A small-diameter single-mode optical fiber and a method for manufacturing the same

By optimizing the relationship between the thickness and modulus of the inner and outer coatings, and combining doping elements and segmented curing processes, the high loss and mechanical reliability problems of thin-diameter optical fibers in bending scenarios were solved, achieving a synergistic improvement in low loss and high bending resistance.

CN123156364APending Publication Date: 2026-11-24FIBERHOME FUJIKURA OPTIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611337529.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-31
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing thin-diameter optical fibers suffer from a sharp increase in macro-bending loss under bending conditions, and it is difficult to maintain mechanical reliability. Traditional processes are unable to maintain low loss and high bending resistance during the process of reducing the diameter.

Method used

By designing the specific thickness and elastic modulus relationship between the inner and outer coatings, setting the modulus decoupling coefficient G≥1000 and the stiffness coefficient K within the range of 1200≤K≤5000, and optimizing the waveguide structure by combining doping elements, a segmented curing process is adopted to ensure the mechanical matching performance of the coating.

Benefits of technology

It achieves reduced microbending loss and improved mechanical reliability in curved scenarios, meets the cabling requirements of fine-diameter optical fibers in confined spaces, and enhances the transmission performance and service life of optical fibers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123156364A_ABST
    Figure CN123156364A_ABST
Patent Text Reader

Abstract

This application relates to a narrow-diameter single-mode optical fiber and its fabrication method, comprising: an optical fiber body and a coating layer, the coating layer including an inner coating layer disposed on the outer surface of the optical fiber body and an outer coating layer covering the inner coating layer; the thickness of the inner coating layer is t1, and the elastic modulus is E1; the thickness of the outer coating layer is t2, and the elastic modulus is E2, and they satisfy the following relationship: the stiffness coefficient of the coating layer K=(t2 / t1)×(E2 / E1), where 1200≤K≤5000; the modulus decoupling coefficient of the coating layer G=E2 / E1, where G≥1000. By setting the modulus decoupling coefficient G≥1000, this invention makes the elastic modulus of the outer coating layer much higher than that of the inner coating layer. This differentiated modulus design allows the inner coating layer to maintain a lower modulus state, thereby effectively absorbing the small deformations experienced by the optical fiber, reducing stress transmission to the glass fiber, and helping to reduce micro-bending loss. By limiting the stiffness coefficient K to the range of 1200 to 5000, it is ensured that the outer coating provides sufficient mechanical support while avoiding excessive compression of the inner coating due to excessive stiffness.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of optical fiber manufacturing technology, and in particular to a narrow-diameter single-mode optical fiber and its preparation method. Background Technology

[0002] In scenarios with extremely limited space requirements, such as indoor cabling, data center interconnection, and 5G fronthaul, traditional conventional outer diameter (250μm) optical fibers face significant construction difficulties due to their large size and limited flexibility, particularly when laying them in conduits, concealed wiring, and turning in confined spaces. To adapt to these complex application scenarios, smaller diameter, high-bending-resistance single-mode optical fibers have become an inevitable trend in the industry.

[0003] However, reducing the outer diameter of optical fibers to below 170 μm (the so-called "narrow-diameter fiber") and maintaining low loss at extremely small bending radii presents a double challenge to optical fiber manufacturing processes. First, at the waveguide structure design level, simply reducing the cladding diameter can lower the outer diameter, but it easily leads to severe mode field leakage when the fiber is bent, causing a sharp increase in macro-bending loss. In existing technologies, some manufacturers have attempted to improve bending resistance by introducing a recessed cladding structure, but due to the lack of precise control over the physical volume of the recessed cladding and its ratio to the core diameter, the fiber often loses its splicing compatibility with existing G.652D fibers while maintaining bending resistance, or suffers from static fatigue risks due to uneven stress distribution.

[0004] Secondly, at the coating and curing process level, the outer coating thickness of small-diameter optical fibers is significantly reduced, which places higher demands on the mechanical protection capabilities of the coating. Traditional inner and outer coatings often use homogeneous materials with the same modulus, making it difficult to simultaneously meet the conflicting requirements of "micro-bending buffer" and "high strength". In addition, conventional curing processes are energy-intensive and the cross-linking reaction is incomplete, affecting the long-term aging resistance of the coating and the overall lifespan of the optical fiber. Summary of the Invention

[0005] This application provides a narrow-diameter single-mode optical fiber and its fabrication method, which can solve the problem in the related technology that the macro-bending loss of existing narrow-diameter optical fibers increases sharply in bending scenarios and it is difficult to maintain mechanical reliability.

[0006] In a first aspect, embodiments of this application provide a narrow-diameter single-mode optical fiber, comprising: an optical fiber body and a coating layer, wherein the coating layer includes an inner coating layer disposed on the outer surface of the optical fiber body and an outer coating layer covering the inner coating layer; the thickness of the inner coating layer is t1, and the elastic modulus is E1; the thickness of the outer coating layer is t2, and the elastic modulus is E2, and they satisfy the following relationship: The stiffness coefficient of the coating layer is K = (t2 / t1) × (E2 / E1), where 1200 ≤ K ≤ 5000; The modulus decoupling coefficient of the coating layer is G=E2 / E1, where G≥1000.

[0007] In conjunction with the first aspect, in one embodiment, the outer diameter of the thin-diameter single-mode optical fiber is 150μm~170μm; The thickness of the coating layer is ≤22.5μm.

