An apparatus and method for drying lithium battery pole pieces
By switching drying units with different energy transfer mechanisms in stages, the problem of changes in the dominant heat and mass transfer mechanisms during the drying process of lithium battery electrodes was solved, achieving rapid heating, rapid dehumidification, and deep solvent removal, thereby improving the quality and production efficiency of electrode drying.
Patent Information
- Application Number
- CN202611550512.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-08
- Publication Date
- 2026-11-24
AI Technical Summary
Existing technologies are unable to adapt to the changes in the dominant heat and mass transfer mechanisms during the drying process of lithium battery electrodes, leading to problems such as electrode surface crusting, high internal stress in the coating, and solvent residue. Furthermore, they suffer from slow response, low measurement reliability, poor system reliability, and poor adaptability to operating conditions.
The adaptive height-adjustable working platform is used for leveling. By switching between different energy transfer mechanisms in stages, including infrared radiation heating, hot air convection drying, induction heating and low temperature hot air units, the drying mechanism is dynamically adjusted according to the electrode drying state parameters to achieve rapid heating, rapid dehumidification and deep solvent removal.
It effectively alleviates problems such as surface crusting of electrode sheets, high internal stress of coating, and solvent residue, improves electrode drying quality and production efficiency, and meets the needs of high-speed coating production of lithium battery electrodes.
Smart Images

Figure CN123154606A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of lithium-ion battery electrode manufacturing technology, specifically relating to an apparatus and method for drying lithium battery electrodes. Background Technology
[0002] After coating, lithium-ion battery electrodes require drying to remove the solvent from the coating. Currently, industrial production primarily uses hot air convection drying, where hot air provides heat to the electrode and promotes solvent evaporation by reducing the solvent vapor concentration near the electrode surface. With the increasing demand for high-speed electrode coating and low-temperature rapid drying, simply increasing the hot air temperature or velocity can easily cause rapid solvent loss from the electrode surface, while the solvent inside the electrode has not yet migrated to the surface in time, resulting in a large temperature and solvent concentration gradient. Infrared drying can rapidly input radiant energy into the electrode, thus increasing the electrode heating rate. However, when infrared drying is used alone, a solvent-rich layer may form on the electrode surface, thus limiting solvent migration to the vapor phase.
[0003] Existing technologies have disclosed infrared and hot air combined drying techniques. For example, CN120576554A discloses a battery electrode infrared and hot air combined drying system and method, which uses an infrared drying device and a hot air drying device to dry the electrode together, and adjusts parameters such as hot air temperature, flow rate, and infrared power. CN121576775A discloses a method for dynamically controlling infrared heating power, hot air temperature, and hot air velocity based on an ideal drying process model and real-time electrode characteristic parameters. In addition, CN105149186A discloses an electrode drying method that uses a medium-frequency or high-frequency induction heating coil to heat the metal foil itself, and uses low-temperature or room-temperature circulating air to remove volatile solvents. Essentially, this method utilizes the self-heating of the current collector to achieve drying from the inside out. However, the above technologies mainly focus on the combined use of different drying methods or the dynamic adjustment of drying parameters. During the electrode drying process, as the coating solvent content decreases, the main factors limiting the drying rate change. In the initial stage of drying, the main challenge is how to quickly impart sufficient heat to the electrode. In the middle stage, the main challenge shifts to how to promptly remove the high concentration of solvent vapor near the electrode surface. In the later stage, the main challenge is how to allow residual solvent inside the coating to continue migrating to the surface while avoiding continuous high-intensity heating of the electrode surface. If the same drying method is used throughout the entire drying process or only the same set of drying parameters is continuously adjusted, it is difficult to fully adapt to the changes in the dominant heat and mass transfer mechanisms during electrode drying.
[0004] Therefore, there is an urgent need for a composite drying method that can dynamically switch the dominant drying mechanism according to the electrode drying state, so as to adapt to the heat and mass transfer law of the entire electrode drying process, alleviate problems such as surface crusting, high internal stress of coating, and high solvent residue, and meet the use requirements of high-speed coating production of lithium battery electrodes. Summary of the Invention
[0005] The purpose of this invention is to provide a leveling method for an adaptive height-adjustable working platform to solve the technical problems existing in the prior art, such as response lag, low measurement reliability, poor system reliability, and poor adaptability to working conditions.
