System and method for carbon dioxide mineralization and hydrate cooperative construction of composite caprock
By employing a method of pre-filling active leaching fluid in the upper part and independently injecting carbon dioxide in the lower part during carbon dioxide geological storage, a composite plugging zone involving both carbonate solid phase and carbon dioxide hydrate is constructed, solving the near-field blockage problem of gas injection wells and achieving dynamic control and stable plugging effect.
Patent Information
- Application Number
- CN202611644778.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-23
- Publication Date
- 2026-11-24
AI Technical Summary
In existing carbon dioxide geological storage technologies, mineral precipitation and hydrate formation may cause premature blockage of the near-field throat of the injection well, affecting the injection capacity, and there is a lack of effective dynamic control methods.
By employing a spatially staggered approach of pre-filled active leaching fluid in the upper part and independently injected carbon dioxide in the lower part, a composite plugging zone is formed with the participation of carbonate solid phase and carbon dioxide hydrate. Dynamic control is achieved through a monitoring system to ensure the stability of the near-field injection capacity and plugging layer status of the gas injection well.
While reducing the risk of near-field blockage in gas injection wells, a composite capping layer with dynamic plugging and thermal disturbance stability is constructed to extend the injection time, improve the plugging effect, and reduce the use of exogenous mineral raw materials.
Smart Images

Figure CN123151101A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of carbon dioxide geological sequestration and industrial solid waste resource utilization technology, specifically to a system and method for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates. Background Technology
[0002] Current technologies for carbon dioxide geological storage typically utilize deep saline aquifers, depleted oil and gas reservoirs, and other suitable geological bodies for long-term storage, relying on mechanisms such as structural traps, capillary sealing, residual trapping, dissolution, and mineral fixation to limit carbon dioxide migration. During engineering implementation, the continuity of the natural caprock, fracture structures, wellbore integrity, and pressure disturbances caused by long-term injection can all affect storage safety. Therefore, it is necessary to establish monitorable and controllable additional sealing barriers within the reservoir-caprock system.
[0003] In low-temperature, high-pressure formations or submarine sedimentary environments, when local temperature, pressure, and salinity conditions are within the carbon dioxide hydrate stability zone, upward-migrating carbon dioxide can form hydrates with pore water. Hydrates can occupy pores and throats, reduce flow channel connectivity, and retain carbon dioxide, but their stability is affected by temperature, pressure, and salinity. When the system approaches or crosses the hydrate stability boundary, localized heating, pressure reduction, or thermal disturbances may cause partial decomposition of hydrates and reduce their sealing capacity. Mineral carbonation can convert carbon dioxide into a relatively stable carbonate solid phase. Industrial solid wastes such as carbide slag, steel slag, magnesium slag, and some tailings contain usable calcium and magnesium components. Leaching and solid-liquid separation can yield active leachates containing calcium and / or magnesium ions, providing exogenous reactive components for in-situ formation mineralization. However, if the highly reactive liquid phase directly contacts carbon dioxide in the near-field of the injection well, mineral precipitation and hydrate formation may concentrate in the near-wellbore area, causing premature pore throat blockage and reducing continuous injection capacity.
[0004] Existing hydrate storage technologies have proposed field configurations that combine liquid injection, gas injection, and monitoring. Mineralization technologies have also utilized calcium-containing media to react with carbon dioxide to form carbonate solid phases. However, how to directionally transfer the mineralization and hydrate plugging effects of active leachate from solid waste to a predetermined layer far from the gas injection well, and how to dynamically regulate the composite plugging layer based on the stratified temperature, pressure, and geophysical response, still requires further solutions.
[0005] Therefore, a composite caprock construction method for on-site geological engineering is needed: first, calcium- and / or magnesium-containing active leaching solutions are pre-placed in the upper target layer, and then carbon dioxide is independently injected in the lower layer, so that the carbon dioxide enters the pre-placed reaction zone along the migration path, forming a composite plugging zone in which carbonate solid phase and carbon dioxide hydrate participate under suitable conditions, while retaining space for monitoring and adjusting the near-field injection capacity of the gas injection well and the state of the plugging layer. Summary of the Invention
[0006] To address the problems existing in the prior art, this invention provides a system and method for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates. By pre-positioning an active leaching solution above the target formation and independently injecting carbon dioxide below, the main mineralization-hydrate reaction zone is transferred to a predetermined overlying layer, thereby reducing the risk of premature blockage in the near-field of the injection well while constructing a composite caprock with dynamic plugging and residual stability against thermal disturbances. To achieve the above objectives, this invention adopts the following technical solution:
[0007] In a first aspect, a system for synergistically constructing a composite caprock through carbon dioxide mineralization and hydrates according to some embodiments of this application includes:
[0008] Surface solid waste treatment system, used to crush and grind industrial solid waste to obtain solid waste residue;
[0009] The leachate preparation and supply system is connected to the surface solid waste treatment system and is used to leach the solid waste residue to obtain an active leachate and to transport the active leachate.
