Preparation process of ultra-small volume composite bridge resistor and composite bridge resistor
The composite bridge resistor, fabricated using a multi-layer structure and high-vacuum hot-pressing process, solves the problems of large size, poor bonding quality, and insufficient shock resistance in existing technologies. It enables the production of miniaturized SMT packaging and high-reliability ignition components, and is suitable for digital electronic detonators and miniature fuses.
Patent Information
- Application Number
- CN202611429029.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-15
- Publication Date
- 2026-11-24
AI Technical Summary
Existing composite bridge resistor ignition elements suffer from problems such as large size, inability to be directly packaged by SMT, poor bonding quality between the energy layer and the transducer interface, lack of integrated dense composite process, and insufficient shock resistance, making it difficult to meet the stringent space and reliability requirements of miniature detonators and fuses.
The multi-layer structure, consisting of an FR-5 fiberglass substrate, a nickel-chromium alloy membrane bridge, an aluminothermic energy layer, a high-modulus inner sealing film, and a rigid cover plate, is prepared through calendering and high-vacuum hot pressing processes. Combined with screen printing and outer sealing film protection, a high-rigidity sandwich protective structure is formed.
It enables miniaturized SMT packaging of devices, improves ignition reliability and vibration resistance, ensures interlayer bonding strength and product consistency, adapts to the automated integration of digital electronic detonators and miniature fuses, and reduces production costs and safety risks.
Smart Images

Figure CN123154709A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the technical field of pyrotechnics and electronic components, and particularly relates to a process for preparing an ultra-small volume composite bridge resistor and the composite bridge resistor thereof. Background Technology
[0002] With the rapid development of digital electronic detonator technology and intelligent fuse technology, ignition transducer elements are gradually moving towards miniaturization, high reliability, and automated integration. Traditional bridge wire ignition elements are large in size, have poor parameter consistency, and cannot be directly surface-mounted (SMT). Although existing semiconductor bridge (SCB) chips have achieved miniaturization, they still have many technical shortcomings.
[0003] Existing related technologies are mainly classified into several categories, including energetic semiconductor bridges / composite thin-film semiconductor bridges, metal thin-film nickel-chromium bridges, and surface-mount bridge wire ignition elements.
[0004] CN112254586A discloses a composite energetic thin-film semiconductor bridge, which uses magnetron sputtering to deposit B / Ti energetic thin films. This method is expensive, has low production efficiency, and is a silicon-based semiconductor bridge, making it incompatible with standard SMT assembly lines. CN112923802A discloses a write-printed energetic semiconductor bridge transducer, where the energetic layer relies on physical adhesion with an adhesive. This layer is prone to delamination under high vibration environments, lacks a vacuum thermoforming densification process, and the product cannot achieve the 0805 micro-package size. CN104976925A uses a template method + calcination + magnetron sputtering to prepare the aluminothermic thin film. This process is complex and costly, the porous structure has poor shock resistance, and there is no standardized surface mount packaging.
[0005] CN105737681A is the closest to existing technology, disclosing the hot-pressing bonding of an FR-5 substrate with a nickel-chromium alloy foil to prepare a thin-film bridge region. However, only a bare bridge region semi-finished product is obtained, without an integrated active layer. The hot pressing only achieves bonding of the foil to the substrate, without vacuum densification of the active layer, and lacks a cover plate and external sealing protection structure, making it unsuitable for direct SMT mounting. CN102927590A discloses a nickel-chromium metal thin-film bridge igniter, which is only a pure resistive transducer element, without an integrated active layer. The overall device size is large, and there is no standard SMT package. CN103528445B's semiconductor bridge ignition assembly relies on bonding wire electrical connection and cannot be directly surface-mount soldered.
[0006] CN212362990U and CN215984216U are patch bridge wire type igniters. They are bridge wire encapsulated structures, which are large in size and do not have integrated energetic agents. They rely on encapsulated blocks for structural protection and are prone to aging and cracking under strong vibration and impact environments.
[0007] Based on existing technologies, composite bridge resistor-type ignition elements currently have the following drawbacks:
[0008] First, it is large in size and lacks standard SMT packaging, making it impossible to directly mount PCBs at high speed, which makes it difficult to meet the strict space constraints of miniature detonators and small fuses.
[0009] Second, the bonding quality between the energy layer and the transducer is poor, magnetron sputtering is costly, direct writing printing only involves physical bonding, manual coating has air bubbles and voids, and the layers are prone to delamination and peeling under vibration and impact conditions, resulting in insufficient ignition reliability.
[0010] Third, there is a lack of integrated and dense composite processes; existing hot pressing is only used for bonding substrates and metal foils, and high vacuum hot pressing is not used to achieve densification of the energy layer and interface strengthening.
[0011] Fourth, the seismic performance is insufficient. Bridge wire products rely on plastic encapsulation for protection, and the interlayer bonding strength of thin film devices is easily weakened by thermal cycling. There is a lack of systematic multi-layer high-modulus encapsulation reinforcement solutions.
[0012] Therefore, it is necessary to invent a fabrication process for an ultra-small volume composite bridge resistor and a composite bridge resistor thereof to solve the above problems. Summary of the Invention
[0013] To address the aforementioned problems, this invention provides a fabrication process for an ultra-small volume composite bridge resistor and the same composite bridge resistor, thereby solving one of the problems mentioned in the background section.
