A multi-layer sealing anti-aging construction method for a wall-penetrating gas pipeline

Through the functional gradient design of the multi-layer sealing structure, the problem of easy cracking and rapid aging of the sealing structure during the construction of gas pipelines penetrating walls is solved, achieving a high-reliability and long-life sealing effect, adapting to various wall and pipeline deformations, and providing construction quality control and operation and maintenance convenience.

CN123154192APending Publication Date: 2026-11-24SIJI JIUTONG (HUBEI PROVINCE) ENGINEERING TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611371774.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-05
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In existing gas pipeline wall penetration construction, single sealing structures are prone to cracking and falling off, age quickly, and have poor water and corrosion resistance, posing safety hazards. Furthermore, gas can easily diffuse into the room after the seal fails, making it difficult to meet the needs of long-term use.

Method used

It adopts a multi-layer sealing structure, including an inner layer of elastic sealing filling, a middle layer of water-proof protective covering, an outer layer of anti-aging sealing and compaction, and a surface layer of anti-corrosion sealing molding, forming a four-level composite sealing system. Through functional gradient matching, it achieves synergistic protection of buffering and shock absorption, water-proofing and seepage prevention, and weather resistance and anti-aging.

Benefits of technology

Significantly improves sealing reliability, extends service life, adapts to different wall and pipe deformations, improves construction quality controllability, provides inspection and maintenance convenience, improves sealing structure reliability by more than 3 times, and achieves a service life of more than 15 years.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123154192A_ABST
    Figure CN123154192A_ABST
Patent Text Reader

Abstract

The application relates to the technical field of gas pipeline engineering construction, and discloses a multi-layer sealing anti-aging construction method for a wall-penetrating gas pipeline, which sequentially comprises the following steps: wall-penetrating hole pretreatment, pipeline positioning and fixing, inner-layer elastic sealing and filling, middle-layer water-blocking protection and coating, outer-layer anti-aging plugging and compaction, and surface-layer corrosion-proof sealing and protection forming; a four-level composite sealing system of 'inner-layer buffer-middle-layer water-blocking-outer-layer weather-resistant-surface-layer sealing and protection' is constructed in the annular gap between the wall-penetrating hole of a wall body and the gas pipeline; the inner-layer elastic sealing layer absorbs pipeline vibration and wall body settlement displacement; the middle-layer double-sided water-blocking layer blocks the horizontal water vapor permeation path; the outer-layer layered compaction plugging layer insulates light oxidation and provides structural support; and the surface-layer sealing and protection layer strengthens the weather-resistant and corrosion-resistant performance; through multi-material layer cooperation and gradient function matching, the application effectively solves the problems of easy cracking and falling off of a single sealing layer, quick aging failure, significantly improves the sealing durability and anti-leakage capacity of the wall-penetrating part, and reduces the gas leakage risk.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of gas pipeline engineering construction technology, specifically a multi-layer sealing and anti-aging construction method for through-wall gas pipelines. Background Technology

[0002] In urban gas transmission and distribution systems, gas pipelines passing through building walls is an essential construction step. The diameter of the opening in the wall is usually 10 to 50 mm larger than the outer diameter of the pipeline, forming an annular gap between the two. Currently, conventional construction methods often use single cement mortar filling, ordinary foam filling, or single-component sealant application for sealing, relying solely on a single layer of material to achieve a seal.

[0003] In actual engineering projects, this type of single-seal structure commonly fails after 3 to 5 years of service. On the one hand, uneven settlement of building walls, radial vibration caused by fluctuations in gas pressure in pipelines, and thermal expansion and contraction of pipelines caused by seasonal temperature changes can cause interface debonding or cracking of the rigid sealing layer, forming leakage channels. On the other hand, the outdoor sealing material is directly exposed to ultraviolet radiation, rainwater erosion, and air oxidation, causing the sealing material to age and become brittle rapidly, resulting in shrinkage and detachment.

[0004] Once rainwater and moisture seep into the annular gap, they will remain between the borehole wall and the pipe for a long time, causing corrosion of the galvanized steel pipe's outer wall and damage to the anti-corrosion layer, further shortening the pipe's service life. More importantly, after the seal fails, gas can diffuse into the room along the annular gap, which can easily cause safety accidents such as deflagration and poisoning. Existing improvement solutions mostly only add water-stop rings or increase the amount of sealant, without building a synergistic protection system from the perspective of functional layering and material gradient matching. Shock absorption, water insulation, and anti-aging performance cannot be taken into account, and the overall sealing durability is still difficult to meet the requirements of long-term use. Therefore, improvements are needed to address the above problems. Summary of the Invention

[0005] In response to the shortcomings of existing technologies where the single sealing layer of a gas pipeline through a wall is prone to cracking and falling off, ages rapidly, has poor water-proof and corrosion-resistant performance, and poses significant safety hazards, this invention provides a multi-layer sealing and anti-aging construction method for gas pipelines through walls. By constructing a multi-layer sealing structure with functional gradients, it achieves multiple synergistic protections of buffering and shock absorption, water-proofing and seepage prevention, and weather resistance and anti-aging, significantly improving the sealing reliability and service life of the wall penetration area.

