A method for determining mechanical properties of ferromagnetic material based on electromagnetic nondestructive testing
By establishing a ridge regression model based on electromagnetic nondestructive testing and using the electromagnetic characteristic parameters of ferromagnetic materials for prediction, the problems of low detection accuracy and online detection in existing technologies are solved, and efficient and accurate determination of the mechanical properties of ferromagnetic materials is achieved.
Patent Information
- Application Number
- CN202510671550.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-23
- Publication Date
- 2026-11-24
AI Technical Summary
Existing electromagnetic nondestructive testing systems can only detect some mechanical performance parameters, have unsatisfactory prediction accuracy, and require auxiliary destructive experiments, making online testing impossible.
The electromagnetic characteristics and mechanical properties of ferromagnetic materials are obtained by training datasets, a ridge regression model is established, and predictions are made using electromagnetic characteristic parameters. A specific range is set to reduce destructive experiments.
It has achieved efficient and non-destructive testing of the mechanical properties of ferromagnetic materials, with a prediction accuracy of over 90%, reducing testing costs and time.
Smart Images

Figure CN123155318A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of ferromagnetic material testing, and in particular to a method for determining the mechanical properties of ferromagnetic materials based on electromagnetic nondestructive testing. Background Technology
[0002] Destructive testing is the primary method for evaluating the mechanical properties of steel materials, including a series of destructive physical tests such as tensile, compression, bending, shear, impact, and fatigue tests. In addition, to optimize production processes, laboratories typically analyze the microstructure of steel materials using X-ray diffraction and optical or electron microscopy. However, these methods suffer from drawbacks such as long testing times, high costs, significant personnel requirements, low efficiency, and high false negative rates.
[0003] To address the problems associated with traditional destructive testing, an electromagnetic non-destructive testing system has been developed in the prior art. This system is based on the periodic magnetization of the strip steel, then measuring the residual magnetic field strength gradient on the upper and lower surfaces of the cold-rolled strip steel, and then using a regression model to calculate the mechanical properties, tensile strength, and yield point of the cold-rolled strip steel and display them on a host computer.
[0004] The system exhibits good stability and reliability, and its on-site installation is relatively simple. However, the system has the following drawbacks:
[0005] (1) The system can detect a limited number of mechanical properties, and can only calculate some mechanical properties such as tensile strength and yield point; (2) The prediction accuracy of the system is not ideal, and it still needs to be tested by destructive experiments. It cannot be considered a true online detection system.
[0006] Therefore, it is necessary to improve the existing technology to overcome the aforementioned defects. Summary of the Invention
[0007] The purpose of this invention is to provide a method for determining the mechanical properties of ferromagnetic materials based on electromagnetic nondestructive testing. By obtaining the mean and standard deviation of the mechanical properties of strip steel through a training dataset and setting an interval range, the method can determine the ferromagnetic material within a specific interval, thereby reducing the need for tensile testing.
[0008] The above-mentioned technical objective of the present invention is achieved through the following technical solution:
[0009] A method for determining the mechanical properties of ferromagnetic materials based on electromagnetic nondestructive testing includes the following steps:
[0010] S1. Electromagnetic nondestructive testing is performed on ferromagnetic materials to obtain their electromagnetic characteristics, and the PCA algorithm is used to screen out electromagnetic characteristics with large differences.
[0011] S2. Conduct destructive experiments on ferromagnetic materials to obtain their mechanical properties;
[0012] S3. Based on the electromagnetic characteristics and mechanical properties of ferromagnetic materials, establish a training dataset; calculate the mean and standard deviation of the mechanical properties based on the training dataset, and set the interval range = mean ± standard deviation;
[0013] S4. Construct a ridge regression model using electromagnetic characteristics as input and mechanical properties as output;
[0014] S5. Input the electromagnetic characteristics of the ferromagnetic material to be determined into the ridge regression model. If the predicted value output by the ridge regression model is within the range, the predicted value is taken as the true value of the mechanical properties. Otherwise, a destructive experiment is conducted to obtain the true value of the mechanical properties.
[0015] Furthermore, the specific method for step S1 is as follows:
[0016] S11. Apply periodic alternating magnetic field excitation to the material in the order of zero magnetic field excitation - positive saturated magnetic field excitation - zero magnetic field excitation - negative saturated magnetic field excitation - zero magnetic field excitation;
[0017] S12. The electromagnetic characteristics of the material are obtained by detecting the magnetization change curve of the material under the above-mentioned periodic alternating magnetic field excitation using a multi-magnetic parameter detection device.
