A multi-beam cooperative polycrystalline ingot silicon carbide laser energy adaptive cutting method and system
By employing multi-beam collaborative silicon carbide laser cutting technology, and using a matrix-type intelligent ingot plate and a multi-beam thermal coupling correction model, the problems of low efficiency and inconsistent quality in polycrystalline ingot processing have been solved, achieving efficient and stable silicon carbide ingot cutting.
Patent Information
- Application Number
- CN202611338214.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-31
- Publication Date
- 2026-11-24
AI Technical Summary
Existing silicon carbide laser cutting technology suffers from low efficiency, inconsistent quality, and local defects in polycrystalline ingot processing, failing to meet the demands of large-scale mass production. Furthermore, multi-beam processing is prone to causing localized overheating breakdown and thermal stress cracking.
By employing a multi-beam collaborative approach, multiple ingots are supported by a matrix-type intelligent ingot plate. Combined with a multi-beam thermal coupling correction model, process matching between ingots and feature partitioning within ingots are performed to optimize beam power, scanning speed, and beam spacing, thereby achieving multi-beam collaborative processing.
It improves the processing efficiency and quality consistency of polycrystalline ingots, reduces defects such as incomplete peeling, interlayer breakdown and edge chipping, and meets the needs of large-scale mass production.
Smart Images

Figure CN123149595A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of crystal ingot cutting technology, and particularly relates to a multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method and system. Background Technology
[0002] Silicon carbide, as a core material for third-generation semiconductors, possesses excellent properties such as wide bandgap, high breakdown field strength, high thermal conductivity, and fast saturated electron drift velocity. It is widely used in high-voltage power devices, radio frequency devices, and optoelectronic devices, and is a key foundational material supporting the development of industries such as new energy, 5G communications, and aerospace. Ingot dicing is one of the core processes in silicon carbide wafer manufacturing, directly determining the wafer yield, surface quality, and processing cost. Compared to traditional diamond wire cutting, laser cutting offers advantages such as non-contact operation, no tool wear, high cutting precision, and low material loss, and has become the mainstream technology for silicon carbide ingot dicing.
[0003] Currently, silicon carbide laser cutting mostly adopts a single-beam fixed-parameter processing mode. Due to the inherent characteristics of the material, such as ingot thickness deviation, lattice defects, and uneven resistivity distribution, quality defects such as incomplete local peeling, interlayer breakdown, and thermal stress edge breakage are prone to occur during the processing. At the same time, a single beam requires multiple round-trip scans to complete multiple processes such as preheating and remodeling in sequence, resulting in low processing efficiency and difficulty in meeting the capacity requirements of large-scale mass production in the silicon carbide industry.
[0004] Chinese patent CN117283152B discloses a method and apparatus for high-efficiency laser cutting of silicon carbide ingots. This method splits a single-beam pulsed laser into a modifying laser and a heating laser. The modifying laser is focused at a predetermined depth inside the ingot to form a modified layer and a crack zone. The heating laser, after frequency conversion and phase delay, is coaxial and synchronized with the modifying laser. Crack propagation is controlled by thermal stress, and finally, wafer separation is completed using the modified layer and crack layer as the interface. This method, through the functional division and synchronous coordination of the two beams, improves the processing efficiency of a single ingot and the quality of the cutting interface to a certain extent.
[0005] However, the aforementioned existing technologies only support single-ingot single-station processing and do not construct a multi-ingot batch support and parallel processing architecture, which cannot meet the capacity requirements of large-scale mass production; multi-beam only achieves functional coordination on a single path and cannot accurately control the superposition effect of temperature field. While improving power and scanning speed, it is easy to cause defects such as local overheating breakdown and thermal stress cracking, making it difficult to balance efficiency improvement and quality control. Summary of the Invention
[0006] The purpose of this invention is to provide a multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method and system, which partially solves or alleviates the above-mentioned shortcomings in the prior art, and can achieve both polycrystalline ingot mass production efficiency and batch quality consistency.
[0007] To solve the aforementioned technical problems, the present invention specifically adopts the following technical solution: A first aspect of the present invention is to provide a multi-beam coordinated adaptive laser energy cutting method for polycrystalline silicon carbide ingots, comprising the following steps: A matrix-type intelligent ingot plate is used to support multiple crystal ingots. The matrix-type intelligent ingot plate is equipped with several independent feeding work stations. Each feeding work station independently completes crystal ingot positioning, adsorption and working condition acquisition. The resistivity, thickness, surface morphology, and lattice defects of all crystal ingots on the matrix-type intelligent ingot plate are scanned. After the data is segmented according to the loading work position, independent feature data is generated for each crystal ingot. The feature data includes overall feature data and internal feature distribution data. Based on the overall feature data of each crystal ingot, the process matching between ingots is performed through a parameter matching model to output the basic process parameters of the whole ingot; based on the feature distribution data inside a single crystal ingot, the feature partitioning within a single ingot is performed, and the corresponding initial partition process parameters are matched for each partition through a parameter matching model. A multi-beam thermal coupling correction model is introduced to calculate the temperature field superposition effect of multi-beam collaborative processing. The beam power, scanning speed and beam spacing in the initial process parameters of each partition are corrected in reverse to obtain the final process parameters of each partition. Based on the final process parameters of each zone, processing areas and process parameters are assigned to multiple laser heads, and the multi-beams are controlled to work together to complete the laser cutting of the crystal ingot.
[0008] Furthermore, each loading station of the matrix-type intelligent ingot plate is configured with: The positioning mechanism includes positioning grippers and gripper tracks, which complete the circumferential positioning and centering of the crystal ingot by the grippers retracting and opening radially along the tracks; Independent negative pressure channels, with each workstation's negative pressure channel isolated from and not connected to the others; The in-situ sensing unit is located in the ingot installation area of the loading station and is used to collect the position and vacuum level parameters of the ingot.
