; based on the segmented effective charge output in S3, perform axial reciprocating segmented electrolytic semi-finishing under the constraint of the dynamic positive bias safety window in the updated electrolysis stage, so that the axial locally conductive working section acts on different axial processing sections in sequence, and the working fluid in the hole is periodically replaced with the axial reciprocating motion of the tool electrode. The passivation film formed and maintained by the sodium nitrate system is used to suppress stray corrosion in non-target areas, and the cumulative effective charge is used to control the remelting layer removal and pre-hole taper reduction process, outputting the semi-finished hole profile and segmented volume removal correction coefficient;
[0101] In S4, a sodium nitrate aqueous solution with a mass fraction of 10%–15% is used as the working fluid, and a solid rigid tool electrode with an aspect ratio of not less than 8 is employed. The solid rigid tool electrode retains only an exposed conductive section along its axial direction. Insulating layers are provided on the outer circumferential surface, bottom surface, and other non-working surfaces, excluding the conductive section. The axial width of the conductive section is less than the length of the corresponding single axial machining segment. Under the influence of an electric field, the sodium nitrate aqueous solution induces the formation of a passivation film on the anode surface of the workpiece, while the non-machined areas remain passivated to suppress stray dissolution. Electrolytic pulses with a peak current density reaching the local depassivation threshold calibrated for the same material—sodium nitrate system—are applied within the target machining gap corresponding to the conductive section. The tool electrode reciprocates axially at a frequency of 10–20 Hz and a stroke of 1–3 mm, and the machining pulses are position-synchronized and gated according to the position of the axial encoder.
[0102] Further implementation details for S4 are as follows:
[0103] Equipment, Media, and Initial Conditions: While maintaining the same clamping reference for the blades, drain the deionized water or low-conductivity working fluid from the pre-hole stage. After bypass cleaning, pump in a 10%–15% sodium nitrate aqueous solution. The working fluid temperature should be controlled at 30–40℃ and filtered. Replace with a solid rigid tool electrode made of tungsten, tungsten-based high-density alloy, or cemented carbide, with an electrode length-to-diameter ratio of not less than 8. Only retain one locally conductive working section continuously conductive with the electrode substrate along the axial direction. Insulation layers should be applied to the outer circumference, bottom end, and other non-working surfaces, excluding this working section. The non-working section can be pre-reduced in diameter before being covered with an insulation layer, ensuring that the outer contour of the completed insulation layer is not higher than the outer diameter of the locally conductive working section to avoid mechanical interference during radial interpolation. The maximum outer diameter of the locally conductive working section and the maximum outer diameter of the completed insulation section should both be smaller than the minimum measured diameter of the pre-hole, with reserved assembly and initial electrolysis gaps. If these dimensional adaptation conditions are not met, the tool is prohibited from entering S4–S6. Axial width of the locally conductive working section. The equivalent radius is denoted as less than the length of a single axial machining segment. Within the target processing gap, a pulsed electrolysis method is used to achieve the calibrated local depassivation threshold, and the pulse interval meets the requirements for local repassivation and product discharge.
[0104] Piston-type fluid change and segmented semi-finishing: A solid rigid tool electrode reciprocates axially within the hole at a frequency of 10–20 Hz and a stroke of 1–3 mm. The downward stroke pushes the electrolytic products within the hole toward the outlet, while the upward stroke replenishes fresh electrolyte using the inlet pressure difference. The periodic pressure difference generated by the pressure sensors at both ends maintains a stable phase correspondence with the encoder. The controller determines the positional relationship between the locally conductive working section and the target segment based on the axial encoder position. Electrolysis pulses are activated and the charge is accumulated to that segment only when the locally conductive working section is completely within the allowable processing range of the target segment. When the locally conductive working section crosses the transition zone of the adjacent segment boundary, the processing pulses are deactivated, maintaining only mechanical reciprocation and fluid change. For segments with a large remelting layer allowance on the inlet side, the effective processing dwell time is increased; for segments on the outlet side that are close to the semi-finished hole target, the dwell time is reduced. The initial segmented volume removal correction factor adopts the reference calibration value of the same material and working fluid. When the cumulative effective charge of any segment reaches the required value for that segment, the processing pulse is paused, allowing the tool electrode to return to the center or leave the detection area. The semi-finished hole profile of that segment is obtained by in-machine low-voltage impedance scanning or in-machine aperture detection, and the corresponding segmented volume removal correction factor is corrected based on the measured removal volume. For segments that have not entered the semi-finishing tolerance zone, the remaining charge is updated based on the remaining contour error before processing continues.
[0105] End Criteria, Output, and Subsequent Use: S4 ends only when the cumulative effective electrical charge of each axial machining segment reaches the corresponding requirement, the in-machine contour verification is completed, the semi-finished hole contour enters the preset semi-finished tolerance zone, and the bottom end of the tool electrode has passed through the workpiece exit. S4 allows the retention of controlled residual taper for radial hole enlargement elimination in S5, without forcibly machining the inlet and outlet to the final size simultaneously through continued axial reciprocating motion. S4 outputs the measured radius of the semi-finished hole. Segmented volume removal correction factor The remaining margin and penetration confirmation signal; the above data are used together in S5 to calculate the initial safe radial offset, target radial offset, effective electrical charge of radial hole enlargement, and axial segment position.
[0106] S5: After the bottom end of the solid rigid tool electrode has completely passed through the workpiece exit, based on the semi-finished hole profile, target hole profile, and segment volume removal correction coefficient output in S4, set the initial safe radial offset, target radial offset, and effective radial enlargement charge for each axial segment; align the locally conductive working segments of the axial direction with the corresponding axial segments in sequence; while maintaining the axial position, make the center of the tool electrode approach the target radial offset step by step from the initial safe radial offset according to the preset radial step size and the allocated effective charge, and perform radial-circumferential closed interpolation around the target hole axis at each offset position to maintain effective machining clearance; after reaching the target radial offset and meeting the corresponding charge and profile tolerance, output the corrected hole profile after eliminating residual taper and the charge completion of each axial segment;
[0107] In S5, after the bottom end of the solid rigid tool electrode completely passes through the workpiece exit, the hole shaft is divided into multiple axial segments. The volume to be removed in each segment is determined based on the local volume difference between the semi-finished hole profile and the target hole profile. The effective charge for radial hole enlargement is determined based on the reference volume electrochemical equivalent and the corresponding segment volume removal correction coefficient. The initial safe radial offset is determined based on the semi-finished hole radius, the equivalent radius of the locally conductive working section, and the machining clearance compensation. The target radial offset is determined based on the target hole radius. During machining, the axial locally conductive working section is sequentially aligned with the corresponding axial segment. The axial position is maintained in any segment. The offset is increased step by step starting from the initial safe radial offset. Each offset layer executes a circumferential closed trajectory. Only when the current offset layer reaches the corresponding allocated charge and the internal profile or clearance state meets the conditions for entering the next offset layer will the machining continue to advance towards the target radial offset.