[0010] Carbon dioxide storage system, used to store carbon dioxide;
[0011] A carbon dioxide supply control system, connected to the carbon dioxide storage system, is used to transport carbon dioxide and adjust carbon dioxide transport parameters;
[0012] A differentiated injection system includes a liquid injection well and a gas injection well. The liquid injection well is connected to the leaching solution preparation and supply system and is used to inject active leaching solution into the liquid injection layer of the target formation. The gas injection well is connected to the carbon dioxide supply and control system and is used to inject carbon dioxide into the gas injection layer of the target formation. The gas injection layer is located below the liquid injection layer, and an isolation layer is provided between the gas injection layer and the liquid injection layer.
[0013] A monitoring system, installed within the target formation, is used to detect the reaction data of the target formation;
[0014] The control system is connected to the extract preparation and supply system, the carbon dioxide supply regulation system, and the monitoring system. It is used to adjust the parameters of the extract preparation and supply system and the carbon dioxide supply regulation system according to the reaction data fed back by the monitoring system, thereby adjusting the injection parameters of the active extract and / or carbon dioxide.
[0015] According to some embodiments of this application, a system for synergistically constructing a composite caprock through carbon dioxide mineralization and hydrates is provided. The surface solid waste treatment system includes a solid waste crusher and a solid waste grinder connected in sequence. The solid waste crusher is used to crush the industrial solid waste to obtain industrial solid waste fragments. The solid waste grinder is used to grind the industrial solid waste fragments to obtain solid waste residue. The solid waste grinder is connected to the leachate preparation and supply system.
[0016] According to some embodiments of this application, a system for synergistically constructing a composite cap layer through carbon dioxide mineralization and hydrates includes a leachate preparation and supply system comprising a stirred leaching vessel, a solid-liquid separation device, a leaching residue treatment device, a leaching solution detection and conditioning device, a leaching solution storage tank, and an injection and pressurization pump. The stirred leaching vessel is connected to a solid waste grinding mill and is used to leach the solid waste residue using a leaching agent to obtain leaching residue and the active leaching solution. The solid-liquid separation device is connected to both the leaching residue treatment device and the leaching solution detection and conditioning device, and is used to separate the active leaching solution and the leaching residue. The solid phase outlet of the solid-liquid separation device is connected to the leaching solution. The leaching residue treatment device is connected to the solid-liquid separation device, and the liquid phase outlet of the solid-liquid separation device is connected to the leaching solution detection and conditioning device. The leaching residue treatment device is used to collect and dry the leaching residue. The leaching solution detection and conditioning device is used to detect one or more of the following in the active leaching solution: calcium ion concentration, magnesium ion concentration, pH value, conductivity, and alkalinity, and obtain the detection results. The leaching solution detection and conditioning device is connected to the leaching solution storage tank, which is used to store the active leaching solution. One end of the injection pressurization pump is connected to the leaching solution storage tank, and the other end is connected to the injection well. The injection pressurization pump is used to pump the active leaching solution into the injection well.
[0017] According to some embodiments of this application, a system for synergistically constructing a composite caprock by carbon dioxide mineralization and hydrate is provided. The carbon dioxide storage system includes a gas storage tank and a gas monitoring device connected in sequence. The gas storage tank is used to store carbon dioxide. The gas monitoring device is connected to the carbon dioxide supply control system and is used to monitor the concentration of carbon dioxide.
[0018] According to some embodiments of this application, a system for synergistically constructing a composite caprock through carbon dioxide mineralization and hydrates is provided. The carbon dioxide supply control system includes a flow control valve group and a gas pressurizing pump connected in sequence. One end of the flow control valve group is connected to the gas monitoring device, and the other end is connected to the gas pressurizing pump. The flow control valve group is used to control the flow rate of carbon dioxide. The gas pressurizing pump is connected to the injection well and is used to adjust the delivery pressure of carbon dioxide and pump carbon dioxide into the injection well.
[0019] According to some embodiments of this application, a system for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates is provided at the downhole end of the injection well. The liquid distribution and diffusion device is used to allow the active leachate to diffuse laterally within the injection layer to form a pre-set reaction zone.
[0020] According to some embodiments of this application, a system for synergistically constructing a composite caprock through carbon dioxide mineralization and hydrates is provided. The monitoring system includes a monitoring well, and temperature monitoring units, pressure monitoring units, and geophysical monitoring units are provided at different depths along the monitoring well. The temperature monitoring unit is used to monitor the temperature of the target formation, obtain temperature monitoring results, and transmit the temperature monitoring results to the control system. The pressure monitoring unit is used to monitor the pressure of the target formation, obtain pressure monitoring results, and transmit the pressure monitoring results to the control system. The geophysical monitoring unit is used to monitor the target formation, obtain geophysical monitoring results, and transmit the geophysical monitoring results to the control system.
[0021] According to some embodiments of this application, a system for synergistically constructing a composite caprock by carbon dioxide mineralization and hydrates is provided, wherein the geophysical monitoring results include one or more of the following: resistivity tomography results, acoustic wave monitoring results, microseismic monitoring results, acoustic emission monitoring results, and distributed optical fiber monitoring results.
[0022] According to some embodiments of this application, a system for synergistically constructing a composite caprock through carbon dioxide mineralization and hydrates is provided. The control system includes a monitoring computer connected to the injection pressurization pump, flow control valve group, gas pressurization pump, temperature monitoring unit, pressure monitoring unit, and geophysical monitoring unit.
