Pre-coated film for leather release and method for preparing the same
By using a biaxially oriented polyester base film on the leather release film and forming a pre-coating on its surface, the anti-scratch and anti-static functions are integrated, solving the problems of insufficient stiffness, poor wear resistance and static electricity of the leather release film. This achieves high stiffness, wear resistance and anti-static effect, simplifies the production process and reduces costs.
Patent Information
- Application Number
- CN202611576991.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-13
- Publication Date
- 2026-11-24
AI Technical Summary
Existing leather release films suffer from insufficient stiffness, poor abrasion resistance, prominent static electricity issues, and separation of functional layers, resulting in poor surface smoothness and texture accuracy of the leather, static electricity adsorption of impurities, and complex and costly production processes.
The biaxially oriented polyester base film is used and a pre-coating is formed on its surface. The pre-coating contains anti-scratch particles and antistatic agents. Through optimized processes, a pre-coated film with high light transmittance, high stiffness, wear resistance and antistatic properties is formed, integrating multiple functions into one layer.
It improves the stiffness and abrasion resistance of leather release film, reduces electrostatic adsorption, ensures the smoothness and texture accuracy of leather surface, reduces production costs and improves product reliability.
Smart Images

Figure CN123152152A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of polymer film materials technology, specifically to a pre-coated film for leather release and its preparation method. Background Technology
[0002] Leather release film is a key auxiliary material in the production process of synthetic leather and artificial leather. Its function is to serve as a carrier substrate during the leather coating process. After the polyurethane (PU) or polyvinyl chloride (PVC) coating dries and forms a film, the release film is peeled off, thereby forming the desired pattern and gloss effect on the leather surface.
[0003] Currently, leather release films mainly face the following technical problems: (1) Insufficient stiffness: Existing PET release films are prone to curling and deformation during high-temperature coating and winding, affecting the smoothness and texture accuracy of the leather surface. Although there are reports of high-stiffness polyester films in the existing technology, research on combining them with release function is still insufficient; (2) Poor abrasion resistance: During repeated use, the surface of the release film is easily scratched and worn, resulting in a decrease in release effect and a shortened service life. Although there are existing technologies that use a wear-resistant hardened layer as an independent functional layer, this increases the complexity and cost of the process; (3) Static electricity problem is prominent: Release film is prone to static electricity during winding and unwinding, which leads to the adsorption of dust and other impurities, affecting the surface quality of leather, and in severe cases, even causing safety accidents such as fire and explosion. Existing antistatic release films mostly use independent antistatic coatings, which have problems such as poor interlayer bonding and short-lasting antistatic effect; (4) Functional layer separation: Existing technologies often achieve functions such as antistatic, wear resistance, and release through multiple independent coatings, which have defects such as complex processes, insufficient interlayer adhesion, and high cost.
[0004] Therefore, developing an integrated pre-coated film for leather release that combines high stiffness, high abrasion resistance, and durable antistatic properties has significant industrial application value. Summary of the Invention
[0005] The purpose of this invention is to address the shortcomings of existing technologies by providing a pre-coated film for leather release and its preparation method.
[0006] The technical solution is as follows: a pre-coated film for leather release, comprising a polyester base film and a pre-coating layer disposed on at least one surface thereon, wherein the outermost surface of the pre-coating layer is provided with a release surface; the light transmittance of the polyester base film is ≥90%, and the bending stiffness is >120mN; the pre-coating layer contains anti-scratch particles and an antistatic agent, and the pencil hardness of the pre-coating layer is ≥4H.
[0007] Preferably, the polyester-based film is a biaxially oriented polyethylene terephthalate film.
[0008] Preferably, the thickness of the polyester base film is 50-250 μm.
[0009] Preferably, the thickness of the pre-coating layer is 0.5-10 μm.
[0010] Preferably, the scratch-resistant particles are selected from at least one of nano-SiO2, nano-Al2O3, and diamond powder, with a particle size of 10-500 nm.
[0011] Preferably, the antistatic agent is selected from at least one of conductive polymers, metal oxide nanoparticles, and ionic liquid antistatic agents.
[0012] Preferably, the pre-coating layer is formed by coating and curing a coating liquid of water-based polyurethane resin, water-based acrylic resin, or UV-curable resin.
