Temperature uniformity adjustment structure and method

By designing a graphite substrate with non-uniform thickness and controlling the distribution of RF eddy current loss density, the problem of temperature non-uniformity in HVPE equipment is solved, improving the quality of semiconductor materials and device performance. This method is suitable for temperature uniformity adjustment in HVPE equipment.

CN123153162APending Publication Date: 2026-11-24WUXI WUYUE SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611375384.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-07
Publication Date
2026-11-24

Smart Images

  • Figure CN123153162A_ABST
    Figure CN123153162A_ABST
Patent Text Reader

Abstract

This invention discloses a temperature uniformity adjustment structure and method, comprising: a radio frequency coil, a quartz reaction cavity, a graphite cover, and a graphite base. The radio frequency coil is arranged around the outside of the quartz reaction cavity, the graphite cover is arranged inside the quartz reaction cavity to receive radio frequency energy and form a heating cavity, and the graphite base is arranged inside the graphite cover. The upper surface of the graphite base is used to support the substrate. The graphite base is constructed with a non-uniform thickness distribution to compensate for the temperature gradient caused by the heating of the graphite cover, so that the temperature of the substrate area tends to be uniform. By designing the non-uniform thickness of the graphite base, the density distribution of radio frequency eddy current loss can be specifically controlled, compensating for the temperature gradient caused by the graphite cover from the root of heat generation, so that the temperature of the substrate area tends to be uniform (temperature difference ≤15℃), and improving the thickness and composition uniformity of the epitaxial layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor manufacturing equipment technology, specifically to a temperature uniformity adjustment structure and method. Background Technology

[0002] Hydride vapor phase epitaxy (HVPE) technology is widely used in the fabrication of thick film materials, self-supporting substrates, and optoelectronic devices of III-V compound semiconductors such as gallium nitride (GaN), gallium arsenide (GaAs), and aluminum gallium nitride (AlGaN) due to its advantages such as extremely high growth rate (up to hundreds of micrometers per hour), relatively low equipment cost, and relatively simple process. In particular, HVPE technology plays a dominant role in the commercial production of large-size self-supporting gallium nitride substrates.

[0003] In HVPE equipment, the temperature field uniformity within the reaction chamber is one of the key factors determining the quality, thickness uniformity, compositional uniformity, and surface morphology of the epitaxial layer. Currently, mainstream HVPE equipment typically employs radio frequency induction heating: a radio frequency coil surrounds the outside of the quartz reaction chamber, applying a high-frequency (typically tens to hundreds of kHz) alternating electromagnetic field; a graphite shroud located inside the reaction chamber acts as an inductor, generating eddy current losses (Joule heating) under the influence of the electromagnetic field and rapidly heating up. This heat then heats the graphite substrate placed inside the shroud through thermal radiation and conduction, ultimately bringing the substrate supported on the graphite substrate to the required process temperature (typically as high as 1000℃-1100℃).

[0004] However, in practical applications, existing HVPE heating structures have significant technical defects. Due to the inherent skin effect of radio frequency electromagnetic fields, current tends to concentrate at the surface of the conductor, resulting in uneven heating of the graphite shield wall. Simultaneously, due to the electromagnetic field edge effect at the ends of the reaction cavity, and the disturbance of the electromagnetic field distribution caused by the complex geometry of the graphite shield and graphite base, unavoidable temperature gradients are generated during the heating process. Specifically, in most device configurations, the temperature of the central and edge regions of the graphite base is inconsistent, exhibiting a radial temperature difference distribution of "cold center, hot edge" or "hot center, cold edge." This uneven temperature field is directly transferred to the substrate surface through contact heat conduction and radiative heat transfer.

[0005] Temperature non-uniformity on the substrate surface can cause a series of serious problems: 1. Uneven growth rate: The HVPE reaction is a thermally activated process. Small differences in temperature can lead to differences in the decomposition efficiency and surface migration rate of the reaction precursors (such as GaCl and NH3), which in turn causes significant differences in the radial growth rate of the epitaxial layer, affecting the thickness uniformity.

[0006] 2. Uneven composition distribution: For alloy materials such as InGaN and AlGaN, the doping efficiency of different elements is extremely sensitive to temperature. Uneven temperature distribution can cause the alloy composition to drift within the wafer, affecting the consistency of the device's emission wavelength.

