Method and system for automatic coating control for preparation of water washable long-lasting antimicrobial bed sheet fabric
By monitoring the state of the base fabric and slurry in real time and adaptively adjusting the coating parameters, the problem of coating bonding strength caused by residual additives on the base fabric surface and fluctuations in slurry composition has been solved, thus improving the quality and production efficiency of water-resistant, long-lasting antibacterial bed sheet fabrics.
Patent Information
- Application Number
- CN202611207127.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-11
- Publication Date
- 2026-11-24
AI Technical Summary
In the process of preparing water-resistant and long-lasting antibacterial bed sheet fabric by coating method, the fluctuation of residual additives and sizing composition on the base fabric surface leads to a decrease in the interfacial bonding strength and cohesive strength between the coating and the base fabric, affecting the water-resistant and antibacterial properties of the fabric.
By collecting real-time interface state parameters of the base fabric and state parameters of the slurry components, and using near-infrared diffuse reflectance detection technology to determine the residual additive contamination level and effective crosslinking component concentration, the pressure of the pressure roller, the speed of the coating roller, and the slurry supply flow rate are adaptively adjusted to compensate for the defects of base fabric surface contamination and slurry component attenuation.
It improves the adhesion and cohesive strength of the coating, enhances the wash resistance and antibacterial properties of the fabric, reduces product rework and scrap rates, and improves batch consistency and production efficiency.
Smart Images

Figure CN123156804A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of coating automation control technology, and in particular to an automated coating control method and system for preparing water-resistant, long-lasting antibacterial bed sheet fabric. Background Technology
[0002] Among functional textiles, bed sheet fabrics with wash-resistant and long-lasting antibacterial properties have received widespread attention due to their ability to meet the dual needs of both medical and consumer sectors. The processing methods for imparting antibacterial properties to fabrics mainly include impregnation, padding, spraying, and coating. In comparison, coating, by applying a functional coating containing antibacterial agents to the surface of the base fabric, forms a relatively independent functional layer with controllable thickness. This achieves high antibacterial activity while having minimal impact on the physical and mechanical properties of the base fabric itself, thus offering significant advantages in preparing bed sheet fabrics that combine wash resistance and long-lasting antibacterial properties. The complete process for preparing antibacterial fabrics using the coating method typically includes several steps such as base fabric pretreatment, antibacterial coating slurry supply and application, coating and setting, pre-drying, and cross-linking curing. Among these, the coating step is the core step, uniformly applying the antibacterial coating slurry to the base fabric surface, determining the initial loading and uniformity of the antibacterial agent on the fabric.
[0003] In existing technologies, the coating process for sheet fabrics with washability and long-lasting antibacterial properties primarily employs a control mode that sets fixed process parameters and executes them sequentially. This means that parameters such as coating amount, pressure roller pressure, and coating roller speed are set according to the target product's process requirements, and the production process continuously runs automatically according to these fixed parameters until the batch production is completed or intermittent manual adjustments are made based on operator experience. This control mode is acceptable under ideal conditions of stable incoming materials and good batch consistency of the sizing agent. However, in actual industrial production, two universally applicable objective variables exist:
[0004] Firstly, antibacterial coating slurry is not a material with constant properties. Coating slurry is usually a multiphase mixed dispersion system composed of various components such as antibacterial agents, crosslinking agents, binders, dispersants, and solvents. Its physicochemical state will drift with factors such as storage time, environmental temperature and humidity, microbial contamination, and slow reactions between components. Specifically, it manifests as a decrease in solid content, a decrease in the concentration of effective ingredients, and a deterioration in dispersion uniformity. These changes directly lead to a reduction in the amount of effective substances in the slurry that can actually participate in film formation and crosslinking. At this time, if the initial coating amount is still used for processing, the actual amount of effective antibacterial agents and crosslinking agents deposited on the fabric per unit area will be lower than expected. The crosslinking density and adhesion of the coating will decrease accordingly, and the antibacterial performance of water resistance will be difficult to meet the standards.
[0005] Secondly, the base fabric used as the coating carrier is not a standardized, ideal substrate. In the textile industry chain, various processing aids such as sizing agents, oils, softeners, and water-repellent agents are introduced into the base fabric during weaving and pre-dyeing and finishing processes. These aids may still exist on the fiber surface in residual form after pretreatment. The types and quantities of residual aids on the surface of base fabrics vary between different batches and even between different rolls of the same batch. When residual aids form a certain degree of coverage on the fiber surface, the direct contact area between the coating sizing agent and the fiber decreases, and the interfacial bonding strength declines. At this point, even if the sizing agent itself is in normal condition and the coating amount meets the set value, the coating is difficult to adhere firmly to the base fabric. After washing, the coating is easily peeled off from the fiber surface or partially detached, and the antibacterial properties rapidly decline.
[0006] The two variables mentioned above often coexist and overlap in actual production: the attenuation of the effective components of the slurry reduces the crosslinking strength and cohesive strength of the coating itself, while fluctuations in impurities on the base fabric surface weaken the interfacial bonding strength between the coating and the substrate. The former affects the "bulk strength" of the coating, while the latter affects the "interfacial strength" of the coating. Both, through different pathways, contribute to the deterioration of the fabric's wash resistance and antibacterial properties. Summary of the Invention
[0007] Therefore, it is necessary to provide an automated coating control method and system for preparing water-resistant, long-lasting antibacterial bed sheet fabric to address the aforementioned technical problems.
[0008] This invention provides a method comprising:
[0009] Before performing the slurry impregnation and coating process on the current base fabric, the interface state parameters of the current base fabric are collected in real time.
[0010] The residual additive contamination level on the current base fabric surface is determined by analyzing the interface state parameters;
[0011] The first adjustment parameter is determined based on the residual additive contamination level and the preset first adjustment mapping table. The first adjustment parameter is used to adjust the coating, wetting and bonding strength of the current base fabric. The first adjustment mapping table is used to reflect the correspondence between the residual additive content level and the first adjustment parameter.