[0013] A method for preparing a pre-coated film for leather release includes the following steps: (1) Polyester chips are melt-extruded, cast, biaxially stretched and heat-set to obtain a polyester base film with light transmittance ≥90% and bending stiffness >120mN; (2) Mix and disperse the resin matrix, anti-scratch particles, antistatic agent, additives and solvent in proportion to obtain a uniform coating liquid; (3) Apply the coating liquid obtained in step (2) to at least one surface of the polyester base film obtained in step (1); (4) Dry and cure the coated film to form a pre-coating layer.
[0014] Further, the coating liquid is prepared in the following parts by weight: Waterborne polyurethane resin: 100-130 parts, nano SiO2 (particle size 50nm): 10-15 parts, conductive polymer antistatic agent: 5-10 parts, crosslinking agent: 3-7 parts, wetting agent: 0.5-1 parts, deionized water: 5-10 parts.
[0015] Compared with the prior art, the present invention has the following beneficial effects: (1) High stiffness: By optimizing the biaxial stretching process and heat setting conditions, the bending stiffness of the polyester base film is >120mN, which effectively solves the problem of curling deformation of the release film during high-temperature coating and winding, and ensures the flatness and texture accuracy of the leather surface. (2) High abrasion resistance: The uniformly dispersed anti-scratch particles in the pre-coating give the coating excellent anti-scratch performance. The pencil hardness is ≥4H, which meets the requirements of repeated scratching during the use of leather release film and significantly extends the service life of release film. (3) Durable antistatic: The antistatic agent in the pre-coating gives the film good antistatic function, which can effectively reduce the adsorption of dust and other impurities by the release film during operation and improve the surface quality of leather. (4) Integrated functional design: This invention integrates multiple functions such as antistatic, wear resistance, and release into the same pre-coating layer, avoiding problems such as poor interlayer adhesion and complex process in traditional multi-layer coating process, reducing production costs and improving product reliability; (5) High light transmittance optical performance: The light transmittance of the polyester base film is ≥90%, which ensures the optical transparency of the release film and is beneficial to online quality inspection in the leather production process. Detailed Implementation
[0016] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention. Attached Figure Description
[0017] Figure 1 Schematic diagram of the pre-coated film structure for leather release Example 1
[0018] 1. Base film preparation: Polyethylene terephthalate (PET) chips were dried and then melt-extruded at 280-300℃ to obtain a thick sheet through casting. The thick sheet was then longitudinally stretched at 90-120℃ (stretch ratio 3.0 times), followed by transverse stretching at 100-130℃ (stretch ratio 3.5 times). Heat setting was then performed at 220℃ to obtain a polyester base film with a thickness of 125 μm. Testing showed that the light transmittance of this base film was 92%, and its bending stiffness was 135 mN. 2. Coating solution preparation: Prepare the coating solution according to the following weight parts: waterborne polyurethane resin: 100 parts, nano SiO2 (particle size 50nm): 15 parts, conductive polymer antistatic agent: 5 parts, crosslinking agent: 3 parts, wetting agent: 0.5 parts, deionized water: 5 parts. After mixing the above components, the mixture is dispersed at high speed and milled to obtain a uniform and stable coating solution. 3. Coating and curing: The above coating liquid is applied to one surface of the polyester base film using a gravure coating method, with a coating amount of 2-5 g / m²; it is then dried and cured at 100-150℃ for 2-5 minutes to obtain a pre-coated film with a pre-coating thickness of 2 μm. 4. Performance Testing: The pre-coated film prepared in this embodiment was subjected to the following performance tests: light transmittance: 92.5% (tested according to GB / T2410), bending stiffness: 135mN (tested according to GB / T 22364), pencil hardness: 4H (tested according to GB / T 6739), surface resistivity: 10 8 -10 10 Ω (tested according to GB / T 1410), release force: < 0.5N / 25mm. Example 2
[0019] 1. Base film preparation: Polyethylene terephthalate (PET) chips were dried and then melt-extruded at 280-300℃ to obtain a thick sheet through casting. The thick sheet was then longitudinally stretched at 90-120℃ (stretch ratio 3.0 times), followed by transverse stretching at 100-130℃ (stretch ratio 3.5 times). Heat setting was then performed at 230℃ to obtain a polyester base film with a thickness of 125 μm. Testing showed that the base film had a light transmittance of 92.5% and a bending stiffness of 138 mN. 2. Preparation of coating solution: The coating solution is prepared according to the following weight parts: waterborne polyurethane resin: 120 parts, nano Al2O3 (particle size 50nm): 15 parts, conductive polymer antistatic agent: 6 parts, crosslinking agent: 3.5 parts, wetting agent: 0.6 parts, deionized water: 8 parts. After mixing the above components, the solution is dispersed at high speed and milled to obtain a uniform and stable coating solution. 3. Coating and curing: The above coating liquid is applied to one surface of the polyester base film using a gravure coating method, with a coating amount of 2-5 g / m²; it is then dried and cured at 100-150℃ for 2-5 minutes to obtain a pre-coated film with a pre-coating thickness of 2.5 μm. 4. Performance Testing: The pre-coated film prepared in this embodiment was subjected to the following performance tests: light transmittance: 92.8% (tested according to GB / T2410), bending stiffness: 138mN (tested according to GB / T 22364), pencil hardness: 5H (tested according to GB / T 6739), surface resistivity: 10 7 -10 9 Ω (tested according to GB / T 1410), release force: < 0.5N / 25mm.