[0108] Further implementation details for S5 are as follows:
[0109] Segmentation and Data Alignment: The hole shaft length L is divided into J axial segments. The length of each segment is determined based on the axial resolution of the contour measurement, the servo positioning accuracy, and the axial width of the locally conductive working section. Determine and make Smaller than the length of a single segment to form a boundary transition zone; semi-finished aperture radius output by S4 Segmented volume removal correction factor With the radius of the target circular hole S1 Interpolation alignment is performed at the same z-coordinate. The penetration confirmation signal is cross-confirmed by at least two of the following: tool electrode axial coded position, outlet pressure abrupt change, inter-electrode waveform change, and outlet flow state change; if low-voltage contact detection is used, it is performed by a separate outlet-side detection probe, not using the insulated bottom end of the tool electrode as the detection electrode. The equivalent radius of the locally conductive working section is denoted as... The controller establishes a data record for each segment, including "segment number - target radius - semi-finished hole radius - equivalent radius of locally conductive working section - machining gap compensation - initial safety offset - target offset - required power - cumulative power - circumferential completion".
[0110] ;
[0111] ;
[0112] ;
[0113] ;
[0114] In the formula, For the first The volume to be removed from radially expanded holes in axial segments, in m³; the formula is as follows: Avoid negative removal volume; For the target hole radius, The semi-finished orifice radius measured by S4. For the first Each segment length; For the first The effective electrical charge required for radial hole enlargement in each segment, in C; For the first The segmented volume relative to the reference calibration condition has a correction factor removed and is dimensionless. The reference volumetric electrochemical equivalent under the calibration conditions; For the first Segmented initial safety radial offset For the first Segmented target radial offset; The equivalent radius of the axially localized conductive working segment; This is the machining clearance compensation amount calibrated based on inter-electrode voltage, conductivity, size of the locally conductive working section, and working fluid condition. Only when... Greater than zero and Greater than The radial expansion of this segment is only performed at that time.
[0115] Motion and Local Termination: The tool electrode is first positioned along the hole axis, aligning the locally conductive axial working section with the j-th axial segment and maintaining the axial position of that segment; the CNC system then moves the electrode center to the initial safe radial offset. Then, according to the preset radial step size Or the effective power demand of this segment. The allocated bias layer sequence is progressively biased towards the target radially. Increase. Each level of bias position executes a 360° closed circular trajectory or an equivalent closed trajectory composed of multiple arc segments around the target hole axis to avoid the outer circle of the tool electrode crossing into material that has not yet been removed in one go. The current bias layer will only continue to increase the bias when the corresponding effective charge is sufficient and the internal contour or effective gap meets the conditions for entering the next bias layer; ultimately reaching... Then, based on the cumulative total The segment ends when the required circumferential profile is met and enters the preset tolerance zone. Verification is performed using in-machine low-voltage impedance scanning or an in-machine aperture detection probe. Offline or external profile measurements are only used for final verification after all segments are completed.
[0116] Verification, output, and subsequent uses: When all segments reach the corresponding target radial offset. The cumulative effective electricity consumption has reached the corresponding level. After completing the segmented profile verification, remeasure the inlet orifice diameter, outlet orifice diameter, orifice profile, and roundness; if the inlet-outlet orifice diameter difference is still out of tolerance, only update the target radial offset of the out-of-tolerance segment. and the remainder The entire hole is not delayed uniformly. The delay continues until the inlet diameter, outlet diameter, and axial segmented diameters enter the target tolerance zone, resulting in a corrected hole profile with near-zero taper. S5 output Radial offset of each segment target, power completion rate, and exit positioning reference; This serves as a benchmark for the target radius of the expanded exit section on one side of S6.
[0117] S6, based on the corrected hole contour and charge completion, segmented volume removal correction coefficient, and target surface of the one-sided expansion exit section output by S5, generates segmented pure electrolytic trajectories that only act on the preset expansion angle domain, and assigns effective charge to each trajectory segment; determines the initial safety offset of exit forming based on the corrected hole radius, the equivalent radius of the local conductive working section, and the exit forming processing gap, and determines the target offset of exit forming based on the target surface radius, so that the local conductive working section is positioned at the exit section and the radial-angular trajectory is executed in stages from the initial safety offset to the target offset, forming the one-sided expansion exit section while maintaining the effective processing gap;
[0118] In S6, the target radius of the expansion exit section on one side is jointly determined by the corrected bore radius, the axial position of the exit section, the half-expansion angle, the profile compensation coefficient, and the angular window function. The angular window function continuously decreases from the center of the preset expansion angle domain to both sides and is zero outside the preset expansion angle domain. The controller first determines the target radius based on the corrected bore radius. Equivalent radius of the local conductive working segment and the gap between the forming process at the outlet Calculate the initial safety bias Then, based on the target surface radius Calculate the target bias Actual processing from Starting from a preset radial step size or trajectory, the effective energy is gradually transferred to the target area. The effective charge of each trajectory segment is determined based on the segment volume difference between the target radius and the corrected aperture radius, the reference volume electrochemical equivalent, and the segment volume removal correction coefficient of the corresponding trajectory segment.
[0119] Further implementation details for S6 are as follows:
[0120] Target surface and trajectory input: S6 reads S5's... Segmented volume removal correction factor Equivalent radius of the local conductive working segment And the orifice positioning reference, and read the design-given exit expansion start position. Target half-expansion angle θ, expansion angular domain half-width and surface compensation coefficient The z-axis points towards the outlet along the hole axis, with the angular position φ zeroed out at the expansion center direction; first hole Determined through graded calibration tests using the same material, working fluid, and outlet profile family, subsequent holes are only subject to S7-limited correction within the verified calibration validity range. For curved blade outlets, the CAD target profile is first projected onto the aforementioned z-φ coordinates along the local surface normal, and then the target hole wall radius is combined with... The gap between the forming process and the export process is converted into the radial-angular interpolation trajectory of the CNC tool center.
