Optical laminate, optical film product obtained from the optical laminate, and method for manufacturing the optical film product
By setting colored marking lines parallel to the optical axis in the optical laminate, the problem of face-back identification and optical axis alignment of small-sized optical film products is solved, improving the bonding efficiency and accuracy of optical film products for wearable displays.
Patent Information
- Application Number
- CN202610706315.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-21
- Filing Date
- 2026-05-21
- Publication Date
- 2026-11-24
AI Technical Summary
Existing technologies make it difficult to accurately distinguish the front and back of very small optical film products, especially in VR and AR wearable displays, which leads to difficulties in the positional relationship and optical axis alignment of optical film products.
At least one of the optical laminates is colored and a marking line is formed on it. The marking line extends parallel to the optical axis of the optical film, and the optical film product is formed by laser cutting into small pieces.
It enables accurate front-back identification and optical axis alignment for very small-sized optical film products, improving the bonding efficiency and accuracy of optical film products in wearable displays.
Smart Images

Figure CN123156340A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to an optical laminate, an optical film product obtained from the optical laminate, and a method for manufacturing the optical film product. Background Technology
[0002] Optical films such as polarizers, retardation films, and optical compensation films, as well as optical laminates including these optical films, are important optical components for enabling image display devices to function properly. Such optical films and optical laminates are typically cut from sheet-like, strip-like, or roll-like raw materials to form optical film products of specified dimensions for use in image display devices. For the optical film product (which, in effect, is the image display device) to function properly, the positional relationship (arrangement order) of the polarizer (essentially the polarizer contained within the polarizer), retardation film, etc., relative to the optical component (e.g., the image display panel) to which the optical film product is bonded, and the axial angles of the optical axes such as the absorption axis of the polarizer and the slow axis of the retardation film, are important. Therefore, determining the front and back of the optical film product is crucial for its proper functioning and bonding with the optical component. For example, Patent Document 1 proposes a technique that uses laser processing to apply markings to the knurling portion of the optical film to determine its front and back. For example, Patent Document 2 proposes a technique that uses a punching die with engraved blades in certain areas to punch out an optical film from a raw material roll.
[0003] Furthermore, in recent years, VR (Virtual Reality) and AR (Augmented Reality) technologies have garnered significant attention. VR is a technology that simulates and experiences computer-generated 3D spaces in a way that resembles reality; AR is a technology that "virtually enhances" the world by overlaying virtual visual information onto real-world scenes. Alongside the development of VR and AR, the development of goggles (VR goggles, AR glasses) and wearable displays such as head-mounted displays (HMDs) is progressing. Optical film products can also become important optical components in such wearable displays. Here, optical film products that can be used in wearable displays can typically be extremely small in size, less than 10mm vertically and less than 10mm horizontally. Therefore, a technology capable of accurately identifying the back of such extremely small optical film products is required.
[0004] Existing technical documents Patent documents Patent Document 1: Japanese Patent Application Publication No. 2003-114328 Patent Document 2: Japanese Patent Application Publication No. 2007-187781 Summary of the Invention
[0005] The main objective of this invention is to provide an optical laminate, which is a raw material roll of an optical film product with a very small size, and can accurately distinguish the front and back of the obtained optical film product.
[0006] [1] An optical laminate according to an embodiment of the present invention comprises: an optical film; a surface protective film temporarily bonded to one side of the optical film in a peelable manner; an adhesive layer disposed on the other side of the optical film; and a release liner temporarily bonded to the adhesive layer in a peelable manner; at least one of the surface protective film or the release liner is colored; an identification line is formed on one of the surface protective film or the release liner; when the optical laminate is miniaturized to produce an optical film product, the identification line is formed to be included in all optical film products.
[0007] [2] In [1] above, the marking line is formed as a stripe extending in a direction parallel to the optical axis of the optical film, and the marking line is formed to include one in each of the optical film products.
[0008] [3] In [1] or [2] above, one of the above-mentioned surface protective film or the above-mentioned release liner is black and opaque.
