A laser and mechanical combined drilling method for ultra-thin PCBs
By applying in-plane prestress to ultra-thin PCB boards and combining laser and mechanical drilling, the problems of bending and copper foil tearing in the large-diameter hole processing of ultra-thin PCB boards were solved, achieving efficient and stable hole processing results.
Patent Information
- Application Number
- CN202611521451.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-29
- Publication Date
- 2026-11-24
AI Technical Summary
When processing large-diameter through holes on ultra-thin PCB boards, existing technologies often result in mechanical drilling causing board bending and copper foil tearing, while laser melting has a long processing cycle and is prone to thermal warping deformation, which cannot meet the needs of industrial-scale production.
The laser-mechanical composite drilling method first applies in-plane pre-tension stress to the PCB board, then locally softens the resin substrate with laser and induces thermal stress microcrack rings on the copper foil layer, and finally achieves efficient hole formation by segmented feeding with mechanical drill bit.
It effectively suppresses board bending and copper foil tearing, shortens the processing cycle, and ensures the electrical insulation performance and smoothness of the hole walls, making it suitable for the industrial-scale production of ultra-thin PCBs.
Smart Images

Figure CN123149556A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the technical field of PCB board processing, and specifically to a laser and mechanical composite drilling method for ultra-thin PCBs. Background Technology
[0002] With the rapid development of smartphone camera modules, wearable smart devices, and high-density interconnect (HDI) microelectronic packaging technologies, printed circuit boards (PCBs) and copper-clad laminates are evolving towards ultra-thinness and high integration, with the total nominal thickness of the boards reduced to [missing information]. Even thinner, ultra-thin profiles. To achieve interlayer interconnects or device assembly, it is often necessary to machine holes with diameters reaching [insert diameter here]. The presence of through holes often results in the ratio of the through hole diameter to the total thickness of the board material exceeding a certain limit. Currently, the industry mainly relies on purely mechanical drilling or full laser ablation to create holes in such plates. When traditional mechanical drill bits cut into the insulating medium at high speed, the cutting speed at the center transverse cutting edge of the drill bit is almost zero. It relies solely on axial force to push and squeeze the material out, generating extremely high axial propulsion reaction force. This forces the ultra-thin board to produce significant off-surface bending and severe high-frequency chatter in the drilling micro-area, which can easily induce micro-cracks in the substrate of the hole wall, interlayer delamination, and micro-chipping at the edges. On the other hand, because the single-layer copper foil on the surface of the ultra-thin single-sided copper-clad laminate is extremely thin and lacks back-side symmetrical constraint, the tangential shearing generated by the high-speed rotating drill bit can easily cause the surrounding copper foil to tear, resulting in large-area peeling, warping, lifting, and curling burrs of the copper foil on the front side of the hole edge, causing a serious decrease in the reliability of the through-hole electrical connection.
[0003] Existing technologies also attempt to use full laser vaporization / melting direct ablation for hole formation. However, when the target hole diameter is relatively large compared to the plate thickness, the laser needs to repeatedly fill and scan the large volume of metal and resin material in the hole layer by layer, which drastically increases the processing cycle of a single hole and cannot meet the needs of industrial-scale mass production. At the same time, the thinness of ultra-thin plates and the narrow lateral heat conduction cross section make it easy for the continuous high-energy laser heat accumulation to diffuse into the normal dielectric layer around the hole, causing thermal warping deformation of the entire plate and causing thermal degradation, carbonization, or severe degradation of the interfacial bonding strength of the insulating resin around the hole wall. Summary of the Invention
[0004] In order to solve the above-mentioned problems in the existing technology, the present invention aims to provide a laser and mechanical composite drilling method for ultra-thin PCBs, which can effectively solve the above problems.
[0005] The technical solution adopted in this invention is: a laser-mechanical composite drilling method for ultra-thin PCBs, comprising the following steps: S1. Board tensioning and clamping: The PCB board to be processed is clamped in a pre-tensioning device, and the pre-tensioning device applies in-plane pre-tensioning stress to the PCB board in two directions or one direction to keep the PCB board in a tensioned and flat state. S2. Reverse contact positioning: The mechanical drill bit is fed from the reverse side of the PCB board toward the predetermined drilling position until the tip of the mechanical drill bit contacts the reverse side of the PCB board, generating a processing trigger signal; S3. Front laser irradiation: In response to the processing trigger signal, the laser processing device located on the front of the PCB board is coaxially aligned with the mechanical drill bit and performs laser irradiation in sequence; S4. Reverse drilling: After laser irradiation, the mechanical drill bit continues to advance axially and completes through drilling within the closed area defined by the predetermined drilling position.
[0006] In one feasible implementation method, the pre-tension is implemented by: inserting the PCB board between the main clamping plate and the movable clamping plate, and adjusting the spacing between the corresponding first clamping piece and the first clamping cover, the second clamping piece and the second clamping cover by rotating the bolts to complete the clamping. If the PCB board has a large mass, the pre-tension can be adjusted.
[0007] In one feasible implementation method, the method for changing the preload is as follows: rotate the movable counterweight block, adjust the position of the movable counterweight block on the rotating rod, and fix it after the preload requirement is met.
[0008] In one feasible implementation, in step S2, the processing trigger signal is generated in any one or a combination of the following ways: The axial contact pressure was detected to have reached a preset threshold by a piezoelectric force sensor located at the rear end of the mechanical drill bit. The mechanical drill bit is detected to cause a preset micro-deformation of the PCB board.
