High-position water washing electroplating device for ceramic circuit board

By using the clamping structure of upper and lower clamps and limiting blocks, as well as the design of the defoaming scraper, the problems of circuit board bending and shaking during electroplating are solved, achieving uniformity and stability in the electroplating of ceramic circuit boards and improving the electroplating quality.

CN123153141APending Publication Date: 2026-11-24湖南高登电子有限公司 +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611673544.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-28
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

When electroplating ceramic circuit boards using existing gantry plating equipment, the circuit boards are prone to bending and shaking due to the resistance of the plating solution, resulting in uneven plating and damage to the circuit boards. Furthermore, unilateral clamping leads to uneven electric field distribution, affecting the plating quality.

Method used

The circuit board is held by upper and lower clamps and limit blocks. The clamping force is adjusted by adjusting the lead screw and limit ring. Combined with the defoaming scraper to disturb the electroplating solution, the stability of the circuit board and the fluidity of the electroplating solution are ensured, and the retention of air bubbles is reduced.

Benefits of technology

It improves the uniformity of the metal coating after electroplating, reduces the probability of circuit board damage, enhances the quality and stability of electroplating, and reduces defects caused by bubbles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123153141A_ABST
    Figure CN123153141A_ABST
Patent Text Reader

Abstract

This invention relates to the field of circuit board electroplating technology, and more particularly to a high-level water-washing electroplating device for ceramic circuit boards. It includes a frame with a crossbeam, the crossbeam being rotatably connected to an array of mounting brackets. Each mounting bracket has symmetrically distributed adjusting components, and each adjusting component has a second mounting bracket. Both mounting brackets are slidably connected to symmetrically distributed clamps, each clamp being fixed to a receiving frame, and the receiving frame being slidably connected to a limiting block. This invention uses the clamps and limiting blocks on both the upper and lower sides to jointly clamp the circuit board, dispersing the clamping force on the circuit board, reducing the probability of the circuit board bending and shaking under the resistance of the electroplating solution, stabilizing the distance between the circuit board and the anode in the electroplating tank, reducing electric field fluctuations, improving the uniformity of the metal plating layer after electroplating, and simultaneously reducing the probability of edge chipping and cracking of the circuit board due to bending and shaking.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of circuit board electroplating technology, and more particularly to a high-level water-washing electroplating apparatus for ceramic circuit boards. Background Technology

[0002] Ceramic circuit boards, with their high thermal conductivity and high insulation properties, are widely used in power semiconductor devices. Strict requirements are placed on the uniformity of the metallization plating layer produced by their surface electroplating process. Existing gantry plating equipment often uses a single-sided clamping method to fix the ceramic circuit boards, with clamps only placed at the top of the board. During electroplating, to ensure real-time updates of the plating solution on both sides of the board, the board moves back and forth with the crossbeam after immersion. However, the ceramic circuit board is prone to bending and shaking due to the resistance of the plating solution, causing irregular changes in the distance between the board surface and the anode in the plating tank. This leads to uneven electric field distribution on the board surface, resulting in uneven metal plating thickness after electroplating. Furthermore, the ceramic circuit board is brittle, and the concentrated force from single-sided clamping makes it prone to chipping, cracking, and scrapping after bending and shaking. Summary of the Invention

[0003] In order to overcome the shortcomings mentioned in the background above, the present invention provides a high-level water washing electroplating apparatus for ceramic circuit boards.

[0004] The technical solution is as follows: A high-level water-washing electroplating device for ceramic circuit boards includes a frame, on which symmetrically distributed drive modules are mounted. The frame is provided with a crossbeam frame, and the drive modules are used to drive the crossbeam frame. The crossbeam frame is rotatably connected to an array of mounting frames. The mounting frames are provided with symmetrically distributed adjustment components. The symmetrically distributed adjustment components are collectively provided with a second mounting frame. Both the first and second mounting frames are slidably connected to symmetrically distributed clamps. Each clamp is fixedly connected to a receiving frame. The receiving frame is rotatably connected to a handle. The handle has a protrusion. The receiving frame is slidably connected to a limit block. The protrusion of the handle is used to press the corresponding limit block. The clamp and the corresponding limit block are used to clamp the circuit board. A tension spring is fixedly connected between the receiving frame and the corresponding limit block.

