Mold for saving water nozzle material

By eliminating the cold runner system in the fine-gate mold and adopting a transfer runner and ejection mechanism, the problems of excessive sprue material and long flow paths are solved, achieving material savings and improved production efficiency, while ensuring the appearance quality of the plastic parts.

CN123150221APending Publication Date: 2026-11-24DONGGUAN HUAJING POWDER METALLURGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611270934.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-20
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing sprue molds with cold runner systems result in excessive sprue material, leading to material waste. Furthermore, the excessively long melt flow path results in low production efficiency, and the limited placement of hot runners affects the appearance of the plastic parts.

Method used

The independent cold runner system is eliminated, and a transfer runner is directly set inside the front mold plate. The hot nozzle outlet is connected to the transfer runner inlet, and the melt is directly delivered to the inner side wall of the cavity. Combined with the ejection mechanism, the plastic part and the sprue are demolded independently.

Benefits of technology

It effectively reduces sprue generation, shortens the flow path, improves production efficiency, ensures the appearance quality of plastic parts, and reduces material waste and production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123150221A_ABST
    Figure CN123150221A_ABST
Patent Text Reader

Abstract

This invention relates to the field of injection mold technology, and more particularly to a mold that saves sprue material. The mold includes a faceplate, a hot runner plate, a front mold plate, and a rear mold plate. The front and rear mold plates enclose a cavity. A hot runner nozzle is connected to the hot runner plate. The hot runner nozzle passes through the front mold plate, which has a transfer runner. The outlet of the hot runner nozzle is connected to the inlet of the transfer runner. The outlet of the transfer runner extends to the inner wall of the cavity and forms a point gate. This invention eliminates the independent cold runner system. By using the transfer runner inside the front mold plate to achieve point gate injection into the cavity, the length of the runner is effectively reduced, sprue material generation is reduced, and raw material loss is decreased. Simultaneously, it ensures that there are no gate marks on the outer surface of the plastic part. This effectively solves the technical problem in the prior art where fine-sprue molds use a cold runner system to meet the surface processing requirements of the plastic part, resulting in excessive sprue material and material waste.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of injection mold technology, and in particular to a mold that saves sprue material. Background Technology

[0002] Injection molds are molding fixtures used to fill molten plastic into a cavity, where it cools and solidifies to form a plastic part. The molten material is delivered through a gating system, and the part is formed and demolded using mechanisms such as parting and ejection. Depending on the structure of the gating system, molds can be classified into different structural forms, such as large gate and small gate molds. Small gate molds (also known as three-plate molds) allow for point injection, leaving no obvious gate marks on the surface of the plastic part. They are often used in injection molding of plastic parts where a strict appearance requirement is present.

[0003] like Figures 1 to 4 As shown, the existing fine-gate mold mainly includes a panel 1, a hot runner plate 2, a sprue plate 3, a front mold plate 4, and a rear mold plate 5 arranged sequentially from top to bottom. The rear mold plate 5 and the front mold plate 4 close to form a cavity 6. During injection molding, the molten material enters the constant-temperature hot runner plate 2 through the injection nozzle of the injection molding machine, enters the cold runner system located between the sprue plate 3 and the front mold plate 4 through the hot nozzle 9, and then is distributed to each injection nozzle 8 through the flow divider 7 in the cold runner system. The material is then delivered to the corresponding dispensing head through the injection nozzle 8, and finally enters the cavity 6 through the dispensing head to fill and form the mold. During mold opening, the mold first separates between the sprue plate 3 and the front mold plate 4. The sprue plate 3 fixes the entire section of cold runner solidified material (i.e., sprue material), including the flow divider 7, injection nozzle 8, and dispensing head, to one side via the pull rod. As the parting action continues, each dispensing head is forcibly pulled off from the plastic part in the cavity 6. At the same time, the tip of the hot nozzle 9 is pulled away from the inlet of the cold runner solidified material, completing the hot nozzle material cutting. After that, the sprue plate 3 continues to retract to the preset stroke, scraping the cold runner solidified material off the pull rod, realizing the automatic fall of waste material. Finally, the front mold plate 4 separates from the rear mold plate 5, the plastic part remains in the rear mold plate 5, and is ejected by the ejection mechanism.