[0009] In one feasible implementation, the laser irradiation includes: First stage laser irradiation: The first laser is aimed at the predetermined drilling position and irradiated to locally heat and soften the resin substrate inside the PCB board. Second stage laser irradiation: A second laser scans along the edge contour of the predetermined drilling position to induce the formation of closed thermal stress microcrack rings or annular microgrooves on the copper foil layer on the front side of the PCB board.
[0010] In one feasible implementation method, the method for detecting the preset micro-deformation is as follows: The laser processing device outputs two probe lasers that are symmetrically incident at a preset angle, so that the focal points of the two probe lasers converge at the center of the predetermined drilling position on the front side of the PCB board. When the mechanical drill bit is not in contact, the two probe laser beams projected onto the PCB board overlap to form a single spot. When the tip of the mechanical drill bit contacts the predetermined drilling position and generates a micro-bulge off the surface, the two probe laser beams are misaligned on the PCB board. When the photoelectric detection module detects that the center-to-center distance between the probe laser spot and the PCB board reaches a preset threshold, it outputs the processing trigger signal.
[0011] In one feasible implementation, the effective irradiation area of the first laser on the front side of the PCB board is a concentric circular region coaxially arranged with the predetermined drilling position: the diameter of the concentric circular region is... The diameter of the hole at the predetermined drilling position is Then the following conditions are met: .
[0012] In one feasible implementation, step S4, the axial advance of the mechanical drill bit includes segmented feed control: When penetrating the softened resin layer on the reverse side of the PCB board, the mechanical drill bit operates at a first feed rate. Advance; When the cutting edge of the mechanical drill bit approaches the copper foil layer on the front side of the PCB board, the feed speed is reduced to the second feed speed. Complete the piercing strike.
[0013] In one feasible implementation, the second feed rate The first feed rate of .
[0014] In one feasible implementation method, while the mechanical drill bit completes the through drilling in step S4, the copper foil fragments and cutting debris that have fallen off along the microcrack ring or the annular microgroove are simultaneously removed by a negative pressure adsorption device set on the front side of the PCB board.
[0015] The beneficial effects of this invention are as follows: 1. By applying appropriate in-plane prestress to the PCB board before processing, the defects in the board's own bending stiffness are effectively reduced, and the off-plane stress chatter and substrate cracking during reverse drilling feed are suppressed. At the same time, the surface copper foil that maintains tension, together with the thermal stress microcrack ring pre-fabricated by the second stage laser, synergistically promotes the shearing and crushing of the copper foil in the hole by the drill tip cutting edge and neat shedding, completely blocking the transmission of cutting shearing torque to the continuous copper foil around the hole, and effectively reducing the tearing and peeling rate of the front copper foil. 2. The frontal laser irradiation is divided into a first stage of local softening and a second stage of microcrack blocking: In the first stage, the insulating medium in the hole core area is softened and heated in advance by micro-energy ultraviolet laser irradiation, which reduces the axial extrusion resistance of the mechanical drill bit and reduces the feed thrust; In the second stage, microcrack rings are rapidly induced only along the hole edge contour, and the depth of hole wall carbonization and thermal damage is small, which effectively ensures the electrical insulation performance of high-frequency and high-speed lines. 3. In the mechanical drilling stage, the present invention adopts differentiated segmented speed control: when cutting into the reverse side and penetrating the softened medium layer, the first feed speed is used to advance at high speed, which ensures the material removal efficiency; when the cutting edge is about to penetrate the copper foil on the front surface, the servo system actively and smoothly decelerates to the second feed speed, avoiding the instantaneous release of the elastic deformation energy accumulated in the ultra-thin plate, which causes the surface rebound chatter and impact, and effectively promotes the smooth hole wall without edge burrs. Attached Figure Description
[0016] The present invention will now be described in further detail with reference to the accompanying drawings and specific implementation methods.
[0017] Figure 1 This is a three-dimensional structural diagram of the prestressing device of the present invention; Figure 2 This is a second-view three-dimensional structural diagram of the pre-tensioning device of the present invention; Figure 3 This is the first schematic diagram of the edge contour trajectory of the present invention; Figure 4 This is the second schematic diagram of the edge contour trajectory of the present invention; Figure 5 This is the third schematic diagram of the edge contour trajectory of the present invention; Figure 6 This is a schematic diagram of the laser processing device outputting the detection laser of the present invention; Figure 7 This is the second schematic diagram of the laser processing device outputting the detection laser of the present invention; Figure 8 This is a schematic diagram illustrating the implementation process of the present invention.
[0018] Reference numerals: 1. Foundation; 12. Support column; 13. Through-drill groove; 21. First clamping piece; 22. First clamping cover; 23. Bolt; 31. Second clamping piece; 32. Second clamping cover; 33. Shaft support rod; 34. Rotating shaft; 341. Rotating ring; 342. Engaging thread; 343. Rotating rod; 344. Counterweight movable block; 35. Lever; 36. Thrust lever; 37. Moving guide rail; 371. Guide rail groove; 5. Predetermined drilling position; 6. Edge contour; 71. Micro-cut hole; 72. Annular micro-cut groove; 73. Thermal stress micro-crack ring; 8. PCB board; 9. Mechanical drill bit; 91. Detection laser. Detailed Implementation
[0019] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only for explaining the invention and are not intended to limit the invention; that is, the described embodiments are merely some embodiments of the invention, and not all embodiments. The components of the embodiments of the invention described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.
[0020] Therefore, the following detailed description of the embodiments of the invention provided in the accompanying drawings is not intended to limit the scope of the claimed invention, but merely to illustrate selected embodiments of the invention. All other embodiments obtained by those skilled in the art based on the embodiments of the invention without inventive effort are within the scope of protection of the invention.