[0008] In conjunction with the first aspect, in one embodiment, the material of the inner coating comprises acrylate and flexible monomer, the elastic modulus E1 of the inner coating is 0.3 MPa to 1.0 MPa, and the elongation at break is ≥100%; The outer coating material includes acrylate and silica nanoparticles, and the elastic modulus E2 of the outer coating is 800MPa to 1500MPa, and the elongation at break is ≥15%.

[0009] In conjunction with the first aspect, in one embodiment, the material of the flexible monomer includes at least one of isooctyl acrylate or laurate. The particle size of the silica nanoparticles is 3 nm to 8 nm; The amount of silica nanoparticles added to the outer coating material is 5% to 15% of the total mass of the outer coating material.

[0010] In conjunction with the first aspect, in one embodiment, the optical fiber body includes a fiber core, a recessed cladding, and a cladding structure arranged sequentially from the inside out; The doping elements of the fiber core include germanium and alkali elements, and the doping elements of the sunken cladding include fluorine.

[0011] In conjunction with the first aspect, in one embodiment, the refractive index difference Δn of the sunken cladding relative to pure silicon dioxide is ≤-0.4%; The ratio of the outer diameter of the sunken cladding to the diameter of the fiber core is 2.5 to 4.

[0012] In conjunction with the first aspect, in one embodiment, the narrow-diameter single-mode fiber has a mode field diameter of 8.2 μm to 9.6 μm at a wavelength of 1310 nm; The bending loss of the thin-diameter single-mode fiber when wound with a radius of 7.5 mm for one turn at a wavelength of 1550 nm is ≤0.5dB / km. The narrow-diameter single-mode optical fiber has a screening tension ≥200kpsi and a dynamic fatigue parameter nd ≥20.

[0013] Secondly, embodiments of this application provide a method for fabricating the thin-diameter single-mode optical fiber as described above, comprising: The optical fiber preform is drawn into an optical fiber body; The outer surface of the optical fiber body is sequentially coated with an inner coating and an outer coating. The thickness of the inner coating is controlled to be t1, the thickness of the outer coating is controlled to be t2, the elastic modulus of the inner coating is E1, and the elastic modulus of the outer coating is E2, so that the formed coating layer satisfies: stiffness coefficient K=(t2 / t1)×(E2 / E1), 1200≤K≤5000, modulus decoupling coefficient G=E2 / E1, G≥1000; The coated optical fiber body is then cured by irradiation.

[0014] In conjunction with the second aspect, in one embodiment, the irradiation curing is ultraviolet lamp irradiation curing, and the curing includes a pre-curing process and a main curing process; In the pre-curing process, the ultraviolet light intensity is 10mW / cm²~20mW / cm², the oxygen concentration is <1000ppm, and the power is 200~400W. In the main curing process, the ultraviolet light intensity is 150mW / cm²~210mW / cm², and the power is 1200~1800W; The distance between the pre-curing oven used in the pre-curing process and the main curing oven used in the main curing process is 0.7m to 1.0m.

[0015] In conjunction with the second aspect, in one embodiment, the material of the outer coating includes acrylate and silica nanoparticles; Before applying the outer coating, the method further includes: Surface modification of silica nanoparticles was performed using silane coupling agents; Surface-modified silica nanoparticles were added to acrylate prepolymer and ultrasonically dispersed to obtain a nano suspension. The outer coating is made from the nano-suspension.

[0016] The beneficial effects of the technical solutions provided in this application include: This application provides a narrow-diameter single-mode optical fiber and its fabrication method. By defining a specific relationship between the thickness and elastic modulus of the inner and outer coatings, the mechanical matching performance of the coating system is optimized. Specifically, by setting the modulus decoupling coefficient G≥1000, the elastic modulus of the outer coating is made much higher than that of the inner coating. This differentiated modulus design allows the inner coating to maintain a lower modulus state, thereby effectively absorbing the small deformations of the optical fiber, reducing stress transmission to the glass fiber, and helping to reduce microbending loss. At the same time, combined with the limitation of the stiffness coefficient K in the range of 1200 to 5000, the thickness ratio and modulus ratio of the inner and outer coatings are coordinated. This ensures that the outer coating provides sufficient mechanical support while avoiding excessive compression of the inner coating due to excessive stiffness. This synergistic configuration of coating mechanical parameters allows the optical fiber to achieve a better balance between buffer protection and mechanical strength when subjected to lateral pressure or bending, thereby improving the transmission performance and mechanical reliability of the optical fiber in bending scenarios. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0018] Figure 1 This is a schematic diagram of a narrow-diameter single-mode optical fiber provided in an embodiment of this application; Figure 2 This is a schematic diagram of wire drawing provided for an embodiment of this application; Figure 3 This is a schematic diagram of a method for fabricating a narrow-diameter single-mode optical fiber provided in an embodiment of this application.

[0019] In the figure: 1. Fiber core; 2. Recessed cladding; 3. Cladding structure; 4. Inner coating; 5. Outer coating. Detailed Implementation

[0020] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0021] This application provides a narrow-diameter single-mode optical fiber and its fabrication method, which can solve the problem in related technologies that the macro-bending loss of existing narrow-diameter optical fibers increases sharply in bending scenarios and it is difficult to maintain mechanical reliability.