[0004] While the aforementioned mold can achieve automatic detachment of the cold runner solidified material, meeting the appearance requirements for injection molding, it still presents the following problems in actual production applications: Firstly, to meet the injection molding requirements, the molten material, after leaving the hot runner system, must flow through multiple sections of the cold runner system, including the manifold, injection nozzle, and dispensing head, before entering the cavity. After each injection molding process, the molten material in the cold runner system solidifies into sprue solidified material during cooling, generating a large amount of sprue waste. This waste cannot become the final plastic part, resulting in raw material waste and increased production costs. Secondly, the addition of the cold runner system as a transition leads to a longer overall flow path of the molten material from the hot nozzle to the molding cavity. This excessively long flow path not only increases the flow resistance of the melt but also slows down the filling process, resulting in longer single injection cycles and lower production efficiency.

[0005] If the cold runner system is directly eliminated and the hot nozzle tip is used as the injection gate, the continuous high temperature of the hot nozzle will make it difficult for the plastic at the gate position to cool and solidify quickly. During the mold opening process, defects such as stringing and cracking of the gate are likely to occur. At the same time, the continuous high temperature will bake the area around the gate of the cavity, which will form obvious heat ring marks or color differences on the surface of the plastic part, affecting the appearance quality of the plastic part.

[0006] Furthermore, conventional hot runner gates are all located on the fixed mold side of the mold, with the hot runner corresponding to the outer surface of the cavity. The hot runner manifold and heating components are fixedly assembled on the fixed mold plate. Due to the spatial constraints of the fixed mold side, the hot runner can only inject material from the outer surface of the plastic part. If, in order to avoid gate marks on the outer surface of the plastic part, a gate is chosen to be opened on the inner wall of the plastic part, the gate position is located inside the cavity. This area is surrounded by the solid plastic part, and there is not enough space to arrange the hot runner, manifold, its wiring, and heating components. The hot runner cannot directly extend into the inner cavity to complete the inner wall injection. Forcing its placement will also cause structural interference with the core. Summary of the Invention

[0007] This invention provides a mold that saves sprue material, thereby solving the technical problem in the prior art where fine sprue molds with cold runner systems generate a lot of sprue material and lead to material waste in order to meet the surface processing requirements of plastic parts.

[0008] To solve the above problems, the mold for saving sprue material provided by the present invention adopts the following technical solution:

[0009] A mold for saving sprue material includes a panel, a hot runner plate, a front mold plate, and a rear mold plate. The front mold plate and the rear mold plate enclose a cavity. The hot runner plate is connected to a hot nozzle. The hot nozzle passes through the front mold plate. A transfer channel is provided in the front mold plate. The outlet of the hot nozzle is connected to the inlet of the transfer channel. The outlet of the transfer channel extends to the inner wall of the cavity and forms a point gate.

[0010] The beneficial effects of the sprue-saving mold provided by this invention are as follows: By eliminating the independent cold runner system and corresponding sprue plate configured in existing fine sprue molds, the transfer runner is directly set inside the front mold plate, and the hot runner is inserted into the front mold plate. The outlet of the hot runner is directly connected to the inlet of the transfer runner. After the melt is output from the hot runner plate through the hot runner, it only needs to pass through the transfer runner inside the front mold plate to be transported to the point gate position on the inner side wall of the cavity and fill the cavity. Compared with the cold runner system with a large span and many segments in the prior art, the transfer runner of this application is integrated and arranged inside the front mold plate, shortening the overall length of the transfer runner. The sprue solidification formed after injection molding and cooling only comes from the limited melt volume inside the transfer runner, effectively reducing the amount of sprue generated, thereby solving the problem of raw material waste caused by excessive sprue. Meanwhile, the outlet of the transfer channel extends to the inner wall of the cavity to form a point gate, which can realize the injection of plastic on the inside of the plastic part, ensuring that there are no gate marks on the outer surface of the plastic part, and still meeting the appearance molding requirements of the plastic part.

[0011] In summary, the present invention effectively solves the technical problem in the prior art where the cold runner system of the fine gate mold is set to meet the processing requirements of the outer surface of the plastic part, resulting in a large amount of gate material and material waste.

[0012] Furthermore, an ejection mechanism is provided below the rear template. The ejection mechanism includes a product ejector pin and a sprue ejector pin. The top of the product ejector pin faces the cavity, and the top of the sprue ejector pin faces the transfer channel.

