A method for on-line detection of laser shock peening defects

By extracting the attenuation segment features of acoustic emission signals using an adaptive amplitude thresholding method and a one-dimensional residual convolutional neural network, the problems of low detection accuracy and poor noise resistance in existing technologies are solved, and efficient online defect detection in the laser shock strengthening process is realized.

CN123155668APending Publication Date: 2026-11-24SHENYANG UNIVERSITY OF TECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611488869.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-23
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing online detection methods for laser shock peening defects rely on manually defined features, resulting in low detection accuracy and poor noise resistance, and are unable to adaptively mine deep defect information from acoustic emission signals.

Method used

An adaptive amplitude thresholding method is used to extract the feature sequence of acoustic emission signal attenuation segment during laser shock strengthening process, and a one-dimensional residual convolutional neural network is used for deep feature adaptive extraction to achieve end-to-end online defect detection.

Benefits of technology

It significantly improves the accuracy of defect identification and noise resistance, enabling accurate identification of internal defects in workpieces under strong background noise, and meeting the online inspection needs of industrial sites.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123155668A_ABST
    Figure CN123155668A_ABST
Patent Text Reader

Abstract

This invention provides an online detection method for defects induced by laser shock strengthening, relating to the interdisciplinary fields of laser shock strengthening and non-destructive testing. The method includes: real-time acquisition of transient high-frequency acoustic emission signals induced by laser shock waves; sequential downsampling, Hilbert transform, and Savitzky-Golay filtering smoothing of the original signal to extract the energy envelope; considering the strong pulse and rapid attenuation characteristics of the acoustic emission signal, and the obvious scattering modulation characteristics of defects such as cracks and holes in the attenuation segment, an adaptive amplitude threshold method is designed to automatically extract the attenuation segment containing the damage scattering mechanism as an independent feature sequence; this sequence is input into an improved one-dimensional residual convolutional neural network to accurately distinguish between normal, cracked, and hole-filled workpieces. This invention provides an efficient and stable technical path for online detection of defects induced by laser shock strengthening, significantly improving quality control and production efficiency in the processing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of laser shock peening and non-destructive testing, and in particular to an online detection method for defects in laser shock peening. Background Technology

[0002] Laser shock peening (LSP), an advanced surface modification technology, utilizes high-energy short-pulse laser-induced high-pressure plasma shock waves to generate significant plastic deformation and deep residual compressive stress fields on the surface and subsurface of materials. This technology can significantly improve the fatigue life and resistance to fretting wear of metallic materials and has been widely used in the strengthening treatment of key components such as aero-engine blades and turbine disks, making it one of the indispensable key processes in the aerospace manufacturing field.

[0003] However, the strengthening effect of LSP technology is highly dependent on the surface quality and internal structural integrity of the workpiece. If the workpiece surface has initial defects such as cracks or holes, the laser shock wave will undergo complex reflection, refraction, and scattering in the defect area. This not only fails to establish a uniform and beneficial residual compressive stress field but may also cause stress concentration, exacerbate surface roughness, and even lead to premature material failure during service. Existing countermeasures require each workpiece to undergo independent defect detection beforehand, and only those that pass the inspection can enter the LSP process. This undoubtedly increases the number of production steps and reduces efficiency. Therefore, simultaneously identifying initial defects of the workpiece online during LSP processing is of paramount engineering significance for ensuring process effectiveness and streamlining processes.

[0004] Currently, for quality monitoring in the LSP (Laser Stimulation Process), some studies have focused on collecting acoustic emission (AE) signals during laser shock and extracting statistical parameters such as sound pressure level factors. These parameters are then compared with preset standards to achieve closed-loop feedback control of the processing status. Alternatively, multiple sensors are placed on the sample surface, and the location of the sound source is inverted using the signal arrival time difference to monitor the working condition at the impact point. These methods all target defect-free normal workpieces and aim to improve the strengthening effect by optimizing process parameters. Their judgment logic is based on the overall intensity or time-domain statistics of the signal, and does not involve the active identification and classification of initial defects (such as cracks and holes) inside the workpiece.