[0009] [4] In any of [1] to [3] above, the surface protective film is black and opaque, and the marking line is formed on the peeling pad and the marking line is red.
[0010] [5] In any of [1] to [3] above, the surface protective film is black and opaque, and the marking line is formed on the surface protective film, and the marking line is a light color that can be distinguished from black.
[0011] [6] According to another aspect of the present invention, a method for manufacturing an optical film product is provided. The method includes miniaturizing an optical laminate as described in any one of [1] to [5] above.
[0012] [7] In [6] above, the miniaturization includes cutting the optical laminate by laser irradiation.
[0013] [8] According to another aspect of the present invention, an optical film product is provided. The optical film product comprises: an optical film; a surface protective film temporarily adhered to one side of the optical film in a peelable manner; an adhesive layer disposed on the other side of the optical film; and a release liner temporarily adhered to the adhesive layer in a peelable manner; the optical film product is rectangular in shape with a longitudinal length of less than 10 mm and a transverse length of less than 10 mm; at least one of the surface protective film or the release liner is colored; and a marking line is formed on one of the surface protective film or the release liner.
[0014] [9] In [8] above, the direction of extension of the marking line is parallel to the optical axis of the optical film.
[0015] Invention Effects According to an embodiment of the present invention, an optical laminate can be realized, which is a raw material roll of an optical film product with a very small size, and the front and back of the obtained optical film product can be accurately identified. Attached Figure Description
[0016] Figure 1 This is a schematic cross-sectional view of an optical laminate according to one embodiment of the present invention.
[0017] Figure 2 This is a schematic diagram illustrating a method for manufacturing an optical film product according to one embodiment of the present invention.
[0018] Explanation of reference numerals in the attached figures 10: Optical film; 20: Surface protective film; 21: Substrate; 22: PF adhesive layer; 30: Adhesive layer; 40: Release liner; 50: Marking line; 100: Optical laminate; 110: Optical film product. Detailed Implementation
[0019] Hereinafter, specific embodiments of the present invention will be described with reference to the accompanying drawings, but the present invention is not limited to these embodiments. It should be noted that the drawings are shown schematically for ease of observation, and the ratios of length, width, thickness, etc., as well as angles, etc., in the drawings differ from the actual figures.
[0020] A. Optical laminate A-1. Overview of Optical Laminates Figure 1 This is a schematic cross-sectional view of an optical laminate according to one embodiment of the present invention; Figure 2 This is a schematic diagram illustrating a method for manufacturing an optical film product according to one embodiment of the present invention, including... Figure 1A schematic top view of an optical laminate. The illustrated optical laminate 100 includes: an optical film 10; a surface protective film 20 temporarily adhered to one side of the optical film 10 in a peelable manner; an adhesive layer 30 disposed on the other side of the optical film 10; and a release liner 40 temporarily adhered to the adhesive layer 30 in a peelable manner. In actual use of the optical laminate 100 (essentially an optical film product 110 obtained by miniaturizing the optical laminate), the release liner 40 is peeled off, and the adhesive layer 30 can be used to bond the optical laminate 100 (essentially the optical film product 110) to an image display device (essentially an optical component of an image display device such as an image display panel or a polarizing beam splitter). Typically, the surface protective film 20 has a substrate 21 and an adhesive layer 22. It should be noted that, to distinguish it from the adhesive layer 30, the adhesive layer 22 of the surface protective film is sometimes referred to as the "PF adhesive layer." The surface protective film 20 is also peeled off during actual use of the optical film product.
[0021] In embodiments of the present invention, at least one of the surface protective film 20 or the release liner 40 is colored. That is, either the surface protective film or the release liner may be colored. Furthermore, depending on the configuration of the optical laminate, sometimes both the surface protective film and the release liner may be optionally colored. The illustrated example shows the case where the surface protective film is colored. In the case where the surface protective film is colored, the substrate 21 is essentially colored. Hereinafter, the colored surface protective film or the release liner may be referred to as a colored film.