[0012] Real-time acquisition of component state parameters of the slurry to be added;
[0013] The effective crosslinking component concentration of the target active substance in the slurry to be added is obtained according to the component state parameters, and the second adjustment parameter is determined according to the effective crosslinking component concentration and the preset second adjustment mapping relationship table. The second adjustment parameter is used to adjust the supply flow rate of the slurry to be added when coating the current base fabric. The second adjustment mapping relationship table is used to reflect the correspondence between the effective crosslinking component concentration and the second adjustment parameter.
[0014] A comprehensive compensation instruction is generated based on the first adjustment parameter and the second adjustment parameter. The comprehensive compensation instruction is used to compensate for defects in the base fabric additives and defects in the crosslinking strength of the slurry through the first adjustment parameter and the second adjustment parameter.
[0015] The slurry impregnation and coating process for the current base fabric is executed according to the comprehensive compensation instruction.
[0016] In one embodiment, the current base fabric is divided into several detection segments along the running direction of the base fabric; the interface state parameters are used to reflect the degree of residual additive contamination on the surface of the current base fabric, and the interface state parameters are obtained by applying a preset first target characteristic band near-infrared diffuse reflectance detection to each of the detection segments of the current base fabric, and the interface state parameters include the real-time spectral intensity parameters corresponding to each of the detection segments of the current base fabric.
[0017] In one embodiment, determining the residual additive contamination level on the current base fabric surface by parsing the interface state parameters specifically includes:
[0018] Based on the preset standard spectral range of the base fabric, normal light intensity parameters within the standard spectral range of the base fabric and abnormal light intensity parameters exceeding the standard spectral range of the base fabric are obtained from the interface state parameters.
[0019] Calculate the average value of all the normal light intensity parameters and use the average value as the adaptive noise floor baseline corresponding to the current base fabric;
[0020] The detection segment corresponding to the abnormal light intensity parameter is taken as the suspected defect segment. Based on the continuous distribution of the suspected defect segment, the ultimate defect light intensity parameter is obtained by screening from the abnormal light intensity parameters.
[0021] Based on the light intensity parameters of the extreme defects and the adaptive noise baseline, the real-time absorbance of the current base fabric is calculated using the Lambert-Beer law.
[0022] Based on the real-time absorbance of the base fabric and the preset auxiliary contamination classification relationship, the residual auxiliary contamination level corresponding to the current base fabric surface is determined.
[0023] In one embodiment, the step of selecting the ultimate defect light intensity parameters from the abnormal light intensity parameters based on the continuous distribution of the suspected defect segments specifically includes:
[0024] Obtain the distribution coordinates of all the suspected defect segments, and determine whether each suspected defect segment has an adjacent relationship with any other suspected defect segment based on the distribution coordinates;
[0025] If the judgment result is yes, the suspected defective segment is taken as the actual defective segment;
[0026] Among all the abnormal light intensity parameters corresponding to the real defect segments, the spectral intensity parameter with the smallest value is selected as the limit defect light intensity parameter.
[0027] In one embodiment, the slurry to be applied is divided into several detection areas; the component state parameters are used to reflect the real-time effective content level of the target active material in the slurry to be applied that can covalently anchor with the current base fabric. The component state parameters are obtained by applying a preset second target characteristic band near-infrared diffuse reflectance detection to each detection area of the slurry to be applied. The component state parameters include the real-time spectral intensity parameters corresponding to each detection area of the slurry to be applied.
[0028] In one embodiment, obtaining the effective crosslinking component concentration based on the component state parameters specifically includes:
[0029] Based on the component state parameters, the real-time absorbance of each detection area of the slurry to be applied is calculated using the Lambert-Beer law.
[0030] Based on the preset standard spectral range of effective components, the peaks of the real-time absorbance of all the slurry segments are identified, the characteristic absorption peaks are located, and the peak absorbance parameters corresponding to the characteristic absorption peaks are extracted. The peak absorbance parameters are the integrated absorbance values obtained by integrating the peak area of the characteristic absorption peaks.
[0031] The peak absorbance is input into a pre-constructed quantitative analysis model for effective crosslinking components to obtain the corresponding concentration of effective crosslinking components. The quantitative analysis model for effective crosslinking components is used to establish a quantitative mapping relationship between absorbance and concentration of effective crosslinking components.
[0032] In one embodiment, generating the comprehensive compensation instruction based on the first adjustment parameter and the second adjustment parameter specifically includes:
[0033] The first execution sub-instruction is generated based on the first adjustment parameters. The first adjustment parameters include the roller pressure compensation parameters of the pressure roller and the roller speed compensation parameters of the coating roller. The first execution sub-instruction is used to adjust the pressure roller and the coating roller according to the first adjustment parameters to compensate for the residual additive contamination defects on the current base fabric surface.
[0034] A second execution sub-instruction is generated based on the second adjustment parameter, the second adjustment parameter including the slurry supply flow rate per unit base fabric, and the second execution sub-instruction is used to adjust the feed pump according to the second adjustment parameter to compensate for the crosslinking strength defects of the slurry to be added;
[0035] The first execution sub-instruction and the second execution sub-instruction are time-coordinated to generate a comprehensive compensation instruction, which is a composite instruction set containing the first execution sub-instruction and the second execution sub-instruction.
[0036] The present invention also provides an automated coating control device for implementing the automated coating control method for preparing washable and long-lasting antibacterial bed sheet fabric as described in any of the above claims, the device comprising:
[0037] The parameter acquisition module is used to collect the interface state parameters of the current base fabric and the component state parameters of the slurry to be applied in real time before performing the slurry impregnation and coating process on the current base fabric.
[0038] The parameter parsing module is used to parse the interface state parameters to determine the residual additive contamination level on the current base fabric surface, and to obtain the effective crosslinking component concentration of the target active substance in the slurry to be added based on the component state parameters.
[0039] The adjustment parameter determination module is used to determine a first adjustment parameter based on the residual additive pollution level and a preset first adjustment mapping table, and to obtain the effective crosslinking component concentration of the target active substance in the slurry to be added based on the component state parameters, and to determine a second adjustment parameter based on the effective crosslinking component concentration and a preset second adjustment mapping table.