[0005] For laser-induced emission (AE) detection of internal material defects, existing technologies attempt to divide the laser-excited AE filter signal into rising, stable, and decaying segments, defining the decaying oscillation energy as a single statistical feature to characterize defect information. While this method has achieved preliminary online defect identification, it still relies on manually defined shallow statistical indicators. In actual industrial settings, strong background noise and fluctuations in process parameters significantly affect the stability of manual features, resulting in insufficient sensitivity to minute defects and limited noise resistance of such methods. Summary of the Invention

[0006] This invention proposes an online detection method for laser shock strengthening defects, aiming to solve the problems of low detection accuracy, poor noise resistance, and inability to adaptively mine deep defect information in acoustic emission signals caused by existing online detection methods for laser shock strengthening defects due to reliance on manually defined features.

[0007] This invention provides an online detection method for laser shock peening defects, the method comprising the following steps: Step 1: During the laser shock hardening process, transient high-frequency acoustic emission signals are collected in real time by an acoustic emission sensor installed on the surface of the workpiece; Step 2: Downsample the acquired raw acoustic emission signal and extract a smooth signal energy envelope using envelope analysis. Step 3: Using the adaptive amplitude threshold method, with the global maximum amplitude of the smooth signal energy envelope as the benchmark, the moment when the envelope falls below the benchmark set percentage threshold for the last time after the peak is defined as the starting point of the attenuation segment, and a fixed length of data segment is extracted from this starting point as the feature sequence. Step 4: Perform data augmentation on the extracted feature sequence, and input the augmented feature sequence into a one-dimensional residual convolutional neural network for training to obtain a trained online defect detection model; Step 5: Input the feature sequence obtained in real time and processed in Step 2 and Step 3 into the online defect detection model. The model outputs the surface state classification result of the current workpiece to realize online detection of defects during laser shock strengthening.

[0008] Furthermore, the acoustic emission sensor mentioned in step 1 is an RS-2A type acoustic emission sensor with a frequency response range of 50-400kHz. During installation, high-vacuum silicone grease is applied as a coupling agent between the sensor and the workpiece surface.

[0009] Furthermore, the acoustic emission sensor mentioned in step 1 is connected in sequence to a preamplifier, an A / D data acquisition card, and an industrial control computer; the gain of the preamplifier is set to 40dB, and the sampling frequency of the A / D data acquisition card is set to 3MHz.

[0010] Furthermore, the downsampling process described in step 2 involves downsampling the original signal with a sampling rate of 3MHz to 1MHz at equal intervals; The envelope analysis method is as follows: Let the downsampled discrete-time signal be x(t), and perform a Hilbert transform on it to construct an analytic signal:

[0011] Analytical signal is represented as Take its modulus to obtain the transient energy envelope. :

[0012] The energy envelope is analyzed using a Savitzky-Golay filter. To perform smoothing and noise reduction, the specific parameter settings are: window width 51, polynomial fitting order 3.

[0013] Furthermore, the set ratio threshold mentioned in step 3 is 85% of the maximum amplitude; the fixed length is 4096 sampling points.

[0014] Furthermore, step 4 involves data augmentation of the truncated feature sequence, which includes a random combination of the following three operations: (1) Time shift enhancement by randomly cyclically shifting the position of the time sequence signal within a time window length of ±10%; (2) Noise addition processing by injecting Gaussian white noise with a mean of 0 and a standard deviation of 1% to 5% of the signal amplitude into the signal; (3) Randomly adjust the signal amplitude to 80% to 120% of the original amplitude range.

