Rock fracture brittleness testing apparatus for non-uniform stress fields
By introducing a high-pressure oil chamber, micro-grooves, spiral sliding grooves, and ball joint components into the rock fracture testing device, the problem of guide sleeve wear in rock fracture testing was solved, achieving high-precision loading and data accuracy, while reducing maintenance frequency and cost.
Patent Information
- Application Number
- CN202611404008.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-10
- Publication Date
- 2026-11-24
AI Technical Summary
Traditional rock fracture testing devices cannot effectively suppress the eccentric impact during rock fracture under non-uniform stress fields, resulting in severe wear of the guide sleeve, decreased loading accuracy, and inaccurate test data.
It adopts a high-pressure oil chamber and guide sleeve structure. The guide sleeve is equipped with micro-ribbed grooves and spiral sliding grooves. Together with the first extrusion ball and the ball head hinge assembly, it automatically scrapes off stone powder, converts impact force, reduces wear, and improves guiding accuracy.
It significantly reduces guide sleeve wear, extends test cycles, improves loading accuracy and data accuracy, reduces maintenance frequency, and lowers maintenance costs.
Smart Images

Figure CN123155352A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of rock fracture brittleness testing technology, specifically to a rock fracture brittleness testing device for non-uniform stress fields. Background Technology
[0002] The rock fracture brittleness testing device is used to simulate the fracture behavior of deep strata rocks under triaxial unequal compressive stress fields. An axial compression bar applies a gradually increasing load to the rock sample until failure, and the brittleness index is obtained. In traditional devices, the compression bar's movement direction is constrained by a guide sleeve, and a ball-and-socket hinge at the top adapts to uneven rock end faces; the base only serves as a support for the sample.
[0003] CN113567255B describes a rock fracture testing device and method. The rock to be tested has a pre-set crack communicating with a pre-set hole, which is rectangular. A first force-applying component abuts against the hole wall parallel to the length direction of the pre-set crack. This application effectively solves the problem in related technologies where the behavior of cracks winding around and penetrating gravel in conglomerate cannot be directly observed.
[0004] In existing technologies, the eccentric load impact generated by the tilted fracture surface at the moment of fracture causes the pressure bar to shift horizontally and tilt at an angle. Neither the smooth inner wall of the guide sleeve nor the ball-and-socket sliding friction pair can effectively suppress this impact. The eccentric load acts directly on the inner wall of the guide sleeve and the contact surface of the ball-and-socket, causing localized wear. At the same time, the high-hardness rock fragments released during fracture invade the guide gap as the pressure bar moves, exacerbating the wear of the guide sleeve during reciprocating sliding. As the clearance widens, the accuracy of the pressure bar movement decreases, ultimately leading to the load deviating from the center. Summary of the Invention
[0005] To address the problem of climbing trees, the present invention provides the following technical solution: a rock fracture brittleness testing device for non-uniform stress fields, comprising: A high-pressure oil chamber is configured as a sealed cavity, the interior of which contains high-pressure oil, and an oil pump is connected to the side of the high-pressure oil chamber. A fixed base is fixedly connected to the bottom of the inner wall of the high-pressure oil chamber. The high-pressure oil chamber is a sealed cavity with an inner diameter of 160 mm, a height of 220 mm, and a wall thickness of 12 mm. An oil pump is connected to the side 40 mm from the bottom, and a fixed base is welded to the bottom of the inner wall. Before the test, the rock core is processed into a standard cylindrical specimen with a diameter of 50 mm and a length of 100 mm. A latex sleeve with open ends is fitted onto the core, and metal pressure heads are wrapped around the top and bottom ends, contacting the top of the fixed base and secured with hose clamps to isolate the specimen from the high-pressure oil inside the high-pressure oil chamber. The fixed base is located at the center of the bottom of the inner wall of the high-pressure oil chamber, and its top plane supports the lower end of the specimen. The oil pump is started, driving high-pressure oil into the high-pressure oil chamber, horizontally compressing the latex sleeve and creating two horizontal compressive forces. Constant pressure control is used, allowing the rock to expand laterally during the compression process. The horizontal compressive force is maintained at a constant value within the range of 10 MPa to 30 MPa, typically 20 MPa. No. 32 anti-wear hydraulic oil is used, and the oil temperature is controlled between 25℃ and 35℃.
[0006] A fixed frame with a frame structure, wherein a guide sleeve is fixedly connected to the inner wall side of the fixed frame, and an extrusion head is slidably connected through the top of the guide sleeve, and a ball joint assembly is sleeved on the top of the extrusion head; The fixing frame is a rectangular frame structure. The guide sleeve is fixed to the inner wall side by four bolts with a nominal diameter of 10mm. The axis of the guide sleeve coincides with the central axis of the fixing base. A top hydraulic cylinder drives the ball joint assembly to advance downwards through the guide sleeve and sealing ring at a constant displacement rate of 0.1mm / min to 0.5mm / min, pushing the extrusion head downwards to apply axial compressive force to the rock until brittle fracture occurs. At the moment of fracture, due to the difference in magnitude between the two horizontal compressive forces, the fracture surface becomes an inclined wedge shape, generating an eccentric bending moment that causes the pressure rod to deflect horizontally and tilt at an angle, simultaneously releasing high-hardness rock fragments. A radial clearance of 0.05mm to 0.12mm is maintained between the inner wall side of the guide sleeve and the side of the extrusion head.