[0021] The following is combined with Figure 1-8 To illustrate the specific embodiments of the present invention, in the prior art, drilling of PCB board material 8 is usually carried out by laser melting or mechanical drilling. The above methods are convenient to use and are common technical means. However, when drilling larger diameter holes in ultra-thin PCB board material 8, the above methods all have some limitations: When using mechanical drilling to drill ultra-thin PCB board 8, the axial thrust and cutting resistance during drill bit entry and top-end can easily cause local elastic bending and chattering of the board, inducing micro-cracks or breakage of the board. At the same time, the copper foil attached to the ultra-thin PCB board 8 is relatively thin, and the interface between it and the resin dielectric layer is also relatively weak. If a large-diameter drill bit is used to cut the front copper foil, the shearing torque and axial force will cause the front copper foil to tear laterally, causing some copper foil to be lifted and the hole edge to delaminate. If laser melting is used, the processing cycle is significantly longer when laser removes material with a larger aperture. The heat dissipation channel of the ultra-thin board is narrow, and the continuous high-energy heat accumulation can easily lead to overall thermal warping of the ultra-thin board and carbonization of the substrate around the hole wall, affecting the service life of the PCB board.
[0022] To address the technical challenges of laser melting or mechanical drilling when drilling large-diameter holes in ultra-thin PCB boards, a combined laser and mechanical drilling method is proposed, comprising the following steps: S1. Board tensioning and clamping: The PCB board 8 to be processed is clamped in the pre-tensioning device. Specifically, the pre-tensioning device can be a device that realizes planar tensioning of the PCB board 8. It is existing technology and is usually a test tool for tensioning or yielding of tension. It is sufficient to realize the function of generating pre-tensioning force in the above-mentioned planar tensioning, so it will not be described in detail. The pre-tensioning device applies planar bidirectional or unidirectional in-plane pre-tensioning stress to the PCB board 8 to keep the PCB board 8 in a tensioned and flat state, thereby suppressing out-of-plane buckling during drilling impact and avoiding plastic deformation of the board. S2. Reverse contact positioning: The mechanical drill bit 9 is fed from the reverse side of the PCB board 8 toward the predetermined drilling position 5 until the tip of the mechanical drill bit 9 contacts the reverse side of the PCB board 8, generating a processing trigger signal; S3. Front laser irradiation: In response to the processing trigger signal, the laser processing device set on the front of the PCB board 8 and the mechanical drill bit 9 are aligned coaxially and perform laser irradiation in sequence; S4. Reverse drilling: After laser irradiation, the mechanical drill bit 9 continues to advance along the axial direction and completes through drilling within the closed area defined by the predetermined drilling position 5.
[0023] The underlying hardware structure, optical path system, servo feed and underlying electrical control mechanism, and photoelectric detection module of the reverse mechanical drill bit 9 drive mechanism and the front laser processing device involved in the above and below embodiments are all existing mature and well-known technologies in the fields of printed circuit boards and precision laser micromachining. Those skilled in the art can fully implement them based on the scheme disclosed in this invention and in combination with existing general commercial equipment.
[0024] In one embodiment, a preferred pre-tensioning device is provided, specifically including a support platform 1, a main clamping plate, a movable clamping plate, and a thrust member; the support platform 1 is provided with a plurality of support columns 12, and the main clamping plate is placed in the middle of the plurality of support columns 12, the specific number depending on the actual use. The attached drawing shows two sets symmetrically arranged, with the movable clamping plate arranged parallel to the main clamping plate. The support platform 1 also has a through-drill groove 13 to facilitate the passage of a mechanical drill bit 9. The drill bit can directly abut the bottom of the PCB board 8 through the through-drill groove 13. The main clamping plate includes a first clamping piece 21 and a first clamping cover 22. The first clamping piece 21 is fixed. The first clamp 22 is connected to the support column 12 and is slidably connected through the support column 12. The first clamp 21 and the first clamp 22 are adjusted by bolts 23. The movable clamp includes a second clamp 31 and a second clamp 32, which are also adjusted by bolts 23. Several movable guide rails 37 are provided below the second clamp 31. The second clamp 31 is provided with a protrusion that can slide in conjunction with the guide rail groove 371 on the movable guide rail 37. One end of the movable guide rail 37 is fixed to the adjacent support column 12. The thrust member is used to guide the movable clamp in the length direction of the movable guide rail 37 to adjust the distance between it and the main clamp. The thrust component includes a rotating shaft 34, a rotating ring 341 sleeved in the middle of the rotating shaft 34, a lever 35 and a rotating rod 343 on the rotating ring 341, the length directions of the lever 35 and the rotating rod 343 intersect the central axis of the rotating ring 341 and are not collinear, a thrust plate 36 is provided on the side of the second clamp 31 near the lever 35, the thrust plate 36 is abutted by the lever 35 on the side facing the support column 12, the rotating rod 343 is provided with a meshing thread 342 in the middle, and a counterweight movable block 344 is provided on the rotating rod 343 to mesh with and thread the meshing thread 342, and the two ends of the rotating shaft 34 are fixed to the middle of the adjacent support column 12 by shaft support rods 33.