[0014] To achieve the above objectives, the present invention provides the following technical solution: an ultra-small volume composite bridge resistor, comprising, from bottom to top: an FR-5 fiberglass substrate, an electrode, a nickel-chromium alloy film bridge, an aluminothermic energy layer, a high-modulus inner sealing film, a rigid cover plate, and an outer sealing film protective layer.
[0015] The nickel-chromium alloy film bridge is a pre-fabricated nickel-chromium alloy thin film by a rolling process, with a film thickness of 2.5 to 5 μm, and is not formed by magnetron sputtering or in-situ deposition.
[0016] The thermite energy layer is formed by printing process and has a thickness of 90 to 150 μm; the elastic modulus of the high modulus inner sealing film and the rigid cover plate are both greater than or equal to 2 GPa.
[0017] The FR-5 fiberglass substrate has a thickness of 0.15 to 0.25 mm; the rigid cover plate has a thickness of 0.15 to 0.25 mm; the electrode includes a front electrode and a back SMT pad electrode, with the back electrode pad width being 0.2 to 0.3 mm.
[0018] Furthermore, the nickel-chromium alloy film has a Ni 80%-Cr 20% mass ratio and a bridge resistance of 0.5 to 10 Ω. The aluminothermic energy layer is composed of a mixture of micron-sized aluminum powder and micron-sized metal oxide powder. The micron-sized aluminum powder has a particle size of 1 to 15 μm, and the micron-sized metal oxide powder has a particle size of 1 to 10 μm. The aluminothermic system is selected from at least one of Al / Fe2O3, Al / CuO, Al / MnO2, Al / NiO, and Al / BiO. The high-modulus inner sealing film material is selected from polyimide (PI), polyetheretherketone (PEEK), liquid crystal polymer (LCP), and their composites. The rigid cover plate is a glass fiber reinforced epoxy resin board or a ceramic-filled polymer board. The outer sealing film protective layer is an epoxy resin or silicone resin encapsulation material.
[0019] This invention also provides a process for preparing the above-mentioned ultra-small volume composite bridge resistor, comprising the following steps:
[0020] S1. Substrate preparation: Cut FR-5 fiberglass board into large sheets, clean and dry them;
[0021] S2. Electrode fabrication: Prepare front electrode patterns and back pad electrodes for SMT reflow soldering on the substrate, and perform plating treatment on the electrode surfaces.
[0022] S3. Bridge body preparation: The pre-fabricated nickel-chromium alloy film is laminated and fixed onto the front electrode area of the substrate, and the shaped bridge body is obtained by photolithography etching or laser fine-tuning.
[0023] S4. Energy layer printing and coating: Prepare the thermite printing paste, and apply the paste to the top of the bridge body by screen printing or stencil printing. Pre-dry at 50 to 80°C for 5 to 30 minutes.
[0024] S5. High vacuum hot pressing: The semi-finished products are stacked in sequence with a high modulus inner sealing film and a rigid cover plate, and placed in a vacuum hot pressing device; the vacuum degree is ≤10Pa, the hot pressing temperature is 80 to 200℃, the pressure is 0.5 to 15MPa, the holding time is 1 to 60min, and the heating rate is 1 to 10℃ / min, to complete the densification of the energetic layer and the bonding of the interlayer interface.
[0025] S6. Application of outer sealing film: Apply outer sealing film material to the top surface of the cover plate and the side wall of the device, and cure it.
[0026] S7. Cutting and sorting: Cut the large panel array into individual units and sort them for electrical performance testing;
[0027] S8. Packaging and shipping: SMT surface mount finished components are obtained by tape or reel packaging.
[0028] Furthermore, the vacuum hot pressing device includes a frame, a base plate on the top of the frame, a ladder detachably mounted on the top of the base plate, an installation groove on the top of the ladder, a horizontally arranged shelf in the installation groove, a deflection component at the bottom of the shelf for deflecting the shelf at any angle in the horizontal direction, a top plate horizontally mounted on the top of the shelf, a pressing component detachably mounted on the bottom of the top plate, multiple guide rods vertically sliding and penetrating between the top plate and the base plate, the bottom end of the guide rods being vertically and fixedly connected to the top of the frame, an electric push rod vertically mounted on the top of the top plate, a mounting frame connected to the top of the electric push rod, and the mounting frame being fixedly connected to the frame.
[0029] Furthermore, the deflection assembly includes a deflection ball, which is fixedly connected to the center of the bottom of the shelf. A connecting block is rotatably sleeved on the bottom of the deflection ball. The connecting block is fixedly connected to the inner wall of the bottom of the mounting groove. Several sleeves are evenly distributed around the connecting block. A support column is slidably inserted into the top of the sleeve. A support spring is fixedly connected between the bottom end of the support column and the inner wall of the bottom of the sleeve. A ball is rotatably connected to the top of the support column. The ball can always keep in contact with the bottom of the shelf under the elastic force of the support spring on the support column. Several limiting posts are vertically fixedly connected to the inner wall of the bottom of the mounting groove. Several limiting springs are evenly fixedly connected between the bottom of the shelf and the inner wall of the bottom of the mounting groove to restrict the shelf and prevent the shelf from rotating in the horizontal direction.
[0030] Furthermore, the pressing assembly includes a pressing plate, the bottom of which has a pressing groove that matches the platform, and a plurality of flexible pressure equalizing plates are arranged in an array on the top inner wall of the pressing groove. The bottom of the flexible pressure equalizing plate is fixedly connected to a rigid pad that matches the size of its bottom surface.