[0006] To achieve the above objectives, the present invention provides the following technical solution: a multi-layer sealing and anti-aging construction method for through-wall gas pipelines, comprising six core processes in sequence: pretreatment of through-wall holes, pipeline positioning and fixing, inner layer elastic sealing filling, middle layer water-proof protection wrapping, outer layer anti-aging sealing and compaction, and surface anti-corrosion sealing and forming, forming a four-level composite sealing system from the inside out in the annular space between the through-wall hole and the gas pipeline.

[0007] Furthermore, the pretreatment process for through-wall holes improves the bonding strength between the sealing material and the wall substrate by roughening the inner wall and applying an interface agent. The chamfered structure of the hole opening increases the adhesion area of ​​the surface sealing layer and prevents edge lifting. By controlling the moisture content of the substrate, the curing effect and bonding performance of the interface agent and the sealing material are ensured.

[0008] The pipeline positioning and fixing process uses multi-point support adjustment to ensure that the pipeline and the borehole are coaxial, making the annular gap uniform and consistent. This avoids insufficient sealing layer thickness due to excessively small gaps on one side, or excessive settlement displacement due to excessively large gaps on one side. The displacement verification after locking can prevent pipeline movement during construction and ensure uniform thickness of each layer.

[0009] The inner elastic sealing filling process uses highly elastic sealing material, which is centrally located in the middle of the wall penetration hole as the first line of defense for sealing. At the same time, it absorbs the relative displacement caused by pipe vibration, thermal expansion and contraction and wall settlement by its own elastic deformation, thereby reducing the risk of cracking at the sealing interface from the root. The bottom-up injection method can effectively expel air in the gap and avoid the formation of pore defects inside the adhesive layer.

[0010] The middle layer waterproof protective coating process sets up a waterproof barrier on each side of the inner layer to form a double-sided waterproof structure, blocking the path of water vapor to penetrate laterally along the annular gap, while protecting the inner layer elastic material from water vapor erosion and extending the service life of the elastic layer; the embedded overlapping structure can eliminate the seepage gaps at the interlayer interface and improve the reliability of waterproofing.

[0011] The outer anti-aging sealing and compaction process uses high-strength, low-shrinkage sealing materials to be compacted in layers, providing structural support and resistance to external impacts. At the same time, it physically isolates ultraviolet rays and air, slowing down the oxidation and aging rate of the internal materials. The interlayer reinforcing mesh improves the crack resistance of the sealing layer, and the pre-embedded inspection holes provide inspection channels for construction acceptance and subsequent operation and maintenance.

[0012] The surface anti-corrosion sealing process forms a continuous weather-resistant sealing film on the outermost side, further blocking rainwater, ultraviolet rays and harmful gases from entering, while covering the walls around the openings to eliminate the risk of leakage at the corners; layered brushing and rounded edge treatment can improve the adhesion and weather resistance of the sealing layer.

[0013] Compared with the prior art, the beneficial effects of the present invention are: Multi-level functional collaboration significantly improves sealing reliability; through a four-level protection system of inner elastic buffer, middle double-sided waterproofing, outer structural sealing, and surface weather-resistant sealing, each layer complements the function and the failure path is blocked from each other. Compared with a single sealing layer, the anti-leakage performance is improved by more than 3 times, and it can withstand ±5mm of wall settlement displacement without leakage. Excellent anti-aging performance and significantly extended service life; the outer sealing layer and the surface sealing layer together form a double weather-resistant barrier, making it difficult for ultraviolet rays and oxygen to contact the internal elastic sealing material. The effective service life of the overall sealing structure can reach more than 15 years, which is 3 to 5 times that of the traditional single sealing method. It has strong deformation adaptability and is applicable to a wide range of scenarios; the inner high elastic material can absorb the radial vibration and axial thermal expansion and contraction displacement of the pipeline, and is suitable for various wall types such as brick-concrete structure and concrete shear wall, as well as the construction of gas pipelines with different pipe diameters; the layering parameters can be flexibly adjusted according to the wall thickness and pipeline specifications. Construction quality is controllable and highly inspectable; layered construction and layer-by-layer acceptance, with clear parameter control standards and quality inspection nodes for each process; pre-embedded inspection holes enable airtightness testing after completion and regular inspections later, facilitating operation and maintenance management, and unqualified parts can be directly repaired through the inspection holes. Attached Figure Description

[0014] The accompanying drawings are provided to further illustrate the invention and form part of the specification. They are used together with the embodiments of the invention to explain the invention and do not constitute a limitation thereof.

