A device for stabilizing tin bath tin liquid convection trajectories

By setting up horizontal and vertical partition components in the tin bath, combined with the counterweight design of graphite baffles and tungsten rods, the convection trajectory of the molten tin is stabilized, solving the problems of glass plate swaying and bright and dark stripes caused by the disorder of the molten tin in the tin bath, thus improving the quality of glass production.

CN123151602APending Publication Date: 2026-11-24CLFG LONGHAI ELECTRONICS GLASS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611613051.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-19
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In existing technologies, turbulent convection of molten tin in the tin bath causes glass plate swaying and bright and dark stripes on the lower surface, affecting glass quality.

Method used

The system employs horizontal and vertical partition components, combined with snap-fit ​​plates, snap-fit ​​slots, fixing components, and connecting components. Through the counterweight design of graphite baffles and tungsten rods, the convection trajectory of molten tin is stabilized, preventing the baffles from floating or shifting, thus enhancing the stability of the partition components.

Benefits of technology

It effectively stabilizes the convection trajectory of molten tin in the tin bath, reduces glass plate swaying and light and dark stripes on the lower surface, improves glass quality, and facilitates measurement operations.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123151602A_ABST
    Figure CN123151602A_ABST
Patent Text Reader

Abstract

This invention discloses a device for stabilizing the convection trajectory of molten tin in a solder bath, relating to the technical field of ultra-thin glass production line equipment. The device includes a solder bath and a snap-fit ​​assembly. The solder bath has a forming zone at its left end and a cooling zone at its right end. A transverse partition assembly and a longitudinal partition assembly are installed inside the forming zone, and a support assembly is installed in the middle of the forming zone. The snap-fit ​​assembly includes snap-fit ​​plates and snap-fit ​​grooves. Snap-fit ​​plates are placed at both ends of the forming zone. Evenly distributed snap-fit ​​grooves are formed on the upper side of each snap-fit ​​plate. A fixing assembly is installed on the side of each snap-fit ​​plate. The transverse partition assembly is installed on the upper side of the two snap-fit ​​plates. Connecting assemblies are installed on the front and rear edges of each snap-fit ​​plate, preventing the appearance of bright and dark stripes on the lower surface of the glass plate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of ultra-thin glass production line equipment technology, specifically to a device for stabilizing the convection trajectory of molten tin in a tin bath. Background Technology

[0002] The production of ultra-thin glass requires a lower drawing volume compared to conventional glass production lines. Electric heating within the tin bath is necessary to supplement the heat required for the forming process, ensuring the normal thinning of the ultra-thin glass. However, improper use of electric heating or fluctuations in heating power can easily cause turbulent convection of the molten tin within the tin bath. This can lead to glass plate swaying, making measurement difficult. Furthermore, the turbulent convection trajectory of the molten tin in the tin bath can impact the lower surface of the glass in the forming zone, causing bright and dark streaks on the lower surface of the glass plate, affecting the quality of the lower surface. Therefore, we propose a device to stabilize the convection trajectory of the molten tin in the tin bath. Summary of the Invention

[0003] The technical problem to be solved by the present invention is to overcome the existing defects and provide a device for stabilizing the convection trajectory of molten tin in a tin bath, which can avoid the appearance of bright and dark stripes on the lower surface of the glass plate and can effectively solve the problems in the background art.

[0004] To achieve the above objectives, the present invention provides the following technical solution: a device for stabilizing the convection trajectory of molten solder in a solder bath, comprising a solder bath and a snap-fit ​​assembly; Solder bath: A forming area is provided at the left end of the interior, a cooling area is provided at the right end of the interior, a horizontal partition component and a vertical partition component are installed inside the forming area of ​​the solder bath, and a support component is installed in the middle of the forming area of ​​the solder bath. The snap-fit ​​assembly includes snap-fit ​​plates and snap-fit ​​slots. Snap-fit ​​plates are placed at both ends of the solder bath forming area. The upper side of each snap-fit ​​plate has evenly distributed snap-fit ​​slots. Fixing components are installed on the sides of the snap-fit ​​plates. A transverse partitioning component is installed on the upper side of the two snap-fit ​​plates. Connecting components are installed on the front and rear edges of each snap-fit ​​plate. Through the partitioning and flow isolation by the transverse and longitudinal partitioning components within the solder bath, and the coordinated positioning of the snap-fit ​​plates, snap-fit ​​slots, fixing components, and connecting components, the convection trajectory of the molten solder in the solder bath forming area can be stabilized, reducing glass plate swaying and bright / dark stripes on the lower surface.

