Wafer electroplating apparatus, method of use, and wafer electroplating system

By using a dual-cathode structure and dynamically adjusting the auxiliary cathode probe, the problem of uneven film thickness caused by uneven electric field distribution in wafer electroplating equipment is solved, achieving precise control and dynamic compensation of current density, and improving electroplating uniformity and adaptability.

CN123153138APending Publication Date: 2026-11-24SUZHOU JUNHUA SEMICONDUCTOR TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611566676.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-10
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In existing wafer electroplating equipment, the problem of uneven film thickness caused by uneven electric field distribution is difficult to solve effectively, especially the large difference in coating thickness gradient from the edge to the center of the wafer, and traditional equipment is difficult to change molds quickly and make flexible adjustments.

Method used

The device employs a dual-cathode structure, including a main cathode and an auxiliary cathode. The auxiliary cathode uses a fast-access mechanism and a servo motor-driven screw to enable rapid probe replacement and dynamic adjustment. The auxiliary cathode probes are spatially programmed and distributed on the wafer surface. Combined with a film thickness monitoring unit and a control unit, the device achieves precise control of the current density.

Benefits of technology

It enables precise control of wafer surface current density, dynamically compensates for uneven film thickness, adapts to different wafer sizes and pattern densities, is compatible with existing processes, has low modification costs, a wide range of applications, and improves product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123153138A_ABST
    Figure CN123153138A_ABST
Patent Text Reader

Abstract

This invention discloses a wafer electroplating equipment, its usage method, and a wafer electroplating system. The wafer electroplating equipment includes an electroplating tank, an anode, a cathode, and an auxiliary cathode. The auxiliary cathode includes an auxiliary cathode probe base, a probe base, and a screw. A quick-draw mechanism is provided between the auxiliary cathode probe base and the probe base, and the auxiliary cathode probe base and the probe base are detachably connected through the quick-draw mechanism to enable rapid replacement of the probe base. The side of the auxiliary cathode probe base facing away from the wafer is connected to the screw. Multiple auxiliary cathode probes are arranged on the side of the probe base that is in contact with the wafer, and the multiple auxiliary cathode probes are arranged on one side of the wafer surface to be electroplated. This invention achieves precise compensation of the current density on the wafer surface through spatial programming and dynamic spacing adjustment of the auxiliary cathode probes, solving the problem of uneven film thickness (thicker at the edges and thinner at the center), and has low modification costs.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the technical field of wafer electroplating equipment, specifically relating to a wafer electroplating equipment, its usage method, and a wafer electroplating system. Background Technology

[0002] As semiconductor manufacturing technology advances towards higher integration and advanced packaging, wafer copper plating has become a key process in chip interconnection and 3D stacked packaging. During the plating process, the wafer typically serves as the cathode. Copper ions in the electrolyte migrate to the wafer surface under the influence of an electric field and are reduced and deposited to form a copper plating layer. The in-plane uniformity of the plating film thickness directly affects subsequent chemical mechanical polishing, patterning, and the electrical performance and reliability of the device.

[0003] Current mainstream copper electroplating processes mostly employ static electrode configurations and peripherally clamped cathodes, applying current from the wafer edge. This results in a radial distribution of the electric field on the wafer surface, typically manifesting as high current density at the edges and low current density at the center. Combined with localized heating differences, flow field distribution, and electrolyte concentration gradients during electroplating, the thickness gradient from the wafer edge to the center can easily exceed 15%, creating the typical unevenness problem of "thick at the edges, thin at the center." Existing methods, such as adjusting the anode position, adding a plating cathode, or optimizing the flow field, are mostly static configurations or can only improve the uniformity of chemical composition. They are insufficient for dynamically compensating for electric field distortion and cannot respond to changes in wafer morphology, pattern density differences, electrolyte concentration gradients, or process differences between different electroplating recipes and equipment. Furthermore, traditional electrode structures are inconvenient to change, hindering rapid mold changes and flexible adjustments.

[0004] Therefore, in view of the above-mentioned technical problems, it is necessary to provide a wafer electroplating equipment, its usage method, and a wafer electroplating system.