[0022] The method of coloring (typically color, transparency, or transmittance) can be any suitable method as long as the effects of the embodiments of the present invention are achieved. Dark colors are representative examples of colors to be colored. Specific examples of dark colors include black, blue, purple, and red. Black is preferred. This is because the surface protective film (substrate) or release liner is easy to color, and it is easy to distinguish the front and back of the optical film product obtained from the optical laminate. The transmittance of the colored film is preferably 20% or less, more preferably 18% or less, further preferably 15% or less, particularly preferably 12% or less, and especially preferably 10% or less. With such a configuration, the front and back of optical film products of very small dimensions obtained from the optical laminate can be distinguished. The lower the transmittance of the colored film, the more preferred it is; for example, its lower limit can be zero. The lower the transmittance of the colored film, the easier it is to distinguish the front and back of the optical film product obtained from the optical laminate, and it is possible to distinguish the front and back of even smaller optical film products. It should be noted that even when the optical laminate includes a polarizer (a film with a single-unit transmittance of approximately 40% to 45%), it is difficult to distinguish the back of very small-sized optical film products. On the other hand, as described above, by reducing the transmittance of the colored film, the back of very small-sized optical film products can be distinguished. The colored film can be, for example, black and opaque (e.g., transmittance of less than 1%). If such a configuration is used, the aforementioned discrimination effect can become more significant. The non-colored surface protective film or release liner can typically be colorless and transparent (transmittance of, for example, 70% or more, and further, for example, 80% or more, and further, for example, 90% or more). It should be noted that in this specification, "able to distinguish the back of the optical film product" means that the back of the optical film product can be distinguished by visual inspection (i.e., without the use of special equipment).
[0023] Furthermore, in embodiments of the present invention, a marking line 50 is formed on either the surface protective film 20 or the release liner 40. The marking line 50 is typically formed by printing. The marking line 50 can be formed on a colored film, or on a surface protective film or release liner that is not a colored film, as long as it is identifiable. The illustrated example shows the case where the marking line is formed on a release liner that is not a colored film. Figure 2 As shown, when the optical laminate 100 is miniaturized to form the optical film product 110, the marking line 50 is formed to be included in all optical film products. With this configuration, the front and back of the optical film products with very small dimensions can be easily distinguished. The marking line 50 is typically formed to be included in each optical film product.
[0024] The marking line 50 is typically formed to extend in a direction parallel to the optical axis of the optical film. With this configuration, not only can the front and back of very small optical film products be easily identified, but also the position and optical axis alignment of the optical film product can be easily performed when it is bonded to the optical components of an image display device. It should be noted that the "optical axis of the optical film" refers to the axis in which light does not separate even when light is incident on it, in an optical film with optical anisotropy. Specifically, in the case of a polarizer, it is the absorption axis (or the transmission axis orthogonal to the absorption axis); in the case of a retardation film, it is the slow axis (or the fast axis orthogonal to the slow axis). In the case of a laminated optical film, the optical film can have more than two optical axes. In the case of a circular polarizer, for example, a polarizer and a quarter-plate laminated together, the circular polarizer has two optical axes (absorption axis and slow axis). The direction in which the marking line extends is set to be parallel to which optical axis can be appropriately determined according to the purpose. More specifically, when bonding an optical film product to the optical components of an image display device, the direction in which the marking line extends can be set so that the position of the optical film product and the direction of the optical axis are aligned most easily. Therefore, regarding the direction in which the marking line extends, for example, if the optical film is a polarizer, it can be set to be parallel to the absorption axis or parallel to the transmission axis; for example, if the optical film is a retardation film, it can be set to be parallel to the slow axis or parallel to the fast axis; for example, if the optical film is a circular polarizer (including a laminate of a polarizer and a quarter plate), it can be set to be parallel to the absorption axis, parallel to the transmission axis, parallel to the slow axis, or orthogonal to the slow axis.
[0025] Marking line 50 is representative of Figure 2 The pattern shown is striped. With this configuration, the marking line 50 can be configured such that one is included in each of the optical film products 110, and the direction in which the marking lines of all the optical film products extend can be uniform.
