Low cost natural rubber composite for seismic isolation bearings and method of manufacture

By using a low-cost natural rubber raw material and additive mixing process, seismic isolation bearing materials were prepared, solving the high cost problem and realizing high-performance and low-cost natural rubber composite materials, thereby improving the quality and market competitiveness of seismic isolation bearings.

CN123152183APending Publication Date: 2026-11-24XISHUANGBANNA HUAREYA RUBBER CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611293074.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-25
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

The production of existing seismic isolation rubber bearings for buildings suffers from high costs, making it difficult to meet the market demand for low-cost, high-performance, customized natural rubber, thus affecting their market competitiveness and service life.

Method used

Using low-cost natural rubber raw rubber as the matrix, and combining it with additives such as zinc oxide, stearic acid, antioxidants, silane coupling agents, reinforcing agents, and aromatic oils, a low-cost natural rubber composite material is prepared through a mixing process. This composite material is then applied to seismic isolation bearings to improve performance and reduce production costs.

Benefits of technology

This has enabled the preparation of low-cost, high-performance natural rubber composite materials, improving the quality and performance of seismic isolation bearings, meeting diverse market demands, reducing production costs, and increasing production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

This invention relates to a graphene-natural rubber composite material for conveyor belt cover rubber and its preparation method. The graphene-natural rubber composite material for conveyor belt cover rubber is prepared using graphene, layered silicates, silica, and natural rubber latex as raw materials through a wet mixing process. The graphene-natural rubber composite material is then plasticized, and zinc oxide, stearic acid, antioxidant, silane coupling agent, reinforcing agent, and aromatic oil are added sequentially for a first mixing. Sulfur and an accelerator are then added for a second mixing to obtain the product. This invention uses a graphene-natural rubber composite material as a conveyor belt cover rubber, improving the mechanical properties and wear resistance of the rubber compound, thereby extending the service life of the conveyor belt. Furthermore, the application of the graphene-natural rubber composite material also reduces environmental pollution and saves energy.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a method for preparing a natural rubber composite material, and more particularly to a low-cost natural rubber composite material for seismic isolation bearings and its preparation method. Background Technology

[0002] Building seismic isolation rubber bearings mainly consist of an upper connecting plate, a lower connecting plate, multiple layers of rubber, and a sandwich steel plate. The upper connecting plate connects the seismic isolation device to the building's superstructure, while the lower connecting plate connects the seismic isolation device to the building's foundation to transfer horizontal shear force. The sandwich steel plate is tightly bonded to the rubber, which not only improves the bearing's vertical bearing capacity but also endows it with greater horizontal deformation capacity and resistance to repeated load fatigue. Natural rubber seismic isolation bearings (LNRs) are made primarily of natural rubber, possessing moderate flexibility and good elastic recovery function. They are an important seismic isolation component for buildings, widely used in buildings, steel structures, bridges, industrial equipment, and other fields. They are composed of multiple layers of rubber and multiple layers of steel plates or other materials stacked alternately. Through unique structural design and material properties, they can play a crucial seismic isolation role during earthquakes, effectively protecting the building, its internal facilities, and the safety of personnel.

[0003] Performance characteristics of natural rubber bearings: (1) Vertical bearing capacity: It has sufficient vertical stiffness and bearing capacity to stably support the building. (2) Extended period: It has sufficient horizontal stiffness to ensure that the basic period of the building is extended by about 1.5-3.0 seconds, reducing the impact of earthquakes on the building. (3) Deformation capacity: It has a large enough reserve of horizontal deformation capacity to ensure that there will be no instability under strong earthquakes. In the production of seismic isolation rubber bearings for buildings, there is a strong demand for low-cost, high-performance customized natural rubber. On the one hand, reducing costs can improve the market competitiveness of products, enabling more building projects to adopt seismic isolation technology; on the other hand, high-performance natural rubber can further improve the seismic isolation effect and service life of the bearings, meeting the needs of different building projects. Summary of the Invention

[0004] The purpose of this invention is to provide a low-cost natural rubber composite material for seismic isolation bearings and its preparation method. It includes a rubber matrix and corresponding additives. Using cost-effective and inexpensive natural raw rubber as raw material, vulcanizing agents, antioxidants, fillers, etc., are added in an open mill or internal mixer to prepare a low-cost natural rubber composite material, which exhibits excellent performance when applied to rubber seismic isolation bearings.