[0015] Furthermore, the one-dimensional residual convolutional neural network described in step 4 sequentially includes: an input layer, an initial convolutional block, at least one residual block, a global average pooling layer, and a fully connected output layer connected to the Softmax function; The initial convolutional block is composed of a one-dimensional convolutional layer, a batch normalization layer, and a ReLU activation function layer connected in sequence; the one-dimensional convolutional layer uses large stride convolution for feature downsampling. The residual blocks consist of two parts, each containing a main branch and a shortcut branch. The main branch comprises two consecutive one-dimensional convolutional layers with kernel sizes of 8 and 4 respectively, and a stride of 2 for each layer to achieve temporal downsampling. The shortcut branch uses a one-dimensional convolutional layer with a kernel size of 1×1 and a stride of 2 to align with the output of the main branch in terms of spatial scale and feature dimension. The outputs of the main branch and the shortcut branch are added element-wise through skip connections and activated by the ReLU activation function. The number of output channels for the two residual blocks are 128 and 256 respectively. The global average pooling layer performs temporal global aggregation on the high-order feature map output by the last residual block, calculates the mean of each feature channel at all time steps, and outputs a one-dimensional feature vector to the fully connected output layer. The number of Softmax nodes in the fully connected output layer is 3.

[0016] Furthermore, the training of the one-dimensional residual convolutional neural network in step 4 uses the Adam optimizer with an initial learning rate of 0.001, a batch size of 32, a maximum number of iterations of 100, and a loss function of multi-class cross-entropy.

[0017] Furthermore, the surface state of the workpiece in step 5 is classified into three categories: normal workpiece, cracked workpiece, and hole workpiece, corresponding to the three nodes of the Softmax of the fully connected output layer.

[0018] Compared with the prior art, the present invention has the following advantages: This invention fully utilizes the transient high-frequency acoustic emission signal excited during laser shock peening as a dynamic carrier for capturing changes in the microstructure of materials. On one hand, this invention abandons the traditional blind analysis or manual experience extraction of signals over the entire time period. Based on the physical mechanism of acoustic wave scattering and damping dissipation, it accurately locks and extracts the attenuation segment time sequence containing the richest defect information through an adaptive amplitude threshold method, making the feature mapping more focused and the physical meaning clear. On the other hand, this invention innovatively introduces a lightweight one-dimensional residual convolutional neural network to directly perform end-to-end deep nonlinear feature adaptive extraction on the enhanced one-dimensional attenuation segment time sequence signal. By deepening feature learning through cascaded residual blocks and using a global average pooling layer to significantly reduce model parameter redundancy, this method not only significantly improves the defect recognition accuracy and noise robustness of acoustic emission signals under strong background noise interference, but also has extremely efficient model computation and extremely fast forward inference, perfectly meeting the engineering deployment requirements for online detection of initial defects in workpieces in industrial settings.

[0019] Based on the implementation methods provided in the above aspects, this application can be further combined to provide more implementation methods. Attached Figure Description

[0020] The above and other objects, features, and advantages of exemplary embodiments of the present invention will become readily apparent upon reading the following detailed description with reference to the accompanying drawings. In the drawings, several embodiments of the invention are illustrated by way of example and not limitation, with the same or corresponding reference numerals denoteing the same or corresponding parts, wherein: Figure 1 A flowchart of an online detection method for laser shock strengthening defects provided by the present invention; Figure 2 This is a schematic diagram of the installation of the acoustic emission sensor and the acquisition of acoustic emission signals inside the workpiece during the laser shock strengthening process in this embodiment of the invention; Figure 3 The shapes and dimensions of the metal material to be impact-processed in this embodiment of the invention are shown; where a is a front view and b is a top view. Figure 4 These are time-domain waveforms of the acoustic emission signal before and after preprocessing in an embodiment of the present invention; where a is the time-domain waveform of the original acoustic emission signal and b is the time-domain waveform of the preprocessed acoustic emission signal. Figure 5 The attenuation range of the acoustic emission signal extracted in the embodiments of the present invention is shown in the figure. Here, a is the signal diagram of a normal workpiece, b is the signal diagram of a cracked workpiece, and c is the signal diagram of a workpiece with holes. Figure 6 This is a network structure diagram of a one-dimensional residual convolutional neural network model in an embodiment of the present invention; Figure 7 This is a confusion matrix diagram of a one-dimensional residual convolutional neural network model in an embodiment of the present invention; Figure 8 This is a noise-resistant histogram of a one-dimensional residual convolutional neural network model in an embodiment of the present invention.