[0040] The instruction generation module is used to generate a comprehensive compensation instruction based on the first adjustment parameter and the second adjustment parameter;
[0041] The instruction execution module is used to execute the slurry impregnation and coating process on the current base fabric according to the comprehensive compensation instruction.
[0042] The present invention also provides an electronic device, including a memory and a processor, wherein the memory stores a computer program, and the processor executes the computer program to implement the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric as described above.
[0043] The present invention also provides a computer storage medium storing a computer program, which, when executed by a processor, implements the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric as described above.
[0044] The aforementioned automated coating control method, device, electronic equipment, and storage medium for preparing water-resistant, long-lasting antibacterial bed sheet fabric have the following advantages compared to existing technologies:
[0045] (1) On the one hand, this invention determines the surface residual additive contamination level by analyzing the interface state parameters of the base fabric and adaptively adjusts the roller pressure of the pressure roller and the roller speed of the coating roller to enhance the interfacial bonding strength between the coating and the base fabric. On the other hand, it obtains the effective crosslinking component concentration by analyzing the slurry component state parameters and adaptively adjusts the slurry supply flow rate to compensate for the loss of bulk crosslinking strength caused by the decay of effective components. Through real-time detection and synergistic compensation of the dual-end states of the base fabric side and the slurry side, the problem of the deterioration of the wash-resistant and antibacterial performance of the fabric caused by the superposition of slurry strength defects and interface contamination defects in the current process of preparing wash-resistant and long-lasting antibacterial fabrics is greatly improved. The compensation instructions of the two aspects take effect in parallel and do not interfere with each other, and synergistically ensure the adhesion and cohesive strength of the coating from the interface path and the bulk path respectively, thereby effectively improving the wash-resistant and antibacterial performance of the fabric.
[0046] (2) This invention achieves accurate quantification of the degree of contamination on the base fabric surface and the concentration of effective components in the slurry through an adaptive quantitative detection strategy based on Lambert-Beer's law. It overcomes the technical defect of traditional fixed process parameter control mode lacking responsiveness to incoming material fluctuations, and helps coating control respond in real time to the incoming material status fluctuations of the base fabric and slurry, greatly improving the batch consistency of coating quality between different batches and different rolls.
[0047] (3) By decoupling the compensation for residual additive contamination on the base fabric surface and the compensation for the attenuation of effective crosslinking components in the slurry into two independent control channels, this invention avoids the problem of overcompensation or undercompensation of one defect by a single compensation strategy, reduces the sensitivity of the coating process to fluctuations in incoming materials from the previous process and the storage time of the slurry, improves the process tolerance and production efficiency, and further reduces the product rework rate and scrap rate caused by slurry failure or base fabric contamination. It has good economic benefits and industrial application prospects. Attached Figure Description
[0048] To more clearly illustrate the technical solutions in this invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this invention. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.
[0049] Figure 1 This is a flowchart illustrating an automated coating control method for preparing a washable, long-lasting antibacterial bed sheet fabric, as provided by the present invention.
[0050] Figure 2 This is a schematic diagram illustrating the implementation architecture of the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric in a specific embodiment of the present invention.
[0051] Figure 3This is a schematic diagram of the parameter acquisition module in the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric, provided in a specific embodiment of the present invention.
[0052] Figure 4 This is a schematic diagram of the data analysis module in the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric, provided in a specific embodiment of the present invention, when compensating for defects in the base fabric.
[0053] Figure 5 This is a schematic diagram of the data analysis module in the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric, provided in a specific embodiment of the present invention, when compensating for slurry defects.
[0054] Figure 6 This is a schematic diagram illustrating the logic of determining the residual additive contamination level on the current base fabric surface using the analytical interface state parameters of the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric in a specific embodiment of the present invention.
[0055] Figure 7 The diagram illustrates the logic of obtaining the effective crosslinking component concentration based on component state parameters in the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric, as provided in a specific embodiment of the present invention.
[0056] Figure 8 This is a schematic diagram of the structure of an automated coating control device provided by the present invention.
[0057] Figure 9 This is a diagram of the internal structure of the electronic device provided by the present invention. Detailed Implementation
[0058] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0059] The following is combined Figures 1 to 9 This invention describes an automated coating control method and system for preparing water-resistant, long-lasting antibacterial bed sheet fabric.
[0060] like Figure 1 As shown in one embodiment, an automated coating control method for preparing a washable, long-lasting antibacterial bed sheet fabric includes the following steps:
[0061] Step S100: Before performing the slurry impregnation and coating process on the current base fabric, the interface state parameters of the current base fabric are collected in real time.
[0062] Combination Figures 2 to 5 As shown, in a specific implementation, the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric provided by this invention is realized through a coating mechanism and an intelligent terminal that communicates with the coating mechanism. The coating mechanism includes, but is not limited to, roller coating mechanisms, doctor blade coating mechanisms, anilox roller coating mechanisms, or slot extrusion coating mechanisms, etc., to ensure that the slurry is uniformly applied to the surface of the base fabric. The coating mechanism includes a coating roller, a pressure roller, and a coating head. The coating roller supports and conveys the current base fabric, and the coating head applies a set amount of slurry to the surface of the current base fabric. The pressure roller is positioned above or opposite the coating roller, forming a coating gap between it and the coating roller to allow the current base fabric to pass through. It applies pressure to the current base fabric, ensuring that the base fabric and the coating head are tightly bonded, so that the slurry is evenly impregnated and adhered to the surface of the base fabric. The intelligent terminal includes a parameter acquisition module, which specifically includes an interface state acquisition unit. The interface state acquisition unit is used to acquire the interface state parameters of the current base fabric in real time before performing the slurry impregnation and coating process on the current base fabric.
[0063] In this embodiment, the current base fabric is divided into several detection segments along the running direction of the base fabric. The interface state acquisition unit consists of multiple first near-infrared detection probes arranged at intervals along the width direction of the base fabric. Each detection segment corresponds to one first near-infrared detection probe. The first near-infrared detection probe is used to apply a preset first target characteristic band to each detection segment of the current base fabric for near-infrared diffuse reflection detection and to acquire the real-time spectral intensity parameters corresponding to each detection segment.