[0026] The color of the marking line 50 can be appropriately set according to the color of the coloring film and the constituent elements of the optical laminate on which the marking line is formed. In essence, any suitable color can be used as the marking line color, as long as it is recognizable in relation to the coloring film. For example, if the surface protective film 20 is a black opaque coloring film and the marking line is formed on the release liner 40, the marking line can be red. This configuration offers excellent versatility and makes the marking line easily identifiable. Furthermore, for example, if the surface protective film 20 is a black opaque coloring film and the marking line is formed on the surface protective film, the marking line can be a light color that is distinguishable from black. Specific examples of light colors include white, light blue, yellow, and pink. White is preferred. This configuration also offers excellent versatility and makes the marking line easily identifiable.
[0027] The optical laminate 100 can be in the form of a single sheet or a strip. A strip-shaped optical laminate can be wound into a roll. The optical laminate is preferably in the form of a single sheet. Since the optical laminate is a raw material roll for optical film products with very small dimensions (e.g., less than 10 mm in length and less than 10 mm in width), large-scale roller conveying is unnecessary. Furthermore, as described later, the miniaturization of the optical laminate (manufacturing of optical film products) is typically performed by laser irradiation; therefore, the optical laminate is preferably a single sheet of a size suitable for laser irradiation (scanning) that corresponds to the size (shape) of the optical film product. For example, the optical laminate can have dimensions of approximately 150 mm to 250 mm in length and approximately 250 mm to 350 mm in width.
[0028] The following is a detailed explanation of the constituent elements of optical laminates.
[0029] A-2. Optical film The optical film 10 can be a film composed of a single layer or a laminate. Specific examples of optical films composed of a single layer include window films, polarizers, and retardation films. Specific examples of optical films composed of a laminate include polarizing plates (representatively a laminate of a polarizer and a protective film), conductive films for touch panels, surface-treated films, and laminates obtained by appropriately stacking these single-layer optical films and / or optical films composed of a laminate according to the purpose (e.g., circular polarizing plates for anti-reflection, polarizing plates with surface-treated films).
[0030] A-3. Surface protective film The surface protective film 20, as described above, typically comprises a substrate 21 and a PF adhesive layer 22. The substrate 21 can be made of any suitable material. Specific examples of the constituent materials include: polyester polymers such as polyethylene terephthalate (PET), polyethylene naphthalate (PEN), and polybutylene terephthalate (PBT); cellulose polymers such as diacetylcellulose and triacetylcellulose; polycarbonate polymers; (meth)acrylic polymers such as polymethyl methacrylate; and cyclic olefin polymers such as polynorbornene. These can be used individually or in combination. Polyester polymers are preferred, and materials with excellent optical properties (e.g., transparency), mechanical strength, thermal stability, moisture shielding, isotropy, flexibility, and dimensional stability are particularly desirable. From this perspective, polyester polymers are preferred as the constituent material of the substrate, and PET is more preferred. The properties of the polyester polymer film can be controlled by adjusting the type and combination of the polycarboxylic acid component and the polyol component. For example, PET and PBT can also be used in combination as the constituent material of the substrate.
[0031] Other examples of constituent materials used as substrates include: styrene-based polymers such as polystyrene and acrylonitrile-styrene copolymers; vinyl chloride-based polymers; amide-based polymers such as nylon 6, nylon 6,6, and aromatic polyamides; imide-based polymers; sulfone-based polymers; polyethersulfone-based polymers; polyetheretherketone-based polymers; polyphenylene sulfide-based polymers; vinyl alcohol-based polymers; vinylidene chloride-based polymers; vinyl butyral-based polymers; aromatic ester-based polymers; polyoxymethylene-based polymers; and epoxy-based polymers. These can be used individually or in combination of two or more.