[0005] Furthermore, the lateral separation component includes a first graphite baffle, a support strip, a locking post, a first tungsten rod, and locking holes. The interior of the tin bath forming area is provided with uniformly distributed first graphite baffles. A support strip is fixed to the lower side of the first graphite baffle. Locking posts are fixed to both the left and right ends of the lower end of the support strip. The locking posts are locked into the interior of corresponding locking grooves. Two corresponding first tungsten rods are fixed inside the first graphite baffle. Locking holes are opened on the circumferential surface of the locking posts. Through the counterweight of the first graphite baffle and the first tungsten rod, and the locking of the support strip, locking posts, and locking grooves, lateral flow isolation can be formed and the position of the baffle can be stabilized to prevent the first graphite baffle from floating or shifting. The height of the first graphite baffle is 5-10 mm lower than the molten tin surface.

[0006] Furthermore, the support component includes a support strip and a support groove. The support strip is fixed in the middle of the solder bath forming area. The upper side of the support strip is provided with evenly distributed support grooves. The support strip is snapped into the inside of the corresponding support groove. By supporting and limiting the support strip through the support strip and the support groove, the installation stability of the transverse partition component can be enhanced, and the retaining wall can be prevented from tilting or shifting due to the flow of molten solder.

[0007] Furthermore, the fixing component includes a slide bar, locking pins, and a pull ring. The side of the locking plate is provided with a slide bar, and the side of the slide bar is fixed with evenly distributed locking pins. The side of the locking plate is provided with evenly distributed guide holes. The locking pins are engaged in the interior of the corresponding guide holes, and the locking pins corresponding to the locking holes are engaged in the interior of the locking holes. The side of the slide bar is fixed with a pull ring. By driving the locking pins into the locking holes through the slide bar, and by operating the pull ring, the locking pins can be locked in the locking groove to prevent the lateral separating component from coming out or moving up and down.

[0008] Furthermore, the connecting assembly includes a sliding column and a spring. The front and rear sides of the snap-fit ​​plate are provided with mounting holes. A sliding column is slidably connected inside the mounting hole. A spring is fixed on the end face of the sliding column. The spring is fixed inside the mounting hole. The two sliding columns are fixed on the sides of the corresponding slide bars. By applying an elastic restoring force to the slide bars through the sliding columns and springs, the snap-fit ​​column can be automatically kept in a snap-fit ​​state, improving the anti-loosening reliability of the fixing assembly.

[0009] Furthermore, the longitudinal separation component includes a second graphite baffle and a second tungsten rod. A second graphite baffle is provided between each pair of first graphite baffles. Two corresponding second tungsten rods are fixed inside the second graphite baffle. All the front and rear second graphite baffles are respectively attached to the front and rear sides inside the tin bath. The second graphite baffles and the second tungsten rods form a longitudinal flow barrier between adjacent first graphite baffles, which can further divide and solidify the molten tin in the forming area, reducing mutual interference between the front and rear areas.

[0010] Furthermore, the interior of the solder bath forming area is provided with evenly distributed sealing posts. The sealing posts are snapped into the interior of the corresponding snap-fit ​​grooves. The upper end of the sealing post is hinged with a connecting ring. The unused snap-fit ​​grooves are blocked by the sealing posts, and the connecting rings facilitate the removal and placement of the components. This can prevent molten solder from entering the snap-fit ​​grooves and causing deposition or jamming, thus ensuring the long-term reliability of the snap-fit ​​assembly.

[0011] Furthermore, the tin bath forming area is provided with two corresponding limiting strips. The limiting strips have a strip-shaped opening in the middle. All the second graphite baffles are located inside the two strip-shaped openings. The second graphite baffles are limited by the strip-shaped openings of the limiting strips, which can prevent the longitudinal separation components from tilting forward or backward or shifting horizontally, thereby improving the longitudinal flow isolation stability. The height of the second graphite baffles is 5-10 mm lower than the tin liquid surface.