[0064] It should be noted that during the weaving and pre-dyeing processes of the base fabric, various processing aids such as sizing agents, oils, softeners, and water repellents are inevitably introduced. Even after pre-washing or desizing processes, these aids may still remain on the fiber surface and in the yarn gaps. Before the sizing and coating process, that is, after the aforementioned pretreatment steps and before entering the coating station, the base fabric has not yet come into contact with any sizing agent. Its surface condition can accurately reflect the residual agent contamination status of the incoming base fabric, reducing interference from sizing agent coverage on the near-infrared diffuse reflectance detection signal. Furthermore, because different chemical groups, such as CH, NH, and OH hydrogen-containing groups, have selective absorption characteristics for specific wavelengths of near-infrared light, various processing aids remaining on the fiber surface, such as oils, softeners, and water repellents, will produce corresponding characteristic absorption or reflection signals in specific bands of the near-infrared spectrum due to the different hydrogen-containing groups in their molecular structures.
[0065] In step S100 above, the interface state parameters are used to reflect the degree of residual additive contamination on the surface of the current base fabric. The interface state parameters are obtained by applying a preset first target characteristic band near-infrared diffuse reflectance detection to each detection segment of the current base fabric. The interface state parameters include the real-time spectral intensity parameters corresponding to each detection segment of the current base fabric. The first target characteristic band is a near-infrared wavelength range with the highest sensitivity and selectivity to residual additives, which is pre-selected through experimental calibration or chemometric methods. Under this characteristic band, the higher the content of residual additives on the surface of the base fabric, the higher the absorbance and the lower the spectral intensity of the reflection. Thus, the degree of residual additive contamination on the surface of the base fabric can be quantitatively characterized by collecting the real-time spectral intensity parameters of each detection segment.
[0066] Step S200: Analyze the interface status parameters to determine the residual additive contamination level on the current base fabric surface.
[0067] Combination Figures 2 to 5 As shown, the intelligent terminal also includes a parameter parsing module, which is used to parse interface status parameters to determine the residual additive contamination level on the current base fabric surface; specifically, step S200 is as follows:
[0068] Step S210: Based on the preset standard spectral range of the base fabric, normal light intensity parameters within the standard spectral range of the base fabric and abnormal light intensity parameters outside the standard spectral range of the base fabric are selected from the interface state parameters.
[0069] The standard spectral range for the base fabric refers to a pre-established spectral intensity reference range based on a large number of clean base fabric samples that are free from pollution or have low pollution levels. This range reflects the intrinsic diffuse reflectance intensity of the base fabric's fiber material in the first target characteristic wavelength band. When there are no or only a very small amount of residual additives on the base fabric surface, its near-infrared diffuse reflectance intensity falls within the corresponding standard spectral range, which is defined as a normal light intensity parameter. When residual additives form a coating layer on the fiber surface, the absorption of near-infrared light in this characteristic wavelength band by hydrogen-containing groups in the additive molecules leads to a decrease in diffuse reflectance intensity, causing the measured value to fall below the lower limit of the standard range, which is defined as an abnormal light intensity parameter.
[0070] Step S220: Calculate the average value of all normal light intensity parameters and use the average value as the adaptive noise baseline corresponding to the current base fabric.
[0071] Different rolls and batches of base fabric exhibit objective differences in fiber material, weaving density, and pre-dyeing treatment, leading to batch-to-batch fluctuations in intrinsic diffuse light intensity. Directly using a fixed theoretical light intensity value as a baseline would introduce systematic errors due to the inherent differences in the base fabric itself. To address this issue, this step uses the average light intensity of the current base fabric's normal detection section as an adaptive noise floor baseline. This baseline is dynamically updated according to the actual state of the current base fabric, without the need for a preset fixed threshold.
[0072] Step S230: The detection segment corresponding to the abnormal light intensity parameter is taken as the suspected defect segment. Based on the continuous distribution of the suspected defect segment, the extreme defect light intensity parameter is obtained by screening from the abnormal light intensity parameters.
[0073] It should be noted that in actual production, abnormal light intensity in individual detection sections may be caused by occasional factors, such as: temporary dust adhering to the base fabric surface, instantaneous signal jitter of the near-infrared detection probe, or brief wrinkling of the base fabric during operation. These occasional anomalies do not represent a true continuous contamination zone on the base fabric. Including them in the absorbance calculation would overestimate the overall contamination level of the base fabric. Considering that residual auxiliaries on the fiber surface usually originate from uneven adhesion or incomplete cleaning of sizing agents, oils, and other auxiliaries in the preceding dyeing and finishing processes, this type of contamination often presents as a continuous band along the fabric's operating direction, rather than as isolated points. Therefore, this embodiment addresses the above problem by introducing a continuous distribution judgment mechanism. Specifically, step S230 is implemented as follows:
[0074] Step S231: Obtain the distribution coordinates of all suspected defect segments, and determine whether each suspected defect segment has an adjacent relationship with any other suspected defect segment based on the distribution coordinates.
[0075] Specifically, the distribution coordinates are the position numbers or sequential indices of each suspected defect segment along the running direction of the base fabric. For example, if the current base fabric is divided into the 1st, 2nd, 3rd...Nth detection segments along the running direction, the detection segment numbers corresponding to the abnormal light intensity parameters determined in step S210 are recorded one by one to form a set of distribution coordinates for suspected defect segments. In this step, for each suspected defect segment in the distribution coordinate set, it is determined whether it has at least one adjacent suspected defect segment. Adjacent association means that if the preceding or following detection segment of a suspected defect segment is also marked as a suspected defect segment along the running direction of the base fabric, then the two are considered to have an adjacent association relationship. If a suspected defect segment has at least one adjacent suspected defect segment, the adjacent association relationship of the suspected defect segment is determined to be yes; if neither the preceding nor following detection segment of a suspected defect segment is a suspected defect segment, the adjacent association relationship of the suspected defect segment is determined to be no.