[0005] The technical solution adopted in this invention: A low-cost natural rubber composite material for seismic isolation bearings is prepared by using 100 parts of low-cost natural rubber raw rubber as the matrix, and then adding 3-10 parts of zinc oxide, 1-5 parts of stearic acid, 2-6 parts of antioxidant, 2-7 parts of silane coupling agent, 0-30 parts of reinforcing agent, and 6-10 parts of aromatic oil to obtain a first-stage compound. Then, 1.5-2.5 parts of sulfur and 1-2 parts of accelerator are added to obtain a second-stage compound, which yields the product.

[0006] A method for preparing a low-cost natural rubber composite material for seismic isolation bearings, comprising the following steps: (1) Preparation of low-cost natural rubber raw rubber: Add various raw rubbers to a mixer, wash and dry them, and then mix them at high speed to prepare a uniformly dispersed low-cost natural rubber raw rubber.

[0007] (2) First stage mixing: Add 100 parts of low-cost natural rubber raw rubber to the internal mixer, then add 3-10 parts of zinc oxide, 1-5 parts of stearic acid, 2-6 parts of antioxidant, 2-7 parts of silane coupling agent, 0-30 parts of reinforcing agent, and 6-10 parts of aromatic oil in sequence, and mix for 4-7 minutes to obtain the first stage compound. (3) Two-stage mixing: Add a first-stage compound to the open mill, then add 1.5-2.5 parts of sulfur and 1-2 parts of accelerator. After mixing for 3-5 minutes, a second-stage compound is obtained, which is the graphene natural rubber composite material used for conveyor belt cover rubber.

[0008] The various raw rubbers mentioned are one or more types of raw rubbers such as smoked sheets, standard rubber, and WF rubber.

[0009] The reinforcing agent is one or more of the following: silica, carbon black, talc, kaolinite, and montmorillonite.

[0010] The beneficial effects of this invention are as follows: Using inexpensive, low-cost natural rubber as raw material, and combining it with natural rubber raw materials and by-products from different origins and types, by adding inorganic fillers and rubber additives, a low-cost, high-performance, customized natural rubber production process is achieved, providing high-quality raw materials for the production of seismic isolation rubber bearings. This process not only improves product quality and performance but also reduces production costs, increases production efficiency, and meets the diverse market demands for seismic isolation rubber bearings. Detailed Implementation

[0011] The specific embodiments of the present invention will be further described in detail below with reference to the examples. The following examples are for illustrative purposes only and are not intended to limit the scope of the invention. Experimental methods in the following examples, unless otherwise specified, are generally performed under conventional conditions.

[0012] Example 1 100 parts of low-cost natural rubber raw rubber were added to a mixer for mastication. Then, 5 parts of zinc oxide, 3 parts of stearic acid, 1 part of antioxidant RD, 1.5 parts of antioxidant 4020, 3 parts of silane coupling agent, 30 parts of N220, and 8 parts of aromatic oil were added sequentially and mixed for 5 minutes to obtain a first-stage compound. The first-stage compound was then added to an open mill, followed by 2 parts of sulfur, 1 part of accelerator NS, and 1 part of accelerator TMTD. After mixing for 5 minutes, a second-stage compound was obtained. Finally, the compound was vulcanized on a flat vulcanizing machine at a vulcanization temperature of 150℃. The physical and mechanical properties of the vibration isolation bearing rubber formulation are shown in Table 1.

