Electrochemical pretreatment method for cathode foil before etching
By introducing electrochemical pretreatment before the cathode foil is etched, uniformly distributed nanoscale point defects are generated, which solves the problem of uneven nucleation sites on the cathode foil surface and improves the specific surface area of the aluminum foil and the performance of the capacitor.
Patent Information
- Application Number
- CN202611580319.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-13
- Publication Date
- 2026-11-24
AI Technical Summary
In existing industrial cathode foil production, the uneven distribution of nucleation sites on the aluminum foil surface results in sparse and uneven nucleation of corrosion pits, making it impossible to achieve directional and uniform nucleation growth, which affects specific capacity and service life.
An electrochemical pretreatment process is introduced before the cathode foil is etched. Electrochemical polarization is used to generate uniformly distributed nanoscale point defects on the aluminum foil surface. The original oxide film on the aluminum foil surface is modified by electrochemical etching. Then, the foil is directly subjected to the AC etching process in a wet state to ensure the uniform nucleation and growth of corrosion pits.
This method achieves a high-density and uniform distribution of corrosion pits on the cathode foil surface, improving the specific surface area and the uniformity of corrosion pits, thereby enhancing the specific capacitance and stability of the capacitor.
Smart Images

Figure CN123153145A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of cathode foil production technology, and specifically to an electrochemical pretreatment method for cathode foil before corrosion. Background Technology
[0002] Aluminum electrolytic capacitors are indispensable passive components in electronic devices, widely used in consumer electronics, new energy, and industrial control equipment. The cathode aluminum foil, as the core material of aluminum electrolytic capacitors, directly determines the capacitor's specific capacitance, stability, and lifespan through its specific surface area and surface structure uniformity. Currently, the core process for industrial production of cathode foil is corrosion, which uses chemical or electrochemical corrosion to create numerous corrosion pits on the aluminum foil surface, thereby increasing the specific surface area of the aluminum foil and improving the energy storage performance of the cathode foil.
[0003] In existing industrial cathode foil production processes, aluminum foil, after simple degreasing and cleaning, is directly fed into the etching tank for continuous etching without any targeted pre-treatment surface conditioning steps. A native oxide film naturally forms on the surface of high-purity aluminum foil. This native oxide film suffers from inherent uneven thickness, loose structure, and randomly distributed defects. Simultaneously, the uneven distribution of trace impurities and second-phase particles within the aluminum foil matrix further exacerbates the surface variability. During conventional etching, etching pits can only nucleate randomly at surface defects and impurity sites, resulting in sparse and unevenly distributed nucleation sites.
[0004] To improve corrosion performance, existing technologies mainly focus on optimizing corrosion electrolyte formulations, adjusting corrosion current waveforms, and controlling corrosion temperature and time, among other downstream corrosion process parameters. These technologies can only passively regulate the corrosion rate during the corrosion process and cannot fundamentally solve the core problem of uneven distribution of nucleation sites on the aluminum foil surface, thus failing to achieve directional and uniform nucleation growth of corrosion pits.
[0005] Therefore, it is necessary to invent an electrochemical pretreatment method for cathode foil before corrosion to solve the above problems. Summary of the Invention
[0006] The purpose of this invention is to provide an electrochemical pretreatment method for cathode foil before corrosion, so as to solve the problems in the above-mentioned technology.
[0007] To achieve the above objectives, the present invention provides the following technical solution: an electrochemical pretreatment method for cathode foil before corrosion, comprising the following steps: S1. Degreasing and cleaning: Take the original aluminum cathode foil to be processed, use an alkaline degreasing process to remove oil, dust and oxidation impurities from the surface of the aluminum foil, and then rinse it with pure water to obtain clean aluminum foil. S2. Electrochemical pretreatment: The cleaned aluminum foil after rinsing is immersed in the pretreatment electrolyte. An electrochemical system is constructed with the original aluminum cathode foil as the working electrode and matched with the counter electrode. A preset electrochemical polarization treatment is applied to controllably etch and modify the original oxide film on the surface of the aluminum foil to obtain a pretreated aluminum foil with pre-formed nano-defects on the surface. S3. Pure water rinsing: The pre-treated aluminum foil is rinsed with pure water at room temperature for a short time to remove residual electrolyte on the surface and keep the aluminum foil wet without drying it. S4. Etching process: The wet aluminum foil is directly fed into the subsequent AC etching process, and the uniform etching pit nucleation and growth are completed by relying on the pre-prepared nano-defect sites.