[0007] 3. Increased crystal defects: Uneven temperature introduces thermal stress into the epitaxial layer. When the thermal stress exceeds the critical shear stress of the material, it can induce dislocations, cracks, or even cause the epitaxial wafer to warp or crack.

[0008] These problems will ultimately significantly reduce product yield and reliability, severely limiting the application of HVPE technology in the fabrication of high-end devices such as laser diodes and high electron mobility transistors.

[0009] To address the aforementioned issues, existing technologies have attempted to optimize the process by adjusting the number of turns or spacing of the RF coil, changing the wall thickness of the graphite cover, or creating slots. However, these methods are often complex, involve replacing core components, are costly, and are difficult to apply precisely and flexibly to specific and complex temperature distributions, resulting in limited effectiveness. Summary of the Invention

[0010] The purpose of this invention is to provide a temperature uniformity adjustment structure and method to solve the problems mentioned in the background art.

[0011] To achieve the above objectives, the present invention provides the following technical solution: a temperature uniformity adjustment structure, comprising: a radio frequency coil, a quartz reaction cavity, a graphite cover, and a graphite base. The radio frequency coil is arranged around the outside of the quartz reaction cavity, the graphite cover is disposed inside the quartz reaction cavity for receiving radio frequency energy and forming a heating cavity, and the graphite base is disposed inside the graphite cover. The upper surface of the graphite base is used to support a substrate. The graphite base is constructed to have a non-uniform thickness distribution to compensate for the temperature gradient caused by the heating of the graphite cover, so that the temperature in the area where the substrate is located tends to be uniform.

[0012] In a preferred embodiment of the present invention, the thickness of the graphite base varies monotonically from the central region to the edge region to reduce the temperature difference between the central region and the edge region. This monotonous variation can be linear or nonlinear.

[0013] Furthermore, for different heating characteristics, the thickness distribution of the graphite base can be implemented in two opposite ways. When the graphite cover is heated and the temperature of the central region of the graphite base is lower than that of the edge region, the thickness of the central region of the graphite base is designed to be greater than that of the edge region. Conversely, when the graphite cover is heated and the temperature of the central region of the graphite base is higher than that of the edge region, the thickness of the central region of the graphite base is designed to be less than that of the edge region.

[0014] As a specific implementation of the present invention, the thickness distribution of the graphite base is achieved by changing the geometry of the upper or lower surface of the graphite base. For example, one surface can be kept as a plane while the other surface is processed into a curved or stepped surface.

[0015] Preferably, the lower surface of the graphite base is a plane, and the upper surface of the graphite base is a stepped surface to form a non-uniform thickness distribution. This structure is easy to process and facilitates stable contact with the bottom surface of the graphite cover below.

[0016] As a quantitative objective of the present invention, the "temperature tends to be uniform" means that, at the process temperature, the temperature difference between any two points in the area on the upper surface of the graphite base used to support the substrate is less than or equal to 15 degrees Celsius, and more preferably, the temperature difference can be controlled within 10 degrees Celsius.

[0017] According to a second aspect of the present invention, a method for adjusting temperature uniformity is also provided, applied to the structure described in any of the above-mentioned technical solutions, the method comprising the following steps: Step S1: Obtain the temperature distribution data of the surface of the graphite substrate with the initial shape under radio frequency heating conditions; Step S2: Based on the temperature distribution data, adjust the geometric parameters of the graphite base through simulation or experimental iteration to design a new shape that can compensate for uneven temperature regions. Step S3: The graphite base is fabricated into a solid with the new shape and placed inside the graphite cover; Step S4: Heat the graphite cover and the graphite base with the radio frequency coil so that the surface temperature of the substrate supported on them tends to be uniform.

[0018] Furthermore, in step S2, the geometric parameters of the graphite substrate are adjusted, specifically including adjusting its radial thickness distribution curve. By changing the thickness distribution, the induced current density distribution and heat conduction path of the graphite substrate in the radio frequency electromagnetic field can be changed, thereby achieving the control of the temperature field.

[0019] Preferably, the new shape design in step S2 aims to achieve a preset threshold for temperature uniformity in the bearing area on the upper surface of the graphite base. This preset threshold is defined as a temperature difference of less than or equal to 15 degrees Celsius between any two points.