[0023] In a second aspect, the method for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates according to some embodiments of this application is characterized in that the construction of the composite caprock using the above-described system includes the following steps:
[0024] S1. Industrial solid waste is crushed and ground through a surface solid waste treatment system to obtain solid waste residue. The solid waste residue is then leached, separated into solid and liquid and tested and conditioned through a leachate preparation and supply system to obtain an active leachate and deliver the active leachate.
[0025] S2. The active leachate is injected into the injection layer of the target formation through an injection well and a liquid distribution and diffusion device to form a pre-set reaction zone;
[0026] S3. Inject carbon dioxide into the gas injection zone of the target formation through the gas injection well, causing the carbon dioxide plume to migrate upward and enter the pre-set reaction zone;
[0027] S4. Collect temperature, pressure and / or geophysical response of the target formation through monitoring wells, and adjust the injection parameters of the active leachate and / or carbon dioxide accordingly.
[0028] The system and method for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates, as described in this invention, employs a spatial decoupling approach: an upper injection of fluid to form a pre-set reaction zone, and an independent injection of carbon dioxide at the lower level. This keeps the main contact area between the active leachate and carbon dioxide away from the near-field of the injection well, facilitating the directional transfer of the composite sealing effect to the pre-set composite caprock area while maintaining the injection channel. Calcium and / or magnesium ions in the active leachate provide mineralization reaction components, while the aqueous phase in the pre-set reaction zone provides conditions for carbon dioxide hydrate formation. Within areas satisfying phase equilibrium and hydrochemical conditions, the carbonate solid phase and carbon dioxide hydrate jointly participate in pore filling and seepage channel reconstruction, thereby forming a composite caprock with both rapid response and residual sealing capacity after disturbance. This invention does not evaluate the caprock state based on a single hydrate formation amount or a single outlet leakage amount. Instead, it identifies the pressure front and potential weak zones through stratified temperature, pressure, and optional geophysical monitoring, providing a basis for adjusting injection intensity, injection mode, or implementing local fluid replenishment. When enhanced local pressure transmission, abnormal carbon dioxide migration, or other signals in weak areas are detected in the composite caprock, local re-sealing can be achieved by supplementing the active leachate and / or adjusting the carbon dioxide supply to induce secondary carbonate mineralization and / or carbon dioxide hydrate regeneration in the weak areas. The coupling of industrial solid waste resource utilization with carbon dioxide geological sequestration reduces the use of exogenous mineralization materials while providing an engineerable composite sealing pathway for low-temperature seafloor sedimentary layers, low-temperature aquifers, and other geological bodies that meet the stability conditions for carbon dioxide hydrates. Attached Figure Description
[0029] Figure 1 This is a schematic diagram of the system for constructing a composite capping layer by synergistically combining carbon dioxide mineralization and hydrates according to the present invention.
[0030] In the diagram: 1. Solid waste crusher, 2. Solid waste grinder, 3. Stirring leaching vessel, 4. Solid-liquid separation device, 5. Leaching residue treatment device, 6. Leaching solution detection and conditioning device, 7. Injection pressurizing pump, 8. Leaching solution storage tank, 9. Gas storage tank, 10. Gas monitoring device, 11. Flow control valve group, 12. Gas pressurizing pump, 13. Monitoring computer, 14. Injection well, 15. Gas injection well, 16. Monitoring well, 17. Injection layer, 18. Gas injection layer, 19. Liquid distribution and diffusion device, 20. Temperature monitoring unit, 21. Pressure monitoring unit, 22. Geophysical monitoring unit, 23. Isolation layer, 24. Carbon dioxide plume, 25. Composite sealing zone. Detailed Implementation
[0031] The embodiments of the present invention will be described in further detail below with reference to the accompanying drawings and examples. The following examples are for illustrative purposes only and should not be construed as limiting the scope of the invention.
[0032] Example 1: This example describes a system for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates. Figure 1 As shown, the system includes a surface solid waste treatment system, a leachate preparation and supply system, a carbon dioxide storage system, a carbon dioxide supply regulation system, a differentiated injection system, a monitoring system, and a control system. Specifically, the surface solid waste treatment system is used to crush and grind industrial solid waste to obtain solid waste residue; the leachate preparation and supply system is connected to the surface solid waste treatment system and is used to leach the solid waste residue to obtain active leachate, and to transport the active leachate; the carbon dioxide storage system is used to store carbon dioxide; the carbon dioxide supply regulation system is connected to the carbon dioxide storage system and is used to transport carbon dioxide and regulate carbon dioxide transport parameters; the differentiated injection system includes injection well 14 and gas injection well 15. Injection well 14 is connected to the leachate preparation and supply system and is used to inject active leachate into the injection layer 17 of the target formation; gas injection well 15... Connected to the carbon dioxide supply control system, it is used to inject carbon dioxide into the gas injection layer 18 of the target formation. The gas injection layer 18 is located below the liquid injection layer 17, and an isolation layer 23 is provided between the gas injection layer 18 and the liquid injection layer 17. Specifically, the isolation layer 23 is not limited to a fixed value and can be determined according to the porosity, permeability, heterogeneity, carbon dioxide migration characteristics, leaching fluid diffusion range, and near-wellbore blockage risk of the target formation. The monitoring system is set in the target formation to detect the reaction data of the target formation. The control system is connected to the leaching fluid preparation and supply system, the carbon dioxide supply control system, and the monitoring system. It is used to adjust the parameters of the leaching fluid preparation and supply system and the carbon dioxide supply control system according to the reaction data fed back by the monitoring system, thereby adjusting the injection parameters of the active leaching fluid and / or carbon dioxide.