[0021] In the diagram: 1. Industrial computer; 2. A / D data acquisition card; 3. Preamplifier; 4. Workpiece; 5. Acoustic emission sensor; 6. Water confinement layer; 7. Black tape absorption layer; 8. Laser shock reinforcement area; 9. Pre-fabricated defect. Detailed Implementation

[0022] Exemplary embodiments disclosed in this application will now be described in more detail with reference to the accompanying drawings. While exemplary embodiments of this application are shown in the drawings, it should be understood that this application can be implemented in various forms and should not be limited to the embodiments set forth herein. Rather, these embodiments are provided to enable a more thorough understanding of this application and to fully convey the scope of this application to those skilled in the art. Unless otherwise specified, the technical means used in the embodiments are conventional means well known to those skilled in the art.

[0023] Among numerous non-destructive testing technologies, acoustic emission (AE) stands out due to its extremely high dynamic response sensitivity. This invention selects AE as a defect detection technology, which can capture in real time the transient high-frequency acoustic emission signals excited by shock waves propagating within materials. The entire AE detection system consists of an industrial control computer 1, an A / D data acquisition card 2, a preamplifier 3, and an AE sensor 5. The industrial control computer 1 stores and analyzes the data, the A / D data acquisition card 2 acquires the data, the sampling frequency is set to 3MHz, and the preamplifier 3's amplification gain is set to 40dB for signal amplification and noise reduction. The selected AE sensor 5 is an RS-2A type sensor.

[0024] like Figure 1 As shown, the present invention provides an online detection method for laser shock peening defects, the method comprising the following steps: Step 1: During the laser shock hardening process, transient high-frequency acoustic emission signals are collected in real time by an acoustic emission sensor installed on the surface of the workpiece.

[0025] Specifically, the acoustic emission sensor is connected in sequence to a preamplifier 3, an A / D data acquisition card 2, and an industrial control computer 1; the gain of the preamplifier 3 is set to 40dB, and the sampling frequency of the A / D data acquisition card 2 is set to 3MHz; wherein, the acoustic emission sensor 2 is an RS-2A type acoustic emission sensor with a frequency response range of 50-400kHz and a center frequency of 150kHz; during installation, high-vacuum silicone grease is applied as a coupling agent between the sensor and the workpiece surface.

[0026] Step 2: Downsample the acquired raw acoustic emission signal and extract a smooth signal energy envelope using envelope analysis.

[0027] Specifically, in step 2, the original acoustic emission signal is downsampled according to the Nyquist sampling theorem. The downsampling process is to downsample the original signal with a sampling rate of 3MHz to 1MHz at equal intervals. The envelope analysis method is a time-domain processing technique for extracting the effective physical features of transient acoustic emission signals. It can define the effective feature interval and improve detection efficiency.

[0028] Let the downsampled discrete-time signal be x(t), and perform a Hilbert transform on it to construct an analytic signal:

[0029] Analytical signal is represented as Take its modulus to obtain the transient energy envelope. :

[0030] The energy envelope is analyzed using a Savitzky-Golay filter. Smoothing and denoising were performed, with a window width of 51 and a polynomial fitting order of 3. This step effectively filtered out high-frequency noise spikes and reconstructed a smooth trend line reflecting the evolution of transient impact energy.