[0009] Furthermore, the overall characteristic data includes the overall resistivity level, average thickness, total defect density and surface morphology grade of the ingot, and the basic process parameters of the whole ingot include the reference laser power and feed rate of the whole ingot for the corresponding grade. The internal feature distribution data includes the local resistivity, lattice defect region and surface morphology anomaly points inside a single crystal ingot, and the initial partitioning process parameters include preset process reference values corresponding to different feature intervals.
[0010] Furthermore, the steps for correcting the beam power, scanning speed, and beam spacing parameters for each zone include: Establish a steady-state moving coordinate system that moves synchronously with the laser along the x-direction, and construct the three-dimensional heat conduction control equations under steady state: ; Where λ is the thermal conductivity of silicon carbide, T is the temperature field distribution, ρ is the density of silicon carbide, and c p denoted as silicon carbide specific heat capacity under constant pressure, v as laser scanning speed, x as the x-axis coordinate of the steady-state moving coordinate system, y as the y-axis coordinate of the steady-state moving coordinate system, and z as the z-axis coordinate of the steady-state moving coordinate system. Based on the aforementioned heat conduction control equation, using the formula:
[0011] Calculate the peak temperature rise at the center of the beam under the action of a single-channel Gaussian beam: where ΔT peak ω0 is the highest temperature rise of the spot center relative to the substrate, A is the absorptivity of silicon carbide to laser, P is the beam power, ω0 is the spot radius, and α is the thermal diffusivity of silicon carbide. Based on the principle of linear superposition of temperature fields, using the formula:
[0012] Calculate the superimposed temperature rise at the midpoint between two adjacent beams with a spacing of d; where ΔT mid To superimpose the temperature rise; Using the target temperature rise as a constraint, the beam power, scanning speed, and beam spacing process parameters of each zone are corrected in reverse.
[0013] Furthermore, the steps for reverse-correcting the beam power, scanning speed, and beam spacing process parameters for each zone include: Using the formula:
[0014] Perform beam power correction; where P 原 P is the initial beam power. 新 To correct the beam power, ΔT 目标 The target peak temperature rise is set; Using the formula:
[0015] Perform scan speed correction; where v 原 v is the initial scan speed. 新 This is the corrected scan speed; Using the formula:
[0016] Beam spacing correction is performed; where d 新 The corrected beam spacing is represented by δ, which is the allowable deviation rate between the inter-channel temperature and the peak temperature.
[0017] Furthermore, a load balancing scheduling algorithm is used to allocate processing areas and process parameters to multiple laser heads; the load balancing scheduling algorithm supports switchable master-slave function beam splitting mode and partitioned parallel scanning mode; The master-slave functional beam splitting mode is used for single-path multi-process coupling scenarios where multiple laser processing functions need to be completed sequentially on the same scanning trajectory, and preheating and modification processing are completed synchronously in a single scan. The partitioned parallel scanning mode is used for large planar processing scenarios where the processing area can be divided into multiple non-interfering sub-regions, and multi-beam regional synchronous processing is used to improve overall efficiency.
[0018] Furthermore, during the processing, the laser modification state data of the ingot is collected in real time, and the process parameters of each zone are dynamically corrected based on the state deviation. After the processing is completed, the characteristic data, process parameters, modification state data and processing quality data of the ingot are fed back to the process database, and the parameter matching model and multi-beam thermal coupling correction model are iteratively optimized.
[0019] Furthermore, plasma spectroscopy and infrared thermography were used to characterize the ingot modification state; The plasma spectroscopy is used to obtain data on the intensity of spectral lines of characteristic elements, plasma electron temperature and electron number density, reflecting the degree of material ablation, energy absorption efficiency and internal defect state. The infrared thermal imaging is used to acquire data on the peak temperature of the processing point, the temperature distribution of the heat-affected zone, and the rate of temperature change, reflecting the degree of phase transformation, the level of thermal stress, and the thermal accumulation effect.
[0020] Furthermore, methods for dynamically adjusting the process parameters of each zone include: A mapping table of state deviation rate to parameter correction amount is generated in advance through process calibration; After calculating the deviation between the state quantity and the target value in real time, the correction value is output by looking up the table; the correction priority is to adjust the laser power first, and then adjust the scanning speed after the power reaches the limit.
[0021] This invention also provides a multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting system, comprising: A matrix-type intelligent ingot plate is used to support multiple crystal ingots for crystal ingot positioning, adsorption, and working condition data collection. The global pre-detection module is used to scan the resistivity, thickness, surface morphology and lattice defects of all crystal ingots on the matrix-type intelligent ingot plate, and after dividing the data according to the loading work position, it generates independent feature data for each crystal ingot; the feature data includes overall feature data and internal feature distribution data; The parameter matching module is used to perform inter-ingot process matching based on the overall feature data of each crystal ingot and output the basic process parameters of the whole ingot; it also performs feature partitioning within a single crystal ingot based on the feature distribution data within the single crystal ingot and matches the corresponding initial partition process parameters for each partition using the parameter matching model. The parameter correction module introduces a multi-beam thermal coupling correction model to calculate the temperature field superposition effect of multi-beam collaborative processing, and reversely corrects the beam power, scanning speed and beam spacing in the initial process parameters of each partition to obtain the final process parameters of each partition. The multi-beam laser processing module is used to allocate processing areas and process parameters to multiple laser heads based on the final process parameters of each zone, and control the multi-beams to work together to complete the laser cutting of the crystal ingot.