[0033] Specifically, the surface solid waste treatment system includes a solid waste crusher 1 and a solid waste grinder 2 connected in sequence. The solid waste crusher 1 is used to crush industrial solid waste to obtain industrial solid waste fragments. The solid waste grinder 2 is used to grind the industrial solid waste fragments to obtain solid waste residue. The solid waste grinder 2 is connected to a leaching solution preparation and supply system, and the solid waste grinder 2 transports the solid waste residue to the leaching solution preparation and supply system. As a preferred embodiment, the industrial solid waste can be one or more of the following: carbide slag, steel slag, fly ash, red mud, magnesium slag, phosphorus slag, calcium-containing tailings, and magnesium-containing tailings.
[0034] Specifically, the leachate preparation and supply system includes a stirred leaching vessel 3, a solid-liquid separation device 4, a leaching residue treatment device 5, a leaching solution detection and conditioning device 6, a leaching solution storage tank 8, and a liquid injection and pressurization pump 7. The stirred leaching vessel 3 is connected to the solid waste grinding mill 2. The stirred leaching vessel 3 is used to leach solid waste residue with a leaching agent to obtain leaching residue and active leachate. During the leaching process, calcium- and magnesium-containing components enter the liquid phase. The active leachate contains calcium ions and / or magnesium ions that can participate in the carbonate mineralization reaction. The solid-liquid separation device 4 is connected to the leaching residue treatment device 5 and the leaching solution detection and conditioning device 6, respectively. The solid-liquid separation device 4 is used to separate the active leachate and the leaching residue. The solid phase outlet of the solid-liquid separation device 4 is connected to the leaching residue treatment device 5 to process the leaching residue. The leaching residue is conveyed to the leaching residue treatment device 5. The liquid phase outlet of the solid-liquid separation device 4 is connected to the leaching solution detection and conditioning device 6, which conveys the active leaching solution to the leaching solution detection and conditioning device 6. The leaching residue treatment device 5 is used to collect and dry the leaching residue. The leaching solution detection and conditioning device 6 is used to detect one or more of the following in the active leaching solution: calcium ion concentration, magnesium ion concentration, pH value, conductivity, and alkalinity, and obtain the detection results. The leaching solution detection and conditioning device 6 is connected to the leaching solution storage tank 8, which conveys the active leaching solution to the leaching solution storage tank 8. The leaching solution storage tank 8 is used to store the active leaching solution. One end of the injection pressurization pump 7 is connected to the leaching solution storage tank 8, and the other end is connected to the injection well 14. The injection pressurization pump 7 is used to pump the active leaching solution into the injection well 14.
[0035] As a preferred embodiment, the stirred leaching vessel 3 uses a water-based medium, an acidic medium, a weakly acidic organic ligand solution, or a combination thereof to leach solid waste residue; after solid-liquid separation of the active leaching solution, the pH, alkalinity, salinity, and / or suspended solids content of the active leaching solution are adjusted according to the salinity, hydrate stability boundary, and mineralization requirements of the target formation.
[0036] Specifically, the carbon dioxide storage system includes a gas storage tank 9 and a gas monitoring device 10 connected in sequence; the gas storage tank 9 is used to store carbon dioxide, and the gas storage tank 9 can store gaseous, liquid or high-density carbon dioxide; the gas monitoring device 10 is connected to the carbon dioxide supply control system, and the gas monitoring device 10 is used to monitor the concentration of carbon dioxide. In addition, the gas monitoring device 10 can also monitor the pressure, temperature and flow rate of carbon dioxide.
[0037] Specifically, the carbon dioxide supply control system includes a flow control valve group 11 and a gas pressurization pump 12 connected in sequence. One end of the flow control valve group 11 is connected to the gas monitoring device 10, and the other end is connected to the gas pressurization pump 12. The flow control valve group 11 is used to control the flow rate of carbon dioxide. The gas pressurization pump 12 is connected to the injection well 15. The gas pressurization pump 12 is used to adjust the delivery pressure of carbon dioxide and pump carbon dioxide into the injection well 15. The gas pressurization pump 12 is used to realize continuous injection, intermittent injection or pulse injection of carbon dioxide. The injection pressure is constrained by the target formation fracture pressure or the preset safety pressure upper limit.
[0038] Specifically, a fluid distribution and diffusion device 19 is provided at the downhole end of the injection well 14. The fluid distribution and diffusion device 19 is used to diffuse the active leaching fluid laterally within the injection layer 17, thereby forming a pre-set reaction zone within the injection layer 17. As a preferred embodiment, the fluid distribution and diffusion device 19 can be one or more of a porous fluid distribution section, a perforated section, a radial branch section, a short horizontal fluid distribution section, or a segmented controllable fluid output assembly. The injected carbon dioxide forms a carbon dioxide plume 24 within the gas injection layer 18 and migrates upward into the pre-set reaction zone. Within the pre-set reaction zone, carbon dioxide reacts with calcium ions and / or magnesium ions in the active leaching fluid to undergo a carbonate mineralization reaction, and carbon dioxide hydrate is generated in the pore region that meets the stability conditions of carbon dioxide hydrate. This allows the carbonate solid phase and carbon dioxide hydrate to participate in pore filling and seepage channel reconstruction, forming a composite plugging zone 25. The composite plugging zone 25 constitutes the cap layer, and the reservoir is located below the cap layer.
