Low temperature rubber for elastic seal and method for its production

By introducing reactive compatibilizing phases of high cis isoprene rubber and carboxyl-terminated liquid butadiene rubber into rubber materials, and combining them with graphene oxide and silica reinforcement, the problems of rubber material failure at extreme low temperatures and plasticizer migration are solved, achieving a balance between high strength and low-temperature flexibility.

CN123152189APending Publication Date: 2026-11-24HUBEI MICHERY NEW MATERIAL TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611591069.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-14
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing rubber materials lose elasticity at extreme low temperatures, leading to seal failure, and traditional plasticizer migration causes performance degradation, making it difficult to balance low-temperature performance and mechanical properties.

Method used

Using high-cis isoprene rubber as the continuous phase skeleton, terminal carboxyl liquid butadiene rubber and epoxy star-shaped polybutadiene form a reactive compatibilizing phase, combined with a composite reinforcing system of graphene oxide and silica, a peroxide/sulfur composite crosslinking system is constructed to avoid small molecule plasticizers and enhance interfacial bonding.

Benefits of technology

Maintaining high tensile strength and tear resistance at extreme low temperatures, avoiding plasticizer migration, and achieving a balance between low-temperature flexibility and mechanical properties in the material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123152189A_ABST
    Figure CN123152189A_ABST
Patent Text Reader

Abstract

This invention belongs to the interdisciplinary frontier technology field of polymer physics, polymer chemistry, and special rubber sealing materials engineering, specifically relating to a low-temperature rubber for elastic seals and its preparation method. It aims to solve the problems of weak interfacial bonding and difficulty in simultaneously achieving low-temperature resistance and mechanical properties in extremely cold environments. The rubber material of this invention uses high-cis isoprene rubber as the macroscopic continuous phase; terminal carboxyl-terminated liquid butadiene rubber as the nanoscale dispersed phase and reactive macromolecular plasticizer; and epoxy-modified star-shaped polybutadiene as a reactive polymeric compatibilizer. During thermomechanical mixing, the epoxy-modified star-shaped polybutadiene reacts with the terminal carboxyl-terminated liquid butadiene rubber and the matrix rubber to form a strongly compatibilizing interface linked by covalent bonds. A composite reinforcing system composed of silane coupling agent-modified silica and two-dimensional graphene oxide is added, and finally, vulcanization and sheeting are performed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the interdisciplinary frontier technology field of polymer physics, polymer chemistry and special rubber sealing materials engineering, and specifically relates to a low-temperature rubber for elastic seals and its preparation method. Background Technology

[0002] Elastic seals are indispensable key components in aerospace, automotive, and petrochemical industries, and their performance directly determines the sealing reliability and service life of equipment. In high-altitude areas, polar environments, high-altitude flight, and cryogenic media transportation, seals must withstand extreme low-temperature environments of -55°C or even lower for extended periods. Ordinary rubber materials lose elasticity at low temperatures due to the freezing of molecular chain segments, undergoing glass transition or crystallization hardening, leading to seal failure, media leakage, and even safety accidents.

[0003] In existing technologies, high-cis-butadiene rubber is often used in combination with isoprene rubber, and small-molecule plasticizers, such as esters and oils, are added to further improve low-temperature resistance. Existing patent CN112812387A discloses a cold-resistant and oil-resistant nitrile rubber for sealing components. By doping modified nitrile rubber and butadiene rubber, low-temperature elasticity can be improved without affecting oil resistance, but the following technical bottlenecks still exist: First, there is the issue of compatibility. Although both butadiene rubber and isoprene rubber belong to the diene rubber family, their different molecular chain structures lead to incomplete thermodynamic compatibility. Simple physical blending easily results in microscopic phase separation structures, and the lack of chemical bonding at the phase interface makes them prone to microcrack propagation during dynamic service or temperature cycling, leading to a decline in mechanical properties.