[0005] Furthermore, both the first mounting bracket and the second mounting bracket are rotatably connected to an adjusting screw, and the clamp is threadedly connected to the corresponding adjusting screw. The adjusting screw is used to adjust the distance between the corresponding clamps.

[0006] Furthermore, the adjustment assembly includes a limiting rod, which is fixedly connected to the corresponding mounting bracket one. The limiting rod is slidably connected to a sleeve, and a return spring is fixedly connected between the limiting rod and the corresponding mounting bracket two. The sleeve is fixedly connected to the corresponding mounting bracket two.

[0007] Furthermore, the limiting rod is slidably connected to a limiting ring, and the limiting ring is threadedly connected to a locking knob. The locking knob is used to lock the corresponding limiting ring onto the corresponding limiting rod, and the limiting ring is used to limit the corresponding sleeve.

[0008] Furthermore, the limiting block has a first guiding arc surface, and the clamp has a second guiding arc surface.

[0009] Furthermore, the crossbeam frame is equipped with symmetrically distributed electric actuators, the telescopic ends of which are all fixedly connected to a rack plate. The mounting frame is also fixedly connected with symmetrically distributed gears, all of which mesh with the rack plate for transmission.

[0010] Furthermore, the mounting frame is rotatably connected to several pairs of equally spaced defoaming scrapers, which are used to agitate the electroplating solution.

[0011] Furthermore, the distance between the lower parts of the same pair of defoaming scrapers gradually decreases from top to bottom.

[0012] Furthermore, the defoaming scraper has a guide plate, which is used to further agitate the electroplating solution.

[0013] Furthermore, the guide plate is composed of an array of guide sections one and an array of guide sections two, and the array of guide sections one and the array of guide sections two on the same guide plate are staggered.

[0014] The beneficial effects are as follows: This invention uses clamps and limiting blocks on both the upper and lower sides to hold the circuit board, dispersing the clamping force and reducing the probability of the circuit board bending and shaking under the resistance of the electroplating solution. This stabilizes the distance between the circuit board and the anode in the electroplating tank, reduces electric field fluctuations, and improves the uniformity of the metal plating layer after electroplating. At the same time, it reduces the probability of the circuit board chipping and cracking due to bending and shaking. By adjusting the lead screw, the corresponding clamps can be adjusted to accommodate circuit boards of different sizes. The adjustment component allows for the deflection amount of the circuit board, and the limiting ring controls the degree of deflection, allowing the circuit board to undergo elastic deformation. This absorbs the impact force of the plating solution on the circuit board during reciprocating movement and reduces the stress concentrated in the rigidly locked state. The oscillation of the defoaming scraper enhances the turbulence of the electroplating solution, destroys the conditions for bubble adsorption on the board surface, and promotes the escape of trapped bubbles in the lower part of the circuit board. This effectively reduces pinholes, missed plating, and thin local plating caused by trapped bubbles, improving the quality of the electroplated ceramic circuit board. Attached Figure Description

[0015] Figure 1 This is a three-dimensional structural diagram of the present invention; Figure 2This is a three-dimensional structural diagram of the crossbeam frame, mounting bracket 1, and rack plate of the present invention; Figure 3 This is a three-dimensional structural cross-sectional view of the crossbeam frame and rack plate of the present invention; Figure 4 This is a three-dimensional structural cross-sectional view of mounting bracket one and mounting bracket two of the present invention; Figure 5 This is a three-dimensional structural diagram of the sleeve and limiting ring of the present invention; Figure 6 This is a three-dimensional structural cross-sectional view of the receiving frame of the present invention; Figure 7 This is a three-dimensional structural cross-sectional view of the mounting bracket of the present invention; Figure 8 This is a three-dimensional structural diagram of the defoaming scraper of the present invention in a deflected state; Figure 9 This is a three-dimensional structural diagram of the defoaming scraper and the guide plate of the present invention.

[0016] In the attached diagram, the following labels are used: 1-frame, 2-drive module, 3-crossbeam frame, 4-mounting bracket one, 5-adjustment component, 6-mounting bracket two, 7-clamp, 8-receiving frame, 9-handle, 10-limiting block, 11-tension spring, 12-adjusting screw, 13-limiting rod, 14-sleeve, 15-reset spring, 16-limiting ring, 17-locking knob, 18-guide arc surface one, 19-guide arc surface two, 20-electric push rod, 21-rack plate, 22-gear, 23-defoaming scraper, 24-guide plate, 2401-guide section one, 2402-guide section two. Detailed Implementation

[0017] The present invention will be described in detail below with reference to the accompanying drawings and specific embodiments. During the electroplating process, air bubbles may be trapped in the lower part of the circuit board and the circuit board may be bent due to the resistance of the electroplating solution. The bending of the circuit board will exacerbate the problem of air bubble trapping.