[0031] Furthermore, a number of positioning posts are uniformly and vertically fixedly connected to the top of the shelf, and a positioning hole is opened at the position of the top of the pressure groove directly opposite the positioning post. The diameter of the positioning hole is larger than the diameter of the positioning post, and the maximum diameter difference between the two is ≤20μm.
[0032] Furthermore, in the initial state, the top of the limiting post remains separated from the bottom of the shelf, and the limiting post can limit the horizontal deflection angle of the shelf to ≤0.2°.
[0033] Furthermore, the preferred process parameters for step S5, high vacuum hot pressing, are: vacuum degree 0.1 to 1 Pa, temperature 120 to 150 °C, pressure 1 to 5 MPa, pressure holding for 5 to 20 min, and heating rate 2 to 5 °C / min.
[0034] Furthermore, the thermite printing paste in step S4 comprises micron-sized aluminum powder, micron-sized metal oxide powder, and an organic carrier, wherein the organic carrier is a nitrocellulose or ethylcellulose solvent solution; the nickel-chromium alloy film thickness in step S3 is 3 to 4 μm; and the thickness of the energetic layer after printing in step S4 is controlled to be 100 to 130 μm.
[0035] The technical effects and advantages of this invention are as follows:
[0036] 1. The device of this invention adopts the 0805 standard SMT package, which is miniaturized and directly compatible with ordinary SMT placement machines and reflow soldering production lines. It does not require customized tooling or bonding wires, reducing downstream integration costs and adapting to the space requirements of digital electronic detonators and miniature fuses.
[0037] 2. The energy layer is formed by screen / stencil printing, which has lower investment and higher mass production efficiency compared to magnetron sputtering equipment; compared to direct writing printing, it has better paste compatibility, which is conducive to stable mass production; all micron-level powders are used, avoiding the safety risks of nano-aluminum powder production, and the ignition consistency is good.
[0038] 3. Creatively introduce a high-vacuum hot pressing process, which removes gas from the interlayer and the interior of the energetic layer, softens the organic carrier with heat, and promotes particle rearrangement and densification with pressure; eliminates bubble and void defects, and achieves a high-strength and tight interface bond between the energetic layer and the nickel-chromium bridge, solving the industry pain point of delamination under vibration environment, and greatly improving the reliability and storage stability of pyrotechnic products.
[0039] 4. A three-layer encapsulation structure consisting of a high-modulus inner sealing film, a rigid cover plate, and an outer sealing film is adopted to form a high-rigidity sandwich protective structure. Without significantly increasing the volume, this greatly improves the device's resistance to vibration, impact, and thermal cycling, meeting military-grade environmental testing conditions; and avoids the aging and cracking problems of traditional plastic-sealed structures.
[0040] 5. The entire process, from substrate processing to finished product testing and sorting, is integrated and outputs standardized surface mount components that can be used directly, simplifying the downstream supply chain and ensuring quality control.
[0041] 6. By incorporating a deflection component, when the placement plate is pressed and subjected to force, the placement plate can achieve multi-directional micro-adaptive deflection using a deflection ball as a fulcrum. This can automatically compensate for planar errors caused by the overall warping of the large workpiece and the tilting of the plate thickness. During the deflection process of the placement plate, the limiting spring can prevent the placement plate from rotating horizontally. Together with the limiting post, it achieves mechanical hard limiting, restricting the maximum deflection angle of the placement plate to ≤0.2°. From a structural perspective, this avoids excessive deflection angles that could cause significant shearing and misalignment of the workpiece, protecting the nickel-chromium alloy film bridge and the thermite energy layer from shearing damage.
[0042] 7. The pressing component of this invention adopts an array-type flexible pressure equalizing plate combined with a rigid pad structure, which can perform local pressure compensation in different areas of the large board, improve the uneven pressure distribution of the large board, and make the composite bridge resistor semi-finished products in various parts of the large board obtain a more consistent pressing pressure, thereby improving the density of the whole board product, the interface bonding strength, and the batch production consistency.
[0043] 8. This invention adds a limiting fit structure between the positioning post and the positioning hole. The maximum diameter difference between the two is ≤20μm. The small gap will not interfere with the adaptive deflection compensation function of the placement plate (≤0.2°) and can strictly limit the relative sliding between the plane of the placement plate and the pressing plate. This controls the maximum plane sliding of the workpiece within a safe range, further suppresses the horizontal shear displacement of the large plate workpiece, avoids the breakage of the nickel-chromium bridge and the interlayer slippage and peeling of the energetic layer, and ensures the integrity of the device stack structure during the hot pressing process.
[0044] It should be understood that both the foregoing general description and the following detailed description are for illustrative purposes and do not necessarily limit the scope of this disclosure. The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate the subject matter of this disclosure. Furthermore, the specification and drawings serve to explain the principles of this disclosure. Attached Figure Description
[0045] To more clearly illustrate the technical solutions in the specific embodiments of this disclosure or the prior art, the accompanying drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this disclosure. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort. The illustrative embodiments of this application and their descriptions are used to explain this application and do not constitute an improper limitation of this application.
[0046] Figure 1 This is a three-dimensional schematic diagram of the composite bridge resistor in this invention;
[0047] Figure 2 This is a three-dimensional schematic diagram of the vacuum hot pressing device in this invention;
[0048] Figure 3 This is a three-dimensional sectional view of the ladder platform in this invention;
[0049] Figure 4 This is a three-dimensional schematic diagram of the pressing plate in this invention;
[0050] Figure 5 In this invention Figure 4 Enlarged view of part A.