[0022] Beneficial effects:
[0023] This invention enables the simultaneous clamping and synchronous processing of multiple crystal ingots through a multi-station matrix-type intelligent ingot plate. Combined with a dual-mode switching mechanism for multi-beam collaborative processing, the master-slave functional beam splitting mode integrates multiple processes such as preheating and quality modification into a single scan, eliminating the redundant time consumption of multiple round trips of a single beam. The partitioned parallel scanning mode achieves a multiple-level improvement in surface processing efficiency through multi-beam spatial regional synchronous processing.
[0024] This invention employs a two-level parameter planning mechanism: inter-ingot process matching and intra-ingot feature partitioning. It adapts to the individual characteristics of different ingots (resistivity, thickness, defect density, etc.) through whole-ingot level matching, and adapts to the uneven feature distribution within a single ingot through partition-level matching. This replaces the traditional uniform parameter mode for the entire plate, fundamentally reducing quality dispersion caused by material property fluctuations. A multi-beam thermal coupling correction model is introduced, quantitatively calculating the temperature field superposition effect based on the silicon carbide thermal diffusion physical equation. This model inversely corrects beam power, scanning speed, and beam spacing, solving problems such as localized overheating breakdown and thermal stress edge chipping caused by simple multi-beam stacking. It can effectively reduce processing defects such as incomplete peeling, interlayer breakdown, and edge chipping. Attached Figure Description
[0025] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. In all the drawings, similar elements or parts are generally identified by similar reference numerals. The elements or parts in the drawings are not necessarily drawn to scale. Obviously, the drawings described below are some embodiments of the present invention, and those skilled in the art can obtain other drawings based on these drawings without any creative effort.
[0026] Figure 1 This is a flowchart of the present invention.
[0027] Figure 2 This is a top view of the matrix-type intelligent ingot plate in this invention.
[0028] Summary of attached labeling and identification: 1-Bearing plate, 11-Loading work station, 111-Positioning gripper, 112-Gripper track, 113-Negative pressure channel. Detailed Implementation
[0029] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of the present invention. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.
[0030] In this document, suffixes such as "module," "part," or "unit" used to denote elements are used only for the purpose of illustrative purposes and have no specific meaning in themselves. Therefore, "module," "part," or "unit" may be used interchangeably.
[0031] In this document, the terms "upper," "lower," "inner," "outer," "front," "rear," "one end," and "the other end," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing the present invention and for simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the present invention. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.
[0032] In this document, unless otherwise explicitly specified and limited, the terms "installed," "equipped with," "connected," etc., should be interpreted broadly. For example, "connection" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, a direct connection, or an indirect connection through an intermediate medium; it can be a connection within two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0033] In this document, "and / or" includes any and all combinations of one or more of the listed related items.
[0034] In this article, "multiple" means two or more, that is, it includes two, three, four, five, etc.
[0035] Example 1:
[0036] This embodiment provides a multi-beam collaborative silicon carbide laser energy adaptive cutting system for polycrystalline ingots. The system consists of a matrix-type intelligent ingot plate, a global pre-detection module, a parameter matching module, a parameter correction module, a multi-beam laser processing module, a real-time closed-loop feedback module, and a process database module. All modules are connected via a main control unit to collaboratively complete the entire processing flow.
[0037] Specifically, such as Figure 2 As shown, the matrix-type intelligent ingot plate is used to carry multiple crystal ingots for crystal ingot positioning, adsorption, and working condition data acquisition.
[0038] The matrix-type intelligent ingot plate adopts a matrix-type 4-station support plate 1 with a marble base, and has a total of 4 sets of independent feeding workstations 11, arranged in a 2×2 matrix. Each plate can simultaneously support 4 standard silicon carbide crystal ingots. Each feeding workstation 11 is independently equipped with a positioning mechanism, an independent negative pressure channel 113, and an in-situ sensing unit.
[0039] The positioning mechanism includes positioning grippers 111 and corresponding gripper tracks 112. Four sets of positioning grippers 111 and corresponding gripper tracks 112 are evenly arranged circumferentially, and the gripper tracks 112 are arranged radially. The positioning grippers 111 are slidably connected to the gripper tracks 112. The grippers use hard contacts coated with polytetrafluoroethylene to avoid scratching the edges of the ingot. During clamping, the four sets of positioning grippers 111 synchronously retract radially along the gripper tracks 112, abutting against the circumferential side of the ingot to complete circumferential positioning and centering. Each station's positioning mechanism is driven by an independent servo motor, responsible only for clamping the ingot at its designated station, with no interference between stations.
[0040] The negative pressure channel 113 is provided with annularly distributed microporous negative pressure adsorption holes on the crystal ingot support platform of each working station. It is connected to an independent vacuum air passage below. The air passages of each working station are isolated from each other and do not communicate with each other. The vacuum on / off and negative pressure are controlled by independent proportional solenoid valves. The adsorption force can be adjusted individually according to the thickness and weight of the crystal ingot, and there is no gas leakage interference between working stations.
[0041] The in-situ sensing unit is integrated in the center area of the table at each workstation, including a photoelectric position sensor and a high-precision vacuum sensor. The position sensor is used to detect whether the ingot is clamped in place and trigger subsequent processes. The vacuum sensor collects the negative pressure value of the gas path at this workstation in real time and provides feedback on the adsorption reliability. The sensing data of each workstation is collected and fed back independently, eliminating the need for indirect detection across workstations.
[0042] The global pre-detection module is used to scan the resistivity, thickness, surface morphology and lattice defects of all crystal ingots on the matrix-type intelligent ingot plate, and after dividing the data according to the loading work position, it generates independent feature data for each crystal ingot.