[0004] Second, there is the issue of plasticizer migration. While traditional small-molecule plasticizers can effectively lower the glass transition temperature, their interaction with the rubber matrix is ​​purely physical. Under long-term use or in environments with alternating high and low temperatures, small-molecule plasticizers are prone to migration, volatilization, or extraction by the working medium, leading to rubber hardening and shrinkage, a sharp deterioration in low-temperature performance, and premature failure of seals.

[0005] Third, it is difficult to achieve both low-temperature performance and mechanical properties simultaneously. To obtain low-temperature resistance below -55℃, existing technologies often require increasing the proportion of butadiene rubber. However, butadiene rubber itself has low strength and poor tear resistance. A high butadiene rubber ratio will lead to a significant decrease in the tensile strength, tensile stress at a given elongation, and abrasion resistance of the rubber compound, making it difficult to meet the mechanical property requirements of high-pressure or dynamic sealing scenarios.

[0006] To address the aforementioned issues, there is an urgent need to develop a rubber material that does not rely on small molecule plasticizers, has strong interfacial bonding, and can maintain excellent low-temperature performance while also possessing high strength properties, in order to meet the application requirements of high-end sealing components. Summary of the Invention

[0007] The purpose of this invention is to overcome the problems of existing technologies and provide a low-temperature rubber for elastic seals and its preparation method. High-cis isoprene rubber is used as a continuous phase skeleton to bear macroscopic stress, providing irreplaceable strain-induced crystallization ability, high tensile strength at a given elongation, and tear resistance. Terminal carboxyl-terminated liquid butadiene rubber with an ultra-low glass transition temperature is used as a uniformly dispersed nanoscale dispersed phase and a highly active reactive macromolecular plasticizer, providing an ultra-low temperature toughness base for the system due to its excellent segmental flexibility. Star-shaped polybutadiene is introduced as a reactive macromolecular compatibilizer. At the inorganic filler level, a composite reinforcing system composed of graphene oxide and silica is used, supplemented by graft modification with a specific silane coupling agent, to construct a peroxide / sulfur composite crosslinking system within the rubber matrix.

[0008] A low-temperature rubber for elastic seals and its preparation method are disclosed below: S1: Add 25-35 parts of carboxyl-terminated liquid butadiene rubber (CTPB) and 4-6 parts of epoxy star-shaped polybutadiene (ESPB) to a reactor and stir to mix, obtaining a premixed reaction solution. S2: 100 parts of high cis isoprene rubber are added to a mixer for plasticizing, then the premixed reaction solution obtained in step S1 is added, and then 0.02-0.04 parts of 2-ethyl-4-methylimidazolium catalyst are added for mixing. The CTPB terminal carboxyl group undergoes ring-opening esterification with the ESPB epoxy group under imidazolium catalysis to form a reactive compatibilizing phase containing β-hydroxy ester bonds. This compatibilizing phase is dispersed in the high cis isoprene rubber and forms an entangled or interpenetrating structure with the rubber chain segments. S3: Add the reinforcing system to the internal mixer in step S2. Specifically, add 30-40 parts of silica, 1-3 parts of graphene oxide, 3-5 parts of KH550 silane coupling agent, 1-3 parts of antioxidant 4020, 4-6 parts of zinc oxide, and 0.5-1.5 parts of stearic acid to the internal mixer and continue mixing for 3-5 minutes to ensure uniform dispersion of the filler. Reduce the temperature to below 80°C, add the vulcanization system, and mix for 1-2 minutes. Control the discharge temperature to not exceed 60°C, adjust the roller gap to 0.8 mm, and perform thin sheeting three times to obtain the low-temperature rubber compound. S4: The compounded rubber is placed in a flat vulcanizing machine for vulcanization to obtain the low-temperature rubber of the present invention for use in elastic seals.

[0009] Furthermore, the reactor described in step S1 is pre-evacuated and filled with high-purity nitrogen.

[0010] Furthermore, the stirring and mixing described in step S1 specifically involves stirring and mixing at a temperature of 60°C to 80°C for 40 to 60 minutes.