[0051] In the diagram: 1. FR-5 fiberglass substrate; 2. Electrode; 3. Nickel-chromium alloy membrane bridge; 4. Thermite energetic layer; 5. High-modulus inner sealing film; 6. Rigid cover plate; 7. Outer sealing film protective layer; 8. Frame; 9. Base plate; 10. Ladder platform; 11. Shelf plate; 12. Top plate; 13. Guide rod; 14. Electric push rod; 15. Mounting bracket; 16. Deflection ball; 17. Connecting block; 18. Sleeve; 19. Support column; 20. Support spring; 21. Ball bearing; 22. Limiting post; 23. Limiting spring; 24. Pressing plate; 25. Flexible equalizing plate; 26. Rigid pad; 27. Positioning post; 28. Positioning hole. Detailed Implementation
[0052] To make the technical solutions and advantages of the embodiments of this application clearer, the exemplary embodiments of this application will be described in further detail below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not an exhaustive list of all embodiments. It should be noted that, unless otherwise specified, the embodiments and features in the embodiments of this application can be combined with each other.
[0053] This invention provides, for example Figures 1 to 5 The ultra-small volume composite bridge resistor shown comprises, from bottom to top: FR-5 fiberglass substrate, electrode 2, nickel-chromium alloy film bridge 3, thermite energy layer 4, high modulus inner sealing film 5, rigid cover plate 6, and outer sealing film protective layer 7.
[0054] The nickel-chromium alloy film bridge 3 is a pre-fabricated nickel-chromium alloy thin film by a rolling process, with a film thickness of 2.5 to 5 μm, and is not formed by magnetron sputtering or in-situ deposition.
[0055] The thermite energy layer 4 is coated and formed by printing process, with a thickness of 90 to 150 μm; the elastic modulus of the high modulus inner sealing film 5 and the rigid cover plate 6 are both greater than or equal to 2 GPa.
[0056] The FR-5 fiberglass substrate has a thickness of 0.15 to 0.25 mm; the rigid cover plate 6 has a thickness of 0.15 to 0.25 mm; the electrode 2 includes a front electrode 2 and a back SMT pad electrode 2, with the back electrode 2 pad width being 0.2 to 0.3 mm;
[0057] The nickel-chromium alloy film has a Ni 80%-Cr 20% mass ratio and a bridge resistance of 0.5 to 10 Ω. The aluminothermic energy layer 4 is composed of micron-sized aluminum powder and micron-sized metal oxide powder; the micron-sized aluminum powder has a particle size of 1 to 15 μm, and the micron-sized metal oxide powder has a particle size of 1 to 10 μm; the aluminothermic system is selected from at least one of Al / Fe2O3, Al / CuO, Al / MnO2, Al / NiO, and Al / BiO; the high-modulus inner sealing film 5 is made of polyimide (PI), polyetheretherketone (PEEK), liquid crystal polymer (LCP), and their composites; the rigid cover plate 6 is a glass fiber reinforced epoxy resin board or a ceramic-filled polymer board; the outer sealing film protective layer 7 is an epoxy resin or silicone resin encapsulation material.
[0058] When this ultra-small volume composite bridge resistor is working, the external circuit current is introduced through the back SMT pad electrode 2 and then delivered to the nickel-chromium alloy film bridge 3 through the front electrode 2. The nickel-chromium alloy film bridge 3 is pre-fabricated to obtain a 2.5 to 5 μm thick Ni 80% to Cr 20% alloy film. Unlike magnetron sputtering and evaporation in-situ film formation, the film layer has high density and stable resistance-temperature characteristics. After being energized, it generates Joule heat by its own resistance, which quickly converts electrical energy into heat energy. When the temperature reaches the reaction triggering condition, the heat is conducted to the aluminothermic agent energy layer 4 composed of micron-sized powder. The aluminothermic agent system (Al / Fe2O3, Al / CuO, etc.) undergoes a violent aluminothermic oxidation-reduction reaction, releasing high-temperature heat and plasma that is much greater than Joule heat, thus achieving reliable ignition of the upper-level agent.
[0059] The thermite energetic layer 4 is coated with a printing process to achieve a thickness of 90 to 150 μm, and all powders adopt micron-level particle size to ensure both production safety and reaction output consistency. A high-modulus inner sealing film 5 with an elastic modulus ≥2 GPa and a rigid cover plate 6 are set above the energetic layer. The two form a high-rigidity sandwich constraint structure, which on the one hand completes the densification of the energetic layer during the vacuum hot pressing preparation stage, strengthens the bonding strength of the energetic layer-nickel-chromium bridge interface, and eliminates interlayer bubbles and voids. On the other hand, it suppresses the risk of interlayer misalignment and delamination caused by vibration, impact, and thermal cycling during product service. The outermost outer sealing film protective layer 7 made of epoxy resin or silicone resin provides moisture-proof, dust-proof, and insulation protection for the entire device.
[0060] The FR-5 fiberglass substrate serves as the underlying mechanical support carrier. Its low thermal conductivity allows it to concentrate the Joule heat generated by the bridge towards the energy layer, reducing heat loss from the substrate side and improving energy utilization efficiency. The thickness range of the substrate and cover plate, as well as the size specifications of the SMT pads on the back, enable the entire stacked device to meet the 0805 standard SMT package size requirements. It can be directly mounted on the PCB circuit board via reflow soldering, making it suitable for automated integration applications of digital electronic detonators, miniature igniters, and gap ignition fuse modules.