[0025] In implementation, firstly, the PCB board 8 is inserted between the main clamping plate and the movable clamping plate. The spacing between the corresponding first clamping piece 21 and first clamping cover 22, and the second clamping piece 31 and second clamping cover 32, is adjusted using bolts 23 to fix both ends of the PCB board 8. Then, the counterweight movable block 344 is rotated to adjust its position on the rotating rod 343. During adjustment, the rotating rod 343 drives the lever 35 to move the push plate 36 and the movable clamping plate. However, since the movable clamping plate is directly connected to the main clamping plate via the PCB board 8, a component of the weight of the counterweight movable block 344 pushes the movable clamping plate away from the main clamping plate, thus generating a certain pre-tension force on the PCB board 8. Simultaneously, the rotating counterweight movable block 344 can be guided by the meshing thread 342 to adjust the distance between the counterweight movable block 344 and the rotating shaft 34, thereby controlling the center of gravity of the meshing thread 342 and the counterweight movable block 344. The change in the center of gravity effectively affects the torque of the component force of the counterweight movable block 344 on the lever 35, thereby controlling the pre-tension force of the main clamping plate and the movable clamping plate on the PCB board 8. Specifically, during the drilling process of the PCB board 8 by the mechanical drill bit 9, since the main clamping plate and the movable clamping plate fixing both ends of the PCB board 8 will not produce Z-axis displacement, and the force transmission path is relatively long, even if the mechanical drill bit 9 generates a pushing force on the PCB board 8, it will not have a significant impact on the pre-tension force.
[0026] In one embodiment, to adapt to different PCB board material structures and thus generate a processing trigger signal, the following method is used, and the processing trigger signal is generated in any one or a combination of the following ways: The axial contact pressure was detected to reach a preset threshold by a piezoelectric force sensor located at the rear end of the mechanical drill bit 9. Specifically, because some thin PCB boards 8 contain different components or reinforcing fibers, the PCB board 8 has high hardness. The piezoelectric force sensor can be directly affected by the board on the mechanical rotating head, and can be triggered by mechanical contact. The response time is in the microsecond range, and it can be captured at the moment the drill tip touches the reverse side. Moreover, it does not require any electrical signal to be applied to the board itself, and has strong versatility.
[0027] A closed microcurrent loop was constructed between the mechanical drill bit 9 and the conductive layer on the reverse side of the PCB board 8, and a loop conduction signal was detected. The system detects that the mechanical drill bit 9 has reached the preset reverse coordinate or that the PCB board 8 has generated a preset micro-deformation.
[0028] If the thin PCB board 8 is made of flexible material, its mechanical drill bit 9 can produce a slight deformation upon contact, which can be effectively utilized. At the same time, some boards are high-end carrier boards that are strictly prohibited from using the electrical circuit method to make electrical contact micro-marks. The mechanical drill bit 9 is used to detect the PCB board 8 to produce a preset slight out-of-plane deformation, without occupying the complex drilling and milling space on the reverse side.
[0029] Specifically, the detection methods and techniques for pre-defined minute out-of-plane deformation are described in detail below: See attached document Figure 6 , 7 As shown, two probe lasers 91 are output from the laser processing device and incident symmetrically at a preset angle, so that the focal points of the two probe lasers 91 converge at the center of the predetermined drilling position 5 on the front side of the PCB board 8. When the reverse mechanical drill bit 9 is not in contact with the PCB board 8, the front surface of the PCB board 8 is in the initial plane. The two probe lasers 91 intersect and overlap on the front surface of the PCB board 8. The photoelectric detection module, which is coaxially configured on the front, collects a concentrated single spot. Specifically, the photoelectric detection module is set in the laser processing device, which is also existing technology, so it will not be described in detail. When the reverse mechanical drill bit 9 feeds at a micro-speed along the Z-axis and contacts the reverse side of the PCB board 8, a small axial thrust causes the ultra-thin PCB board 8 with low stiffness to produce an elastic, slightly raised surface in the predetermined drilling micro-area. The increase in the height of the surface causes the actual interception point of the two obliquely incident probe lasers 91 on the front surface of the PCB board 8 to shift in the horizontal direction; The photoelectric detection module acquires images of the light spot in real time and monitors its status. When the light spot morphology is detected to split from a single peak to a double peak and the center distance between the two light spots reaches a preset threshold, it is determined that the reverse mechanical drill bit 9 has made contact. The main control system immediately outputs a hardware-level processing trigger signal to start the first stage of laser irradiation on the front side. The advantage of the above method is that conventional single-beam laser reflection ranging methods rely on the absolute position of the reflected spot on the receiver. However, the misalignment between the copper foil on the surface of the ultra-thin PCB board 8 and the board itself can easily lead to distortion of the single-point reflected spot, causing misjudgment. This method, because its criterion is based on the relative separation distance between the two spots rather than their absolute coordinates, significantly reduces the adverse effects of the micro-roughness and uneven reflective properties of the PCB board 8 surface on triggering stability.
[0030] Specifically, when machining relatively large-diameter through holes on ultra-thin PCB boards, the front-side laser irradiation process is divided into two independent, sequential control processes: localized heat softening and thermal stress-induced micro-cracks. These are elaborated below. In the first stage of laser irradiation, in response to the processing trigger signal, the laser processing device rapidly increases its energy from an ultra-low power detection state, and uses the first laser processing parameters to irradiate the predetermined drilling position, causing the resin in the predetermined drilling core area to heat up; specifically, this can be achieved by using extremely low single-pulse energy density, high repetition frequency, and short duration, so that the cumulative injection energy per hole is controlled within a certain range. The micro-heat range causes a significant reduction in local hardness and shear resistance, resulting in a decrease in the shear yield strength of the drilling area and the formation of local strength differences. The second stage of laser irradiation involves scanning along the edge contour of the predetermined drilling location with a second laser to induce the formation of closed thermal stress microcracks or annular microgrooves on the copper foil layer on the front side of the PCB board. Specifically, this is achieved by switching to a focused micro-spot, significantly increasing the single-pulse energy density. At the same time, the repetition frequency was reduced to To obtain a higher single-pulse peak power density ( ); By guiding the micro-spot along the edge contour trajectory of the predetermined drilling position (diameter is...) Perform high-speed dot matrix overlap scanning or ring scanning on the circular edge (see attached diagram). Figure 3 , 4 5. Microcracks can be categorized into annular microgrooves, circumferential array microcracks, thermal stress microcracks, and annular microcracks. For example, micro-hole circumferential array microcracks (with high array density; the attached diagram uses a suggested drawing method to illustrate the implementation process) can be adaptively adjusted according to the PCB board hardness and copper foil thickness. Specifically, due to the influence of pre-tension on the PCB board in its initial state, the elastic strength of its resin area and copper foil differs. When irradiated by the second-stage laser, the cracks promote the natural pyrolysis of the copper foil between the irradiated areas. Even if it is not completely irradiated into a ring, the effect of natural pyrolysis into a ring can still be achieved. This method also solves the problem of low rate in high-energy laser irradiation in the second stage.