[0032] In one embodiment, the substrate may also have a laminated structure of resin layer / adhesive layer / resin layer. The constituent materials of the resin layer include those described above as constituent materials of the substrate. The constituent materials of the adhesive layer include adhesives, binders, and tackifying coatings. The adhesive layer may also have a laminated structure of an adhesive layer or a binder layer and a tackifying coating. By sandwiching an adhesive layer with specified properties (e.g., elastic modulus) between two resin layers, the elastic modulus (e.g., tensile elastic modulus) can be reduced to a desired degree corresponding to the purpose.
[0033] The tensile modulus of the substrate 21 is, for example, 2.3 × 10⁻⁶. 9 Pa below, preferably 1.5 × 10 Pa 9 Pa or less, more preferably 1.3 × 10 Pa. 9 Pa below, more preferably 1.0 × 10 Pa 7 Pa ~ 1.3 × 10 9 Pa, preferably 1.0 × 10 Pa. 8 Pa ~ 1.3 × 109 Pa. It should be noted that the tensile modulus of elasticity was determined according to JIS K 7161.
[0034] In one embodiment, the thickness of the substrate is, for example, 20 μm to 100 μm, or more specifically, 25 μm to 80 μm, or even 30 μm to 50 μm. If the substrate thickness is within this range, poor peeling during the removal of the surface protective film can be prevented very well. In another embodiment, the substrate thickness can, for example, be 60 μm to 90 μm. If the substrate thickness is within this range, poor peeling can be appropriately suppressed, and dents can be well suppressed.
[0035] When the surface protective film is a colored film, as described above, the substrate is essentially colored. The substrate can be colored in any suitable manner. Specific examples of coloring methods are as follows: (1) forming a film (substrate) by molding a constituent material containing a coloring material (e.g., pigment); (2) dyeing a colorless and transparent film (substrate); (3) coating a colorless and transparent film (substrate) with paint or ink and covering it completely; (4) printing solid ink on a colorless and transparent film (substrate).
[0036] The PF adhesive layer 22 can be composed of any suitable material. Specific examples include acrylic adhesives, rubber adhesives, silicone adhesives, polyester adhesives, urethane adhesives, epoxy adhesives, and polyether adhesives. By adjusting the type, quantity, combination, and proportion of monomers in the base resin forming the adhesive, as well as the amount of crosslinking agent, reaction temperature, and reaction time, an adhesive with desired properties corresponding to the purpose can be prepared. The base resin of the adhesive can be used alone or in combination of two or more. The base resin is preferably an acrylic resin (i.e., the PF adhesive layer is preferably composed of an acrylic adhesive). Regarding the adhesive constituting the PF adhesive layer, it is preferable that the base resin contains a polymer having a functional group containing active hydrogen (e.g., hydroxyl groups). If such a base resin is used, a PF adhesive layer with a desired storage modulus can be obtained. Details of the adhesive constituting the PF adhesive layer are described, for example, in Japanese Patent Application Publication No. 2018-123281, the description of which is incorporated herein by reference.
[0037] The thickness of the PF adhesive layer 22 can be, for example, 5 μm to 50 μm, or, for example, 10 μm to 40 μm, or, for example, 10 μm to 30 μm.
[0038] The storage modulus G' of the PF adhesive layer 22 at 25°C can be, for example, 0.5 × 10⁻⁶. 6 (Pa) ~3.0×10 6(Pa). If the storage modulus is within this range, an adhesive layer with an excellent balance between adhesion and peelability can be obtained (resulting in a surface protective film). It should be noted that the storage modulus can be determined, for example, by dynamic viscoelasticity measurement.
[0039] The thickness of the surface protective film 20 is, for example, less than 100 μm, and further, for example, 30 μm to 90 μm, 40 μm to 80 μm, or 45 μm to 70 μm. If the thickness of the surface protective film is within such a range, poor peeling during the removal of the surface protective film can be prevented very well. The thickness of the surface protective film can also be, for example, 70 μm to 100 μm. If the thickness of the surface protective film is within such a range, poor peeling can be appropriately suppressed, and dents can be well suppressed. It should be noted that the thickness of the surface protective film refers to the combined thickness of the substrate and the PF adhesive layer.
