Multistage electromagnetic stirring vacuum melting homogenization device and process
By combining a multi-stage electromagnetic stirring vacuum melting device with a segmented variable diameter casting pipe, the problems of insufficient electromagnetic field penetration and low grain refinement efficiency in the existing technology are solved, realizing the full homogenization of the alloy liquid and the low segregation ingot forming.
Patent Information
- Application Number
- CN202611654925.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-26
- Publication Date
- 2026-11-24
AI Technical Summary
Existing external low-frequency electromagnetic stirring technology suffers from insufficient electromagnetic field penetration, poor grain refinement and compositional segregation control, and high energy consumption in the production of ultra-large ingots due to the electromagnetic shielding effect of the heavy crucible and copper crystallizer.
A multi-stage electromagnetic stirring vacuum melting device is adopted, including a multi-stage electromagnetic stirring unit and a segmented variable diameter casting pipe. Combined with ultrasonic vibration, the multi-stage electromagnetic stirring components apply a variable frequency/variable amplitude electromagnetic field at each stage of melting, refining, casting and solidification to form a multi-dimensional flow field. In conjunction with ultrasonic vibration, the homogenization of the alloy liquid is achieved throughout the process.
It significantly reduces the macrosegregation index of the alloy, improves crystallization quality and compositional uniformity, reduces energy consumption, and solves the problems of insufficient electromagnetic field penetration and low grain refinement efficiency in existing technologies.
Smart Images

Figure CN123154633A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of metal casting technology, and in particular to a multi-stage electromagnetic stirring vacuum melting homogenization device and process. Background Technology
[0002] Vacuum melting furnaces are key equipment in metal casting. In the metal alloy melting process within vacuum melting furnaces, multiple metallic elements are typically added to the melt to improve the performance of the finished alloy. These added alloying elements must be uniformly dispersed through thorough electromagnetic stirring to avoid compositional segregation. Therefore, the industry's process objective is to apply variable frequency / amplitude electromagnetic fields during the four stages of melting, refining, casting, and directional solidification. This forces melt convection to break up the dendritic framework, resulting in a macroscopic segregation index of 0.15 to 0.11 for the alloy.
[0003] Current electromagnetic stirring technologies generally employ low-frequency electromagnetic pulse schemes, based on the Lorentz force driving oscillations in the molten metal: an excitation coil is placed on the outside of the crucible or crystallizer, and a low-frequency pulse current is passed into the coil to generate a strong instantaneous magnetic field. This generates a reciprocating Lorentz force within the conductive molten metal, driving the melt to form a global circulating oscillation, thereby achieving dendrite breakage and grain refinement, shifting the grain growth mode towards uniform equiaxed crystal growth. However, existing technologies have significant limitations: on the one hand, the crucible needs to withstand the corrosion of active metals during the smelting process, resulting in a heavy structure; on the other hand, the industry-standard structure of the crystallizer is made of copper with a water-cooling structure, and copper is a material with excellent electromagnetic shielding properties. These structural characteristics lead to low crystal refinement efficiency and high energy consumption in the production of ultra-large ingots, making it difficult to achieve ideal process results with current electromagnetic stirring technologies. Summary of the Invention
[0004] To address the aforementioned problems, the present invention aims to provide a multi-stage electromagnetic stirring vacuum melting homogenization device and process, thereby solving the technical problems of insufficient electromagnetic field penetration, poor grain refinement and compositional segregation control, and high energy consumption in the production of ultra-large ingots due to the electromagnetic shielding effect of the existing external low-frequency electromagnetic stirring technology caused by the heavy crucible and copper crystallizer.
[0005] To achieve the above objectives, the present invention adopts the following technical solution:
[0006] The present invention provides a multi-stage electromagnetic stirring vacuum melting homogenization device, comprising a multi-stage electromagnetic stirring unit and a melting crucible group, a refining crucible, a casting system and a forming module connected in sequence for feeding materials; the melting crucible group is used for vacuum melting of metal and supplying liquid to the refining crucible, and the refining crucible is used for refining the melt and supplying liquid to the forming module through the casting system.