[0013] Beneficial effects: By setting an ejection mechanism including part ejector pins and sprue ejector pins below the rear mold plate, the part ejector pins apply ejection force to the plastic part inside the cavity, achieving reliable demolding of the molded plastic part; the sprue ejector pins are arranged facing the transfer runner, and can push the sprue material formed by cooling in the transfer runner, so that the sprue material can be separated from the mold. Through the division of labor and cooperation between the part ejector pins and the sprue ejector pins, the molded plastic part and the sprue material can be demolded independently, avoiding the sprue material from being stuck inside the mold and causing mold jamming failure, and ensuring that the mold can carry out continuous and stable injection molding production.

[0014] Furthermore, the transition channel is disposed on the parting surface of the front template and the rear template. When the mold is opened, the front template and the rear template are separated, and the sprue ejector pin is used to eject the solidified sprue material in the transition channel.

[0015] Beneficial effects: By arranging the transition runner on the parting surface of the front and rear mold plates, the front and rear mold plates separate during mold opening. The solidified sprue material formed in the transition runner can remain on the moving mold side during the parting action, facilitating the ejector pin's push-out operation. The sprue ejector pin can eject the solidified sprue material from the parting surface, preventing sprue material from remaining in the mold runner and causing jamming. This ensures that the two processes of plastic part molding and sprue material demolding do not interfere with each other, which is conducive to the automated continuous injection molding operation of the mold.

[0016] Furthermore, a nozzle is provided inside the front template, the nozzle is connected to the hot nozzle, and the nozzle is provided with the transfer channel.

[0017] Beneficial effects: By setting the nozzle connected to the hot nozzle inside the front template and setting the transfer channel inside the nozzle, there is no need to process the channel on the front template. This makes it easier to process, repair and replace the transfer channel. When the transfer channel is worn or clogged by material accumulation, maintenance can be completed by simply disassembling the nozzle. There is no need to disassemble the entire front template, which reduces the difficulty of mold processing and subsequent maintenance.

[0018] Furthermore, the nozzle has a Y-shaped structure, including a connecting section connected to the hot nozzle, and a first branch and a second branch respectively connected to the connecting section. The first branch and the second branch are arranged at an angle. The first branch is provided with the transfer channel, and the second branch is provided with the cold material channel. The top of the sprue pin faces the cold material channel.

[0019] Beneficial effects: The Y-shaped nozzle structure allows the molten material to be delivered to the connecting section via a hot nozzle and then split into two paths. One path flows through the transfer channel inside the first branch to the mold cavity for filling, while the other path flows into the cold slug channel of the second branch. The cold slug channel can accommodate the molten material at a lower temperature during the initial injection molding process, preventing cold slug from directly entering the mold cavity and causing defects in the molded part's appearance. At the same time, the solidified material formed by the cold slug channel provides a stable pushing force position for the sprue ejector pins, facilitating the ejector pins to push out the sprue material as a whole, reducing the risk of scrap breakage and retention inside the mold, and ensuring the stability of the mold production process.

[0020] Furthermore, the ejection mechanism also includes a pin panel and a pin base plate that are fixed to each other, and the bottom end of the product pin and the bottom end of the sprue pin are both fixed between the pin panel and the pin base plate.

[0021] Beneficial effects: By fixing the ejector plate and ejector base plate together, and fixing the bottom ends of the ejector pins and sprue pins together between them, synchronous assembly and positioning of the two types of ejector pins can be achieved. This ensures that the ejector pins and sprue pins can complete the ejection and resetting actions synchronously, keeping the ejection actions of the plastic part and sprue material consistent in timing. This avoids problems such as whitening of the ejector pins, gate scratches, or sprue material residue caused by asynchronous ejection. At the same time, after the ejector plate and ejector base plate are fixed together, they can form a stable axial limit and support for the ejector pins, reducing axial movement or radial runout of the ejector pins during repeated ejection and resetting, improving the overall rigidity and motion accuracy of the ejection mechanism, and helping to extend the service life of the ejector pins and mold.

[0022] Furthermore, it also includes a reset assembly, which includes a reset rod and a spring sleeved on the outside of the reset rod; the bottom end of the reset rod is connected to the ejector plate, and the top end passes through the rear template and is connected to the front template.