[0018] Example 1: A high-level water-washing electroplating device for ceramic circuit boards, such as Figures 1-4 and Figure 6As shown, the system includes a frame 1, which contains a gantry frame, a hoisting mechanism, and an electroplating tank. The electroplating tank contains an anode plate. The frame 1 is equipped with symmetrically distributed drive modules 2, each including a reciprocating mechanism and a drive motor to control the reciprocating movement of a crossbeam frame 3 and its components. The frame 1 has a crossbeam frame 3, and all drive modules 2 are used to drive the crossbeam frame 3. The crossbeam frame 3 is located on the corresponding electroplating tank. The crossbeam frame 3 is rotatably connected to an array of mounting brackets 4, which are located below the crossbeam frame 3. Each mounting bracket 4 consists of a crossbeam and hinge ears. The crossbeam has a rectangular through slot for sliding the corresponding clamp 7. For example, in the figure, there are three mounting brackets 4, with two symmetrically distributed... Adjustment components 5 are located on the left and right sides of the corresponding mounting bracket 4. The symmetrically distributed adjustment components 5 are collectively mounted on a second mounting bracket 6, which is located below the corresponding adjustment components 5. The projections of the first mounting bracket 4 and the second mounting bracket 6 on the horizontal plane overlap. The second mounting bracket 6 has a rectangular through slot for sliding of the corresponding clamp 7. Both the first mounting bracket 4 and the second mounting bracket 6 are slidably connected to two symmetrically distributed clamps 7. Each clamp 7 is fixedly connected to a receiving frame 8. The receiving frame 8 is rotatably connected to a handle 9, located in front of the corresponding receiving frame 8. The handle 9 has a protrusion located on its rotation axis and is used to press against the corresponding limiting block 10. The receiving frame 8 is slidably connected to the limiting block 10. The limiting block 10 consists of a crossbar and a locking element. The crossbar of the limiting block 10 is slidably connected to the corresponding receiving frame 8. The limiting block 10 has a first guiding arc surface 18, which is located on the side of the corresponding limiting block 10 near the corresponding clamp 7. The clamp 7 has a second guiding arc surface 19, which is located on the side of the corresponding clamp 7 near the corresponding limiting block 10. The first guiding arc surface 18 of the limiting block 10 and the second guiding arc surface 19 of the corresponding clamp 7 are used together to guide and clamp the circuit board. Both the clamp 7 and the limiting block 10 are connected to existing conductive structures, and the conductive structures located in the electroplating solution have an insulating protective structure. The clamp 7 and the limiting block 10 are used together to supply power to the circuit board to reduce the uneven voltage drop caused by single-sided conductivity and increase the current on the board surface. The supply stability is improved, and the upper clamp 7 and the limiting block 10 can be staggered with the lower clamp 7 and the limiting block 10 to further improve the stability of the current supply to the board surface. The clamp 7 and the corresponding limiting block 10 are used together to clamp the circuit board. A tension spring 11 is fixed between the receiving frame 8 and the corresponding limiting block 10. The tension spring 11 is sleeved on the outside of the corresponding limiting block 10. The mounting frame 1 4 and the mounting frame 2 6 are rotatably connected to the adjusting screw 12. The adjusting screw 12 consists of an end cover, a threaded rod and a knob end. The thread of the threaded rod is a forward and reverse thread to drive the two corresponding clamps 7 to move in opposite directions or in the same direction, thereby adapting to circuit boards of different sizes. The clamp 7 is threadedly connected to the corresponding adjusting screw 12. The adjusting screw 12 is used to adjust the distance between the corresponding clamps 7.