[0006] To achieve the purpose of the invention, the present invention provides a staged composite drying device for lithium battery electrodes, including a conveying mechanism, at least one drying area arranged along the conveying direction of the battery electrodes, a drying unit arranged in the drying area, a detection unit for detecting the drying state parameters of the electrodes, and a control unit electrically connected to the drying unit and the detection unit. When there is only one drying area, at least two different energy transfer mechanisms are installed within the drying area. When there are two or more drying zones, each drying zone is equipped with a drying unit with a different energy transfer mechanism; The drying unit with different energy transfer mechanisms includes at least two of the following: infrared radiation heating unit, hot air convection drying unit, induction heating unit, and low-temperature hot air unit.
[0007] Preferably, when there are two or more drying areas, a first drying area, a second drying area and a third drying area are arranged sequentially along the battery electrode conveying direction. The first drying area is provided with an infrared radiation heating unit, the second drying area is provided with a hot air convection drying unit, and the third drying area is provided with an induction heating unit and a low-temperature hot air unit.
[0008] Preferably, when there is only one drying area, a fourth drying area is provided along the battery electrode conveying direction. The fourth drying area is not physically divided, and an infrared radiation heating unit and a hot air convection drying unit are arranged therein.
[0009] Preferably, when there is only one drying area, a fifth drying area is provided along the battery electrode conveying direction, wherein infrared radiation heating units and hot air convection drying units are alternately arranged in the fifth drying area.
[0010] The present invention also provides a method for staged composite drying of lithium battery electrodes using the above-mentioned drying equipment, comprising the following steps: S1. The conveying mechanism continuously conveys the lithium battery electrode sheet coated with electrode slurry along the conveying direction, and the detection unit acquires at least one drying state parameter of the lithium battery electrode sheet during the drying process. S2. Determine the drying stage: The control unit determines the drying stage of the lithium battery electrode based on the drying state parameters, and determines whether the lithium battery electrode should be transported to the next drying area. When the battery electrode to be transported is to be transported to the next drying area, the control unit controls the conveying mechanism to complete the transport of the lithium battery electrode. S3. Output the dried battery electrode. When the residual solvent in the lithium battery electrode reaches the target content, the dried battery electrode is output. Preferably, the drying stage includes a first drying stage, a second drying stage, and an nth drying stage, where n is an integer greater than or equal to 2, and adjacent drying stages have different dominant drying mechanisms.
[0011] Preferably, in step S2, the drying state parameters include at least one of the following: electrode surface temperature, electrode current collector side temperature, electrode temperature change rate, electrode mass change, mass loss per unit time, drying rate per unit area, electrode surface solvent concentration, oven gas solvent concentration, and electrode thickness direction temperature difference.
[0012] The drying state parameters of this invention are used to characterize the degree of drying and the drying environment during the electrode drying process. For example, the oven gas solvent concentration reflects the level of gaseous solvent in the drying chamber and determines the driving force of solvent mass transfer. The oven gas solvent concentration mentioned in this invention refers to the gaseous solvent concentration in the current drying area (corresponding to a drying stage of the oven chamber segment). This can be either the average concentration of the entire drying area or the local gas solvent concentration measured at a point near the electrode within the drying area. The electrode surface solvent concentration reflects the solvent retention on the electrode coating surface. Other drying state parameters can also characterize the current degree of drying of the electrode.
[0013] It should be noted that the solvent concentration in the oven gas of this invention can be detected online by an infrared gas sensor built into the oven, or by gas chromatography analysis of extracted oven gas samples, which are conventional monitoring methods in the field of lithium battery drying. The solvent concentration on the electrode surface can be detected online non-destructively using near-infrared spectroscopy (NIR); alternatively, samples can be taken at the drying station, and after peeling off the electrode surface coating, the surface solvent concentration can be tested using thermogravimetric analysis or Karl Fischer method. Other drying state parameters are also obtained using techniques commonly found in this field.
[0014] Preferably, the drying state parameter in step S2 is the drying rate per unit area, wherein the formula for calculating the drying rate per unit area is as follows: ; among which, J m (t) represents the drying rate per unit area at time t, A c Let m(t) be the actual area of the coating, and m(t) be the electrode mass at time t.