[0031] Beneficially, the effective irradiation area of the first laser on the front side of the PCB board is a concentric circular area coaxial with the predetermined drilling position: the diameter of the concentric circular area is... The diameter of the hole at the predetermined drilling position is Then the following conditions are met: Since the energy transmitted by the laser irradiation in the first stage has a marginal decrease effect in the PCB board, the heating area is fixed inside the final drilling outline to avoid excessive heat diffusion to the normal insulating dielectric layer outside the finished hole wall, and to prevent thermal degradation, carbonization or peel strength degradation of the resin around the hole. Beneficially, in step S4, while the mechanical drill bit 9 completes the through drilling, the copper foil fragments and cutting debris that fall off along the microcrack ring or annular microgroove 72 are simultaneously removed by the negative pressure adsorption device set on the front side of the PCB board 8. Specifically, the negative pressure adsorption device is a traditional garbage suction device, including but not limited to a vacuum cleaner, which can remove the above-mentioned residual structure. It is existing technology and will not be described in detail.
[0032] In one embodiment, a method for adjusting the drilling rate to effectively suppress PCB board board 8 vibration is also provided, including step S4, in which the axial advance of the mechanical drill bit 9 includes segmented feed control: When penetrating the softened resin layer on the reverse side of the PCB board, the mechanical drill bit operates at the first feed rate. Advancement; During the initial drilling entry stage, the reverse resin medium layer has been locally softened by the first-stage laser irradiation, reducing cutting resistance. At this point, the mechanical drill bit adopts a higher initial feed rate. The propulsion mechanism can cut and penetrate most of the material inside the hole in a short time. When the cutting edge of the mechanical drill bit approaches the copper foil layer on the front side of the PCB board, the feed rate is reduced to the second feed rate. To complete the penetration, specifically, the second feed rate... First feed rate of As the mechanical drill bit is about to penetrate the front surface and exit, the axial cutting reaction force on the drill tip disappears. The elastic deformation energy accumulated by the previous axial pressure on the ultra-thin PCB board is released in a concentrated manner, inducing the board to spring back along the thickness direction and mechanical impact. This can easily cause the substrate at the hole edge to break or scratch. By actively reducing the feed rate to a lower second feed rate when the cutting edge approaches the front copper foil, the problem can be mitigated. This effectively mitigates the aforementioned issues; combined with the thermal stress microcrack ring or annular microgroove induced by the front, the mechanical drill bit operates at a lower second feed rate. The cutting edge is rotated and moves at a low speed across the closed area defined by the microcrack ring, causing the residual copper foil sheet inside the hole to fall off along the boundary of the pre-made microcrack, effectively solving the technical problem of irregular plastic flanging of the local copper foil edge.
[0033] The industry-standard ultra-thin copper-clad laminate is selected, with a total nominal thickness of [missing information]. (The front surface is the thickness) The electrolytic copper foil layer, with a thickness of approximately [thickness missing] on the inside and back. (For insulating dielectric substrates), the target through-hole diameter is set to the standard hole diameter. (The ratio of aperture to plate thickness is approximately) Based on the laser-mechanical composite drilling method provided above, output the following: Example 1: The pre-tensioning device is used to apply in-plane pre-tension stress to the PCB board 8. The specific in-plane pre-tension stress is 3.0 MPa. The mechanical drill bit 9 feeds at a low speed toward the reverse side of the PCB board 8, with a cutting edge outer diameter of 0.40 mm. The front dual-probe laser 91 detects a separation gap of 2.0 μm on the front surface and outputs a hardware processing trigger signal. The system outputs two-stage laser irradiation: the first stage uses a first laser to irradiate the predetermined drilling position 5 concentrically, causing localized heating and softening of the insulating dielectric substrate inside the PCB board 8; the second stage uses a second laser to perform dot matrix scanning along the edge contour 6 of the predetermined drilling position 5, inducing the formation of thermal stress microcrack rings 73 on the copper foil layer on the front side of the PCB board 8; then, the mechanical drill bit 9 is driven to perform segmented feed drilling at a spindle speed of 200,000 rpm; when cutting into the substrate and softened area from the reverse side, the mechanical drill bit 9 advances at a first feed speed of 30 mm / s; when the drill tip of the mechanical drill bit 9 approaches the copper foil on the front surface, the feed is decelerated, and the feed speed is reduced to a second feed speed of 12 mm / s to complete the cutting; the front negative pressure adsorption device is activated to simultaneously remove the detached copper fragments and cutting debris.