[0007] The guide sleeve is configured with: A lower guide ring and an upper guide ring are used to slide and limit the extrusion head. A connecting frame is fixedly connected to the side of the lower guide ring, and a guide assembly is fixedly connected to the inner wall side of the upper guide ring. A first extrusion ball is provided on the side of the guide assembly. The lower and upper guide rings are coaxially connected in series via a connecting frame consisting of two vertical connecting columns. The lower end of the connecting frame is welded to the outer wall of the lower guide ring, and the upper end is fixed to the outer wall of the upper guide ring with bolts. The axial distance between the lower and upper guide rings is 35mm to 45mm. The lower and upper guide rings guide and fix the sides of the extrusion head. The extrusion head passes through the middle of the lower and upper guide rings and slides up and down along their inner walls. High-hardness stone powder generated when the rock fractures adheres to the outer wall of the extrusion head and is carried into the gap formed between the lower and upper guide rings and the extrusion head as the extrusion head moves up and down. The stone powder is repeatedly crushed in the gap by the reciprocating motion of the extrusion head, resulting in continuous abrasion of the inner walls of the lower and upper guide rings and the outer wall of the pressure rod. After dozens to hundreds of tests, the inner walls of the lower and upper guide rings wear down, the clearance widens, the movement accuracy of the extrusion head decreases, the load deviates from the center, and the test data becomes inaccurate.
[0008] It is also provided with micro-grooves for guiding stone powder. The micro-grooves are set at the top and bottom of the inner wall of the upper guide ring, and the side of the micro-grooves contacts the side of the extrusion head.
[0009] The micro-grooves are rows of small, straight grooves extending from top to bottom. The groove width ranges from 0.3mm to 0.6mm, the groove depth from 0.2mm to 0.5mm, and the spacing between adjacent grooves from 1.8mm to 2.4mm. Eight to 12 micro-grooves are evenly distributed on the inner walls of both the lower and upper guide rings, with rounded corner radii of 0.05mm to 0.1mm at the groove openings. When the extrusion head carries stone powder into the lower and upper guide rings, the edges of the micro-grooves scrape the stone powder off the surface of the extrusion head. The stone powder falls into the micro-grooves and, under gravity, slides down the groove walls, exiting from the lower ends of the lower and upper guide rings. When the extrusion head retracts upwards, the groove walls block the stone powder that has already fallen into the micro-grooves, preventing it from being carried back up. A small amount of extremely fine stone powder that is not discharged slowly accumulates and compacts at the bottom of the micro-groove, forming a thin stone powder pad. This pad separates the extrusion head from the inner walls of the lower and upper guide rings. When the extrusion head slides, it contacts the stone powder pad instead of the metal surface, resulting in a lower coefficient of friction than direct metal-to-metal contact. With the micro-groove structure, stone powder is continuously discharged, while the guide assembly and the first extrusion ball support the sides of the extrusion head. No abrasive material accumulates inside the lower and upper guide rings, preventing grinding wear within the mating gaps.
[0010] Preferably, the guiding component includes: A guide base for supporting the first extrusion ball, the top of which is fixedly connected to the bottom of the upper guide ring; It also includes a sliding groove for guiding the first extrusion ball. The sliding groove is disposed on the inner wall side of the guide base. The sliding groove is configured as a spiral structure. The portion of the sliding groove located in the middle of the guide base is provided with a deepening structure.
[0011] The top of the guide base is fixedly connected to the bottom of the upper guide ring with screws. A sliding groove is located on the inner wall of the guide base. The sliding groove has a spiral structure with a lead of 15mm to 20mm, a circular arc cross-section, a width of 2.4mm to 3.0mm, and a depth of 0.6mm to 0.8mm at both ends. The deepened section of the sliding groove in the middle of the guide base has a depth of 1.4mm to 1.8mm, and the axial length of the deepened section accounts for 35% to 45% of the total length of the sliding groove. A first extrusion ball with a diameter of 2.2mm to 2.5mm is placed inside the sliding groove, with a radial gap of 0.03mm to 0.08mm between the first extrusion ball and the inner wall of the sliding groove. When the extrusion head deviates, it presses the first extrusion ball against the slope of the sliding groove, where it rolls, converting the lateral impact force into rolling force. Without the first extrusion ball, the lateral force acts directly on the inner wall of the guide base, resulting in excessive local stress. Over time, this can cause marks or even scratches on the inner wall. After the first extrusion ball is installed, the impact force is absorbed by the rolling motion of the first extrusion ball, and the inner wall of the guide base will not directly bear the lateral force. High-hardness stone powder generated during rock fragmentation is carried into the gap formed between the guide base and the extrusion head by the movement of the extrusion head. The sliding grooves and micro-ridges on the inner wall of the guide base scrape off the stone powder, which falls into the sliding grooves or micro-ridges and slides down under gravity, exiting from the bottom and not remaining on the mating surface of the guide base and the first extrusion ball. At the moment of fracture, the guide base and the first extrusion ball automatically compensate for the off-center load; the first extrusion ball dissipates the impact, and the groove structure removes the stone powder. Both functions are automatically triggered when fracture occurs, requiring no additional operation.
[0012] Preferably, the extrusion head includes a lower moving rod, the bottom of which is fixedly connected to a lower pressing head, and the bottom of which is fixedly connected to a guide strip.
[0013] The bottom of the lower moving rod is threadedly fixed to the top of the lower pressure head, and the guide strip is welded to one side of the bottom plane of the lower pressure head. The top hydraulic cylinder pushes the ball joint assembly, which in turn causes the lower moving rod to descend. The bottom plane of the lower pressure head directly presses against the upper surface of the rock, and the guide strip is positioned in conjunction with the upper end of the latex sleeve. The axial loading rate is 0.1 mm / min to 0.5 mm / min. At the moment of fracture, the lateral force released from the rock fracture surface is transmitted to the lower moving rod through the lower pressure head. The lateral displacement of the lower moving rod is constrained by the lower guide ring and the upper guide ring.