[0015] The electrode drying stage is determined based on the relationship between the drying rate per unit area and a preset threshold: when J m When (t) is greater than J1, the battery electrode is determined to be in the first drying stage; When J mWhen (t) is less than or equal to J1 and greater than J2, the battery electrode is determined to be in the second drying stage, which is the rapid dehumidification stage. When J m When (t) is less than or equal to J2, the electrode is determined to be in the third drying stage; the third drying stage is the deep desolventizing stage electrode; where J1 is greater than J2, and both J1 and J2 are preset drying rate thresholds greater than zero.
[0016] Preferably, when the electrode enters the third drying zone, the drying state parameters also need to be measured for the temperature difference in the thickness direction. The formula for calculating the temperature difference in the thickness direction is: ΔT = T i -T s , among which, T s Electrode coating surface temperature, T i This refers to the temperature inside the electrode or on the current collector side.
[0017] Compared with the prior art, the present invention has the following beneficial effects: The method provided by this invention divides the entire drying process into multiple stages based on the electrode drying state, with different dominant drying mechanisms employed in each stage. The first drying stage focuses on rapidly heating the electrode by inputting heat; the second drying stage enhances mass transfer to promptly remove solvent vapor from the electrode surface; and the third drying stage promotes the migration of residual solvent from the coating interior. By switching the dominant drying mechanism in stages, this invention sequentially achieves the drying goals of rapid heating, rapid dehumidification, and deep solvent removal, adapting to the heat and mass transfer patterns throughout the electrode drying process. This effectively alleviates problems such as electrode surface crusting, high internal stress in the coating, and high solvent residue, meeting the requirements of high-speed coating production of lithium battery electrodes and improving electrode drying quality and production efficiency. Attached Figure Description
[0018] Figure 1 This is a schematic diagram of the overall structure of the lithium battery electrode composite drying equipment of the present invention.
[0019] Figure 2 This is a flowchart of the composite drying method based on the switching of the dominant mechanism in the drying stage according to the present invention.
[0020] Figure 3 This is a schematic diagram of the drying stage determination logic of the present invention.
[0021] Figure 4 This is a schematic diagram illustrating the principle of temperature difference along the thickness direction of the electrode sheet in this invention.
[0022] Among them, 10-electrode, 20-first drying area, 21-infrared radiation heating unit, 30-second drying area, 31-hot air convection drying unit, 40-third drying area, 41-induction heating unit, 42-low temperature hot air unit, 50-detection unit, 60-control unit; 71-coating, 72-current collector. Detailed Implementation
[0023] To further illustrate the technical means and effects adopted by the present invention in order to achieve the intended purpose, the following detailed description of the specific implementation methods, structures, features and effects of the present invention is provided in conjunction with the accompanying drawings and preferred embodiments.
[0024] Example 1
[0025] like Figure 1 As shown, this embodiment provides a staged composite drying device for lithium battery electrodes, including a conveying mechanism (not shown) for carrying and conveying lithium battery electrodes 10 coated with electrode slurry, three drying zones arranged sequentially along the conveying direction of the battery electrodes, drying units with different energy transfer mechanisms respectively arranged in the three drying zones, a detection unit 50 for detecting the drying state parameters of the electrodes, and a control unit 60 electrically connected to the drying units and the detection unit 50. The drying unit includes an infrared radiation heating unit 21, a hot air convection drying unit 31, an induction heating unit 41, and a low-temperature hot air unit 42.
[0026] Specifically, the three drying zones include a first drying zone 20, a second drying zone 30, and a third drying zone 40 arranged sequentially. The first drying zone 20 is equipped with an infrared radiation heating unit 21 for radiation-dominated drying; the second drying zone 30 is equipped with a hot air convection drying unit 31 for convection-dominated drying; and the third drying zone 40 is equipped with an induction heating unit 41 and a low-temperature hot air unit 42 for removing residual solvents. Each drying unit is electrically connected to a control unit 60 via a signal cable. The control unit 60 adjusts the start / stop and power of the drying units in real time based on drying status parameters fed back by the detection unit 50, thereby switching the dominant drying mechanism for different drying stages.