[0034] The specific process control for the two-stage laser irradiation is as follows: The first stage laser irradiation uses a solid-state ultraviolet laser with a wavelength of 355nm and a single-pulse energy density of 0.09 J / cm². 2 The first stage involved a repetition frequency of 150 kHz, an irradiation duration of 1.0 ms, a cumulative injection energy of 2.5 mJ per hole, and an effective concentric circle diameter of 0.30 mm, which softened the resin in the hole core and raised its temperature to 80℃~100℃. The second stage of laser irradiation switched to a focused micro-spot with a spot diameter of 20 μm and a single-pulse energy density of 3.2 J / cm². 2 The repetition frequency is 30 kHz, and the peak power density is greater than 10. 7 W / cm 2 The high-speed galvanometer performs rapid dot matrix scanning along an edge trajectory with a diameter of 0.40 mm.
[0035] This embodiment employs a coordinated approach of standard in-plane pre-stress, two-stage laser graded control, and reverse mechanical segmented speed-changing feed. It utilizes pre-tension to enhance the rigidity of the thin plate and provide kinetic energy for the auxiliary cracking of copper foil. The first stage laser softens the PCB board material 8, and the second stage laser pre-fabricates the fractured copper layer. Combined with the end deceleration blade, it effectively solves the technical problems of copper foil lifting, board chatter, and thermal carbonization conflicting in the processing of large-diameter ultra-thin boards.
[0036] Example 2: Using the pre-tensioning device, an in-plane pre-tension stress is applied to the ultra-thin copper-clad laminate by rotating and adjusting the counterweight movable block 344. The specific in-plane pre-tension stress is 4.0 MPa. The mechanical drill bit 9 feeds at a low speed toward the reverse side of the PCB board 8, with a cutting edge outer diameter of 0.45 mm. A piezoelectric force sensor located at the rear end of the drill bit 9 detects an axial contact pressure of 0.15 N and outputs a hardware processing trigger signal. It then outputs a two-stage laser irradiation: the first stage uses a first laser to irradiate the predetermined drilling position 5 concentrically, causing localized heating and softening of the insulating substrate inside the PCB board 8; the second stage uses a second laser to perform annular microgroove 72 array scanning along the edge contour 6 of the predetermined drilling position 5, inducing the formation of discontinuous microgroove closed loops on the copper foil layer on the front side of the PCB board 8. Afterwards, the mechanical drill bit 9 is driven to perform segmented drilling, with a spindle speed of 200,000 rpm. When cutting into the substrate and softened area from the reverse side, the mechanical drill bit 9 advances at a first feed rate of 25 mm / s; when the drill tip cutting edge approaches the copper foil on the front surface, the feed rate decreases to a second feed rate of 10 mm / s. Complete the micro-stress cutting process; activate the front negative pressure adsorption device to simultaneously remove chips.
[0037] The specific process control for the two-stage laser irradiation is as follows: The first stage laser irradiation uses a solid-state ultraviolet laser with a wavelength of 355nm and a single-pulse energy density of 0.10 J / cm². 2 The repetition frequency was 150 kHz, the irradiation duration was 1.2 ms, and the effective concentric circle diameter was 0.36 mm; the second stage of laser irradiation switched to a focused micro-spot with a single pulse energy density of 3.5 J / cm². 2 With a repetition frequency of 30 kHz, a multi-segment micro-arc slot array scan is performed by a high-speed galvanometer along an edge trajectory with a diameter of 0.45 mm at a speed of 600 mm / s, so that the gaps between each slot segment can be spontaneously extended and connected under the action of prestress.
[0038] Compared to Example 1, this embodiment adjusts the pretension and triggering method for the PCB board 8 structure containing reinforced high-hardness glass fiber / filler, and uses piezoelectric force sensing to directly capture micro-mechanical contact force. It also adopts annular microgrooves 72 to deal with thick copper foil and high-modulus substrate, which enhances the process adaptability to boards with high hardness and large bending resistance. Even under the condition of slightly increased hole diameter, it still maintains excellent hole wall quality and low defect rate.
[0039] In Example 3, the pre-tensioning device is used to apply in-plane pre-tension stress to the PCB board 8 by rotating and adjusting the counterweight movable block 344. The specific in-plane pre-tension stress is 3.0 MPa. The mechanical drill bit 9 feeds at a low speed toward the reverse side of the PCB board 8, with a cutting edge outer diameter of 0.40 mm. The front dual-probe laser 91 detects a separation gap of 2.0 μm on the front surface and outputs a hardware processing trigger signal. It outputs two-stage laser irradiation: the first stage laser irradiation uses the first laser to irradiate the concentric inner surface of the predetermined drilling position 5, softening the concentric circle diameter and adjusting it to the upper limit boundary value; the second stage laser irradiation uses the second laser to perform dot matrix scanning along the edge contour 6 of the predetermined drilling position 5, inducing the formation of a closed thermal stress microcrack ring 73; then, the mechanical drill bit 9 is driven to feed and drill in segments, with a first feed speed of 30 mm / s, which is reduced to a second feed speed of 12 mm / s before the drill bit exits; the front negative pressure adsorption device is activated to remove chips synchronously.
[0040] The specific process control for the two-stage laser irradiation is as follows: In the first stage of laser irradiation, the diameter of the effective concentric circle is increased and adjusted to 0.35 mm, and the energy density of the remaining single pulses is 0.09 J / cm². 2 The repetition frequency of 150 kHz and the duration of 1.0 ms remained unchanged; the laser irradiation parameters for the second stage were the same as in Example 1.
[0041] Compared to Example 1, this embodiment verifies the process tolerance when the softened region in the first stage is at the high boundary. The experiment shows that increasing the softening diameter can further reduce the mechanical propulsion resistance on the reverse side, but because the softening boundary is close to the hole edge, the thermal diffusion effect of the insulating medium around the hole wall increases slightly, and the carbonization depth increases slightly.