[0015] In the attached diagram: Figure 1 This is a block diagram of the hierarchical modules of the multi-layer sealing system of the present invention; Figure 2 This is a flowchart of the entire construction process of the present invention. Figure 3 This is a block diagram of the construction tooling and testing module of the present invention; In the diagram: 1. Wall; 2. Through-wall hole; 3. Beveled surface; 4. Gas pipeline; 5. Positioning bracket; 6. Inner elastic sealing layer; 7. Middle waterproof protective layer; 8. Outer anti-aging sealing layer; 9. Surface anti-corrosion protective layer; 10. Rough surface; 11. Interface agent; 12. Ring clamp; 13. Adjustable support leg; 14. Special pressure head; 15. Ring reinforcing mesh; 16. Primer coating; 17. Weather-resistant topcoat; 18. Barrier ring; 19. Inspection hole. Detailed Implementation

[0016] The technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.

[0017] Example 1: Construction of gas pipelines penetrating the exterior walls of brick-concrete residential buildings This embodiment is applied to the construction of gas inlet on the exterior wall of a 6-story brick-concrete residential building. The wall 1 is 240mm thick, and the gas pipe 4 is a hot-dip galvanized steel pipe with an outer diameter of 57mm and a wall thickness of 3.5mm. The diameter of the through-wall hole 2 is 110mm. Before construction, the ambient temperature was confirmed to be 20℃ and the relative humidity to be 60%, meeting the temperature and humidity requirements for construction. All materials were inspected and qualified upon arrival, including neutral silicone structural sealant, butyl rubber self-adhesive waterproof tape, polymer cement mortar, epoxy sealing primer, and acrylic weather-resistant topcoat. Construction tools were prepared: electric hammer chisel head, high-pressure air gun, angle grinder, feeler gauge (accuracy 0.02mm), pressure caulking gun, tension controller, silicone roller, special ring pressure head, trowel, probe-type compaction tester, etc. The specific construction steps are as follows: 1. Pre-treatment of through-wall holes The inner wall of the through-hole 2 on wall 1 was mechanically roughened using an electric hammer with a pointed chisel head. The chisel was evenly moved along the hole axis to form a continuous rough surface 10 with a depth of 3mm and a texture spacing of 6mm, ensuring that no smooth areas were missed. After roughening, a high-pressure air gun with a pressure of 0.5MPa was used to blow twice along the hole axis to remove floating dust, broken brick fragments, and loose particles. The inner wall was then wiped with a clean, damp cloth and allowed to dry until the moisture content of the base surface was 7%, meeting the control requirement of ≤8%. An angle grinder with a diamond grinding disc was used to grind a 45° chamfered surface 3 at both ends of the through-hole 2. The radial width of the chamfered slope 3 is 15mm. After sanding, the edge of the slope is sanded with fine sandpaper to remove sharp corners and burrs, ensuring a smooth slope. After cleaning, cement-based penetrating crystalline interface agent 11 is applied in two coats to the uneven rough surface 10 and the chamfered slope 3 with a brush. The second coat is applied after the first coat has dried for about 20 minutes. The total amount used is 0.35kg / ㎡. The coating is even, without dripping or missing any areas. After standing for 30 minutes until the interface agent 11 is dry to the touch, the quality inspector checks the roughness of the base surface, moisture content, and the quality of the interface agent application. Once these conditions are met, the process proceeds to the next step.

[0018] 2. Pipe positioning and fixing The gas pipe 4 is horizontally inserted into the wall penetration hole 2, and the axial position of the pipe is adjusted so that the length of each end extending out of the wall 1 is 200mm. Two sets of positioning brackets 5 are installed on the gas pipe 4, respectively 30mm away from the two ends of the wall penetration hole 2. The annular clamps 12 of the positioning brackets 5 are made of ABS engineering plastic, and their inner diameter is clearance-fitted with the outer diameter of the gas pipe 4. They are tightened to the outer wall of the pipe by bolts on both sides. Each annular clamp 12 has three adjustable support legs 13 evenly distributed at 120° circumference. The support legs are threaded and adjustable with an adjustment accuracy of 0.5mm. The outer end is equipped with an anti-slip rubber pad; rotate to adjust the extension length of each adjustable support leg 13, and use a feeler gauge to measure the width of the annular gap at four points: top, bottom, left, and right. Repeatedly calibrate to ensure that the gas pipe 4 and the wall penetration hole 2 are coaxial, and the gap deviation at the four points is controlled within 1.2mm, meeting the requirement of ≤1.5mm; after adjustment, tighten the locking nut of the adjustable support leg 13, and manually shake the pipe along the axial and radial directions to check the displacement. After confirming that the pipe has no movement and the support is not loose, mark the contact point between the pipe and the support for easy inspection and relocation later.