[0022] In a first aspect, embodiments of this application provide a narrow-diameter single-mode optical fiber, comprising: an optical fiber body and a coating layer, the coating layer comprising an inner coating 4 disposed on the outer surface of the optical fiber body and an outer coating 5 covering the inner coating 4; the thickness of the inner coating 4 is t1 and the elastic modulus is E1, the thickness of the outer coating 5 is t2 and the elastic modulus is E2, and satisfying the following relationship: the stiffness coefficient of the coating layer K=(t2 / t1)×(E2 / E1), where 1200≤K≤5000; the modulus decoupling coefficient of the coating layer G=E2 / E1, where G≥1000.

[0023] This application optimizes the mechanical matching performance of the coating system by defining a specific relationship between the thickness and elastic modulus of the inner coating 4 and the outer coating 5. Specifically, by setting the modulus decoupling coefficient G≥1000, the elastic modulus of the outer coating 5 is made much higher than that of the inner coating 4. This differentiated modulus design allows the inner coating 4 to maintain a lower modulus state, thereby effectively absorbing the small deformations of the optical fiber, reducing stress transmission to the glass fiber, and helping to reduce microbending loss. At the same time, combined with the limitation of the stiffness coefficient K in the range of 1200 to 5000, the thickness ratio and modulus ratio of the inner and outer coatings 5 ​​are coordinated, ensuring that the outer coating 5 provides sufficient mechanical support while avoiding excessive compression of the inner coating 4 due to excessive stiffness. This synergistic configuration of coating mechanical parameters allows the optical fiber to achieve a better balance between buffer protection and mechanical strength when subjected to lateral pressure or bending, thereby improving the transmission performance and mechanical reliability of the optical fiber in bending scenarios.

[0024] By setting a specific range for the stiffness coefficient K and the modulus decoupling coefficient G, the coating layer is decoupled in terms of mechanical properties. The inner coating 4 mainly serves to buffer micro-bending stress, while the outer coating 5 mainly serves to resist external mechanical extrusion, thus avoiding the decrease in fiber strength or the increase in transmission loss due to stress concentration, and ensuring that the fiber still has excellent mechanical reliability under the condition of narrow diameter.

[0025] This application sets 1200≤K≤5000, see Table 1: When K<1200, the outer coating 5 has insufficient stiffness and cannot offset the lateral pressure on the inner coating 4, resulting in a significant increase in micro-bending loss; when K>5000, the outer coating 5 is too rigid and loses its deformation buffering capacity, which in turn exacerbates micro-bending; when G<1000, the modulus difference between the inner and outer coatings 5 ​​is insufficient, the inner coating 4 cannot effectively absorb micro-bending deformation, and the outer coating 5 has insufficient protective strength.

[0026]

[0027] Furthermore, the fiber body of the waveguide structure includes a core 1, a recessed cladding 2, and a cladding structure 3 arranged sequentially from the inside out. The outer diameter of the thin-diameter single-mode fiber is 150μm~170μm; the diameter of the cladding structure 3 is 125μm. In specific implementations, the core 1 is doped with germanium and alkali elements, and the recessed cladding 2 is doped with fluorine. The core 1 is doped with germanium and alkali elements to enhance light confinement capability, and the recessed cladding 2 is doped with fluorine to form a trench-assisted structure. The refractive index difference Δn of the recessed cladding 2 relative to pure silicon dioxide is ≤-0.4%, and the ratio of the outer diameter of the recessed cladding 2 to the diameter of the core 1 is 2.5~4. This waveguide design reduces the outer diameter of the fiber while ensuring low bending loss and splicing compatibility with standard fibers, meeting the transmission performance requirements of optical communication networks for thin-diameter fibers.

[0028] This application preferably uses potassium as the alkali metal dopant element. Its ionic radius has a high matching degree with the silicon-oxygen network, which can effectively improve the doping efficiency of germanium and reduce the stress of the fiber core 1. In the high-temperature molten state, potassium can reduce the viscosity of the glass melt, promote the uniform diffusion of the dopant, and reduce refractive index fringes caused by composition fluctuations. This results in a smoother refractive index distribution inside the fiber core 1, further suppressing scattering loss during signal transmission and improving mechanical strength, ensuring the optical performance stability of the optical fiber during long-term use.

[0029] In fiber core 1, the molar percentage of GeO2 doping is 3%~5%, and the molar percentage of K2O doping is 0.5%~1.0%. This ratio range ensures that fiber core 1 has sufficient refractive index increment to meet single-mode transmission requirements, while avoiding viscosity decrease and diffusion effects caused by excessive germanium content, thus guaranteeing the geometric accuracy of the waveguide structure. The appropriate addition of potassium compensates for the stress concentration caused by high germanium doping, minimizing the difference in thermal expansion coefficients between fiber core 1 and cladding structure 3, preventing microcracks at the interface due to thermal mismatch, and improving the fiber's resistance to static fatigue.

[0030] The fluorine doping concentration in the recessed cladding 2 is 0.3~0.5wt%. This concentration range can stably achieve a relative refractive index difference of ≤-0.4% for the recessed cladding 2, while avoiding the loosening problem of the cladding structure 3 caused by excessive fluorine doping. At this concentration, fluorine can effectively reduce the cladding refractive index to form a trench structure without significantly weakening the mechanical strength of the silica glass network. This ensures that the optical fiber body maintains structural integrity during subsequent coating and cabling processes, meeting the technical requirements of bending insensitivity and long-term reliability for small-diameter single-mode optical fibers, and preventing fiber breakage due to cladding defects during cabling.