[0121] Based on the axial position of the β-th exit trajectory segment, the correction factor is removed from the volume of each axial segment output by S5. Mapping to the corresponding exit trajectory segment, we obtain the segment volume removal correction coefficient for that trajectory segment. .
[0122] ;
[0123] ;
[0124] The above target radius only applies to z≥ Expand the outlet end on one side; when z < At that time, take After obtaining Then, the initial safety offset for exit forming is determined first by the current corrected hole radius, and the target offset for exit forming is determined by the target profile radius; the exit forming machining clearance... The calibration was obtained based on the inter-electrode voltage, conductivity, size of the locally conductive working section, and flow state under the same material—sodium nitrate working solution conditions.
[0125] ;
[0126] ;
[0127] In the formula, Axial position and angular position The initial safety offset for exit forming is determined by the current modified hole profile. The target offset for the outlet forming is determined according to the target profile, and the unit is m; The equivalent radius of the axially localized conductive working segment, in meters (m). The effective processing clearance during the export forming stage, in meters (m). Only when... and Additional radial feed is executed at the same time; the actual trajectory is determined by... Towards The hierarchical approximation method does not allow for a one-step move to the final target bias.
[0128] In the formula, The target profile of the expansion outlet section on one side is located in the axial position. and angular position The radius at that location, in meters; The corrected hole radius is output by S5, in meters. The surface compensation coefficient is dimensionless. Position of the hole shaft, in meters; The starting position of the expansion, in meters; The target half-expansion angle is expressed in rad. When the design value is expressed in degrees, it should be converted to radians before being substituted into the tangent function. It is an angular window function, dimensionless; The angular position relative to the center of expansion, in rad; The full width at half maximum (FWHM) of the extended angular domain is expressed in rad. Pi is a dimensionless mathematical constant; subscripts are used. Indicates the target surface. Indicates the need to correct the hole body. Represents the boundary of the angular domain. At the expansion center of 1, The amount of additional removal is continuously reduced to 0 at the point of origin and 0 outside the corner region, thus limiting the additional removal amount to the outlet side.
[0129] Track unit power consumption: Divide the exit section into axial-angular track units, and calculate the additional removal volume and power consumption of the β-th track segment according to the following formula; the β-th exit track segment corresponds to the axial interval. And cover the preset expansion area , G represents the total number of segments in the exit trajectory.
[0130] ;
[0131] ;
[0132] In the formula, For the first Additional removal volume for each exit trajectory segment, in m³; , These are the axial start and end points of the trajectory segment, respectively; , and The meaning and units are the same as before; For the first The effective electrical energy required for each exit trajectory segment, in C; The correction factor is removed from the segmented volume of the trajectory relative to the reference calibration condition, and it is dimensionless; Reference volumetric electrochemical equivalent under calibration conditions, unit m³ / C; subscript Indicates selective shaping for export. This represents the segmentation of the trajectory. Before the integral... Used to convert volume based on the sector area relationship in polar coordinates.
[0133] Execution, Interlocking, and Output: After S5 has completed the circumferential uniform radial reaming and formed a constant-diameter hole, the axially locally conductive working section is positioned in the exit forming area. The solid rigid tool electrode can continue to rotate, interpolating unit by unit only in the exit section according to the radial-angular trajectory of the tool center. Axial reciprocating motion covering the entire hole and uniform radial reaming covering 360° of the circumference are no longer performed. Each trajectory unit advances stepwise towards the target bias from its initial safety bias. The current bias layer only continues to advance when the allocated effective charge reaches the requirement and the effective gap or local profile meets the conditions for entering the next bias layer. After finally reaching the target bias, the condition for switching to the next unit is that the cumulative effective charge of the unit reaches the requirement and the local surface enters the allowable tolerance. If the positive bias safety window of any control cycle fails, the interpolation trajectory is immediately frozen. If a non-zero protection bias still exists in the current stage, it is maintained at the protection value; otherwise, the positive bias source is cut off, and the window is restored by enhancing the flushing fluid, adjusting the gap, etc. After the window is restored, it continues from the remaining charge of the interrupted unit. The S6 outputs the final outlet profile, the electrical completion rate of each trajectory segment, the minimum positive bias safety margin, and the number of abnormal recovery times. These data serve as inputs for the S7 geometry / flow rate comparison and the correction of the next orifice parameters.
[0134] S7 detects the bore geometry, inlet-outlet diameter difference, outlet profile, and pressure-flow characteristics of the completed orifice. Based on the detection error, dynamic positive bias safety margin during processing, and abnormal records, it generates the parameter correction amount for the next film gas orifice, which is limited by the calibration data. The parameter correction amount is then sent back to S1, S3, S5, and S6 to correct the initial processing control parameters, effective charge for remelting layer removal, radial offset, effective charge for radial orifice expansion, profile compensation coefficient, and segmented pure electrolysis trajectory of the next film gas orifice. The pressure-flow coefficient error is used to assist in correcting the profile compensation coefficient or local trajectory dwell amount of the expansion outlet section on one side under the constraints of bore geometry and outlet profile tolerance.
[0135] In S7, the detection errors include orifice diameter error, inlet-outlet orifice diameter difference, expansion angle error, outlet profile error, and pressure difference-flow coefficient error. Based on the orifice diameter error and inlet-outlet orifice diameter difference, and combined with the taper correction weight corresponding to the axial position, the radial offset and effective radial expansion charge of the next film gas orifice are corrected. In cases where the inlet is already too large, the taper correction weight of the inlet side segment is reset to zero. The profile compensation coefficient and segmented pure electrolytic trajectory of the next film gas orifice are corrected based on the expansion angle error and outlet profile error. Under the constraints of orifice geometry and outlet profile tolerance, the pressure difference-flow coefficient error is used to assist in correcting the profile compensation coefficient or local trajectory dwell time. The initial positive bias, pulse interval, and working fluid circulation parameters of the next film gas orifice are corrected based on the minimum dynamic positive bias safety margin and the number of dynamic positive bias safety window recovery times of each control cycle of the previous film gas orifice. The correction amounts for each parameter are limited within the calibration upper and lower limits of the workpiece material and working fluid.