[0011] Furthermore, the plasticizing described in step S2 specifically involves plasticizing at 60°C to 80°C for 1 to 2 minutes.

[0012] Furthermore, the mixing described in step S2 specifically involves heating to 120℃~140℃ and mixing for 6~8 minutes.

[0013] Furthermore, the vulcanization system described in step S3 specifically comprises: 2-3 parts dicumyl peroxide and 0.2-0.4 parts sulfur.

[0014] Furthermore, the vulcanization described in step S4 specifically involves vulcanization at a pressure of 15 MPa and at a temperature of 150°C to 170°C for 10 to 20 minutes.

[0015] Compared with the prior art, the present invention has the following beneficial effects: (1) In this invention, the terminal carboxyl groups of terminal carboxyl liquid butadiene rubber (CTPB) and the epoxy groups of epoxy star-shaped polybutadiene (ESPB) undergo a ring-opening esterification reaction under the catalysis of 2-ethyl-4-methylimidazolium to generate a CTPB-ESPB graft copolymer containing β-hydroxy ester bonds in situ. This graft copolymer combines the flexible segments of CTPB with the multi-arm rigid skeleton of ESPB, and acts as a reactive macromolecular compatibilizer to form a nanoscale dispersed phase in a high cis isoprene rubber matrix. It forms a strong physical interaction with the matrix through segment entanglement and interpenetrating network structure.

[0016] (2) The present invention uses carboxyl-terminated liquid butadiene rubber to replace traditional small molecule plasticizers. Its high molecular weight makes it difficult to migrate; the carboxyl-terminated group can participate in crosslinking or interact with fillers, achieving low-temperature flexibility while completely avoiding the performance degradation problem caused by plasticizer precipitation.

[0017] (3) Without relying on small molecule plasticizers, the present invention enables the material to maintain high tensile strength while resisting low temperature through the synergistic effect of interface compatibilization and nano-composite reinforcement, thus breaking through the technical bottleneck of traditional blended adhesives that are difficult to balance low temperature performance and mechanical properties. Attached Figure Description

[0018] Figure 1 The image shows the FTIR spectrum obtained from Experiment Example 1.

[0019] Figure 2 This is a microscope image of the test in Experiment Example 2. Detailed Implementation

[0020] The endpoints and any values ​​of the ranges disclosed herein are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of the various ranges, the endpoint values ​​of the various ranges and individual point values, and individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed herein.

[0021] The preferred embodiments of the present invention are described in detail below; however, the present invention is not limited thereto. Within the scope of the inventive concept, various simple modifications can be made to the technical solutions of the present invention, including combinations of various technical features in any other suitable manner. These simple modifications and combinations should also be considered as the content disclosed in the present invention and are all within the protection scope of the present invention. A process flow for preparing low-temperature rubber for elastic seals, the detailed preparation steps of which are as follows: 1. Premixed reaction solution First, the reactor is evacuated and filled with high-purity nitrogen to completely replace any residual oxygen inside. Then, carboxyl-terminated liquid butadiene rubber and epoxy-modified star-shaped polybutadiene are added to the reactor cavity. The mixture is heated and stirred. At an appropriate heating temperature, both high-viscosity polymers transform into easily flowing fluids. Continuous constant-temperature stirring allows these two macromolecular fluids, which have slight polarity differences, to achieve uniform diffusion and miscibility at the molecular level under the influence of thermal motion. This physically shortens the spatial distance between the two reactive macromolecules, bringing the polar end groups closer together. This provides a spatial advantage for subsequent in-situ grafting reactions in the high-viscosity, low-diffusion-coefficient solid-phase reactor of the internal mixer, ultimately yielding a premixed reaction solution.