[0040] A-4. Adhesive layer The adhesive layer 30 can be of any suitable composition. Specific examples of adhesives constituting the adhesive layer include acrylic adhesives, rubber adhesives, silicone adhesives, polyester adhesives, urethane adhesives, epoxy adhesives, and polyether adhesives. By adjusting the type, quantity, combination, and proportion of monomers in the base resin forming the adhesive, as well as the amount of crosslinking agent, reaction temperature, and reaction time, an adhesive with desired properties corresponding to the purpose can be prepared. The base resin of the adhesive can be used alone or in combination of two or more. From the viewpoints of transparency, processability, and durability, acrylic adhesives are preferred. Details of the adhesive constituting the adhesive layer are described, for example, in Japanese Patent Application Publication No. 2014-115468, the description of which is incorporated herein by reference. The thickness of the adhesive layer 30 can be, for example, 10 μm to 100 μm. The storage modulus G' of the adhesive layer 30 at 25°C can be, for example, 1.0 × 10⁻⁶. 4 (Pa) ~1.0×10 6 (Pa).
[0041] A-5. Peeling off the liner As the release liner 40, any suitable release liner can be used. Specific examples include plastic films, non-woven fabrics, or paper with a surface coating using a release agent. Specific examples of release agents include: silicone-based release agents, fluorinated release agents, and long-chain alkyl acrylate-based release agents. Specific examples of plastic films include: polyethylene terephthalate (PET) films, polyethylene films, and polypropylene films. The thickness of the release liner can be, for example, from 10 μm to 100 μm.
[0042] When the release liner is a colored film, the release liner can be colored in any suitable manner. Specific examples of coloring methods are described in section A-3 above regarding the coloring of the surface protective film (substrate).
[0043] B. Manufacturing methods for optical film products As briefly explained in item A-1 above, and as... Figure 2 As shown, optical film product 110 can be obtained by miniaturizing the optical laminate 100. Therefore, a method for manufacturing such an optical film product can also be included in embodiments of the present invention. Miniaturization can be performed by cutting the optical laminate. Cutting can be performed in any suitable manner. Specifically, cutting can be performed using a cutting blade such as a cutter, a punching die, or laser irradiation. Laser irradiation is preferred. Laser irradiation has the advantages of enabling high-precision / high-quality processing of fine and complex shapes, and superior end quality compared to processing using cutting tools. Hereinafter, cutting using laser irradiation will be described. Cutting using a punching die is obvious or readily understood by those skilled in the art, and therefore a detailed description is omitted.
[0044] Cutting using laser irradiation can be typically achieved by irradiating a position within the optical laminate that corresponds to the shape of the optical film product while simultaneously moving the laser irradiation position at a predetermined speed. In the example shown, this can be done by... Figure 2 The cutting line was irradiated with laser at 60°.
[0045] As a laser source, a representative example is an infrared laser, such as a CO2 laser source with a wavelength of 9μm to 11μm in the infrared region, which contains oscillating laser light. Such a laser source can achieve high productivity. Infrared lasers can easily achieve power levels in the tens of W, thereby enabling optical laminates to be efficiently heated by molecular vibrations accompanying infrared absorption, which in turn induces etching accompanied by phase transitions in the material.
[0046] As a laser source, a CO laser source with an oscillating laser wavelength of approximately 5 μm can also be used. Furthermore, near-infrared (NIR), visible (Vis), and ultraviolet (UV) pulsed laser sources can be used as laser sources. Examples of NIR, Vis, and UV pulsed laser sources include laser sources with oscillating laser wavelengths of 1064 nm, 532 nm, 355 nm, 349 nm, or 266 nm (high harmonics of solid-state laser sources using Nd:YAG, Nd:YLF, or YVO4 as the medium), excimer laser sources with oscillating laser wavelengths of 351 nm, 248 nm, 222 nm, 193 nm, or 157 nm, and F2 laser sources with an oscillating laser wavelength of 157 nm.