[0014] Preferably, the bottom of the pressing head is configured as a planar structure, the guide strip is positioned on one side of the bottom planar surface of the pressing head, the top of the lower moving rod is fixedly connected to the bottom of the ball head hinge assembly, the side of the lower moving rod contacts the side of the first extrusion ball, and the side of the lower moving rod contacts the side of the micro-groove.
[0015] The bottom plane of the pressure head is in direct contact with the upper surface of the rock, and the axial force is transmitted along the centerline. The guide strip is located on one side of the bottom plane of the pressure head, aligned with the upper edge of the latex sleeve. The top of the lower moving rod is threaded to the bottom of the ball joint assembly, and the side of the lower moving rod simultaneously contacts the first extrusion ball and the micro-groove. When the pressure rod shifts horizontally at the moment of fracture, the first extrusion ball rolls in the sliding groove to absorb the impact, and the micro-groove scrapes away the stone powder adhering to the side of the lower moving rod.
[0016] Preferably, the ball joint assembly includes a ball head seat, an extrusion groove is formed on the inner wall side of the ball head seat, a second extrusion ball is formed on the inner wall side of the extrusion groove, a ball head rod is provided inside the extrusion groove above the second extrusion ball, and an upper connecting rod is fixedly connected to the bottom of the ball head seat.
[0017] The ball head seat is located between the hydraulic cylinder and the upper connecting rod and the lower moving rod. The bottom of the ball head seat is fixedly connected to the top of the upper connecting rod, and the bottom of the upper connecting rod is fixedly connected to the top of the lower moving rod. The ball head rod passes through the top of the fixing frame and slides through it. A radial clearance of 0.1mm to 0.2mm is maintained between the outer diameter of the ball head rod and the inner hole of the copper sliding sleeve in the guide hole at the top of the fixing frame. The mating length between the ball head rod and the top sliding sleeve of the fixing frame is 25mm to 30mm, and the inner wall roughness of the copper sliding sleeve is 0.8 micrometers. The concave spherical radius of the ball head seat is 14.5mm to 14.8mm, the ball head radius of the ball head rod is 14.2mm to 14.4mm, and the mating clearance between the ball head rod and the concave spherical surface of the ball head seat is 0.3mm to 0.6mm. The ball head rod is embedded in the ball head seat, forming a spherical mating pair. The upper connecting rod and the lower moving rod can automatically adjust their angles to adapt to uneven rock surfaces and the tilting impact during fracture. An extrusion groove is machined on the concave spherical surface of the ball head seat. A second extrusion ball is placed in the extrusion groove. When the ball head rod shakes, the second extrusion ball rolls in the groove, and the sliding friction is changed into rolling friction, which greatly reduces the wear rate.
[0018] Preferably, the bottom of the upper connecting rod is fixedly connected to the top of the lower moving rod, and the ball joint passes through the top of the fixing frame and is slidably connected to the top of the fixing frame.
[0019] The upper connecting rod and the lower moving rod are fixed by threads, and the ball head rod slides up and down in the guide hole at the top of the fixing frame. At the moment of fracture, the tilted fracture surface of the rock gives the lower moving rod an oblique reaction force. The lower moving rod transmits the reaction force to the upper connecting rod and the ball head rod. The ball head rod slides slightly in the copper sliding sleeve, and the ball head of the ball head rod swings in the concave spherical surface of the ball head seat, thus buffering the off-center impact.
[0020] Preferably, the extrusion groove includes a lower guide groove, and an upper guide groove is provided at the top of the lower guide groove. The lower guide groove and the upper guide groove are configured with different curvatures and depths, and the upper guide groove is configured with a deeper structure.
[0021] The lower guide groove has a depth of 1.2mm to 2.0mm, and the upper guide groove has a depth of 2.5mm to 3.8mm. The lower guide groove has a radius of curvature of 2.5mm, and the upper guide groove has a radius of curvature of 1.8mm. Six second extrusion balls, each with a diameter of 4.0mm to 4.5mm, are placed within the lower and upper guide grooves, evenly distributed circumferentially. The depths of the lower and upper guide grooves are unevenly distributed circumferentially, with a shallower section directly facing the direction of the maximum horizontal principal stress and a deeper section on the opposite side. When the ball head is tilted to the shallower side of the lower or upper guide groove, the second extrusion balls are compressed more tightly, resulting in a greater rebound force. This rebound force pushes the ball head back, creating an auxiliary restoring torque, which is superimposed on the straightening force of the upper guide ring. There is an area at the center of the bottom of the ball head seat that the ball head cannot reach during normal operation. Red dye is pre-embedded in this central area, and the area is protected by nickel plating. After the lower and upper guide grooves wear down to a certain extent, the ball joint sinks and begins to touch the center area of the bottom of the ball joint seat. Once the nickel layer is worn through, the red dye is exposed. The operator can determine whether to replace it by seeing red spots through the side observation window. After the improvement, the wear rate of the ball joint seat is reduced to about 10% of the original, the angle tilt of the upper connecting rod and the lower moving rod is reduced, the off-center load impact is further buffered, and the replacement time can be determined visually, without the need for periodic disassembly and inspection.