[0005] The information disclosed in this background section is intended only to enhance the understanding of the overall background of the invention and should not be construed as an admission or in any way implying that the information constitutes prior art known to those skilled in the art. Summary of the Invention

[0006] The purpose of this invention is to provide a wafer electroplating equipment and its usage method, as well as a wafer electroplating system, which can realize spatial programming and dynamic compensation of the current density on the wafer surface, thereby significantly improving the uniformity of copper electroplating.

[0007] To achieve the above objectives, a specific embodiment of the present invention provides the following technical solution:

[0008] A wafer electroplating apparatus includes an electroplating tank, an anode, a cathode, and an auxiliary cathode. The electroplating tank contains an electrolyte. The anode and cathode are disposed within the electroplating tank and are used to clamp the periphery of the wafer and apply a main electroplating current to the wafer. The auxiliary cathode includes an auxiliary cathode probe base, a probe base, and a screw. A quick-draw mechanism is provided between the auxiliary cathode probe base and the probe base. The auxiliary cathode probe base and the probe base are detachably connected via the quick-draw mechanism to enable rapid replacement of the probe base. The side of the auxiliary cathode probe base facing away from the wafer is connected to the screw. Multiple auxiliary cathode probes are disposed on the side of the probe base that is in contact with the wafer. The multiple auxiliary cathode probes are disposed on one side of the wafer to be electroplated and are spaced apart from the wafer to provide spatial compensation for the current density on the wafer surface.

[0009] In one or more embodiments of the present invention, the distribution density of the auxiliary cathode probe located in the central region of the wafer is greater than that located in the edge region of the wafer.

[0010] In one or more embodiments of the present invention, the distance between the auxiliary cathode probe located in the center region of the wafer and the wafer is less than the distance between the auxiliary cathode probe located in the edge region of the wafer and the wafer.

[0011] In one or more embodiments of the present invention, a displacement mechanism is further included, the displacement mechanism including a servo motor, the servo motor being used to drive a screw to adjust the distance between the auxiliary cathode probe and the wafer during the electroplating process.

[0012] The present invention also provides a method of using the above-mentioned wafer electroplating equipment, comprising the following steps:

[0013] S1. Obtain the specific film thickness compensation value by clamping the periphery of the wafer with the cathode and achieving electrical conduction;

[0014] S2. Prepare an auxiliary cathode. Based on the film thickness compensation value and current density compensation formula, set the distribution density, height and distance between the auxiliary cathode probe and the wafer, and place it on one side of the wafer to be electroplated.

[0015] S3. Electrolyte is introduced into the electroplating tank and electricity is applied to cause metal ions to deposit on the wafer surface;

[0016] S4. During the electroplating process, the distance between the auxiliary cathode probe and the wafer is dynamically adjusted based on the film thickness monitoring results.

[0017] In one or more embodiments of the present invention, the formula for the electroplating current density compensation in step S2 is:

[0018] ΔJ = k × (N × h / d²);

[0019] Where N is the probe density (probes / cm²), h is the probe height (mm), d is the vertical distance from the probe to the wafer surface (mm), and k is the conductivity of the probe material (S / m).

[0020] In one or more embodiments of the present invention, in step S2, the probe base corresponding to different electroplating recipes is replaced by the quick-draw mechanism to adapt to the uniformity compensation requirements under different process conditions.

[0021] In one or more embodiments of the present invention, in step S4, the displacement mechanism is dynamically adjusted to ensure that the distance error between the probe and the wafer surface is ≤0.1mm, thereby avoiding local short circuits or current dispersion.

[0022] The present invention also provides a wafer electroplating system, including the above-described wafer electroplating equipment, and further comprising:

[0023] Film thickness monitoring unit, used to monitor the film thickness on the wafer surface;

[0024] The control unit, connected to the film thickness monitoring unit and the auxiliary cathode, is used to adjust the distance between the auxiliary cathode probe and the wafer based on the film thickness monitoring results, thereby achieving dynamic compensation for uniformity during the electroplating process.

[0025] In one or more embodiments of the present invention, the wafer plating system is compatible with both rack plating and cup plating.