[0061] This invention also provides a process for preparing the above-mentioned ultra-small volume composite bridge resistor, comprising the following steps:
[0062] S1. Substrate preparation: Cut FR-5 fiberglass board into large sheets, clean and dry them;
[0063] S2, Electrode 2 fabrication: The front electrode 2 pattern and the back pad electrode 2 for SMT reflow soldering are fabricated on the substrate, and the surface of the electrode 2 is plated.
[0064] S3. Bridge body preparation: The pre-fabricated nickel-chromium alloy thin film is bonded and fixed to the front electrode 2 area of the substrate, and the shaped bridge body is obtained by photolithography etching or laser fine-tuning.
[0065] S4. Energy layer printing and coating: Prepare the thermite printing paste, and apply the paste to the top of the bridge body by screen printing or stencil printing. Pre-dry at 50 to 80°C for 5 to 30 minutes.
[0066] S5. High vacuum hot pressing: The semi-finished products are stacked sequentially with high modulus inner sealing film 5 and rigid cover plate 6, and placed in a vacuum hot pressing device; vacuum degree ≤10Pa, hot pressing temperature 80 to 200℃, pressure 0.5 to 15MPa, holding time 1 to 60min, heating rate 1 to 10℃ / min, to complete the densification of the energetic layer and the bonding of the interlayer interface.
[0067] S6. Application of outer sealing film: Apply outer sealing film material to the top surface of the cover plate and the side wall of the device, and cure it.
[0068] S7. Cutting and sorting: Cut the large panel array into individual units and sort them for electrical performance testing;
[0069] S8. Packaging and shipping: SMT surface mount finished components are obtained by tape or reel packaging.
[0070] The preferred process parameters for high-vacuum hot pressing in step S5 are: vacuum degree 0.1 to 1 Pa, temperature 120 to 150 °C, pressure 1 to 5 MPa, holding pressure for 5 to 20 min, and heating rate 2 to 5 °C / min. The thermite printing paste in step S4 contains micron-sized aluminum powder, micron-sized metal oxide powder, and an organic carrier, wherein the organic carrier is a nitrocellulose or ethyl cellulose solvent solution. The thickness of the nickel-chromium alloy film in step S3 is 3 to 4 μm. The thickness of the energetic layer after printing in step S4 is controlled to be 100 to 130 μm.
[0071] like Figures 2 to 5As shown, the vacuum hot press device includes a frame 8, a base plate 9 on the top of the frame 8, a ladder 10 detachably mounted on the top of the base plate 9, an installation groove on the top of the ladder 10, a horizontally arranged shelf 11 in the installation groove, a deflection component at the bottom of the shelf 11 for deflecting the shelf 11 at any angle in the horizontal direction, a top plate 12 horizontally mounted on the top of the shelf 11, a pressing component detachably mounted on the bottom of the top plate 12, a plurality of guide rods 13 vertically sliding and penetrating between the top plate 12 and the base plate 9, the bottom end of the guide rods 13 being vertically fixedly connected to the top of the frame 8, an electric push rod 14 vertically mounted on the top of the top plate 12, a mounting frame 15 connected to the top of the electric push rod 14, and the mounting frame 15 being fixedly connected to the frame 8.
[0072] The deflection assembly includes a deflection ball 16, which is fixedly connected to the center of the bottom of the shelf 11. A connecting block 17 is rotatably sleeved on the bottom of the deflection ball 16. The connecting block 17 is fixedly connected to the inner wall of the bottom of the mounting groove. Several sleeves 18 are evenly distributed around the connecting block 17. A support column 19 is slidably inserted into the top of the sleeve 18. A support spring 20 is fixedly connected between the bottom end of the support column 19 and the inner wall of the bottom of the sleeve 18. A ball bearing 21 is rotatably connected to the top of the support column 19, and the ball bearing 21 can rotate through the support spring 20. Under the elastic force of the support column 19, it always stays in contact with the bottom of the shelf 11. Several limiting columns 22 are vertically fixedly connected to the bottom of the mounting groove. Several limiting springs 23 are evenly fixedly connected between the bottom of the shelf 11 and the inner wall of the bottom of the mounting groove to restrict the shelf 11 and prevent the shelf 11 from rotating in the horizontal direction. In the initial state, the top of the limiting column 22 is separated from the bottom of the shelf 11, and the limiting column 22 can limit the horizontal deflection angle of the shelf 11 to ≤0.2°.
[0073] The pressing assembly includes a pressing plate 24. The bottom of the pressing plate 24 is provided with a pressing groove that matches the platform 10. Several flexible pressure equalizing plates 25 are arranged in an array on the top inner wall of the pressing groove. The bottom of the flexible pressure equalizing plate 25 is fixedly connected with a rigid pad 26 that matches the size of its bottom surface.