[0022] 2. In-situ grafting reaction High-cis isoprene rubber is fed into an internal mixer with a catalyst for mechanical plasticization. During this process, the extremely long macromolecular chains of the isoprene rubber undergo mechanical breakage and degradation. The resulting terminal macromolecular free radicals are rapidly quenched or reorganized in an oxygen-deficient or low-oxygen environment. Ultimately, this results in a sharp increase in the plasticity of the entire raw rubber material, a partial loss of elasticity, and a significant decrease in apparent viscosity. The premixed reaction solution is then slowly added to the internal mixer along with another catalyst. With the catalyst's intervention, the thermal shear field of the internal mixer is effectively converted into a reaction driving force. The catalyst rapidly promotes the dissociation of carboxyl groups from the terminal carboxyl groups of the liquid butadiene rubber, releasing nucleophilic carboxylate anions. These anions can efficiently attack the less sterically hindered carbon atoms on the three-membered ring of the star-shaped polybutadiene backbone epoxy resin, forcing them to undergo ring-opening esterification. This catalytic mechanism breaks the kinetic constraints of high activation energy in interfacial reactions during low-temperature, high-viscosity polymer melts. During the plasticizing process, in the initial stage of thermomechanical plasticizing, the high-cis isoprene rubber molecular backbone undergoes mechanochemical degradation due to high shear friction, generating highly active carbon-centered macromolecular free radicals. These free radicals are rapidly oxidized into terminal polar groups with the participation of trace amounts of oxygen infiltration within the system, and then these secondary polar groups are used to couple with the epoxy system. The isoprene macromolecules, with their reduced molecular weight after being cleaved, deeply intertwine with the in-situ generated CTPB-ESPB elastic polymer network due to their more flexible segmental conformation.

[0023] 3. Filler dispersion and sulfur addition for sheet formation Inorganic reinforcing fillers, including silica and two-dimensional graphene oxide, silane coupling agent KH550, and various activators such as zinc oxide powder, high-purity stearic acid, and antioxidants that provide anti-aging genes, are added to the mixing chamber. KH550, silica, and GO are added to the mixing system to improve filler wetting, dispersion, and filler-rubber interface bonding.

[0024] 4. Vulcanization molding The compounded rubber was placed in a flat vulcanizing machine for high-temperature vulcanization for 15 minutes to obtain the low-temperature rubber of the present invention for use in elastic seals.

[0025] Example 1 Table 1 Raw Material Information Table A low-temperature rubber for use in elastic seals and its preparation method are disclosed below: S1: Take 30 parts by mass of carboxyl-terminated liquid butadiene rubber and 4.9 parts by mass of epoxy star-shaped polybutadiene and add them to a reactor that has been evacuated and filled with high-purity nitrogen. Stir at 150 r / min and mix at 70℃ for 50 min to obtain a premixed reaction solution, wherein the epoxy / carboxyl equivalent ratio is 1.05. S2: Add 100 parts of high cis isoprene rubber to a 1.5L internal mixer, set the filling coefficient to 0.65, and plasticize at 70℃ for 1.5 min. Then add the premixed reaction liquid obtained in step S1, and then add 0.03 parts of 2-ethyl-4-methylimidazolium catalyst. To avoid the catalyst from being directly added and adhering to the top plug of the internal mixer, resulting in uneven dispersion, dissolve the catalyst with 5 parts of the premixed reaction liquid and then add it to the internal mixer. Heat to 130℃ and mix for 7 min. The torque curve shows a peak and then declines, and the torque fluctuation range is stable within ±5% within the next 3 min, which is used as the basis for determining the process endpoint. S3: Add the reinforcing system to the internal mixer in step S2. Specifically, add 35 parts of silica, 2 parts of graphene oxide, 4 parts of KH550 silane coupling agent, 2 parts of antioxidant 4020, 5 parts of zinc oxide, and 1 part of stearic acid to the internal mixer. First, pre-mix half of the total amount of graphene oxide and silica physically for 2 minutes. After adding all the reinforcing system to the internal mixer, continue mixing for 4 minutes to ensure uniform dispersion of the filler. Lower the temperature to below 80°C and add the vulcanization system, which contains 2.5 parts of dicumyl peroxide and 0.3 parts of sulfur. After mixing for 1.5 minutes, control the discharge temperature to not exceed 60°C, adjust the roller gap to 0.8 mm, and perform thin sheeting three times to obtain the low-temperature rubber compound. S4: Place the compounded rubber in a flat vulcanizing machine, vulcanize at a pressure of 15 MPa and at a temperature of 160°C for 15 minutes to obtain the low-temperature rubber of the present invention for elastic seals.

