Method for form-fittingly joining at least two joining partners and joining partner arrangement
By using a laser beam to melt and join mating parts to form molten protrusions, and utilizing the hump effect to generate regular material overhangs, the problem of shape-locking connection of mating parts that cannot be material-locked is solved, and efficient connection without additional materials or special shapes is achieved.
Patent Information
- Application Number
- CN202610705522.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-23
- Filing Date
- 2026-05-21
- Publication Date
- 2026-11-24
Smart Images

Figure CN123149574A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for shape-locking at least two mating pieces without the use of additional materials by means of a laser beam method. Background Technology
[0002] The later-published document DE 10 2023 211 662 describes a method for form-locking two components. Here, the components are arranged at least in or within each other in corresponding engagement regions, wherein one component is fused in the engagement region of the component by means of a laser beam such that, through plastic deformation, the molten material of the component flows around a protrusion of the other component from the protrusion to the other component, and / or flows into a void in the other component, thereby form-locking the components together. Summary of the Invention
[0003] The subject of this invention is a method for shape-lockingly joining at least two mating members, particularly those that cannot be materially locked together, having the features of claim 1, and a mating member arrangement structure having the features of claim 12.
[0004] Preferred or advantageous embodiments of the invention are obtained from the dependent claims, the following description, and the accompanying drawings.
[0005] The subject of this invention is a method for form-locking at least two mating parts that are particularly unable to be material-locked or physically connected. Specifically, the method is used to form-lock at least two mating parts that cannot be welded to each other.
[0006] Here, at least two mating members are arranged relative to each other in a form-locking engagement region. Specifically, the mating members are arranged relative to each other in direct contact, particularly without gaps, or relative to each other at a defined distance, particularly corresponding to a gap or tolerance. The mating members can here have the same or different geometries, at least in the form-locking engagement region. The mating members are arranged such that each of the two mating members prevents relative movement of the corresponding other mating member in at least one direction. Specifically, the mating members can also be arranged between each other, wherein, preferably, the mating members have geometries that are at least partially corresponding to each other.
[0007] Here, the shape-locking engagement region is the region in which shape locking between the at least two mating members is created in a further process of the method. The shape-locking engagement region extends within the range of at least one segment of each of the two mating members.
[0008] In a further step of the method, the material of one of the mating components is melted by means of a heat input method using a laser beam. At least one laser beam is generated here. The laser beam is generated, in particular, by a laser welding apparatus. The laser welding method is used in the absence of additional material, for example, in the form of wire or powder.
[0009] Here, a laser beam is directed onto the surface area of the at least one mating member, where the material should melt. The energy of the laser beam generates a heat input from the irradiated surface into the material. The intensity or energy of the laser beam is chosen such that a sufficiently high heat input is generated into the material, causing it to melt. Specifically, the material is heated to its melting temperature or higher in the region of the laser beam's irradiation point, particularly through heat conduction welding or deep welding.
[0010] The method is configured to generate relative movement between the laser beam and the mating member, at which the material should melt. Specifically, the angle of the laser beam with respect to the molten surface area is varied, and / or the firing point or firing area of the laser beam on the surface area is changed. For example, the laser beam can be moved or shifted. In particular, the laser beam can be made perpendicular to the surface or oriented at an angle relative to the surface.
[0011] Here, at least the mating member in which heat input should be carried out is made of a molten material in at least a portion of the section or region where the heat input, or the laser beam, is carried out.
[0012] Specifically, the material of only one of the mating members is melted. The material of the other mating member is not melted, and the material is located near the melted material or is located near the melted material due to the physical contact between the two mating members.
[0013] According to the method, molten protrusions are generated by melting material. Here, the molten protrusions are formed by, constituted by, or generated from the molten material. The molten protrusions are generated such that they protrude from the molten material. Here, the molten protrusions constitute at least a portion of the volume of the molten material, which extends within a horizontal range above the height of the surface being irradiated by the laser beam.