[0076] In step S232, if the judgment result is yes, the suspected defect segment is treated as a real defect segment; if the judgment result is no, the suspected defect segment is treated as an isolated noise segment and excluded.
[0077] Specifically, based on the judgment result of step S231 above, suspected defect segments with adjacent relationships are identified as real defect segments—that is, defect segments caused by continuous contamination from residual additives; isolated suspected defect segments without any adjacent relationships are identified as isolated noise segments—that is, misjudged anomalies caused by occasional factors (such as instantaneous dust adhesion or probe signal jitter), and are removed from subsequent calculations. Through the above mechanism, this step can effectively filter out the interference of occasional noise on the detection results while retaining the true contamination characteristics, greatly reducing the situation of misjudging instantaneous or local occasional anomalies as contamination from residual additives on the base fabric surface, thereby improving the accuracy of contamination level determination.
[0078] Step S233: Among all the abnormal light intensity parameters corresponding to the real defect segments, select the spectral intensity parameter with the smallest value as the limit defect light intensity parameter.
[0079] Specifically, after screening in step S232, each real defect segment corresponds to an original abnormal light intensity parameter, which is the real-time spectral intensity value corresponding to the detection segment when it was determined to be abnormal in step S210. It should be noted that in near-infrared diffuse reflectance detection, the smaller the light intensity value, the stronger the absorption and attenuation of the characteristic near-infrared light band of the detection segment, indicating a more severe coverage of the fiber surface by residual additives. Therefore, in this embodiment, the smallest value among these abnormal light intensity parameters is selected as the limiting defect light intensity parameter. The minimum light intensity value among all real defect segments corresponds to the detection segment with the most severe residual additive coverage in the continuous contamination zone. Using this limiting value as the benchmark for subsequent absorbance calculation can characterize the most severe working condition of the current base fabric surface contamination, thereby ensuring effective interfacial bonding between the coating and the base fabric as much as possible.
[0080] Step S240: Based on the light intensity parameters of the limit defect and the adaptive noise baseline, the real-time absorbance of the current base fabric is calculated using the Lambert-Beer law.
[0081] The Lambert-Beer law is the fundamental quantitative basis for spectral analysis. Its principle is that when a beam of light of a specific wavelength shines on a material surface, the degree to which the material absorbs light energy is positively correlated with the concentration of the light-absorbing substance in the optical path and the optical path length. In this embodiment, a modified form of the Lambert-Beer law is used, that is, the absorption attenuation effect of residual additives on the near-infrared characteristic wavelength band of the base fabric is converted into a quantifiable absorbance index.
[0082] In a pollution-free state, the base fabric surface contains little or no residual additives. After diffuse reflection of near-infrared light on the base fabric surface, the intensity of the reflected light received by the detection probe is relatively high. This intensity is characterized by the adaptive noise floor baseline, and its physical meaning is equivalent to the "incident light intensity" reference value in the Lambert-Beer law. However, when residual additives are present on the base fabric surface, the corresponding hydrogen-containing groups in the additive molecules will selectively absorb near-infrared light in the first target characteristic band, resulting in a decrease in diffuse reflection intensity. The measured light intensity after this decrease is the limiting defect light intensity parameter. Specifically, by comparing the adaptive noise floor baseline with the limiting defect light intensity parameter, taking the logarithm of the ratio, and then taking the negative value, the real-time absorbance value of the current base fabric can be obtained. This absorbance value directly reflects the absorption intensity of residual additives on the characteristic band light energy. The stronger the absorption, the greater the equivalent coverage of residual additives on the base fabric surface, i.e., the more severe the pollution. Through the above calculations, the original light intensity data, which was originally affected by the intrinsic differences between batches of base fabric, can be transformed into an absorbance index that is only related to the content of residual additives, thus realizing a unified quantitative measurement of the degree of contamination between different base fabrics.
[0083] Step S250: Determine the residual additive contamination level on the current base fabric surface based on the real-time absorbance of the base fabric and the preset additive contamination classification relationship.
[0084] The calibration relationship for additive contamination is pre-established experimentally. Specifically, several sets of base fabric standard samples with different known residual additive contents are prepared. The near-infrared diffuse reflectance intensity of each standard sample is measured in the same detection area, and the real-time absorbance of each base fabric is calculated according to steps S210 to S240. Simultaneously, the actual residual additive content of each sample is determined by weighing or chemical extraction. A calibration curve is established with the measured absorbance as the abscissa and the residual additive content as the ordinate. Based on a preset contamination level range, three levels—low contamination, medium contamination, and high contamination—absorbance threshold ranges are defined. In this embodiment, the calculated real-time absorbance of the base fabric is compared with the aforementioned threshold ranges to determine the current residual additive contamination level of the base fabric. This contamination level is a discrete qualitative or semi-quantitative indicator, facilitating rapid lookup of the corresponding first adjustment parameter according to a preset first adjustment mapping relationship table.
[0085] Step S300: Determine the first adjustment parameter based on the residual additive contamination level and the preset first adjustment mapping table.
[0086] The first adjustment mapping table is a data structure pre-stored in the smart terminal, used to record the mapping relationship between different residual additive pollution levels and the corresponding first adjustment parameters. The first adjustment parameters are used to adjust the coating impregnation and bonding strength of the current base fabric. In this embodiment, the first adjustment parameters include the roller pressure compensation parameter of the pressure roller and the roller speed compensation parameter of the coating roller. The roller pressure compensation parameter is an additional adjustment amount on top of the base roller pressure value originally set by the coating mechanism, and the roller speed compensation parameter is an additional adjustment amount on top of the base roller speed value originally set by the coating mechanism. Roller pressure refers to the linear pressure applied by the pressure roller to the surface of the current base fabric, that is, the contact pressure between the pressure roller and the coating roller per unit width, with the unit being kN / m. Roller speed refers to the rotational linear speed of the coating roller, with the unit being m / min. In actual execution, the final actual control values applied to the pressure roller and the coating roller are the algebraic sum of the base roller pressure value and the roller pressure compensation parameter, and the algebraic sum of the base roller speed value and the roller speed compensation parameter, respectively.