[0020] Compared with the prior art, the beneficial effects of the present invention are: 1. This temperature uniformity adjustment structure and method can specifically control the density distribution of radio frequency eddy current loss by designing a non-uniform thickness for the graphite substrate, thereby compensating for the temperature gradient caused by the graphite cover from the root of heat generation, making the temperature in the substrate area more uniform (temperature difference ≤15℃), and improving the thickness and composition uniformity of the epitaxial layer. 2. This temperature uniformity adjustment structure and method only requires changing the geometry of the graphite base, a single component, without altering the core structure such as the radio frequency coil and reaction chamber. It is suitable for both new equipment manufacturing and low-cost upgrades of existing equipment. 3. This temperature uniformity adjustment structure and method can flexibly adapt to different temperature gradient conditions such as "cold center and hot edge" or "hot center and cold edge" by setting two opposite thickness variation trends, such as thick center and thin edge or thin center and thick edge. It has good universality. Attached Figure Description

[0021] Figure 1 This is a cross-sectional view of the overall structure in Embodiment 1 of the present invention; Figure 2 This is a schematic diagram of the overall structure in Embodiment 1 of the present invention; Figure 3 This is a schematic diagram of the graphite base structure in Embodiment 1 of the present invention; Figure 4 This is a schematic diagram of the graphite base in Embodiment 2 of the present invention; Figure 5 This is a flowchart of the adjustment method described in Embodiment 3 of the present invention.

[0022] In the attached diagram, the following are the reference numerals: 1. Radio frequency coil; 2. Quartz reaction chamber; 3. Graphite cover; 4. Graphite base; 5. Substrate. Detailed Implementation

[0023] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Identical components are denoted by the same reference numerals. It should be noted that the terms "front," "rear," "left," "right," "up," and "down" used in the following description refer to directions in the accompanying drawings, while the terms "bottom" and "top," "inner" and "outer" refer to directions toward or away from the geometric center of a specific component, respectively.

[0024] Example 1: As Figure 1 , Figure 2 As shown, this embodiment provides a temperature uniformity adjustment structure, which mainly includes a radio frequency coil 1, a quartz reaction chamber 2, a graphite cover 3, and a graphite base 4.

[0025] The radio frequency coil 1 is spirally arranged around the outside of the quartz reaction cavity 2 to generate a high-frequency alternating electromagnetic field. The quartz reaction cavity 2 is a cylindrical structure made of quartz material with high temperature resistance and good wave transmission. The graphite cover 3 is a hollow cover. The graphite cover 3 is placed at the bottom of the inner part of the quartz reaction cavity 2 as the main induction heating element. The graphite cover 3 absorbs radio frequency energy and heats up to form a heating cavity for epitaxial growth.

[0026] The graphite base 4 is placed inside the graphite cover 3, and the lower surface of the graphite base 4 is in close contact with the bottom of the quartz reaction chamber 2 to ensure good heat conduction. The upper surface of the graphite base 4 is a flat bearing surface used to place and support one or more substrates 5 to be grown. The substrate is a gallium nitride substrate. In this embodiment, under the specific operating conditions of the HVPE equipment (such as specific coil turns, frequency and graphite cover size), due to the skin effect of the electromagnetic field and the edge effect of the barrel structure, when the graphite cover 3 is heated, the temperature of the central region of the graphite base 4 located inside the graphite cover 3 is lower than the temperature of the edge region of the graphite cover 3. That is, there is a radial temperature gradient of "cold center and hot edge". The temperature difference between the center and the edge of the initially uniform thickness base can reach 20-30℃.

[0027] To compensate for this temperature gradient, such as Figure 3 As shown, in this embodiment, the graphite base 4 is designed with a non-uniform thickness distribution, specifically, the thickness of the central region is greater than that of the edge region, and the thickness changes monotonically from the center to the edge in an arc-shaped surface. The principle is that by changing the thickness distribution of the base, the equivalent resistance distribution inside the base is essentially changed, thereby regulating the density distribution of eddy current loss generated by radio frequency induction. The thicker region changes the path of the induced current due to the change in its cross-section, thereby generating more heat to compensate for the lower temperature in that region, and finally makes the temperature distribution of the entire upper surface tend to be uniform.

[0028] Furthermore, after testing, it was found that after adopting the graphite base 4 of this embodiment, at typical process temperatures (e.g., but not limited to 1000℃-1100℃), the temperature difference between any two points in the area on the upper surface of the graphite base 4 used to support the substrate 5 can be controlled within 15 degrees Celsius, which meets the process requirements for temperature uniformity.