[0027] The detection unit 50 in this embodiment includes an infrared temperature sensor, a contact thermocouple, an online weighing module, and a solvent concentration sensor. The infrared temperature sensor is positioned above the battery electrode and is used for non-contact measurement of the surface temperature T of the electrode coating. s The contact thermocouple is installed on the current collector side of the back of the battery electrode to measure the current collector side temperature T. i The online weighing module is located between the conveyor rollers to measure the change in electrode mass in real time; the solvent concentration sensor is located at the air outlet of the drying area to detect the concentration of gaseous solvent in the third drying area 40.
[0028] Example 2
[0029] This embodiment is basically the same as Embodiment 1, except that there is only one drying area in this embodiment. A fourth drying area is set along the battery electrode conveying direction. The fourth drying area is not physically divided, and an infrared radiation heating unit 21 and a hot air convection drying unit 31 are arranged therein. According to the real-time detected drying status parameters, the power ratio of infrared and hot air is dynamically adjusted to realize the switching of the dominant drying mechanism over time within the same drying area.
[0030] Example 3
[0031] This embodiment is basically the same as Embodiment 1. The difference is that in this embodiment, there is one drying area. A fifth drying area is set along the battery electrode conveying direction. The fifth drying area alternately arranges infrared radiation heating unit 21 and hot air convection drying unit 31 to realize a cyclical alternating drying mode of heating-dehumidification-reheating-redehumidification.
[0032] Additionally, it should be noted that the heating unit in the drying area of the present invention can be any type of heating unit, that is: the heating unit in the drying area can be at least two of the following heating units: infrared radiation heating unit 21, hot air convection drying unit 31, induction heating unit 41, and low temperature hot air unit 42.
[0033] Example 4
[0034] This embodiment uses the equipment from Embodiment 1 to implement the staged composite drying method for lithium battery electrodes, referring to... Figure 2 This includes the following steps: S1. Continuously conveying the electrode sheet and acquiring drying state parameters, the conveying mechanism continuously conveys the lithium battery electrode sheet coated with electrode slurry along the conveying direction, and the detection unit 50 acquires at least one drying state parameter of the lithium battery electrode sheet 10 during the drying process. S2. Determine the drying stage. The control unit 60 determines the drying stage of the lithium battery electrode sheet based on the drying state parameters, and determines whether the lithium battery electrode sheet should be conveyed to the next drying area. When the battery electrode sheet to be conveyed is to be conveyed to the next drying area, the control unit controls the conveying mechanism to complete the conveying of the lithium battery electrode sheet. In this embodiment, one drying area corresponds to one drying stage. The drying stages include a first drying stage, a second drying stage, and an nth drying stage, where n is an integer greater than or equal to 2. Adjacent drying stages have different dominant drying mechanisms. The dominant drying mechanism includes at least one of an energy input mechanism and a solvent mass transfer mechanism. In this embodiment, n is 3. The first drying region 20, the second drying region 30 and the third drying region 30 in embodiment 1 correspond to the first drying stage, the second drying stage and the third drying stage, respectively.
[0035] S3. Output the dried battery electrode. When the residual solvent in the lithium battery electrode reaches the target content, the dried battery electrode is output.
[0036] Specifically, in step S2, the drying state parameters include at least one of the following: electrode surface temperature, electrode current collector side temperature, electrode temperature change rate, electrode mass change, mass loss per unit time, drying rate per unit area, electrode surface solvent concentration, oven gas solvent concentration, and electrode thickness direction temperature difference.
[0037] In this embodiment, the drying state parameter in step S2 is the drying rate per unit area, and the formula for calculating the drying rate per unit area is as follows: ; among which, J m (t) represents the drying rate per unit area at time t, A c Let m(t) be the actual area of the coating, and m(t) be the electrode mass at time t.
[0038] Of course, under continuous production conditions, the drying rate per unit area can also be calculated using the mass difference between adjacent electrode positions, and the specific formula is as follows: Where Δm is the mass loss within the time interval Δt, and Δt is the time taken for the electrode to pass through two detection positions.