[0087] It should be noted that when the residual additive contamination level on the base fabric surface is high, the proportion of the fiber surface covered by additives increases, reducing the effective contact area between the coating slurry and the fiber, and consequently decreasing the interfacial bonding strength. To compensate for this interfacial strength deficiency, it is necessary to increase the roller pressure between the pressure roller and the coating roller, forcing the slurry in the coating head into the fiber gaps and yarn interior under greater mechanical pressure, thereby increasing the physical interlocking degree and interfacial contact area between the slurry and the fiber. Simultaneously, the roller speed of the coating roller can be adaptively reduced to extend the spreading and wetting time of the slurry on the base fabric surface, allowing the slurry to achieve more thorough wetting and penetration before entering the subsequent drying and setting processes. Conversely, when the residual additive contamination level is low or almost non-existent, the base fabric surface has good hydrophilicity and wettability. In this case, there is no need to increase the roller pressure or reduce the roller speed; smaller roller pressure compensation parameters or zero compensation parameters, as well as smaller roller speed compensation parameters or zero compensation parameters, can be applied to balance coating efficiency and energy consumption control.
[0088] In this embodiment, the residual additive contamination level determined in step S250 is a discrete level index, including but not limited to no contamination, low contamination level, medium contamination level, and high contamination level. The first adjustment mapping relationship table is constructed as follows: for each contamination level, the roller pressure compensation parameter and roller speed compensation parameter adapted to it are pre-calibrated through experiments or experience; the specific calibration principle is: the higher the contamination level, the larger the positive increment of the corresponding roller pressure compensation parameter, that is, the greater the pressure added above the basic roller pressure value, and the larger the negative increment of the roller speed compensation parameter, that is, the greater the speed reduction above the basic roller speed value; the lower the contamination level, the smaller the absolute value of the corresponding roller pressure compensation parameter and roller speed compensation parameter. When there is no detectable contamination on the base fabric surface, both the roller pressure compensation parameter and the roller speed compensation parameter can be taken as zero. In the actual control process, after the intelligent terminal determines the residual additive contamination level of the current base fabric in step S250, it directly uses the contamination level as an index to look up the table to obtain the first adjustment parameter that uniquely corresponds to the contamination level, and outputs it to the subsequent step S600 as one of the inputs for generating the comprehensive compensation command. This table lookup method has a fast response speed and small calculation amount, which can meet the time constraint requirements of online real-time control of the coating process.
[0089] For example, when the residual additive contamination level is low, the roller pressure compensation parameter is +2kN / m, that is, an increase of 2kN / m above the basic roller pressure value, and the roller speed compensation parameter is -2m / min, that is, a decrease of 2m / min above the basic roller speed value; when the residual additive contamination level is medium, the roller pressure compensation parameter is +5kN / m, and the roller speed compensation parameter is -5m / min; when the residual additive contamination level is high, the roller pressure compensation parameter is +10kN / m, and the roller speed compensation parameter is -10m / min. The above values are only illustrative examples, and the specific values are determined through experimental calibration based on the actual coating equipment and slurry system. The actual value of the compensated roller pressure should not exceed the maximum allowable linear pressure value of the coating mechanism design, and the actual value of the compensated roller speed should not exceed the maximum allowable operating speed value of the coating mechanism design. When the theoretical value after compensation exceeds the upper limit allowed by the equipment, the upper limit allowed by the equipment shall be used as the actual execution value.
[0090] It should be understood that the specific form of the aforementioned first adjustment parameter varies depending on the type of coating mechanism: for coating mechanisms with pressure rollers and coating rollers, including but not limited to roller coating mechanisms and anilox roller coating mechanisms, the first adjustment parameter is expressed as the linear pressure compensation value between the pressure roller and the coating roller and the roller speed compensation parameter of the coating roller; for coating mechanisms using doctor blade coating heads, the first adjustment parameter is expressed as the contact pressure compensation value between the doctor blade and the coating roller and the roller speed compensation parameter of the coating roller; for coating mechanisms using slit extrusion coating heads, the first adjustment parameter is expressed as the coating gap compensation value between the die head and the base fabric and the roller speed compensation parameter of the coating roller.
[0091] Step S400: Real-time acquisition of component state parameters of the slurry to be added.
[0092] Combination Figures 2 to 5 As shown, in a specific implementation, the parameter acquisition module further includes a component state acquisition unit. This unit is located upstream of the coating head and is used to acquire the component state parameters of the slurry in real time before it enters the coating head. In this embodiment, the slurry to be added is divided into several detection areas. The component state acquisition unit includes a flow cell located in the supply pipeline and a second near-infrared detection probe installed outside the flow cell. The second near-infrared detection probe is used to apply a preset second target characteristic band to each detection area for near-infrared diffuse reflectance detection and to acquire the real-time spectral intensity parameters corresponding to each detection area. The component state parameters include the real-time spectral intensity parameters corresponding to each detection area of the slurry to be added. The second target characteristic band is a near-infrared wavelength range that has a characteristic response to the molecular structure of the target active substance, pre-selected by chemometric methods. This band can partially overlap with or be completely independent of the first target characteristic band, depending on the vibrational characteristics of the chemical groups of the target active substance and the residual additives in the base fabric.
[0093] It should be noted that the component state parameters are collected just before the slurry enters the coating head, i.e., during the stable flow stage after the slurry has been fully stirred or circulated in the supply pipeline. At this time, the slurry is uniformly mixed, at a stable temperature, and has not come into contact with the base fabric. This allows for a true reflection of the real-time effective content level of the target active substance in the slurry to be added, effectively avoiding detection deviations caused by slurry sedimentation or stratification in the pipeline. Simultaneously, dividing the slurry into several detection areas and performing multi-point detection effectively captures the concentration distribution differences of the slurry across the pipeline cross-section. The average value or weighted composite value of the real-time spectral intensity parameters from multiple detection areas serves as the basis for subsequent quantitative analysis. Furthermore, the slurry flow cell has a fixed optical path length, which remains unchanged after assembly, ensuring comparability between detection data from different time points or different batches of slurry.