[0023] Beneficial effects: By setting up a reset assembly consisting of a reset rod and a spring, where the bottom end of the reset rod is connected to the ejector platen and the top end passes through the rear mold platen and connects to the front mold platen, the front mold platen pushes the reset rod during mold closing, causing the ejector platen, along with the ejector pins in the mold and the sprue pins, to retract synchronously. This ensures that each ejector pin accurately returns to its initial position before the cavity closes. The spring, sleeved outside the reset rod, provides auxiliary thrust during the reset process and maintains the stability of the ejector platen position after mold opening and ejection, preventing abnormal extension of the ejector pins due to gravity or inertia. This structure is compact, does not occupy additional mold platen space, and the reset action is directly driven by the closing stroke of the front mold platen, ensuring reliable timing. It effectively avoids collisions and interference between the ejector pins and the cavity or front mold platen, guaranteeing the safety of the mold closing action and the long-term stable operation of the ejection mechanism during continuous injection molding.

[0024] Furthermore, the outlet of the transfer channel is formed as a submarine gate or a horn gate, which obliquely penetrates the core side of the cavity.

[0025] Beneficial effects: By setting the runner outlet as a submarine gate or a horn gate, with the gate angled to penetrate the core side of the cavity, the gate can be located inside the plastic part. After injection molding, the gate can be automatically cut off during the mold opening and ejection process, eliminating the need for manual removal of the sprue head. Simultaneously, setting the outlet as a submarine gate or a horn gate ensures a clean and intact outer surface of the plastic part, leaving no obvious gate marks. The angled gate channel facilitates smooth melt flow into the cavity, reducing molding defects caused by melt jetting and turbulence, and meeting the injection molding requirements of plastic parts with high appearance requirements.

[0026] Furthermore, the hot runner plate is connected to a plurality of hot nozzles, each hot nozzle corresponding to a cavity.

[0027] Beneficial effects: The hot runner plate connects to several hot nozzles simultaneously, each corresponding to a cavity. Molten metal can be supplied to multiple cavities simultaneously through a single hot runner plate, maximizing the utilization of the mold's internal space. This allows for the simultaneous molding of multiple plastic parts in a single injection cycle. While ensuring consistent feeding conditions in each cavity, it effectively increases the output per injection cycle, improving overall injection molding efficiency and reducing the molding cost per part. Furthermore, with each cavity supplied by an independent hot nozzle, the molten metal's path from the hot runner plate to each cavity is more direct, eliminating the need for a shared, long cold runner. This increases the number of parts molded per mold while reducing molten metal residue and sprue buildup in non-product areas. The one-to-one correspondence between hot nozzles and cavities also helps to balance the injection pressure and temperature in each cavity, reducing dimensional deviations, density differences, or appearance defects caused by inconsistent filling across multiple cavities, and improving the consistency of product quality within the same mold.

[0028] Furthermore, it also includes a temperature control system, which includes a temperature control box installed on the outer wall of the mold. The temperature control box is electrically connected to the hot nozzle and is used to control the heating temperature of the hot nozzle.

[0029] Beneficial effects: By installing a temperature control box electrically connected to the hot runner, mounted on the outer wall of the mold, it facilitates wiring, maintenance, and parameter adjustment by operators. The temperature control box allows for independent control of the hot runner's heating temperature, enabling precise adjustment based on the plastic material and molding conditions. This maintains the melt inside the hot runner in a suitable molten state, reducing abnormalities such as melt degradation and premature solidification of the sprue, ensuring stable melt delivery, and ultimately improving the quality of the molded plastic parts. Attached Figure Description

[0030] Figure 1 This is a schematic diagram of the structure of a fine sprue mold in the prior art; Figure 2 for Figure 1 Schematic diagram of the intercooler flow channel system; Figure 3 for Figure 2 Top view; Figure 4 for Figure 3 Sectional view of AA in the middle; Figure 5 This is a schematic diagram of the structure of the mold for saving sprue material provided by the present invention; Figure 6 for Figure 5 Top view; Figure 7 for Figure 6 Sectional view of AA in the middle; Figure 8 for Figure 7 A magnified view of a portion of point A in the middle; Figure 9 for Figure 6 Cross-sectional view of the middle section (BB).