[0007] The forming module includes a support turntable and a crystallizer and a solidification casting mold arranged sequentially from bottom to top on the support turntable; the support turntable is used for overall support and rotation, the crystallizer is used for directional solidification of the alloy liquid, and the solidification casting mold is used for casting and forming of the alloy liquid.
[0008] The multi-stage electromagnetic stirring unit includes one to four stages of electromagnetic stirring components respectively corresponding to the melting crucible group, refining crucible, gating system and solidification casting mold, so as to apply electromagnetic stirring to the alloy liquid at each stage of melting, refining, casting and solidification, so as to achieve homogenization of the alloy liquid throughout the process and complete the low segregation ingot forming.
[0009] The casting system includes a segmented variable diameter casting pipe. The large diameter section of the casting pipe is equipped with a three-stage electromagnetic stirring assembly. The three-stage electromagnetic stirring assembly is used to make the flowing alloy liquid form a circumferential rotating metal flow field, and the circumferential rotating metal flow fields generated by two adjacent three-stage electromagnetic stirring assemblies are in opposite directions.
[0010] The three-stage electromagnetic stirring assembly includes two sets of spiral coils arranged in parallel on both sides inside the large-diameter section. The magnetic field generated by the two sets of spiral coils causes the alloy liquid to form a circumferential rotating metal flow field.
[0011] The solidification casting mold includes an inner ring and an outer ring arranged coaxially, and an annular solidification cavity is formed between the inner ring and the outer ring; the four-stage electromagnetic stirring assembly is disposed in the annular solidification cavity.
[0012] The smelting crucible group includes a first smelting crucible and a second smelting crucible; the first smelting crucible and the second smelting crucible alternately replenish the refining crucible with molten alloy.
[0013] The first melting crucible, the second melting crucible, and the refining crucible have the same structure, each including a crucible body and a plug; the bottom of the crucible body is provided with a discharge port, and the plug is used to block or open the discharge port at the bottom of the crucible body.
[0014] The primary, secondary, and quaternary electromagnetic stirring assemblies have identical structures, each including an electromagnetic stirring coil, an ultrasonic transducer, and a six-degree-of-freedom vacuum manipulator end flange. The six-degree-of-freedom vacuum manipulator end flange is located at the execution end of the six-degree-of-freedom vacuum manipulator. The ultrasonic transducer and the electromagnetic stirring coil are sequentially connected to the six-degree-of-freedom vacuum manipulator end flange. The electromagnetic stirring coil is a vortex-shaped coil arranged inside the alloy liquid. The electromagnetic stirring coil and the ultrasonic transducer work together to apply electromagnetic stirring and ultrasonic vibration.
[0015] The electromagnetic stirring coil is a hollow spiral structure made of yttrium-stabilized zirconia ceramic pipe. The liquid metal inside the yttrium-stabilized zirconia ceramic pipe is interconnected with the heat exchange circulation system and the low-frequency electromagnetic pulse power supply; the liquid metal is a gallium-based liquid alloy.
[0016] An ultrasonic echo sensor is installed on the solidification casting mold. The ultrasonic echo sensor is used to provide online feedback on the distance between the electromagnetic stirring coil and the solid-liquid mixing interface inside the solidification casting mold.
[0017] Another aspect of the present invention provides a multi-stage electromagnetic stirring vacuum melting homogenization process, which is implemented using the multi-stage electromagnetic stirring vacuum melting homogenization device described above. The process includes the following steps:
[0018] S1. The melting crucible group alternately melts metal and supplies molten metal alloy to the refining crucible. The primary electromagnetic stirring component simultaneously performs primary electromagnetic stirring and ultrasonic vibration on the molten metal.