[0014] In particular, this creates melting protrusions, each formed by a volume reduction of a portion of the molten material. In other words, this means that a volume reduction or decrease occurs, forming a portion of the melt volume, while the excess volume or increase in volume is constituted or formed by the volume reduction in the form of melting protrusions. In other words, here, the melt recovers from a portion of the molten region to another portion of the molten region or a previously molten region, the previously molten region having a lower temperature than the molten region.
[0015] In another step of the method, after the molten material, or molten protrusion, cools, and especially after solidification, the molten protrusion exists as a material overhang within the basic contour or height of the surface irradiated by the laser beam for the purpose of molten material. In other words, this means that the material overhang is formed by the cooling of the molten material, or by the cooling of the molten protrusion. Here, the molten material, or molten protrusion, can also be actively cooled, for example, by an airflow. In particular, it is arranged to produce several, preferably multiple, molten protrusions. Here, it is preferable to produce molten protrusions at a spacing of 1 to 5 mm between two corresponding molten protrusions.
[0016] In particular, the material of one of the mating components is melted such that the molten material exists as a weld after cooling, wherein the material protrusions are arranged along the weld and are spaced apart from each other. It is also possible, in particular, to produce discontinuous welds. In other words, this means, for example, interrupting the heat input and / or laser beam during laser and / or mating component movement, such that multiple regions with material protrusions are created on the mating components, which may take the form of, for example, interrupted welds or multiple welds.
[0017] Here, the at least two mating members are form-locked together in a form-locking engagement region by means of a material protrusion. The material protrusion is arranged at a segment of one of the mating members in the form-locking engagement region. The material protrusion exists specifically as a geometrical change portion of the segment and serves to form-lock a segment of the other mating member located within the form-locking engagement region. The material protrusion on one of the mating members prevents relative movement between the mating members in at least one direction.
[0018] The advantage obtained here is that, in order to form a form-locking connection between the two mating parts, the mating parts, especially those with material protrusions, do not need to have a special geometry or require special geometry preparation. Furthermore, this method can form-lock two mating parts that cannot be connected by, for example, fusion welding or material locking. Moreover, by utilizing the material of one of the mating parts to form the material protrusion, no additional material is needed, thereby saving costs.
[0019] The method is preferably designed such that the molten protrusions are formed at regular intervals, particularly in time and / or in space. Here, the molten protrusions are generated at substantially the same intervals. Specifically, molten protrusions are generated at regular intervals in continuous molten regions, wherein the continuous molten regions are areas melted by laser melting or already melted. For example, the molten regions can be constructed or formed in a manner consistent with continuous weld seams.
[0020] Particularly preferably, the molten protrusion is generated in accordance with or through the appearance of a hump effect, especially in accordance with the hump effect that occurs during laser welding.
[0021] The hump effect in laser welding specifically describes weld defects. Here, the periodic or regular bulges formed by the molten material along the weld seam are also called "humps" or "mounds." Various theories exist to describe the occurrence or causes of the hump effect. For example, the hump effect can occur when the laser is guided within a surface area at a specific speed, especially at a speed greater than a specific critical speed. In particular, the shape or geometry and / or intensity distribution of the material being processed and / or the laser beam can also cause or at least promote the occurrence of the hump effect.
[0022] Preferably, the molten protrusions, or material overhangs, are generated according to the hump effect, wherein the occurrence of the hump effect is utilized in a targeted and controlled manner. The regions or sections of the mating members in which the molten protrusions form material overhangs, especially after the formation of the material overhangs, exist as welds, particularly laser welds, wherein the material overhangs are formed along the weld at regular intervals relative to each other. In particular, the material overhangs are formed in such a way that recesses and corresponding material overhangs alternately appear. Here, the recesses are constituted or formed by the volume reduction of the molten material as previously described. The advantage obtained is that, with the material overhangs arranged at regular intervals, a uniform stress distribution can be obtained when the two mating members are shape-locked. Another advantage obtained is that the hump effect, which has been considered a defect until now, can be utilized in a targeted manner.
