Method and system for testing mechanical properties of iso standard oriented ceramic orthopedic products
By processing three-dimensional tomographic images of ceramic orthopedic implants and applying continuous loading, quantitative analysis and localization of internal defects were achieved, solving the problem that existing technologies could not establish the relationship between defects and critical fracture loads, and improving the accuracy and reliability of the test.
Patent Information
- Application Number
- CN202611363304.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-04
- Publication Date
- 2026-11-24
AI Technical Summary
Existing technologies cannot locate and quantify internal defects in ceramic orthopedic products, nor can they establish a quantitative relationship between defects and critical fracture loads. This results in test data lacking specificity and failing to provide a reliable basis for defining product safety boundaries.
By acquiring three-dimensional tomographic images of ceramic orthopedic implants, voxel analysis and noise reduction are performed to distinguish between pore and crack regions. Curvature calculation and fitting are then carried out. Combined with continuously increasing loading and stress state data, the displacement of the crack tip is tracked, the critical fracture load at the moment of penetrating fracture is extracted, and a quantitative correspondence between defect size and critical fracture load is established.
It enables precise classification and spatial localization of internal defects in ceramic orthopedic products, establishes the correlation between internal damage evolution and macroscopic mechanical failure, provides reliable mechanical performance test reports and auxiliary analysis basis, and improves the accuracy and reliability of testing.
Smart Images

Figure CN123155349A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of mechanical performance testing technology for ceramic orthopedic products, and in particular to a method and system for testing the mechanical performance of ceramic orthopedic products in accordance with ISO standards. Background Technology
[0002] Ceramic materials occupy an irreplaceable position in the field of orthopedic implants due to their excellent biocompatibility and wear resistance. In the process of evaluating the mechanical properties of implants, mechanical sensors, as the core devices for collecting mechanical load and displacement signals, directly determine the reliability of test data based on their measurement accuracy.
[0003] Currently, the industry's assessment of the mechanical properties of ceramic orthopedic products mainly relies on macroscopic loading tests conducted by deploying mechanical sensors on the surface of the entire sample, treating the product as a homogeneous, ideal, and defect-free whole. However, micropores and grain boundary microcracks inevitably form within ceramic materials during the sintering process. These internal defects become stress concentration points when loads are applied, eventually developing into the initiation points of macroscopic fracture. The overall fracture load and failure mode of the product are actually dominated by the size, location, and propagation behavior of these internal defects during the stress process. Existing macroscopic testing procedures do not distinguish between samples containing specific defects and defect-free samples, nor can they establish a correspondence between defect size and critical fracture load. This results in test data lacking specificity and failing to provide a reliable basis for defining the product's safety boundaries.
[0004] In summary, existing technologies have the problem of being unable to locate and quantify internal defects in ceramic orthopedic products and establish a quantitative relationship between them and critical fracture loads. Summary of the Invention
[0005] This invention provides a method and system for testing the mechanical properties of ceramic orthopedic products in accordance with ISO standards, in order to solve the problem in the prior art that it is impossible to locate and quantify the internal defects of ceramic orthopedic products and establish a quantitative relationship between them and the critical fracture load.
[0006] Firstly, to address the aforementioned technical problems, this invention provides a method for testing the mechanical properties of ceramic orthopedic products conforming to ISO standards, comprising: A three-dimensional tomographic image of the target ceramic orthopedic implant is acquired, and the three-dimensional tomographic image is subjected to voxel analysis and noise reduction processing to obtain internal defect features. The curvature of the internal defect features is calculated to distinguish between the pore region and the crack region. The pore region is fitted with a spherical surface to obtain the micropore size. The crack region is fitted with a trajectory to obtain the grain boundary crack position. The micropore size and the grain boundary crack position are mapped with coordinates to obtain the defect location information. The defect location information is then archived and bound. The target ceramic orthopedic implant is subjected to continuous incremental loading according to a preset loading mode, and stress state data is collected simultaneously. The stress state data is combined with the defect location information to identify crack tips and track displacement to obtain damage distribution data. The damage distribution data of each loading step is tracked to obtain the geometric morphology evolution trajectory. The connectivity analysis of the geometric morphology evolution trajectory is performed to obtain the defect propagation path. The critical fracture load at the moment of penetrating fracture is extracted based on the defect propagation path. Mechanical performance indicators are calculated based on the critical fracture load and the preset sample specifications. The mechanical performance indicators are compared with the preset mechanical performance thresholds to generate a mechanical performance test report. The defect location information, the defect propagation path, and the mechanical performance test report are associated and stored.
[0007] Secondly, the present invention provides a mechanical performance testing system for ceramic orthopedic products oriented towards ISO standards, comprising: a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the program to implement the mechanical performance testing method for ceramic orthopedic products oriented towards ISO standards as described above.
[0008] Compared with the prior art, the present invention has the following beneficial effects: (1) This invention obtains internal defect features by acquiring three-dimensional tomographic images, performing voxel analysis and noise reduction, calculating the curvature of the defect features to distinguish between pores and cracks, and fitting quantization and coordinate mapping to obtain defect location information. On this basis, continuously increasing load is applied according to the ISO standard loading mode and the displacement of crack tip and damage evolution are tracked to obtain the defect propagation path. Then, the critical fracture load at the moment of penetrating fracture is extracted, and a quantitative correspondence between the internal defect size and critical fracture load of ceramic orthopedic products is established, which solves the problem that the existing technology cannot correlate internal damage evolution with macroscopic mechanical failure.
[0009] (2) This invention extracts the geometric curvature tensor by performing principal component analysis on the internal defect features, distinguishes the pore region from the crack region by using the ratio of the first principal curvature to the second principal curvature, and uses spherical fitting and polynomial trajectory fitting for quantitative description, thereby realizing the accurate classification and spatial positioning of different types of defects inside ceramics and improving the accuracy of defect characterization.
[0010] (3) By associating and storing defect location information, defect propagation path and mechanical performance test report, this invention constructs a coupled data matrix of internal damage evolution and mechanical failure, which provides a traceable auxiliary analysis basis for subsequent ceramic material formulation improvement and sintering process optimization, and the storage process is independent of the qualification judgment process. Attached Figure Description
[0011] Figure 1 This is a flowchart illustrating a method for testing the mechanical properties of ceramic orthopedic products according to ISO standards, provided as an embodiment of the present invention. Detailed Implementation
[0012] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0013] Reference Figure 1 The first embodiment of the present invention provides a method for testing the mechanical properties of ceramic orthopedic products according to ISO standards, including the following steps: S11, acquire a three-dimensional tomographic image of the target ceramic orthopedic implant, perform voxel analysis and noise reduction on the three-dimensional tomographic image to obtain internal defect features; S12, perform curvature calculation on the internal defect features, distinguish between pore regions and crack regions, perform spherical fitting on the pore regions to obtain the micropore size, perform trajectory fitting on the crack regions to obtain the grain boundary crack position, perform coordinate mapping between the micropore size and the grain boundary crack position to obtain defect location information, and archive and bind the defect location information. S13, apply continuous incremental loading to the target ceramic orthopedic implant according to a preset loading mode, simultaneously collect stress state data, combine the defect location information to identify crack tips and track displacement of the stress state data to obtain damage distribution data, perform evolution tracking of the damage distribution data of each loading step to obtain geometric morphology evolution trajectory, and perform connectivity analysis of the geometric morphology evolution trajectory to obtain defect propagation path. S14. Extract the critical fracture load at the moment of penetrating fracture based on the defect propagation path, calculate the mechanical performance index based on the critical fracture load and the preset sample specifications, compare the mechanical performance index with the preset mechanical performance threshold to generate a mechanical performance test report, and associate and store the defect location information, the defect propagation path and the mechanical performance test report.