[0039] Specifically, in this embodiment, such as Figure 3 As shown, the electrode drying stage is determined based on the relationship between the drying rate per unit area and a preset threshold: when J m When (t) is greater than J1, the battery electrode is determined to be in the first drying stage. The first drying stage is a rapid heating stage. At this time, the solvent content of the electrode is high. The battery electrode in the first drying area 20 uses the infrared radiation heating unit 21 as the main energy input (radiation drying is the main energy input method). The hot air adopts low intensity, and the goal is to quickly increase the overall temperature of the electrode.
[0040] When J m When (t) is less than or equal to J1 and greater than J2, the electrode is determined to be in the second drying stage. The second drying stage is the rapid dehumidification stage. At this time, the electrode enters the second drying area 30, reducing the proportion of radiation heating and improving the mass transfer effect of the hot air convection drying unit 31, thus completing the switch from energy input-dominated to mass transfer removal solvent vapor-dominated.
[0041] When J m When (t) is less than or equal to J2, the electrode is determined to be in the third drying stage; the third drying stage is the deep solvent removal stage electrode, at which time the electrode enters the third drying region 40, reducing the radiation heating on the coating side; where J1 is greater than J2, and both J1 and J2 are preset drying rate thresholds greater than zero.
[0042] It should be noted that J1 and J2 in this invention are preset drying rate thresholds used to distinguish different dominant drying mechanism stages, and are not fixed constants. These thresholds need to be calibrated through pre-experiments based on process conditions such as electrode slurry formulation and coating thickness: by monitoring the drying rate per unit area during the drying process, the critical point corresponding to the change in drying mechanism is found, thereby determining J1 and J2. Those skilled in the art can obtain suitable J1 and J2 for different electrode products through conventional experiments, which will not be elaborated here.
[0043] Specifically, when the electrode enters the third drying zone 40, the drying status parameters also need to be measured for the temperature difference in the thickness direction, such as... Figure 4 As shown, the formula for calculating the temperature difference in the thickness direction is: ΔT = T i -T s , among which, T s The electrode coating surface temperature, the temperature inside the electrode or on the current collector side, in this embodiment, is the current collector side temperature T. i The thermal state in the electrode thickness direction is determined based on ΔT. Specifically, when the absolute value of ΔT is greater than the preset threshold ΔT1, it indicates a large temperature gradient between the electrode's interior and surface. In this case, the drying strategy needs to be adjusted to reduce the radiative heating intensity on the electrode coating side and increase the heat input on the current collector side or maintain low-temperature convection drying. The heat input on the current collector side uses induction heating to generate heat in the electrode metal current collector, which then transfers heat to the coating. Specifically, the induction heating unit 41 is activated, in conjunction with the low-temperature hot air unit 42, to drive the solvent inside the coating 71 to migrate outwards until the electrode reaches the target residual solvent content. The radiative heating intensity on the electrode coating side is reduced, and the heat input on the current collector side is increased or low-temperature convection drying is maintained. The heat input on the current collector side uses induction heating to generate heat in the electrode metal current collector, which then transfers heat to the coating.
[0044] Specifically, in step S2, the electrode conveying speed v and the stage time t required for each drying stage are determined according to the electrode conveying speed v and the stage time t required for each drying stage. i Determine the length L along the electrode conveying direction of the corresponding drying stage. i The calculation formula is as follows: L i =v·t i , where L i Let v be the length of the i-th drying stage, v be the electrode running speed, and t be the length of the i-th drying stage. i This represents the time required for the i-th drying stage.
[0045] Among them, the electrode conveying speed v is the operating linear speed of the electrode conveying on the production line, which can be set according to the actual production capacity requirements; the stage time t iIt is the residence time required for the electrode to complete the current stage of drying and switch to the dominant drying mechanism, which is obtained through drying kinetics calculation and pre-experiment calibration.
[0046] Formula L i =v·t i This is used to calculate the length Li of the drying region corresponding to each drying stage, ensuring that the residence time of the electrode in the corresponding drying section meets the requirement t. i This allows the electrode to complete the drying process in this area before moving on to the next drying area, thus achieving staged drying.
[0047] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the claimed invention. The scope of protection claimed by the appended claims and their equivalents is defined.