[0043] The full-domain pre-detection module uses a marble base equipped with a high-precision air-float motion platform as its mechanical support. Four types of detection modules are integrated sequentially along the motion direction on the platform, enabling simultaneous full-parameter scanning of all ingots on the entire plate in a single operation. These modules specifically include: The microwave resistivity detection module uses the non-contact detection principle of microwave resonant cavity to collect the spatial distribution of bulk resistivity of crystal ingots. The single-sided laser interferometric thickness measurement module uses the principle of laser interferometric thickness measurement to collect the thickness distribution and thickness deviation of crystal ingots; The surface morphology detection module consists of a 3D line laser sensor and a high-definition area array camera, used to collect morphological features such as unevenness, growth lines, and mechanical damage on the surface of the crystal ingot. The line-scan photoluminescence lattice defect detection module uses an ultraviolet pulse excitation light source in conjunction with a hyperspectral imager to detect lattice defects such as dislocations, microtubes, and inclusions inside the crystal ingot.
[0044] After scanning is completed, the data processing unit divides the full-domain scan data according to the spatial coordinates of the workstation, and independently generates a feature dataset for each crystal ingot, which includes overall feature data and internal feature distribution data.
[0045] The parameter matching module is used to perform inter-ingot process matching based on the overall feature data of each crystal ingot and output the basic process parameters of the whole ingot; it also performs feature partitioning within a single crystal ingot based on the feature distribution data within the single crystal ingot and matches the corresponding initial partition process parameters for each partition using the parameter matching model.
[0046] It incorporates a two-level parameter matching model, corresponding to coarse matching between ingots and fine matching within ingots, respectively. The inter-ingot process matching sub-model has built-in rules for classifying crystal ingot feature levels and a process calibration database. It can automatically determine the feature level based on the overall feature data of each crystal ingot and match and output the basic process parameters of the whole ingot for the corresponding level. The intra-ingot partition parameter matching sub-model has built-in feature partitioning rules and a parameter offset calculation unit. It can complete the processing partitioning according to the feature consistency principle based on the internal feature space distribution data of a single crystal ingot, and calculate the initial partitioning process parameters of each partition based on the basic process parameters of the whole ingot and combined with the local feature offset.
[0047] The parameter correction module introduces a multi-beam thermal coupling correction model to calculate the temperature field superposition effect of multi-beam collaborative processing, and reversely corrects the beam power, scanning speed and beam spacing in the initial process parameters of each zone to obtain the final process parameters of each zone.
[0048] Its built-in multi-beam thermal coupling correction model, based on the silicon carbide thermal diffusion physical equation, quantitatively calculates the temperature field superposition effect of multi-beam collaborative processing, reversely corrects the beam power, scanning speed and beam spacing in the initial process parameters of each zone, and outputs the final process parameters of each zone that can be directly executed, eliminating the temperature deviation caused by multi-beam thermal accumulation.
[0049] The multi-beam laser processing module is used to allocate processing areas and process parameters to multiple laser heads based on the final process parameters of each zone, and control the multi-beams to work together to complete the laser cutting of the crystal ingot.
[0050] It includes four independently controllable fiber laser heads, a beam focusing and attitude control unit, a two-dimensional high-precision scanning motion platform, and a load balancing scheduling unit. The load balancing scheduling unit has a built-in load balancing scheduling algorithm, supports switching between master-slave functional beam splitting mode and partitioned parallel scanning mode, and can dynamically allocate the processing area, functional role, and process parameters of each laser head according to the processing task type and process difficulty.
[0051] The real-time closed-loop feedback module is used to collect laser modification status data of the ingot in real time during the processing and dynamically correct the process parameters of each zone based on the status deviation. After the processing is completed, the characteristic data, process parameters, modification status data and processing quality data of the ingot are fed back to the process database to iteratively optimize the parameter matching model and the multi-beam thermal coupling correction model.
[0052] It includes a plasma spectral acquisition unit, an infrared thermal imaging acquisition unit, and a parameter lookup and correction unit.
[0053] The plasma spectral acquisition unit uses a high-resolution fiber optic spectrometer to acquire the plasma emission spectrum of the processing point in real time and analyze parameters such as characteristic spectral line intensity, electron temperature, electron number density, and compositional uniformity.
[0054] The infrared thermal imaging acquisition unit uses a mid-wave cooled infrared thermal imager to acquire the temperature field distribution of the processing area in real time and analyze parameters such as peak temperature, temperature gradient, heat accumulation, and residence time in the phase transition zone.
[0055] The parameter lookup and correction unit has a built-in pre-calibrated state deviation rate-parameter correction amount mapping table, which can quickly look up and output parameter correction values based on real-time state deviation. The correction strategy is to first adjust the laser power, and then adjust the scanning speed after the power reaches the upper and lower limits.
[0056] Example 2:
[0057] like Figure 1 As shown, this embodiment provides a multi-beam coordinated adaptive laser energy cutting method for silicon carbide ingots. This method is based on the system described in Embodiment 1, and the specific steps are as follows: S1 uses a matrix-type intelligent ingot plate to carry multiple crystal ingots. The matrix-type intelligent ingot plate is equipped with several independent feeding work stations, and each feeding work station independently completes crystal ingot positioning, adsorption and working condition acquisition.
[0058] Four 6-inch silicon carbide ingots to be cut are placed in the four feeding stations of the matrix-type intelligent ingot plate; the independent positioning mechanism of each station is activated, and the four sets of positioning claws synchronously retract along the radial direction of the track and abut against the circumferential side of the ingot to complete the centering and clamping.
[0059] Each station has an independent negative pressure channel. The negative pressure is adjusted according to the thickness of the ingot to stably adsorb and fix the ingot on the table. The in-situ sensing unit collects the ingot position signal and vacuum signal in real time. After confirming that all stations are clamped in place, the ingot is moved to the testing station by the air flotation platform.