[0023] In a preferred embodiment of the method, a material overhang is formed by molten protrusions, each material overhang having a geometry at least partially constructed as a spherical or ellipsoidal segment, or the material overhang is formed entirely by molten protrusions. In particular, each individual material overhang is formed by, or constituted by, a corresponding individual molten protrusion. The material overhang is formed by, or constituted by, molten protrusions, as is achieved through the solidification of molten material, especially a molten metal. The material overhangs are particularly constructed as rounded-corner protrusions. For example, the material overhangs can be respectively constructed at least partially as hemispherical or ellipsoidal segments or portions.
[0024] A feasible design configuration involves at least one of the mating members having a protrusion, wherein another mating member is arranged at, and particularly within, the protrusion. Preferably, one of the mating members is arranged at and / or within the protrusion such that it is supported or arranged to be able to move only in one direction, wherein a material overhang is formed or produced, such that movement in that direction is prevented or prevented by a form-locking engagement created by the material overhang. Here, the protrusion can be arranged in and / or adjacent to the form-locking engagement region. Here, the geometry of the other mating member can be at least partially adapted to the geometry of the protrusion. The advantage obtained here is that an additional form-locking engagement can be generated, which can be used as a fixing part against the torsion and / or movement of the mating members relative to each other. In particular, this can improve manufacturing accuracy.
[0025] In alternative or supplementary designs, at least one of the mating members has a gap, in which another mating member is arranged. Preferably, the other mating member is arranged in the gap such that it is supported or arranged to be able to move only in one direction, wherein a material overhang is created or formed to prevent or prevent movement in that direction. The gap can be arranged particularly in and / or adjacent to the form-locking engagement area. Here, the geometry of the other mating member can be particularly adapted to the geometry of the gap. It is also particularly feasible that one of the mating members has a protrusion as described, and the other mating member has a gap, wherein the geometry of the protrusion is adapted to the geometry of the gap. The advantage obtained here is that an additional form lock can be generated, which can serve as a fixing part against the torsion and / or movement of the mating members relative to each other. In particular, this can improve manufacturing accuracy.
[0026] Another feasible embodiment involves one of the mating members having a gap or notch in the form-locking engagement area, and thus creating a molten protrusion on the other mating member that extends into the gap or notch. It is feasible that not all molten protrusions, but only a portion, i.e., a defined number, extend into the gap. Here, the gap or notch can be constructed as a groove. It is also particularly feasible to create a molten protrusion within the gap. The advantage obtained here is that the form-locking already achieved by the mutual arrangement of the mating members can be supplemented by the form-locking created by the material overhang, or in other words, a form-locking can be ensured by another form-locking.
[0027] In the specific embodiment, the mating components are configured to have or be constructed of materials of the same type and having the same melting point relative to each other, wherein one of the mating components is heated to or beyond its respective melting point. Preferably, the materials of the mating components are selected from the group consisting of metallic materials (especially aluminum, aluminum alloys, iron, iron-carbon alloys (steel), copper, and copper alloys) and plastics. In particular, this is done such that the material of one of the mating components is melted in the shape-locking joint area by a laser beam method to create a molten protrusion, wherein the material of the other mating component does not melt. The advantage obtained here is that, although the two mating components may be weldable, an alternative form of shape-locking connection can be produced. Another advantage obtained is that, through targeted laser guidance or targeted heat input, the material of only one mating component can be melted.
[0028] Alternatively, the mating components are configured to have materials that are different from each other and have different melting points, or are constructed from said materials, wherein one of the mating components is heated to or above its respective melting point. Preferably, the materials of the mating components are selected from the group consisting of metallic materials (especially aluminum, aluminum alloys, iron, iron-carbon alloys (steel), copper, copper alloys) and plastics. In particular, this is done such that the material of one of the mating components is melted in the shape-locking region by a laser beam method to create a molten protrusion, wherein the material of the other mating component does not melt. The advantage of this is that mating components that cannot be joined by material locking or material locking based on their respective materials can be joined by shape locking. Furthermore, by selecting different materials for the respective mating components, it is possible to obtain a pure shape-locking of the mating components without welding or producing material locking.