[0031] Step 3: Using the adaptive amplitude threshold method, with the global maximum amplitude of the smooth signal energy envelope as the benchmark, the moment when the envelope falls below the benchmark set percentage threshold for the last time after the peak is defined as the starting point of the attenuation segment, and a fixed length of data segment is extracted from this starting point as the feature sequence. Specifically, during laser shock peening, when elastic waves propagate inside the workpiece, they encounter cracks or holes, resulting in significant mode conversion, scattering, and damping dissipation. These physical characteristics are highly concentrated in the signal decay oscillation phase. This step employs an adaptive amplitude threshold method to define the characteristic interval. This method can avoid strong background interference from the initial main energy burst region of the laser shock and extract the attenuation segment information of the acoustic emission waveform: First, the global maximum amplitude of the smooth envelope is optimized; then, searching behind the peak, the moment when the envelope last drops below 85% of the maximum amplitude is defined as the starting point of the characteristic attenuation segment. From this starting point, a one-dimensional acoustic emission data segment of a fixed length of 4096 sampling points is uniformly extracted. This segment is the effective characterization space for mapping internal micro-defects. This space contains the characteristic acoustic impedance fluctuations induced by waveform mode conversion, scattering, and damping dissipation when the shock wave passes through the interface of cracks and holes.

[0032] Step 4: Perform data augmentation on the extracted feature sequence, and input the augmented feature sequence into a one-dimensional residual convolutional neural network for training to obtain a trained online defect detection model.

[0033] Specifically, to address the complex random disturbances in industrial settings and improve the model's generalization robustness, the extracted feature attenuation segments are subjected to the following random combination of data augmentation operations to construct a training sample set. These data augmentation methods include: Time-shift enhancement is applied to the timing signal by random cyclic position offset within a time window length of ±10%. Noise addition processing: injecting Gaussian white noise with a mean of 0 and a standard deviation of 1% to 5% of the signal amplitude into the signal; And amplitude scaling operations that randomly adjust the signal amplitude to 80% to 120% of the original range.

[0034] A one-dimensional residual convolutional neural network is built within the TensorFlow / Keras framework. This network sequentially comprises: an input layer, an initial convolutional block, at least one residual block, a global average pooling layer, and a fully connected output layer connected to a Softmax function, constructing a lightweight end-to-end network architecture. Specifically: The input layer is a one-dimensional signal with a length of 4096 and a channel number of 1.

[0035] The initial convolutional block consists of a one-dimensional convolutional layer, a batch normalization layer, and a ReLU activation function layer connected in sequence. The one-dimensional convolutional layer has a kernel size of 16, a channel number of 64, and a stride of 2.

[0036] Each of the two residual blocks contains a main branch and a shortcut branch. The main branch consists of two consecutive one-dimensional convolutional layers with kernel sizes of 8 and 4 respectively, and a stride of 2 for both layers to achieve temporal downsampling. The shortcut branch uses a one-dimensional convolutional layer with a kernel size of 1×1 and a stride of 2 to align with the output of the main branch in terms of spatial scale and feature dimension. The outputs of the main branch and the shortcut branch are added element-wise through skip connections and activated by the ReLU activation function. The number of output channels for the two residual blocks are 128 and 256 respectively. The global average pooling layer performs temporal global aggregation on the high-order feature map output by the last residual block, calculates the mean of each feature channel at all time steps, and outputs a one-dimensional feature vector to the fully connected output layer. The fully connected output layer has 3 Softmax nodes, corresponding to the three categories of workpiece surface states: normal workpiece, cracked workpiece, and holed workpiece.

[0037] The training of the one-dimensional residual convolutional neural network uses the Adam optimizer with an initial learning rate of 0.001, a batch size of 32, a maximum number of iterations of 100, and a loss function of multi-class cross-entropy. The total number of network parameters is only 637,123, which has excellent lightweight characteristics.

[0038] Step 5: Input the feature sequence obtained in real time and processed in Step 2 and Step 3 into the online defect detection model. The model outputs the surface state classification result of the current workpiece to realize online detection of defects during laser shock strengthening.