[0031] Explanation of reference numerals in the attached figures: 1. Panel; 2. Hot runner plate; 3. Sprue plate; 4. Front mold plate; 5. Rear mold plate; 6. Cavity; 7. Manifold; 8. Injection nozzle; 9. Hot nozzle; 10. Panel; 11. Hot runner plate; 12. Front mold plate; 13. Rear mold plate; 14. Base plate; 15. Cavity; 16. Product ejector pin; 17. Sprue ejector pin; 18. Nozzle; 181. Connecting section; 182. First branch; 183. Second branch; 19. Ejector pin panel; 20. Ejector pin base plate; 21. Reset rod; 22. Spring; 23. Temperature control box; 24. Square iron; 25. Hot nozzle. Detailed Implementation

[0032] The principles and spirit of the present invention will be explained in detail below with reference to several representative embodiments.

[0033] An embodiment of the mold for saving sprue material provided by the present invention: like Figures 5 to 9 As shown, the mold for saving sprue material includes a panel 10, a hot runner plate 11, a front template 12, a rear template 13 and a base plate 14 arranged from top to bottom. The mold also includes a hot nozzle 25, a nozzle head 18, an ejection mechanism, a reset assembly, a temperature control system and a square iron 24.

[0034] The hot runner plate 11 is fixed below the panel 10, and the front mold plate 12 is located on the lower end face of the hot runner plate 11. After the front mold plate 12 and the rear mold plate 13 are closed, they enclose to form a cavity 15 for molding the plastic part. There are two square irons 24, which are symmetrically arranged between the rear mold plate 13 and the base plate 14. The ejector plate 19 and the ejector base plate 20 are located in the movable space enclosed by the two square irons 24. The ejection mechanism includes the ejector plate 19, the ejector base plate 20 and the ejection assembly. The ejection assembly and the reset assembly are both assembled on the ejector plate 19 and the ejector base plate 20. The temperature control system is externally connected to the side wall of the mold and electrically connected to the hot nozzle 25. The entire mold conveys molten plastic through the hot runner plate 11 and introduces the plastic into the cavity 15 through the transfer channel inside the front mold plate 12. After molding, the ejection mechanism is used to simultaneously complete the demolding operation of the plastic part and the sprue.

[0035] like Figure 5 , Figure 7 , Figure 9As shown, in this embodiment, panel 10 is located at the top of the entire mold set and is used for installation and fixation with the fixed mold side of the injection molding machine. The lower end face of panel 10 is locked and fitted with hot runner plate 11, providing an installation positioning reference for hot runner plate 11. The hot runner plate 11 has a main melt channel inside, which is used to divert and transport the molten plastic injected by the injection molding machine to each hot nozzle 25. There are eight cavities 15. Correspondingly, eight hot nozzles 25 are connected to the lower end of hot runner plate 11. Each hot nozzle 25 extends vertically downward and enters the upper area of ​​the front mold plate 12. The temperature control system includes a temperature control box 23 installed on the outer wall of the mold. The temperature control box 23 is electrically connected to the eight hot nozzles 25 and can independently adjust the heating temperature of each hot nozzle 25 to maintain the plastic inside the hot nozzle 25 in a stable molten flow state and prevent the plastic from cooling and solidifying prematurely or undergoing high-temperature degradation.

[0036] In other embodiments, the number of hot nozzles 25 connected to the hot runner plate 11 can also be set to two, four, or sixteen, etc., depending on the number of cavities 15.

[0037] In other embodiments, the temperature control box 23 can also be arranged in a separate external form, for example, the temperature control box 23 can be fixed on the side frame of the injection molding machine and electrically connected to the hot nozzle 25 in the mold through a connecting wire harness, etc.

[0038] like Figure 7 As shown, in this embodiment, the front mold plate 12 serves as the front mold forming component, and a nozzle 18 is embedded inside it. The upper end of the nozzle 18 is connected to the discharge end of the hot nozzle 25. The nozzle 18 adopts a Y-shaped structure, with a connecting section 181 connected to the hot nozzle 25 at the upper part. The connecting section 181 extends downward to branch out into a first branch 182 and a second branch 183 arranged at an angle. A transfer flow channel is opened inside the first branch 182, and the discharge port of the transfer flow channel extends to the inner side wall of the cavity 15 and forms a point gate.

[0039] In other embodiments, the nozzle 18 can also adopt a split splicing structure, for example, the connecting section 181, the first branch 182 and the second branch 183 are processed separately and then combined into a whole by threaded connection and interference fit.