[0019] 3. Inner layer elastic sealing filler First, wipe the surface of the corresponding filling area on the outer wall of the gas pipeline 4 with a clean cotton cloth soaked in acetone to remove oil, dust, and zinc passivation film. After drying, install two PE plastic barrier rings 18 at the preset position. The axial distance between the two barrier rings 18 is 120mm, accounting for 50% of the total length of the through hole 2. Apply a small amount of silicone sealant to the contact area between the barrier rings 18 and the outer wall of the pipeline to fill the small gaps and prevent side leakage during sealant injection. Use neutral silicone structural sealant as an elastic filler with a Shore A hardness of 25 and an elongation at break of 350%, which meets the displacement buffering requirements. Apply pressure sealant. Insert the nozzle of the gun into the lowest point of the annular gap and slowly and evenly inject adhesive from bottom to top at an injection pressure of 0.3 MPa, so that the adhesive gradually fills and expels the air in the gap, avoiding the trapping of air bubbles; when the top of the gap continuously overflows with uniform adhesive without air bubbles, seal the overflow port with a plug, continue to maintain pressure for 8 seconds, and then turn off the adhesive gun; use a scraper to smooth the excess adhesive overflowing from both sides, so that the adhesive surface is flush with the outer end face of the barrier ring 18; let it stand for 4 hours to allow the sealant to dry to the touch, and after lightly pressing the surface with your hand, there should be no stickiness or dents. After checking that the adhesive layer is continuous without air bubbles or detachment, proceed to the next process to form the inner elastic sealing layer 6.

[0020] 4. Middle layer waterproof protective covering On the outer walls of the gas pipeline 4 on both sides of the inner elastic sealing layer 6, butyl rubber self-adhesive waterproof tape is wrapped to form a middle waterproof protective layer 7; the waterproof tape is 1.5mm thick, 50mm wide, and has a peel strength of 1.2N / mm at room temperature, exhibiting excellent waterproof performance; the wrapping starting point is located 5mm outside the barrier ring 18, spirally wrapped towards the orifice, and the wrapping tension is controlled at 6N by a tension controller to ensure tight adhesion of the tape without stretching or deformation; the overlap width between adjacent rings is 25mm, i.e., 1 / 2 of the tape width, and a total of 2 layers are wrapped, the first... The first layer is wrapped clockwise, and the second layer is wrapped counterclockwise, overlapping to cover the seams. After each layer is wrapped, a silicone roller is used to roll it evenly twice around the circumference to completely remove air bubbles between layers and ensure that the tape is completely adhered to the outer wall and inner end face of the pipe. The total axial length of the single middle layer waterproof protective layer 7 is 40mm, and its outer end extends 25mm into the subsequent outer anti-aging sealing layer 8, forming an embedded overlapping sealing structure. After wrapping, a circle of silicone sealant is applied to the outer edge of the waterproof tape to prevent it from curling up later and forming a seepage channel.

[0021] 5. Outer layer anti-aging sealing and compaction Polymer cement mortar with added polypropylene fibers was used as the sealing material. The fiber length was 12mm, and the dosage was 0.9kg / m³. 3 The mortar has a water-cement ratio of 0.35 and is mechanically stirred for 3 minutes until it is uniformly mixed and free of lumps. Its 28-day compressive strength is 25 MPa, and its impermeability grade is P8. Filling begins from the outer side of the middle waterproof protective layer 7 towards the orifice, with the first layer being 25 mm thick. After filling, a special annular pressure head 14 is used to apply pressure point by point along the circumference clockwise, with a working pressure of 0.2 MPa, ensuring uniform circumferential compaction. The compaction degree is tested using a probe-type compaction tester and reaches 93%, meeting the requirement of ≥90%. When the filling reaches half the total thickness, a layer of galvanized steel wire annular reinforcing mesh 15 is embedded, with a wire diameter of 0.8 mm and a mesh size of 10. mm×10mm, adjust the position of the mesh to be in the middle of the sealing layer thickness, and make the gap between it and the inner and outer walls uniform; continue to fill the second layer of sealing material and compact it in the same way until the end face of the sealing material is flush with the inner edge of the chamfered slope 3, forming the outer anti-aging sealing layer 8; before the initial setting of the sealing layer, use a trowel to perform a second troweling to eliminate surface plastic cracks and ensure the end face is flat; during construction, symmetrically embed two copper pipes as inspection holes 19 in the outer anti-aging sealing layer 8 on each side, with a pipe diameter of 5mm, the inner end extending to the outer interface of the middle waterproof protective layer 7, and the outer end extending 12mm out of the hole end face, and temporarily seal the pipe opening with tape to prevent mortar from entering.