[0014] In step S11, the three-dimensional tomographic image is subjected to voxel analysis and noise reduction processing to obtain internal defect features, including: The initial voxel grayscale matrix is obtained by analyzing the three-dimensional tomographic image; The initial voxel grayscale matrix is decomposed to obtain high-frequency noise components and low-frequency structural components; The low-frequency structural components are processed by a convolutional neural network to obtain a multi-scale feature map; If the gradient of the multi-scale feature map is greater than a preset threshold, the multi-scale feature map is fused with the high-frequency noise component to obtain a denoising feature tensor. If the gradient of the multi-scale feature map is less than or equal to the preset threshold, the original voxel value of the multi-scale feature map is retained as the value of the corresponding position in the denoising feature tensor. Clustering the denoised feature tensor yields morphologically connected regions, and the boundary coordinates of these regions are extracted to obtain internal defect features.
[0015] It should be noted that, for the target ceramic orthopedic implant, images of its internal structure were acquired using a micro-computed tomography (CT) scanner. The scanning resolution was set to 512×512×512 voxels, with each voxel corresponding to a spatial size of 20μm×20μm×20μm. This resolution was chosen because the critical micropore size to be detected inside the ceramic orthopedic implant is approximately 15μm to 60μm, and a voxel resolution of 20μm satisfies the Nyquist sampling theorem's requirement that the minimum resolvable feature size is twice the voxel size, i.e., 40μm. The scanned image data was analyzed layer by layer, and the X-ray attenuation coefficient of each spatial voxel was extracted and mapped to a grayscale value range of 0 to 255 to construct a three-dimensional initial voxel grayscale matrix. The grayscale value directly reflects the density distribution of the ceramic material at different spatial locations; high grayscale values correspond to dense ceramic matrix regions, while low grayscale values correspond to porous or loose regions. For example, using alumina ceramic femoral head as the scanning object, the scanning voltage was set to 90kV, the scanning current was set to 200μA, and the single scan exposure time was 800ms. In the obtained initial voxel grayscale matrix, the grayscale values of the dense ceramic matrix were concentrated in the range of 200 to 240, while the grayscale values of the internal microporous region were distributed in the range of 30 to 80. The grain boundary microcrack region showed a transition zone of sudden drop and rebound in grayscale value due to its narrow geometric characteristics.
[0016] It should be noted that wavelet transform is used to perform multi-scale decomposition of the initial voxel grayscale matrix. The approximation coefficients are reconstructed to obtain the low-frequency structural components, and the detail coefficients are reconstructed to obtain the high-frequency noise components. The wavelet basis functions chosen have high-order vanishing moments, which effectively capture the singularity characteristics of the defect boundaries within the ceramic. The selection of the decomposition level ensures that the voxel size of the low-frequency structural components obtained after decomposition is exactly larger than the maximum micropore size. This preserves the pore structure information in the low-frequency components without decomposing it to high-frequency details. The high-frequency detail information of the pore boundaries is carried by the high-frequency noise components and recovered in subsequent fusion steps. The low-frequency structural components retain the main framework of the ceramic material, the macroscopic pore contour, and large-scale density gradient information, while the high-frequency noise components contain interfering high-frequency signals such as tiny impurity particles, local density abrupt changes at grain boundaries, and equipment scanning artifacts. This decomposition process effectively separates the essential geometric information of defects from random noise. For example, a three-level wavelet decomposition is performed on the grayscale matrix of 512×512×512 voxels, reducing the voxel size of the low-frequency structural components to 128×128×128. Each voxel corresponds to a spatial size of 80μm, which is just larger than the maximum micropore size of 60μm to be detected. This ensures that the overall pore outline is preserved in the low-frequency components, while avoiding excessive downsampling that would cause the pore details to be averaged.
[0017] It should be noted that the low-frequency structural components are input into a convolutional neural network for feature extraction. This network employs a three-dimensional convolutional encoder structure, consisting of three cascaded feature extraction layers. Each feature extraction layer contains two 3×3×3 convolutional layers, a batch normalization layer, and a modified linear unit activation layer. Adjacent layers are downsampled through convolutional operations with a stride of 2. The number of output channels for the three layers is set to 32, 64, and 128, respectively. The input 128×128×128 low-frequency structural components, after passing through the three feature extraction layers, correspond to half, one-quarter, and one-eighth of the spatial resolution of the original image, respectively. The large-scale feature maps preserve global structural information, while the small-scale feature maps focus on the edge texture features of local micro-cracks. The training dataset for the convolutional neural network contains 500 sets of labeled CT scan voxel data of ceramic orthopedic implants. Each set of data underwent wavelet decomposition preprocessing to extract low-frequency structural components. Professional materials inspectors then performed voxel-by-voxel annotation of the true boundaries of internal pores and microcracks. Annotation consistency was evaluated using the Cohen's Kappa coefficient, with a value greater than 0.85. During training, a standard classification loss function and gradient optimization method were used, with an initial learning rate set to 1×10⁻⁶. -4 The batch size was set to 8, and training was iterated until the loss function converged to less than 0.05.
[0018] It should be noted that the spatial gradient magnitude of each voxel in the multi-scale feature map is calculated, with a preset gradient threshold of 50. The gradient threshold of 50 is determined by statistically analyzing the gradient magnitudes of defect edge voxels and non-edge voxels in 500 training datasets. The median gradient magnitude of defect edge voxels is approximately 78, while the median gradient magnitude of smooth background voxels is approximately 18. The threshold of 50 is taken as the optimal Bayesian decision boundary for both distributions. When the calculated gradient magnitude of a voxel is greater than 50, it indicates a significant density abrupt change boundary at that location, most likely corresponding to the edge of a microcrack rather than a smooth background region. In this case, the activation value of that voxel in the multi-scale feature map is weighted and fused with the corresponding position in the high-frequency noise component. The fusion weights are calculated through a gated fusion module. This module first concatenates the multi-scale feature map with the high-frequency noise component along the channel dimension. The concatenated feature is then input into a 1×1×1 convolutional layer for voxel-by-voxel linear transformation, resulting in a single-channel weight response map. The weight response map is then normalized to the 0-1 range using a Sigmoid activation function, outputting normalized fusion coefficients. The fusion output is obtained by adding the product of the normalized fusion coefficient and the high-frequency noise component, and the product of 1 minus the coefficient and the multi-scale feature map. This automatically assigns higher weights to high-frequency noise components at locations with larger gradient magnitudes, thus suppressing random noise signals while preserving the high-frequency structural information of the true crack edges, outputting a denoised feature tensor. When the gradient magnitude is less than or equal to 50, the voxel is considered a smooth background region, requiring no high-frequency detail enhancement; its original voxel value is directly retained in the multi-scale feature map as the corresponding component of the denoised feature tensor. The training of the weighted fusion coefficients is performed jointly with the convolutional neural network, sharing the same loss function and optimizer configuration.
[0019] It should be noted that, based on the feature vectors of each voxel in the denoising feature tensor, density clustering is used to group and cluster anomalous voxels that are close in distance in the feature space. The clustering neighborhood radius is set to 3 voxel units, and the minimum number of neighborhood voxels is set to 10. The neighborhood radius of 3 is selected based on the fact that the minimum size of a single micropore is approximately 15 μm, or about 0.75 voxels, and the gray-scale transition band of defect edge voxels typically occupies 2 to 3 voxel widths. A neighborhood radius of 3 ensures that adjacent defect voxels are included in the same cluster across the transition band. The minimum number of neighborhood voxels of 10 is used to exclude false defect clusters formed by residual isolated noise points. After clustering is completed, boundary voxels are extracted along the outer surface of each cluster, and the three-dimensional coordinates (X, Y, Z) of each boundary voxel in the scanning coordinate system are recorded to form a set of boundary coordinates of the morphologically connected region. This set of boundary coordinates is the internal defect feature, including the three-dimensional geometric contour information of each independent defect. For example, after performing the above treatment on an alumina ceramic femoral head sample, seven independent defect regions were detected inside, three of which were identified as near-spherical pores and four as lamellar grain boundary cracks.