[0012] Furthermore, two corresponding fixing holes are provided on the front side of the limiting strip, and a counterweight is fixed inside the fixing hole. The counterweight increases the weight and stability of the limiting strip, which can keep the limiting strip in a fixed position in the molten solder and prevent it from drifting due to the convection impact of the molten solder.

[0013] Furthermore, the support bar has connecting grooves on both the left and right sides, and a third tungsten rod is fixed inside the connecting groove. The third tungsten rod acts as a counterweight for the support bar, which can lower the center of gravity of the support component and improve its stability at the bottom, preventing the support bar from floating or shifting in the molten solder.

[0014] Compared with the prior art, the beneficial effects of the present invention are as follows: This device for stabilizing the convection trajectory of molten solder in a solder bath has the following advantages: 1. By dividing the molten solder in the solder bath forming area into convection zones using horizontal and vertical partition components, the flow trajectory of the molten solder can be stabilized, the glass plate can be reduced to oscillate, and the measurement operation can be facilitated.

[0015] 2. By combining the first graphite retainer, the second graphite retainer, and the first tungsten rod and the second tungsten rod with counterweights, the retainer can be stably submerged in the molten tin, preventing it from floating and shifting. At the same time, the top of the retainer is 5-10mm below the molten tin surface and will not come into contact with the glass strip.

[0016] 3. Through the cooperation of snap-fit ​​plates, snap-fit ​​slots, fixing components and connecting components, the retaining wall can be quickly installed, reliably locked and easily disassembled, adapting to different production needs.

[0017] 4. The stability of each partition component can be enhanced by the support components, limit bars, counterweight bars and third tungsten rod, preventing tilting, drifting and horizontal displacement.

[0018] 5. By sealing unused slots with sealing posts, molten solder can be prevented from entering the slots and causing deposits or jamming, ensuring long-term reliable operation. Attached Figure Description

[0019] Figure 1 This is a schematic diagram of the front structure of the present invention; Figure 2 This is a schematic diagram of the snap-fit ​​assembly structure of the present invention; Figure 3 For the present invention Figure 2 Enlarged view of point A in the middle; Figure 4 This is a front sectional view of the present invention; Figure 5 For the present invention Figure 5 Enlarged view of section B in the middle; Figure 6 This is a schematic diagram of the supporting component structure of the present invention; Figure 7 This is a schematic diagram of the fixed component structure of the present invention; Figure 8 This is a schematic diagram of the sealing column structure of the present invention.

[0020] In the diagram: 1. Tin bath, 2. Snap-fit ​​assembly, 21. Snap-fit ​​plate, 22. Snap-fit ​​groove, 3. Horizontal partition assembly, 31. First graphite retaining wall, 32. Support bar, 33. Snap-fit ​​post, 34. First tungsten rod, 35. Snap-fit ​​hole, 4. Support assembly, 41. Support bar, 42. Support groove, 5. Fixing assembly, 51. Sliding bar, 52. Snap-fit ​​post, 53. Pull ring, 6. Connecting assembly, 61. Sliding post, 62. Spring, 7. Sealing post, 8. Connecting ring, 9. Longitudinal partition assembly, 91. Second graphite retaining wall, 92. Second tungsten rod, 10. Limiting bar, 11. Counterweight bar, 12. Third tungsten rod. Detailed Implementation