[0018] Furthermore, in step S3, let the mean of the mechanical properties be E, and the standard deviation of the mechanical properties be σ, which are respectively obtained by the following formulas:
[0019]
[0020] In the formula: n represents the total number of samples, x i Let μ represent the mechanical property value of the i-th sample, and let μ represent the mean mechanical property value of the n samples.
[0021] Furthermore, in step S4, the input electromagnetic characteristic parameters include all types of electromagnetic characteristics, the square root of the electromagnetic characteristics, the thickness of the material, the lift-off of the material, and the tension of the material as inputs, and the output mechanical properties of the material include tensile strength, yield strength, and elongation.
[0022] Furthermore, the construction process of the ridge regression model is as follows:
[0023] In matrix X T Add a constant value λ to the diagonal elements of X, and the coefficients are calculated as follows:
[0024]
[0025] In the formula: X is the design matrix, containing the feature data of all samples; Y is the response variable vector; I is the identity matrix, with dimensions equal to X. T X is the same;
[0026] The cost function adds the L2 norm to the sum of squared residuals, shrinks the penalty term, and reduces the variance of the linear regression; the cost function J β (β) is:
[0027]
[0028] In the formula: y i X represents the observed value of the response variable for the i-th sample; i Let λ represent the feature value of the i-th sample; λ represent the regularization parameter; β represent the regression coefficient; and P represent the number of features.
[0029] Furthermore, the accuracy of the ridge regression model within the interval is evaluated using the error rate. With a confidence level > 90% within the interval, the error rate is defined as:
[0030]
[0031] Where m is the predicted value Y in the validation set. ci Compared with the true value Y i The number of values with an error ρ less than n%, where N is the total number of validation sets, which is equivalent to the total number of true values within the interval, n = {2.5, 5, 7.5, 10};
[0032] Then there is
[0033]
[0034] In summary, the present invention has the following beneficial effects:
[0035] The mechanical properties (tensile strength, yield strength, elongation, etc.) of materials are obtained through destructive experiments. Simultaneously, electromagnetic non-destructive testing (EMD) of ferromagnetic materials is performed using multi-magnetic detection equipment to obtain electromagnetic parameters characterizing the material's magnetic properties. A training dataset is created by combining the actual mechanical property values and electromagnetic parameters. The mean and standard deviation of the mechanical properties are obtained from the training dataset, and interval ranges are defined. Using the material's electromagnetic characteristic parameters as input and the material's mechanical properties as output, the dimensionality of the electromagnetic characteristics is reduced using the PCA algorithm to establish a ridge regression model. This enables the determination of ferromagnetic materials within specific intervals, reducing the need for destructive testing in the mechanical property determination process. Attached Figure Description
[0036] Figure 1 This is a flowchart illustrating the method for determining the mechanical properties of ferromagnetic materials based on electromagnetic nondestructive testing as described in this invention.
[0037] Figure 2 This is a schematic diagram of the ridge trace of the ridge regression model described in this invention. Detailed Implementation
[0038] To make the technical means, creative features, objectives and effects of this invention easier to understand, the invention will be further described below with reference to the figures and specific embodiments.
[0039] like Figure 1 As shown, the present invention proposes a method for determining the mechanical properties of ferromagnetic materials based on electromagnetic nondestructive testing, comprising the following steps:
[0040] First, during the strip steel production process, multi-magnetic detection equipment is used to perform electromagnetic non-destructive testing on the strip steel to obtain electromagnetic signals that characterize the reversible and irreversible motion of magnetic domains. At the same time, the corresponding electromagnetic characteristic parameters of the strip steel are defined and extracted.
[0041] Then, tensile specimens measuring 150mm*600mm were extracted from both ends of the sheared steel strip and subjected to destructive testing to obtain the material's mechanical properties. Combined with electromagnetic characteristic parameters, a training dataset was created. The mean and standard deviation of the mechanical properties were calculated from the training dataset, and the interval range was defined.
[0042] Finally, using the electromagnetic characteristic parameters of the strip as input and the material mechanical properties of the strip as output, a ridge regression model is established by combining the PCA algorithm.
[0043] When making predictions using the ridge regression model, the electromagnetic characteristics of the ferromagnetic material to be determined are input into the ridge regression model. If the predicted value output by the ridge regression model is within the range, the predicted value is taken as the true value of the mechanical properties; otherwise, a destructive experiment is conducted to obtain the true value of the mechanical properties.