[0039] Specifically, the weights of the trained, qualified one-dimensional residual convolutional neural network model are fixed and deployed to the industrial control computer 1 of the on-site laser shock enhancement control system. During continuous processing, preprocessing and adaptive truncation are performed in real time, and the extracted millisecond-level attenuation segment data is directly fed into the model. The model performs rapid forward inference calculations and outputs the classification results of the current processing area simultaneously with processing, accurately indicating whether the workpiece is a normal workpiece, a workpiece with holes, or a cracked workpiece, thereby completely replacing the traditional offline flaw detection process.

[0040] Since the acoustic emission generated by laser shock peening is a strong pulse signal with strong attenuation characteristics, and defects such as cracks and holes exhibit obvious scattering modulation features in the attenuation range, the attenuation range of the signal is extracted and used as a feature input to a one-dimensional residual convolutional neural network for classification and recognition, thereby achieving online detection of defects generated by laser shock peening.

[0041] Example

[0042] like Figure 2 The diagram shown illustrates the installation and connection of the workpiece to be impacted and the acoustic emission acquisition system in this embodiment. The acoustic emission defect detection system, consisting of an industrial control computer 1, an A / D data acquisition card 2, a preamplifier 3, and an acoustic emission sensor 5, is set to a sampling rate of 3MHz. The laser shock process parameters used in this embodiment are: single-pulse laser energy of 6J, square spot side length of 4mm, processing frequency of 1Hz, laser pulse width of 15ns, constraint layer 6 being stable deionized water, and energy absorption layer 7 being black tape. In this embodiment, the processing path for the workpiece to be impacted is selected as S-shaped, with an overlap rate of 50%.

[0043] like Figure 3 The diagram shown illustrates the shape and size of the workpiece 4 to be impacted in this embodiment. Figure 3 (a) is the front view of the workpiece. Figure 3 (b) is a top view of the workpiece; the workpiece used in this embodiment is a hollow cylinder of 7075 aluminum alloy with an outer diameter of 150 mm and an inner diameter of 110 mm, which is wire-cut into a 6-part curved surface with a height of 30 mm. The effectiveness of the proposed method is verified by pre-fabricating defects 9 on the workpiece surface to simulate defects during processing. The acoustic emission sensor 5 is located at the middle position of the outer surface of the workpiece, and the pre-fabricated defect 9 is located between the laser shock strengthening region 8 and the acoustic emission sensor 5.

[0044] In this embodiment, the acoustic emission sensor 5 is correctly arranged as required, and industrial coupling agent and fixtures are used to ensure that the sensor fits tightly and does not wobble during laser processing. Subsequently, before laser shock hardening, a lead-breaking test is performed on the workpiece to ensure that the acoustic emission detection system can collect signals normally.

[0045] In this embodiment, after the acoustic emission sensor 5 is arranged on the workpiece 4 to be impacted as required, the acoustic emission signal of the laser shock is synchronously acquired by the acoustic emission detection system. After determining the maximum frequency component of the acoustic emission signal, the sampling rate of the acoustic emission signal is reduced from 3MHz to 1MHz. Subsequently, a Hilbert transform is performed to construct an analytical signal, and its magnitude is extracted as a transient energy envelope reflecting the energy evolution trend. The energy envelope is then smoothed and denoised using a Savitzky-Golay filter. Figure 4 The figure shows the time-domain waveforms of the original acoustic emission signal and the preprocessed acoustic emission signal.

[0046] like Figure 5 The attenuation interval shown in this embodiment is extracted using the adaptive amplitude threshold method, wherein... Figure 5 (a) is a normal workpiece. Figure 5 (b) is a cracked workpiece. Figure 5 (c) is a workpiece with holes. The waveform of a normal workpiece is a smooth, exponentially decaying long tail; the waveform of a cracked workpiece is characterized by high-frequency burrs, and the energy decays rapidly in the early stage; while the waveform of a workpiece with holes shows multiple amplitude rebounds and continuous long-range oscillations in the middle and late stages.