[0021] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0022] Please see Figure 1-8 This embodiment provides a technical solution: a device for stabilizing the convection trajectory of molten solder in a solder bath, comprising a solder bath 1 and a snap-fit ​​assembly 2; Solder bath 1: A forming area is provided at the left end of the interior, a cooling area is provided at the right end of the interior, a horizontal partition component 3 and a vertical partition component 9 are installed inside the forming area of ​​the solder bath 1, and a support component 4 is installed in the middle of the forming area of ​​the solder bath 1. Snap-fit ​​assembly 2: includes snap-fit ​​plate 21 and snap-fit ​​groove 22. Snap-fit ​​plate 21 is placed at both ends of the molding area inside the solder bath 1. Snap-fit ​​groove 22 is evenly distributed on the upper side of snap-fit ​​plate 21. Fixing assembly 5 is installed on the side of snap-fit ​​plate 21. Horizontal partition assembly 3 is installed on the upper side of the two snap-fit ​​plates 21. Connecting assembly 6 is installed on the front and rear edges of snap-fit ​​plate 21. Through the partitioning and flow isolation of horizontal partition assembly 3 and vertical partition assembly 9 in the solder bath 1, and the cooperative positioning of snap-fit ​​plate 21, snap-fit ​​groove 22, fixing assembly 5 and connecting assembly 6, the convection trajectory of molten solder in the molding area of ​​the solder bath 1 can be stabilized, reducing glass plate swaying and bright and dark stripes on the lower surface. The transverse separation component 3 includes a first graphite baffle 31, a support bar 32, a locking post 33, a first tungsten rod 34, and a locking hole 35. The interior of the molding area of ​​the tin bath 1 is provided with uniformly distributed first graphite baffles 31. The lower side of the first graphite baffle 31 is fixed with a support bar 32. The left and right ends of the lower end of the support bar 32 are fixed with locking posts 33. The locking posts 33 are locked in the interior of the corresponding locking groove 22. The interior of the first graphite baffle 31 is fixed with two corresponding first tungsten rods 34. The circumferential surface of the locking post 33 is provided with a locking hole 35. Through the counterweight of the first graphite baffle 31 and the first tungsten rod 34, and the locking of the support bar 32, the locking post 33 and the locking groove 22, a transverse flow barrier can be formed and the position of the baffle can be stabilized to prevent the first graphite baffle 31 from floating or shifting. The support component 4 includes a support bar 41 and a support groove 42. The support bar 41 is fixed in the middle of the molding area of ​​the solder bath 1. The support bar 41 has evenly distributed support grooves 42 on its upper side. The support bar 32 is snapped into the inside of the corresponding support groove 42. By supporting and limiting the support bar 32 through the support bar 41 and the support groove 42, the installation stability of the transverse partition component 3 can be enhanced, and the retaining wall can be prevented from tilting or shifting due to the flow of molten solder. The fixing component 5 includes a slide bar 51, a locking post 52, and a pull ring 53. The side of the locking plate 21 is provided with a slide bar 51, and the side of the slide bar 51 is fixed with evenly distributed locking posts 52. The side of the locking plate 21 is provided with evenly distributed guide holes, and the locking posts 52 are locked into the corresponding guide holes. The locking posts 52 corresponding to the locking holes 35 are locked into the locking holes 35. The side of the slide bar 51 is fixed with a pull ring 53. The slide bar 51 drives the locking posts 52 to be inserted into the locking holes 35, and the pull ring 53 can be used to lock the locking posts 33 in the locking groove 22 to prevent the transverse separating component 3 from coming out or moving up and down. The connecting component 6 includes a sliding post 61 and a spring 62. The front and rear sides of the snap-fit ​​plate 21 are provided with mounting holes. The sliding post 61 is slidably connected inside the mounting hole. The spring 62 is fixed on the end face of the sliding post 61 and is fixed inside the mounting hole. The two sliding posts 61 are fixed on the side of the corresponding slide bar 51. By applying an elastic restoring force to the slide bar 51 through the sliding post 61 and the spring 62, the snap-fit ​​post 52 can be automatically kept in a snap-fit ​​state, improving the anti-loosening reliability of the fixing component 5. The longitudinal separation component 9 includes a second graphite baffle 91 and a second tungsten rod 92. A second graphite baffle 91 is provided between each pair of first graphite baffles 31. Two corresponding second tungsten rods 92 are fixed inside the second graphite baffle 91. All the front and rear second graphite baffles 91 are respectively attached to the front and rear sides inside the tin bath 1. The second graphite baffles 91 and the second tungsten rods 92 form a longitudinal flow barrier between adjacent first graphite baffles 31, which can further divide and solidify the molten tin in the forming area and reduce mutual interference between the front and rear areas.

[0023] The tin bath 1 has uniformly distributed sealing pillars 7 inside the forming area. The sealing pillars 7 are snapped into the corresponding snap-fit ​​grooves 22. The upper end of the sealing pillar 7 is hinged with a connecting ring 8. The unused snap-fit ​​grooves 22 are blocked by the sealing pillars 7, and the connecting ring 8 facilitates the removal and placement. This can prevent molten tin from entering the snap-fit ​​grooves 22 and causing deposition or jamming, thus ensuring the long-term reliability of the snap-fit ​​assembly 2.