[0019] S2. Add alloy blocks for composition adjustment into the refining crucible according to the process sequence. The secondary electromagnetic stirring assembly simultaneously performs secondary electromagnetic stirring and ultrasonic vibration on the melt and monitors the dissolution of the alloy blocks.
[0020] S3. When the alloy liquid flows through the casting system, the two adjacent three-stage electromagnetic stirring components in the casting tube generate circumferential rotating metal flow fields with opposite directions. The alloy liquid forms a twisted composite flow field in the casting tube, which breaks up crystal dendrites and reduces the segregation of melt elements.
[0021] S4. The alloy liquid enters the solidification casting mold for bottom-up directional solidification. The four-stage electromagnetic stirring assembly applies electromagnetic stirring and ultrasonic vibration to the solid-liquid mixed phase interface area. Through the synergistic effect of multi-stage electromagnetic stirring, a homogeneous ingot is obtained.
[0022] The advantages and positive effects of this invention are as follows:
[0023] 1. Variable diameter flow channel self-stirring, assisting in crystal breaking and reducing segregation: The casting pipe adopts a segmented variable diameter structure. The diameter of the second and fourth sections of the casting pipe is larger than that of the other sections. By changing the axial flow velocity of the melt, the fluid self-stirring is achieved, which can directly break crystal dendrites and reduce component segregation.
[0024] 2. Variable frequency / amplitude magnetic field throughout the entire process, significantly reducing macroscopic segregation: Variable frequency / amplitude electromagnetic fields are applied throughout the four process stages of smelting, refining, casting, and directional solidification to force melt convection and break the dendritic skeleton. This can reduce the macroscopic segregation index of the alloy from the conventional 0.15 to below 0.03, significantly improving the uniformity of alloy composition and crystal quality.
[0025] 3. Built-in multi-degree-of-freedom stirring to eliminate flow dead zones: Equipped with one to four levels of multi-stage electromagnetic stirring components, it can apply ultrasonic vibration and local electromagnetic stirring jets deep into the metal melt; the device has six degrees of freedom in spatial position adjustment capability, which can accurately act on the target area, solving the defect of flow dead zones in existing external electromagnetic coils, and enhancing the dendrite breakage and segregation control effect.
[0026] 4. Multidimensional flow field enhances crystal fragmentation capability: The third-stage stirring component uses four electromagnetic stirring coils, which can form an electromagnetic stirring flow field in the shape of a "twisted rope", further enhancing the crystal dendrite fragmentation effect and improving the segregation suppression effect.
[0027] Other features and advantages of the invention will be set forth in the following description, and will be apparent in part from the description, or may be learned by practicing the invention. The objects and other advantages of the invention may be realized and obtained by means of the structures particularly pointed out in the written description and the accompanying drawings.
[0028] The technical solution of the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Attached Figure Description
[0029] The accompanying drawings are provided to further illustrate the invention and form part of the specification. They are used in conjunction with embodiments of the invention to explain the invention and do not constitute a limitation thereof. In the drawings:
[0030] Figure 1 This is an isometric view of a multi-stage electromagnetic stirring vacuum melting homogenization device according to the present invention;
[0031] Figure 2 for Figure 1 Enlarged view of a section at point D;
[0032] Figure 3 This is a side view of a multi-stage electromagnetic stirring vacuum melting homogenization device according to the present invention;
[0033] Figure 4 for Figure 3 AA section view;
[0034] Figure 5 This is a top view of a multi-stage electromagnetic stirring vacuum melting homogenization device according to the present invention;
[0035] Figure 6 for Figure 5 BB cross-sectional view;
[0036] Figure 7 for Figure 6 Enlarged view of a section at point C.