[0022] Preferably, the fixed base includes a fixed seat, the fixed seat has a fastening groove on its side, a flat base is fixedly connected to the top of the fixed seat, the bottom of the fixed seat is connected to the bottom of the inner wall of the high-pressure oil chamber, and the bottom of the fixed seat is connected to an external constant negative pressure air source.
[0023] The top of the mounting base supports the lower end of the rock sample. The fastening groove on the side of the mounting base is a rectangular annular groove, 1.5mm deep and 5mm wide, 8mm from the top of the mounting base. The excess portion of the latex sleeve at the lower end is rolled down and wrapped around the fastening groove on the side of the mounting base. A hose clamp is used to tighten the latex sleeve to the side of the fastening groove on the outer wall of the mounting base. After the hose clamp is tightened, the latex sleeve forms a sealing ring on the outer wall of the mounting base. The lower end of the rock directly contacts the flat base, while the side is wrapped by the latex sleeve. The rock and the interior of the latex sleeve form a closed cavity, isolating it from the external high-pressure oil. The bottom of the mounting base is connected to an external constant negative pressure air source, and the negative pressure interface continuously draws air during the test.
[0024] Preferably, the planar base includes a pressing base, a limiting plate is fixedly connected to the top edge of the pressing base, an air extraction hole is provided on the top of the pressing base at one side of the limiting plate, and the bottom of the pressing base is fixedly connected to the top of the fixed base.
[0025] The limiting plate is a ring-shaped protrusion with an inner diameter of 50.2mm to 50.5mm, a height of 3mm to 4mm, and a wall thickness of 2mm. Eight evacuation holes are located on the top of the lower base, inside the limiting plate, evenly distributed around the center of the lower base. The hole diameter is 1.2mm to 1.5mm, and the distance from the hole opening to the center of the lower base is 12mm to 15mm. The limiting plate fixes the sample in the center of the top of the lower base, eliminating the need for manual alignment. The placement position is consistent each time, resulting in a smaller initial off-center load compared to traditional methods. The evacuation holes are connected to an external constant negative pressure air source at the bottom of the fixed base. The negative pressure draws away the stone powder, which is discharged along the evacuation holes instantly upon generation, preventing accumulation on the lower base. Therefore, no special cleaning of the base is required after the test.
[0026] The beneficial effects of the technical solution provided by this invention include: 1. The longitudinal micro-grooves on the inner wall of the guide ring continuously scrape off the high-hardness stone powder adhering to the surface during the reciprocating motion of the extrusion head. After the stone powder falls into the groove, it slides down the groove wall and is discharged by itself, no longer entering the lower guide ring. The fit gap between the upper guide ring and the extrusion head is repeatedly crushed. The expansion of the fit gap due to grinding and wear is reduced by about 70% to 80% compared with the traditional smooth guide sleeve. The guide accuracy maintenance cycle is extended from dozens of tests to hundreds of tests. The frequency of disassembly and replacement and regular cleaning is greatly reduced. The load center offset of long-term test data is significantly narrowed.
[0027] 2. The spiral sliding groove, in conjunction with the first extrusion ball, prevents the lateral impact generated during the moment of rock sample fracture from acting on the inner wall of the guide base in a hard contact manner. The impact force is absorbed and transformed by the rolling motion, and the risk of indentation and scratches on the inner wall of the guide base is basically eliminated. After the stone powder enters the gap between the guide base and the extrusion head, it is immediately scraped into the groove by the micro-ridge groove and the sliding groove and discharged. The mating surface between the first extrusion ball and the sliding groove remains clean. The resistance to eccentric load impact is improved by at least one order of magnitude compared with the structure without the extrusion ball. The integrity and smoothness of the guide component under repeated fracture impact conditions are significantly improved.
[0028] 3. The lower and upper guide grooves on the concave spherical surface of the ball head are arranged with different curvatures and depths along the circumference. The sliding friction of the ball head rod during the second extrusion ball is converted into rolling friction, reducing the wear rate of the ball head to about 10% of the original structure. The angle tilt is reduced simultaneously, and the impact of the off-center load is further buffered. After the wear accumulates to the threshold, the ball head rod touches the center area at the bottom of the ball head and wears through the nickel layer to expose the red dye. The operator can visually determine the replacement time through the side observation window. There is no need to regularly disassemble and inspect the ball head hinge assembly, which significantly reduces maintenance costs and downtime.
[0029] 4. The annular limiting plate at the top of the fixed base automatically centers the sample each time it is placed, reducing the initial off-center load by more than 50% compared to manual visual centering, thus improving the repeatability of test data. The evenly distributed air extraction holes on the lower base continuously draw in air under negative pressure throughout the test, and the stone powder generated at the moment of fracture is immediately extracted from the surface of the base without accumulation. There is no need to clean the flat base after the test, and the auxiliary operation time for a single test is reduced by about 30%, improving both positioning consistency and test flow efficiency. Attached Figure Description
[0030] Figure 1 This is a schematic diagram of the rock fracture brittleness testing device for non-uniform stress fields according to the present invention. Figure 2 This is a schematic diagram of the guide sleeve structure of the present invention; Figure 3 This is a schematic diagram of the guiding component structure of the present invention; Figure 4 This is a schematic diagram of the extrusion head structure of the present invention; Figure 5 This is a schematic diagram of the ball joint assembly structure of the present invention; Figure 6 This is a schematic diagram of the extrusion groove structure of the present invention; Figure 7 This is a schematic diagram of the fixed base structure of the present invention; Figure 8 This is a schematic diagram of the planar base structure of the present invention.