[0020] In step S12, the curvature of the internal defect features is calculated to distinguish between the porosity region and the crack region, including: Principal component analysis is performed on the internal defect features to obtain a geometric curvature tensor, which includes a first principal curvature and a second principal curvature. If the ratio of the first principal curvature to the second principal curvature is less than a preset curvature ratio threshold and both the first principal curvature and the second principal curvature are greater than a preset minimum curvature threshold, then the corresponding voxel region is determined to be a pore region. If the ratio of the first principal curvature to the second principal curvature is greater than or equal to the preset curvature ratio threshold, the corresponding voxel region is determined to be a crack region.
[0021] It should be noted that the boundary coordinate set of each defect region is extracted as the input point cloud data. For each boundary voxel point and its neighboring voxels in its spatial neighborhood, a 3×3 covariance matrix is first constructed. The matrix elements are the coordinate covariances of all voxels in the neighborhood in the X, Y, and Z directions. Eigenvalue decomposition is performed on the covariance matrix to obtain three eigenvalues and their corresponding eigenvectors. The eigenvector corresponding to the smallest eigenvalue is used as the local surface normal vector at that point, and the eigenvectors corresponding to the largest and second largest eigenvalues span the local tangent plane at that point. Subsequently, within this local tangent plane, a quadratic surface z=a is fitted to the neighboring voxels using the moving least squares method. x x 2 +a y y 2 +a xy xy+b x x+b y Let y+c be a 2×2 curvature tensor at the point y+c, constructed from the second-order partial derivatives of the quadratic surface. Eigenvalue decomposition of this curvature tensor yields two eigenvalues and their corresponding eigenvectors. Since the eigenvalues of the curvature tensor have the dimension of the reciprocal of length, i.e., μm... -1 The physical meaning of κ1 is the degree of curvature of the surface at that point along the corresponding principal direction. Therefore, the two eigenvalues are taken as the first principal curvature κ1 and the second principal curvature κ2, respectively, and their corresponding eigenvectors are the directions of the first principal curvature and the second principal curvature. The geometric curvature tensor is composed of the first principal curvature κ1, the second principal curvature κ2, and their direction vectors.
[0022] It should be noted that the preset curvature ratio threshold is set to 10, and the preset minimum curvature threshold is set to 0.5. When the ratio κ1 / κ2 of the first principal curvature κ1 to the second principal curvature κ2 of a voxel point is less than 10, and the values of κ1 and κ2 are both greater than 0.5, it indicates that the local surface at that voxel point has similar curvature in all directions, that is, it exhibits approximately isotropic curved surface characteristics, which conforms to the geometric morphological characteristics of pore-type defects. In this case, the connected region where the voxel point is located is determined to be a pore region.
[0023] The preset curvature ratio threshold of 10 was set based on the following: Statistical analysis of the curvature ratio distribution of 120 labeled defect samples showed that the κ1 / κ2 values of porosity defects were concentrated in the range of 1.2 to 7.8, while those of crack defects were concentrated in the range of 15 to 240. Threshold 10 effectively separated these two distributions, achieving a classification accuracy of 96.7%. The 120 labeled defect samples were obtained from systematic CT scans of five different batches of alumina and zirconia ceramic orthopedic implants. The gold standard for defects was determined by the majority consensus of three independent material testing experts. The preset minimum curvature threshold was 0.02 μm. -1 The settings are used to exclude flat, spurious defect boundaries caused by scanning noise. For micropores and grain boundary cracks of engineering significance within ceramic orthopedic implants, the minimum reliable detection size is approximately 40 μm (equivalent to 2 voxels), corresponding to a minimum radius of curvature of approximately 20 μm and a principal curvature value of approximately 1 / 20 μm = 0.05 μm. -1 The threshold is set at the minimum engineering defect curvature value of 0.05μm. -1 40%, or 0.02μm -1 The aim is to exclude curvature values below 0.02 μm caused by scanning noise. -1 It creates flat, spurious defect boundaries while preserving the curvature characteristics of real defects.
[0024] It should be noted that when the ratio of the first principal curvature κ1 to the second principal curvature κ2 of a voxel point is greater than or equal to 10, it indicates that the voxel point has a much greater degree of curvature in one direction than in the other, exhibiting obvious anisotropic geometric characteristics, consistent with the morphological characteristics of a crack extending narrowly in a single direction. In this case, the connected region where the voxel point is located is identified as a crack region. For example, in the analysis of the above-mentioned alumina ceramic femoral head sample, among the seven internal defects detected, three regions had κ1 / κ2 ratios between 2.3 and 5.1, with both κ1 and κ2 greater than 0.5, and were identified as porosity regions; four regions had κ1 / κ2 ratios between 19 and 87, and were identified as crack regions.
[0025] In one implementation, spherical fitting is performed on the porous region to obtain the micropore size, trajectory fitting is performed on the crack region to obtain the grain boundary crack location, and coordinate mapping is performed on the micropore size and the grain boundary crack location to obtain defect location information, including: The radius value is obtained by performing least-squares spherical fitting on the pore region, and the radius value is used as the micropore size; Extract the skeleton center point from the crack region, perform polynomial trajectory fitting on the skeleton center point to obtain a space curve equation, and use the space curve equation as the location of the grain boundary crack. The defect location information is obtained by performing an affine transformation coordinate mapping between the size of the micropores and the location of the grain boundary cracks.
[0026] It should be noted that, for the set of voxels identified as porous regions, the set of three-dimensional coordinate points of their boundaries is extracted as the fitting input data, and a spherical objective function F=∑[(X i -X0) 2 +(Y i -Y0) 2 +(Z i -Z0) 2 -R 2 ] 2 , where (X) i ,Y i Z i Let (X0, Y0, Z0) be the voxel coordinates of the pore boundary, (X0, Y0, Z0) be the coordinates of the center of the sphere to be solved, and R be the radius of the sphere to be solved. The objective function is minimized through iterative optimization to find the optimal sphere's center coordinates (X0, Y0, Z0) and radius R. The obtained radius R is taken as the characteristic size of this micropore. The convergence condition for iterative optimization is set to the change in the objective function value being less than 1 × 10⁻⁶. -6 Or, if the number of iterations reaches 500, the convergence threshold is less than the voxel volume of 20 μm. 3 The fluctuation of the equivalent objective function corresponding to the grayscale change ensures that the fitting accuracy is not affected by numerical truncation error. For example, after performing spherical fitting on the three pore regions in the above sample, the output pore radii are 26μm, 41μm and 28μm, respectively, and the root mean square error of the fitting residuals is less than 3μm.
[0027] It should be noted that for the set of voxels identified as crack regions, the central skeleton line of the crack region is extracted by iteratively stripping boundary voxels. The refinement iteration removes boundary voxels in six directions (north, south, east, west, top, and bottom) each time, stopping when no more voxels can be removed. All voxel points on the skeleton line are extracted as discrete sampling points, and a cubic polynomial is used to fit the spatial curve of the skeleton points to establish parametric equations. X(s) = ax0 +a x1 s+a x2 s 2 +a x3 s 3 ; Y(s)=a y0 +a y1 s+a y2 s 2 +a y3 s 3 ; Z(s) = a z0 +a z1 s+a z2 s 2 +a z3 s 3 ; Where parameter s is the normalized arc length parameter along the crack length direction, and its value ranges from 0 to 1, a x0 a x1 a x2 The polynomial coefficients were obtained using the least squares method. The cubic polynomial was chosen because the crack propagation path at ceramic grain boundaries typically exhibits a smooth, curved characteristic; a cubic order can adequately capture the curvature of the crack without overfitting local minor perturbations. The output spatial curve equation represents the specific propagation location and orientation of the grain boundary crack. For example, after processing the four crack regions in the above sample, four spatial curves were obtained, with crack lengths ranging from 45 μm to 180 μm. The coefficient of determination R0 for the fitted curves was... 2 All are greater than 0.95.