[0024] Among them, the tin bath 1 forming area is provided with two corresponding limiting strips 10. The limiting strips 10 have a strip-shaped opening in the middle. All the second graphite baffles 91 are located inside the two strip-shaped openings. The second graphite baffles 91 are limited by the strip-shaped openings of the limiting strips 10, which can prevent the longitudinal separation component 9 from tilting forward or backward or shifting horizontally, and improve the longitudinal flow isolation stability.

[0025] Specifically, the front side of the limiting strip 10 has two corresponding fixing holes, and a counterweight strip 11 is fixed inside the fixing holes. The counterweight strip 11 increases the weight and stability of the limiting strip 10, which enables the limiting strip 10 to maintain a fixed position in the molten solder and avoids drifting due to the convection impact of the molten solder.

[0026] The support bar 41 has connecting grooves on both the left and right sides. A third tungsten rod 12 is fixed inside the connecting groove. The third tungsten rod 12 serves as a counterweight for the support bar 41, which can lower the center of gravity of the support assembly 4 and improve its bottom stability, preventing the support bar 41 from floating or shifting in the molten solder.

[0027] The working principle of the device for stabilizing the convection trajectory of molten tin in a solder bath provided by this invention is as follows: In the forming area of ​​the solder bath 1, snap-fit ​​plates 21 are first placed at the left and right ends of the forming area. Snap-fit ​​grooves 22 are evenly distributed on the upper side of the snap-fit ​​plates 21. The snap-fit ​​posts 33 at both ends of the support strip 32 below the first graphite baffle 31 of the transverse separating component 3 are inserted into the corresponding snap-fit ​​grooves 22. Two first tungsten rods 34 are fixed inside the first graphite baffle 31. The high density of tungsten serves as a counterweight for the graphite baffle, enabling it to sink stably into the molten tin. The top of the first graphite baffle 31 is 5-10 mm below the molten tin surface, preventing contact with the floating glass strip above. The support strip 41 of the supporting component 4 is fixed in the middle of the forming area, and its upper support groove 42 supports the support strip 32, further enhancing the stability of the transverse separating component 3.

[0028] Then, the locking pin 33 is locked in place by the fixing component 5. Operating the pull ring 53 moves the slide bar 51, causing the locking pin 52 on the slide bar 51 to pass through the guide hole on the side of the locking plate 21 and insert into the locking hole 35 on the circumferential surface of the locking pin 33, thereby fixing the locking pin 33 within the locking groove 22 and preventing the lateral separating component 3 from coming out or moving up and down. The slide pin 61 and spring 62 in the connecting component 6 apply an elastic restoring force to the slide bar 51, automatically keeping the locking pin 52 in a locked state and improving the reliability of the anti-loosening mechanism.

[0029] A second graphite baffle 91 is installed between adjacent first graphite baffles 31. Two second tungsten rods 92 are fixed inside the second graphite baffle 91. All the second graphite baffles 91 are fitted to the front and rear sides of the tin bath 1, forming a longitudinal flow barrier. The strip-shaped opening in the middle of the limiting strip 10 limits the second graphite baffles 91, preventing them from tilting forward or backward or shifting horizontally. A counterweight strip 11 is fixed in the fixing hole on the front side of the limiting strip 10 to increase its weight and stability. Third tungsten rods 12 are fixed in the connecting grooves on the left and right sides of the support strip 41 to counterweight the support assembly 4, lower the center of gravity, and prevent floating or displacement.

[0030] For unused snap-fit ​​slots 22, use sealing posts 7 to snap-fit ​​and seal them. The upper end of the sealing post 7 is hinged with a connecting ring 8 for easy removal and placement, and to prevent molten solder from entering the snap-fit ​​slots 22 and causing deposition or jamming.

[0031] Through the aforementioned horizontal and vertical separation, the convection of molten solder within the forming zone of solder bath 1 is confined to multiple small areas. The convection trajectory within each area is relatively fixed, making them less prone to mutual interference. When the electric heating power fluctuates, the turbulence is less likely to spread throughout the entire solder bath, thereby stabilizing the flow trajectory of the molten solder, reducing glass plate swaying, facilitating measurement, and reducing bright and dark streaks on the lower surface of the glass plate, thus improving the quality of the lower surface of the glass. All retaining walls and counterweights are made of high-temperature resistant graphite and tungsten materials that do not contaminate the molten solder, making them suitable for long-term use in the high-temperature environment of the solder bath.