[0047] From the perspective of suppressing thermal damage to optical laminates, pulsed oscillation is a more preferable oscillation mode than continuous wave (CW) oscillation as a laser source. The pulse width can be 10 femtoseconds (10^6 femtoseconds). -14 (seconds) ~ 1 millisecond (10) -3 The pulse repetition frequency is set appropriately within the range of seconds. The preferred pulse repetition frequency is 1kHz to 1000kHz, more preferably 10kHz to 500kHz. Processing can also be performed by setting two or more pulse widths.
[0048] There are no restrictions on the polarization state of the laser. Specifically, any polarization of light, including linearly polarized, circularly polarized, and randomly polarized light, can be used. There are also no restrictions on the spatial intensity distribution of the laser. A Gaussian beam is preferred because it exhibits good focusing properties, can be miniaturized, and promises increased productivity. The laser can be shaped into a flat-top beam using diffractive optical elements, aspherical lenses, etc., depending on the purpose.
[0049] The number of laser irradiations can be appropriately set according to the purpose. If the desired shape can be cut, the laser can be applied only once along the shape of the target optical film product, or the desired cutting depth can be achieved through multiple irradiations. In the case of multiple laser irradiations, the conditions for each irradiation can be the same or different.
[0050] The laser scanning method can be appropriately set according to the purpose. Specific examples include: stage drive systems such as XY precision stages, optical scanning systems such as galvano scanners and polygon scanners, or combinations thereof (multi-axis synchronous control). By appropriately selecting and / or combining these, the relative position of the workpiece (optical laminate) and the laser can be changed at a specified speed. Furthermore, by using mechanical shutters, AOM (acoustic optics), etc., to control the laser irradiation on / off, the desired shape can be processed. The laser scanning speed can be appropriately set according to the purpose (e.g., the desired cutting depth).
[0051] The diameter of the laser beam's focal spot (which results in the cutting width) can be appropriately set according to the purpose. The focal spot diameter can be adjusted to the desired diameter or range, for example, by using an objective lens such as an Fθ lens to focus the laser beam. Such a configuration improves processing efficiency and suppresses thermal damage. The focal spot diameter is preferably 500 μm or less, more preferably 300 μm or less, further preferably 200 μm or less, and particularly preferably 100 μm or less. The focal spot diameter can be defined, for example, as the laser beam attenuates to 1 / e compared to the peak intensity value. 2 The diameter of the laser at the location of the desired intensity. It should be noted that, when using a galvanometer scanner, a telecentric Fθ lens is preferred for the purpose of perpendicularly irradiating the workpiece (optical laminate). Furthermore, to obtain the desired focal point diameter (which results in the cut-off width), a beam spreader unit for adjusting the beam diameter can be used in the optical path from the laser oscillator exit end to the objective lens.
[0052] The laser output can be appropriately set according to the thickness and properties of the optical laminate to be processed. For example, when using a CO2 laser as the laser source, the output is preferably 5W to 300W, and more preferably 20W to 200W.
[0053] As mentioned above, optical film products can be manufactured.
[0054] C. Optical film products Optical film product 110 can be as described in items A and B above, and as... Figure 2 As shown, the optical laminate 100 is obtained by miniaturizing the optical laminate. Therefore, the basic structure of the optical film product can correspond to the basic structure of the optical laminate, except for the size difference. Specifically, the optical film product 110 has: an optical film 10; a surface protective film 20 temporarily adhered to one side of the optical film 10 in a peelable manner; an adhesive layer 30 disposed on the other side of the optical film 10; and a release liner 40 temporarily adhered to the adhesive layer 30 in a peelable manner. Furthermore, at least one of the surface protective film 20 or the release liner 40 is colored, and a marking line 50 is formed on one of the surface protective film 20 or the release liner 40. Typically, each optical film product 110 includes one marking line 50. Furthermore, the extending direction of the marking line is typically parallel to the optical axis of the optical film. For a detailed description of the optical film product 110, please refer to the description in paragraph A above.