[0022] 6. Surface anti-corrosion sealing molding After the outer anti-aging sealing layer 8 has initially set for 12 hours, the surface sealing construction is carried out. First, use fine sandpaper to sand the surface laitance and burrs on the end face of the sealing layer and the chamfered slope 3, and clean the dust with a brush to ensure that the base surface is dry and clean. First, apply a coat of epoxy sealing primer 16 evenly, with a coating amount of 0.2 kg / ㎡. The coating area covers the end face of the outer anti-aging sealing layer 8, the chamfered slope 3, and extends to a width of 60 mm around the outer surface opening of the wall 1, ensuring no missed areas or drips. After standing for 6 hours to allow the primer 16 to fully dry, apply the first coat of acrylic weather-resistant topcoat 17. After the surface is dry for 4 hours, apply the second coat. The two coats are applied perpendicular to each other, with a total dry film thickness of about 80 μm, forming a continuous and complete surface anti-corrosion sealing layer 9. At the edge of the sealing layer, use a small trowel to make an arc transition to avoid stress concentration that could lead to later warping and cracking.

[0023] After 72 hours of static curing, confirm that all layers are completely cured and remove the two sets of positioning brackets 5. For the small holes left after the brackets are removed, fill and compact them with silicone sealant and smooth them. Then, conduct an airtightness test: first, remove the temporary plug of test hole 19, introduce 0.01MPa compressed air, apply soapy water to the interfaces of each layer and around the hole to check for leaks, and observe that no bubbles overflow. Then, increase the pressure to 0.02MPa, close the air inlet valve and hold the pressure for 5 minutes, and record that the pressure drops to 7%, which meets the qualified standard of ≤10%. After the test is qualified, install a copper sealing plug with a nitrile rubber sealing ring at the port of test hole 19 and tighten it to seal. After the construction is completed, protect the finished product and avoid pipe collisions, external impacts and water immersion within 7 days.

[0024] Example 2: Construction of Gas Pipelines Penetrating Concrete Shear Walls in Commercial Buildings This embodiment applies to the construction of a gas pipeline penetrating a reinforced concrete shear wall in a commercial building. Wall 1 is 300mm thick with a strength grade of C30. Gas pipeline 4 is a seamless steel pipe with an outer diameter of 89mm and a wall thickness of 4mm. The penetration hole 2 has a diameter of 160mm. Before construction, the ambient temperature was confirmed to be 25℃ and the relative humidity 70%, meeting the construction conditions. All materials arriving on site had test reports, and the performance indicators of the single-component polyurethane elastic sealant, butyl rubber self-adhesive waterproof tape, polymer-modified anti-seepage mortar, and fluorocarbon weather-resistant topcoat met the standards. Construction equipment included sandblasting equipment, industrial vacuum cleaners, diamond grinding discs, dial indicators, high-pressure injection equipment, tension controllers, and specialized compaction tools. The specific construction steps are as follows: 1. Pre-treatment of through-wall holes The inner wall of the through-hole 2 on wall 1 was roughened using a dry sandblasting process. Quartz sand with a particle size of 0.5–1 mm was selected, and the sandblasting pressure was 0.6 MPa. The spray gun moved at a uniform speed along the hole axis, forming a uniformly roughened surface 10 with a depth of 4 mm and a texture spacing of 7 mm, completely covering the inner wall of the hole without any smooth blind spots. After sandblasting, an industrial vacuum cleaner was used to thoroughly remove dust and sand particles from the hole. Then, the inner wall was wiped with acetone to remove concrete release agent and oil stains. After drying, the moisture content of the base surface was measured to be 6.5%. The content meets the requirement of ≤8%; use diamond grinding discs to grind the 30° chamfered slope 3 at both ends of the through hole 2. The radial width of the chamfered slope 3 is 20mm. After grinding, the slope is smooth without concrete chipping or sharp edges; after cleaning, apply a coat of epoxy interface agent 11 to the uneven rough surface 10 and the chamfered slope 3. The coating is even and without omissions. The total amount is 0.4kg / ㎡. Let it stand for 45 minutes until the interface agent 11 reaches a semi-cured and sticky state. After passing the quality inspection, proceed to the next process.