[0136] Further implementation details for S7 are as follows:
[0137] Test data and orifice index: Inlet orifice diameter, outlet orifice diameter, roundness, and orifice profile are obtained by coordinate measurement, 3D optical profile measurement, or industrial CT. The inlet-outlet orifice diameter difference is used to characterize the residual taper of the orifice body. Expansion angle and outlet profile error are obtained by registering the measured point cloud with the CAD target surface. Flow rate is measured at specified inlet pressure, outlet pressure, and gas temperature, and the pressure difference-flow coefficient is calculated. All test values are compared with those of the same orifice number stored in S2 to S6. , , , , The minimum safety margin and the number of abnormal recovery times are correlated; the pressure difference-flow coefficient is only used as an auxiliary feedback quantity for outlet forming when the orifice geometry and outlet profile meet the preset tolerance constraints, so as to avoid destroying the geometric dimensions that have already met the requirements by correcting the flow rate.
[0138] Error decoupling: Define the error of the j-th axial segmented aperture. Average aperture error For overall judgment only; defines the inlet-outlet aperture difference error. Half-expansion angle error and flow coefficient error The average diameter of the bore is relatively small. When approaching zero, the radial offset of each segment target and the effective electrical charge of radial hole enlargement are increased in the same direction under limited conditions; When the value is positive and the inlet is too large, a taper correction weight related to the axial position is used. The segmented entrance is already too large. =0, assigning positive correction weights only to the export side or the lower middle section of the out-of-tolerance segment, so that the corresponding target radial offset and Increase; the aperture meets the requirements and Or, if the export profile is out of tolerance, correct it. And the corresponding exit trajectory unit resides; it is only activated when both the hole geometry and the exit profile are within the allowable tolerances. The corresponding flow correction item is used; otherwise, the item is set to 0.
[0139] Therefore, the circumferential uniform radial hole expansion error of S5 and the one-sided expansion error of S6 are treated separately.
[0140] ;
[0141] ;
[0142] ;
[0143] ;
[0144] In the formula, superscript and They represent the current number. One hole and the next hole; For the first The target radial offset of each axial segment; This corresponds to the effective electrical charge for radial bore expansion; This refers to the aperture error of this segment; This refers to the error caused by the difference in inlet and outlet orifice diameters. For the first The segmented taper correction weight is applied when the inlet segment is already too large. Take 0, and take positive values for the export side or the middle and lower part of the segment to be compensated; , , and Radial aperture expansion limitation correction gain; This is the surface compensation coefficient; This is the half-expansion angle error; This is the error in pressure difference versus flow coefficient. and These are the limited correction gains for the expansion angle and the flow coefficient, respectively. Three All functions explicitly use the upper and lower bounds of the corresponding parameters. The flow correction term is only enabled when the orifice geometry and outlet profile meet the preset tolerances; otherwise, it is set to... The value is 0. If the error directions of two consecutive holes are opposite, the corresponding correction gain is reduced to avoid batch closed-loop oscillation.
[0145] Feedback Link: The initial positive bias voltage of the next hole is corrected based on the minimum safety margin and safety window recovery times for each cycle of the current hole; the effective charge for remelting layer removal in S3 is corrected based on the discharge energy per unit removal volume, pre-hole anomaly distribution, and volumetric electrochemical equivalent calibration value; the target radial bias in S5... and effective electrical charge of radial enlargement Based on the aperture error of each segment, the inlet-outlet aperture difference, and the taper correction weight Correction; S6 The outlet trajectory is corrected based on the expansion angle, outlet profile error, and flow coefficient error under the premise of meeting geometric tolerances. S7 outputs the initial pulse / fluid flow parameter correction amount for the current stage. Correction amount Correction amount and The exit trajectory correction amount is sent back to S1, S3, S5 and S6 respectively, and written into the next hole control package.
[0146] The aforementioned preset lower boundary margin, preset upper boundary margin, maximum allowable positive bias voltage change per control cycle, and each constrained correction gain are all determined through calibration tests for specific workpiece materials, working fluids, processing stages, and machine tool response characteristics. Specifically, the boundary margin is determined based on voltage, current, temperature, conductivity, and pressure detection errors, calibration model fitting errors, and safety redundancy. The maximum allowable positive bias voltage change per control cycle is constrained by the constraint that the updated positive bias voltage does not exceed the current dynamic positive bias voltage safety window and does not cause abrupt changes in the inter-electrode state. Each correction gain is adjusted incrementally from a conservative initial value, determined by the criterion that the corresponding error can converge stably without continuous reverse correction or closed-loop oscillation. The final allowable values and their upper and lower bounds are then written into the corresponding material-working fluid calibration data.
[0147] Example 1: Complete machining process of film cooling holes in nickel-based superalloy blades;
[0148] The blade to be machined is a nickel-based high-temperature alloy. The target circular hole diameter is 0.80 mm, the hole depth is 6.0 mm, the target full expansion angle is 25°, and the starting position of the exit expansion is 2.0 mm from the outer surface of the exit. The blade is mounted on the worktable of a five-axis EDM-Electrolytic composite machine tool. The transformation relationship between the machine tool coordinate system and the blade model coordinate system is established using a reference ball and a blade profile probe. The hole axis pose is entered into the CNC system after collision checking. The blade is not loosened during subsequent electrode changes and working fluid changes.
[0149] During S1 implementation, two sets of calibration data were established: Under deionized water or low-conductivity working fluid conditions, the generation and discharge characteristics of corrosion removal products in the pre-hole stage, the migration, enrichment, and deposition trends of exogenous impurity cations towards the processed hole wall, the gas-containing inter-electrode breakdown parameters, and the allowable bias voltage and dynamic positive bias voltage safety window for the anodic reaction in the pre-hole stage were calibrated. Under sodium nitrate aqueous solution conditions, anodic polarization curves were obtained using test pieces from the same batch of materials, and the passivation film formation and maintenance bias voltage, the allowable bias voltage for passivation film destruction, the oxygen evolution or excessive anodic reaction initiation potential, the reference volume electrochemical equivalent under reference conditions, and the volume removal correction relationship were calibrated. Simultaneously, based on the normal design composition of the sodium nitrate working fluid, the types of exogenous impurity cations requiring anti-backflow control in this processing stage and their allowable concentration ranges were redefined. All parameters used actual calibration results as control boundaries, and reference values from a single material or device were not used as universal fixed thresholds.