[0040] In other embodiments, the transfer channel can also be directly formed inside the body of the front template 12, for example, the channel hole is formed inside the front template 12, and the discharge end of the hot nozzle 25 is directly connected to the inlet end of the transfer channel.

[0041] like Figure 8 As shown, in this embodiment, the point gate adopts a submerged structure, obliquely penetrating the core side of the cavity 15. A cold slug channel is provided inside the second branch 183 to accommodate the melt with a low initial injection temperature, preventing the cold slug from directly entering the cavity 15 and affecting the appearance quality of the plastic part. In other embodiments, the point gate can also adopt a horn-shaped structure.

[0042] like Figure 7 , Figure 9 As shown, in this embodiment, the rear template 13 serves as the rear mold forming component, and its contact surface with the front template 12 constitutes the parting surface of the mold. The transfer runner inside the nozzle 18 is arranged in the upper area of ​​the parting surface. When the mold opens, the front template 12 moves upward with the fixed mold side and separates from the rear template 13 along the parting surface. The plastic part formed inside the cavity 15 and the sprue material solidified in the transfer runner are left on the moving mold side by the rear template 13, which facilitates the subsequent ejection mechanism to perform demolding operations. The lower end face of the rear template 13 is locked and fixed to the upper end of the square iron 24, and the lower end of the square iron 24 is locked and connected to the base plate 14. The hollow area between the two square irons 24 provides lifting and lowering space for the ejection mechanism. The base plate 14 is located at the bottom of the entire mold and is used to install and fix it to the moving mold side of the injection molding machine to bear the overall weight of the mold.

[0043] like Figure 7 , Figure 8 As shown, in this embodiment, the ejection assembly includes a product ejector pin 16 and a sprue ejector pin 17. The bottom ends of both the product ejector pin 16 and the sprue ejector pin 17 are clamped and fixed between the ejector plate 19 and the ejector base plate 20. The ejector plate 19 and the ejector base plate 20 are locked together to form a whole, which can drive the product ejector pin 16 and the sprue ejector pin 17 to move up and down synchronously. The top end of the product ejector pin 16 penetrates the rear mold plate 13 upward and extends into the cavity 15 to push the molded plastic part. The top end of the sprue ejector pin 17 penetrates the rear mold plate 13 upward and is aligned with the cold sprue channel of the nozzle 18 to push the solidified sprue material. The synchronous movement of the product ejector pin 16 and the sprue ejector pin 17 can ensure that the ejection sequence of the plastic part and the sprue material is consistent, avoiding problems such as product whitening, gate scratches, or sprue material residue caused by asynchronous ejection. It should be noted that in this embodiment, the number of ejector pins 16 is the same as the number of cavities 15, and the number of sprue ejector pins 17 is also the same as the number of cavities 15.

[0044] In other embodiments, the bottom ends of the product ejector pin 16 and the sprue ejector pin 17 can also be fixed in other ways, such as by pressing with a pressure block, locking with screws, or fixing to the ejector pin panel 19 by riveting.

[0045] like Figure 5 , Figure 7 , Figure 9As shown, in this embodiment, the reset assembly includes a reset rod 21 and a spring 22. The spring 22 is sleeved on the outside of the reset rod 21. The bottom end of the reset rod 21 is fixedly connected to the ejector plate 19, and the top end of the reset rod 21 extends upward through the rear template 13 and reaches the parting surface. During mold closing, the lower end face of the front template 12 presses against the top end of the reset rod 21, pushing the reset rod 21 downward and compressing the spring 22. Simultaneously, the ejector plate 19 and the ejector base plate 20 fall back to their initial positions, so that the ejection mechanism is completely reset, avoiding collision and interference between the ejector pin and the front mold components during mold closing, and ensuring the smoothness of mold opening and closing actions.

[0046] In other embodiments, the reset assembly may also employ other reset structures, such as a built-in spring-loaded reset rod, a forced reset pull rod structure, etc.