[0031] For the coating layer, the thickness of the coating layer is ≤22.5μm. This thickness parameter refers to the thickness of the coating layer on one side of the fiber radially, which is determined based on the overall design requirement of compressing the outer diameter of the fiber to 150μm~170μm. A thinner coating layer helps to reduce the overall volume of the fiber and increase the cable's density, while ensuring sufficient mechanical protection. Therefore, under the premise of meeting the requirements for smaller diameter, the total thickness of the coating layer is controlled within a specific range to balance space occupation and protective performance, ensuring the applicability of the fiber in narrow spaces and avoiding the impact on the laying efficiency in existing duct resources due to excessively thick coating leading to an excessively large outer diameter of the fiber.

[0032] In the coating layer, the inner coating 4 is made of acrylate and flexible monomer. The elastic modulus E1 of the inner coating 4 at 23℃ (standard conditions) is 0.3MPa~1.0MPa, and the elongation at break is ≥100%. The acrylate here is a low-modulus UV-cured acrylate. The flexible monomer is made of at least one of isooctyl acrylate or laurate. The low modulus characteristic allows the inner coating 4 to undergo large elastic deformation when the optical fiber is subjected to lateral pressure or bending, thereby effectively absorbing and buffering external stress and preventing stress from being directly transmitted to the surface of the glass fiber and causing microbending loss. The high elongation at break ensures the integrity of the coating under tension and avoids coating cracking that leads to protection failure. The introduction of flexible monomer further enhances the mobility of polymer chain segments, optimizes the flexibility of the inner coating 4, and ensures that it still maintains a good buffering effect in low-temperature environments, reducing additional losses caused by temperature changes.

[0033] The outer coating 5 consists of acrylate and silica nanoparticles. The outer coating 5 has an elastic modulus E2 of 800 MPa to 1500 MPa and an elongation at break ≥15% at 23°C (standard conditions). The acrylate used here is a high-modulus UV-curable acrylate. Silica nanoparticles with a particle size of 3 nm to 8 nm are dispersed in the outer coating 5. The amount of silica nanoparticles added to the outer coating 5 is 5% to 15% of the total mass of the outer coating 5, and the particle size is less than one-tenth of the optical fiber transmission wavelength to avoid Rayleigh scattering. After surface modification with a silane coupling agent, the nanoparticles are uniformly dispersed in the acrylate matrix, forming an enhanced composite structure. This improves the rigidity and aging resistance of the outer coating 5. Combined with its high modulus properties, it prevents excessive deformation of the optical fiber during cabling or use, ensuring the long-term reliability and environmental adaptability of the optical fiber. At the same time, controlling the particle size to be less than one-tenth of the transmission wavelength effectively avoids light scattering loss caused by excessively large particle size, ensuring that the optical transmission performance is not affected by the coating material, meeting the requirements of high bandwidth transmission. Furthermore, the nanoparticles have strong adhesion to the matrix, preventing aggregation or precipitation during use and maintaining the long-term stability of the coating performance.

[0034] Based on the above embodiments, in this embodiment, the mode field diameter of the thin-diameter single-mode fiber at a wavelength of 1310nm is 8.2μm~9.6μm; the bending loss of the thin-diameter single-mode fiber at a wavelength of 1550nm when wound with a radius of 7.5mm is ≤0.5dB / km; the doped structure design of the fiber core 1 and the recessed cladding 2 enhances the optical field confinement ability and suppresses signal leakage under bending conditions, so that the fiber can maintain low-loss transmission in a small bending radius environment, which is suitable for laying in narrow spaces such as indoor wiring, ensuring signal transmission stability, verifying the effect of waveguide structure optimization on bending performance improvement, and meeting the technical specifications of bending-insensitive fiber.

[0035] The screening tension of the narrow-diameter single-mode optical fiber is ≥200 kpsi, and the dynamic fatigue parameter nd is ≥20. The screening tension is used to eliminate weak points with microcracks on the surface to ensure minimum mechanical strength. The dynamic fatigue parameter nd characterizes the ability to resist stress corrosion crack propagation. A higher nd value means better anti-aging performance. Combined with the coating protection structure to prevent moisture erosion and stress-induced strength degradation, this ensures the long-term safe operation and durability of the optical fiber in complex environments, meets the reliability standards of the communications industry, and guarantees the service life of network infrastructure.

[0036] In summary, this application modifies the core layer by doping with germanium and alkali metals to enhance the optical confinement capability of the fiber core 1. Simultaneously, a soft buffer layer is introduced, specifically by doping the recessed cladding 2 with fluorine, utilizing the low refractive index of fluorine to form a trench-assisted structure. The addition of alkali metals adjusts the viscosity of the glass network, promotes the uniform distribution of germanium, and reduces scattering loss caused by refractive index fluctuations. Fluorine doping effectively reduces the cladding refractive index without significantly reducing mechanical strength, forming a refractive index trench. This structure helps reflect leaked mode fields back to the fiber core 1 region when the fiber is bent, thus establishing a foundation for bend insensitivity at the microstructural level and ensuring the optical performance stability of the waveguide structure during the reduction of its diameter.

[0037] The refractive index difference of the depressed cladding 2 is strictly controlled to be ≤-0.4%, and the ratio of the outer diameter of the depressed cladding 2 to the outer diameter of the inner cladding is controlled within 2.5~4. This specific volume optimization design can effectively re-confine the leaked evanescent field back to the fiber core 1, significantly improving the fiber's bend insensitivity. The limitation of the refractive index difference avoids excessively deep trenches leading to increased fusion loss or excessively shallow trenches leading to insufficient bending resistance. The range of the outer diameter ratio balances the relationship between the mode field diameter and the cladding size, ensuring that while meeting the bending performance of the G.657 standard, mode field matching with conventional single-mode fiber is maintained, reducing signal reflection and loss at link connection points, and achieving synergistic optimization of optical performance and geometric dimensions.