[0028] It should be noted that an affine transformation matrix is established by mapping the local defect coordinates to the global standard physical coordinate system of the ceramic orthopedic implant. The affine transformation matrix contains a 3×3 rotation component and a 3×1 translation component. The matrix parameters are obtained through the following calibration procedure: Six non-coplanar reference points are selected on the implant surface. The selection principle for these six points is that at least three points are distributed on the upper surface of the implant and at least three points are distributed on the lower surface, ensuring complete constraint of the six degrees of freedom of rotation and translation. The coordinates (X, Y, X) in the local scan coordinate system are recorded. s ,Y s Z s ) and coordinates in the global physical coordinate system (X p ,Y p Z pThe rotation and translation components are solved using the least squares method. For pore defects, the fitted sphere center coordinates and radius values are subjected to affine transformations to obtain the sphere center coordinates and dimensions in the global coordinate system. For crack defects, the control point coordinates of the spatial curve equation are subjected to affine transformations to obtain the crack path equation in the global coordinate system. The final output defect location information includes the type identifier, global physical coordinates, and size parameters for each defect. For example, the root mean square error of the coordinate mapping residuals of the six reference markers during the calibration process is 15 μm, which is less than the spatial resolution of a single voxel (20 μm), meeting the defect location accuracy requirements.
[0029] In one implementation, the step of filing and binding the defect location information includes: The coordinate values and size parameters extracted from the defect location information are concatenated to obtain a text sequence; The text sequence is hashed and encrypted to obtain a unique identification hash value; The defect location information is associated with the unique identification hash value and stored to obtain an initial internal state record, thus completing the filing and binding.
[0030] It should be noted that the type identifier, global physical coordinates (X,Y,Z), and size parameters of each defect are extracted sequentially from the structured data of defect location information. The strings are then concatenated in the format of "type_coordinate X_coordinate Y_coordinate Z_size", with multiple defects separated by semicolons, to generate a text sequence containing all defect information. For example, for a sample containing 7 defects, the generated text sequence is "P_12.5_34.2_8.1_22;P_15.3_28.7_10.2_41;P_9.8_41.5_6.3_28;C_18.2_22.1_11.5_78;C_25.4_16.8_13.2_135;C_30.1_19.3_7.8_45;C_33.7_24.6_9.4_180", where P represents porosity, C represents crack, and the last digit is the size value in μm.
[0031] It should be noted that the concatenated text sequence is used as input, and a hash encryption method is used for one-way encryption, outputting a fixed-length hash value. This hash value is unique and irreversible; any tiny change to the input text sequence will cause a significant change in the output hash value. Therefore, each sample with a different internal defect state will generate a globally unique hash identifier. For example, the text sequence of the above 7 defect samples, after hash encryption, outputs a 64-bit hexadecimal hash value, which serves as the digital fingerprint of the sample's internal defect state.
[0032] It should be noted that a relational database table structure is established, named "specimen_defect_record", containing fields: the specimen number as a VARCHAR primary key, the hash value as a CHAR type with a length of 64 characters, the defect location information as JSONB type storing complete structured data, and the record creation timestamp as TIMESTAMP type. The complete defect location information data, along with the unique identification hash value, is written to this database table, using the specimen number as the retrieval primary key, completing the initial internal state documentation and binding for this ceramic orthopedic implant. The database engine uses a relational database that supports transactional consistency and row-level locking, and the data persistence storage path is configured with a redundant disk array to ensure data security.
[0033] In step S13, the target ceramic orthopedic implant is subjected to a continuously increasing load according to a preset loading mode, while simultaneously collecting stress state data. It should be noted that the preset loading mode is set according to the mechanical testing specifications for ceramic orthopedic implants specified in ISO 6474-1. For the sample specifications of the target ceramic orthopedic implant, its geometric dimensional parameters are extracted as input data, and the initial contact preload is set to 20N, with a maximum breaking load threshold of 5000N. The total loading interval is divided into 100 equidistant loading steps, generating a continuously increasing loading sequence with a step size of 50N. A servo hydraulic actuation cylinder applies axial compression loading to the implant according to this loading sequence at a loading rate of 500N / s. During loading, a piezoelectric mechanical sensor located at the bottom of the loading head collects mechanical response signals in real time at a sampling frequency of 2000Hz. The selection of the 2000Hz sampling frequency ensures that 40 data points are collected within each 50N loading step, meeting the data density requirements. Simultaneously, a grating ruler displacement sensor mounted on the side wall synchronously acquires deformation displacement signals with a displacement resolution of 1 μm. Cross-correlation analysis is used to calculate the time delay between the two sets of signals, and translation compensation is applied to the two sets of signals based on this time delay to achieve time-domain synchronization. The aligned force and displacement values are then mapped and stitched together point-by-point to output a load-displacement response sequence. This sequence is then combined with the loaded cross-sectional area to calculate the principal stresses σ1, σ2, and σ3, and the shear stress τ. 12 τ 23 τ 31 Numerical force state data.
[0034] It should be noted that an in-situ micro-computed tomography loading system was used to acquire voxel images during the loading process described above. This system integrates a servo-hydraulic loading device within the CT scanning cavity, with the loading axis arranged perpendicular to the CT scanning plane. After each loading step and before the next, a rapid CT scan of the sample is performed, with a single scan time of 45 seconds. The scanning parameters remain consistent with the initial scan in step S11. The voxel images obtained from each loading step provide the necessary sequence of grayscale data for displacement tracking.
[0035] In one implementation, the step of combining the defect location information to perform crack tip identification and displacement tracking on the stress state data to obtain damage distribution data includes: The stress concentration degree of each node is calculated by comparing the principal stress values in the stress state data with the defect coordinates in the defect location information. If the stress concentration exceeds a preset stress concentration threshold, the corresponding node will be marked as a crack tip. The strain components are obtained by performing digital image correlation displacement tracking on the crack tip; Equivalent strain calculation is performed on the strain components, and voxels whose equivalent strain exceeds a preset strain threshold are marked as damaged voxels to obtain damage distribution data.
[0036] It should be noted that the coordinates of the pore center and the crack skeleton nodes, contained in the defect location information, are imported into the finite element mesh model to construct a local stress analysis coordinate system at the defect boundary nodes. For each defect boundary node, the maximum principal stress along the crack tip opening direction at that node under the current loading step is extracted as the local stress value σ. loc Simultaneously calculate the average stress σ of the matrix. far The local stress value σ loc With the average stress σ of the matrix far The ratio of these values is used as the stress concentration factor K at that node. t =σ loc / σ far The stress concentration factor represents the degree of stress concentration at that node. The average stress σ of the matrix... far The average principal stress in a homogeneous ceramic matrix unit that is at least 10 times the average grain size (50 μm) away from any defect boundary under the current loading step is selected. This distance ensures that the selected unit is located outside the defect stress disturbance zone, and its stress state is not affected by the local stress concentration of the defect.