[0060] S2 scans the resistivity, thickness, surface morphology, and lattice defects of all crystal ingots on the matrix-type intelligent ingot plate, and after dividing the data according to the loading work position, generates independent feature data for each crystal ingot; the feature data includes overall feature data and internal feature distribution data.
[0061] The air-floating motion platform propels the entire crystal ingot through the detection area of the full-domain pre-inspection module at a constant speed. Four types of detection modules are simultaneously triggered for sampling, completing a full-domain scan of the resistivity, thickness, surface morphology, and lattice defects of four crystal ingots in one go. After scanning, the data processing unit divides the full-domain scan data according to the spatial coordinates of the workstation, generating a feature dataset for each crystal ingot independently. Among them, the overall feature data includes the overall average resistivity, average thickness, total defect density, and comprehensive surface morphology level of the crystal ingot, serving as the basis for process matching between ingots; the internal feature spatial distribution data includes the local resistivity distribution, lattice defect location distribution, and surface morphology anomalies at various locations within the processed surface of the crystal ingot, serving as the basis for feature partitioning within a single ingot.
[0062] S3 uses the overall feature data of each crystal ingot to perform inter-ingot process matching through a parameter matching model and outputs the basic process parameters of the whole ingot; it also performs feature partitioning within a single crystal ingot based on the feature distribution data within the single ingot and matches the corresponding initial partition process parameters for each partition through a parameter matching model.
[0063] The parameter matching module performs two-level parameter planning, and the specific process is as follows: S31 ingot process matching.
[0064] The matching input is the overall characteristic data of the crystal ingot obtained from the pre-collection of the entire domain, namely the overall average resistivity, average thickness, total defect density, and comprehensive surface morphology level of the crystal ingot.
[0065] The overall resistivity level is the most crucial matching criterion. The resistivity of silicon carbide directly determines the material's absorption efficiency of laser photons. The higher the resistivity, the lower the carrier concentration, the weaker the laser energy absorption, and the higher the laser power required to achieve the same phase transition effect.
[0066] The average thickness of the ingot affects the penetration depth and energy attenuation of the laser energy. The greater the thickness, the lower the energy density at the focusing position. At the same time, thicker ingots have higher heat capacity and slower temperature rise rate, requiring corresponding adjustments to the laser power and scanning speed.
[0067] Total defect density represents the overall material integrity of the ingot. The higher the defect density, the worse the uniformity of thermal conduction of the material, the more significant the thermal stress concentration effect, and the more likely it is to cause edge chipping, crack propagation, and local breakdown during processing. It is necessary to match a gentler temperature gradient and a lower processing speed.
[0068] Surface morphology grade reflects the roughness and unevenness of the crystal ingot surface, which directly affects the reflectivity and energy coupling efficiency of the laser. Areas with rough surfaces and obvious growth lines have greater reflection loss and lower effective energy actually incident into the material, requiring corresponding power compensation.
[0069] The matching process is based on a mapping database that has been calibrated in advance through a large number of systematic process tests, and the parameter mapping is completed by the gear matching method.
[0070] Specifically, the four types of overall characteristics are pre-divided into multiple levels according to threshold values. For example, resistivity is divided into three levels: high resistance, medium resistance, and low resistance; thickness is divided into three levels: thin material, standard material, and thick material; defect density is divided into three levels: level 1, level 2, and level 3; and surface morphology is divided into three levels: excellent, good, and poor.
[0071] For a single crystal ingot, the overall process grade of the ingot is determined by weighting the results of various characteristics and weighting coefficients; among them, resistivity has the highest weight, followed by thickness and defect density, and surface morphology has the lowest weight.
[0072] Based on the overall process level, the corresponding basic process parameters of the ingot are matched and output from the mapping database, including the reference power of laser cutting, the reference scanning feed speed, etc.
[0073] The feature partitions within the S32 single ingot are matched with the initial parameters.
[0074] This step addresses the uneven distribution of feature space within a single crystal ingot. Based on the basic parameters of the entire ingot, the processed surface of the ingot is further divided into several sub-regions with relatively uniform material properties, and each region is matched with its own initial process parameters.
[0075] The input for partitioning is the characteristic distribution differences within a single crystal ingot, namely, the local resistivity distribution, the distribution of lattice defect locations, and surface morphology anomalies.
[0076] Local resistivity distribution is the primary basis for zoning. Due to the segregation effect of impurities during crystal growth, the resistivity of the edge region of the same ingot is usually significantly higher than that of the central region. The difference in local resistivity will lead to differences in local temperature rise under the same laser power.
[0077] Lattice defect regions refer to areas within a crystal ingot where defects such as dislocation clusters, microtubes, and impurity inclusions are concentrated. These regions exhibit uneven thermal conductivity, are more prone to thermal stress concentration, and are susceptible to defect propagation and localized breakdown during processing. Therefore, they require separate regions with more moderate process parameters.
[0078] Surface morphology abnormalities refer to local growth lines, pits, mechanical damage, and other morphological abnormalities on the surface of the crystal ingot. These abnormalities can cause local abrupt changes in laser reflectivity and fluctuations in energy coupling efficiency, requiring separate energy compensation for each region.
[0079] More detailed partitioning is not necessarily better. It's crucial to balance processing quality and process feasibility, ensuring minimal differences in material properties within the same partition. This means controlling fluctuations in key characteristics such as resistivity, defect density, and thickness within the same partition to within preset thresholds, guaranteeing uniform processing results when using the same set of process parameters. Significant characteristic differences are permissible between different partitions, each matched with different parameter levels.
[0080] Avoid overly fragmented partitions, as too many partitions will lead to frequent switching of the laser processing path, increasing the complexity of motion control and reducing processing efficiency; at the same time, too small partitions will increase the difficulty of thermal effect control.