[0150] When implementing S2, a 0.62mm diameter hollow copper electrode is selected, with an approximately 30μm aluminum oxide insulating layer formed on the sidewall. Only the bottom surface is conductive, and the radial runout is no greater than 2μm. The initial pulse peak current is 15A, the pulse width is 8μs, the pulse interval is 8μs, and the initial positive bias voltage is 6V, which does not return to zero during the interval. The controller forms a control cycle every 100 pulses and calculates... , Abnormal pulse ratio and the latest safety window. Based on the allowable limit of the backflow characterization charge obtained under the same material, working fluid, and corresponding exogenous impurity cation conditions, the risk of exogenous impurity cations migrating back to, enriching, and depositing on the processed hole wall is assessed. The backflow characterization charge is only used as a risk control indicator and is not directly equivalent to the actual migration charge of the exogenous impurity cations. A 0.8 MPa internal flushing fluid is used, and the electrode is fed at 800 r / min. After the pre-hole is completed, the single-hole discharge energy history, axial abnormal pulse distribution, and pre-hole profile are output.
[0151] When implementing S3, first calculate the actual material removal volume based on the pre-hole contours. , and then Obtain the discharge energy per unit volume The equivalent remelted layer thickness of each hole shaft segment was calculated based on the cross-sectional calibration relationship of the same batch of materials, the same working fluid, and the corresponding pulse energy range. Determine the verified delamination safety margin by combining the calibration residuals. Construct the minimum envelope removal When the target semi-finished hole profile is completely outside the minimum removal envelope and still retains a positive radial finishing allowance relative to the final target hole body, the total material volume difference between the original measured profile of the pre-hole and the target semi-finished hole profile is used to calculate the total material volume difference. Then, the reference volume electrochemical equivalent obtained under the reference calibration conditions is used. Current operating condition volume removal correction factor calculate If the above two geometric conditions cannot be satisfied simultaneously, or If the proportion of abnormal pulses exceeds the calibration range, the automatic extrapolation will not continue, and the process will switch to manual verification, recalibration, or safe shutdown.
[0152] During S4 implementation, the pre-hole working fluid is drained and a filtered sodium nitrate aqueous solution is pumped in. A solid rigid tool electrode made of cemented carbide with an aspect ratio of not less than 8 is then used. This electrode retains only the exposed conductive section in the axial direction, while the remaining outer peripheral surface, bottom end surface, and other non-working surfaces are insulated. The outer contour of the non-working section after being covered with an insulating layer is not higher than the outer circular surface of the conductive section. In this embodiment, the hole depth is divided into multiple axial segments, and the axial width of the locally conductive working section is less than the length of a single segment. When the tool electrode reciprocates axially, the controller implements machining pulse gating based on the position of the axial encoder. Electrolytic pulses are activated only after the locally conductive working section has fully entered the allowable machining range of the target segment, and machining pulses are deactivated when crossing the segment boundary, maintaining only mechanical reciprocation and fluid replacement. After the segment reaches the corresponding required charge, the machining pulses are paused and an internal contour check is performed. The segment volume removal correction coefficient is updated based on the measured removal volume. Once all segments meet the semi-finishing tolerance and the through-through is confirmed, proceed to S5.
[0153] When implementing S5, the 6.0mm hole depth is divided into 12 0.5mm axial segments, based on the semi-finished hole radius. Target radius Calculate the volume to be removed in each segment. Then, the correction factor is removed using the segmented volume. and reference volume electrochemical equivalent Calculate the effective charge of radial enlargement Initial safety radial offset according to Equivalent radius of the local conductive working segment and machining clearance compensation amount Determine the target radial offset. according to , and Confirmed. The electrode is positioned along the hole axis, aligning the locally conductive working section with the j-th segment and maintaining its axial position, then first moving radially to... Then, proceed step by step according to the preset radial step size. Each stage executes a 360° closed circular trajectory around the target hole axis and allocates corresponding effective electrical charge; only after the electrical charge and internal contour / clearance conditions of the current layer are met will it proceed to the next layer. Ultimately, this achieves... ,Grand total Once the requirements are met and the profile enters the tolerance zone, proceed to the next segment. After all segments are completed, remeasure the inlet and outlet bore diameters, and update the segments with residual taper separately. and the remainder .
[0154] When S6 is implemented, Taking a point 2.0 mm from the outer surface of the outlet, the designed half-expansion angle is 12.5°, which is converted to [value missing] during calculation. ; The first hole is determined according to the designed fan width. Determined by calibration results. After the S5 forms a constant diameter hole, the CNC system first... , and Calculate the initial safety bias for outlet forming And then according to , and Calculate target bias , by e c Towards Radial-angular interpolation is performed in stages according to trajectory units; each stage only proceeds to the next bias layer after the allocated charge and effective gap / local surface conditions are met. Locally conductive working sections are processed only within the preset exit angular region, and uniform radial hole enlargement covering 360° circumference is no longer performed; the total charge requirement for each unit is determined by... , and Once the target offset is achieved and the total charge and surface tolerances are met, switch to the next unit.
[0155] During S7 implementation, measure the inlet orifice diameter, outlet orifice diameter, roundness, half-expansion angle, outlet profile, and flow coefficient under a specified pressure differential. If the overall orifice diameter of each segment is too small, but the inlet-outlet orifice diameter difference is within acceptable limits, then increase the diameter of the next orifice in the same direction within the calibration upper limit. and If the inlet diameter is larger than the outlet diameter and the residual taper is out of tolerance, then the already oversized segment on the inlet side should be repositioned. Set to zero, only adding to the out-of-tolerance segment on the export side or in the lower middle section. and If the hole body meets the requirements but the expansion angle is too small, then raise the next hole. Alternatively, add corresponding outlet unit dwell time; only when the orifice geometry and outlet profile are within allowable tolerances but the flow coefficient is still low, according to... Slight improvement within the calibration boundaries Alternatively, the corresponding outlet trajectory unit can be added to the station. If the safety margin is insufficient, the positive bias voltage should not be increased; instead, the pulse interval or circulation flow rate should be increased.