[0008] Preferably, the pretreatment electrolyte is an aqueous solution of inorganic acid, and the electrolyte solute includes one or more of hydrochloric acid, sulfuric acid, and nitric acid, and the total hydrogen ion concentration of the electrolyte is 0.2 mol / L to 2.5 mol / L.
[0009] Preferably, the pretreated electrolyte also contains a trace amount of activating agent, which is a chloride salt, with a molar concentration of 0.005 mol / L to 0.15 mol / L.
[0010] Preferably, the electrochemical pretreatment adopts a constant potential mode, with the working electrode potential controlled at -0.8V to -1.6V relative to the saturated calomel electrode; the pretreatment time is 5s to 60s; and the electrolyte temperature is controlled at 25℃ to 55℃.
[0011] Preferably, the electrochemical pretreatment adopts a constant current mode, with the current density controlled at 20mA / cm² to 150mA / cm² and the energizing time at 3s to 45s.
[0012] Preferably, the counter electrode is a graphite electrode or a platinum electrode; the electrode spacing between the aluminum foil and the counter electrode is set to 2cm to 10cm.
[0013] Preferably, in step S1, the degreasing cleaning is performed by immersion cleaning in an alkaline degreasing solution at a cleaning temperature of 40℃~65℃ and a cleaning time of 1min~5min. After cleaning, the aluminum foil is rinsed with pure water until a continuous water film forms on the surface.
[0014] Preferably, in step S2, after electrochemical pretreatment, the original oxide film on the aluminum foil surface undergoes uniform local etching, generating a large number of discrete and uniformly distributed nanoscale point defects on the foil surface.
[0015] Preferably, in step S3, the water washing is a room temperature pure water spray washing, the washing time is 2s to 10s, no drying treatment is performed, and the wet state is directly entered into the corrosion process.
[0016] Preferably, in step S4, the aluminum foil that has undergone electrochemical pretreatment and water washing is then subjected to AC etching in a wet state. Surface nanoscale point defects serve as preferential dissolution nucleation sites, achieving high-density and uniform formation of etching pits.
[0017] The technical effects and advantages provided by the present invention in the above technical solution are as follows: 1. By adding an electrochemical pretreatment process before the formal corrosion process, high-density and uniformly distributed nanoscale point defects are actively pre-formed on the aluminum foil surface, changing the status quo of random nucleation of corrosion pits in traditional processes, and promoting the generation of a large number of corrosion pits in a uniform manner during the subsequent AC corrosion process, effectively increasing the effective specific surface area of the cathode foil. 2. After pretreatment, the aluminum foil is directly fed into the etching process while wet, eliminating the drying step and avoiding the formation of a dense oxide film during the drying process, which could cause pre-fabrication defects and failure. Attached Figure Description
[0018] Figure 1 This is a flow chart of the electrochemical pretreatment process for cathode foil corrosion according to the present invention. Detailed Implementation
[0019] To enable those skilled in the art to better understand the technical solution of the present invention, the present invention will be further described in detail below with reference to the accompanying drawings.