[0029] In a preferred design of the method, at least the material in the heat input region is loaded with a protective gas. This can be achieved by performing the method in a protective gas atmosphere and / or by actively supplying the protective gas to the heat input region. Here, the molten material of one of the mating components can be loaded with the protective gas by the flow of the melt. In particular, the material of both mating components in the shape-locking joint region can also be loaded with the protective gas. For example, commonly used protective gases, such as those used in other welding methods or specifically in laser welding, can be used. This can have a particularly positive impact on the properties of the molten material, or melt, thereby improving process accuracy.
[0030] An improved version of the method involves at least one of the mating components moving, particularly rotating, and / or vibrating during heat input. Particularly feasible here is that one of the mating components moves while the laser beam remains in a fixed position. Here, the relative movement between the at least one mating component and the laser beam is generated solely by the movement of the at least one mating component. Alternatively, it is also feasible that not only at least one of the mating components but also the laser beam moves. Here, the relative movement between the at least one mating component and the laser beam is generated such that the laser's firing point on the at least one mating component moves, causing different areas, particularly along the weld seam, to melt. Here, the movement of the at least one mating component is generated, particularly mechanically or automatically. The advantage of this is that simple laser welding equipment or easily designed laser beam generators can be used, which cannot generate the movement of the laser beam, wherein the movement of the at least one mating component is generated by simple and inexpensive mechanical motion devices. Alternatively, the advantage of combining the movement of the at least one mating component with the movement of the laser beam is that the method can provide greater flexibility and / or improved process accuracy.
[0031] In feasible designs of the method, it is possible for the method parameters, particularly those of the laser beam method, to remain constant or change continuously during the generation of the molten protrusion or during the formation of the material overhang. For example, the laser beam can be guided within the surface of one of the mating members at a constant moving speed. Alternatively or supplementarily, the shape of the laser beam and / or the power and intensity distribution of the laser beam can also remain constant. Alternatively, it is also possible for the moving speed, moving direction, laser beam shape, and / or laser power and / or intensity distribution to change during the method or during the generation of the molten protrusion. For example, beam oscillation, i.e., so-called "wobbling," is also feasible. Alternatively or supplementarily, the movement of one of the mating members, particularly the direction of rotation and / or rotational speed, can also remain constant or change during the method. It is also particularly possible for the processing line of the laser beam and / or one of the mating members to be linear or curved. Another alternative or supplementary solution involves, for example, defocusing the laser beam by adjusting the optical system or changing the distance between the optical system and the surface to be processed. This alters the beam diameter and intensity, or intensity distribution, on the surface. Consequently, it can affect the appearance of material protrusions, particularly the spacing of these protrusions, and other characteristics.
[0032] Another subject of the invention is a mating member arrangement structure having at least two mating members, particularly as previously described, wherein the at least two mating members are preferably form-locked together by means of a method previously described. Here, the mating member arrangement structure is particularly constructed such that only form-locking occurs through material protrusions as previously described, and no material lock or material-locking occurs between the two mating members. Therefore, the mating member arrangement structure comprises at least two mating members form-locked together in a form-locking engagement region, wherein the mating members are form-locked together by material protrusions in the form of molten protrusions made of solidified material in the form-locking engagement region. Attached Figure Description
[0033] Further features, advantages, and effects of the invention will become apparent from the following description of preferred embodiments and the accompanying drawings. These figures illustrate: Figure 1 A partial cutaway of the mating component arrangement structure is shown. Figure 2 The arrangement of mating parts with material protrusions is shown. Figure 3 A mating arrangement with two mating members is shown, wherein one of the mating members has a material overhang and the other has a groove, wherein the material overhang extends into the groove. Detailed Implementation
[0034] Figure 1 The diagram shows a partial cross-section of the mating member arrangement structure 1. Here, the mating member arrangement structure 1 includes a first mating member 2 and a second mating member 3. The mating member arrangement structure 1 is constructed with rotational symmetry, wherein mating members 1 and 2 are each constructed as rotationally symmetric bodies. The axis of rotation is indicated by a dashed line. The first mating member 2 has a recess 6, in which the second mating member 3 is arranged. Figure 1 The diagram also shows the shape-locking engagement region 4, in which the second engagement mating member 3 is arranged at the first engagement mating member 2. Here, the second engagement mating member 3 is arranged at the first engagement mating member 2 and in the empty portion 6 of the first engagement mating member 2 such that the second engagement mating member 3 can be moved in the direction indicated by arrow 7 solely due to its arrangement at and within the first engagement mating member 2.