[0081] The laser scanning feed direction is divided into continuous strip-shaped partitions to adapt to the motion characteristics of laser reciprocating scanning, avoid irregular shapes and isolated point-like partitions, reduce the number of beam turning and speed changes, and ensure smooth processing and temperature field stability.
[0082] For isolated, minor anomalies, instead of dividing them into separate zones, local parameter fine-tuning is used to balance machining accuracy and efficiency.
[0083] Based on the basic process parameters of the whole ingot, the initial process parameters of each partition are calculated according to the offset of the local features of each partition relative to the overall features and the pre-calibrated parameter offset rules. These parameters include the initial beam power, initial scanning speed, and initial beam spacing.
[0084] S4 multi-beam thermal coupling parameter correction.
[0085] A multi-beam thermal coupling correction model is introduced to calculate the temperature field superposition effect of multi-beam collaborative processing. The beam power, scanning speed and beam spacing in the initial process parameters of each partition are corrected in reverse to obtain the final process parameters of each partition. The parameter correction module introduces a multi-beam thermal coupling correction model to quantitatively correct the initial process parameters of each partition, thereby obtaining the final process parameters for each partition. The specific calculation process is as follows: S41 establishes the steady-state heat conduction control equation.
[0086] Establish a steady-state moving coordinate system (x, y, z) that moves synchronously with the laser along the x-direction, and construct the three-dimensional heat conduction control equations under steady state: ; Where λ is the thermal conductivity of silicon carbide, T is the temperature field distribution, ρ is the density of silicon carbide, and c p denoted as silicon carbide specific heat capacity at constant pressure, v as laser scanning speed, x as the x-axis coordinate of the steady-state moving coordinate system, y as the y-axis coordinate of the steady-state moving coordinate system, and z as the z-axis coordinate of the steady-state moving coordinate system.
[0087] S42 calculates the peak temperature rise of a single beam.
[0088] Based on the above heat conduction control equation, the analytical formula for the peak temperature rise at the center of the beam spot under the action of a single-channel Gaussian beam is derived:
[0089] Where, ΔT peak ω0 is the highest temperature rise of the spot center relative to the substrate, A is the absorptivity of silicon carbide to laser, P is the beam power, ω0 is the spot radius, and α is the thermal diffusivity of silicon carbide. Substituting the initial beam power, initial scanning speed, and spot radius parameters of each zone, the peak temperature rise of a single beam in that zone is calculated.
[0090] S43 calculates the temperature superposition of multiple scans.
[0091] Based on the principle of linear superposition of temperature fields, when the distance between two adjacent beams is d, the superimposed temperature rise at the midpoint of the two beams is the sum of the temperature rises of the two beams at that point. The calculation formula is as follows:
[0092] Where, ΔT mid To superimpose the temperature rise.
[0093] S44 process parameter reverse correction.
[0094] Constrained by the target peak temperature rise and interchannel temperature uniformity requirements, the beam power, scanning speed and beam spacing of each zone are reverse-corrected.
[0095] Specifically, using the formula:
[0096] Perform beam power correction; where P 原 P is the initial beam power. 新 To correct the beam power, ΔT 目标 The target peak temperature rise is set; Using the formula:
[0097] Perform scan speed correction; where v 原 v is the initial scan speed. 新 This is the corrected scan speed; Using the formula:
[0098] Beam spacing correction is performed; where d 新 The corrected beam spacing is represented by δ, which is the allowable deviation rate between the inter-channel temperature and the peak temperature. The beam spacing is increased when there is overheating due to inter-channel superposition, and decreased when the temperature is insufficient.
[0099] Through the above quantitative correction, the influence of the superposition effect of multi-beam temperature fields on the processing temperature is eliminated, ensuring that the processing temperature of each zone is stable within the target range, and avoiding local overheating and breakdown or insufficient modification.
[0100] Based on the final process parameters of each zone, S5 assigns processing areas and process parameters to multiple laser heads, and controls multiple beams to work together to complete the laser cutting of the ingot.
[0101] The load balancing scheduling unit of the multi-beam laser processing module allocates processing areas, functional roles, and process parameters to the four laser heads based on the final process parameters of each zone, controlling the multi-beams to collaboratively complete the cutting process. The load balancing scheduling algorithm supports switching between two processing modes, as detailed below: S51 partition parallel scan mode.
[0102] When processing large-size crystal ingots and prioritizing mass production efficiency, a partitioned parallel scanning mode is adopted.
[0103] The load balancing scheduling algorithm divides the processing surface of a single crystal ingot into sub-partitions corresponding to the number of available laser heads, quantifies the processing load by combining the process difficulty coefficient of each partition, and adjusts the partition boundaries.
[0104] The thermal coupling correction results are used to verify the center-to-center distance between adjacent beam zones, ensuring that the minimum thermal safety distance requirement is met.
[0105] Each laser head is assigned a corresponding partition and the final process parameters for that partition. The four laser heads independently perform reciprocating scanning processing within their respective partitions, starting and completing synchronously, maximizing processing efficiency through spatial parallelism.
[0106] S52 master-slave functional beam splitting mode.
[0107] When machining challenging areas with high resistance and high defects, and prioritizing machining quality, a master-slave functional beam splitting mode is adopted.
[0108] The load balancing scheduling algorithm assigns a master-slave beam to each scanning path, with one beam as the master beam and one to two beams as slave beams. The master beam is precisely focused on the preset modification depth inside the ingot and undertakes the material phase transformation modification function. The slave beams are arranged in front of the master beam along the scanning direction and undertake the material preheating function.
[0109] The optimal axial spacing between the master and slave beams is set based on the thermal coupling correction results, and the two beams are controlled to scan synchronously at the same speed, so that the preheating temperature field and the modification temperature field are precisely connected, ensuring sufficient preheating effect and avoiding excessive heat accumulation.