[0025] 2. Pipe positioning and fixing Insert the gas pipeline 4 horizontally into the wall penetration hole 2, and adjust the axial position of the pipeline so that the lengths extending from both ends of the wall 1 are equal. Install three sets of positioning brackets 5 on the gas pipeline 4, located at both ends and the middle of the wall penetration hole 2, respectively, to ensure the support rigidity of the long-distance pipeline. The annular clamps 12 of each positioning bracket 5 are made of aluminum alloy and are fastened to the outer wall of the gas pipeline 4 with bolts. Each annular clamp 12 has four adjustable support legs 13 evenly arranged at 90° circumference, with a thread adjustment accuracy of 0.5mm and rubber anti-slip pads on the outer ends. During the adjustment process, use a dial indicator to measure the radial runout of the pipeline, repeatedly fine-tune the extension length of each adjustable support leg 13, and calibrate the levelness and coaxiality of the gas pipeline 4. The four-point deviation of the annular gap is controlled within 1.0mm. After the adjustment is completed, tighten all fixing nuts, apply a 100N thrust along the axial direction to check the pipeline displacement, and after confirming that there is no movement and the brackets are not deformed, mark the positioning.

[0026] 3. Inner layer elastic sealing filler First, sand the oxide layer on the outer wall of the gas pipe 4 corresponding to the filling area, then wipe it clean with acetone to remove oil. After drying, install two rubber barrier rings 18 in the preset position. The inner diameter of the barrier rings is interference-fitted with the pipe for a tight fit. The distance between the two barrier rings 18 is 150mm, accounting for 50% of the total length of the through hole 2. Apply a small amount of polyurethane sealant to both sides of the barrier rings to seal the edges. Use a single-component polyurethane elastic sealant as the inner filler, with a Shore A hardness of 22, an elongation at break of 400%, and elastic recovery. With a rate of ≥90% and excellent displacement compensation capability, the adhesive is injected from the lower side of the gap through a high-pressure injection device at a pressure of 0.35MPa. The injection speed is slow and uniform, allowing the adhesive to fill the entire filling area from bottom to top and expel internal air. When the upper overflow port continues to dispense adhesive without air bubbles, the overflow port is sealed, and the pressure is maintained for 10 seconds before the injection device is turned off. The excess adhesive is scraped off and left to stand for 6 hours to allow the sealant to dry and set. The surface of the adhesive layer is checked for air bubbles and cracks, and it is found to be firmly bonded to the pipe and the hole wall, forming an inner elastic sealing layer 6.

[0027] 4. Middle layer waterproof protective covering Butyl rubber self-adhesive waterproof tape is wrapped around both sides of the inner elastic sealing layer 6 to form a middle waterproof protective layer 7. The waterproof tape is 2mm thick, 60mm wide, has a peel strength of 1.5N / mm at room temperature, and exhibits excellent high and low temperature resistance. The wrapping starting point is located 5mm outside the barrier ring 18, and the tape is spirally wound towards the orifice. The wrapping tension is controlled at 7N by a tension controller to ensure full adhesion of the tape. The overlap width between adjacent loops is 30mm, which is half the width of the tape. A total of 3 layers are wrapped, with adjacent layers wrapped in opposite directions. The gaps are covered layer by layer in a crisscross pattern; after each layer is wrapped, a hard silicone roller is used to roll it circumferentially three times to completely remove air between layers, ensuring no air bubbles or curling edges; the total axial length of the single-layer middle waterproof protective layer 7 is 75mm, extending from the outside of the barrier ring 18 to 30mm from the orifice, of which 30mm extends into the inner part of the outer anti-aging sealing layer 8, forming a deeply embedded overlapping structure to completely block the interlayer penetration path; after wrapping, the outer edge of the waterproof tape is sealed with polyurethane sealant to create an arc edge.

[0028] 5. Outer layer anti-aging sealing and compaction The outer sealing material is polymer-modified cement-based impermeable mortar, with alkali-resistant glass fiber added internally. The fiber length is 15mm, and the dosage is 1.2kg / m³. 3The mortar has a 28-day compressive strength of 30 MPa, a permeability grade of P10, and a shrinkage rate of ≤0.15%. It is filled and compacted in four layers, with the thickness of each layer controlled within 28 mm. After each layer is filled, a special pressure head 14 is used to apply pressure evenly along the circumference, and the compaction degree of each layer is ≥93%. A stainless steel ring reinforcing mesh 15 with a wire diameter of 1 mm and a mesh size of 8 mm × 8 mm is embedded between the second and third layers. The mesh is placed in the center to effectively improve the crack resistance and impact resistance of the sealing layer. The filling is smoothed to the opening and connected to the chamfered slope 3. The surface is smoothed with a trowel and a second troweling treatment is performed before initial setting to form a dense outer anti-aging sealing layer 8. During construction, two stainless steel inspection holes 19 with a pipe diameter of 6 mm are symmetrically embedded along the circumference of the inner side of the outer layer. The inner end reaches the middle layer water-proof interface, and the outer end extends 15 mm beyond the end face of the hole to temporarily seal the pipe opening to prevent mortar from entering.