[0042] Comparative Example 1: The PCB board 8 is clamped on the worktable in a normal horizontal position without tension. The reverse mechanical drill bit 9 is fed at a microspeed toward the predetermined drilling position 5, with an outer diameter of 0.40 mm for the cutting edge. A trigger signal is output by detecting micro-bulges through the intersection of dual beams. The output is exactly the same as the two-stage laser irradiation in Example 1, wherein the second stage laser still uses a dot matrix discrete pulse scanning; then the mechanical drill bit 9 is driven to cut in at a first feed speed of 30 mm / s, and the speed is reduced to a second feed speed of 12 mm / s before the drill bit is withdrawn; the front negative pressure adsorption device is turned on to pick up the chips.
[0043] Compared to Example 1, this comparative example omits the step of applying in-plane prestress. Because the thin plate is in a relaxed, free state, its equivalent bending stiffness is insufficient, resulting in significant out-of-plane flutter during reverse mechanical feeding. Simultaneously, due to the lack of tensile potential energy from the in-plane prestress field, the tips of the micro-holes in the second-stage laser cannot spontaneously extend and connect into a closed loop, causing localized tearing of the copper foil at the hole edge during mechanical shearing, and extending processing time.
[0044] Comparative Example 2: The pre-tensioning device is used to apply an in-plane pre-tension stress of 3.0 MPa to the PCB board 8; the reverse mechanical drill bit 9 feeds into the reverse side and triggers. The first stage of laser local softening irradiation in step S3 is omitted. The second stage high-energy laser is directly used to scan and induce the formation of thermal stress microcrack ring 73 along the edge contour 6 of the predetermined drilling position 5. Then, the mechanical drill bit 9 is driven to advance from the reverse side at the first feed speed of 30 mm / s. When it approaches the front side, the speed is reduced to 12 mm / s and the drill bit is removed. The negative pressure chip removal on the front side is activated.
[0045] The specific process control for laser irradiation is as follows: Upon triggering, the second stage of laser irradiation is directly initiated, using a focused micro-spot with a spot diameter of 20 μm and a single-pulse energy density of 3.2 J / cm². 2 The high-speed dot matrix scanning was performed at 800 mm / s along an edge trajectory with a diameter of 0.40 mm at a repetition frequency of 30 kHz; no preheating or softening treatment was performed on the resin inside the pores.
[0046] Compared to Example 1, this comparative example omits the first-stage local softening pretreatment of the resin substrate. During the cutting process, the central chisel edge of the reverse-side mechanical drill bit 9 directly pushes against the room-temperature, high-hardness resin medium, increasing cutting resistance and axial reaction force. This results in the ultra-thin sheet material experiencing excessive axial compressive load during cutting, causing localized vibration.
[0047] Comparative Example 3: The pre-tensioning device described above applies an in-plane pre-tension stress of 3.0 MPa to the PCB board 8; the reverse mechanical drill bit 9 feeds into the reverse side and triggers the feed. The first stage of resin softening and the second stage of copper foil microcrack scanning are performed sequentially. In step S4, the mechanical drill bit 9 maintains a constant high-speed feed of 30 mm / s throughout the entire process of cutting into the resin medium from the reverse side and penetrating the front copper foil, omitting the deceleration process when approaching the front copper foil. Turn on the front negative pressure chip removal.
[0048] The specific process control for the two-stage laser irradiation is completely consistent with that in Example 1.
[0049] Compared to Example 1, this comparative example did not implement segmented speed reduction control during the mechanical cutting phase. At the instant the mechanical drill bit 9 was about to penetrate the surface, the axial cutting resistance at the front end disappeared, resulting in instantaneous mechanical unloading. The previously elastic deformation energy of the PCB board 8 was released instantaneously, inducing rebound chatter and mechanical impact, causing micro-fracture of the substrate at the hole edge, and the edges of the detached copper sheet were rough with slight burrs.
[0050] Based on the above embodiments and the median values from multiple comparative implementations, the following implementation process record table can be obtained:
[0051] Comparing Example 1 and Comparative Example 1, it can be seen that when the in-plane prestressing in step S1 is omitted, the PCB board 8 lacks rigid constraints and is prone to out-of-plane bending chatter under the axial force of reverse drilling, resulting in a significant increase in the substrate chattering and breakage rate from Example 1 to 5.8%. Simultaneously, due to the lack of in-plane tensile prestress, the difficulty of laser-induced micro-notches in the second stage increases, leading to a dramatic increase in the front copper foil tearing rate from 0.2% to 7.6%. This indicates that an in-plane prestress of 3.0 MPa can effectively improve the equivalent out-of-plane stiffness of the PCB board 8. When the mechanical drill bit 9 cuts, the tensioned copper foil rapidly concentrates the cutting force and converts it into pure shear stress. This, combined with the micro-crack ring, promotes the shearing and neat shearing of the copper layer by the drill bit, preventing the transmission of cutting stress to the copper foil around the hole. Comparing Example 1 and Comparative Example 2, it can be seen that when the first stage of laser concentric retraction softening irradiation in step S3 is omitted, the central transverse cutting edge of the mechanical drill bit 9 directly cuts into the room-temperature high-modulus insulating substrate, and the axial extrusion reaction force of the drill bit increases sharply. The local elasticity of the plate causes the substrate chattering and cracking rate to rise significantly to 5.2%; the incidence of peeling and tearing of the surrounding copper foil when the drill bit breaks the copper layer rebounds to 3.4%. Example 1 softens and heats the substrate inside the hole core, reducing the axial extrusion resistance and suppressing extrusion damage and drilling chatter. Comparing Example 1 and Comparative Example 3, it can be seen that when step S4 uses a constant high-speed feed of 30 mm / s throughout without deceleration, the accumulated elastic deformation energy of the drill tip is released instantaneously just before penetrating the front single-layer copper foil, inducing high-frequency rebound and impact, causing the substrate fracture rate to rise to 4.4%. Furthermore, the violent impact of the high-speed cutter significantly increases the incidence of the drill bit breaking the copper layer and causing the surrounding copper foil to peel and tear, reaching 5.8%. Example 1 reduces the feed speed to the second feed speed when the cutter approaches the front copper foil. This effectively suppressed the vibration during the cutting tool's upward thrust. As shown in Examples 2 and 3, for ultra-thin plates containing high-hardness reinforcing phases, appropriately increasing the prestress and reducing the cutting speed still maintained an extremely low copper foil peeling and tearing rate of 0.4% and an extremely low substrate chipping rate of 0.2% even with a relatively large hole diameter of 0.45 mm. When the first-stage softening diameter was relaxed to the upper limit, although the hole wall thermal damage depth slightly increased to 4.8 mm... However, the tearing rate and breakage rate remained at extremely low levels, proving that the method of the present invention has good stability and applicability in different material systems and process tolerance ranges.