[0019] like Figures 2-5 As shown, the adjustment assembly 5 includes limit rods 13, which are fixedly connected to the corresponding mounting bracket 4. The limit rods 13 are located on the lower side of the corresponding mounting bracket 4. As shown in the figure, there are six limit rods 13, with two limit rods 13 on each mounting bracket 4. A sleeve 14 is slidably connected to the lower side of the limit rod 13. A return spring 15 is fixedly connected between the limit rod 13 and the corresponding mounting bracket 6. The return spring 15 is located inside the corresponding sleeve 14. Under normal conditions, the return spring 15 is in a naturally extended state. The sleeve 14 is fixedly connected to the corresponding mounting bracket 6 and is located on the upper side of the corresponding mounting bracket 6. A limit ring 16 is slidably connected to the limit rod 13. The limit ring 16 is located on the movement path of the corresponding sleeve 14. A locking knob 17 is threadedly connected to the limit ring 16. The side of the locking knob 17 closest to the axis of the corresponding limit rod 13 is made of anti-slip rubber. The locking knob 17 is used to lock the corresponding limit ring 16. Locked on the corresponding limit rod 13, the limit ring 16 is used to limit the corresponding sleeve 14. The position of the limit ring 16 on the corresponding limit rod 13 can be adjusted to control the movement distance of the corresponding sleeve 14 relative to the corresponding limit rod 13. The crossbeam frame 3 is equipped with two symmetrically distributed electric push rods 20, which are located on the left and right sides of the crossbeam frame 3 respectively. The telescopic ends of the symmetrically distributed electric push rods 20 are fixedly connected to a rack plate 21. The rack plate 21 is slidably connected to the crossbeam frame 3. The mounting frame 4 is fixedly connected with two symmetrically distributed gears 22, which are located on the front and rear sides of the hinge ear of the mounting frame 4 respectively. The axis of the gears 22 is collinear with the axis of the hinge ear of the mounting frame 4. All gears 22 mesh with the rack plate 21 for transmission. The rack plate 21 is pushed to move back and forth left and right by the two electric push rods 20, thereby driving the mounting frame 4 and its parts to swing left and right.

[0020] Working Principle: When electroplating a ceramic circuit board, taking a mounting bracket 4 and its components as an example, first adjust the distance between the clamps 7 and their components according to the size of the circuit board to be electroplated. Rotate the two adjusting screws 12 to adjust the distance between the two clamps 7 on mounting bracket 4 and the distance between the two clamps 7 on mounting bracket 6 until the clamps 7 and their components move to the appropriate position. Stop rotating the adjusting screws 12, place the circuit board to be electroplated between the four clamps 7, and rotate the handle 9 corresponding to the clamp 7 until the limiting block 10 and the clamp 7 together clamp the circuit board. During this process, the protrusion of the handle 9 presses the corresponding limiting block 10 and pushes the limiting block 10 towards the circuit board. The tension spring 11 corresponding to the limiting block 10 is stretched and stores force. When the limiting block 10 contacts the circuit board, it continues to drive the circuit board towards the corresponding clamp. Move the seat 7 in the direction until the limit block 10 and the clamp 7 clamp the circuit board. Stop rotating the handle 9 to complete the clamping action of one point of the circuit board. Similarly, other points are clamped in the same way. After the clamping operation of the circuit board is completed, adjust the reserved deflection amount of the circuit board according to the size of the circuit board by using the limit ring 16. Turn the locking knob 17 to release the lock on the corresponding limit ring 16 and adjust the limit ring 16 to the appropriate height on the corresponding limit rod 13. When the height of the circuit board to be processed is large, the limit ring 16 moves upward relative to the corresponding limit rod 13. Conversely, the limit ring 16 moves downward relative to the corresponding limit rod 13 to leave the corresponding reserved deflection amount for circuit boards of different sizes. Then, tighten the corresponding locking knob 17. The rubber end of the locking knob 17 presses against the corresponding limit rod 13 and completes the locking of the corresponding limit ring 16.

[0021] After all circuit boards are clamped, the crossbeam frame 3 and its components are moved to the top of the corresponding electroplating tank using a gantry crane and hoisting mechanism. The crossbeam frame 3 and its components are then lowered using the hoisting mechanism until they contact and are supported by the drive module 2. The hoisting mechanism is then removed, leaving the circuit boards completely submerged in the electroplating solution. The drive motor and two electric push rods 20 of the drive module 2 are then activated. The drive motor in the drive module 2 controls the reciprocating mechanism, causing the crossbeam frame 3 and its components to reciprocate in the electroplating tank. The two electric push rods 20 push the rack plate 21 to move in the left and right directions. The circuit board is then switched on and the electroplating process begins. At this time, the anode plate on the inner wall of the electroplating tank is energized. The current flows through the electroplating solution, the circuit board, the clamp 7, and the limiting block 10 before being discharged through the conductive structure, reducing the voltage difference rate. The circuit board is the cathode. During the reciprocating movement of the crossbeam 3 and its components, the circuit board is resisted by the electroplating solution and flexes, which in turn drives the mounting bracket 6, the lower clamp 7, and its components to move upward. The sleeve 14 moves upward synchronously. If the flexing amplitude of the circuit board is too large, the sleeve 14 will contact the corresponding limiting ring 16 and limit the flexing amplitude of the circuit board to prevent excessive flexing from causing cracks in the circuit board.