[0031] In the diagram: 1. High-pressure oil chamber; 2. Oil pump; 3. Fixed base; 4. Fixed frame; 5. Guide sleeve; 6. Extrusion head; 7. Ball head hinge assembly; 501. Lower guide ring; 502. Connecting frame; 503. Upper guide ring; 504. Micro-groove; 505. Guide assembly; 506. First extrusion ball; 5051. Guide base; 5052. Sliding groove; 601. Lower moving rod; 602. Lower pressure head; 603. Guide strip; 701. Ball head seat; 702. Extrusion groove; 703. Second extrusion ball; 704. Ball head rod; 705. Upper connecting rod; 7021. Lower guide groove; 7022. Upper guide groove; 301. Fixed base; 302. Fastening groove; 303. Flat base; 3031. Lower pressure base; 3032. Limiting plate; 3033. Air extraction hole. Detailed Implementation
[0032] Example 1, please refer to Figures 1-2This invention provides a technical solution: a rock fracture brittleness testing device for non-uniform stress fields. The high-pressure oil chamber 1 is a sealed cavity with an inner diameter of 160mm, a height of 220mm, and a wall thickness of 12mm. An oil pump 2 is connected to the side of the high-pressure oil chamber 1 40mm from the bottom. A fixed base 3 is welded to the bottom of the inner wall of the high-pressure oil chamber 1. The fixed frame is a rectangular frame structure. A guide sleeve 5 is fixed to the inner wall of the fixed frame by four M10 bolts. The axis of the guide sleeve 5 coincides with the central axis of the fixed base 3. A pressing head 6 is slidably connected to the top of the guide sleeve 5. A ball-head hinge assembly 7 is fitted onto the top of the pressing head 6. The fixed frame 4 provides overall support for the equipment. Before the test, the rock core is processed into a standard cylindrical sample φ50×100mm, fitted with a latex sleeve with openings at both ends. The upper and lower ends are wrapped with metal indenters that contact the top of the fixed base 3 and are secured with hose clamps to isolate the sample from the high-pressure oil inside the high-pressure oil chamber 1. The fixed base 3 is located at the center of the bottom of the inner wall of the high-pressure oil chamber 1, and the top plane of the fixed base 3 is used to support the sample. At the lower end, the assembled sample is placed inside the high-pressure oil chamber 1, and the oil pump 2 is started. The oil pump 2 drives the high-pressure oil into the high-pressure oil chamber 1, squeezing the latex sleeve horizontally to form two horizontal extrusion forces. Constant pressure control is adopted to allow the rock to expand laterally during the compression process. After maintaining the horizontal extrusion force constant, the top hydraulic cylinder drives the ball joint assembly 7 to pass through the guide sleeve 5 and the sealing ring downward at a constant displacement rate of 0.1 mm / min to 0.5 mm / min. The horizontal extrusion force is maintained at a constant value within the range of 10 MPa to 30 MPa, usually 20 MPa. The high-pressure oil is No. 32 anti-wear hydraulic oil, and the oil temperature is controlled between 25℃ and 35℃. By pushing the extrusion head 6 down, axial extrusion force is applied to the rock until the rock undergoes brittle fracture. At the moment of fracture, the fracture surface is inclined wedge-shaped, generating an off-center bending moment that causes the pressure rod to deviate horizontally and tilt at an angle, while releasing high-hardness rock chips. The inner wall side of the guide sleeve 5 and the side of the extrusion head 6 are separated by 0.05 mm to 0.With a radial clearance of 12mm, the lower guide ring 501 and the upper guide ring 503 are coaxially connected in series via a connecting frame 502. The connecting frame 502 consists of two vertical connecting columns. The lower end of the connecting frame 502 is welded to the outer wall of the lower guide ring 501, and the upper end of the connecting frame 502 is fixed to the outer wall of the upper guide ring 503 by bolts. The axial distance between the lower guide ring 501 and the upper guide ring 503 is 35mm to 45mm. The lower guide ring 501 and the upper guide ring 503 guide and fix the side of the extrusion head 6. The extrusion head 6 passes through the middle of the lower guide ring 501 and the upper guide ring 503, along the lower guide ring 501 and the upper guide ring 503. The inner wall of the guide ring 503 slides up and down; the extrusion head 6 consists of a lower moving rod 601, a lower pressing head 602, and a guide strip 603. The bottom of the lower moving rod 601 is threadedly fixed to the top of the lower pressing head 602. The bottom of the lower pressing head 602 is set as a flat structure. The guide strip 603 is welded to one side of the bottom flat surface of the lower pressing head 602. The top of the lower moving rod 601 is threadedly fixed to the bottom of the ball head hinge assembly 7. The side of the lower moving rod 601 contacts the side of the first extrusion ball 506, and the side of the lower moving rod 601 also contacts the side of the micro-groove 504. The inner wall of the traditional guide sleeve is smooth, and the rock fractures... The high-hardness stone powder generated during the process adheres to the outer wall of the extrusion head 6. As the extrusion head 6 moves up and down, it is carried into the gap between the lower guide ring 501, the upper guide ring 503, and the extrusion head 6. Within this gap, the stone powder is repeatedly crushed by the reciprocating motion of the extrusion head 6, resulting in continuous abrasion of the inner walls of the lower guide ring 501 and the upper guide ring 503, as well as the outer wall of the pressure rod. After dozens to hundreds of tests, the inner walls of the lower guide ring 501 and the upper guide ring 503 are worn, the clearance widens, the movement accuracy of the extrusion head 6 decreases, the load deviates from the center, and the test data becomes inaccurate. The lower guide ring 501 and the upper guide ring 503... 