[0047] In this embodiment, the structure of the constructed one-dimensional residual convolutional neural network is as follows: Figure 6 As shown in Table 1, where a is the acoustic emission signal, b is the input layer, c is the convolutional layer, d is residual layer 1, e is residual layer 2, f is the global average pooling layer, and g is the output layer. The hyperparameter table corresponding to this one-dimensional residual convolutional neural network is shown in Table 1, and its model structure is shown in Table 2. The hyperparameter settings are gradually established during network training, but are not unique solutions; other similar hyperparameter settings are considered extensions of this invention. The selection and placement order of network layers are not unique; other similar network stackings are considered extensions of this invention.

[0048] Table 1 shows the hyperparameters of the one-dimensional residual convolutional neural network model.

[0049] Table 2 shows the structure of a one-dimensional residual convolutional neural network model.

[0050] In this embodiment, laser shock peening was performed on normal workpieces, cracked workpieces, and workpieces with holes, with 800 samples collected for each category. The samples were divided into training and testing sets in an 8:2 ratio. Data augmentation was applied to the training set to improve the model's generalization ability under complex conditions and to expand the sample size for the three workpiece states, resulting in 5760 samples input into the network for training. The testing set consisted of 480 samples (160 per class) as completely independent, un-augmented real test data. The confusion matrix is ​​used as a form of accuracy evaluation for classification problems; the model's classification performance can be evaluated by observing the diagonal of the confusion matrix. The confusion matrix results are shown below. Figure 7 As shown, the model's predictions are highly concentrated on the main diagonal, with only 5 extremely rare local misjudgments, demonstrating its ability to accurately distinguish the characteristics of weak and complex acoustic emission signals.

[0051] In this embodiment, to further verify the noise resistance performance of the proposed one-dimensional residual convolutional neural network model in complex industrial environments, Gaussian white noise of different intensities was introduced into the acoustic emission signal for comparative experiments. The noise intensity was quantified using the signal-to-noise ratio (SNR), which is defined as follows:

[0052] In the formula, Ps represents the signal power; Pn represents the noise power. The signal-to-noise ratios were set to 20dB, 15dB, 10dB, and 5dB, and the specific noise immunity test results are as follows: Figure 8 As shown, under operating conditions of 20dB to 10dB, the model's classification accuracy remained between 95.83% and 98.54%. Furthermore, even under strong noise interference conditions with an SNR as low as 5dB, the model still maintained an effective recognition rate of 80.42%. This demonstrates that the one-dimensional residual convolutional neural network model proposed in this invention can effectively overcome strong background noise interference in complex industrial environments, exhibiting outstanding noise robustness and reliability, and meeting the online detection needs of actual workshops.

[0053] The above description is merely a specific embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in the present invention should be included within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be determined by the scope of the claims.

Claims

1. A method for on-line detection of defects in laser shock peening, characterized in that, The method includes the following steps: Step 1: During the laser shock hardening process, transient high-frequency acoustic emission signals are collected in real time by an acoustic emission sensor installed on the surface of the workpiece; Step 2: Downsample the acquired raw acoustic emission signal and extract a smooth signal energy envelope using envelope analysis. Step 3: Using the adaptive amplitude threshold method, with the global maximum amplitude of the smooth signal energy envelope as the benchmark, the moment when the envelope falls below the benchmark set percentage threshold for the last time after the peak is defined as the starting point of the attenuation segment, and a fixed length of data segment is extracted from this starting point as the feature sequence. Step 4: Perform data augmentation on the extracted feature sequence, and input the augmented feature sequence into a one-dimensional residual convolutional neural network for training to obtain a trained online defect detection model; Step 5: Input the feature sequence obtained in real time and processed in Step 2 and Step 3 into the online defect detection model. The model outputs the surface state classification result of the current workpiece to realize online detection of defects during laser shock strengthening.