[0037] It should be noted that the preset stress concentration threshold is set to 3. When the stress concentration at a defect edge node is greater than 3, the node is considered to have reached the critical condition for crack initiation and propagation, and its coordinates are marked as a crack tip. Otherwise, the node is considered not to have reached the critical condition for crack initiation, is not marked as a crack tip, and its stress concentration is continuously monitored in subsequent loading steps. The preset stress concentration threshold is determined by preparing 100 sets of ceramic standard specimens containing pre-existing cracks, using a step-by-step loading method, and simultaneously recording the stress concentration at the defect tip of each specimen after each loading step. CT scans are then used to determine whether crack initiation has occurred in that loading step. The criterion for crack initiation is that in three consecutive loading steps, a connected dark region with a size of not less than 5 voxels first appears in the same defect region, and this connected region continues to expand in subsequent loading steps; in this case, the loading step is marked as the crack initiation moment. A binary logistic regression analysis was performed on the experimental data, with crack initiation as the dependent variable and stress concentration as the independent variable. The crack initiation probability curve was obtained by fitting the curve, and the stress concentration level corresponding to a crack initiation probability of 50% was taken as the preset stress concentration level threshold.
[0038] It should be noted that within each loading step of the continuously increasing loading sequence, a reference sub-region of 100μm×100μm×100μm is selected around the crack tip with a tracking step size of 50μm. Digital image correlation is used to perform cross-correlation matching on the voxel grayscale distribution of this sub-region obtained in each loading step. The cross-correlation matching employs a frequency domain cross-correlation algorithm based on Fast Fourier Transform (FFT). The normalized cross-correlation operation between the reference sub-region and the search window is performed point-by-point in the frequency domain using Fourier transform, thus reducing the computational cost of the three-dimensional cross-correlation operation. To obtain a sub-voxel displacement accuracy of 0.01 voxels, cubic spline interpolation is used to perform sub-voxel interpolation on the grayscale distribution around the cross-correlation peak. The sub-voxel-level peak position is located by fitting the analytical expression of the cross-correlation peak surface. The deformation assumption for the sub-region adopts a first-order affine deformation mapping function, which assumes that the displacement field within the sub-region is linearly distributed. For a 100μm×100μm×100μm sub-region, linear mapping is sufficient to describe its deformation under micrometer-level displacement. The natural gray-level gradient characteristics of grain boundaries and micropores within the ceramic material provide the equivalent speckle pattern required for displacement tracking. The gray-level gradient generated by density changes at grain boundaries is approximately 15 to 25 gray levels / voxel, satisfying the basic requirement for gray-level contrast in cross-correlation matching. By comparing the gray-level distribution function of the reference sub-region between the current load step and the previous load step, the displacement components u of each voxel point within the sub-region in the X, Y, and Z directions are calculated. x u y u z Further differential calculations of the displacement field yielded six strain components ε. xx ε yy εzz γ xy γ yz γ zx The search window size for cross-correlation matching is set to 21×21×21 voxels, the sub-voxel interpolation accuracy is 0.01 voxels, the matching criterion uses a normalized cross-correlation function, and the correlation coefficient threshold is set to 0.8. When the correlation coefficient is lower than 0.8, the tracking step size is adaptively halved to 25 μm and rematching is performed.
[0039] It should be noted that the six strain components ε xx ε yy ε zz γ xy γ yz γ zx Calculate the von Mises equivalent strain. First, calculate the mean normal strain ε. m =(ε xx +ε yy +ε zz ) / 3, subtract the average normal strain from each normal strain component to obtain the normal strain component e of the strain deviator tensor. xx =ε xx -ε m e yy =ε yy -ε m e zz =ε zz -ε m The shear strain deviator component is equal to the corresponding shear strain component, i.e., e xy =γ xy / 2、e yz =γ yz / 2、e zx =γ zx / 2. Then, the von Mises equivalent strain ε is calculated from the six independent components of the strain deviator tensor. eq =(2 / 3×e ij ×e ij ) 1 / 2 Where i and j are subscripts and satisfy Einstein's summation convention, e ij ×e ij This represents the sum of squares over six independent partial components, expanded using tensor symmetry to e. xx 2 +e yy 2 +e zz 2 +2e xy 2 +2e yz 2 +2e zx 2The preset strain threshold is set to 0.5%, which is 5 × 10⁻⁶. -3 The threshold is determined based on the following: the elastic limit strain of alumina ceramic materials is approximately 0.1%, while the critical strain point for microcrack initiation is approximately 5 times the elastic limit, i.e., 0.5%. Exceeding this value indicates that the material has transitioned from elastic deformation to the microcrack initiation and propagation stage. When the equivalent strain calculated for a voxel exceeds 0.5%, the voxel is marked as a damaged voxel; when the equivalent strain calculated for a voxel is less than or equal to 0.5%, the voxel is determined to have not yet entered the microcrack initiation stage and is marked as a non-damaged voxel. For all voxels within a spherical neighborhood centered on the crack tip node with a radius of 5 voxels (100 μm), equivalent strain calculation and threshold determination are performed voxel by voxel, resulting in a binary three-dimensional voxel array containing damaged and non-damaged voxels. This array represents the damage distribution data for that loading step. By traversing all loading steps, the damage distribution data sequence for each loading step is obtained, where 1 represents a damaged voxel and 0 represents a non-damaged voxel.
[0040] In one implementation, the step of performing evolutionary tracking on the damage distribution data at each loading step to obtain a geometric morphology evolution trajectory, and performing connectivity analysis on the geometric morphology evolution trajectory to obtain a defect propagation path, includes: The damage distribution data of each loading step is labeled with voxel connected components to obtain the set of connected regions of each loading step. The set of connected regions in adjacent loading steps is morphologically compared, and the expansion and merging changes of the connected regions are tracked to obtain the geometric morphological evolution trajectory. The connected regions in the geometric evolution trajectory are abstracted as graph structure nodes, and the shortest path is calculated on the graph structure nodes to obtain the defect expansion path.
[0041] It should be noted that the damage distribution data for each loading step is labeled with connected components using the 26-neighborhood connectivity criterion. The choice of 26 neighborhoods ensures that all possible face-shared, edge-shared, and corner-shared voxels within a 3×3×3 neighborhood are included in connectivity detection, enabling the capture of the bifurcation and merging characteristics of ceramic grain boundary microcracks in any direction. All damage voxels in the current loading step are traversed. For each unlabeled damage voxel, it is checked whether there are damage voxels in its 26 neighborhood directions. If so, the same connected component label is assigned. After traversal, each connected component corresponds to a spatially connected damage region in the corresponding loading step. The set of connected regions for each loading step is output, with each connected region recording its voxel count, centroid coordinates, and bounding box extent. The preset minimum number of voxels in a connected region is 5, and the spatial volume corresponding to a single voxel is 20μm×20μm×20μm=8000μm. 3 The damage volume corresponding to 5 voxels is 40,000 μm. 3This corresponds to a spherical damage region with an equivalent radius of approximately 10 μm. Isolated damage points smaller than this scale cannot be reliably distinguished from spurious damage points formed by scanning noise. Therefore, isolated damage points with fewer than 5 voxels are considered noise and discarded. For example, three main connected regions are marked during loading step 60, corresponding to the damage propagation regions that develop from the initial pore 1, crack 2, and crack 3, respectively.