[0156] Example 2: Recovery process for dynamic positive bias safety window failure;
[0157] During deep hole machining, if the working fluid temperature increases, conductivity increases, and the deionization time constant is prolonged, problems may occur. rise and Decline. When When this happens, the controller immediately freezes the feed; if the current... If a non-zero protection bias is still permissible, reduce the positive bias source to a non-zero protection value not exceeding the current upper boundary. If no non-zero permissible value exists, immediately disconnect the positive bias source. Upon entering the sodium nitrate electrolysis stage, if the lower limit increases due to the need to maintain the passivation film, prioritize increasing the working fluid refresh rate, adjusting the gap, and reducing the temperature rise recovery window, rather than simply reducing it to a positive bias that the passivation film cannot stably maintain. If three consecutive recovery attempts fail, keep the positive bias source disconnected and disconnect the main processing power supply, saving any abnormal data.
[0158] Example 3: Method for obtaining calibration and public parameters;
[0159] The remelted layer calibration relationship was established using test holes made of the same material and working fluid as the blade, and with multiple pulse energy levels: the thickness of the remelted layer on the cross-section of the hole wall was measured, and the discharge energy removed per unit volume was calculated. and abnormal pulse ratio Using the equivalent remelted layer thickness as the output, a constrained fit is performed, and the upper confidence bound of the fitting residual is used as the delamination safety margin for S3. This relationship applies only to the corresponding material grade, working fluid, pulse energy, and temperature range; direct extrapolation is not permitted outside these ranges. Reference volume electrochemical equivalent. Under specified reference operating conditions, the known processing power is used. With material removal volume The calibration was obtained. Volume removal correction factor under current processing conditions Defined as the volume removed per unit of actual electricity relative to The ratio of , therefore the actual effective volume equivalent is . And can perform segmentation after phase contour retesting. Make corrections. This is an empirical correction factor, which can be greater than, equal to, or less than 1 based on the actual removal capacity of the current operating condition relative to the reference operating condition. The passivation film formation and maintenance bias, the allowable bias for passivation film destruction, the oxygen evolution or excessive anodic reaction threshold, and the local depassivation current density threshold are jointly calibrated by the anodic polarization curve and repeated pulse tests.
[0160] Surface compensation coefficient Obtained through grading and calibration tests using the same materials, working fluid, and outlet type family: [In multiple candidate...] The calibration holes are machined, and the measured outlet profile is registered with the CAD target profile. Parameters that minimize the combined expansion angle error, local profile error, and pressure-flow deviation without exceeding geometric tolerances are selected as the initial values for the first hole. Subsequent holes are then... The correction is limited to the validated calibration range.
[0161] Although embodiments of the invention have been shown and described, the scope of the invention will be defined by the appended claims and their equivalents by those skilled in the art.
Claims
1. A method of biasing anti-bleed turbine blade film hole machining by pulsed direct current composite electric field, for machining a film hole with a hole body and a one-side expanded exit section on a turbine blade, characterized in that, Includes the following steps: S1, acquire the pore geometry data of the film gas pores, the calibration data of the workpiece material and the working fluid, and the inter-electrode state data; establish a dynamic positive bias safety window according to the processing stage, wherein, in the pre-hole stage of electrical discharge machining, characterize the corrosion removal products formed by the local melting, vaporization, peeling, or dispersion of the workpiece material through electrical discharge machining and entering the working fluid, and based on the migration state of exogenous impurity cations in the working fluid and processing environment that are different from the intrinsic elements of the workpiece matrix and do not belong to the current working fluid design components, and the migration state of the exogenous impurity cations into the already processed fluid. The trend of backflow, enrichment, and deposition on the borehole wall is used to determine the lower limit of the positive bias voltage required to prevent backflow. At the same time, the upper limit of the positive bias voltage is determined based on the gas-containing inter-electrode breakdown constraint and the allowable conditions of the anodic reaction at this stage. In the sodium nitrate electrolysis stage, the larger of the positive bias voltage required to prevent backflow and the positive bias voltage required to form and maintain the passivation film is used as the lower limit of the positive bias voltage, and the minimum of the allowable voltage of gas-containing inter-electrode breakdown, the allowable voltage of passivation film destruction, and the allowable voltage of oxygen evolution or excessive anodic reaction is used as the upper limit of the positive bias voltage. The initial processing control parameters are output under the constraint of the dynamic positive bias voltage safety window of the current processing stage. S2, perform pre-hole drilling using electrical discharge machining (EDM). A positive bias is superimposed on the EDM pulse, ensuring the workpiece maintains a positive polarity relative to the tool electrode and remains non-zero during the pulse interval. The inter-electrode electrical signal and working fluid status are acquired according to the control cycle. Based on the acquisition results, the lower and upper limits of the positive bias for the current stage are updated, limiting the positive bias within the updated dynamic positive bias safety window. When the dynamic positive bias safety window fails, the feed is immediately paused. If the current upper boundary still allows a non-zero protection bias, the positive bias is limited to a non-zero protection value within the upper boundary. If no non-zero allowable value exists, the positive bias source is cut off. At least one of the inter-electrode gap, pulse interval, and working fluid circulation status is adjusted until the dynamic positive bias safety window is restored. The pre-hole discharge history, pre-hole geometry data, and anomaly records are output. S3, based on the pre-hole discharge history, pre-hole geometry data, and anomaly records output by S2, and in conjunction with the calibration data, determine the unit removal volume discharge energy and the remelting layer removal allowance of the pre-hole wall during the pre-hole stage; divide the hole axis into multiple axial processing segments, establish the minimum removal envelope for each axial processing segment based on the equivalent thickness of the remelting layer, determine the target semi-finished hole contour under the condition that the target semi-finished hole contour is outside the minimum removal envelope and retains a positive processing allowance for subsequent radial hole enlargement, and determine the volume to be removed by the material volume difference between the original measured contour of the pre-hole and the target semi-finished hole contour; when the above two conditions cannot be met simultaneously, stop automatic processing or switch to manual verification; based on the reference volume electrochemical equivalent calibrated under the same material-working fluid reference conditions and the volume removal correction coefficient corresponding to the current processing conditions, convert the volume to be removed into the effective charge required for electrolytic semi-finishing; S4, drain the pre-hole working fluid and replace it with sodium nitrate aqueous solution, and replace it with a solid rigid tool electrode with only the axially partially conductive working section exposed and conductive, and the rest of the non-working surfaces insulated; based on the segmented effective charge output in S3, perform axial reciprocating segmented electrolytic semi-finishing under the constraint of the updated electrolysis stage dynamic positive bias safety window, so that the axially partially conductive working section acts on different axial processing sections in sequence, and the working fluid in the hole is periodically replaced with the axial reciprocating motion of the tool electrode. The passivation film formed and maintained