[0110] Under the constraint of total available power, the power ratio of master and slave beams is dynamically allocated; when the power of the master beam is close to the rated upper limit, the preheating power of the slave beam is increased, and the energy threshold of the quality improvement is reduced by preheating to avoid overload of single beam power.
[0111] In this mode, the preheating and modification processes can be completed simultaneously in a single scan, eliminating the need for multiple beam passes. This also reduces the internal temperature gradient of the material, effectively suppressing defects such as thermal stress edge breakage and uncontrolled propagation of microcracks.
[0112] During the S6 processing, the laser modification state data of the ingot is collected in real time, and the process parameters of each zone are dynamically corrected based on the state deviation. After processing, the characteristic data, process parameters, modification state data and processing quality data of the ingot are fed back to the process database to iteratively optimize the parameter matching model and the multi-beam thermal coupling correction model.
[0113] S61 Real-time Status Acquisition and Dynamic Correction.
[0114] During the processing, the real-time closed-loop feedback module synchronously collects the processing status through two channels.
[0115] The plasma spectral acquisition unit collects characteristic spectral line intensities in real time, analyzes plasma electron temperature, electron number density, etc., and determines the degree of material ablation, energy absorption efficiency, and internal defect state.
[0116] The infrared thermal imaging acquisition unit collects the peak temperature of the processing point, the temperature distribution of the heat-affected zone, and the temperature difference between the upper and lower surfaces in real time. It calculates the heating rate, cooling rate, and heat accumulation, and determines the degree of phase transformation, the level of thermal stress, and the thermal superposition effect of subsequent scans.
[0117] The parameter lookup and correction unit calculates the deviation rate between the state quantity and the target value in real time, queries the mapping table of state deviation rate to parameter correction quantity generated in advance through process calibration, and outputs the parameter correction value; it prioritizes adjusting the laser power, and then adjusts the scanning speed after the power is adjusted to the upper and lower limits, dynamically correcting the process parameters of the corresponding partition to ensure the stability of the processing state.
[0118] S62 Data Feedback and Model Iteration.
[0119] After a single crystal ingot is processed, its characteristic data, process parameters, modification status data, and subsequent processing quality data (such as modification depth uniformity, defect rate, edge chipping amount, and peeling yield) are all fed back to the process database. Regularly iteratively train the matching model (including the inter-spindle process matching sub-model and the intra-spindle partition parameter matching sub-model) based on accumulated batch data, update the parameter values of the process calibration database, optimize the feature classification threshold and parameter offset rules, and calibrate the physical property parameters of the thermal coupling correction model to continuously improve the parameter matching accuracy and processing stability, thereby achieving self-evolution of process capabilities.
[0120] It should be noted that, in this document, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Unless otherwise specified, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes that element.
[0121] Through the above description of the embodiments, those skilled in the art can clearly understand that the methods of the above embodiments can be implemented by means of software plus necessary general-purpose hardware platforms. Of course, they can also be implemented by hardware, but in many cases the former is a better implementation method. Based on this understanding, the technical solution of the present invention, or the part that contributes to the prior art, can be embodied in the form of a software product. This computer software product is stored in a storage medium (such as ROM / RAM, magnetic disk, optical disk) and includes several instructions to cause a computer terminal (which may be a mobile phone, computer, server, or network device, etc.) to execute the methods described in the various embodiments of the present invention.
[0122] The embodiments of the present invention have been described above with reference to the accompanying drawings. However, the present invention is not limited to the specific embodiments described above. The specific embodiments described above are merely illustrative and not restrictive. Those skilled in the art can make many other forms under the guidance of the present invention without departing from the spirit and scope of the claims. All of these forms are within the protection scope of the present invention.
Claims
1. A multi-beam coordinated adaptive laser energy cutting method for polycrystalline silicon carbide ingots, characterized in that, Includes the following steps: A matrix-type intelligent ingot plate is used to support multiple crystal ingots. The matrix-type intelligent ingot plate is equipped with several independent feeding work stations. Each feeding work station independently completes crystal ingot positioning, adsorption and working condition acquisition. The resistivity, thickness, surface morphology, and lattice defects of all crystal ingots on the matrix-type intelligent ingot plate are scanned. After the data is segmented according to the loading work position, independent feature data is generated for each crystal ingot. The feature data includes overall feature data and internal feature distribution data. Based on the overall feature data of each crystal ingot, the process matching between ingots is performed through a parameter matching model to output the basic process parameters of the whole ingot; based on the feature distribution data inside a single crystal ingot, the feature partitioning within a single ingot is performed, and the corresponding initial partition process parameters are matched for each partition through a parameter matching model. A multi-beam thermal coupling correction model is introduced to calculate the temperature field superposition effect of multi-beam collaborative processing. The beam power, scanning speed and beam spacing in the initial process parameters of each partition are corrected in reverse to obtain the final process parameters of each partition. Based on the final process parameters of each zone, processing areas and process parameters are assigned to multiple laser heads, and the multi-beams are controlled to work together to complete the laser cutting of the crystal ingot.
2. The multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method according to claim 1, characterized in that, Each loading station of the matrix-type intelligent ingot plate is configured with: The positioning mechanism includes positioning grippers and gripper tracks, which complete the circumferential positioning and centering of the crystal ingot by the grippers retracting and opening radially along the tracks; Negative pressure channels: The negative pressure channels of each workstation are isolated from each other and not connected. The in-situ sensing unit is located in the ingot installation area of the loading station and is used to collect the position and vacuum level parameters of the ingot.