[0052] In the description of this invention, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal communication between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0053] The above description is merely an example and illustration of the structure of the present invention. Those skilled in the art can make various modifications or additions to the specific embodiments described or use similar methods to replace them, as long as they do not deviate from the structure of the invention or the scope defined by the claims of the present invention, they should all fall within the protection scope of the present invention.
Claims
1. A laser-mechanical composite drilling method for ultra-thin PCBs, characterized in that, Includes the following steps: S1. Board tensioning and clamping: The PCB board (8) to be processed is clamped in a pre-tensioning device to generate pre-tension. The pre-tensioning device applies in-plane pre-tension stress to the PCB board (8) in two directions or one direction to keep the PCB board (8) in a tensioned and flat state. S2. Reverse contact positioning: The mechanical drill bit (9) is fed from the reverse side of the PCB board (8) toward the predetermined drilling position (5) until the tip of the mechanical drill bit (9) contacts the reverse side of the PCB board (8) and a processing trigger signal is generated; S3. Front laser irradiation: In response to the processing trigger signal, the laser processing device located on the front of the PCB board (8) is coaxially aligned with the mechanical drill bit (9) and performs laser irradiation in sequence; S4. Reverse drilling: After laser irradiation, the mechanical drill bit (9) continues to advance along the axial direction and completes through drilling within the closed area defined by the predetermined drilling position (5).
2. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 1, characterized in that: The method for implementing the pre-tension is as follows: insert the PCB board 8 between the main clamping plate and the movable clamping plate, and adjust the distance between the corresponding first clamping piece 21 and first clamping cover 22, second clamping piece 31 and second clamping cover 32 by rotating the bolt 23 to complete the clamping. If the mass of the PCB board is large, the pre-tension can be adjusted.
3. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 2, characterized in that: The method for changing the preload is as follows: rotate the counterweight movable block 344, adjust the position of the counterweight movable block 344 on the rotating rod 343, and fix it after the preload requirement.
4. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 1, characterized in that: In step S2, the processing trigger signal is generated in any one or a combination of the following ways: The axial contact pressure reached a preset threshold was detected by a piezoelectric force sensor located at the rear end of the mechanical drill bit (9); The mechanical drill bit (9) is detected to cause a preset micro-deformation of the PCB board (8).
5. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 1, characterized in that: The laser irradiation includes: First stage laser irradiation: The first laser is aimed at the predetermined drilling position (5) and irradiated to locally heat and soften the resin substrate inside the PCB board (8); Second stage laser irradiation: The second laser scans along the edge contour (6) of the predetermined drilling position (5) to induce the formation of closed thermal stress microcrack rings (73) or annular microgrooves (72) on the copper foil layer on the front side of the PCB board (8).
6. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 4, characterized in that: The method for detecting the preset micro-deformation is as follows: Two probe lasers (91) are output from the laser processing device and incident symmetrically at a preset angle, so that the focal points of the two probe lasers (91) converge at the center of the predetermined drilling position (5) on the front side of the PCB board (8). When the mechanical drill bit (9) is not in contact, the two beams of the detection laser (91) projected onto the PCB board (8) coincide to form a single beam. When the tip of the mechanical drill bit (9) contacts the predetermined drilling position (5) and produces a micro-bulge off the surface, the two probe lasers (91) are misaligned on the PCB board (8); When the center-to-center distance between the probe laser (91) and the PCB board (8) reaches a preset threshold, the processing trigger signal is output by the photoelectric detection module.
7. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 5, characterized in that: The effective irradiation area of the first laser on the front side of the PCB board is a concentric circular region coaxial with the predetermined drilling position: the diameter of the concentric circular region is The diameter of the hole at the predetermined drilling position is Then the following conditions are met: .
8. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 7, characterized in that: In step S4, the axial advance of the mechanical drill bit (9) includes segmented feed control: When penetrating the softened resin layer on the reverse side of the PCB board, the mechanical drill bit operates at a first feed rate. Advance; When the cutting edge of the mechanical drill bit approaches the copper foil layer on the front side of the PCB board, the feed speed is reduced to the second feed speed. Complete the piercing strike.
9. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 8, characterized in that: Second feed rate The first feed rate of .
10. The laser-mechanical composite drilling method for ultra-thin PCBs according to claim 9, characterized in that: In step S4, while the mechanical drill bit (9) completes the through drilling, the copper foil fragments and cutting debris that fall off along the microcrack ring or the annular microgroove (72) are simultaneously removed by the negative pressure adsorption device set on the front of the PCB board (8).