[0022] During the upward movement of sleeve 14, the corresponding return spring 15 is compressed and stores force. When the circuit board moves in the opposite direction with the crossbeam 3, the direction of the resistance of the electroplating liquid on the circuit board changes, causing the circuit board to flex in the opposite direction. This causes the mounting bracket 6, the lower clamp 7, and the upper parts to move downward. During this process, the elastic force of the return spring 15 is released until sleeve 14 returns to its original position relative to the corresponding limit rod 13. As the crossbeam 3 continues to move, the mounting bracket 6, the lower clamp 7, and the upper parts move upward again, and the return spring 15 is compressed again. As the crossbeam 3 moves back and forth, the mounting bracket 6, the lower clamp 7, and the upper parts cycle through the above actions, thereby absorbing the impact force of the electroplating liquid on the circuit board during the reciprocating movement and reducing the stress concentrated in the rigidly locked state.

[0023] During electroplating, air bubbles generated during electroplating are trapped in the raised area at the bottom of the circuit board. During the reciprocating motion of the rack plate 21, the rack plate 21 meshes with the transmission gear 22, causing the gear 22 to rotate periodically. This drives the mounting bracket 4 and its components to oscillate back and forth, changing the resistance of the circuit board protrusions on the air bubbles along their upward path, thus assisting in the expulsion of air bubbles trapped in the bottom of the circuit board. After the circuit board electroplating is completed, the power is turned off, stopping the supply of power to the anode plate in the electroplating tank. After the crossbeam 3 is reset relative to the electroplating tank, the drive motor of the drive module 2 is turned off. The rack plate 21 is then moved relative to the crossbeam 3 via two electric push rods 20. After beam frame 3 is reset, the electric push rod 20 is turned off. Then, the beam frame 3 and its parts are removed from the electroplating tank by the hoisting mechanism. All parts on the beam frame 3 are removed from the electroplating tank and transported to the next stage for washing. After all processes are completed, the handle 9 is turned to release the compression limit of the corresponding limit block 10 by the protrusion of the handle 9. The tension spring 11 returns to its natural length and pulls the limit block 10 to reset relative to the corresponding support frame 8, releasing the clamping of the circuit board. After all clamping points are released, the circuit board is removed. The circuit board electroplating work is now complete. If the circuit board needs to be electroplated again, the above operation can be repeated.

[0024] Example 2: Based on Example 1, as follows Figure 2 , Figure 3 and Figures 7-9 As shown, mounting bracket 4 is rotatably connected to several pairs of equally spaced defoaming scrapers 23. The defoaming scrapers 23 are used to agitate the electroplating solution. Each mounting bracket 4 has three pairs of defoaming scrapers 23. The distance between the lower parts of the same pair of defoaming scrapers 23 gradually decreases from top to bottom. During the left-right swinging of mounting bracket 4, the corresponding defoaming scraper 23 swings relative to the mounting bracket 4 under its own weight. The defoaming scraper 23 does not contact the circuit board and maintains a gap. The coverage area generated by the swinging of adjacent defoaming scrapers 23 on the same mounting bracket 4 overlaps to improve the defoaming effect. The plate 23 is used to agitate the electroplating solution. The defoaming scraper 23 has a guide plate 24, which is composed of an array of guide sections 2401 and guide sections 2402. The guide sections 2401 and guide sections 2402 are arranged in an alternating pattern on the same guide plate 24. The guide sections 2401 and guide sections 2402 have guide protrusions with opposite tilt directions. The guide plate 24 is used to further agitate the electroplating solution, disrupt the bubble adsorption conditions on the plate surface, promote the escape of trapped bubbles in the lower part of the circuit board, and effectively reduce pinholes, missed plating, and thin local plating caused by trapped bubbles.