2. The method according to claim 1, wherein The acoustic emission sensor mentioned in step 1 is an RS-2A type acoustic emission sensor with a frequency response range of 50-400kHz. During installation, high-vacuum silicone grease is applied as a coupling agent between the sensor and the workpiece surface.

3. The method according to claim 1, wherein In step 1, the acoustic emission sensor is connected in sequence to a preamplifier, an A / D data acquisition card, and an industrial control computer; the gain of the preamplifier is set to 40dB, and the sampling frequency of the A / D data acquisition card is set to 3MHz.

4. The method according to claim 1, wherein The downsampling process described in step 2 involves downsampling the original signal with a sampling rate of 3MHz to 1MHz at equal intervals. The envelope analysis method is as follows: Let the down-sampled discrete-time signal be Perform a Hilbert transform on it to construct the analytic signal: Analytical signal is represented as Take its modulus to obtain the transient energy envelope. : The energy envelope is analyzed using a Savitzky-Golay filter. To perform smoothing and noise reduction, the specific parameter settings are: window width 51, polynomial fitting order 3. Where PV represents the Cauchy principal value, τ is the integration variable, t is the time variable, y(t) is the transformed output signal, and the coefficients are... This is the normalization constant.

5. The online detection method for laser shock peening defects according to claim 1, characterized in that, The set ratio threshold in step 3 is 85% of the maximum amplitude; the fixed length is 4096 sampling points.

6. The online detection method for laser shock peening defects according to claim 1, characterized in that, Step 4 involves data augmentation of the truncated feature sequence, which includes at least one random combination of the following three operations: (1) Time shift enhancement by randomly cyclically shifting the position of the time sequence signal within a time window length of ±10%; (2) Noise addition processing by injecting Gaussian white noise with a mean of 0 and a standard deviation of 1% to 5% of the signal amplitude into the signal; (3) Randomly adjust the signal amplitude to 80% to 120% of the original amplitude range.

7. The online detection method for laser shock peening defects according to claim 1, characterized in that, The one-dimensional residual convolutional neural network described in step 4 sequentially includes: an input layer, an initial convolutional block, at least one residual block, a global average pooling layer, and a fully connected output layer connected to the Softmax function; The initial convolutional block is composed of a one-dimensional convolutional layer, a batch normalization layer, and a ReLU activation function layer connected in sequence; the one-dimensional convolutional layer uses large stride convolution for feature downsampling. The residual blocks consist of two parts, each containing a main branch and a shortcut branch. The main branch comprises two consecutive one-dimensional convolutional layers with kernel sizes of 8 and 4 respectively, and a stride of 2 for each layer to achieve temporal downsampling. The shortcut branch uses a one-dimensional convolutional layer with a kernel size of 1×1 and a stride of 2 to align with the output of the main branch in terms of spatial scale and feature dimension. The outputs of the main branch and the shortcut branch are added element-wise through skip connections and activated by the ReLU activation function. The number of output channels for the two residual blocks are 128 and 256 respectively. The global average pooling layer performs temporal global aggregation on the high-order feature map output by the last residual block, calculates the mean of each feature channel at all time steps, and outputs a one-dimensional feature vector to the fully connected output layer. The number of Softmax nodes in the fully connected output layer is 3.

8. The online detection method for laser shock peening defects according to claim 1, characterized in that, The training of the one-dimensional residual convolutional neural network in step 4 uses the Adam optimizer with an initial learning rate of 0.001, a batch size of 32, a maximum number of iterations of 100, and a loss function of multi-class cross-entropy.

9. The online detection method for laser shock peening defects according to claim 1, characterized in that, In step 5, the surface condition of the workpiece is classified into three categories: normal workpiece, cracked workpiece, and hole workpiece, corresponding to the three nodes of the Softmax of the fully connected output layer.