[0074] When the vacuum hot pressing device is working, the large plate semi-finished product to be pressed is placed on the placement plate 11. Then, the electric push rod 14 is started. The electric push rod 14 outputs driving force to drive the top plate 12 and the pressing plate 24 at the bottom to move downward along multiple guide rods 13. During the pressing process of the pressing plate 24, when the pressing plate 24 is completely pressed together with the ladder 10, the pressing groove can cooperate with the ladder 10 to seal the large plate semi-finished product. Multiple sets of flexible pressure equalizing plates 25 arranged in an array on the top wall of the pressing groove, together with their corresponding hard pads 26, can achieve local pressure compensation at different positions of the large plate, improve the problem of uneven pressure distribution within the large plate, and ensure that the workpieces in all parts of the large plate obtain relatively uniform pressing pressure.
[0075] When the rigid pad 26 at the bottom of the flexible equalizing plate 25 is pressed together with the large plate semi-finished product, the placement plate 11 can deflect slightly around the deflection ball 16 under pressure to compensate for the planar error caused by the overall warping and thickness tilt of the large plate workpiece to be pressed. As the placement plate 11 deflects, the support column 19 on the downward deflection side of the placement plate 11 can be squeezed downward, thereby driving the corresponding support spring 20 at its bottom to be compressed as well. The support column 19 on the upward deflection side of the placement plate 11 can move upward under the elastic force of the corresponding support spring 20 at its bottom, thus always maintaining contact with the bottom of the placement plate 11. In this way, the stability of the placement plate 11 is ensured by the support of multiple support columns 19. In addition, during the deflection of the placement plate 11, the ball 21 can roll against the bottom of the placement plate 11, thereby reducing the friction between the bottom of the placement plate 11 and the top of the support column 19, so that the placement plate 11 can deflect more smoothly.
[0076] The limiting spring 23 arranged between the placement plate 11 and the bottom of the mounting groove can constrain the placement plate 11 and prevent the placement plate 11 from rotating in the horizontal direction. The limiting post 22 set at the bottom of the mounting groove is initially separated from the bottom surface of the placement plate 11. When the placement plate 11 deflects to the maximum allowable position, the limiting post 22 contacts the bottom surface of the placement plate 11, thereby limiting the deflection angle of the placement plate 11 and constraining the deflection angle of the placement plate 11 to ≤0.2°. This avoids excessive deflection angle causing shearing and misalignment of the workpiece, and prevents the nickel-chromium bridge and energetic layer from being sheared and damaged. After hot pressing and pressure holding are completed, the electric push rod 14 drives the top plate 12 and the pressing assembly to lift upwards, and the pressed semi-finished product can be taken out.
[0077] like Figures 2 to 5 As shown, a number of positioning posts 27 are uniformly and vertically fixedly connected to the top of the shelf 11. A positioning hole 28 is opened at the top of the groove and directly opposite the positioning post 27. The diameter of the positioning hole 28 is larger than the diameter of the positioning post 27, and the maximum diameter difference between the two is ≤20μm.
[0078] When the vacuum hot press device performs the pressing operation, several positioning posts 27 vertically fixed on the placement plate 11 move together with the placement plate 11. During the pressing process of the pressing plate 24 being fed downwards, the positioning posts 27 are inserted into the positioning holes 28 at the top of the pressing groove. The diameter of the positioning hole 28 is larger than the diameter of the positioning post 27, and the maximum diameter difference between the two is controlled within 20μm. This small gap can accommodate the small adaptive deflection of the placement plate 11 within the range of ≤0.2°, and will not obstruct the angle of the placement plate 11 due to the positioning posts 27 being rigidly jammed with the positioning holes 28. The compensation action can also strictly constrain the relative planar displacement between the placement plate 11 and the pressing plate 24, limiting the maximum planar slip between the placement plate 11 and the pressing plate 24 to within 20μm. This suppresses the horizontal shear displacement of the large plate workpiece caused by the slight deflection of the placement plate 11 and the equipment assembly gap during the pressing process, preventing the nickel-chromium alloy film bridge 3 on the large plate from being broken by shear. At the same time, it prevents interlayer misalignment and interface peeling of the thermite energetic layer 4, ensuring the integrity of the interlayer structure of the composite bridge resistor semi-finished product during the hot pressing densification process.
[0079] The present invention will be further described in detail below with reference to specific embodiments, but the present invention is not limited to the embodiments.
[0080] Example 1: JMD0805 type composite bridge resistor for digital electronic detonator
[0081] Product dimensions: 2.0mm × 1.2mm × 0.4mm; Bridge resistance: 2.5Ω ± 5%; Nickel-chromium film: calendered pre-fabricated Ni80 / Cr20 film, 4μm thick; Energetic layer: Al / Fe2O3, mass ratio 26:74; Aluminum powder D50≈4μm; Fe2O3 D50≈3μm; Printing thickness: 110μm; Inner sealing film: 25μm polyimide; Cover plate: 0.2mm fiberglass epoxy board; Outer sealing film: green epoxy resin.
[0082] Preparation process: Cut S1, 0.2mm FR-5 fiberglass board into 100×100mm large boards, plasma clean and dry;
[0083] S2, double-sided copper electrode 2, back side SMT pad, front side bridge electrode 2; surface plated with nickel-tin;
[0084] S3, Tilted NiCr thin film hot-pressed transfer and bonding substrate; Photolithography etching to obtain a 0.3mm×0.5mm rounded rectangular bridge;
[0085] S4. Prepare a slurry with a solid content of 75% and a viscosity of 8000 mPa·s; screen print on a 200-mesh screen; dry at 80℃ for 10 min.