[0026] Compared with the prior art, the wafer electroplating equipment, its usage method, and its wafer electroplating system of the present invention have the following advantages: they enable precise control of the current density on the wafer surface, effectively solving the problem of uneven film thickness; they can be adjusted according to different wafer sizes and pattern densities, exhibiting high dynamic adaptability and process flexibility; they are compatible with existing processes, have low modification costs, a wide range of applications, and improve product quality. Attached Figure Description

[0027] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0028] Figure 1 This is a top view of the auxiliary cathode in Embodiment 1 of the present invention;

[0029] Figure 2 This is a partial structural diagram of the auxiliary cathode in Embodiment 1 of the present invention;

[0030] Figure 3This is a schematic diagram of the structure of a wafer electroplating device according to Embodiment 1 of the present invention;

[0031] Figure 4 This is a schematic diagram of the structure of a wafer electroplating device according to Embodiment 2 of the present invention;

[0032] Figure 5 This is a comparison diagram of the effects of the present invention and conventional methods.

[0033] Explanation of key figure labels:

[0034] 1. Electroplating tank; 2. Anode; 3. Cathode; 4. Auxiliary cathode; 401. Auxiliary cathode probe base; 402. Probe base; 4021. Auxiliary cathode probe; 4022. Quick suction mechanism; 403. Screw. Detailed Implementation

[0035] To enable those skilled in the art to better understand the technical solutions in this disclosure, the technical solutions in the embodiments of this disclosure will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this disclosure, and not all embodiments. Based on the embodiments in this disclosure, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of this disclosure.

[0036] Example 1

[0037] like Figures 1 to 3 As shown, this embodiment provides a wafer electroplating apparatus, including an electroplating tank 1, an anode 2, a cathode 3, and an auxiliary cathode 4. This embodiment is a hanging electroplating system. The electroplating tank 1 contains the electrolyte, the anode 2 is disposed within the electroplating tank 1, and the cathode 3 is used to clamp the periphery of the wafer and apply the main electroplating current to the wafer. The auxiliary cathode 4 includes an auxiliary cathode probe base 401, a probe base 402, and a screw 403. The auxiliary cathode probe base 401 and the probe base 402 are magnetically connected via a quick-draw mechanism 4022. The side of the auxiliary cathode probe base 401 facing away from the wafer is connected to the screw 403. Multiple auxiliary cathode probes 4021 are disposed on the side of the wafer that is in contact with the probe base 402. These multiple auxiliary cathode probes 4021 are disposed on one side of the wafer's surface to be electroplated and spaced apart from the wafer, for spatial compensation of the current density on the wafer surface.

[0038] Specifically, the wafer to be electroplated is placed on cathode 3, with both sides of the wafer exposed in the electroplating solution. The wafer is clamped around its perimeter by fixtures, ensuring electrical conductivity. Auxiliary cathode 4 is positioned on one side of the wafer's electroplating surface, forming a dual-cathode structure together with cathode 3. The auxiliary cathode probe 4021 is preferably made of gold-plated tungsten, with a conductivity k≈1.8×10⁻⁶. 6 S / m, balancing conductivity, corrosion resistance and mechanical stability.

[0039] like Figure 1 As shown, the distribution of auxiliary cathode probes 4021 on the probe base 402 adopts a spatial programming design. The distribution density of auxiliary cathode probes 4021 in the wafer center region is greater than that in the wafer edge region, and the distance between the auxiliary cathode probes in the wafer center region and the wafer is smaller than that in the wafer edge region. In this embodiment, the density in the center region is set to 8~12 probes / cm², and gradually decreases to 2 probes / cm² in the edge region, forming a gradient distribution to achieve reverse compensation of "thickening at the center and thinning at the edge". At the same time, the height of the auxiliary cathode probes 4021 in the center region can be controlled at 1~2mm, and the height of the auxiliary cathode probes 4021 in the edge region can be increased to 4~5mm, using the physical property that the current field decreases with the square of the distance to precisely weaken the edge contribution.