[0037] In the diagram: 1. First melting crucible; 101. Crucible body; 102. Insert plug; 103. First-stage electromagnetic stirring coil; 104. End flange of the six-degree-of-freedom vacuum manipulator; 2. Second melting crucible; 3. Refining crucible; 4. Casting system; 401. First section of casting pipe; 402. Second section of casting pipe; 403. Third section of casting pipe; 404. Fourth section of casting pipe; 405. Fifth section of casting pipe; 406. First spiral coil; 407. Second spiral coil; 408. Third spiral coil; 409. Fourth spiral coil; 5. Solidification casting mold; 501. Outer ring; 502. Inner ring; 503. Fourth-stage electromagnetic stirring coil; 6. Crystallizer; 7. Support turntable. Detailed Implementation
[0038] In this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0039] The preferred embodiments of the present invention will be described below with reference to the accompanying drawings. It should be understood that the preferred embodiments described herein are for illustration and explanation only and are not intended to limit the present invention.
[0040] See Figures 1 to 7 As shown, one embodiment of the present invention provides a multi-stage electromagnetic stirring vacuum melting homogenization device, including a multi-stage electromagnetic stirring unit and a melting crucible group, a refining crucible 3, a casting system 4, and a forming module connected in sequence for feeding materials; the melting crucible group is used for vacuum melting of metal and feeding liquid to the refining crucible 3, the refining crucible 3 is used for refining the melt and feeding liquid to the forming module through the casting system 4; the forming module includes a support turntable 7, a crystallizer 6, and a solidification casting mold 5, the bottom of the support turntable 7 is fixed to the ground, the output end drives the crystallizer 6 to rotate, and the support turntable 7 has a built-in infinite rotation joint. The crystallizer 6 is used to supply multiple circulating cooling water and connect the sensor lines of each device; the solidification casting mold 5 is detachably installed above the crystallizer 6 and is driven to rotate synchronously by the support turntable 7 through the crystallizer 6 to complete the bottom-up directional solidification casting process; the multi-stage electromagnetic stirring unit includes one to four stages of electromagnetic stirring components respectively corresponding to the melting crucible group, refining crucible 3, gating system 4 and solidification casting mold 5, so as to apply electromagnetic stirring to the alloy liquid in each stage of melting, refining, casting and solidification to achieve full homogenization of the alloy liquid and complete the low segregation ingot forming.
[0041] See Figure 1As shown, in an embodiment of the present invention, the melting crucible group includes a first melting crucible 1 and a second melting crucible 2; the first melting crucible 1 and the second melting crucible 2 are used to melt metal alloy blocks to obtain liquid alloy, and alternately replenish the alloy liquid to the refining crucible 3. The refining crucible 3 adds the composition alloy block according to the process sequence. After the alloy block is placed on the bottom side wall of the crucible, the electromagnetic stirring assembly uses a melt jet formed by ultrasonic waves and an electromagnetic coil to directionally melt the alloy block; the refining crucible 3 is equipped with an ultrasonic echo detector to detect the degree of dissolution of the alloy block in real time.
[0042] See Figure 2 As shown, in an embodiment of the present invention, the first smelting crucible 1 includes a crucible body 101 and a plug 102; the bottom of the crucible body 101 is provided with a discharge port, and the plug 102 is used to block or open the discharge port at the bottom of the crucible body 101.
[0043] The second melting crucible 2 and the refining crucible 3 have the same structure as the first melting crucible 1. The first melting crucible 1 and the second melting crucible 2 work alternately, one melting metal and the other feeding molten metal alloy into the refining crucible 3; block metal materials are fed in through multi-stage gate valves, buffer vacuum chambers and vacuum manipulators to achieve melting or refining of alloying elements. This part is a mature existing vacuum melting technology and will not be described in detail.
[0044] Specifically, vacuum melting electromagnetic induction coils and coil water-cooling structures are installed on the outside of the first melting crucible 1, the second melting crucible 2, and the refining crucible 3. The coil water-cooling structure is used to maintain the temperature field of the vacuum melting electromagnetic induction coils. In addition to the function of vacuum casting and melting metal, the vacuum induction coils also have the function of low-frequency electromagnetic stirring.