[0047] The working principle of the mold for saving sprue material provided by this invention is as follows: First, the mold is installed and fixed on the injection molding machine. The operator sets the working temperature of the hot runner 25 through the temperature control box 23. The injection molding machine injects molten plastic into the main runner of the hot runner plate 11. After being divided, the plastic enters each hot runner 25 and is conveyed downwards along the hot runner 25 to the connecting section 181 of the nozzle 18. Then, the plastic is divided into two paths. The main melt flows smoothly into the cavity 15 through the transfer runner of the first branch 182 and the point gate on the inner wall of the cavity 15. The low-temperature cold material from the injection front flows into the cold material runner of the second branch 183 for temporary storage. After the cavity 15 is filled, it is held under pressure and cooled to solidify the plastic. The plastic part is formed, and the plastic in the transfer runner and cold runner solidifies into sprue material. After molding, the mold opens, the front mold plate 12 and the rear mold plate 13 separate along the parting surface, and the plastic part and sprue material remain on the side of the rear mold plate 13. The ejector roller of the injection molding machine pushes the ejector base plate 20 and ejector plate 19 to move upward, and the product ejector pin 16 and the sprue ejector pin 17 rise synchronously, pushing the plastic part and sprue material out of the mold respectively. After demolding, the mold closes, the front mold plate 12 presses down the reset rod 21, and drives the entire ejection mechanism back to the initial position. The spring 22 is compressed during this process, and then the next injection cycle begins.

[0048] Based on the above description in this specification, those skilled in the art will also understand that the following terms, such as "upper," "lower," "front," "back," "left," "right," "inner," and "outer," which indicate orientation or positional relationship, are based on the orientation or positional relationship shown in the accompanying drawings of this specification and should not be understood or interpreted as limiting the present invention.

[0049] In addition, in the description of this specification, "multiple" means at least two, such as two, three or more, etc., unless otherwise expressly and specifically defined.

Claims

1. A mold for saving sprue material, comprising a face plate, a hot runner plate, a front mold plate, and a rear mold plate, wherein the front mold plate and the rear mold plate enclose a cavity, and the hot runner plate is connected to a hot nozzle; characterized in that, The hot nozzle is inserted into the front template, and a transfer channel is provided in the front template. The outlet of the hot nozzle is connected to the inlet of the transfer channel, and the outlet of the transfer channel extends to the inner wall of the cavity and forms a spot gate.

2. The mold for saving sprue material according to claim 1, characterized in that, The rear template is provided with an ejection mechanism, which includes a product ejector pin and a sprue ejector pin. The top of the product ejector pin faces the cavity, and the top of the sprue ejector pin faces the transfer channel.

3. The mold for saving sprue material according to claim 2, characterized in that, The transition channel is located on the parting surface between the front template and the rear template. When the mold is opened, the front template and the rear template separate, and the sprue ejector pin is used to eject the solidified sprue material in the transition channel.

4. The mold for saving sprue material according to claim 2, characterized in that, The front template is provided with a nozzle, which is connected to the hot nozzle, and the nozzle is provided with the transfer channel.

5. The mold for saving sprue material according to claim 4, characterized in that, The nozzle has a Y-shaped structure, including a connecting section connected to the hot nozzle, and a first branch and a second branch respectively connected to the connecting section. The first branch and the second branch are arranged at an angle. The first branch is provided with the transfer channel, and the second branch is provided with the cold material channel. The top of the sprue pin faces the cold material channel.

6. The mold for saving sprue material according to claim 2, characterized in that, The ejection mechanism also includes a ejector plate and an ejector base plate that are fixed to each other, and the bottom end of the product ejector and the bottom end of the sprue ejector are both fixed between the ejector plate and the ejector base plate.

7. The mold for saving sprue material according to claim 6, characterized in that, It also includes a reset assembly, which includes a reset rod and a spring sleeved on the outside of the reset rod; the bottom end of the reset rod is connected to the ejector plate, and the top end passes through the rear template and is connected to the front template.

8. The mold for saving sprue material according to any one of claims 1 to 7, characterized in that, The outlet of the transfer channel forms a submarine gate or a horn gate, which obliquely penetrates the core side of the cavity.

9. The mold for saving sprue material according to any one of claims 1 to 7, characterized in that, The hot runner plate is connected to a plurality of hot nozzles, each hot nozzle corresponding to a cavity.

10. The mold for saving sprue material according to any one of claims 1 to 7, characterized in that, It also includes a temperature control system, which includes a temperature control box installed on the outer wall of the mold. The temperature control box is electrically connected to the hot nozzle and is used to control the heating temperature of the hot nozzle.