[0042] It should be noted that the set of connected components in loading step k is paired and compared with the set of connected components in loading step k+1. For each connected component R in loading step k... k i Find the connected region R with the largest spatial overlap in the set of connected regions at loading step k+1. k+1 j The overlap rate is defined as the number of primes of the intersection of two connected regions divided by R. k i The number of voxels. If the overlap rate is greater than 50%, then R is determined. k+1 j For R k i The system continues to record the centroid displacement, volume change, and damage propagation direction. The 50% overlap threshold is set based on the fact that the load increment between adjacent loading steps is 50N, the expansion of the damage region within a single loading step is limited, and the overlap rate of truly continuous connected regions remains largely unchanged between adjacent loading steps, typically exceeding 70%. In contrast, the overlap rate between false matches or newly emerging damage regions caused by noise and the previous loading step is usually less than 30%. Therefore, 50% is taken as the safe boundary threshold between the two. If multiple connected regions in loading step k all overlap with the same connected region R in loading step k+1... k+1 j If the spatial overlap rate is greater than 50%, a connected region merging event is determined to have occurred. If the overlap rate between the new connected region appearing in loading step k+1 and any connected region in loading step k is less than 50%, a new damage initiation event is determined to have occurred. The above expansion, merging, and initiation changes are tracked pairwise according to the loading step sequence to generate a spatiotemporal evolution record of each connected region, which is the geometric morphological evolution trajectory. For example, the evolution tracking of the alumina ceramic femoral head specimen shows that an independent damage connected region first appears at the initial pore 1 at loading step 30; at loading step 45, the damage region at crack 2 merges with the adjacent newly initiated damage region; and at loading step 60, the total volume of the three main connected regions has expanded to approximately 8 times the initial defect volume.
[0043] It should be noted that all connected regions appearing in the geometric evolution trajectory at each loading step are abstracted as nodes in a graph structure. Node attributes include the loading step number where the connected region first appears, centroid coordinates (X, Y, Z), volume, and final state. Virtual start and end nodes are added to the graph structure. The start node connects to all connected region nodes containing the initial defect location (i.e., the coordinates of the defect location information recorded in step S12). The end node connects to all connected region nodes satisfying the following condition: at least one voxel in the connected region is adjacent to a voxel on the outer surface of the specimen within a 26-neighborhood, meaning the distance between them is no more than one voxel, indicating that the damage area has extended to the specimen surface. The weights of the edges between nodes are directly set to the Euclidean distance between the centroids of the two connected regions, making the shortest path the crack propagation path with the shortest geometric distance in space. Based on the graph structure, the path with the minimum total weight between the start and end nodes is searched. The three-dimensional spatial curve formed by the centroids of the connected regions sequentially connected by this path is the defect propagation path. This path visually represents which damage areas the crack passes through from its initial defect location, along what spatial trajectory it ultimately extends to the sample surface or forms a through fracture surface.
[0044] In step S14, the critical fracture load at the instant of penetrating fracture is extracted based on the defect propagation path, including: The stress concentration region is obtained by fitting a spatial surface to the defect propagation path, and the fracture section is obtained by triangulation of the stress concentration region. During the continuous incremental loading process, acoustic emission data are simultaneously collected from the fracture section region to obtain the load response sequence. Stiffness degradation features are extracted based on the load response sequence; If the stiffness degradation characteristics meet the preset fracture conditions, then the moment of penetrating fracture is determined, and the peak force value is extracted from the load response sequence to obtain the critical fracture load.
[0045] It should be noted that the S13 defect propagation path tracing step and the S14 critical fracture load extraction step are two analytical dimensions within the same continuously increasing loading process, not two independent sequential experiments. The former focuses on tracing the crack propagation path and evolution trajectory from the defect location, while the latter focuses on determining the precise moment of penetrating fracture and extracting the critical load when the crack propagates to near the penetration stage. During continuous loading, the damage evolution tracing in S13 and the acoustic emission monitoring in S14 are performed simultaneously. When S13 determines that the damage connectivity region has extended to near the specimen surface, S14 uses load-displacement data to accurately determine the moment of fracture. This design avoids the physical infeasibility of performing two independent loading experiments on the same specimen.
[0046] It should be noted that a surface fitting was performed on the 3D coordinate point set along the defect propagation path. The surface order was set to 3×3, and the number of control points was set to 15 along the path direction and 10 perpendicular to the path direction. The control point density was selected to ensure that the fitting error on each control curve was less than 10μm, ensuring that the surface accuracy matched the CT voxel resolution. The principal stress gradient was calculated along the normal direction of the fitted surface. The principal stress data came from the interpolation of the stress state data obtained in step S13 at the corresponding spatial locations. Regions with a principal stress gradient change rate exceeding 50MPa / mm were identified as stress concentration regions. The threshold of 50MPa / mm was taken as 1% of the elastic modulus of the ceramic matrix (approximately 350GPa) divided by the average grain size of 5μm. Under this gradient, crack propagation would span multiple grain scales within a single loading step. Based on the 3D point set within the stress concentration region, triangulation was performed to connect the spatial scattered points into a network of triangular facets. The triangulation process ensured that the circumscribed sphere of each triangular facet did not contain other point set elements. The generated 3D mesh surface is smoothed by iterating 5 times with a smoothing coefficient of 0.3 to generate a fracture section characterizing the potential fracture location. For example, the projected area of the fracture section is 30.1 mm², the peak stress gradient is 87 MPa / mm, and it is located at the propagation front of the crack derived from the initial pore 1.
[0047] It should be noted that the acoustic emission sensor was installed on the sample surface before the continuous incremental loading began, and acoustic emission signals were continuously acquired throughout the loading process. A 4-channel acoustic emission sensor array was used, with the sensor resonant frequency set to 150kHz, the preamplifier gain set to 40dB, the signal sampling rate set to 5MHz, and the threshold voltage for triggering the acoustic emission signal set to 100mV. The 150kHz resonant frequency was chosen because the main frequency of the acoustic emission signal generated by the microcrack propagation in ceramic materials is concentrated in the range of 100kHz to 300kHz, and 150kHz is at the center of this frequency band, which can efficiently capture crack propagation events. The acoustic emission characteristic parameters acquired at each loading step include ring count, signal energy, peak amplitude, duration, and rise time. The acquired acoustic emission parameters were used to construct a multidimensional time series according to the loading step, forming a load response sequence containing the loading step number, load amplitude, acoustic emission ring count, and signal energy. The corresponding data of the load-displacement response sequence in step S13 were also recorded in the load response sequence, ensuring that the acoustic emission characteristics and mechanical response are strictly aligned on the time axis.
[0048] It should be noted that the secant modulus E is calculated at each loading step using the load-displacement response sequence synchronously acquired in step S13. sec=ΔF / Δd, where ΔF is the load increment of this loading step, and Δd is the corresponding displacement increment. The average secant modulus of the initial loading steps (loading steps 1 to 5) is taken as the initial elastic modulus E0. The normalized secant modulus E0 of each subsequent loading step is calculated. sec The secant modulus decays with loading steps, calculated as / E0. A linear fit is then performed on this decay curve, with the fitting interval being a sliding window from the current loading step to the previous five loading steps. The resulting fitting slope represents the stiffness degradation characteristic, characterizing the decrease in the material's resistance to deformation. The stiffness degradation characteristic is expressed as a dimensionless slope value; a larger value indicates a more rapid stiffness decay. For example, when the secant modulus transitions from a stable initial value to an accelerated decay phase, the fitting slope increases sharply from approximately 0.002 per loading step to approximately 0.015 per loading step.
[0049] It should be noted that the preset fracture condition is set to a normalized secant modulus decreasing to 0.15, which is 15% of the initial elastic modulus. When the normalized secant modulus E is actually monitored... sec When / E0 drops to 0.15, it is determined that the microcracks inside the ceramic matrix have converged and fused to form a through-fracture surface, thus determining the instant of through-fracture at the grain boundary. The preset fracture condition of 15% of the initial elastic modulus is based on the following statistical analysis of 30 sets of destructive tests on alumina ceramic standard specimens: when the secant modulus of the macroscopic load-displacement curve drops to 15% of the initial value, all specimens exhibit visible macroscopic fracture within the subsequent 5 loading steps. The time deviation between this criterion and the actual fracture instant is less than 3 loading steps. The specimens for the 30 sets of destructive tests were cylinders with a diameter of 10 mm and a height of 20 mm, with a loading rate of 500 N / s. Based on the loading step number corresponding to the determined through-fracture instant, the peak force values within that loading step and the two loading steps before and after it are retrieved and extracted from the load response sequence. The average of these 5 values is taken as the final output critical fracture load. For example, the extracted critical fracture load is 2485 N.