[0045] See Figure 2 As shown, in an embodiment of the present invention, the primary electromagnetic stirring assembly includes a primary electromagnetic stirring coil 103, an ultrasonic transducer, and a six-degree-of-freedom vacuum manipulator end flange 104. The six-degree-of-freedom vacuum manipulator end flange 104 is disposed at the execution end of the six-degree-of-freedom vacuum manipulator. The ultrasonic transducer and the primary electromagnetic stirring coil 103 are sequentially connected to the six-degree-of-freedom vacuum manipulator end flange 104. The primary electromagnetic stirring coil 103 is a vortex-shaped coil, arranged inside the alloy liquid, and maintains a set process distance from the solid-liquid mixing interface. The primary electromagnetic stirring coil 103 and the ultrasonic transducer work together to apply electromagnetic stirring and ultrasonic vibration in the solid-liquid mixing interface region. Specifically, the secondary and quaternary electromagnetic stirring assemblies have the same structure as the primary electromagnetic stirring assembly.
[0046] Furthermore, each stage of the electromagnetic stirring coil is composed of yttrium-stabilized zirconia ceramic pipes. The liquid metal inside the yttrium-stabilized zirconia ceramic pipes is interconnected with the heat exchange circulation system and the low-frequency electromagnetic pulse power supply. The liquid metal is preferably MG3 type gallium-based liquid alloy conforming to the national standard GB / T39859-2021, with a thermal conductivity ≥25W / (m·K), a melting point of 16℃, and a boiling point of 2400℃, which is 1500℃~1650℃ higher than the high-temperature alloy melting temperature range.
[0047] A primary electromagnetic stirring coil 103, a secondary electromagnetic stirring coil, and a quaternary electromagnetic stirring coil 503 are arranged within the liquid metal region. The quaternary electromagnetic stirring coil 503 maintains a set process distance with the solid-liquid mixing interface, simultaneously implementing electromagnetic stirring and ultrasonic vibration. An ultrasonic echo sensor is installed on the solidification casting mold 5. The ultrasonic echo sensor is used for online feedback of the distance between the quaternary electromagnetic stirring coil 503 and the solid-liquid mixing interface. See [link to relevant documentation] Figure 6 As shown.
[0048] In an embodiment of the present invention, the casting system 4 includes a segmented variable diameter casting pipe. The large diameter section of the casting pipe is equipped with a three-stage electromagnetic stirring assembly. The three-stage electromagnetic stirring assembly is used to form a circumferential rotating metal flow field through the flowing alloy liquid. The circumferential rotating metal flow fields generated by two adjacent three-stage electromagnetic stirring assemblies are in opposite directions. The alloy liquid forms a twisted composite flow field in the casting pipe, which can effectively break the primary dendrites of the melt, enhance the mass transfer of elements inside the melt, inhibit the adsorption of metal elements on the wall of the casting pipe, and significantly reduce the segregation of elements in the ingot.
[0049] Specifically, the three-stage electromagnetic stirring assembly includes two sets of spiral coils arranged parallel to each other on both sides of the large-diameter section. The magnetic field generated by the two sets of spiral coils causes the molten alloy to form a circumferentially rotating metal flow field. Preferably, the spiral coils are constructed with yttrium oxide-stabilized zirconia ceramic pipes to form a hollow spiral structure, which is immersed in the molten metal alloy for operation. The liquid metal inside the spiral coils is connected to an external cooling heat exchange system and an electromagnetic power supply. The direction of the molten jet generated by the excitation of the spiral coils is spatially perpendicular to the axis of the casting pipe and does not intersect with it.