[0025] Working principle: During the reciprocating swing of the mounting bracket 4, the defoaming scraper 23 deflects relative to the corresponding mounting bracket 4 under its own gravity. Through the reciprocating swing of the defoaming scraper 23 relative to the mounting bracket 4, the electroplating solution in the lower part of the circuit board is disturbed, which disrupts the adsorption conditions of bubbles on the circuit board surface. Under the guiding action of the guide plate 24, the turbulence of the electroplating solution is enhanced, which promotes the escape of trapped bubbles in the lower part of the circuit board. This effectively reduces pinholes, missed plating, and thin local plating caused by trapped bubbles, and improves the quality of the electroplated ceramic circuit board.

[0026] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. A high-position water washing electroplating device for ceramic circuit board, comprising a frame (1), the frame (1) is provided with symmetrically distributed driving modules (2), the frame (1) is provided with a beam frame (3), the driving modules (2) are used for driving the beam frame (3), characterized in that, The crossbeam frame (3) is rotatably connected to an array of mounting brackets (4). The mounting brackets (4) are provided with symmetrically distributed adjustment components (5). The symmetrically distributed adjustment components (5) are together provided with a second mounting bracket (6). The mounting brackets (4) and the second mounting bracket (6) are slidably connected to symmetrically distributed clamps (7). The clamps (7) are fixedly connected to a support frame (8). The support frame (8) is rotatably connected to a handle (9). The handle (9) has a protrusion. The support frame (8) is slidably connected to a limit block (10). The protrusion of the handle (9) is used to press the corresponding limit block (10). The clamps (7) and the corresponding limit block (10) are used to clamp the circuit board. A tension spring (11) is fixedly connected between the support frame (8) and the corresponding limit block (10).

2. The high-level water-washing electroplating device for ceramic circuit boards according to claim 1, characterized in that, Both the first mounting bracket (4) and the second mounting bracket (6) are rotatably connected to an adjusting screw (12). The clamp (7) is threadedly connected to the corresponding adjusting screw (12). The adjusting screw (12) is used to adjust the distance between the corresponding clamps (7).

3. The high-level water-washing electroplating device for ceramic circuit boards according to claim 1, characterized in that, The adjustment component (5) includes a limiting rod (13), which is fixedly connected to the corresponding mounting bracket one (4). The limiting rod (13) is slidably connected to a sleeve (14). A return spring (15) is fixedly connected between the limiting rod (13) and the corresponding mounting bracket two (6). The sleeve (14) is fixedly connected to the corresponding mounting bracket two (6).

4. The high-level water-washing electroplating device for ceramic circuit boards according to claim 3, characterized in that, The limiting rod (13) is slidably connected to the limiting ring (16), and the limiting ring (16) is threadedly connected to the locking knob (17). The locking knob (17) is used to lock the corresponding limiting ring (16) onto the corresponding limiting rod (13), and the limiting ring (16) is used to limit the corresponding sleeve (14).

5. The high-level water-washing electroplating device for ceramic circuit boards according to claim 1, characterized in that, The limiting block (10) has a first guiding arc surface (18), and the clamp (7) has a second guiding arc surface (19).

6. The high-level water-washing electroplating device for ceramic circuit boards according to claim 1, characterized in that, The crossbeam frame (3) is equipped with symmetrically distributed electric push rods (20), and the telescopic ends of the symmetrically distributed electric push rods (20) are fixedly connected to a rack plate (21). The mounting frame (4) is fixedly connected with symmetrically distributed gears (22), and all the gears (22) mesh with the rack plate (21) for transmission.

7. The high-level water-washing electroplating apparatus for ceramic circuit boards according to claim 6, characterized in that, The mounting bracket (4) is rotatably connected to several pairs of defoaming scrapers (23) that are evenly distributed, the defoaming scrapers (23) being used to agitate the electroplating solution.

8. The high-level water-washing electroplating apparatus for ceramic circuit boards according to claim 7, characterized in that, The distance between the lower parts of the same pair of defoaming scrapers (23) gradually decreases from top to bottom.

9. A high-level water-washing electroplating apparatus for ceramic circuit boards according to claim 8, characterized in that, The defoaming scraper (23) has a guide plate (24) for further agitating the electroplating solution.

10. A high-level water-washing electroplating apparatus for ceramic circuit boards according to claim 9, characterized in that, The guide plate (24) is composed of an array of guide sections one (2401) and an array of guide sections two (2402), and the array of guide sections one (2401) and the array of guide sections two (2402) on the same guide plate (24) are staggered.