[0013] Example 2 100 parts of low-cost natural rubber raw rubber were added to a mixer for mastication. Then, 5 parts of zinc oxide, 3 parts of stearic acid, 1 part of antioxidant RD, 1.5 parts of antioxidant 4020, 4 parts of silane coupling agent, 20 parts of N220, and 8 parts of aromatic oil were added sequentially and mixed for 5 minutes to obtain a first-stage compound. The first-stage compound was then added to a two-roll mill, followed by 2 parts of sulfur, 1 part of accelerator NS, and 1 part of accelerator TMTD. After mixing for 5 minutes, a second-stage compound was obtained. The compound was then vulcanized on a flat vulcanizing machine at a vulcanization temperature of 150℃. The physical and mechanical properties of the seismic isolation bearing rubber formulation are shown in Table 1.

[0014] Example 3 100 parts of low-cost natural rubber raw rubber were added to a mixer for mastication. Then, 5 parts of zinc oxide, 3 parts of stearic acid, 1 part of antioxidant RD, 1.5 parts of antioxidant 4020, 4 parts of silane coupling agent, 25 parts of N220, and 8 parts of aromatic oil were added sequentially and mixed for 5 minutes to obtain a first-stage compound. The first-stage compound was then added to an open mill, followed by 2 parts of sulfur, 1 part of accelerator NS, and 1 part of accelerator TMTD. After mixing for 5 minutes, a second-stage compound was obtained. The compound was then vulcanized on a flat vulcanizing machine at a vulcanization temperature of 150℃. The physical and mechanical properties of the seismic isolation bearing rubber formulation are shown in Table 1.

[0015] Comparative Example 1 100 parts of natural rubber SCRWF were added to a mixer for mastication. Then, 5 parts of zinc oxide, 3 parts of stearic acid, 1 part of antioxidant RD, 1.5 parts of antioxidant 4020, 40 parts of N220, and 8 parts of aromatic oil were added sequentially and mixed for 5 minutes to obtain a first-stage compound. The first-stage compound was then added to an open mill, followed by 2 parts of sulfur, 1 part of accelerator NS, and 1 part of accelerator TMTD. After mixing for 5 minutes, a second-stage compound was obtained. The compound was then vulcanized on a flat vulcanizing machine at a vulcanization temperature of 150℃. The physical and mechanical properties of the vibration isolation bearing rubber formulation are shown in Table 1.

[0016] Table 1 Performance Comparison of Embodiments and Comparative Examples of the Invention

Claims

1. A method for preparing a low-cost natural rubber composite material for seismic isolation bearings, characterized in that, Includes the following steps: (1) Preparation of low-cost natural rubber raw rubber: Add various raw rubbers to a mixer, wash and dry them, and then mix them at high speed to prepare a uniformly dispersed low-cost natural rubber raw rubber. (2) First stage mixing: Add 100 parts of low-cost natural rubber raw rubber to the internal mixer, then add 3-10 parts of zinc oxide, 1-5 parts of stearic acid, 2-6 parts of antioxidant, 2-7 parts of silane coupling agent, 0-30 parts of reinforcing agent, and 6-10 parts of aromatic oil in sequence, and mix for 4-7 minutes to obtain the first stage compound. (3) Two-stage mixing: Add a first-stage compound to the open mill, then add 1.5-2.5 parts of sulfur and 1-2 parts of accelerator. After mixing for 3-5 minutes, a second-stage compound is obtained, which is the graphene natural rubber composite material used for conveyor belt cover rubber.

2. The method for preparing a low-cost natural rubber composite material for seismic isolation bearings according to claim 1, characterized in that: The various raw rubbers mentioned are one or more types of raw rubbers such as smoked sheets, standard rubber, and WF rubber.

3. The method for preparing a low-cost natural rubber composite material for seismic isolation bearings according to claim 1, characterized in that: The reinforcing agent is one or more of the following: silica, carbon black, talc, kaolinite, and montmorillonite.