[0039] Specifically, the monitoring system includes a monitoring well 16, with a temperature monitoring unit 20, a pressure monitoring unit 21, and a geophysical monitoring unit 22 arranged at different depths along the monitoring well 16. The temperature monitoring unit 20 monitors the temperature of the target formation, obtains temperature monitoring results, and transmits the temperature monitoring results to the control system. The pressure monitoring unit 21 monitors the pressure of the target formation, obtains pressure monitoring results, and transmits the pressure monitoring results to the control system. The geophysical monitoring unit 22 monitors the target formation, obtains geophysical monitoring results, and transmits the geophysical monitoring results to the control system. Preferably, the geophysical monitoring results may include one or more of the following: resistivity tomography results, acoustic wave monitoring results, microseismic monitoring results, acoustic emission monitoring results, and distributed optical fiber monitoring results.
[0040] Specifically, the control system includes a monitoring computer 13, which is connected to a liquid injection pressurization pump 7, a flow control valve group 11, a gas pressurization pump 12, a temperature monitoring unit 20, a pressure monitoring unit 21, and a geophysical monitoring unit 22. The monitoring computer 13 is used to comprehensively judge the carbon dioxide migration, pressure front propagation, and composite cap layer development status based on the temperature monitoring results fed back by the temperature monitoring unit 20, the pressure monitoring results fed back by the pressure monitoring unit 21, and the geophysical monitoring results fed back by the geophysical monitoring unit 22. It then adjusts the parameters of the liquid injection pressurization pump 7, the flow control valve group 11, and the gas pressurization pump 12 to regulate the injection flow rate of the active extract, the injection flow rate of carbon dioxide, the injection pressure of carbon dioxide, and / or the injection mode of carbon dioxide. The carbon dioxide injection modes include continuous injection, intermittent injection, and pulse injection.
[0041] This embodiment also provides a method for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates. The method for constructing the composite caprock using the above-described system includes the following steps:
[0042] S1. Industrial solid waste is crushed and ground through a surface solid waste treatment system to obtain solid waste residue. The solid waste residue is then leached, separated into solid and liquid, and tested and conditioned through a leachate preparation and supply system to obtain active leachate and deliver it.
[0043] Specifically, industrial solid waste is crushed by a solid waste crusher 1 to obtain industrial solid waste fragments. The industrial solid waste fragments are then ground by a solid waste grinder 2 to obtain solid waste residue. The solid waste residue is leached by a stirring leaching kettle 3 using a leaching agent to obtain leaching residue and active leaching solution. The active leaching solution and leaching residue are separated by a solid-liquid separation device 4. The leaching solution detection and conditioning device 6 is used to detect one or more of the following in the active leaching solution: calcium ion concentration, magnesium ion concentration, pH value, conductivity, and alkalinity, and obtain the detection results. In addition, the leaching solution detection and conditioning device 6 also conditions the active leaching solution according to the salinity, hydrate stability boundary, and mineralization requirements of the target formation, adjusting the pH, alkalinity, salinity, and / or suspended solids content. The injection pressurization pump 7 pumps the active leaching solution into the injection well 14.
[0044] S2. The active leachate is injected into the injection layer 17 of the target formation through the injection well 14 and the liquid distribution and diffusion device 19 to form a pre-set reaction zone. In this method, the active leachate is injected into the injection layer 17 before carbon dioxide injection, and a diffusion or settling stage is set to allow the active leachate to form a pre-set reaction zone within the injection layer 17 that is spatially separated from the near-field space of the injection well 15. This reduces the risk of blockage caused by premature reaction between carbon dioxide and the active leachate in the near-field of the injection well 15. At least a portion of the injection layer 17 has in-situ temperature, pore pressure, and formation water salinity conditions located within the carbon dioxide hydrate stable zone or possessing the thermodynamic driving force for carbon dioxide hydrate formation.
[0045] S3. Carbon dioxide is injected into the gas injection layer 18 of the target formation through the gas injection well 15, forming a carbon dioxide plume 24. The carbon dioxide plume 24 migrates upward and enters the pre-set reaction zone. In the pre-set reaction zone, carbon dioxide reacts with calcium ions and / or magnesium ions in the active leaching solution to undergo carbonate mineralization reaction. Carbon dioxide hydrate is generated in the pore region that meets the stability conditions of carbon dioxide hydrate. The carbonate solid phase and carbon dioxide hydrate participate together in pore filling and seepage channel reconstruction, forming a composite plugging zone 25. The composite plugging zone 25 is the caprock, and the reservoir is below the caprock.
[0046] Specifically, an isolation layer 23 is provided between the injection layer 17 and the gas injection layer 18. The vertically staggered isolation layer 23 is determined based on the porosity, permeability, heterogeneity, carbon dioxide migration characteristics, diffusion range of active leachate, and near-wellbore blockage risk of the target formation, so that the pre-positioned reaction zone is located above the gas injection layer 18 and spatially intersects with the migration front of the carbon dioxide plume 24.