[0040] Furthermore, the specific design position of the auxiliary cathode probe 4021 on the probe base 402 can be flexibly changed according to the process capabilities or process level of different equipment. For example, some equipment tends to produce a thicker electroplated film on the left side of the center, and the film gradually thins out to the right. In this case, the probe layout can have a higher density on the left side of the center, and then gradually become sparser as it expands outward from this area. By analogy, different equipment can be flexibly designed to further improve its electroplating capabilities.

[0041] The auxiliary cathode 4 also includes a displacement mechanism, which comprises a servo motor. The servo motor is connected to a screw 403 and drives the auxiliary cathode probe base 401 to move closer to or further away from the wafer, thereby dynamically adjusting the distance between the auxiliary cathode probe 4021 and the wafer. Through precise adjustment of the displacement mechanism, the distance error between the auxiliary cathode probe 4021 and the wafer surface is ensured to be ≤0.1mm, avoiding localized short circuits or current dispersion. During the electroplating process, as the electroplated film thickness increases, the servo motor drives the screw 403 to move the auxiliary cathode probe 4021 away from the wafer, thus dynamically adjusting the electroplating uniformity.

[0042] like Figure 2 As shown, the quick-draw mechanism 4022 is disposed between the auxiliary cathode probe base 401 and the probe base 402. The quick-draw mechanism 4022 can adopt a magnetic, snap-fit, or vacuum adsorption structure to achieve rapid replacement of the probe base 402. For the same equipment, different electroplating recipes may have potential differences in electroplating uniformity. Different probe distribution densities, heights, and arrangement patterns can be preset according to a specific recipe. Through the quick-draw mechanism 4022, the probe base 402 corresponding to different electroplating recipes can be quickly replaced to adapt to the uniformity compensation requirements under different process conditions.

[0043] Example 2

[0044] like Figure 4 As shown, this embodiment provides a cup-type wafer electroplating device, which differs from Embodiment 1 mainly in the electroplating tank 1 and the wafer placement method. In this embodiment, the electroplating tank 1 adopts a cup-type structure, the anode 2 is placed in the anode cup, the wafer is supported and fixed by a wafer carrier, and the cathode 3 contacts the contact area on the wafer surface to achieve circuit conduction. The auxiliary cathode 4 is placed on one side of the wafer to be electroplated, and its specific structure is the same as in Embodiment 1, including an auxiliary cathode probe base 401, a probe base 402, a screw 403, and a quick-suction mechanism 4022. The auxiliary cathode probe 4021 is placed on the end face of the probe base 402 that is in contact with the wafer and is spaced apart from the wafer.

[0045] This embodiment also provides a method for using a wafer electroplating equipment, which includes the following steps:

[0046] S1. The wafer periphery is clamped by cathode 3 and electrical conduction is achieved to obtain the specific film thickness compensation value.

[0047] The wafer is loaded onto cathode 3, which clamps the periphery of the wafer and enables circuit conduction. The film thickness is monitored under different process conditions of the electroplating equipment to obtain specific film thickness compensation values. For example, film thickness data for different regions of the wafer can be obtained through pre-plated test pieces or an online film thickness monitoring unit to calculate the thickness difference between the edge and the center, and determine the current density distribution that needs compensation.

[0048] S2. Prepare the auxiliary cathode 4. Set the distribution density, height and distance between the auxiliary cathode probe 4021 and the wafer according to the film thickness compensation value and current density compensation formula, and set it on one side of the wafer to be electroplated.

[0049] Based on the film thickness compensation value obtained in step S1, the auxiliary cathode 4 is designed according to the current density compensation formula: ΔJ=k×(N×h / d²). Specifically, the probe material is selected, such as a gold-plated tungsten needle, whose conductivity k≈1.8×10⁻⁶. 6 The probe density is set to 8-12 probes / cm² in the central region and 2 probes / cm² in the edge region, with a probe height of 1-2mm in the central region and 4-5mm in the edge region. The auxiliary cathode probe 4021 is placed on the probe base 402, and the probe base 402 is installed onto the auxiliary cathode probe base 401 using the quick-access mechanism 4022. The auxiliary cathode 4 is positioned on one side of the wafer to be electroplated, with the auxiliary cathode probe 4021 spaced apart from the wafer.