by the sodium nitrate system is used to suppress stray corrosion in non-target areas, and the cumulative effective charge is used to control the remelting layer removal and pre-hole taper reduction process, and output the semi-finished hole profile and segmented volume removal correction coefficient; S5, after the bottom end of the solid rigid tool electrode has completely passed through the workpiece exit, based on the semi-finished hole profile, target hole profile, and segmented volume removal correction coefficient output in S4, set the initial safe radial offset, target radial offset, and effective radial expansion charge for each axial segment; align the axial locally conductive working segment sequentially with the corresponding axial segment, and while maintaining the axial position, make the center of the tool electrode approach the target radial offset step by step from the initial safe radial offset according to the preset radial step size and the allocated effective charge, and perform radial-circumferential closed interpolation around the target hole axis at each offset position to maintain the effective machining gap between the tool electrode and the current hole wall; perform circumferentially uniform segmented radial expansion finishing according to the effective radial expansion charge, and output the corrected hole profile after eliminating residual taper and the charge completion degree of each axial segment; S6, based on the corrected hole contour and charge completion rate output from S5, the segmented volume removal correction coefficient, and the target surface of the one-sided expansion outlet section, generate segmented pure electrolytic trajectories that only act on the preset expansion angle domain, and configure effective charge for each trajectory segment; determine the initial safety offset of outlet forming based on the corrected hole radius, the equivalent radius of the axially locally conductive working section, and the outlet forming processing gap; determine the target offset of outlet forming based on the target surface radius, the equivalent radius of the axially locally conductive working section, and the outlet forming processing gap; position the axially locally conductive working section at the outlet section and perform radial-angular interpolation in stages from the initial safety offset to the target offset, forming the one-sided expansion outlet section while maintaining the effective processing gap; S7: After detecting the hole geometry, inlet-outlet diameter difference, outlet profile, and pressure-flow characteristics of the completed hole, generate the next film gas hole parameter correction amount limited by the calibration data based on the detection error, dynamic positive bias safety margin during processing, and abnormal records. The parameter correction amount is then sent back to S1, S3, S5, and S6 respectively to correct the initial processing control parameters, effective charge for remelting layer removal, radial offset, effective charge for radial hole expansion, and forming parameters of the expansion outlet section on one side of the next film gas hole.
2. The method of claim 1, wherein the method is a method of pulse DC compound electric field bias anti-back diffusion turbine blade film hole processing. In S1, the lower limit of the positive bias voltage in the pre-hole stage of the electrical discharge machining is determined according to the anti-backflow requirement corresponding to the trend of the exogenous impurity cations migrating back, accumulating and depositing to the processed hole wall. The upper limit of the positive bias voltage is the smaller value between the allowable voltage of the bubble equivalent channel breakdown and the allowable voltage of the anodic reaction in the pre-hole stage. After entering the sodium nitrate electrolysis stage, the lower limit of the positive bias voltage is the larger value between the positive bias voltage required to prevent backflow and the positive bias voltage required to form and maintain the passivation film. The upper limit of the positive bias voltage is the minimum value among the allowable voltage of the bubble equivalent channel breakdown, the allowable voltage of the passivation film destruction obtained by calibration with the same material and working fluid, and the allowable voltage of oxygen evolution or excessive anodic reaction. When the difference between the upper and lower limits of the positive bias voltage at the current stage is greater than the sum of the preset lower boundary margin and the preset upper boundary margin, the dynamic positive bias voltage safety window is determined to be valid.
3. The method of claim 2, wherein the method further comprises: In S2, the interelectrode current during the pulse interval is attenuated and fitted to obtain the deionization time constant, and the current component higher than the steady-state leakage current is integrated to obtain the backflow characterization charge. The backflow characterization charge is a control characterization quantity that corresponds to the risk of the exogenous impurity cations migrating back, enriching, and depositing to the processed pore wall after calibration with the same material and working fluid. Its allowable limit is obtained by calibration test. When the dynamic positive bias voltage safety window is effective, the positive bias voltage of the next control cycle is updated in a restricted manner according to the difference between the required anti-backflow field strength and the measured positive bias voltage field strength and the deviation of the backflow characterization charge relative to the allowable limit. The maximum positive bias voltage change in a single control cycle is limited so that the positive bias voltage remains non-zero during the update process and does not exceed the dynamic positive bias voltage safety window. When the dynamic positive bias safety window fails, it should be handled according to the abnormal recovery procedure.
4. The method for machining film pores in a biased anti-backflow turbine blade using a pulsed DC composite electric field according to claim 1, characterized in that, In S2, a hollow copper tool electrode with sidewall insulation and only bottom surface conductivity is used for EDM pre-holeing. The initial positive bias voltage calibration range during the EDM pre-holeing stage is 3-8V. When at least two of the following conditions are met: inter-electrode voltage drop, peak current exceeding the limit, breakdown delay shortening, and pulse interval current decay slowing down, the corresponding control cycle is marked as an abnormal pulse cycle, and the hole shaft position and discharge data of the abnormal pulse cycle are written into the abnormal record.
5. The method for machining film pores in a biased anti-backflow turbine blade using a pulsed DC composite electric field according to claim 1, characterized in that, In S3, the product of the inter-electrode voltage and inter-electrode current of each effective pulse in the pre-hole stage is integrated over time to obtain the single-hole discharge energy. The single-hole discharge energy is divided by the actual material removal volume in the pre-hole stage to obtain the unit removal volume discharge energy. The unit removal volume discharge energy and the abnormal pulse ratio are input into the remelting layer calibration relationship established with the same material, working fluid, and corresponding pulse energy range to obtain the equivalent thickness of the remelting layer. A minimum removal envelope is established based on the measured profile of the pre-hole, the equivalent thickness of the remelting layer, and the verified delamination safety margin. The target semi-finished hole profile is determined under the condition that the target semi-finished hole profile is outside the minimum removal envelope and smaller than the target hole body profile to retain the subsequent radial hole enlargement margin. The volume difference between the original measured profile of the pre-hole and the target semi-finished hole profile is used as the volume to be removed by electrolysis. Then, based on the reference volume electrochemical equivalent calibrated under the same material and working fluid reference conditions and the volume removal correction coefficient corresponding to the current processing conditions, the volume to be electrolyzed for removal is converted into the effective charge required for electrolytic semi-finishing. When the target semi-finished hole contour cannot simultaneously satisfy the complete removal of the remelted layer and the retention of positive radial finishing allowance, automatic processing is stopped or manual verification is initiated. When the discharge energy per unit removal volume or the proportion of abnormal pulses exceeds the applicable range of the calibration relationship, extrapolation of the calibration relationship is prohibited, and a recalibration or safe shutdown process is initiated.