3. After wear, it needs to be disassembled and replaced. In daily use, it also needs to be disassembled and cleaned regularly, resulting in a large amount of maintenance work. By machining longitudinally penetrating micro-grooves 504 on the inner walls of the lower guide ring 501 and the upper guide ring 503, the micro-grooves 504 are rows of small straight grooves that run from top to bottom. The groove width of the micro-grooves 504 is 0.3mm to 0.6mm, the groove depth is 0.2mm to 0.5mm, and the spacing between adjacent grooves is 1.8mm to 2.4mm. There are 8 to 12 micro-grooves 504 evenly distributed on the inner walls of the lower guide ring 501 and the upper guide ring 503. The edges of the groove openings of the micro-grooves 504 are provided with a rounded corner radius of 0.05mm to 0.1mm, micro-grooves 504 are set at the top and bottom of the inner wall of the upper guide ring 503 and the top and bottom of the inner wall of the lower guide ring 501, and the side of the micro-grooves 504 contacts the side of the extrusion head 6; when the extrusion head 6 carries stone powder into the lower guide ring 501 and the upper guide ring 503, the edges of the micro-grooves 504 scrape the stone powder off the surface of the extrusion head 6. After the stone powder falls into the micro-grooves 504, it slides down the groove wall by itself under the action of gravity and is discharged from the lower end of the lower guide ring 501 and the upper guide ring 503; when the extrusion head 6 is pulled back upwards, the groove wall of the micro-grooves 504 blocks the stone powder that has fallen into the micro-grooves 504 and will not be carried back up by the extrusion head 6; a small amount of extremely fine stone powder that is not discharged remains at the bottom of the micro-grooves 504. The material is gradually piled up and compacted, forming a thin layer of stone powder. This stone powder layer separates the extrusion head 6 from the inner walls of the lower guide ring 501 and the upper guide ring 503. When the extrusion head 6 slides, it contacts the stone powder layer, not the metal surface, resulting in a lower coefficient of friction than direct metal-to-metal contact. With the micro-groove structure 504, the stone powder is continuously discharged. Simultaneously, a guide assembly 505 is fixedly connected to the inner wall of the upper guide ring 503. A first extrusion ball 506 is positioned on the side of the guide assembly 505. The guide assembly 505 and the first extrusion ball 506 support the side of the extrusion head 6, further reducing friction. No abrasive material accumulates inside the lower guide ring 501 and the upper guide ring 503, preventing grinding wear within the mating gaps.
[0033] Example 2, please refer to Figures 1-3Based on the first embodiment, when the rock column breaks, at the instant of fracture, the internal cracks of the rock suddenly penetrate, forming an inclined fracture surface; this inclined surface will give the extrusion head 6 a lateral impact force, causing the extrusion head 6 to bend to the side; the guide assembly 505 consists of a guide base 5051 and a sliding groove 5052. The top of the guide base 5051 is fixedly connected to the bottom of the upper guide ring 503 by screws. The sliding groove 5052 is set on the inner wall side of the guide base 5051. The sliding groove 5052 has a spiral structure, the spiral lead of the sliding groove 5052 is 15mm to 20mm, the groove cross-section of the sliding groove 5052 is arc-shaped, and the groove width of the sliding groove 5052 is 2. The sliding groove 5052 has a depth of 0.4mm to 3.0mm at both ends, and a depth of 0.6mm to 0.8mm at the ends. The deepened section of the sliding groove 5052 located in the middle of the guide base 5051 has a depth of 1.4mm to 1.8mm. The axial length of the deepened section of the sliding groove 5052 accounts for 35% to 45% of the total length of the sliding groove 5052. A first extrusion ball 506 with a diameter of 2.2mm to 2.5mm is placed inside the sliding groove 5052. A radial gap of 0.03mm to 0.08mm is maintained between the first extrusion ball 506 and the inner wall of the sliding groove 5052. When the extrusion head 6 is deflected, it will press the first extrusion ball 506 against the slope section of the sliding groove 5052. The compression ball 506 rolls on the slope, converting the lateral impact force into rolling force, instead of directly impacting the inner wall of the guide base 5051. Without the first compression ball 506, this lateral force would act directly on the inner wall of the guide base 5051, causing excessive local stress, which over time would leave marks or even scratches on the inner wall. With the first compression ball 506 installed, the impact force is absorbed by the rolling motion of the first compression ball 506, and the inner wall of the guide base 5051 does not directly bear this lateral force. At the same time, when the rock breaks, a large amount of high-hardness stone powder is generated, which is carried into the gap formed between the guide base 5051 and the compression head 6 as the compression head 6 moves. Without the first compression ball 506, the impact force would be absorbed by the rolling motion of the first compression ball 506, and the inner wall of the guide base 5051 would not directly bear this lateral force. With proper treatment, the stone powder will be repeatedly crushed in the gaps, like sandpaper abrading the inner wall of the guide base 5051 and the outer wall of the extrusion head 6. However, the inner wall of the guide base 5051 has sliding grooves 5052 and micro-ribbed grooves 504. Once the stone powder enters, it will be scraped off and fall into the sliding grooves 5052 or micro-ribbed grooves 504. Under the action of gravity, the stone powder slides down and is discharged from the bottom, without remaining on the mating surface of the guide base 5051 and the first extrusion ball 506. At the moment of fracture, the guide base 5051 and the first extrusion ball 506 automatically compensate for the off-center load. The first extrusion ball 506 dissipates the impact, and the stone powder is discharged by the groove structure. Both functions are automatically triggered when fracture occurs, without any additional operation.