[0086] S5, laminated PI inner sealing film, glass fiber epoxy cover plate; vacuum hot pressing conditions: vacuum 0.5Pa, heating rate 3℃ / min, temperature 140℃, pressure 3MPa, holding pressure for 15min; remove after cooling to below 60℃;
[0087] S6. The outer surface is coated with green epoxy resin and cured at 130℃ for 30 minutes.
[0088] S7, laser-cut single unit, 100% resistance and insulation testing;
[0089] S8, braided packaging.
[0090] Performance: SMT placement yield > 99.5%; resistance change less than 1% after random vibration test under GJB150.8A; ignition delay < 50μs under 9V / 22μF conditions; 100% ignition success rate of 500 samples.
[0091] Example 2: Low-resistance igniter thin composite bridge resistor
[0092] Dimensions: 2.0mm × 1.2mm × 0.35mm; Bridge resistance: 1.0Ω ± 5%; Nickel-chromium rolled film thickness: 5μm; Energetic layer: Al / CuO system, printed thickness: 95μm; Cover plate thickness: 0.15mm; Vacuum hot pressing parameters: Vacuum 0.1Pa, temperature 130℃, pressure 2MPa, holding pressure for 10min; Effect: Achieves reliable ignition at 3V / 22μF, suitable for PCB integration in battery-powered handheld ignition devices.
[0093] Example 3: High-energy output composite bridge resistor for gap ignition fuze module
[0094] Dimensions: 2.0mm × 1.2mm × 0.45mm; Bridge resistance: 5.0Ω ± 5%; Energetic layer: Al / NiO, printing thickness: 140μm; Inner sealing film: PEEK film; Cover plate: 0.2mm; Vacuum hot pressing parameters: Vacuum 0.01Pa, temperature 160℃, pressure 5MPa, holding pressure for 20min; Results: Ignition distance in air gap ≥ 1.5mm, suitable for ignition requirements of fuse spacer, PEEK inner sealing film withstands multiple high-energy ignitions without structural degradation.
[0095] Based on the embodiments in this disclosure, all other embodiments obtained by those skilled in the art without inventive effort are within the scope of protection of this disclosure.
[0096] In the description of this disclosure, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this disclosure and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this disclosure. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.
[0097] In the description of this disclosure, it should be noted that, unless otherwise expressly specified and limited, the terms "installation," "connection," and "linkage" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection between two components. Those skilled in the art can understand the specific meaning of the above terms in this disclosure based on the specific circumstances.
[0098] Although preferred embodiments of this application have been described, those skilled in the art, upon learning the basic inventive concept, can make other changes and modifications to these embodiments. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments as well as all changes and modifications falling within the scope of this application.
[0099] Obviously, those skilled in the art can make various modifications and variations to this application without departing from the spirit and scope of this application. Therefore, if such modifications and variations fall within the scope of the claims of this application and their equivalents, this application also intends to include such modifications and variations.
Claims
1. A small-volume composite bridge resistor, characterized in that, From bottom to top, the components are: FR-5 fiberglass substrate, electrode (2), nickel-chromium alloy membrane bridge (3), thermite energy layer (4), high modulus inner sealing film (5), rigid cover plate (6), and outer sealing film protective layer (7). The nickel-chromium alloy film bridge (3) is a nickel-chromium alloy thin film prefabricated by rolling process, with a film thickness of 2.5 to 5 μm, and is not formed by magnetron sputtering or in-situ deposition. The thermite energy layer (4) is coated and formed by printing process, with a thickness of 90 to 150 μm; the elastic modulus of the high modulus inner sealing film (5) and the rigid cover plate (6) are both greater than or equal to 2 GPa; The thickness of the FR-5 fiberglass substrate is 0.15 to 0.25 mm; the thickness of the rigid cover plate (6) is 0.15 to 0.25 mm; the electrode (2) includes a front electrode (2) and a back SMT pad electrode (2), the width of the back electrode (2) pad is 0.2 to 0.3 mm.
2. The fabrication process of the ultra-small volume composite bridge resistor and the composite bridge resistor according to claim 1, characterized in that: The nickel-chromium alloy film has a Ni 80%-Cr 20% mass ratio and a bridge resistance of 0.5 to 10Ω. The aluminothermic energy layer (4) is composed of micron-sized aluminum powder and micron-sized metal oxide powder. The micron-sized aluminum powder has a particle size of 1 to 15 μm, and the micron-sized metal oxide powder has a particle size of 1 to 10 μm. The aluminothermic system is selected from at least one of Al / Fe2O3, Al / CuO, Al / MnO2, Al / NiO, and Al / BiO. The high-modulus inner sealing film (5) is made of polyimide PI, polyether ether ketone (PEEK), liquid crystal polymer (LCP), and their composites. The rigid cover plate (6) is a glass fiber reinforced epoxy resin plate or a ceramic-filled polymer plate. The outer sealing film protective layer (7) is an epoxy resin or silicone resin encapsulation material.