[0044] Example
[0045] A method for determining the mechanical properties of ferromagnetic materials based on electromagnetic nondestructive testing includes the following steps:
[0046] Step 1) Electromagnetic nondestructive testing (NDT) is performed on different ferromagnetic steel materials using a multi-magnetic detection device to extract their electromagnetic characteristics. During testing, different alternating magnetic field excitations are applied to the ferromagnetic materials, starting from zero magnetic field excitation, progressing to positive saturation and back to zero magnetic field excitation, then increasing to negative saturation and back to zero magnetic field excitation. Throughout the entire repeated magnetization cycle, the magnetization process differs for different microstructures. The cumulative effect of magnetic domain movement leads to changes in the material's permeability, deepening the magnetization and ultimately causing changes in the overall magnetization curve. The signals obtained in this process can reflect the magnetic properties and microstructural characteristics of different ferromagnetic materials.
[0047] This embodiment selected 41 micro-electromagnetic features to characterize the magnetic parameters of cold-rolled steel. During the experiment, it was found that the material thickness, lift-off, and tension had a significant impact on the electromagnetic signal. Therefore, the input parameters of the ridge regression model were expanded to include 41 electromagnetic parameters, the square root of the 41 electromagnetic parameters, and thickness, lift-off, and tension, totaling 85 input parameters.
[0048] Step 2) Extract tensile specimens with dimensions of 150mm*600mm from both ends of the sheared strip and conduct destructive tests to obtain the material's mechanical properties.
[0049] Step 3) By repeating steps 1) and 2), the electromagnetic characteristics, thickness, lift-off, tension and mechanical properties of different ferromagnetic materials are obtained, a training dataset is created, and the existence of electromagnetic signal errors caused by unexpected factors in the production process is eliminated.
[0050] Step 4) Let the mean of the mechanical properties be E, and the standard deviation of the mechanical properties be σ. Based on the training dataset, calculate the values using the following formulas:
[0051]
[0052] In the formula: n represents the total number of samples, x i Let μ represent the mechanical property value of the i-th sample, and μ represent the mean mechanical property value of the n samples.
[0053] The defined interval range is E±σ.
[0054] Step 5) For electromagnetic features, use the PCA algorithm to filter out features with large differences and remove highly correlated features to reduce the interference of duplicate variables on the prediction results. Set the corresponding removed features to 0 to facilitate the subsequent creation of the coefficient table.
[0055] Step 6) The 41 electromagnetic characteristics obtained, plus the square root of the electromagnetic characteristics, thickness, lift-off, and tension, are used as inputs, and the mechanical properties of the ferromagnetic material are used as outputs. To solve the problem of multilinearity in the input parameters, a ridge regression model is established.
[0056] Ridge regression, compared to least squares, in matrix X T Add a constant value λ to the diagonal elements of X, and the coefficients are calculated as follows:
[0057]
[0058] In the formula: X is the design matrix, containing the feature data of all samples; Y is the response variable vector; I is the identity matrix, with dimensions equal to X. T X is the same.
[0059] The cost function adds the L2 norm to the sum of squared residuals, shrinks the penalty term, and reduces the variance of the linear regression; the cost function J β (β) is:
[0060]
[0061] In the formula: y i X represents the observed value of the response variable for the i-th sample; i Let λ represent the feature value of the i-th sample; λ represent the regularization parameter; β represent the regression coefficient; and P represent the number of features.
[0062] During the training of the ridge regression model, a suitable λ value is selected using a ridge trace plot, and the presence of multicollinearity among the variables is observed. For ridge trace plots of some electromagnetic features, such as... Figure 2 As shown, the ridge estimates of the regression coefficients are basically stable after λ = 1.5.
[0063] Step 7) The accuracy of the ridge regression model within the interval is evaluated using the error rate. The confidence level is set to >90% within the interval, and the error rate is defined as:
[0064]
[0065] Where m is the predicted value Y in the validation set. ci Compared with the true value Y i The number of values with an error ρ less than n%, where N is the total number of validation sets, which is equivalent to the total number of true values within the interval, n = {2.5, 5, 7.5, 10};
[0066] Then there is
[0067]
[0068] Step 8) Evaluate the predicted data in conjunction with the actual values, as shown in Table 1 below.