[0026] Example 2 The preparation method is the same as in Example 1, but with the following differences: In step S1: 25 parts of carboxyl-terminated liquid butadiene rubber and 4.08 parts of epoxy star-shaped polybutadiene are added to a reactor that has been evacuated and filled with high-purity nitrogen, and stirred and mixed at 60°C for 60 min. In step S2: 100 parts of high cis isoprene rubber are added to a mixer and plasticized at 60°C for 2 minutes. Then, the premixed reaction liquid obtained in step S1 is added, followed by 0.02 parts of 2-ethyl-4-methylimidazolium catalyst. The mixture is heated to 120°C and mixed for 8 minutes. In step S3: 30 parts of silica, 1 part of graphene oxide, 3 parts of KH550 silane coupling agent, 1 part of antioxidant 4020, 4 parts of zinc oxide and 0.5 parts of stearic acid are added to the internal mixer and mixed for 3 minutes. Then, 2 parts of dicumyl peroxide and 0.2 parts of sulfur are added to the vulcanization system and mixed for 1 minute. In step S4: vulcanize at 150°C for 20 minutes.

[0027] Example 3 The preparation method is the same as in Example 1, but with the following differences: In step S1: 35 parts of carboxyl-terminated liquid butadiene rubber and 5.71 parts of epoxy star-shaped polybutadiene are added to a vacuum reactor filled with high-purity nitrogen and stirred at 80°C for 40 minutes. In step S2: 100 parts of high cis isoprene rubber are added to a mixer and plasticized at 80°C for 1 min. Then, the premixed reaction liquid obtained in step S1 is added, followed by 0.04 parts of 2-ethyl-4-methylimidazolium catalyst. The mixture is heated to 140°C and mixed for 6 min. In step S3: 40 parts of silica, 3 parts of graphene oxide, 5 parts of KH550 silane coupling agent, 3 parts of antioxidant 4020, 6 parts of zinc oxide and 1.5 parts of stearic acid are added to the internal mixer and mixed for 5 minutes. Then, the vulcanization system, 3 parts of dicumyl peroxide and 0.4 parts of sulfur are added and mixed for 2 minutes. In step S4: vulcanize at 170℃ for 10 minutes.

[0028] Comparative Example 1 The preparation method of Example 1 is followed, but star-shaped polybutadiene is not added in step S1. The remaining steps are the same.

[0029] Comparative Example 2 The preparation method of Example 1 is used, but in step S1, an equal amount of ordinary polybutadiene without any terminal carboxyl active functional group modification is used to replace the terminal carboxyl liquid butadiene rubber.

[0030] Comparative Example 3 The preparation method of Example 1 is followed, but graphene oxide is not added in step S3. The remaining steps are the same.

[0031] Comparative Example 4 The preparation method is the same as in Example 1, but KH550 silane coupling agent is not added in step S3. The remaining steps are the same.