[0050] In one implementation, the step of calculating mechanical performance indicators based on the critical fracture load and a preset specimen specification, and comparing the mechanical performance indicators with a preset mechanical performance threshold to generate a mechanical performance test report includes: The cross-sectional geometric feature parameters are obtained by contour projection of the three-dimensional scanning model of the target ceramic orthopedic implant. Mechanical performance indicators are obtained by stress calculation based on the cross-sectional geometric characteristic parameters and the critical fracture load. The mechanical performance index is compared with a preset mechanical performance threshold. If it is lower than the threshold, a first quality level label is assigned; if it is greater than or equal to the threshold, a second quality level label is assigned. The quality grade label is matched with the mechanical performance index using a text template to obtain a structured text block, and the structured text block is then formatted and packaged to obtain a mechanical performance test report.
[0051] It should be noted that the 3D scanning model of the ceramic orthopedic implant constructed from the 3D tomographic images obtained in step S11 is orthogonally projected onto the contour at the fracture section along the loading axis, and the discrete point set of the contour is extracted. The area of the region enclosed by the contour is then calculated. Where N is the number of discrete points on the contour, (X i ,Y i The coordinates of the projection plane of the contour points are given. Simultaneously, the minimum and maximum diameters of the cross-section in this direction are extracted as auxiliary geometric parameters. For example, the effective load-bearing cross-sectional area of the alumina ceramic femoral head specimen at the fracture section is calculated to be 30.1 mm², with a minimum diameter of 5.2 mm and a maximum diameter of 7.8 mm.
[0052] It should be noted that for the critical fracture load F crit With effective load-bearing cross-sectional area A eff Perform stress calculations to determine the ultimate compressive strength σ. u =F crit / A eff For example, the critical fracture load of 2485 N divided by the effective load-bearing cross-sectional area of 30.1 mm² yields an ultimate compressive strength of 82.6 MPa for the ceramic implant.
[0053] It should be noted that the preset mechanical performance threshold is based on an ultimate compressive strength baseline of 80 MPa. This threshold is set according to the minimum compressive strength requirements for load-bearing alumina ceramic orthopedic implants in ISO 6474-1 standard. The calculated ultimate compressive strength of 82.6 MPa is compared with the 80 MPa threshold. When the ultimate compressive strength of 82.6 MPa is greater than the 80 MPa baseline, the target ceramic orthopedic implant is assigned a second quality grade label, indicating that it has the mechanical qualifications for implantation in load-bearing bone sites. If the calculated ultimate compressive strength is less than 80 MPa, a first quality grade label is assigned, indicating that it can only be used in non-load-bearing sites or needs to be scrapped.
[0054] It should be noted that the quality grade label, ultimate compressive strength value, critical fracture load value, and specimen specification parameters are used as key entities. Following a pre-defined medical device testing specification corpus template, the quality grade label is mapped to the corresponding judgment conclusion statement, and the ultimate compressive strength value is filled into the test result field. This automatically generates a structured text block containing test condition, test result, and judgment conclusion fields. For example, when the quality grade label is the second quality grade, the generated judgment conclusion statement is "This specimen meets the mechanical performance requirements for implantation in load-bearing parts"; when it is the first quality grade, it generates "This specimen does not meet the mechanical performance requirements for implantation in load-bearing parts." The structured text block is then rendered, and the page margins are set to 25mm, the line spacing to 1.5, the table borders to 0.75pt solid lines, the title to 12pt bold Song font, and the body text to 10.5pt Song font, according to the general format requirements for medical device testing reports. After formatting and encapsulation, a complete mechanical performance test report is output.
[0055] It should be noted that the defect location information obtained in step S12 and the defect propagation path obtained in step S13 are associated and stored with the mechanical performance test report. Based on the propagation trajectory of the microcrack during loading, the spatial propagation path is mapped to the temporal dimension, generating a damage evolution sequence containing the crack length changes at five discrete time nodes: loading step 0, loading step 25, loading step 50, loading step 75, and loading step 100. The damage evolution sequence is then time-aligned with the load time axis in the mechanical performance test report. The aligned crack propagation rate and stress concentration factor are extracted and fused to construct a 12-dimensional evolution feature vector. These 12 dimensions include the crack length at the five time nodes, the average crack propagation rate, the maximum crack propagation rate, the average stress concentration factor, the maximum stress concentration factor, the time span of the damage evolution sequence, the ultimate compressive strength value in the report, and the fracture timestamp. An associated data matrix is constructed by performing an outer product operation on the evolutionary feature vectors. Each element (i,j) of this matrix represents the strength of the covariance relationship between the i-th feature and the j-th feature, reflecting the coupling characteristics between the evolution of internal defects and macroscopic mechanical properties.
[0056] The preset matrix norm threshold is 60. This threshold is determined by statistically analyzing the norms of the correlation data matrix of 30 sets of samples. The norm distribution of qualified and unqualified samples forms a bimodal distribution in the range of 45 to 75. The valley between the two peaks is taken as the criterion threshold for 60. When the norm of the correlation data matrix is greater than 60, a judgment isolation mark is generated for that batch of data. This judgment isolation mark indicates a significant statistical coupling relationship between damage evolution and mechanical failure in that batch, and has value for further analysis. The correlation data matrix is structured and packaged according to the judgment isolation mark to obtain a correlation storage set. This correlation storage set is stored in the background database and is only used as an auxiliary analysis basis for subsequent R&D personnel to improve ceramic material formulations or optimize sintering processes. It should be noted that this correlation storage process is independent of the regular quality inspection process and does not participate in the qualification determination of whether the ceramic orthopedic implant meets the load-bearing standard.
[0057] In summary, this invention discloses a method for testing the mechanical properties of ceramic orthopedic products according to ISO standards. This invention obtains internal defect features by acquiring three-dimensional tomographic images, performing voxel analysis and noise reduction, calculating the curvature of these internal defect features to distinguish between pore and crack regions, and then fitting quantization and coordinate mapping to obtain defect location information. While applying continuously increasing loads according to the ISO standard loading mode, the invention tracks the crack tip displacement and damage evolution to obtain the defect propagation path, and then extracts the critical fracture load to calculate mechanical performance indicators. These indicators are then compared with ISO thresholds to generate a test report. This establishes a quantitative correspondence between internal defects and critical fracture loads in ceramic orthopedic products, achieving a deep integration of internal defect identification and macroscopic mechanical testing.
[0058] The second embodiment of the present invention provides a mechanical performance testing system for ceramic orthopedic products oriented towards ISO standards, comprising: a memory, a processor, and a computer program stored in the memory and executable on the processor. When the processor executes the program, it implements the steps of the mechanical performance testing method for ceramic orthopedic products oriented towards ISO standards as described above.
[0059] It should be noted that the mechanical performance testing system for ceramic orthopedic products oriented towards ISO standards provided in this embodiment of the invention is used to execute all the process steps of the mechanical performance testing method for ceramic orthopedic products oriented towards ISO standards described in the above embodiment. The working principles and beneficial effects of the two are one-to-one, so they will not be described again.
[0060] It should be noted that the device embodiments described above are merely illustrative. The units described as separate components may or may not be physically separate, and the components shown as units may or may not be physical units; that is, they may be located in one place or distributed across multiple network units. Some or all of the modules can be selected to achieve the purpose of this embodiment according to actual needs. Furthermore, in the accompanying drawings of the device embodiments provided by this invention, the connection relationships between modules indicate that they have communication connections, which can be specifically implemented as one or more communication buses or signal lines. Those skilled in the art can understand and implement this without any creative effort.