3. The multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method according to claim 1, characterized in that: The overall characteristic data includes the overall resistivity level, average thickness, total defect density and surface morphology grade of the ingot, and the basic process parameters of the whole ingot include the reference laser power and feed rate of the whole ingot at the corresponding level. The internal feature distribution data includes the local resistivity, lattice defect region and surface morphology anomaly points inside a single crystal ingot, and the initial partitioning process parameters include preset process reference values corresponding to different feature intervals.
4. The multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method according to claim 1, characterized in that, The steps for correcting the beam power, scanning speed, and beam spacing parameters for each zone include: Establish a steady-state moving coordinate system that moves synchronously with the laser along the x-direction, and construct the three-dimensional heat conduction control equations under steady state: ; Where λ is the thermal conductivity of silicon carbide, T is the temperature field distribution, ρ is the density of silicon carbide, and c p denoted as silicon carbide specific heat capacity under constant pressure, v as laser scanning speed, x as the x-axis coordinate of the steady-state moving coordinate system, y as the y-axis coordinate of the steady-state moving coordinate system, and z as the z-axis coordinate of the steady-state moving coordinate system. Based on the aforementioned heat conduction control equation, using the formula:
5. Calculate the peak temperature rise at the center of the beam spot under the action of a single-channel Gaussian beam: where, ΔT peak ω0 is the highest temperature rise of the spot center relative to the substrate, A is the absorptivity of silicon carbide to laser, P is the beam power, ω0 is the spot radius, and α is the thermal diffusivity of silicon carbide. Based on the principle of linear superposition of temperature fields, using the formula:
6. Calculate the superimposed temperature rise at the midpoint between two adjacent beams with a spacing of d; where, ΔT mid To superimpose the temperature rise; Using the target temperature rise as a constraint, the beam power, scanning speed, and beam spacing process parameters of each zone are corrected in reverse.
7. The multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method according to claim 4, characterized in that, The steps for reverse correction of the beam power, scanning speed, and beam spacing process parameters for each zone include: Using the formula:
8. Perform beam power correction; among which, P 原 P is the initial beam power. 新 To correct the beam power, ΔT 目标 The target peak temperature rise is set; Using the formula:
9. Perform scan speed correction; where v 原 v is the initial scan speed. 新 This is the corrected scan speed; Using the formula:
10. Perform beam spacing correction; among which, d 新 The corrected beam spacing is represented by δ, which is the allowable deviation rate between the inter-channel temperature and the peak temperature.
11. The multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method according to claim 1, characterized in that, A load balancing scheduling algorithm is used to allocate processing areas and process parameters to multiple laser heads; the load balancing scheduling algorithm supports switchable master-slave function beam splitting mode and partitioned parallel scanning mode. The master-slave functional beam splitting mode is used for single-path multi-process coupling scenarios where multiple laser processing functions need to be completed sequentially on the same scanning trajectory, and preheating and modification processing are completed synchronously in a single scan. The partitioned parallel scanning mode is used for large planar processing scenarios where the processing area can be divided into multiple non-interfering sub-regions, and multi-beam regional synchronous processing is used to improve overall efficiency.
12. The multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method according to claim 1, characterized in that, During the processing, the laser modification state data of the ingot is collected in real time, and the process parameters of each zone are dynamically corrected based on the state deviation. After the processing is completed, the characteristic data, process parameters, modification state data and processing quality data of the ingot are fed back to the process database to iteratively optimize the parameter matching model and the multi-beam thermal coupling correction model.
13. The multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method according to claim 7, characterized in that, Plasma spectroscopy and infrared thermography were used to characterize the modified state of the crystal ingot; The plasma spectroscopy is used to obtain data on the intensity of spectral lines of characteristic elements, plasma electron temperature and electron number density, reflecting the degree of material ablation, energy absorption efficiency and internal defect state. The infrared thermal imaging is used to acquire data on the peak temperature of the processing point, the temperature distribution of the heat-affected zone, and the rate of temperature change, reflecting the degree of phase transformation, the level of thermal stress, and the thermal accumulation effect.
14. The multi-beam coordinated polycrystalline silicon carbide laser energy adaptive cutting method according to claim 7, characterized in that, Methods for dynamically adjusting process parameters for each zone include: A mapping table of state deviation rate to parameter correction amount is generated in advance through process calibration; After calculating the deviation between the state quantity and the target value in real time, the correction value is output by looking up the table; the correction priority is to adjust the laser power first, and then adjust the scanning speed after the power reaches the limit.
15. A multi-beam synergistic polycrystalline silicon carbide laser energy adaptive cutting system, characterized in that, include: A matrix-type intelligent ingot plate is used to support multiple crystal ingots for crystal ingot positioning, adsorption, and working condition data collection. The global pre-detection module is used to scan the resistivity, thickness, surface morphology and lattice defects of all crystal ingots on the matrix-type intelligent ingot plate, and after dividing the data according to the loading work position, it generates independent feature data for each crystal ingot; the feature data includes overall feature data and internal feature distribution data; The parameter matching module is used to perform inter-ingot process matching based on the overall feature data of each crystal ingot and output the basic process parameters of the whole ingot; it also performs feature partitioning within a single crystal ingot based on the feature distribution data within the single crystal ingot and matches the corresponding initial partition process parameters for each partition using the parameter matching model. The parameter correction module introduces a multi-beam thermal coupling correction model to calculate the temperature field superposition effect of multi-beam collaborative processing, and reversely corrects the beam power, scanning speed and beam spacing in the initial process parameters of each partition to obtain the final process parameters of each partition. The multi-beam laser processing module is used to allocate processing areas and process parameters to multiple laser heads based on the final process parameters of each zone, and control the multi-beams to work together to complete the laser cutting of the crystal ingot.
Citation Information
Patent Citations
Method and apparatus for high efficiency laser cutting of silicon carbide ingots
CN117283152B