[0094] Step S500: Obtain the effective crosslinking component concentration of the target active substance in the slurry to be added based on the component state parameters, and determine the second adjustment parameter based on the effective crosslinking component concentration and the preset second adjustment mapping relationship table.
[0095] Specifically, step S500, which involves obtaining the effective crosslinking component concentration based on the component state parameters, includes the following steps:
[0096] Step S510: Based on the component state parameters, the real-time absorbance of each detection area of the slurry to be added is calculated using the Lambert-Beer law.
[0097] Specifically, in step S510, for each detection area, its corresponding real-time spectral intensity parameter is acquired as the corresponding component state parameter. Simultaneously, a reference light intensity value is acquired. The reference light intensity value refers to the baseline spectral intensity collected under conditions of no slurry absorption, i.e., when the flow cell contains a blank solvent or air. For each detection area, the real-time spectral intensity parameter of that detection area is compared with the reference light intensity value, and the logarithm of the ratio is taken, followed by a negative value, to obtain the segmented real-time absorbance of the slurry in that detection area.
[0098] It should be noted that the higher the concentration of the target active substance in the slurry, the stronger the absorption of the slurry by the second target characteristic band near-infrared light, the lower the measured light intensity, and the larger the calculated absorbance value. Through the above calculation, the original light intensity parameters corresponding to each detection area are converted into corresponding absorbance values, resulting in a set of segmented real-time absorbance values equal to the number of detection areas, which serve as the data basis for subsequent peak identification. The calculation principle of the above-mentioned segmented real-time absorbance of the slurry is the same as that of the calculation principle of the real-time absorbance of the base fabric in step S240, but the underlying physical mechanism is different: the absorbance on the base fabric side reflects the absorption attenuation of residual additives on the base fabric surface, while the absorbance on the slurry side reflects the selective absorption of the target active substance molecules in the slurry by the characteristic band near-infrared light.
[0099] Step S520: Based on the preset standard spectral range of effective components, peak identification is performed on the real-time absorbance of all slurry segments, the characteristic absorption peaks are located, and the peak absorbance parameters corresponding to the characteristic absorption peaks are extracted.
[0100] Among them, the peak absorbance parameter is the integrated absorbance value obtained by integrating the peak area of the characteristic absorption peak; the effective component standard spectral range refers to the characteristic wavelength range corresponding to the stretching vibration or overtone absorption of specific chemical groups in the molecular structure of the target active substance, such as hydrogen-containing groups such as CH bonds, NH bonds or OH bonds, in the near-infrared spectrum. The effective component spectral range is determined by pre-scanning the near-infrared spectrum of the pure target active substance and analyzing its absorption peak positions.
[0101] In this embodiment, since the slurry is a multiphase mixed dispersion system containing various components such as antibacterial agents, crosslinking agents, binders, dispersants, and solvents, different components may have superimposed absorption in the same wavelength range, forming overlapping broad peaks. If quantification is performed only based on the absorbance of a single peak, it is easily affected by the absorption peaks of adjacent components or baseline drift, leading to distorted quantitative results. Therefore, step S520 performs peak identification of the real-time absorbance of the slurry in segments within the standard spectral range of the effective components.
[0102] Specifically, the peak identification is implemented as follows: For the real-time absorbance data of the slurry segments obtained in step S510, perform first or second derivative calculations within the standard spectral range of the effective components to identify the peak points in the absorption spectrum curve as the apex positions of the characteristic absorption peaks. Then, using this apex position as the center, extend to the valley position or the half-width at half-maximum boundary to determine the integration interval of the characteristic absorption peak. Integrate the absorbance values within this integration interval to obtain the peak area integral value of the characteristic absorption peak, which is output as the peak absorbance parameter. For multiple detection areas, perform the above peak identification and peak area integration processing on the segmented real-time absorbance of each detection area to obtain multiple integrated absorbance values corresponding to each detection area. In other embodiments, the average value of the multiple integrated absorbance values can also be taken as the input value for subsequent quantitative analysis to improve the representativeness of the detection results.
[0103] Step S530: Input the peak absorbance into the pre-constructed quantitative analysis model of the effective crosslinking component to obtain the corresponding concentration of the effective crosslinking component.
[0104] Among them, the quantitative analysis model of effective crosslinking components is used to establish a quantitative mapping relationship between absorbance and the concentration of effective crosslinking components; the quantitative analysis model of effective crosslinking components is a mathematical model pre-constructed using chemometric methods, and the construction method of the model is as follows:
[0105] First, several sets of slurry standard samples with known concentrations of the target active substance are prepared. The concentration gradient of the standard samples covers the possible concentration range of the slurry to be tested, such as from the initial concentration of fresh slurry to the decay concentration after a certain period of storage.
[0106] Then, under the same conditions as the actual detection, including the same flow cell optical path length, the same second target characteristic band, and the same ambient temperature, the near-infrared diffuse reflectance spectrum of each standard sample is collected, and the peak absorbance parameter of each standard sample, i.e., the integrated absorbance value, is calculated according to the method of steps S510 to S520.
[0107] Finally, using the known concentration of each standard sample as the dependent variable and the corresponding measured integrated absorbance value as the independent variable, linear regression or partial least squares regression is performed to establish a quantitative mapping equation between the integrated absorbance value and the effective crosslinking component concentration. The quantitative mapping equation can be in the form of a linear equation C=k×A+b, where C is the concentration, A is the integrated absorbance value, and k and b are regression coefficients; it can also be a multivariate nonlinear equation or a partial least squares correction model containing multiple characteristic wavelength points, depending on the complexity of the slurry system. In this step, the peak absorbance parameter extracted in step S520 is substituted into the pre-constructed quantitative mapping equation, and after model calculation, the effective crosslinking component concentration value of the target active substance in the slurry to be added can be output.
[0108] Step S600: Generate a comprehensive compensation command based on the first adjustment parameter and the second adjustment parameter.