[0032] Experimental Example 1 The premixed reaction solution prepared in Example 1 and the low-temperature rubber were subjected to FTIR spectroscopy. The test mode was transmission mode, and the spectral scanning range was 4000 cm⁻¹. -1 -500cm -1 The spectral resolution was set to 4cm. -1 The number of scans was 64; the test results are as follows. Figure 1 As shown; In the spectrum of the premixed reaction solution, it is located at 915 cm⁻¹. -1 The characteristic asymmetric stretching vibration absorption peaks of the ESPB molecule's epoxy three-membered ring backbone exhibit extremely sharp and clear shapes, accompanied by a peak at 3056 cm⁻¹. -1The characteristic weak peaks nearby; in the low-temperature rubber spectrum after the addition of a catalyst and high-temperature thermomechanical mixing, 915 cm⁻¹ -1 The integral area of ​​the peak decayed exponentially and almost disappeared completely, proving that a large number of epoxy groups underwent high-frequency ring-opening reactions. The carboxyl and carbonyl groups at the ends of the CTPB molecule undergo a red shift due to strong hydrogen bonding, and are widely distributed around 1701 cm⁻¹. -1 ~1712cm -1 In the wavenumber range of low-temperature rubber spectra, this broadened carboxyl characteristic peak gradually weakens and disappears, replaced by a peak at approximately 1750 cm⁻¹. -1 ~1770cm -1 A sharp, strong absorption peak, highly geometrically distinctive, suddenly emerges; this new peak is attributed to the isolated carbonyl stretching vibration in the newly formed aliphatic covalent ester bond that does not participate in hydrogen bonding, proving that a strong covalent graft has been formed between the flexible segment of CTPB and the multi-arm rigid framework of ESPB; at 1089 cm⁻¹ -1 (Asymmetric stretching) and 800cm -1 The area near the (symmetrical bend) exhibits an extremely broad and strong characteristic absorption band, which is due to the robust silicon-oxygen-silicon network structure formed by the dehydration condensation of the KH550 silane coupling agent with the silanol groups and oxygen-containing groups of graphene oxide on the surface of silica after hydrolysis. In rubber systems where KH550 was added but not present in the premix, the terminal primary amine group undergoes a ring-opening addition reaction with the residual epoxy group, resulting in a 3300cm... -1 The bimodal characteristics of the primary amine NH3 in the vicinity evolved into a single peak or a broadened peak, and at 1109 cm⁻¹ -1 The presence of a characteristic CN stretching vibration peak nearby confirms the ring-opening reaction between the amino and epoxy groups; at 1636 cm⁻¹ in the low-temperature rubber spectrum... -1 ~1655cm -1 The region exhibits a characteristic strong absorption peak of amide bonds, which is due to the dehydration and amidation of the amino groups and oxygen-containing functional groups at the edges or sheets of graphene oxide at high temperatures.

[0033] Experiment Example 2 (1) Field emission scanning electron microscopy test: The low-temperature rubber sample prepared in Example 1 was cut into strips and completely immersed in liquid nitrogen for 15 minutes. Using a specific tooling, it was quickly broken in liquid nitrogen, and a very thin gold conductive layer was uniformly sputtered onto the fracture surface. Then, a field emission scanning electron microscope was used for testing. The accelerating voltage was set to 3.0-5.0 kV, the working distance to 5.0-8.0 mm, and the magnification to 10000x-50000x. The test results are as follows: Figure 2 As shown in (a); Due to the deep reaction that occurred in the high-temperature mixing field, the interfaces between the rubber matrix and the dispersed phases are soft, blurred, and integrated under the field of view, making it impossible to find any large-sized droplet islands with distinct boundaries. The equivalent diameter of the CTPB phase is reduced geometrically, extremely refined to the limit scale of tens to hundreds of nanometers, and uniformly dispersed in the polyisoprene substrate. The material exhibits extremely strong cryogenic toughness deformation capability, and the entire fracture surface shows typical "rough, torn, and scaly" ductile fracture morphology. Densely distributed dimples can be observed in the figure, while traditional filler pull-out pores are completely absent, which proves the extremely strong interfacial bonding between the matrix, dispersed phase, and filler. (2) Transmission electron microscopy test: The low-temperature rubber sample prepared in Example 1 was trimmed into 1mm x 1mm x 2mm pieces. Using a cryo-microtome, slices with a thickness of 100nm were cut with a diamond knife under liquid nitrogen temperature. The cut ultrathin slices were transferred to a standard 200-mesh pure copper screen and allowed to dry naturally at room temperature. Then, a transmission electron microscope was used for testing. The accelerating voltage was set to 120-200kV, and the magnification was 50000x-150000x. The test results are as follows: Figure 2 As shown in (b); The contrast between light and dark in the image stems from the intrinsic properties of the materials. The electron density of the two-dimensional graphene oxide carbon skeleton contrasts with that of the polyisoprene hydrocarbon matrix, and the high-density silica nanoparticles have a large electron scattering cross section, creating a striking contrast between light and dark. A multi-level, layered, three-dimensional spatial structure can be observed in the image: large, flexible, and rolled translucent GO sheets are layered and staggered within the matrix. High-contrast, dark spherical silica particles are densely trapped, embedded, and even firmly anchored in the wide interlayer spaces and highly active edge areas of the GO sheets. The silane coupling agent KH550 acts as an invisible binder, enabling the filler particles and sheets to form a continuous, crisscrossing, deep black three-dimensional network of load-bearing skeleton that runs through the transparent organic polymer phase.