6. The method for machining film pores in a biased anti-backflow turbine blade using a pulsed DC composite electric field according to claim 1, characterized in that, In S4, a sodium nitrate aqueous solution with a mass fraction of 10%–15% is used as the working fluid, and a solid rigid tool electrode with an aspect ratio of not less than 8 is used. The solid rigid tool electrode only retains an exposed conductive section with localized axial conductivity. The outer peripheral surface, bottom surface, and other non-working surfaces, excluding the localized conductive section, are provided with an insulating layer, and the axial length of the localized conductive section is less than the length of a single axial machining segment. Under the action of an electric field, the sodium nitrate aqueous solution causes a passivation film to form on the anode surface of the workpiece, while the non-machined area remains passivated. Electrolytic pulses with a peak current density reaching the local depassivation threshold calibrated by the same material-sodium nitrate system are used within the target machining gap corresponding to the localized conductive section, and the pulse interval meets the calibration requirements for repassivation and discharge of reaction products. The tool electrode reciprocates axially at a frequency of 10–20 Hz and a stroke of 1–3 mm, and the machining pulses are position-synchronized and gated according to the axial position of the tool electrode. The effective charge is accumulated according to the axial segments to complete the removal of the remelted layer and the initial reduction of the pre-hole taper.
7. The method for machining film pores in a biased anti-backflow turbine blade using a pulsed DC composite electric field according to claim 6, characterized in that, In S5, after the bottom end of the solid rigid tool electrode has completely passed through the workpiece exit, the axially locally conductive working section is sequentially aligned with each axial segment; based on the semi-finished hole profile, the target hole profile, the machining clearance compensation amount, the equivalent radius of the axially locally conductive working section, and the segment volume removal correction coefficient of the corresponding axial segment, the volume to be removed, the effective electrical charge for radial hole enlargement, the initial safe radial offset, and the target radial offset of each axial segment are determined respectively. After the tool electrode reaches any axial segment, it maintains the axial position of that segment. Starting from the initial safe radial offset, it gradually increases the radial offset according to the preset radial step size and the allocated effective electrical charge, and performs at least one radial-circumferential closed interpolation around the target hole axis at each offset position. When the target radial offset is finally reached, the cumulative effective charge reaches the corresponding effective charge for radial hole enlargement, and the profile enters the preset tolerance zone, the process moves to the next axial segment. If the conditions are not met, the remaining effective charge and subsequent radial offset layers are updated based on the remaining profile error.
8. The method for machining film pores in a biased anti-backflow turbine blade using a pulsed DC composite electric field according to claim 1, characterized in that, In S6, the target radius of the expansion exit section on one side is determined by the modified hole radius, the axial position of the exit section, the half-expansion angle, the profile compensation coefficient, and the angular window function. The angular window function continuously decreases from the center of the preset expansion angle domain to both sides and is zero outside the preset expansion angle domain. The initial safety offset of the exit forming is determined based on the modified hole radius, the equivalent radius of the axially locally conductive working section, and the exit forming processing gap. The target offset of the exit forming is determined based on the target radius, the equivalent radius of the axially locally conductive working section, and the exit forming processing gap. The effective charge of each trajectory segment is determined based on the segmented volume difference between the target radius and the modified hole radius, the reference volume electrochemical equivalent, and the segmented volume removal correction coefficient of the corresponding trajectory segment. The tool electrode performs radial-angular interpolation in the exit section from the initial safety offset to the target offset in stages, and does not perform axial reciprocating motion covering the entire hole.
9. The method for machining film pores in a biased anti-backflow turbine blade using a pulsed DC composite electric field according to claim 2, characterized in that, When the lower limit of the positive bias voltage is not less than the upper limit of the positive bias voltage minus the sum of the preset lower boundary margin and the preset upper boundary margin, the feed is immediately frozen; if the current upper boundary of the positive bias voltage still allows a non-zero protection bias voltage, the positive bias voltage source is adjusted to not exceed the non-zero protection value of the upper boundary of the positive bias voltage; if there is no non-zero allowable value, the positive bias voltage source is immediately cut off; then, at least one of the following is executed: tool electrode retraction, increasing pulse interval, increasing working fluid circulation flow rate, and decreasing working fluid temperature, to resample and re-establish the current stage dynamic positive bias voltage safety window, and processing continues only when the safety window is restored to effectiveness; if it is not restored within the preset number of restorations, the main processing power is cut off and the corresponding hole position and abnormal data are recorded.
10. The method for machining film pores in a biased anti-backflow turbine blade using a pulsed DC composite electric field according to claim 1, characterized in that, In S7, the detection errors include orifice diameter error, inlet-outlet orifice diameter difference, expansion angle error, outlet profile error, and pressure difference-flow coefficient error. Based on the orifice diameter error and inlet-outlet orifice diameter difference, and combined with the taper correction weight corresponding to the axial position, the radial offset and effective radial expansion charge of the next film gas orifice are corrected. In cases where the inlet is already too large, the taper correction weight of the inlet-side segment is reset to zero. The profile compensation coefficient and segmented pure electrolytic trajectory of the next film gas orifice are corrected based on the expansion angle error and outlet profile error. Under the constraints of orifice geometry and outlet profile tolerance, the pressure difference-flow coefficient error is used to assist in correcting the profile compensation coefficient or local trajectory dwell time. The initial positive bias, pulse interval, and working fluid circulation parameters of the next film air hole are corrected according to the minimum dynamic positive bias safety margin and the number of dynamic positive bias safety window recovery times of each control cycle of the previous film air hole; the correction amount of each parameter is limited within the calibration upper and lower limits of the workpiece material and working fluid.