[0055] Optical film product 110 is typically used in wearable image display devices (wearable displays: e.g., VR goggles, AR glasses, HMDs). Therefore, the optical film product can be of a very small size. The size of the optical film product is typically less than 10 mm in length and less than 10 mm in width, preferably less than 8 mm in length and less than 8 mm in width, more preferably less than 7 mm in length and less than 7 mm in width, further preferably less than 6 mm in length and less than 6 mm in width, and particularly preferably less than 5 mm in length and less than 5 mm in width. According to an embodiment of the invention, the back of such a very small optical film product can be accurately determined visually (i.e., without the use of special equipment). The inventors have produced a very small optical film product suitable for wearable displays and found that the back of such a very small optical film product is particularly difficult to determine compared to optical film products of sizes used to date (e.g., sizes larger than smartphones), and cannot be determined using conventional determination techniques. Furthermore, the inventors conducted repeated experiments on the identification of the back surface of such extremely small optical film products. They discovered that by coloring at least one of the surface protective film or the release liner and forming a marking line on one of the surface protective film or the release liner, accurate visual identification is possible, thus completing the present invention. In other words, the embodiments of the present invention solve a newly recognized technical problem concerning extremely small optical film products applicable to wearable displays, resulting in unexpectedly excellent effects.
[0056] The optical film product can have a shape corresponding to the shape of the optical component it is attached to. The optical film product can be typically rectangular, but is preferably square. If the optical film product is square, it can be suitable for attachment to a polarizing beam splitter, typically a cube. As a result, the optical film product is preferably suitable for wearable displays. Furthermore, if the optical film product is square, it is difficult to determine the direction of the optical axis of the optical film, thus the effect of the marking lines can become even more significant.
[0057] Industrial availability The optical laminates of embodiments of the present invention can preferably be used as raw material rolls for optical film products of very small dimensions. The optical film products of embodiments of the present invention can preferably be used in image display devices, and particularly preferably in wearable image display devices (wearable displays). Representative examples of wearable displays include VR goggles, AR glasses, and head-mounted displays (HMDs).
Claims
1. An optical laminate comprising: an optical film; a surface protective film temporarily adhered to one side of the optical film in a peelable manner; an adhesive layer disposed on the other side of the optical film; and a release liner temporarily adhered to the adhesive layer in a peelable manner. One of the surface protective film or the release liner is colored. A marking line is formed on either the surface protective film or the release liner. When the optical laminate is miniaturized to form an optical film product, the marking line is formed to be included in all optical film products.
2. The optical laminate according to claim 1, wherein, The marking line is formed as a stripe extending in a direction parallel to the optical axis of the optical film, and one marking line is included in each of the optical film products.
3. The optical laminate according to claim 1, wherein, One of the surface protective film or the release liner is black and opaque.
4. The optical laminate according to claim 3, wherein, The surface protective film is black and opaque, and the marking line is formed on the release liner and is red.
5. The optical laminate according to claim 3, wherein, The surface protective film is black and opaque, and the marking line is formed on the surface protective film. The marking line is a light color that can be distinguished from black.
6. A method of making an optical film product comprising: The optical laminate as described in any one of claims 1 to 5 is miniaturized.
7. The method for manufacturing the optical film product according to claim 6, wherein, The miniaturization includes cutting the optical laminate by laser irradiation.
8. An optical film product comprising: an optical film; a surface protective film temporarily adhered to one side of the optical film in a peelable manner; an adhesive layer disposed on the other side of the optical film; and a release liner temporarily adhered to the adhesive layer in a peelable manner. The optical film product is rectangular in shape with a vertical dimension of less than 10mm and a horizontal dimension of less than 10mm. One of the surface protective film or the release liner is colored. Identification lines are formed on either the surface protective film or the release liner.
9. The optical film product according to claim 8, wherein, The marking line extends in a direction parallel to the optical axis of the optical film.
Citation Information
Patent Citations
Optical member and device for judging set direction of the same
JP2003114328A
Method for manufacturing optical film product
JP2007187781A
Optical film having adhesive agent on both sides, and manufacturing method of image display unit using the same
JP2014115468A
Adhesive composition, adhesive layer, surface protection film and optical member
JP2018123281A