[0050] See Figures 3 to 7 As shown, in this embodiment, the casting pipe includes a first casting pipe 401, a second casting pipe 402, a third casting pipe 403, a fourth casting pipe 404, and a fifth casting pipe 405 arranged sequentially along the axial direction; wherein the upper end of the first casting pipe 401 is connected to the bottom outlet of the refining crucible 3; the outlet of the fifth casting pipe 405 is suspended above the opening of the solidification casting mold 5. The second casting pipe 402 and the fourth casting pipe 404 have the same diameter, which is larger than the diameter of the first casting pipe 401, the third casting pipe 403, and the fifth casting pipe 405; two sets of three-stage electromagnetic stirring components are respectively installed in the second casting pipe 402 and the fourth casting pipe 404.
[0051] Specifically, a first helical coil 406 and a second helical coil 407 are symmetrically arranged inside the second casting pipe 402, and a third helical coil 408 and a fourth helical coil 409 are symmetrically arranged inside the fourth casting pipe 404. The first helical coil 406 and the second helical coil 407 form a first circumferential stirring melt flow field inside the second casting pipe 402; the third helical coil 408 and the fourth helical coil 409 form a second axial stirring melt flow field with opposite directions of rotation inside the fourth casting pipe 404. The two opposing flow fields converge inside the third casting pipe 403, forming a twisted melt flow, breaking up dendrites and suppressing compositional segregation; sufficient melt flow can prevent alloying elements from adhering and accumulating on the inner wall of the casting pipe.
[0052] See Figure 6 As shown, in an embodiment of the present invention, the solidification casting mold 5 includes an inner ring 502 and an outer ring 501 arranged coaxially, and an annular solidification cavity is formed between the inner ring 502 and the outer ring 501; a four-stage electromagnetic stirring assembly is disposed in the annular solidification cavity.
[0053] Preferably, the crystallizer 6 is disc-shaped and made of copper-cobalt-beryllium alloy. It has an internal cooling cavity through which circulating cooling water is introduced to form a high thermal conductivity cold end, serving as a heat dissipation channel during the solidification process. The inner ring 502 and outer ring 501 of the solidification casting mold 5, the spiral coil, and the various stages of electromagnetic stirring coils are all made of yttrium-stabilized zirconia (YSZ) ceramic material, which can control the solidification thermal resistance.
[0054] An embodiment of the present invention provides a multi-stage electromagnetic stirring vacuum melting homogenization device. This device employs multi-stage electromagnetic stirring units to apply stirring action step-by-step along the flow path of the molten metal. This is combined with ultrasonic vibration to synergistically regulate the solid-liquid mixing interface. An ultrasonic echo sensor monitors the solid-liquid interface position online, and a rotating platform drives the mold to rotate, achieving bottom-up directional solidification. Through variable-diameter pouring pipes with variable flow rates for self-stirring, a full-process variable-frequency / variable-amplitude electromagnetic field, a six-degree-of-freedom adjustable built-in multi-stage electromagnetic stirring assembly, and a multi-coil twisted flow field, the device continuously breaks up primary grains, suppresses component segregation, and gradually homogenizes the molten metal. It precisely controls the solidification process, effectively improving the uniformity and density of the cast billet structure, reducing casting defects, and achieving high-quality alloy casting.
[0055] See Figures 1 to 7 As shown, another embodiment of the present invention provides a multi-stage electromagnetic stirring vacuum melting homogenization process, which is implemented using the multi-stage electromagnetic stirring vacuum melting homogenization device described above. The process includes the following steps:
[0056] S1, the first melting crucible 1 and the second melting crucible 2 work alternately, one melting metal and the other feeding molten metal alloy into the refining crucible 3; the primary electromagnetic stirring assembly simultaneously performs primary electromagnetic stirring and ultrasonic vibration on the molten metal;
[0057] S2. Add alloy blocks for composition adjustment into the refining crucible 3 according to the process sequence. The secondary electromagnetic stirring assembly simultaneously performs secondary electromagnetic stirring and ultrasonic vibration on the melt, and monitors the dissolution of the alloy blocks through an ultrasonic echo detector.