[0035] exist Figure 1The cross-section of the structure 1 arranged by the mating members shown also extends through the material protrusion 5. Only one of the multiple material protrusions 5 is shown here. Here, the material protrusion 5 is produced by the material of the first mating member 2. Here, the material protrusion 5 is shown as a protrusion of the surface 8 of the first mating member 2, indicated by dashed lines in the diagram. Here, the surface 8 indicated by dashed lines is the surface of the first mating member 2 in its basic state before the material protrusion 5 is produced. Here, the material protrusion 5 has a geometry that is at least partially hemispherical or constructed as spherical segments, shown by a cross-section that is at least partially semicircular.
[0036] Here, the material protrusion 5 is formed in the shape-locking engagement region 4 and is arranged as part of the first engagement mating member 2 in this shape-locking engagement region. The material protrusion 5 is formed and arranged such that it creates a shape lock between the second engagement mating member 3 and the first engagement mating member 2. The displacement of the second engagement mating member 3 in the direction of arrow 7 is prevented by the material protrusion 5, and especially by another material protrusion 5 not shown. The material protrusion 5 is arranged only on the first engagement mating member 2. The material protrusion 5 is formed such that no material-locking connection or material-locking connection is constructed between the first engagement mating member 2 and the second engagement mating member 3.
[0037] To illustrate how material has been or will be produced beyond section 5, in Figure 1 An exemplary laser beam 13 is also shown. The laser beam has an angle relative to the surface 8 in the beam direction. An exemplary method can be implemented such that the laser beam 13 irradiates the surface 8 of the first mating member 2, and the laser 13 moves in the line of sight or opposite to the line of sight to generate a molten protrusion on the rotationally symmetrical first mating member 2, the molten protrusion being constructed by cooling the molten material or by constructing a material protrusion 5.
[0038] Figure 2 The diagram shows a partial cutaway of the rotationally symmetric mating member 2. This is shown from... Figure 1 The diagram shows the first mating member 2. Here, the first mating member 2 shown has a plurality of material protrusions 5, which are arranged around the first mating member 2 and are formed by their material at the first mating member 2. Furthermore, Figure 2 The diagram shows the extension region 9 of the material extending beyond the portion 5. Here, the extension region 9 forms a surrounding section of the first engaging member 2. Here, the extension region 9 is the passage of the first engaging member 2... Figure 2The area or section that has been melted by the laser beam method (not shown) is used to create a melt protrusion (not shown), which forms the material extension 5 shown. Here, the extension region 9 can be considered as a blind seam.
[0039] Here, Figure 2 The material protrusions 5 shown are generated or arranged along the extension region 9 at regular intervals relative to each other. Here, the material protrusions 5 are constructed as protrusions extending in the circumferential direction or along the extension region 9. In other words, the material protrusions 5 are constructed as protrusions having a geometry that is at least partially ellipsoidal or constructed as ellipsoidal segments.