[0034] Experimental Example 3 The comprehensive properties of the low-temperature rubbers prepared in combined Examples 1-3 and Comparative Examples 1-4 were determined. Tensile property test: The test was conducted in accordance with the standard GB / T 528-2009 "Determination of tensile stress-strain properties of vulcanized rubber or thermoplastic rubber". The vulcanized rubber sheet was cut into type 2 dumbbell-shaped specimens and tested at a tensile rate of 500 mm / min on a universal testing machine. Right-angle tear strength test: The test is conducted in accordance with the standard GB / T 529-2008 "Determination of tear strength of vulcanized rubber or thermoplastic rubber (trouser-shaped, right-angle and crescent-shaped specimens)". The vulcanized rubber sheet is cut into right-angle specimens and tested at a tensile rate of 500 mm / min on a universal testing machine. Low-temperature brittleness test: The test is conducted in accordance with the standard GB / T 1682-2014 "Determination of Low-Temperature Brittleness of Vulcanized Rubber - Single Specimen Method". The vulcanized rubber sheet is cut into specimens of specified size and placed in a low-temperature brittleness tester. The specimens are impacted at different temperatures, and the highest temperature at which the specimens show brittle fracture is recorded as the brittleness temperature. The specific test comparison results are shown in Table 2: Table 2. Comparison of overall performance between Examples 1-3 and Comparative Examples 1-4 The comparison results above show that Comparative Example 1, without the addition of epoxy star-shaped polybutadiene, lacks covalent bonds at the two-phase interface, resulting in significantly lower tensile and tear strengths than Example 1. This indicates that the weak phase interface leads to reduced stress transfer efficiency. Comparative Example 2 uses unmodified ordinary liquid polybutadiene instead of carboxyl-terminated liquid butadiene rubber. Although epoxy star-shaped polybutadiene is added, the lack of carboxyl groups at the end of the liquid rubber prevents grafting reactions with epoxy groups, limiting the compatibilization effect. Therefore, the tensile and tear strengths are still lower than in Example 1, and the low-temperature brittleness temperature is also lower. The results showed that the large molecular plasticizers without chemical bonds still had migration problems. In Comparative Example 3, no graphene oxide was added, and only silica was used for reinforcement. The tensile strength and tear strength were lower than those of the example, indicating that graphene oxide and silica play an important role in improving the reinforcement effect and stability. In Comparative Example 4, no KH550 silane coupling agent was added. The low-temperature rubber could still obtain good low-temperature performance due to the reactive compatibilization system. However, due to the lack of chemical bonding at the filler-rubber interface, the mechanical properties were significantly reduced, and the synergistic reinforcement advantage of graphene oxide and silica could not be fully utilized.

[0035] Those skilled in the art will readily understand that the present invention is perfectly suited to achieving the stated objectives, fulfilling the purposes, and realizing the advantages inherent in the invention as described above. The chemical substances, methods, steps, processes, molecules, and specific compounds mentioned herein are presently representative of preferred embodiments and are exemplary, and should not be construed as limiting the scope of the invention. Various variations and other applications will occur to those skilled in the art, all of which are included within the spirit of the invention and are defined by the scope of the claims.

[0036] It will be apparent to those skilled in the art that various substitutions and modifications can be made to the invention disclosed herein without departing from the scope and spirit of the invention.