[0032] The above description is merely an embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural or procedural transformations made based on the content of the present invention specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of the present invention.

Claims

1. A device for stabilizing the convection trajectory of molten solder in a solder bath, characterized in that: Includes a solder bath (1) and a snap-fit ​​assembly (2); Solder bath (1): A forming area is provided at the left end of the interior, a cooling area is provided at the right end of the interior of the solder bath (1), a horizontal partition component (3) and a vertical partition component (9) are installed inside the forming area of ​​the solder bath (1), and a support component (4) is installed in the middle of the forming area of ​​the solder bath (1). The snap-fit ​​assembly (2) includes a snap-fit ​​plate (21) and a snap-fit ​​groove (22). The snap-fit ​​plate (21) is placed at both ends of the molding area of ​​the solder bath (1). The snap-fit ​​plate (21) has a snap-fit ​​groove (22) evenly distributed on its upper side. The snap-fit ​​plate (21) is equipped with a fixing component (5) on its side. The transverse separation component (3) is installed on the upper side of the two snap-fit ​​plates (21). The snap-fit ​​plate (21) is equipped with a connecting component (6) on its front and rear sides.

2. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 1, characterized in that: The transverse partition component (3) includes a first graphite sill (31), a support strip (32), a locking post (33), a first tungsten rod (34), and a locking hole (35). The tin bath (1) forming area is provided with a uniformly distributed first graphite sill (31). The lower side of the first graphite sill (31) is fixed with a support strip (32). The left and right ends of the lower end of the support strip (32) are fixed with locking posts (33). The locking posts (33) are locked in the interior of the corresponding locking groove (22). The interior of the first graphite sill (31) is fixed with two corresponding first tungsten rods (34). The circumferential surface of the locking post (33) is provided with a locking hole (35).

3. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 2, characterized in that: The support component (4) includes a support strip (41) and a support groove (42). The support strip (41) is fixed in the middle of the molding area of ​​the tin bath (1). The upper side of the support strip (41) is provided with evenly distributed support grooves (42). The support strip (32) is snapped into the interior of the corresponding support groove (42).

4. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 2, characterized in that: The fixing component (5) includes a slide bar (51), a locking post (52) and a pull ring (53). The side of the locking plate (21) is provided with a slide bar (51). The side of the slide bar (51) is fixed with evenly distributed locking posts (52). The side of the locking plate (21) is provided with evenly distributed guide holes. The locking posts (52) are locked inside the corresponding guide holes. The locking posts (52) corresponding to the locking holes (35) are locked inside the locking holes (35). The side of the slide bar (51) is fixed with a pull ring (53).

5. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 4, characterized in that: The connecting assembly (6) includes a sliding column (61) and a spring (62). The front and rear sides of the snap-fit ​​plate (21) are provided with mounting holes. The sliding column (61) is slidably connected inside the mounting hole. The spring (62) is fixed on the end face of the sliding column (61). The spring (62) is fixed inside the mounting hole. The two sliding columns (61) are fixed on the side of the corresponding slide bar (51).

6. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 2, characterized in that: The longitudinal partition component (9) includes a second graphite sill (91) and a second tungsten rod (92). All the first graphite sills (31) are provided with a second graphite sill (91) between each other. The second graphite sill (91) has two corresponding second tungsten rods (92) fixed inside. All the front and rear second graphite sills (91) are respectively attached to the front and rear sides inside the tin bath (1).

7. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 1, characterized in that: The tin bath (1) has uniformly distributed sealing posts (7) inside the forming area. The sealing posts (7) are snapped into the corresponding snap-fit ​​grooves (22). The upper end of the sealing posts (7) is hinged with a connecting ring (8).

8. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 6, characterized in that: The tin bath (1) forming area is provided with two corresponding limiting strips (10), and the limiting strips (10) have a strip-shaped opening in the middle. All the second graphite baffles (91) are located inside the two strip-shaped openings respectively.

9. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 8, characterized in that: Two corresponding fixing holes are provided on the front side of the limiting strip (10), and a counterweight strip (11) is fixed inside the fixing hole.

10. The device for stabilizing the convection trajectory of molten solder in a solder bath according to claim 1, characterized in that: The support bar (41) has connecting grooves on both the left and right sides, and a third tungsten rod (12) is fixed inside the connecting groove.