[0034] Example 3, please refer to Figures 1-6Based on the second embodiment, the ball joint assembly 7 consists of a ball head seat 701, an extrusion groove 702, a second extrusion ball 703, a ball head rod 704, and an upper connecting rod 705. The ball head seat 701 is located between the hydraulic cylinder, the upper connecting rod 705, and the lower moving rod 601. The bottom of the ball head seat 701 is fixedly connected to the top of the upper connecting rod 705, and the bottom of the upper connecting rod 705 is fixedly connected to the top of the lower moving rod 601. The ball head rod 704 passes through the top of the fixed frame and slides along the top of the fixed frame. The ball joint 704 has a radial clearance of 0.1mm to 0.2mm between its outer diameter and the inner hole of the copper sleeve in the guide hole at the top of the mounting bracket. The mating length between the ball joint 704 and the top sleeve of the mounting bracket is 25mm to 30mm. The inner wall roughness of the copper sleeve is Ra 0.8μm. The concave spherical radius of the ball head seat 701 is 14.5mm to 14.8mm, and the ball head radius of the ball joint 704 is 14.2mm to 14.4mm. The ball head of the ball joint 704 and the ball head seat 701 are connected. The concave spherical mating clearance is 0.3mm to 0.6mm. The ball head rod 704 is embedded in the ball head seat 701, forming a spherical mating pair. Its function is to allow the upper connecting rod 705 and the lower moving rod 601 to automatically adjust their angles to adapt to the unevenness of the rock end face and the tilting impact during fracture. In this design, a compression groove 702 is machined on the concave spherical surface of the ball head seat 701. The compression groove 702 consists of a lower guide groove 7021 and an upper guide groove 7022. The lower guide groove 7021 has a depth of 1.2mm. The upper guide groove 7022 has a depth of 2.5mm to 3.8mm, the lower guide groove 7021 has a radius of curvature of 2.5mm, and the upper guide groove 7022 has a radius of curvature of 1.8mm. The lower guide groove 7021 and the upper guide groove 7022 are set with different curvatures and depths, and the upper guide groove 7022 is set with a deeper structure. A second extrusion ball 703 is placed in the lower guide groove 7021 and the upper guide groove 7022. The diameter of the second extrusion ball 703 is 4.0mm to 4.0mm.The second extrusion ball 703 is evenly distributed circumferentially. When the ball head rod 704 shakes, the second extrusion ball 703 rolls in the lower guide groove 7021 and the upper guide groove 7022, turning sliding friction into rolling friction, which greatly reduces the wear rate. The depth of the lower guide groove 7021 and the upper guide groove 7022 is unevenly distributed circumferentially, with a shallower section facing the direction of the maximum horizontal principal stress and a deeper section on the opposite side. When the ball head rod 704 tilts to the shallower side of the lower guide groove 7021 and the upper guide groove 7022, the second extrusion ball 703 is pressed tighter and the rebound force is greater. The rebound force pushes the ball head rod 704 back, forming an auxiliary return torque, which is superimposed on the straightening force of the upper guide ring 503. The bottom of the ball head seat 701 There is a central area that the ball joint 704 cannot reach during normal operation. Red dye is embedded in the central area of the bottom of the ball joint 701, which is protected by nickel plating. When the lower guide groove 7021 and upper guide groove 7022 wear down to a certain extent, the ball joint 704 sinks and begins to touch the central area of the bottom of the ball joint 701. Once the nickel layer is worn through, the red dye is exposed. The operator can see red spots through the side observation window to indicate that replacement is necessary. After the improvement, the wear rate of the ball joint 701 is reduced to about 10% of the original. The angle of inclination of the upper connecting rod 705 and the lower moving rod 601 is reduced, further buffering the impact of off-center loads. Replacement can be determined visually, eliminating the need for periodic disassembly and inspection.
[0035] Example 4, please refer to Figures 1-8Based on the third embodiment, first, a latex sleeve is placed over the outside of the rock sample, extending beyond the rock at both the top and bottom. The rock sample with the latex sleeve on is placed on top of the fixing base 301. The excess portion of the latex sleeve is pulled down and tucked into the fastening groove 302 on the side of the fixing base 301. A hose clamp is used to secure the latex sleeve to the side of the fastening groove 302 on the outer wall of the fixing base 301. The fastening groove 302 on the side of the fixing base 301 is a rectangular annular groove, 1.5mm deep and 5mm wide, 8mm from the top of the fixing base 301. The upper pressure head is then pressed against the upper surface of the rock, with the upper end of the latex sleeve... The extra section is pulled upwards to cover the outer wall of the pressure head 602 and aligned with the guide strip 603, then tightened with a hose clamp. After the hose clamp is tightened, the latex sleeve forms two sealing rings on the outer wall of the fixing base 301 and the outer wall of the pressure head 602. The upper and lower end faces of the rock directly contact the pressure base 3031 and the pressure head 602, while the sides are wrapped by the latex sleeve. The entire rock and the interior of the latex sleeve form a closed cavity, isolating it from the external high-pressure oil. When the high-pressure oil squeezes the outer wall of the latex sleeve from all sides, the latex sleeve is pressed against the side of the rock. The higher the oil pressure, the tighter the fit and the better the sealing effect. The upper surface of the traditional base is flat, and after the sample is placed on it, it needs to be manually aligned with the center. There is always a deviation in the placement position. During loading, the center of the pressure head 602 is not aligned with the center of the rock, resulting in initial off-center loading. Stone powder generated during fracture directly scatters onto the surface of the flat base 303, requiring time for cleaning after each test. The limiting plate 3032 fixes the sample at the center of the top of the pressure base 3031, eliminating the need for manual alignment and ensuring a consistent placement position. The initial off-center loading is smaller than with traditional methods. The limiting plate 3032 is fixedly connected to the top edge of the pressure base 3031. The limiting plate 3032 is an annular protrusion with an inner diameter of 50.2mm to 50.5mm, a height of 3mm to 4mm, and a wall thickness of [missing information]. The top of the lower base 3031, located inside the limiting plate 3032, has eight air extraction holes 3033, evenly distributed around the center of the lower base 3031. The diameter of the air extraction holes 3033 is 1.2mm to 1.5mm, and the distance from the opening of the air extraction hole 3033 to the center of the lower base 3031 is 12mm to 15mm. The bottom of the lower base 3031 is fixedly connected to the top of the fixed seat 301, and the bottom of the fixed seat 301 is connected to an external constant negative pressure air source. The negative pressure interface continuously draws air during the test, and the stone powder is sucked away along the air extraction holes 3033 the moment it is generated, and will not accumulate on the lower base 3031. After the test, there is no need to clean the base.