[0058] S3. When the alloy liquid flows through the casting system 4, the two adjacent three-stage electromagnetic stirring components generate circumferential rotating metal flow fields with opposite directions. The alloy liquid forms a twisted composite flow field in the casting tube, which breaks up the dendrites and reduces the segregation of melt elements.
[0059] S4. The alloy liquid enters the solidification casting mold 5 for bottom-up directional solidification. The four-stage electromagnetic stirring coil 503 maintains the set process spacing with the solid-liquid mixing interface, and electromagnetic stirring and ultrasonic vibration are implemented simultaneously. Through the synergistic effect of multi-stage electromagnetic stirring, a homogeneous ingot is obtained.
[0060] The melting and casting process of this invention applies electromagnetic stirring at each stage throughout the melting, refining, pouring, and solidification of the molten metal alloy. Ultrasonic vibration is coupled at the solid-liquid interface, and an ultrasonic echo sensor monitors the solid-liquid interface position online to maintain a stable process spacing. Combined with a rotating platform, bottom-up directional solidification is achieved. This process continuously breaks down dendrites, homogenizes the melt composition, effectively suppresses defects such as segregation and shrinkage cavities, refines the casting grains, precisely controls the solidification process, and stably obtains alloy castings with uniform microstructure, high density, and excellent mechanical properties. This invention is applicable to vacuum melting and solidification processes for high-temperature alloys, titanium alloys, precision and magnetic alloys, high-end special steels, ultra-high-strength structural steels, high-entropy alloys, refractory alloys, precious metals, and high-purity non-ferrous metals.
[0061] Obviously, those skilled in the art can make various modifications and variations to this invention without departing from its spirit and scope. Therefore, if these modifications and variations fall within the scope of the claims of this invention and their equivalents, this invention also intends to include these modifications and variations.
Claims
1. A multi-stage electromagnetic stirring vacuum melting homogenization device, characterized in that, It includes a multi-stage electromagnetic stirring unit and a smelting crucible group, a refining crucible (3), a casting system (4) and a forming module that are connected in sequence for feeding materials; the smelting crucible group is used for vacuum smelting of metal and supplying liquid to the refining crucible (3), and the refining crucible (3) is used for refining the melt and supplying liquid to the forming module through the casting system (4); The forming module includes a bearing turntable (7) and a crystallizer (6) and a solidification casting mold (5) arranged sequentially from bottom to top on the bearing turntable (7); the bearing turntable (7) is used for overall bearing rotation, the crystallizer (6) is used for directional solidification of the alloy liquid, and the solidification casting mold (5) is used for alloy liquid casting and forming. The multi-stage electromagnetic stirring unit includes first to fourth stage electromagnetic stirring components respectively arranged for the melting crucible group, refining crucible (3), casting system (4) and solidification casting mold (5) to apply electromagnetic stirring to the alloy liquid in each stage of melting, refining, casting and solidification, so as to achieve full homogenization of the alloy liquid and complete the low segregation ingot forming.
2. The multi-stage electromagnetic stirring vacuum melting homogenization device according to claim 1, characterized in that, The casting system (4) includes a segmented variable diameter casting pipe. The large diameter section of the casting pipe is equipped with a three-stage electromagnetic stirring assembly. The three-stage electromagnetic stirring assembly is used to make the flowing alloy liquid form a circumferential rotating metal flow field, and the circumferential rotating metal flow fields generated by two adjacent three-stage electromagnetic stirring assemblies are in opposite directions.
3. The multi-stage electromagnetic stirring vacuum melting homogenization device according to claim 2, characterized in that, The three-stage electromagnetic stirring assembly includes two sets of spiral coils arranged in parallel on both sides inside the large-diameter section. The magnetic field generated by the two sets of spiral coils causes the alloy liquid to form a circumferential rotating metal flow field.