[0029] 6. Surface anti-corrosion sealing molding After the outer anti-aging sealing layer 8 has been cured for 24 hours, the surface sealing construction is carried out. First, the surface slurry is sanded off with sandpaper, and the dust is cleaned with a vacuum cleaner to ensure that the base surface is dry and clean. First, a polyurethane primer 16 is applied, covering the end face of the sealing layer, the chamfered slope 3, and the area around the opening of the wall 1 within 70mm, to fully seal the capillaries of the base surface. The application rate is 0.25kg / ㎡. After the primer 16 has been left to dry for 8 hours, two coats of fluorocarbon weather-resistant topcoat 17 are applied, with an interval of 6 hours between the two coats. The application directions are perpendicular to each other, and the total dry film thickness is about 120μm, forming the surface anti-corrosion sealing layer 9. This sealing layer has an artificial accelerated aging time of ≥1500h and excellent resistance to acid rain and ultraviolet rays. The edges of the sealing layer are rounded to ensure a smooth appearance and reliable sealing.

[0030] After 7 days of overall curing, all positioning brackets 5 were removed, and the remaining holes in the brackets were filled and smoothed with anti-seepage mortar, and the surface was coated with a protective coating. Then, an airtightness test was conducted: first, compressed air at 0.01MPa was introduced through the test hole 19, and leak detection liquid was applied to all interfaces. No bubbles were observed. Then, the pressure was increased to 0.025MPa and held for 5 minutes. The pressure drop was measured to be 6%, which meets the qualified standard of ≤10%. After the test was passed, stainless steel sealing plugs with fluororubber sealing rings were installed and tightened to seal. After the construction was completed, the finished product was protected and avoided from heavy object collisions, direct sunlight exposure and water immersion for 10 days.

[0031] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A method for constructing a multi-layer sealing anti-aging system for through-wall gas pipelines, characterized in that, Includes the following steps: S1 Pretreatment of through-wall hole: The inner wall of the through-wall hole (2) on the wall (1) is roughened to form a uniform uneven rough surface (10), the floating dust and debris in the hole are removed and the moisture content of the base surface is controlled, and an interface agent (11) is applied to the surface of the uneven rough surface (10). At the same time, a smooth chamfered slope (3) is processed at both ends of the through-wall hole (2). S2 Pipeline positioning and fixing: Insert the gas pipeline (4) horizontally into the wall hole (2), adjust the coaxiality of the gas pipeline (4) and the wall hole (2) by at least two sets of positioning brackets (5) distributed along the axial direction, calibrate the uniformity deviation of the annular gap ≤2mm, lock and fix it, and perform displacement verification. S3 Inner layer elastic seal filling: Clean the outer wall of the gas pipeline (4) and install two sets of barrier rings (18) to limit the filling area. Use pressure injection to inject elastic seal filler from the lower side of the annular gap to the space between the two barrier rings (18). After injecting glue until the glue overflows evenly on the opposite side, maintain pressure and shape to form an inner layer elastic seal layer (6) that completely wraps the gas pipeline (4). S4 Middle Layer Waterproof Protection Covering: On both sides of the inner elastic sealing layer (6), self-adhesive waterproof tape is used to wrap the outer wall of the gas pipeline (4) in a spiral winding manner, controlling the winding overlap ratio and tension. After winding, the gas is vented by roller pressing to form two independent middle layer waterproof protection layers (7), and the outer end of the middle layer waterproof protection layer (7) is embedded in the subsequent outer layer sealing structure to form an overlap seal. S5 outer anti-aging sealing compaction: Fiber modified sealing material is used to fill the annular gap outside the middle water-proof protective layer (7) in layers. After each layer is filled, a special pressure head (14) is used to apply pressure evenly in the circumference and compact it. Annular reinforcing mesh (15) is buried between layers to enhance crack resistance. Layer by layer construction forms a dense outer anti-aging sealing layer (8), and detection holes (19) are pre-embedded at the same time. S6 Surface Anti-corrosion Sealing Formation: Grind and clean the outer end face of the outer anti-aging sealing layer (8), apply sealing coating in layers on the end face of the sealing layer, the chamfered slope (3) and the surrounding wall (1) surface, and carry out the next layer of construction after each layer of coating is fully dry to form a continuous closed surface anti-corrosion sealing layer (9). After the overall curing is completed, remove the positioning bracket (5) and complete the finishing touches.

2. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to claim 1, characterized in that, In step S1, the rough surface (10) is roughened to a depth of 2-5 mm and the texture spacing is 5-8 mm; the moisture content of the inner wall base of the through hole (2) after cleaning is ≤8%; the interface agent (11) is a cement-based penetrating crystalline interface agent or an epoxy interface agent, applied in two coats, with a total dosage of 0.3-0.5 kg / m²; the chamfered slope (3) has an angle of 30°-45° and a radial width of 15-25 mm, and the slope is ground smooth without sharp corners or burrs.

3. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to claim 2, characterized in that, In step S2, the positioning bracket (5) includes an annular clamp (12) that grips the outer wall of the gas pipeline (4) and at least three adjustable support legs (13) evenly arranged around the annular clamp (12). The adjustment accuracy of the adjustable support legs (13) is not less than 0.5mm, and the outer end abuts against the inner wall of the through hole (2). The coaxiality is calibrated by using a feeler gauge and a dial indicator. The four-point deviation of the annular gap is ≤1.5mm. After fixing, the anti-displacement verification is carried out to ensure that the pipeline does not move.

4. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to claim 3, characterized in that, In step S3, the axial length of the inner elastic sealing layer (6) is 40% to 60% of the total length of the through hole (2); the elastic sealing filler is a neutral silicone structural sealant or a single-component polyurethane elastic sealant with a Shore A hardness of 20 to 30 and an elongation at break of ≥300%; the injection pressure is 0.2 to 0.4 MPa, and the glue is injected at a uniform speed from bottom to top. After the glue overflows, the pressure is maintained for 5 to 10 seconds, and the excess material is scraped off and left to dry.

5. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to claim 4, characterized in that, In step S4, the middle waterproof protective layer (7) is made of butyl rubber self-adhesive waterproof tape with a peel strength of ≥1.0N / mm at room temperature; the spiral winding overlap width is 1 / 2 of the tape width, the number of winding layers is 2 to 3, and the winding tension is controlled at 5 to 8N; after winding, the air is vented by rolling along the circumference for no less than 2 times using a roller pressing tool, and the length of the middle waterproof protective layer (7) embedded in the outer anti-aging sealing layer (8) is ≥20mm, and the end is sealed with sealant.

6. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to any one of claims 1 to 5, characterized in that, In step S5, the fiber-modified sealing material is a polymer cement mortar with added polypropylene fibers or alkali-resistant glass fibers, the fiber length is 10-15 mm, and the dosage is 0.8-1.2 kg / m³. 3 The sealing material has a 28-day compressive strength ≥20MPa and an impermeability grade ≥P8; the single-layer filling thickness is ≤30mm, the construction interval between adjacent layers is ≤30min, and the compaction degree of each layer is ≥90%; the ring-shaped reinforcing mesh (15) is set in the middle of the thickness direction of the outer anti-aging sealing layer (8), and galvanized steel wire mesh or stainless steel wire mesh is used, with a mesh size of 8~12mm.

7. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to any one of claims 1 to 5, characterized in that, In step S6, the surface anti-corrosion protective layer (9) includes a base layer (16) and a weather-resistant top layer (17) from the inside out; the base layer (16) is an epoxy sealing primer or a polyurethane primer with an adhesion grade ≥1; the weather-resistant top layer (17) is an acrylic or fluorocarbon topcoat with an artificial accelerated aging time ≥1000h; the coating area covers a ≥50mm wide area around the opening of the wall (1), the total dry film thickness is 80~150μm, and the edge is rounded.

8. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to claim 1, characterized in that, In step S5, the detection hole (19) is made of copper or stainless steel pipe with a diameter of 4-6 mm. Two detection holes are symmetrically arranged along the circumference of the outer anti-aging sealing layer (8) on each side. The inner end of the detection hole (19) extends to the outer interface of the middle water-proof protective layer (7), and the outer end extends 10-15 mm beyond the outer surface of the surface anti-corrosion sealing layer (9). The port is equipped with a sealing plug with a rubber sealing ring.

9. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to claim 8, characterized in that, After completing the maintenance in step S6, conduct an airtightness test: first, introduce 0.01MPa compressed air into the test hole (19), apply leak detection liquid to the interface of each layer to check for no bubbles overflow, then increase the pressure to 0.01~0.03MPa and hold for 5 minutes. If the pressure drop is ≤10%, it is considered qualified; if it is not qualified, inject sealant through the test hole (19) to repair the leak.

10. The multi-layer sealing and anti-aging construction method for through-wall gas pipelines according to claim 1, characterized in that, The ambient temperature for each construction process is 5-35℃ and the relative humidity is ≤85%. The inner elastic sealing layer (6) can be constructed after the surface is dry for ≥4 hours. The outer anti-aging sealing layer (8) can be constructed after the initial setting for ≥12 hours. The overall curing period is ≥72 hours. During the curing period, avoid pipe vibration, external force collision and water immersion.