[0069] performance E (Expectation) Standard deviation (δ) Error rate (%) Percentage of all data (%) <![CDATA[ Rp ( Mpa )]]> 158.18 8.74 5.50 61.24 <![CDATA[Rm( Mpa )]]> 303.91 5.11 2.00 69.66 A(%) 45.40 1.49 3.00 71.91
[0070] Table 1 Evaluation Results
[0071] This embodiment provides a method for determining the mechanical properties of ferromagnetic materials based on electromagnetic nondestructive testing, thereby improving testing efficiency and reducing testing costs. The nondestructive testing of the mechanical properties (tensile strength, yield strength, elongation) of ferromagnetic steel materials has a performance prediction error of less than 6% under the condition that the confidence rate is greater than 90%.
[0072] In this document, the terms "upper," "lower," "front," "back," "left," "right," "top," "bottom," "inner," "outer," "vertical," and "horizontal," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only used for the clarity of expressing the technical solution and for the convenience of description, and therefore should not be construed as limiting the present invention.
[0073] In this document, the terms “comprising,” “including,” or any other variations thereof are intended to cover non-exclusive inclusion, which includes not only the elements listed but also other elements not expressly listed.
[0074] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the present invention as claimed. The scope of protection of this invention is defined by the appended claims and their equivalents.
Claims
1. A method for determining the mechanical properties of ferromagnetic material based on electromagnetic non-destructive testing, characterized in that, Includes the following steps: S1. Electromagnetic nondestructive testing is performed on ferromagnetic materials to obtain their electromagnetic characteristics, and the PCA algorithm is used to screen out electromagnetic characteristics with large differences. S2. Conduct destructive experiments on ferromagnetic materials to obtain their mechanical properties; S3. Establish a training dataset based on the electromagnetic characteristics and mechanical properties of ferromagnetic materials; The mean and standard deviation of the mechanical properties are calculated based on the training dataset, and the interval range is set as mean ± standard deviation. S4. Construct a ridge regression model using electromagnetic characteristics as input and mechanical properties as output; S5. Input the electromagnetic characteristics of the ferromagnetic material to be determined into the ridge regression model. If the predicted value output by the ridge regression model is within the range, the predicted value is taken as the true value of the mechanical properties. Otherwise, a destructive experiment is conducted to obtain the true value of the mechanical properties.
2. The electromagnetic non-destructive testing based method for determining mechanical properties of a steel strip according to claim 1, characterized in that, The specific method for step S1 is as follows: S11. Apply periodic alternating magnetic field excitation to the material in the order of zero magnetic field excitation - positive saturated magnetic field excitation - zero magnetic field excitation - negative saturated magnetic field excitation - zero magnetic field excitation; S12. The electromagnetic characteristics of the material are obtained by detecting the magnetization change curve of the material under the above-mentioned periodic alternating magnetic field excitation using a multi-magnetic parameter detection device.
3. The electromagnetic non-destructive testing based method for determining mechanical properties of a steel strip according to claim 1, characterized in that, In step S3, let the mean of the mechanical properties be E and the standard deviation of the mechanical properties be σ, which are respectively obtained by the following formulas: In the formula, n represents the total number of samples, x i represents the mechanical property value of the i-th sample, and μ represents the mechanical property mean value of the n samples.
4. The electromagnetic non-destructive testing based method for determining mechanical properties of a steel strip according to claim 1, characterized in that, In step S4, the input electromagnetic characteristic parameters include all types of electromagnetic characteristics, the square root of the electromagnetic characteristics, the thickness of the material, the lift-off of the material, and the tension of the material. The output mechanical properties of the material include tensile strength, yield strength, and elongation.
5. The electromagnetic non-destructive testing based method for determining mechanical properties of a steel strip according to claim 1, characterized in that, The ridge regression model is constructed as follows: In matrix X T Add a constant value λ on the diagonal elements of X, and the coefficient solution is: where: X is the design matrix containing the feature data for all samples; Y is the response variable vector; I is the identity matrix of the same dimension as X T X The cost function adds L2 norm on the basis of the residual sum of squares, shrinks the penalty term, and reduces the variance of linear regression; the cost function J β (b) is: where: y i represents the response variable observation of the i-th sample; X i represents the feature value of the i-th sample; λ represents the regularization parameter; β represents the regression coefficient; P represents the number of features.
6. The electromagnetic non-destructive testing based method for determining mechanical properties of a steel strip according to claim 5, characterized in that, The accuracy of the ridge regression model within the interval is evaluated using the error rate. With a confidence level > 90% within the interval, the error rate is defined as: wherein m is the predicted value Y in the validation set ci the number of errors p between the predicted value Y i and the true value Y less than n%, N is the total number of the validation set, which is equivalent to the total amount of true values in the interval range, n = {2.5, 5, 7.5, 10}; Then there is