[0050] S3. Electrolyte is introduced into electroplating tank 1 and electricity is applied to cause metal ions to be deposited on the wafer surface.

[0051] Electrolyte is introduced into electroplating tank 1, and the power is turned on to create an electric field between anode 2 and cathode 3. Metal ions such as Cu in the electrolyte... 2+ The metal coating migrates to and is reduced and deposited on the wafer surface. During the electroplating process, the wafer can be rotated to improve flow uniformity.

[0052] S4. During the electroplating process, the distance between the auxiliary cathode probe 4021 and the wafer is dynamically adjusted based on the film thickness monitoring results.

[0053] The wafer surface film thickness is monitored in real time or intermittently by a film thickness monitoring unit. Based on the film thickness monitoring results, the control unit calculates the required distance adjustment amount according to the current density compensation formula and controls the servo motor to drive the screw 403 to adjust the distance between the auxiliary cathode probe 4021 and the wafer. For example, as the electroplated film thickness increases, the auxiliary cathode probe 4021 is controlled to move away from the wafer to achieve the effect of dynamically adjusting the electroplating uniformity. Through dynamic adjustment by the displacement mechanism, the distance error between the auxiliary cathode probe 4021 and the wafer surface is ensured to be ≤0.1mm, avoiding local short circuits or current dispersion.

[0054] Furthermore, when it is necessary to adapt to different electroplating recipes, the probe base 402 corresponding to different electroplating recipes can be replaced by the quick-draw mechanism 4022 to quickly switch the probe layout and meet the uniformity compensation requirements under different process conditions.

[0055] This embodiment also provides a wafer electroplating system, including the aforementioned wafer electroplating equipment, namely, an electroplating tank 1, an anode 2, a cathode 3, and an auxiliary cathode 4, and further including a film thickness monitoring unit and a control unit. The anode 2 is disposed within the electroplating tank 1, and the cathode 3 is used to hold the periphery of the wafer. The auxiliary cathode 4 includes multiple independently adjustable auxiliary cathode probes 4021. The film thickness monitoring unit is used to monitor the film thickness on the wafer surface. The control unit is connected to the film thickness monitoring unit and the auxiliary cathode 4, and is used to control the distribution density, height, and distance between the auxiliary cathode probes 4021 and the wafer based on the film thickness monitoring results and a current density compensation formula.

[0056] The control unit can control the displacement mechanism to drive the screw 403 via a servo motor, dynamically adjusting the distance between the auxiliary cathode probe 4021 and the wafer, so that the spacing error is ≤0.1mm.

[0057] The wafer plating system of this embodiment is compatible with both rack plating and cup plating. In rack plating, the auxiliary cathode 4 is connected to the displacement mechanism via a screw 403; in cup plating, the auxiliary cathode 4 is integrated into the wafer carrier side of the cup plating equipment. The system can be flexibly configured according to different equipment configurations to achieve spatial programming and dynamic compensation of the wafer surface current density.

[0058] like Figure 5As shown, COMSOL was used to simulate and compare this design with conventional methods. It was found that this design can significantly optimize the distribution of the electromagnetic field, thereby achieving the goal of optimizing the uniformity of electroplating.

[0059] In summary, this invention possesses spatial programming capability for current density. By adjusting the distribution density and distance from the wafer of the auxiliary cathode probe 4021, pixel-level control of the current density on the wafer surface can be achieved, directly solving the classic problem of "thick edges and thin center." It exhibits high dynamic adaptability and process flexibility; probe parameters (density, height) can be preset or adjusted in real-time based on different wafer sizes and pattern densities (such as BGA areas and copper pillar arrays). It is compatible with existing processes, does not change the cathode clamping method, and requires no replacement of the plating tank or rectifier system; only an auxiliary electrode module is added, making it easy to integrate into existing plating equipment with low modification costs. It allows for controllable adjustments to different equipment and processes, enabling rapid film replacement, improving efficiency and product quality. It is also compatible with both hanging plating and cup plating.