[0020] This invention provides, for example Figure 1 An electrochemical pretreatment method for cathode foil before corrosion is shown, comprising the following steps: S1. Degreasing and cleaning: Take the original aluminum cathode foil to be processed, use an alkaline degreasing process to remove oil, dust and oxidation impurities from the surface of the aluminum foil, and then rinse it with pure water to obtain clean aluminum foil. S2. Electrochemical pretreatment: The cleaned aluminum foil after rinsing is immersed in the pretreatment electrolyte. An electrochemical system is constructed with the original aluminum cathode foil as the working electrode and matched with the counter electrode. A preset electrochemical polarization treatment is applied to controllably etch and modify the original oxide film on the surface of the aluminum foil to obtain a pretreated aluminum foil with pre-formed nano-defects on the surface. S3. Pure water rinsing: The pre-treated aluminum foil is rinsed with pure water at room temperature for a short time to remove residual electrolyte on the surface and keep the aluminum foil wet without drying it. S4. Etching process: The wet aluminum foil is directly fed into the subsequent AC etching process, and the uniform etching pit nucleation and growth are completed by relying on the pre-prepared nano-defect sites.
[0021] In one aspect of this embodiment, the pretreatment electrolyte is an aqueous solution of an inorganic acid, and the electrolyte solute includes one or more of hydrochloric acid, sulfuric acid, and nitric acid, with a total hydrogen ion concentration of 0.2 mol / L to 2.5 mol / L; the pretreatment electrolyte also contains a trace amount of activating agent, which is a chloride ion salt, with a molar concentration of 0.005 mol / L to 0.15 mol / L.
[0022] The electrochemical pretreatment adopts a constant potential mode, with the working electrode potential controlled at -0.8V to -1.6V relative to the saturated calomel electrode; the pretreatment time is 5s to 60s; the electrolyte temperature is controlled at 25℃ to 55℃; the electrochemical pretreatment adopts a constant current mode, with the current density controlled at 20mA / cm² to 150mA / cm², and the energizing time is 3s to 45s; the counter electrode is a graphite electrode or a platinum electrode; the electrode spacing between the aluminum foil and the counter electrode is set to 2cm to 10cm.
[0023] In step S1, the degreasing cleaning is carried out by immersion cleaning in an alkaline degreasing solution at a cleaning temperature of 40℃~65℃ and a cleaning time of 1min~5min. After cleaning, the aluminum foil is rinsed with pure water until the water film on the surface is continuous.
[0024] In step S2, after electrochemical pretreatment, the original oxide film on the aluminum foil surface undergoes uniform local etching, generating a large number of discrete and uniformly distributed nanoscale point defects on the foil surface.
[0025] In step S3, the water washing is a room temperature pure water spray wash, with a washing time of 2s to 10s. No drying treatment is performed, and the wet state is directly introduced into the etching process.
[0026] In step S4, the aluminum foil that has undergone electrochemical pretreatment and water washing is then subjected to AC etching in a wet state. The nanoscale point defects on the surface serve as preferential dissolution nucleation sites, thereby achieving high-density and uniform formation of etching pits.
[0027] Working principle of this invention: Refer to the instruction manual appendix Figure 1 The process of this invention is as follows: First, the oil stains, dust impurities on the surface of the aluminum cathode foil are removed by degreasing and cleaning in step S1, eliminating the interference of external pollutants on the subsequent electrochemical treatment, and obtaining a clean aluminum foil. Then, the electrochemical pretreatment process proceeds to step S2, where a clean aluminum foil is placed in an acidic pretreatment electrolyte as the working electrode. Through constant potential or constant current cathodic polarization, the natural uneven primary oxide film on the aluminum foil surface is locally and controllably etched using the cathodic hydrogen evolution effect and the activation effect of chloride ions in the electrolyte. A large number of discrete and uniformly distributed nanoscale point defects are actively generated on the aluminum foil surface. These nanoscale point defects have higher atomic activity and become the preferred nucleation sites for subsequent etching processes. After the treatment is completed, step S3 is performed to rinse with pure water to remove only the residual electrolyte adhering to the surface of the aluminum foil. The aluminum foil is kept wet throughout the process and is not dried to avoid the formation of a dense oxide film on the surface of the aluminum foil during the drying process, which would destroy the pre-made nano defects. In step S4, the wet aluminum foil is directly fed into the AC etching process. The corrosive medium preferentially dissolves at the pre-made nanoscale point defects, inducing a large number of uniform nucleation growth of corrosion pits, reducing over-corrosion and uncorrosion areas, and finally obtaining cathodic corrosion aluminum foil with good uniformity of corrosion pit distribution and high specific surface area utilization.