[0047] S4. Collect temperature, pressure and / or geophysical response of the target formation through monitoring well 16, and adjust the injection parameters of active leachate and / or carbon dioxide accordingly.
[0048] Specifically, monitoring well 16 determines the development level, pressure front location, or potential weak zone of the composite plugging zone 25 based on the amplitude, propagation order, and / or time difference of the temperature and pressure response at different depths within the injection layer 17, combined with geophysical monitoring results. When the monitoring results meet the preset control conditions, the carbon dioxide injection intensity is reduced or adjusted, the injection mode is changed, and / or active leaching fluid is injected. Active leaching fluid is injected and / or the carbon dioxide supply is adjusted for identified weak zones, causing the carbon dioxide entering the weak zones to induce secondary carbonate mineralization and / or carbon dioxide hydrate regeneration, thereby achieving local re-plugging. This invention does not limit the composite plugging zone 25 to a fixed mineral core-hydrate shell microstructure. In the formed composite plugging zone 25, carbonate solids and carbon dioxide hydrates are distributed on the surface of sedimentary particles, in particle contact areas, and in pore spaces through coexistence, adhesion, bridging, local coating, and / or pore throat filling, thereby reducing the scale of interconnected pore throats and the vertical migration capacity of carbon dioxide, prolonging the carbon dioxide breakthrough time, and improving the residual plugging capacity after disturbance.
[0049] Example 2 provides a field engineering application of a system and method for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates. First, injection sites 17 and 18 are selected based on the target formation's temperature, pore pressure, formation water salinity, porosity, permeability, and heterogeneity. Injection site 17 should have at least a portion of the area possessing the thermodynamic conditions for carbon dioxide hydrate formation, while 18 is located below injection site 17. The industrial solid waste is calcium carbide slag. The calcium carbide slag is crushed, ground, and then leached in an aqueous medium. Solid-liquid separation yields an active leachate containing calcium ions. The calcium ion concentration, pH, conductivity, and alkalinity of the obtained active leachate are measured. Based on the target formation's salinity, hydrate stability boundary, and mineralization requirements, the active leachate is conditioned and stored in leachate storage tank 8. If an acidic leaching medium is used, necessary neutralization or pH conditioning should be performed before injection according to the target formation requirements, rather than equating the acid leaching process with the final alkaline injected solution state.
[0050] Injection wells 14 and a liquid distribution and diffusion device 19 are arranged at injection layer 17, and gas injection wells 15 are arranged at gas injection layer 18 below injection layer 17. Monitoring wells 16 are arranged near the target reaction zone. First, active leachate is injected into injection layer 17 through injection well 14, allowing it to diffuse laterally along the bedding planes and connecting pores under the action of the liquid distribution and diffusion device 19, forming a pre-set reaction zone. A diffusion or settling stage is set if necessary. Subsequently, carbon dioxide is injected from gas injection layer 18 through gas injection well 15, causing the carbon dioxide to migrate upwards under the action of density difference and / or pressure gradient. When the carbon dioxide plume 24 enters the pre-set reaction zone, carbonate mineralization occurs under suitable hydrochemical conditions, and carbon dioxide hydrates are formed in the pore regions that meet the hydrate stability conditions. Both processes reduce pore throat connectivity.
[0051] During the injection process, the reaction zone status is acquired by temperature monitoring unit 20, pressure monitoring unit 21, and optional geophysical monitoring unit 22. Based on the amplitude, propagation sequence, and time difference of the pressure response at different depths, the degree of upward propagation of the pressure front can be determined. When enhanced pressure transmission, temperature deviation from hydrate stability conditions, or abnormal carbon dioxide migration are detected, the carbon dioxide injection intensity can be reduced, the injection mode can be changed, active leachate can be added, or local re-sealing of weak areas can be implemented. This forms the field implementation process of "pre-setting the reaction zone - lower gas injection - upward convergence - composite sealing - monitoring and control".
[0052] To verify the macroscopic effect of calcium-containing reactive phases and carbon dioxide hydrates jointly participating in caprock sealing, a reservoir-caprock coupling system was constructed using two identical 10.35 L high-pressure reactors. The lower reactor simulated a carbon dioxide hydrate-containing reservoir, and the upper reactor simulated a caprock. The porous medium in the target formation was 110-mesh quartz sand. The target porosity for the reservoir and caprock was 50% and 30%, respectively, with a water saturation of 50% for both. The pure water hydrate caprock was denoted as PW, and the CaO-modified caprock was calculated to have a theoretical calcium source of 50 mmol·L⁻¹. -1 200 mmol·L -1 and 400 mmol·L -1 The equivalent calcium ion levels are denoted as Ca50, Ca200, and Ca400, respectively. It should be noted that the equivalent calcium ion concentration is only used to characterize the initial CaO addition level and is not equivalent to the measured concentration of free calcium ions in the liquid phase; this embodiment is used to verify the technical principle of the change in the performance of the composite capping layer after the participation of the calcium-containing reactive phase, and is not used to limit the actual composition of the solid waste leachate on site.