[0060] It will be apparent to those skilled in the art that this disclosure is not limited to the details of the exemplary embodiments described above, and that this disclosure can be implemented in other specific forms without departing from its spirit or essential characteristics. Therefore, the embodiments should be considered in all respects as exemplary and non-limiting, and the scope of this disclosure is defined by the appended claims rather than the foregoing description. Thus, all variations falling within the meaning and scope of equivalents of the claims are intended to be included within this disclosure. No reference numerals in the claims should be construed as limiting the scope of the claims.

[0061] Furthermore, it should be understood that although this specification describes embodiments, not every embodiment contains only one independent technical solution. This narrative style is merely for clarity. Those skilled in the art should consider the specification as a whole, and the technical solutions in each embodiment can also be appropriately combined to form other embodiments that can be understood by those skilled in the art.

Claims

1. A wafer electroplating equipment, characterized in that, include: Electroplating tank, used to hold electrolyte; The anode is disposed within the electroplating tank; The cathode is disposed in the electroplating tank and is used to hold the periphery of the wafer and apply the main electroplating current to the wafer; The auxiliary cathode includes an auxiliary cathode probe base, a probe base, and a screw. A quick-access mechanism is provided between the auxiliary cathode probe base and the probe base. The auxiliary cathode probe base and the probe base are detachably connected through the quick-access mechanism to enable rapid replacement of the probe base. The side of the auxiliary cathode probe base facing away from the wafer is connected to the screw. Multiple auxiliary cathode probes are provided on the side of the probe base that is in contact with the wafer. The multiple auxiliary cathode probes are located on one side of the wafer to be electroplated and are spaced apart from the wafer to provide spatial compensation for the current density on the wafer surface.

2. The wafer electroplating equipment according to claim 1, characterized in that, The distribution density of the auxiliary cathode probe located in the central region of the wafer is greater than that located in the edge region of the wafer.

3. The wafer electroplating equipment according to claim 1, characterized in that, The distance between the auxiliary cathode probe located in the center region of the wafer and the wafer is smaller than the distance between the auxiliary cathode probe located in the edge region of the wafer and the wafer.

4. The wafer electroplating equipment according to claim 1, characterized in that, It also includes a displacement mechanism, which includes a servo motor used to drive a screw during the electroplating process to adjust the distance between the auxiliary cathode probe and the wafer.

5. A method of using the wafer electroplating equipment according to any one of claims 1 to 4, characterized in that, Includes the following steps: S1. Obtain the specific film thickness compensation value by clamping the periphery of the wafer with the cathode and achieving electrical conduction; S2. Prepare an auxiliary cathode. Based on the film thickness compensation value and current density compensation formula, set the distribution density, height and distance between the auxiliary cathode probe and the wafer, and place it on one side of the wafer to be electroplated. S3. Electrolyte is introduced into the electroplating tank and electricity is applied to cause metal ions to deposit on the wafer surface; S4. During the electroplating process, the distance between the auxiliary cathode probe and the wafer is dynamically adjusted based on the film thickness monitoring results.

6. The method of using a wafer electroplating equipment according to claim 5, characterized in that, In S2, the formula for the electroplating current density compensation is: ΔJ = k × (N × h / d²); Where N is the probe density (probes / cm²), h is the probe height (mm), d is the vertical distance from the probe to the wafer surface (mm), and k is the conductivity of the probe material (S / m).

7. The method of using a wafer electroplating equipment according to claim 5, characterized in that, In step S2, the probe base corresponding to different electroplating recipes is replaced by the quick-draw mechanism to adapt to the uniformity compensation requirements under different process conditions.

8. The method of using a wafer electroplating equipment according to claim 5, characterized in that, In step S4, the displacement mechanism is dynamically adjusted to ensure that the distance error between the probe and the wafer surface is ≤0.1mm, thus avoiding local short circuits or current dispersion.

9. A wafer electroplating system, characterized in that, The wafer electroplating equipment as described in any one of claims 1-4 further includes: Film thickness monitoring unit, used to monitor the film thickness on the wafer surface; The control unit, connected to the film thickness monitoring unit and the auxiliary cathode, is used to adjust the distance between the auxiliary cathode probe and the wafer based on the film thickness monitoring results.

10. A wafer electroplating system according to claim 9, characterized in that, The wafer plating system is compatible with both hanging plating and cup plating.