[0038] The coating parameters are constrained by constructing a stiffness balance formula and a mechanical decoupling formula, replacing the single proportional constraint: Stiffness coefficient K: defined as K = (t2 / t1) * (E2 / E1), where t2 and t1 are the thicknesses of the outer coating 5 and the inner coating 4, respectively, and E2 and E1 are the corresponding moduli, constrained to 1200 ≤ K ≤ 5000. This formula ensures the rationality of stress distribution in the coating system under lateral pressure, preventing excessive compression of the inner coating 4 that could lead to micro-bending loss. The stiffness coefficient K comprehensively considers the dual effects of thickness ratio and modulus ratio. If the K value is too low, the outer coating 5 will lack sufficient support; if the K value is too high, the coating system as a whole will be rigid and brittle. Limiting it within this range allows the inner coating 4 to play a buffering role while the outer coating 5 provides necessary protection, preventing stress concentration from being transferred to the glass surface and causing static fatigue or fracture.

[0039] Modulus decoupling G: Defined as G = E2 / E1, and limited to G ≥ 1000. This design ensures that the inner coating 4 is in an extremely low modulus state to absorb minute deformations, while the outer coating 5 provides high modulus support. The high modulus decoupling coefficient means that the hardness difference between the inner and outer coatings 5 ​​is significant. The inner coating 4 acts as a soft layer to isolate the glass from external hard forces, while the outer coating 5 acts as a hard layer to resist cable extrusion. This mechanically layered design solves the problem of reduced protective force caused by thin coatings in small-diameter optical fibers, ensuring that even with a reduced total coating thickness, effective stress isolation and mechanical protection can still be achieved through differences in material properties, maintaining the long-term reliability of the optical fiber.

[0040] While maintaining excellent optical and mechanical properties, the outer diameter of the optical fiber is compressed to ≤170μm (coating thickness on one side ≤22.5μm), greatly improving the adaptability of optical fiber cabling in confined spaces. The slim design directly reduces the cross-sectional area of ​​the optical cable, allowing more fiber cores to be accommodated in the same conduit volume, or enabling capacity expansion and upgrades without changing the existing conduit infrastructure. The controlled coating thickness on one side ensures the overall flexibility of the optical fiber, facilitating small-radius bending installations in confined spaces such as indoor cabling and high-density patch panels in data centers, meeting the practical needs of modern communication networks for high space utilization and flexible deployment.

[0041] Secondly, embodiments of this application provide a method for fabricating a narrow-diameter single-mode optical fiber as provided in any of the above embodiments of this application, comprising: The fiber preform is drawn into an optical fiber body: an optical fiber preform with a step-index profile is prepared, the profile including a germanium-doped core 1 and a fluorine-doped cladding 2; in a specific implementation, the core 1 is also doped with alkali metal elements to adjust viscosity and stress, and the cladding 2 is formed with refractive index grooves by fluorine doping. The structure of this preform determines the waveguide characteristics of the final optical fiber body. The preform is softened by high temperature heating and stretched to the target diameter under tension to form an optical fiber body with a diameter of 125 μm including the cladding structure 3. This ensures that the waveguide geometry remains stable during the drawing process, provides a standard glass substrate for subsequent coating, and avoids structural deformation from affecting optical performance. The outer surface of the optical fiber body is sequentially coated with an inner coating 4 and an outer coating 5. The thickness of the inner coating 4 is controlled to be t1, the thickness of the outer coating 5 to be t2, the elastic modulus of the inner coating 4 to be E1, and the elastic modulus of the outer coating 5 to be E2. The resulting coatings satisfy the following conditions: stiffness coefficient K = (t2 / t1) × (E2 / E1), 1200 ≤ K ≤ 5000; modulus decoupling coefficient G = E2 / E1, G ≥ 1000. The preform is then heated and drawn into fibers, and the inner coating 4 and outer coating 5 are sequentially coated along the drawing path. The outer coating 5 is a coating material; the inner coating 4 is a low-modulus acrylate containing flexible monomers, and the outer coating 5 is a high-modulus acrylate containing silica nanoparticles. The thickness of the liquid layer is adjusted by the coating system, and the coating formula is adjusted by combining the modulus test feedback after curing to ensure that the mechanical parameters of the coating after curing fall within the specified range. This achieves mechanical decoupling and stiffness balance between the inner and outer coatings 5, avoids increased micro-bending loss or insufficient mechanical protection due to parameter deviation, and ensures the fine diameter requirement of coating thickness ≤22.5μm.

[0042] The coated optical fiber body is then cured by irradiation. Irradiation curing is performed using ultraviolet (UV) lamps, and the curing process includes a pre-curing step and a main curing step.

[0043] In the pre-curing process, the ultraviolet light intensity is 10mW / cm²~20mW / cm², and the oxygen concentration in the curing environment is <1000ppm to allow the coating to form a semi-gel state. The power is 200~400W, used to correct the concentricity of the coating using surface tension. The low light intensity and low oxygen environment inhibit excessively rapid surface curing, prolonging the residence time of the coating material in the liquid state. Surface tension automatically aligns the center position, reducing stress asymmetry caused by eccentricity and preventing concentricity deviation due to curing shrinkage.