[0029] Example 2: This example shows another implementation of the present invention to deal with completely opposite temperature difference conditions. The overall structure of this example is basically the same as that of Example 1, and will not be repeated here. The core difference is that the thickness distribution direction of the graphite base 4 is opposite.

[0030] Under another device configuration or process parameters corresponding to this embodiment (for example, when the bottom of the graphite cover 3 is thicker or the coupling method of the radio frequency coil is different), it was found that heating the graphite cover 3 caused the temperature of the central area of ​​the graphite base 4 to be higher than the temperature of the edge area of ​​the graphite base 4, that is, there is a temperature gradient of "hot center and cold edge". At this time, if the graphite base 4 of Embodiment 1 is still used, the temperature difference will be aggravated.

[0031] Therefore, as Figure 4 As shown, in this embodiment, the graphite base 4 is designed such that the thickness of the central region is less than that of the edge region, and the thickness increases monotonically from the center to the edge in a stepped manner. This stepped structure, by setting different thicknesses in the annular regions with different radii, can regulate the induced heating power in different radial regions. The thinner central region generates less heat, while the thicker edge region generates more heat, thereby compensating for the temperature gradient in the opposite direction. This also makes the temperature in the region where the substrate 5 is located tend to be uniform. As a variation of this embodiment, this thickness variation can also be achieved by processing the lower surface into a concave curved surface, which can also achieve the purpose of adjusting the induced current distribution.

[0032] Example 3: Figure 5 As shown, this embodiment provides a method for adjusting temperature uniformity. This method can be implemented based on the structure described in Embodiment 1 or Embodiment 2. This method is a typical "measurement-modeling-manufacturing-verification" engineering closed loop, including the following detailed steps: Step S1: Obtain initial temperature distribution data; A graphite base 4 with an initial shape (e.g., a conventional uniform thickness plate) is placed inside a graphite shroud 3. The reaction chamber is closed, evacuated, and a typical process gas (such as N2 or H2) is introduced. Under the set standard RF heating power and process atmosphere, the temperature at various points on the upper surface of the graphite base 4 is measured using multiple infrared thermometers arranged outside the quartz reaction chamber 2. The data is recorded, and a two-dimensional temperature distribution cloud map is plotted. This data should clearly and quantitatively reflect the distribution of high-temperature and low-temperature regions, the maximum temperature difference, and the direction and magnitude of the temperature gradient. This data serves as the baseline for subsequent optimization.

[0033] Step S2: Design a new shape; Based on the baseline temperature distribution data obtained in step S1, an accurate simulation model of the HVPE equipment heating system is established using finite element analysis software (such as the AC / DC module and heat transfer module coupling of COMSOL Multiphysics). In the model, the geometric parameters of the graphite base 4 (especially its radial thickness distribution curve, which can be set as a spline curve or piecewise function) are used as variables. The optimization objective is to minimize the temperature root mean square error of the target area on the upper surface of the graphite base 4 (i.e., the area where the substrate 5 is placed). Parametric scanning or topology optimization simulation is performed. The physical essence of this design is to reshape the induced current density distribution and heat conduction path in the radio frequency electromagnetic field by changing the radial thickness of the base, aiming to increase the power coupling density in the low-temperature region and decrease the power coupling density in the high-temperature region. The simulation will output a theoretically optimal base shape. As an alternative to the simulation method, when simulation conditions are not available, an experimental iteration method can also be used: based on the baseline temperature data, design and manufacture 2-3 graphite bases with different shape parameters based on experience, repeat step S1 for actual measurement, and gradually approach the optimal shape by comparing the test results.

[0034] Step S3: Fabricate and install the new base; Based on the precise geometric parameters of the new shape determined in step S2, high-purity, fine-particle, high-density isotropic graphite material is processed into a graphite base 4 with the new shape through high-precision CNC machining. After processing, the base is subjected to strict purification treatments such as ultrasonic cleaning and high-temperature vacuum baking to remove surface processing residues and adsorbed gases. Finally, in a dust-free environment, the graphite base 4 is carefully placed in the predetermined position inside the graphite cover 3 to ensure stable placement and good contact.