[0053] The sample was injected with carbon dioxide at 10 °C and pressurized to approximately 4.5 MPa, then cooled to approximately 2.5 °C to form hydrates. After the formation stage, both the reservoir vessel and the caprock vessel were adjusted to approximately 2.5 MPa before connection to reduce the impact of the initial pressure difference on subsequent migration assessment. Using a 4 °C increase in reservoir temperature as a representative perturbation condition, PW and Ca400 were compared under the same boundary conditions. The results showed that the upper pressure breakthrough delay of Ca400 increased from 114 min in PW to 202 min, the cumulative carbon dioxide escape from the top decreased from 4.86 STP L to 1.94 STP L, and the mass-conserving plugging efficiency increased from 62% to 73%; the ratio characterizing vertical pressure compartmentation increased from 4.37 to 10.16. These results indicate that under these representative experimental conditions, a composite caprock with a higher calcium source level can delay upward pressure front penetration and reduce top leakage.
[0054] During the formation stage, CaO addition was observed to alter the temporal distribution of the reaction process. Compared to PW, Ca400 delayed the peak temperature by approximately 100 minutes, reduced the sudden temperature rise by 24.89%, and simultaneously increased the pressure drop and apparent carbon dioxide consumption during the formation stage by 24.65% and 27.29%, respectively. Since this experiment did not conduct a complete set of microscopic characterizations of the post-reaction samples to directly distinguish the spatial locations of specific mineral phases, the above temperature, pressure, and gas volume results are used to illustrate changes in the macroscopic reaction pathway and sealing performance after the participation of the calcium-containing reactive phase, and are not interpreted as a fixed mineral core-hydrate shell structure.
[0055] In the same dual-reactor system, the effect was verified under thermal disturbance conditions. The reservoir temperature rise was set to 2 ℃, 4 ℃, and 6 ℃, and the dynamic plugging response of PW and Ca400 was compared. When the reservoir temperature increased from 2 ℃ to 6 ℃, both types of caprocks showed earlier breakthrough and increased leakage. However, the average sensitivity of Ca400's cumulative leakage at the top to temperature rise was reduced by 54.7% compared to PW, and the temperature sensitivity of the upper / lower pressure transmission coefficient was reduced by 45.8%. Under the disturbance condition of 6 ℃, the leakage at the top of Ca400 was reduced by 56.9% compared to PW, and the plugging efficiency was improved by 14 percentage points. This result indicates that the calcium-containing reactive phase cannot eliminate the hydrate response to temperature, but it can improve the residual plugging level of the composite caprock under strong thermal drive.
[0056] Further, while raising the reservoir temperature by 4 °C, a localized thermal disturbance of 15 °C circulating water was applied to the lower part of the caprock. After the thermal disturbance, the pressure transmission coefficient of the upper / lower part of the PW increased to 5.64 times that of the baseline without additional thermal disturbance, while that of Ca400 only increased to 1.72 times; the instantaneous peak value of Ca400 at the top decreased by 77.2% compared to PW, and the comprehensive thermal damage index decreased from 1.163 of PW to 0.617, a reduction of 46.9%. These results are compatible with the mechanism of multiple hindrance provided by the hydrate plugging phase and the relatively heat-resistant calcium-containing reactive solid phase, providing technical proof for the effectiveness of the mineralization-hydrate composite caprock in improving the residual plugging capacity after thermal disturbance.
[0057] The embodiments of the present invention are given for illustrative and descriptive purposes only, and are not intended to be exhaustive or to limit the invention to the forms disclosed. Many modifications and variations will be apparent to those skilled in the art. The embodiments were chosen and described in order to better illustrate the principles and practical application of the invention, and to enable those skilled in the art to understand the invention and to design various embodiments with various modifications suitable for a particular purpose.
Claims
1. A system for synergistically constructing a composite caprock through carbon dioxide mineralization and hydrates, characterized in that, include: Surface solid waste treatment system, used to crush and grind industrial solid waste to obtain solid waste residue; The leachate preparation and supply system is connected to the surface solid waste treatment system and is used to leach the solid waste residue to obtain an active leachate and to transport the active leachate. Carbon dioxide storage system, used to store carbon dioxide; A carbon dioxide supply control system, connected to the carbon dioxide storage system, is used to transport carbon dioxide and adjust carbon dioxide transport parameters; The differentiated injection system includes a liquid injection well (14) and a gas injection well (15). The liquid injection well (14) is connected to the leaching solution preparation and supply system and is used to inject active leaching solution into the liquid injection layer (17) of the target formation. The gas injection well (15) is connected to the carbon dioxide supply and control system and is used to inject carbon dioxide into the gas injection layer (18) of the target formation. The gas injection layer (18) is located below the liquid injection layer (17), and an isolation layer (23) is provided between the gas injection layer (18) and the liquid injection layer (17). The downhole end of the liquid injection well (14) is provided with a liquid distribution and diffusion device (19). The liquid distribution and diffusion device (19) is used to make the active leaching solution diffuse laterally within the liquid injection layer (17) to form a pre-set reaction zone. A monitoring system, installed within the target formation, is used to detect the reaction data of the target formation; The control system is connected to the extract preparation and supply system, the carbon dioxide supply regulation system and the monitoring system, and is used to adjust the parameters of the extract preparation and supply system and the carbon dioxide supply regulation system according to the reaction data fed back by the monitoring system, thereby adjusting the injection parameters of