[0061] The specific embodiments described above further illustrate the purpose, technical solution, and beneficial effects of the present invention. It should be understood that the above descriptions are merely specific embodiments of the present invention and are not intended to limit the scope of protection of the present invention. In particular, it should be noted that any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention for those skilled in the art.
Claims
1. A method for testing the mechanical properties of ceramic orthopedic products conforming to ISO standards, characterized in that, include: A three-dimensional tomographic image of the target ceramic orthopedic implant is acquired, and the three-dimensional tomographic image is subjected to voxel analysis and noise reduction processing to obtain internal defect features. The curvature of the internal defect features is calculated to distinguish between the pore region and the crack region. The pore region is fitted with a spherical surface to obtain the micropore size. The crack region is fitted with a trajectory to obtain the grain boundary crack position. The micropore size and the grain boundary crack position are mapped with coordinates to obtain the defect location information. The defect location information is then archived and bound. The target ceramic orthopedic implant is subjected to continuous incremental loading according to a preset loading mode, and stress state data is collected simultaneously. The stress state data is combined with the defect location information to identify crack tips and track displacement to obtain damage distribution data. The damage distribution data of each loading step is tracked to obtain the geometric morphology evolution trajectory. The connectivity analysis of the geometric morphology evolution trajectory is performed to obtain the defect propagation path. The critical fracture load at the moment of penetrating fracture is extracted based on the defect propagation path. Mechanical performance indicators are calculated based on the critical fracture load and the preset sample specifications. The mechanical performance indicators are compared with the preset mechanical performance thresholds to generate a mechanical performance test report. The defect location information, the defect propagation path, and the mechanical performance test report are associated and stored.
2. The method for testing the mechanical properties of ceramic orthopedic products conforming to ISO standards according to claim 1, characterized in that, The process of performing voxel analysis and noise reduction on the three-dimensional tomographic image to obtain internal defect features includes: The initial voxel grayscale matrix is obtained by analyzing the three-dimensional tomographic image; The initial voxel grayscale matrix is decomposed to obtain high-frequency noise components and low-frequency structural components; The low-frequency structural components are processed by a convolutional neural network to obtain a multi-scale feature map; If the gradient of the multi-scale feature map is greater than a preset threshold, the multi-scale feature map is fused with the high-frequency noise component to obtain a denoising feature tensor. If the gradient of the multi-scale feature map is less than or equal to the preset threshold, the original voxel value of the multi-scale feature map is retained as the value of the corresponding position in the denoising feature tensor. Clustering the denoised feature tensor yields morphologically connected regions, and the boundary coordinates of these regions are extracted to obtain internal defect features.
3. The method for testing the mechanical properties of ceramic orthopedic products oriented towards ISO standards according to claim 1, characterized in that, The curvature calculation of the internal defect features to distinguish between porosity regions and crack regions includes: Principal component analysis is performed on the internal defect features to obtain a geometric curvature tensor, which includes a first principal curvature and a second principal curvature. If the ratio of the first principal curvature to the second principal curvature is less than a preset curvature ratio threshold and both the first principal curvature and the second principal curvature are greater than a preset minimum curvature threshold, then the corresponding voxel region is determined to be a pore region. If the ratio of the first principal curvature to the second principal curvature is greater than or equal to the preset curvature ratio threshold, the corresponding voxel region is determined to be a crack region.
4. The method for testing the mechanical properties of ceramic orthopedic products oriented towards ISO standards according to claim 1, characterized in that, The process involves performing spherical fitting on the porous region to obtain the micropore size, performing trajectory fitting on the crack region to obtain the grain boundary crack location, and performing coordinate mapping between the micropore size and the grain boundary crack location to obtain defect location information, including: The radius value is obtained by performing least-squares spherical fitting on the pore region, and the radius value is used as the micropore size; Extract the skeleton center point from the crack region, perform polynomial trajectory fitting on the skeleton center point to obtain a space curve equation, and use the space curve equation as the location of the grain boundary crack. The defect location information is obtained by performing an affine transformation coordinate mapping between the size of the micropores and the location of the grain boundary cracks.
5. The method for testing the mechanical properties of ceramic orthopedic products oriented towards ISO standards according to claim 1, characterized in that, The step of establishing and binding the defect location information includes: The coordinate values and size parameters extracted from the defect location information are concatenated to obtain a text sequence; The text sequence is hashed and encrypted to obtain a unique identification hash value; The defect location information is associated with the unique identification hash value and stored to obtain an initial internal state record, thus completing the filing and binding.
6. The method for testing the mechanical properties of ceramic orthopedic products conforming to ISO standards according to claim 1, characterized in that, The step of combining the defect location information with the stress state data to perform crack tip identification and displacement tracking to obtain damage distribution data includes: The stress concentration degree of each node is calculated by comparing the principal stress values in the stress state data with the defect coordinates in the defect location information. If the stress concentration exceeds a preset stress concentration threshold, the corresponding node will be marked as a crack tip. The strain components are obtained by performing digital image correlation displacement tracking on the crack tip; Equivalent strain calculation is performed on the strain components, and voxels whose equivalent strain exceeds a preset strain threshold are marked as damaged voxels to obtain damage distribution data.
7. The method for testing the mechanical properties of ceramic orthopedic products oriented towards ISO standards according to claim 1, characterized in that, The process of evolutionarily tracking the damage distribution data at each loading step to obtain the geometric morphology evolution trajectory, and performing connectivity analysis on the geometric morphology evolution trajectory to obtain the defect propagation path, includes: The damage distribution data of each loading step is labeled with voxel connected components to obtain the set of connected regions of each loading step. The set of connected regions in adjacent loading steps is morphologically compared, and the expansion and merging changes of the connected regions are tracked to obtain the geometric morphological evolution trajectory. The connected regions in the geometric evolution trajectory are abstracted as graph structure nodes, and the shortest path is calculated on the graph structure nodes to obtain the defect expansion path.
8. The method for testing the mechanical properties of ceramic orthopedic products oriented towards ISO standards according to claim 1, characterized in that, The step of extracting the critical fracture load at the instant of penetrating fracture based on the defect propagation path includes: The stress concentration region is obtained by fitting a spatial surface to the defect propagation path, and the fracture section is obtained by triangulation of the stress concentration region. During the continuous incremental loading process, acoustic emission data are simultaneously collected from the fracture section region to obtain the load response sequence. Stiffness degradation features are extracted based on the load response sequence; If the stiffness degradation characteristics meet the preset fracture conditions, then the moment of penetrating fracture is determined, and the peak force value is extracted from the load response sequence to obtain the critical fracture load.
9. The method for testing the mechanical properties of ceramic orthopedic products oriented towards ISO standards according to claim 1, characterized in that, The step of calculating mechanical performance indicators based on the critical fracture load and preset specimen specifications, and comparing the mechanical performance indicators with preset mechanical performance thresholds to generate a mechanical performance test report includes: The cross-sectional geometric feature parameters are obtained by contour projection of the three-dimensional scanning model of the target ceramic orthopedic implant. Mechanical performance indicators are obtained by stress calculation based on the cross-sectional geometric characteristic parameters and the critical fracture load. The mechanical performance index is compared with a preset mechanical performance threshold. If it is lower than the threshold, a first quality level label is assigned; if it is greater than or equal to the threshold, a second quality level label is assigned. The quality grade label is matched with the mechanical performance index using a text template to obtain a structured text block. The structured text block is then formatted and packaged to obtain a mechanical performance test report.
10. A mechanical performance testing system for ceramic orthopedic products conforming to ISO standards, comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, characterized in that, When the processor executes the program, it implements the mechanical performance testing method for ceramic orthopedic products oriented towards ISO standards as described in any one of claims 1 to 9.