3. The fabrication process of the ultra-small volume composite bridge resistor according to any one of claims 1 to 2, characterized in that, Includes the following steps: S1. Substrate preparation: Cut FR-5 fiberglass board into large sheets, clean and dry them; S2, Electrode (2) fabrication: The front electrode (2) pattern and the back pad electrode (2) for SMT reflow soldering are prepared on the substrate, and the surface of the electrode (2) is plated. S3, Bridge preparation: The rolled pre-made nickel-chromium alloy film is bonded and fixed to the front electrode (2) area of the substrate, and the shaped bridge is obtained by photolithography etching or laser fine-tuning. S4. Energy layer printing and coating: Prepare the thermite printing paste, and apply the paste to the top of the bridge body by screen printing or stencil printing. Pre-dry at 50 to 80°C for 5 to 30 minutes. S5. High vacuum hot pressing: The semi-finished products are stacked in sequence with a high modulus inner sealing film (5) and a rigid cover plate (6), and placed in a vacuum hot pressing device; the vacuum degree is ≤10Pa, the hot pressing temperature is 80 to 200℃, the pressure is 0.5 to 15MPa, the holding time is 1 to 60min, and the heating rate is 1 to 10℃ / min, to complete the densification of the energetic layer and the bonding of the interlayer interface. S6. Application of outer sealing film: Apply outer sealing film material to the top surface of the cover plate and the side wall of the device, and cure it. S7. Cutting and sorting: Cut the large panel array into individual units and sort them for electrical performance testing; S8. Packaging and shipping: SMT surface mount finished components are obtained by tape or reel packaging.
4. The fabrication process of the ultra-small volume composite bridge resistor according to claim 3, characterized in that: The vacuum hot pressing device includes a frame (8), a base plate (9) is provided on the top of the frame (8), a ladder (10) is detachably installed on the top of the base plate (9), an installation groove is provided on the top of the ladder (10), a shelf (11) is horizontally arranged in the installation groove, a deflection component is provided at the bottom of the shelf (11) to realize the deflection operation of the shelf (11) at any angle in the horizontal direction, and a top plate is horizontally arranged on the top of the shelf (11). (12) A pressing assembly is detachably installed at the bottom of the top plate (12). A plurality of guide rods (13) are vertically slidably inserted between the top plate (12) and the bottom plate (9). The bottom end of the guide rod (13) is vertically fixedly connected to the top of the frame (8). An electric push rod (14) is vertically installed at the top of the top plate (12). A mounting bracket (15) is connected to the top end of the electric push rod (14). The mounting bracket (15) is fixedly connected to the frame (8).
5. The fabrication process of the ultra-small volume composite bridge resistor according to claim 4, characterized in that: The deflection assembly includes a deflection ball (16), which is fixedly connected to the center of the bottom of the shelf (11). A connecting block (17) is rotatably sleeved on the bottom of the deflection ball (16). The connecting block (17) is fixedly connected to the inner wall of the bottom of the mounting groove. Several sleeves (18) are evenly distributed around the connecting block (17). A support column (19) is slidably inserted into the top of the sleeve (18). A support spring is fixedly connected between the bottom end of the support column (19) and the inner wall of the bottom of the sleeve (18). 20), the top of the support column (19) is rotatably connected to a ball (21), and the ball (21) can always keep in contact with the bottom of the shelf (11) under the elastic force of the support spring (20) on the support column (19). Several limiting columns (22) are vertically fixedly connected to the bottom of the mounting groove. Several limiting springs (23) are uniformly fixedly connected between the bottom of the shelf (11) and the inner wall of the bottom of the mounting groove to restrict the shelf (11) and prevent the shelf (11) from rotating in the horizontal direction.
6. The fabrication process of the ultra-small volume composite bridge resistor according to claim 5, characterized in that: The pressing assembly includes a pressing plate (24), the bottom of which is provided with a pressing groove that matches the platform (10), and a number of flexible pressure equalizing plates (25) are arranged in an array on the top inner wall of the pressing groove. The bottom of the flexible pressure equalizing plate (25) is fixedly connected with a rigid pad (26) that matches the size of its bottom surface.
7. The fabrication process of the ultra-small volume composite bridge resistor according to claim 6, characterized in that: The top of the shelf (11) is uniformly and vertically fixed with a number of positioning posts (27). The top of the pressure groove is provided with a positioning hole (28) opposite to the positioning post (27). The diameter of the positioning hole (28) is larger than the diameter of the positioning post (27), and the maximum diameter difference between the two is ≤20μm.
8. The fabrication process of the ultra-small volume composite bridge resistor according to claim 7, characterized in that: In the initial state, the top of the limiting post (22) is separated from the bottom of the shelf (11), and the limiting post (22) can limit the horizontal deflection angle of the shelf (11) to ≤0.2°.
9. The fabrication process of the ultra-small volume composite bridge resistor according to claim 8, characterized in that: The preferred process parameters for step S5, high vacuum hot pressing, are: vacuum degree 0.1 to 1 Pa, temperature 120 to 150 °C, pressure 1 to 5 MPa, pressure holding for 5 to 20 min, and heating rate 2 to 5 °C / min.
10. The fabrication process of the ultra-small volume composite bridge resistor according to claim 9, characterized in that: The thermite printing paste in step S4 contains micron-sized aluminum powder, micron-sized metal oxide powder, and an organic carrier, wherein the organic carrier is a nitrocellulose or ethylcellulose solvent solution; the nickel-chromium alloy film thickness in step S3 is 3 to 4 μm; and the thickness of the energetic layer after printing in step S4 is controlled to be 100 to 130 μm.
Citation Information
Patent Citations
Metal film bridge igniter and preparation method thereof
CN102927590A
Low-igniting-voltage miniature semiconductor bridge igniting assembly
CN103528445B
Energetic semiconductor bridge and preparation method thereof
CN104976925A
Preparation method for bridge area of film bridge initiator
CN105737681A
Composite energetic thin film semiconductor bridge
CN112254586A