[0035] Step S4: Verify the uniform heating process; Start the radio frequency coil 1 and heat the graphite cover 3 and the graphite base 4 of the new shape according to the same process procedure (power, atmosphere, time) as in step S1. After the temperature stabilizes, use the same temperature measuring device and measuring point as in step S1 to monitor the temperature distribution on the upper surface of the graphite base 4. Compare the measurement results with the baseline data of step S1 and the simulation target of step S2. If the measured maximum temperature difference is less than or equal to the preset threshold (e.g., 15℃), the verification is successful and the new shape can be finalized and put into mass production. If the temperature difference still exceeds the expectation, the measured data is used as the new input and the process returns to step S2 for another round of optimization iteration.

[0036] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the invention can be implemented in other specific forms without departing from its spirit or essential characteristics. Therefore, the embodiments should be considered in all respects as exemplary and non-limiting, and the scope of the invention is defined by the appended claims rather than the foregoing description. Thus, all variations falling within the meaning and scope of equivalents of the claims are intended to be included within the present invention. No reference numerals in the claims should be construed as limiting the scope of the claims.

[0037] In the description of this invention, unless otherwise stated, "a plurality of" means two or more; the terms "upper," "lower," "left," "right," "inner," "outer," "front end," "rear end," "head," "tail," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the invention. Furthermore, the terms "first," "second," "third," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0038] In the description of this invention, it should be noted that, unless otherwise explicitly specified and limited, the terms "connected" and "linked" should be interpreted broadly. For example, they can refer to fixed connections or detachable connections; mechanical connections or electrical connections; direct connections or indirect connections through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.

Claims

1. A temperature uniformity adjustment structure, characterized in that, include: The radio frequency coil (1), quartz reaction cavity (2), graphite cover (3) and graphite base (4) are arranged around the outside of the quartz reaction cavity (2). The graphite cover (3) is located inside the quartz reaction cavity (2) to receive radio frequency energy and form a heating cavity. The graphite base (4) is located inside the graphite cover (3). The upper surface of the graphite base (4) is used to support the substrate (5). The graphite base (4) has a non-uniform thickness distribution to compensate for the temperature gradient caused by the heating of the graphite cover (3) so that the temperature of the area where the substrate (5) is located tends to be uniform.

2. The temperature uniformity adjustment structure according to claim 1, characterized in that, The thickness of the graphite base (4) varies monotonically from the central region to the edge region in order to reduce the temperature difference between the central region and the edge region.

3. The temperature uniformity adjustment structure according to claim 2, characterized in that, The thickness of the central region of the graphite base (4) is greater than the thickness of the edge region.

4. The temperature uniformity adjustment structure according to claim 2, characterized in that, The thickness of the central region of the graphite base (4) is less than the thickness of the edge region.

5. The temperature uniformity adjustment structure according to claim 1, characterized in that, The thickness distribution of the graphite base (4) is achieved by changing the geometry of the upper or lower surface of the graphite base (4).

6. The temperature uniformity adjustment structure according to claim 5, characterized in that, The lower surface of the graphite base (4) is a plane, and the upper surface of the graphite base (4) is a stepped surface to form a non-uniform thickness distribution.

7. The temperature uniformity adjustment structure according to claim 1, characterized in that, The temperature tends to be uniform when, at the process temperature, the temperature difference between any two points on the upper surface of the graphite base (4) used to support the substrate (5) is less than or equal to 15 degrees Celsius.

8. A method for adjusting temperature uniformity, applied to the structure as described in any one of claims 1 to 7, characterized in that, Includes the following steps: Step S1: Obtain the temperature distribution data of the surface of the graphite base (4) with the initial shape under radio frequency heating conditions; Step S2: Based on the temperature distribution data, adjust the geometric parameters of the graphite base (4) through simulation or experimental iteration to design a new shape that can compensate for the temperature unevenness region; Step S3: The graphite base (4) is made into a solid with the new shape and placed inside the graphite cover (3); Step S4: Heat the graphite cover (3) and the graphite base (4) through the radio frequency coil (1) so that the surface temperature of the substrate (5) supported thereon tends to be uniform.

9. The method according to claim 8, characterized in that, In step S2, the geometric parameters of the graphite base (4) are adjusted, including adjusting its radial thickness distribution curve, so as to change the induced current density distribution and heat conduction path of the graphite base (4) in the radio frequency electromagnetic field.

10. The method according to claim 8, characterized in that, The new shape designed in step S2 is aimed at achieving a preset threshold for the temperature uniformity of the bearing area on the upper surface of the graphite base (4). The preset threshold is a temperature difference of less than or equal to 15 degrees Celsius between any two points.