[0036] The above are merely specific embodiments of the present invention, but the scope of protection of the present invention is not limited thereto. The scope of protection of the present invention should be determined by the scope of the claims.
Claims
1. A rock fracture brittleness testing apparatus for non-uniform stress fields, characterized by, include: A high-pressure oil chamber is configured as a sealed cavity, the interior of which contains high-pressure oil, and an oil pump is connected to the side of the high-pressure oil chamber. A fixed base is fixedly connected to the bottom of the inner wall of the high-pressure oil chamber. A fixed frame with a frame structure, wherein a guide sleeve is fixedly connected to the inner wall side of the fixed frame, and an extrusion head is slidably connected through the top of the guide sleeve, and a ball joint assembly is sleeved on the top of the extrusion head; The guide sleeve is configured with: A lower guide ring and an upper guide ring are used to slide and limit the extrusion head. A connecting frame is fixedly connected to the side of the lower guide ring, and a guide assembly is fixedly connected to the inner wall side of the upper guide ring. A first extrusion ball is provided on the side of the guide assembly. It is also provided with micro-grooves for guiding stone powder. The micro-grooves are set at the top and bottom of the inner wall of the upper guide ring, and the side of the micro-grooves contacts the side of the extrusion head.
2. The apparatus for testing the brittleness of rock fracture under a non-uniform stress field according to claim 1, wherein The guiding component includes: A guide base for supporting the first extrusion ball, the top of which is fixedly connected to the bottom of the upper guide ring; It also includes a sliding groove for guiding the first extrusion ball. The sliding groove is disposed on the inner wall side of the guide base. The sliding groove is configured as a spiral structure. The portion of the sliding groove located in the middle of the guide base is provided with a deepening structure.
3. The apparatus for testing rock fracture brittleness in a non-uniform stress field according to claim 1, characterized in that: The extrusion head includes a lower moving rod, a lower pressing head is fixedly connected to the bottom of the lower moving rod, and a guide strip is fixedly connected to the bottom of the lower pressing head.
4. The apparatus for testing the brittleness of rock fracture under a non-uniform stress field according to claim 3, characterized in that: The bottom of the pressing head is set as a planar structure, the guide strip is set at one side of the bottom planar surface of the pressing head, the top of the lower moving rod is fixedly connected to the bottom of the ball head hinge assembly, the side of the lower moving rod contacts the side of the first extrusion ball, and the side of the lower moving rod contacts the side of the micro-groove.
5. The apparatus for testing rock fracture brittleness in a non-uniform stress field according to claim 1, wherein: The ball joint assembly includes a ball joint seat, an extrusion groove is formed on the inner side of the ball joint seat, a second extrusion ball is formed on the inner side of the extrusion groove, a ball joint rod is provided inside the extrusion groove above the second extrusion ball, and an upper connecting rod is fixedly connected to the bottom of the ball joint seat.
6. The apparatus for testing the brittleness of rock fracture under a non-uniform stress field according to claim 5, characterized in that: The bottom of the upper connecting rod is fixedly connected to the top of the lower moving rod, and the ball head rod passes through the top of the fixing frame and is slidably connected to the top of the fixing frame.
7. The apparatus for testing rock fracture brittleness under non-uniform stress field according to claim 5, characterized in that: The extrusion groove includes a lower guide groove, and an upper guide groove is provided at the top of the lower guide groove. The lower guide groove and the upper guide groove are configured with different curvatures and depths, and the upper guide groove is configured with a deeper structure.
8. The apparatus for testing rock fracture brittleness under non-uniform stress field of claim 1, wherein: The fixed base includes a fixed seat, a fastening groove is provided on the side of the fixed seat, a flat base is fixedly connected to the top of the fixed seat, the bottom of the fixed seat is connected to the bottom of the inner wall of the high-pressure oil chamber, and the bottom of the fixed seat is connected to an external constant negative pressure air source.
9. The apparatus for testing the brittleness of rock fracture under a non-uniform stress field according to claim 8, characterized in that: The planar base includes a pressing base, a limiting plate is fixedly connected to the top edge of the pressing base, an air extraction hole is opened on the top of the pressing base at one side of the limiting plate, and the bottom of the pressing base is fixedly connected to the top of the fixed base.
Citation Information
Patent Citations
Rock fracture testing apparatus and rock fracture testing method
CN113567255B