4. The multi-stage electromagnetic stirring vacuum melting homogenization device according to claim 2, characterized in that, The solidification casting mold (5) includes an inner ring (502) and an outer ring (501) arranged coaxially, and an annular solidification cavity is formed between the inner ring (502) and the outer ring (501); the four-stage electromagnetic stirring assembly is arranged in the annular solidification cavity.
5. The multi-stage electromagnetic stirring vacuum melting homogenization device according to claim 2, characterized in that, The smelting crucible group includes a first smelting crucible (1) and a second smelting crucible (2); the first smelting crucible (1) and the second smelting crucible (2) alternately replenish the refining crucible (3) with alloy liquid.
6. The multi-stage electromagnetic stirring vacuum melting homogenization device according to claim 5, characterized in that, The first smelting crucible (1), the second smelting crucible (2), and the refining crucible (3) have the same structure, each including a crucible body (101) and a plug (102); the bottom of the crucible body (101) is provided with a discharge port, and the plug (102) is used to block or open the discharge port at the bottom of the crucible body (101).
7. The multi-stage electromagnetic stirring vacuum melting homogenization device according to claim 2, characterized in that, The first-stage, second-stage, and fourth-stage electromagnetic stirring components have the same structure, each including an electromagnetic stirring coil, an ultrasonic transducer, and a six-degree-of-freedom vacuum manipulator end flange (104). The six-degree-of-freedom vacuum manipulator end flange (104) is located at the execution end of the six-degree-of-freedom vacuum manipulator. The ultrasonic transducer and the electromagnetic stirring coil are connected to the six-degree-of-freedom vacuum manipulator end flange (104) in sequence. The electromagnetic stirring coil is a vortex-shaped coil arranged inside the alloy liquid. The electromagnetic stirring coil and the ultrasonic transducer work together to apply electromagnetic stirring and ultrasonic vibration.
8. The multi-stage electromagnetic stirring vacuum melting homogenization device according to claim 7, characterized in that, The electromagnetic stirring coil is a hollow spiral structure made of yttrium-stabilized zirconia ceramic pipe. The liquid metal inside the yttrium-stabilized zirconia ceramic pipe is interconnected with the heat exchange circulation system and the low-frequency electromagnetic pulse power supply; the liquid metal is a gallium-based liquid alloy.
9. The multi-stage electromagnetic stirring vacuum melting homogenization device according to claim 7, characterized in that, An ultrasonic echo sensor is provided on the solidification casting mold (5). The ultrasonic echo sensor is used to provide online feedback on the distance between the electromagnetic stirring coil and the solid-liquid mixing interface inside the solidification casting mold (5).
10. A multi-stage electromagnetic stirring vacuum melting homogenization process, characterized in that, The process is achieved using the multi-stage electromagnetic stirring vacuum melting homogenization apparatus described in any one of claims 2-9, and includes the following steps: S1. The melting crucible group alternately melts metal and supplies metal alloy liquid to the refining crucible (3). The primary electromagnetic stirring assembly simultaneously performs primary electromagnetic stirring and ultrasonic vibration on the molten metal. S2. Add alloy blocks for composition adjustment in the refining crucible (3) according to the process sequence. The secondary electromagnetic stirring assembly simultaneously performs secondary electromagnetic stirring and ultrasonic vibration on the melt and monitors the dissolution of the alloy blocks. S3. When the alloy liquid flows through the casting system (4), the two adjacent three-stage electromagnetic stirring components in the casting tube generate circumferential rotating metal flow fields with opposite directions. The alloy liquid forms a twisted composite flow field in the casting tube, which breaks up the dendrites and reduces the segregation of melt elements. S4. The alloy liquid enters the solidification casting mold (5) for directional solidification from bottom to top. The four-stage electromagnetic stirring assembly applies electromagnetic stirring and ultrasonic vibration to the solid-liquid mixed phase interface area. Through the synergistic effect of multi-stage electromagnetic stirring, a homogeneous ingot is obtained.