the active extract and / or carbon dioxide. The surface solid waste treatment system includes a solid waste crusher (1) and a solid waste grinder (2) connected in sequence; the solid waste crusher (1) is used to crush the industrial solid waste to obtain industrial solid waste fragments; the solid waste grinder (2) is used to grind the industrial solid waste fragments to obtain solid waste residue, and the solid waste grinder (2) is connected to the leachate preparation and supply system; The leaching solution preparation and supply system includes a stirred leaching vessel (3), a solid-liquid separation device (4), a leaching residue treatment device (5), a leaching solution detection and conditioning device (6), a leaching solution storage tank (8), and a liquid injection and pressurization pump (7). The stirred leaching vessel (3) is connected to the solid waste grinding mill (2). The stirred leaching vessel (3) is used to leach the solid waste residue with a leaching agent to obtain leaching residue and the active leaching solution. The solid-liquid separation device (4) is connected to the leaching residue treatment device (5) and the leaching solution detection and conditioning device (6) respectively. The solid-liquid separation device (4) is used to separate the active leaching solution and the leaching residue. The solid phase outlet of the solid-liquid separation device (4) is connected to the leaching residue treatment device (5). The liquid phase outlet of the liquid separation device (4) is connected to the leaching solution detection and conditioning device (6); the leaching residue treatment device (5) is used to collect and dry the leaching residue; the leaching solution detection and conditioning device (6) is used to detect one or more of the calcium ion concentration, magnesium ion concentration, pH value, conductivity and alkalinity of the active leaching solution, and obtain the detection results; the leaching solution detection and conditioning device (6) is connected to the leaching solution storage tank (8), which is used to store the active leaching solution; one end of the injection pressurizing pump (7) is connected to the leaching solution storage tank (8), and the other end is connected to the injection well (14), which is used to pump the active leaching solution into the injection well (14).
2. The system for synergistic construction of a composite caprock by carbon dioxide mineralization and hydrates according to claim 1, characterized in that, The carbon dioxide storage system includes a gas storage tank (9) and a gas monitoring device (10) connected in sequence; the gas storage tank (9) is used to store carbon dioxide; the gas monitoring device (10) is connected to the carbon dioxide supply control system and is used to monitor the concentration of carbon dioxide.
3. The system for synergistic construction of a composite caprock by carbon dioxide mineralization and hydrates according to claim 2, characterized in that, The carbon dioxide supply control system includes a flow control valve group (11) and a gas pressurizing pump (12) connected in sequence. One end of the flow control valve group (11) is connected to the gas monitoring device (10), and the other end is connected to the gas pressurizing pump (12). The flow control valve group (11) is used to control the flow rate of carbon dioxide. The gas pressurizing pump (12) is connected to the gas injection well (15). The gas pressurizing pump (12) is used to adjust the delivery pressure of carbon dioxide and pump carbon dioxide into the gas injection well (15).
4. The system for synergistic construction of a composite caprock by carbon dioxide mineralization and hydrates according to claim 3, characterized in that, The monitoring system includes a monitoring well (16), and a temperature monitoring unit (20), a pressure monitoring unit (21), and a geophysical monitoring unit (22) are provided at different depths along the monitoring well (16). The temperature monitoring unit (20) is used to monitor the temperature of the target formation to obtain temperature monitoring results and transmit the temperature monitoring results to the control system. The pressure monitoring unit (21) is used to monitor the pressure of the target formation to obtain pressure monitoring results and transmit the pressure monitoring results to the control system. The geophysical monitoring unit (22) is used to monitor the target stratum to obtain geophysical monitoring results and transmit the geophysical monitoring results to the control system.
5. The system for synergistic construction of a composite caprock by carbon dioxide mineralization and hydrates according to claim 4, characterized in that, The geophysical monitoring results include one or more of the following: resistivity tomography results, acoustic wave monitoring results, microseismic monitoring results, acoustic emission monitoring results, and distributed optical fiber monitoring results.
6. The system for synergistic construction of a composite caprock by carbon dioxide mineralization and hydrates according to claim 4, characterized in that, The control system includes a monitoring computer (13), which is connected to the liquid injection pressurization pump (7), the flow control valve group (11), the gas pressurization pump (12), the temperature monitoring unit (20), the pressure monitoring unit (21), and the geophysical monitoring unit (22).
7. A method for synergistically constructing a composite caprock using carbon dioxide mineralization and hydrates, characterized in that, The construction of a composite capping layer using the system of claim 6 includes the following steps: S1. Industrial solid waste is crushed and ground through a surface solid waste treatment system to obtain solid waste residue. The solid waste residue is then leached, separated into solid and liquid and tested and conditioned through a leachate preparation and supply system to obtain an active leachate and deliver the active leachate. S2. The active leachate is injected into the injection layer (17) of the target formation through the injection well (14) and the liquid distribution and diffusion device (19) to form a pre-set reaction zone; S3. Carbon dioxide is injected into the gas injection layer (18) of the target formation through the gas injection well (15), so that the carbon dioxide plume (24) migrates upward and enters the pre-set reaction zone; S4. The temperature, pressure and / or geophysical response of the target formation are collected by monitoring well (16), and the injection parameters of the active leachate and / or carbon dioxide are adjusted accordingly.