[0044] In the main curing process, the ultraviolet light intensity is 150mW / cm²~210mW / cm², and the power is 1200~1800W, used to complete the deep cross-linking reaction of the coating. High light intensity ensures that ultraviolet light penetrates into the coating, initiating full polymerization of monomers and establishing the final mechanical strength and aging resistance. The distance between the pre-curing oven used in the pre-curing process and the main curing oven used in the main curing process is 0.7m to 1.0m. This distance provides the necessary cooling and stress release area, preventing thermal stress cracks inside the coating due to sudden temperature changes. It also ensures that the semi-gel structure formed during pre-curing maintains a stable morphology before entering the main curing oven, ensuring that the final curing quality and coating concentricity meet the requirements of small-diameter single-mode optical fibers.

[0045] In this application, the pre-curing stage forms a semi-gel state in a low-light-intensity, low-oxygen environment, which retains the fluidity of the coating and allows for automatic concentricity correction using surface tension, while also preventing coating displacement and resin flow during fiber drawing. The low-light-intensity irradiation combined with an oxygen concentration of <1000ppm inhibits the rapid curing reaction of the coating surface, allowing the coating material to maintain a low viscosity in the early stages of UV irradiation. At this time, the liquid coating tends to reach the minimum surface area morphology under the action of surface tension, thereby automatically centering the glass fiber body in the center of the coating, effectively compensating for the mechanical deviation of the coating mold. At the same time, the semi-gel state has appropriate yield stress, which can resist the coating flow caused by fiber drawing vibration, prevent uneven coating thickness or resin flow defects caused by coating displacement, and ensure the geometric uniformity and initial morphological stability of the coating layer of the small-diameter fiber.

[0046] High light intensity and high power during the main curing stage achieve deep cross-linking, ensuring coating strength. High-power UV lamps provide sufficient energy density, allowing UV rays to penetrate to the bottom of the coating, triggering full polymerization of internal monomers to form a dense three-dimensional network structure. This improves the coating's elastic modulus and aging resistance, avoiding the problems of stickiness or insufficient strength caused by surface curing without internal drying. It ensures that the outer coating 5 can withstand mechanical stress without plastic deformation during subsequent cabling processes, meeting the mechanical reliability requirements of small-diameter single-mode optical fibers. Simultaneously, the high degree of cross-linking reduces volume shrinkage of the coating during long-term use, maintaining the stability of the fiber's optical performance.

[0047] The traditional "one-time curing" process is replaced with a segmented curing process of "pre-curing + main curing". The pre-curing stage is carried out at a lower temperature to allow the adhesive to initially establish strength and prevent flow and displacement during stringing; the main curing stage is carried out at a higher temperature to complete the main cross-linking reaction and establish the final strength and dimensional stability. See Table 2: Comparison between conventional one-time curing and the segmented curing of this application:

[0048] Comparative data shows that, while maintaining a drawing speed of 2000 m / min, this application reduced the coating concentricity deviation from 2.6 μm to 0.7 μm and increased the curing crosslinking degree from 89% to 96%. This indicates that segmented curing effectively solved the contradiction between incomplete coating curing and concentricity control under high-speed drawing. The low concentricity deviation reduced the additional microbending loss caused by coating unevenness, and the high crosslinking degree ensured the dimensional stability of the coating during long-term use. This verifies the significant effect of pre-curing and main curing on improving the performance of small-diameter optical fibers, and achieves simultaneous optimization of production efficiency and product quality.

[0049] Furthermore, the outer coating 5 comprises acrylate and silica nanoparticles; the silica nanoparticles have a particle size of 3nm to 8nm and are added to the outer coating 5 at a rate of 5% to 15% of the total mass of the outer coating 5. The nanoparticles are dispersed in the acrylate matrix as a reinforcing phase, improving the rigidity and aging resistance of the coating through the nano-effect. Combined with the high modulus characteristics, they prevent excessive deformation of the optical fiber during cabling, while ensuring the curing crosslinking degree and environmental adaptability of the coating layer. This ensures that the outer coating 5 provides mechanical protection without causing light scattering loss due to excessively large particles, thus maintaining the stability of optical transmission performance.

[0050] Before applying the outer coating 5, the method further includes: First, the surface of silica nanoparticles was modified using a silane coupling agent; The surface-modified silica nanoparticles were then added to the acrylate prepolymer and ultrasonically dispersed to obtain a nano-suspension. The outer coating 5 was made from this nano-suspension.

[0051] Silica nanoparticles are surface-modified with a silane coupling agent, and then dispersed in an acrylate prepolymer for 30-60 minutes using an ultrasonic cell disruptor to form a stable nanoparticle suspension, preventing nanoparticle aggregation. Ultrasonic cavitation breaks down the van der Waals forces between particles, ensuring uniform distribution of nanoparticles within the prepolymer. This prevents agglomerates from forming micro-defects or stress concentration sources after curing, guaranteeing the uniformity of the mechanical properties of the outer coating. This ensures the final coating meets the design requirements for stiffness coefficient K and modulus decoupling coefficient G, achieving long-term reliability and environmental adaptability of the thin-diameter single-mode optical fiber.