[0040] exist Figure 3 The diagram illustrates another embodiment of the mating member arrangement structure 1. Here, the mating member arrangement structure 1 is shown in cross-section. Here, the first mating member 2 is arranged at the second mating member 3 at the shape-locking engagement region 4, indicated by dashed lines. Here, the mating members 1 and 2 are arranged end-to-end, or in the butt-welding configuration, at each other. Here, the second mating member 3 has a groove 12, which is arranged at the end-to-end of the second mating member 3 within the shape-locking engagement region 4. The diagram also shows one of a plurality of material protrusions 5, arranged behind the shown material protrusion 5 in the line-of-sight direction. Only the shown material protrusion 5 is visible, and the other material protrusions are constructed as shown. Here, the material protrusions 5 are each constructed as protrusions projecting from the surface at the end-to-end of the first mating member 2. The diagram shows that the material protrusion 5 extends into the groove 12 in the protrusion direction. Here, the relative movement caused by the two mating parts 1 and 2 pushing against each other is prevented in the direction of arrows 10 and 11 by the material extension 5 extending into the groove 12.
[0041] An exemplary method for manufacturing such a mating arrangement 1 can be designed such that at least one of the mating members 1 and 2 is pushed and / or rotated along the groove 7 or in a direction transverse to the arrows 10 and 11 during the generation or formation of the material protrusion 5, such that the material protrusion 5 is pushed into the groove, or formed in the groove 7 by the resulting molten protrusion through cooling.
Claims
1. A method for form-fitting engagement of at least two mating parts (2, 3), particularly those that cannot be materially fitted together. in, The at least two mating members (2, 3) are arranged relative to each other in the shape-locking mating area (4). In this process, the material of one of the mating components (2, 3) is melted by heat input via a laser beam method. Its features are, Melting creates molten protrusions that protrude from the molten material. The molten protrusion exists as a material extension (5) after the molten material has cooled, and the mating members (2, 3) are shaped-locked together in the shape-locking mating area (4) by means of the material extension (5).
2. The method according to claim 1, characterized in that, The molten protrusions are created at regular intervals.
3. The method according to any one of the preceding claims, characterized in that, The molten protrusions are generated in accordance with the hump effect.
4. The method according to any one of the preceding claims, characterized in that, The material extension (5) is formed by the molten protrusion, and the material extension has at least a portion of its geometry constructed as a spherical segment or an ellipsoidal segment.
5. The method according to any one of the preceding claims, characterized in that, At least one of the mating members (2, 3) has a protrusion, wherein the other mating member is disposed at the protrusion.
6. The method according to any one of the preceding claims, characterized in that, At least one of the mating members (2, 3) has a void (6), wherein the other mating member (2, 3) is arranged in the void (6).
7. The method according to any one of the preceding claims, characterized in that, One of the mating parts (2, 3) has a void (6) in the shape-locking mating area (4), and thus a melting protrusion is formed on the other mating part, such that the material protrusion (5) extends into the void (6).
8. The method according to any one of the preceding claims, characterized in that, The mating parts (2, 3) are made of materials of the same kind as each other and have the same melting point relative to each other, or are constructed of said materials.
9. The method according to any one of the preceding claims, characterized in that, The mating parts (2, 3) are made of materials that have different melting points from each other, or are constructed from said materials.
10. The method according to any one of the preceding claims, characterized in that, The material is loaded with a protective gas at least in the area of heat input.
11. The method according to any one of the preceding claims, characterized in that, At least one of the mating components (2, 3) moves, particularly rotates, and / or is subjected to vibration during heat input.
12. A mating arrangement structure (1) having at least two mating parts (2, 3) that are form-locked together in a form-locking engagement region (4), characterized in that, The mating parts (2, 3) are joined together by a material overhang (5) in the form of a molten protrusion made of solidified material in the shape-locking mating region (4).
13. The mating member arrangement structure (1) according to claim 12, characterized in that, The at least two mating pieces (2, 3) are joined together in a form-locking manner by means of any one of claims 1 to 11.
Citation Information
Patent Citations
Method for the positive joining of two components, component arrangement
DE102023211662A1