Claims
1. A staged composite drying device for lithium battery electrodes, comprising a conveying mechanism, characterized in that, It also includes at least one drying area arranged along the battery electrode conveying direction, a drying unit arranged in the drying area, a detection unit for detecting electrode drying state parameters, and a control unit electrically connected to the drying unit and the detection unit; When there is only one drying area, at least two different energy transfer mechanisms are installed within the drying area. When there are two or more drying zones, each drying zone is equipped with a drying unit with a different energy transfer mechanism; The drying unit with different energy transfer mechanisms includes at least two of the following: infrared radiation heating unit, hot air convection drying unit, induction heating unit, and low-temperature hot air unit.
2. The drying equipment according to claim 1, characterized in that, When there are two or more drying areas, a first drying area, a second drying area, and a third drying area are set up sequentially along the battery electrode conveying direction. An infrared radiation heating unit is set on the first drying area, a hot air convection drying unit is set above the second drying area, and an induction heating unit and a low-temperature hot air unit are set above the third drying area.
3. The drying equipment according to claim 1, characterized in that, When there is one drying area, a fourth drying area is set along the battery electrode conveying direction. The four drying areas are not physically divided, and infrared radiation heating units and hot air convection drying units are arranged at the same time.
4. The drying equipment according to claim 1, characterized in that, When there is one drying area, a fifth drying area is provided along the battery electrode conveying direction. The fifth drying area alternately arranges infrared radiation heating units and hot air convection drying units.
5. A staged composite drying method for lithium battery electrodes, characterized in that, Includes the following steps: S1. Continuously conveying the electrode sheet and acquiring drying state parameters: The conveying mechanism continuously conveys the lithium battery electrode sheet coated with electrode slurry along the conveying direction, and the detection unit acquires at least one drying state parameter of the lithium battery electrode sheet during the drying process. S2. Determine the drying stage: The control unit determines the drying stage of the lithium battery electrode based on the drying state parameters, and determines whether the lithium battery electrode should be transported to the next drying area. When the battery electrode to be transported is to be transported to the next drying area, the control unit controls the conveying mechanism to complete the transport of the lithium battery electrode. S3. Determine the drying stage. When the residual solvent in the lithium battery electrode reaches the target content, output the dried battery electrode.
6. The staged composite drying method for lithium battery electrodes according to claim 5, characterized in that, The drying stages include a first drying stage, a second drying stage, and an nth drying stage, where n is an integer greater than or equal to 2, and adjacent drying stages have different dominant drying mechanisms.
7. The staged composite drying method for lithium battery electrodes according to claim 5, characterized in that, In step S2, the drying state parameters include at least one of the following: electrode surface temperature, electrode current collector side temperature, electrode temperature change rate, electrode mass change, mass loss per unit time, drying rate per unit area, electrode surface solvent concentration, oven gas solvent concentration, and electrode thickness direction temperature difference.
8. The staged composite drying method for lithium battery electrodes according to claim 7, characterized in that, The drying state parameter in step S2 is the drying rate per unit area, and the formula for calculating the drying rate per unit area is as follows: ; among which, J m (t) represents the drying rate per unit area at time t, A c Let m(t) be the actual area of the coating, and m(t) be the electrode mass at time t. The electrode drying stage is determined based on the relationship between the drying rate per unit area and a preset threshold: when J m When (t) is greater than J1, the battery electrode is determined to be in the first drying stage; When J m When (t) is less than or equal to J1 and greater than J2, the electrode is determined to be in the second drying stage, which is the rapid dehumidification stage. When J m When (t) is less than or equal to J2, the electrode is determined to be in the third drying stage; the third drying stage is the deep desolventizing stage electrode; where J1 is greater than J2, and both J1 and J2 are preset drying rate thresholds greater than zero.
9. The staged composite drying method for lithium battery electrodes according to claim 7, characterized in that, When the electrode enters the third drying zone, the drying status parameters also need to be measured for the temperature difference in the thickness direction. The formula for calculating the temperature difference in the thickness direction is: ΔT = T i -T s , among which, T s Electrode coating surface temperature, T i This refers to the temperature inside the electrode or on the current collector side.
Citation Information
Patent Citations
Drying method and drying device for pole pieces in pole piece plating process of lithium battery
CN105149186A
Infrared and hot air combined drying system and method for battery pole piece
CN120576554A
Dynamic control method and system of battery pole piece infrared-hot air combined drying equipment