[0052] The combination of waveguide structure optimization, coating mechanical design, and segmented curing process in this application produces significant synergistic gains. Waveguide structure optimization adjusts the refractive index profile of the fiber core 1 and the recessed cladding 2, enhancing the light confinement capability through germanium doping and alkali metals. Coating mechanical design matches the thickness and modulus parameters of the inner coating 4 and the outer coating 5, achieving stress buffering using the stiffness coefficient K and the modulus decoupling coefficient G. The segmented curing process controls the energy distribution and oxygen concentration environment under ultraviolet irradiation, ensuring geometric accuracy through pre-curing and main curing. These three processes act on the optical transmission path, the stress buffer layer, and the structural forming process, respectively. Improvements in a single dimension can only solve local problems, while the systematic combination can cover the entire performance requirements of thin-diameter optical fibers from materials to processes. Thus, at the overall level, the combination of waveguide structure optimization, coating mechanical design, and segmented curing process in this application produces significant synergistic gains.

[0053] With the trend towards smaller fiber diameters, the reduced outer diameter of optical fibers leads to thinner coatings. Traditional processes struggle to simultaneously ensure low bending loss and high mechanical strength, often resulting in trade-offs. However, this application overcomes these performance constraints by utilizing the synergistic effects of waveguide-based light field confinement, coating-based stress buffering, and curing-based precision assurance. This allows for simultaneous improvements in bending resistance, mechanical strength, and concentricity, rather than a trade-off between the two. Comparative experimental data reveals that individual improvements to any single technical aspect significantly reduce performance gains compared to the combined approach, demonstrating that this application's solution achieves a synergistic effect greater than the sum of its parts. This solves the industry challenge of simultaneously achieving high bending resistance, mechanical strength, and concentricity in small-diameter optical fibers.

[0054] See Table 3:

[0055] The embodiments described below are some of the embodiments of this application: Fabrication of a small-diameter, bend-insensitive single-mode fiber: In this embodiment, the waveguide structure is first determined: the core 1 has a diameter of 8.8 μm and is doped with GeO2; the recessed cladding 2 has a diameter of 35 μm and is doped with F, Δn = -0.45%. This waveguide parameter design aims to enhance the light-binding ability by increasing the refractive index of the core 1 through germanium doping, while simultaneously utilizing the fluorine-doped recessed cladding 2 to form a trench-assisted structure. The refractive index difference Δn = -0.45% meets the technical requirement of less than or equal to -0.4%, effectively suppressing mode leakage during bending and providing an optical basis for narrower diameter fiber fabrication.

[0056] Next, the coating structure was determined: the inner coating 4 is made of isooctyl acrylate modified acrylate with a modulus of 0.8 MPa; the outer coating 5 is made of acrylate containing 10 wt% nano-SiO2 (particle size 5 nm) with a modulus of 1200 MPa. The inner coating 4 is modified with flexible monomers to reduce the modulus, while the outer coating 5 introduces nanoparticles to increase the modulus. The two coatings form a significant modulus difference, providing a material basis for subsequent mechanical parameter calculations, ensuring that the inner coating 4 buffers stress while the outer coating 5 provides support.

[0057] Parameter verification was performed: the thickness of the inner coating 4 was t1 = 15 μm, and the thickness of the outer coating 5 was t2 = 30 μm. The stiffness coefficient was calculated as K = 30 / 15 * 1200 / 0.8 = 3000, which meets the protection range of 1200 ≤ K ≤ 5000. The modulus decoupling coefficient was calculated as G = 1200 / 0.8 = 1500, which meets the requirement of G ≥ 1000. The K and G values ​​selected in this embodiment are both located in the middle of the preferred range, verifying the feasibility of the stiffness balance formula and the mechanical decoupling formula in the actual formulation. This ensures that the stress distribution of the coating system is reasonable under lateral pressure, preventing excessive compression of the inner coating 4 leading to micro-bending loss, while ensuring that the inner coating 4 is in an extremely low modulus state to absorb minor deformations.

[0058] Production Process: Fiber Drawing: Fiber drawing tower temperature 2100℃, fiber drawing speed 2000m / min. High temperature ensures sufficient softening of the preform, and high-speed fiber drawing matches mass production efficiency. Coating Pretreatment: The outer coating 5 flows through an ultrasonic dispersion module at a frequency of 30kHz and a power density of 1.0W / cm². It then enters a static mixer, with temperature control via 20℃ circulating water. Ultrasonic dispersion breaks up nanoparticle agglomeration, and temperature control ensures stable coating viscosity. Coating: Two layers of coating are applied using a precision mold. The inner coating viscosity is 4500cps, and the outer coating viscosity is 12000cps. Viscosity matching ensures uniform coating thickness and avoids interfacial mixing. Pre-curing: LED-UV light source, power 300W, main wavelength 365nm, light intensity 15mW / cm², nitrogen protection maintains oxygen content <800ppm. Spacing 0.8m. Main Curing: Mercury lamp, power 1500W, broad spectrum (including deep ultraviolet band), light intensity 180mW / cm². The segmented curing process uses low-intensity pre-curing to correct concentricity, and high-intensity main curing to complete deep cross-linking, with a spacing of 0.8m to provide a stress release area.

[0059] Finally, performance tests were conducted: the cladding diameter was 124.7 μm, the inner coating 4 thickness was 15 μm, the outer coating 5 thickness was 30 μm, and the total outer diameter was 165 μm. The fiber screening tension reached 220 kpsi, and the dynamic fatigue parameter nd=22. Under a lateral pressure of 100 N / cm, the additional attenuation was <0.05 dB / km. The 1310 nm mode field diameter was 9.2 μm, and the bending loss when the 1550 nm mode field was wound around the fiber with a radius of 7.5 mm was 0.3 dB / km. Experimental data demonstrate that the coating structure defined by the above formula has excellent mechanical reliability and optical stability. The total outer diameter of 165 μm meets the requirement of a small diameter of ≤170 μm, the bending loss of 0.3 dB / km is better than the standard of ≤0.5 dB / km, and the dynamic fatigue parameter nd=22 is higher than the requirement of ≥20, verifying that the technical solution of this application achieves synergistic optimization of bending resistance, mechanical strength, and concentricity under the condition of small diameter.