[0020] The present invention manufactures a pre-coated film for leather release, which optimizes the biaxial stretching process and heat setting conditions to achieve a bending stiffness of >120mN for the polyester base film. This effectively solves the problem of curling and deformation of the release film during high-temperature coating and winding, and ensures the smoothness and texture accuracy of the leather surface. The uniformly dispersed anti-scratch particles in the pre-coating give the coating excellent anti-scratch properties, with a pencil hardness of ≥4H, which meets the requirements of repeated scratching during the use of leather release film and significantly extends the service life of release film. The antistatic agent incorporated in the pre-coating gives the film excellent antistatic properties, which can effectively reduce the adsorption of dust and other impurities by the release film during operation and improve the surface quality of the leather. This invention integrates multiple functions such as antistatic, wear resistance, and release properties into the same pre-coating layer, avoiding problems such as poor interlayer adhesion and complex processes in traditional multi-layer coating processes, reducing production costs and improving product reliability. The polyester-based film has a light transmittance of ≥90%, which ensures the optical transparency of the release film and is beneficial for online quality inspection during the leather production process.
[0021] The above embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit it. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A precoat film for leather release, comprising a polyester-based film and a precoat layer provided on at least one surface thereof, characterized in that: The outermost surface of the pre-coating has a release surface; the light transmittance of the polyester base film is ≥90%, and the bending stiffness is >120mN; the pre-coating contains anti-scratch particles and antistatic agents, and the pencil hardness of the pre-coating is ≥4H.
2. The pre-coat film for leather release according to claim 1, characterized by: The polyester-based film is a biaxially oriented polyethylene terephthalate film.
3. The pre-coat film for leather release according to claim 1, characterized by: The thickness of the polyester base film is 50-250 μm.
4. The pre-coat film for leather release according to claim 1, characterized by: The thickness of the pre-coating is 0.5-10 μm.
5. The pre-coat film for leather release according to claim 1, characterized by: The scratch-resistant particles are selected from at least one of nano-SiO2, nano-Al2O3, and diamond powder, with a particle size of 10-500nm.
6. The pre-coat film for leather release according to claim 1, characterized by: The antistatic agent is selected from at least one of conductive polymers, metal oxide nanoparticles, and ionic liquid antistatic agents.
7. The pre-coat film for leather release according to claim 1, characterized by: The pre-coating layer is formed by coating and curing an aqueous polyurethane resin, aqueous acrylic resin, or UV-curable resin coating solution.
8. The method of claim 1-8, wherein the method is characterized by: Includes the following steps: (1) Polyester chips are melt-extruded, cast, biaxially stretched and heat-set to obtain a polyester base film with light transmittance ≥90% and bending stiffness >120mN; (2) Mix and disperse the resin matrix, anti-scratch particles, antistatic agent, additives and solvent in proportion to obtain a uniform coating liquid; (3) Apply the coating liquid obtained in step (2) to at least one surface of the polyester base film obtained in step (1); (4) Dry and cure the coated film to form a pre-coating layer.
9. The method of claim 8, wherein the method is characterized by: The coating liquid is prepared in the following parts by weight: waterborne polyurethane resin: 100-130 parts, nano SiO2 (particle size 50nm): 10-15 parts, conductive polymer antistatic agent: 5-10 parts, crosslinking agent: 3-7 parts, wetting agent: 0.5-1 parts, deionized water: 5-10 parts.