Claims

1. A low-temperature rubber for elastic seals, comprising a peroxide / sulfur composite crosslinking system and a multiphase blend system with a strong interfacial structure, characterized in that, Based on 100 parts by weight of high cis isoprene rubber, the composition includes the following components in parts by weight: 25-35 parts of carboxyl-terminated liquid butadiene rubber; 4-6 parts of epoxy star-shaped polybutadiene; 0.02-0.04 parts of 2-ethyl-4-methylimidazolium; 30-40 parts of silica; 1-3 parts of graphene oxide; 3-5 parts of γ-aminopropyltriethoxysilane; 1-3 parts of antioxidant 4020; 4-6 parts of zinc oxide; 0.5-1.5 parts of stearic acid; 2-3 parts of dicumyl peroxide; and 0.2-0.4 parts of sulfur.

2. The low-temperature rubber for elastic seals according to claim 1, characterized in that, The number-average molecular weight of the terminal carboxyl liquid butadiene rubber is limited to 4000-6000, and the mass fraction of its terminal carboxyl groups is 1.5wt%-2.25wt%.

3. The low-temperature rubber for elastic seals according to claim 1, characterized in that, The epoxy star-shaped polybutadiene has an epoxy equivalent of 400 to 600 g / eq; the 2-ethyl-4-methylimidazolium has an epoxy equivalent of 0.5% to 2%.

4. A method for preparing a low-temperature rubber for an elastic seal according to any one of claims 1-3, characterized in that, Includes the following steps: S1: Add carboxyl-terminated liquid butadiene rubber and epoxy star-shaped polybutadiene to a reaction vessel and stir to obtain a premixed reaction solution. S2: Add high cis isoprene rubber to a mixer for plasticizing, then add the premixed reaction liquid obtained in step S1, and then add 2-ethyl-4-methylimidazolium catalyst for mixing; S3: Add the reinforcing system to the internal mixer in step S2. Specifically, add silica, graphene oxide, KH550 silane coupling agent, antioxidant 4020, zinc oxide and stearic acid to the internal mixer and continue mixing for 3-5 minutes to ensure uniform dispersion of the filler. Reduce the temperature to below 80°C, add the vulcanization system, and mix for 1-2 minutes. Control the discharge temperature to not exceed 60°C, adjust the roller gap to 0.8 mm, and perform thin sheeting 3 times to obtain the low-temperature rubber compound. S4: The compounded rubber is placed in a flat vulcanizing machine for vulcanization to obtain the low-temperature rubber of the present invention for use in elastic seals.

5. A method for preparing low-temperature rubber for elastic seals according to claim 4, characterized in that, The reactor described in step S1 is pre-evacuated and filled with high-purity nitrogen.

6. A method for preparing low-temperature rubber for elastic seals according to claim 4, characterized in that, The stirring and mixing described in step S1 specifically involves stirring and mixing at a temperature of 60℃ to 80℃ for 40 to 60 minutes.

7. A method for preparing low-temperature rubber for elastic seals according to claim 4, characterized in that, The plasticizing process described in step S2 specifically involves plasticizing at 60℃~80℃ for 1~2 minutes.

8. A method for preparing low-temperature rubber for elastic seals according to claim 4, characterized in that, The mixing conditions described in step S2 are 120℃~140℃ and the mixing time is 6~8min.

9. A method for preparing low-temperature rubber for elastic seals according to claim 4, characterized in that, The vulcanization system described in step S3 specifically comprises: 2-3 parts dicumyl peroxide and 0.2-0.4 parts sulfur.

10. A method for preparing low-temperature rubber for elastic seals according to claim 4, characterized in that, The vulcanization described in step S4 specifically involves a vulcanization pressure of 15 MPa and a vulcanization temperature of 150℃~170℃ for 10~20 min.

Citation Information

Patent Citations

  • Cold-resistant oil-resistant nitrile rubber for sealing element and preparation method of cold-resistant oil-resistant nitrile rubber

    CN112812387A