[0028] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. An electrochemical pretreatment method for cathode foil before corrosion, characterized in that, Includes the following steps: S1. Degreasing and cleaning: Take the original aluminum cathode foil to be processed, use an alkaline degreasing process to remove oil, dust and oxidation impurities from the surface of the aluminum foil, and then rinse it with pure water to obtain clean aluminum foil. S2. Electrochemical pretreatment: The cleaned aluminum foil after rinsing is immersed in the pretreatment electrolyte. An electrochemical system is constructed with the original aluminum cathode foil as the working electrode and matched with the counter electrode. A preset electrochemical polarization treatment is applied to controllably etch and modify the original oxide film on the surface of the aluminum foil to obtain a pretreated aluminum foil with pre-formed nano-defects on the surface. S3. Pure water rinsing: The pre-treated aluminum foil is rinsed with pure water at room temperature for a short time to remove residual electrolyte on the surface and keep the aluminum foil wet without drying it. S4. Etching process: The wet aluminum foil is directly fed into the subsequent AC etching process, and the uniform etching pit nucleation and growth are completed by relying on the pre-prepared nano-defect sites.
2. The electrochemical pretreatment method for cathode foil corrosion according to claim 1, characterized in that: The pretreatment electrolyte is an aqueous solution of inorganic acid, and the electrolyte solute includes one or more of hydrochloric acid, sulfuric acid, and nitric acid, with a total hydrogen ion concentration of 0.2 mol / L to 2.5 mol / L.
3. The electrochemical pretreatment method for cathode foil corrosion according to claim 2, characterized in that: The pretreated electrolyte also contains a trace amount of activating agent, which is a chloride ion salt, with a molar concentration of 0.005 mol / L to 0.15 mol / L.
4. The electrochemical pretreatment method for cathode foil corrosion according to claim 1, characterized in that: The electrochemical pretreatment adopts a constant potential mode, with the working electrode potential controlled at -0.8V to -1.6V relative to the saturated calomel electrode; the pretreatment time is 5s to 60s; and the electrolyte temperature is controlled at 25℃ to 55℃.
5. The electrochemical pretreatment method for cathode foil before corrosion according to claim 1, characterized in that: The electrochemical pretreatment adopts a constant current mode, with the current density controlled at 20mA / cm² to 150mA / cm² and the energizing time at 3s to 45s.
6. The electrochemical pretreatment method for cathode foil corrosion according to claim 1, characterized in that: The counter electrode is a graphite electrode or a platinum electrode; the electrode spacing between the aluminum foil and the counter electrode is set to 2cm to 10cm.
7. The electrochemical pretreatment method for cathode foil corrosion according to claim 1, characterized in that: In step S1, the degreasing cleaning is carried out by immersion cleaning in an alkaline degreasing solution at a cleaning temperature of 40℃~65℃ and a cleaning time of 1min~5min. After cleaning, the aluminum foil is rinsed with pure water until the water film on the surface is continuous.
8. The electrochemical pretreatment method for cathode foil before corrosion according to claim 1, characterized in that: In step S2, after electrochemical pretreatment, the original oxide film on the aluminum foil surface undergoes uniform local etching, generating a large number of discrete and uniformly distributed nanoscale point defects on the foil surface.
9. The electrochemical pretreatment method for cathode foil corrosion according to claim 1, characterized in that: In step S3, the water washing is a room temperature pure water spray wash, the washing time is 2s to 10s, no drying treatment is performed, and the wet state is directly entered into the corrosion process.
10. The electrochemical pretreatment method for cathode foil corrosion according to claim 1, characterized in that: In step S4, the aluminum foil that has undergone electrochemical pretreatment and water washing is then subjected to AC corrosion in a wet state. The nanoscale point defects on the surface serve as preferential dissolution nucleation sites, thereby achieving high-density and uniform formation of corrosion pits.