[0060] In the description of this application, it should be noted that the terms "upper," "lower," etc., indicating the orientation or positional relationship are based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application. Unless otherwise expressly specified and limited, the terms "installed," "connected," and "linked" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication between two elements. For those skilled in the art, the specific meaning of the above terms in this application can be understood according to the specific circumstances.

[0061] It should be noted that in this application, relational terms such as "first" and "second" are used merely to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.

[0062] The above description is merely a specific embodiment of this application, enabling those skilled in the art to understand or implement this application. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of this application. Therefore, this application is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features claimed herein.

Claims

1. A small-diameter single-mode optical fiber, characterized by, It includes: Optical fiber body; The coating layer includes an inner coating (4) disposed on the outer surface of the optical fiber body and an outer coating (5) covering the inner coating (4). The thickness of the inner coating (4) is t1, and the elastic modulus is E1. The thickness of the outer coating (5) is t2, and the elastic modulus is E2. They satisfy the following relationship: The stiffness coefficient of the coating layer is K = (t2 / t1) × (E2 / E1), where 1200 ≤ K ≤ 5000; The modulus decoupling coefficient of the coating layer is G=E2 / E1, where G≥1000.

2. The narrow-diameter single-mode optical fiber as described in claim 1, characterized in that: The outer diameter of the thin-diameter single-mode optical fiber is 150μm~170μm; The thickness of the coating layer is ≤22.5μm.

3. The narrow-diameter single-mode optical fiber as described in claim 1, characterized in that: The material of the inner coating (4) includes acrylate and flexible monomer, and the elastic modulus E1 of the inner coating (4) is 0.3MPa to 1.0MPa, and the elongation at break is ≥100%; The material of the outer coating (5) includes acrylate and silica nanoparticles. The elastic modulus E2 of the outer coating (5) is 800MPa to 1500MPa, and the elongation at break is ≥15%.

4. The narrow-diameter single-mode optical fiber as described in claim 3, characterized in that: The flexible monomer material includes at least one of isooctyl acrylate or laurate. The particle size of the silica nanoparticles is 3 nm to 8 nm; The amount of silica nanoparticles added to the outer coating (5) material is 5% to 15% of the total mass of the outer coating (5) material.

5. The narrow-diameter single-mode optical fiber as described in claim 1, characterized in that: The optical fiber body includes a fiber core (1), a recessed cladding (2), and a cladding structure (3) arranged sequentially from the inside to the outside. The doping elements of the fiber core (1) include germanium and alkali elements, and the doping elements of the sunken cladding (2) include fluorine.

6. The narrow-diameter single-mode optical fiber as described in claim 5, characterized in that: The refractive index difference Δn between the sunken cladding (2) and pure silicon dioxide is ≤ -0.4%; The ratio of the outer diameter of the sunken cladding (2) to the diameter of the fiber core (1) is 2.5 to 4.

7. The narrow-diameter single-mode optical fiber as described in claim 1, characterized in that: The narrow-diameter single-mode fiber has a mode field diameter of 8.2 μm to 9.6 μm at a wavelength of 1310 nm; The bending loss of the thin-diameter single-mode fiber when wound with a radius of 7.5 mm for one turn at a wavelength of 1550 nm is ≤0.5dB / km. The narrow-diameter single-mode optical fiber has a screening tension ≥200kpsi and a dynamic fatigue parameter nd ≥20.

8. A method of making a small effective area single mode optical fiber as claimed in any one of claims 1 to 7, characterized in that, It includes: The optical fiber preform is drawn into an optical fiber body; The outer surface of the optical fiber body is coated with an inner coating (4) and an outer coating (5) in sequence. The thickness of the inner coating (4) is controlled to be t1, the thickness of the outer coating (5) is controlled to be t2, the elastic modulus of the inner coating (4) is E1, and the elastic modulus of the outer coating (5) is E2, so that the formed coating layer satisfies: stiffness coefficient K=(t2 / t1)×(E2 / E1), 1200≤K≤5000, modulus decoupling coefficient G=E2 / E1, G≥1000; The coated optical fiber body is then cured by irradiation.

9. The method for fabricating a narrow-diameter single-mode optical fiber as described in claim 8, characterized in that: The curing process is ultraviolet lamp curing, and the curing process includes a pre-curing process and a main curing process. In the pre-curing process, the ultraviolet light intensity is 10mW / cm²~20mW / cm², the oxygen concentration is <1000ppm, and the power is 200~400W. In the main curing process, the ultraviolet light intensity is 150mW / cm²~210mW / cm², and the power is 1200~1800W; The distance between the pre-curing oven used in the pre-curing process and the main curing oven used in the main curing process is 0.7m to 1.0m.

10. The method for fabricating a narrow-diameter single-mode optical fiber as described in claim 8, characterized in that: The material of the outer coating (5) includes acrylate and silica nanoparticles; Before applying the outer coating (5) paint, the method further includes: Surface modification of silica nanoparticles was performed using silane coupling agents; Surface-modified silica nanoparticles were added to acrylate prepolymer and ultrasonically dispersed to obtain a nano suspension. The outer coating (5) is made from the nano suspension.