[0109] Specifically, step S600 includes:
[0110] Step S610: Generate a first execution sub-instruction based on the first adjustment parameters.
[0111] The first adjustment parameters include the roller pressure compensation parameters of the pressure roller and the roller speed compensation parameters of the coating roller. The first execution sub-instruction is used to adjust the pressure roller and the coating roller according to the first adjustment parameters to compensate for the residual additive contamination defects on the current base fabric surface. In this step, the intelligent terminal first reads the current basic roller pressure value and basic roller speed value of the coating mechanism; then, it algebraically sums the basic roller pressure value with the roller pressure compensation parameters to obtain the actual target roller pressure value of the pressure roller; simultaneously, it algebraically sums the basic roller speed value with the roller speed compensation parameters to obtain the actual target roller speed value of the coating roller. A positive value for the roller pressure compensation parameter indicates an increase in roller pressure, and a negative value indicates a decrease in roller pressure; a positive value for the roller speed compensation parameter indicates an increase in roller speed, and a negative value indicates a decrease in roller speed.
[0112] In a typical application scenario of this embodiment, the higher the residual additive contamination level, the larger the positive increment of the roller pressure compensation parameter, meaning that a greater pressure needs to be added on top of the base roller pressure value. Conversely, the larger the negative increment of the roller speed compensation parameter, meaning that a greater speed needs to be reduced on top of the base roller speed value. Subsequently, the intelligent terminal generates a pressure roller control signal based on the actual target roller pressure value and a speed control signal for the coating roller drive motor based on the actual target roller speed value. The above control signals are packaged into a first execution sub-instruction and sent to the actuator of the coating mechanism, such as the hydraulic or pneumatic adjustment device of the pressure roller and the frequency conversion drive motor of the coating roller. This increases the linear pressure between the pressure roller and the coating roller, forcing the slurry into the fiber gaps and yarn interior under greater mechanical pressure, thereby increasing the physical interlocking degree and interfacial contact area between the slurry and the fiber. At the same time, by reducing the roller speed of the coating roller, the spreading and wetting time of the slurry on the base fabric surface is extended, allowing the slurry to achieve more sufficient wetting and penetration before entering the subsequent drying and setting process. The two work together to compensate for the decrease in interfacial bonding strength caused by the residual additives covering the base fabric surface.
[0113] Step S620: Generate a second execution sub-instruction based on the second adjustment parameters.
[0114] The second execution sub-instruction is used to adjust the feed pump according to the second adjustment parameter to compensate for the crosslinking strength defects of the slurry to be applied; the second adjustment parameter includes the slurry supply flow rate per unit of base fabric, and the target slurry mass or volume to be applied per square meter of base fabric in the coating process.
[0115] In step S620, the intelligent terminal calculates the target output flow rate of the feed pump based on the target slurry supply flow rate and the current roller speed of the coating roller (or the base fabric running speed). The corresponding conversion relationship is: target output flow rate of the feed pump = target slurry supply flow rate × current base fabric width × current base fabric running speed. This conversion relationship ensures that the total amount of slurry output by the feed pump per unit time meets the target supply amount per unit area of base fabric at the current running speed. Subsequently, the intelligent terminal generates a feed pump control signal based on the target output flow rate of the feed pump, such as adjusting the operating frequency of the feed pump to change its output speed, or adjusting the opening of the regulating valve of the coating head feed pipeline, etc., and packages it into a second execution sub-instruction and sends it to the actuator of the feed pump to adjust the supply flow rate of the slurry to be added. Since the concentration of effective crosslinking components in the slurry has decreased, by increasing the slurry supply amount per unit area of base fabric, even under the condition of decreased effective component concentration in the slurry, the total amount of effective crosslinking components actually deposited on the base fabric per unit area can still be maintained near the target level, thereby compensating for the defects in the crosslinking strength of the slurry.
[0116] Step S630: The first execution sub-instruction and the second execution sub-instruction are time-coordinated to generate a comprehensive compensation instruction.
[0117] Among them, the comprehensive compensation instruction is a composite instruction set that includes a first execution sub-instruction and a second execution sub-instruction.
[0118] Since the first execution sub-instruction targets the pressure roller and coating roller, acting on the coating station where the base fabric contacts the slurry, while the second execution sub-instruction targets the feed pump, acting on the slurry delivery pipeline, their execution paths and response times differ. If the two sub-instructions are simply sent independently without timing coordination, situations may arise where the slurry supply flow rate has been adjusted to the correct level but the roller pressure has not yet responded, or vice versa, leading to fluctuations in coating quality during the transition phase.
[0119] To address this issue, this step introduces a timing coordination mechanism, which specifically includes: obtaining the response delay time of the feed pump after receiving the second execution sub-instruction, i.e., the response time required from the issuance of the instruction to the actual output flow of the feed pump stabilizing to the target value, and the response delay time of the pressure roller and coating roller after receiving the first execution sub-instruction; comparing the order of their response delay times and generating a time offset to ensure that the two execution sub-instructions take effect synchronously on the time axis.
[0120] For example, if the response delay time of the feed pump is long, the smart terminal first sends the second execution sub-instruction, and then sends the first execution sub-instruction after the corresponding response delay time difference has elapsed, so that the two are synchronized at the actual execution level; and vice versa.
[0121] Through the aforementioned timing coordination, a composite instruction set containing the first and second execution sub-instructions is generated. This set is then output to the corresponding actuator of the coating mechanism as a comprehensive compensation instruction, enabling the pressure roller adjustment, coating roller adjustment, and feed pump adjustment to take effect simultaneously. This achieves coordinated compensation of interface strength and body strength at the coating station.
[0122] Step S700: Perform the slurry impregnation and coating process on the current base fabric according to the comprehensive compensation instruction.
[0123] The first execution sub-instruction is sent to the roller pressure adjustment device of the pressure roller and the drive motor of the coating roller, and the second execution sub-instruction is sent to the drive motor or frequency converter of the feed pump. After receiving the corresponding sub-instruction, each actuator synchronously performs the adjustment action according to the target parameters carried by the sub-instruction.
[0124] The roller pressure adjustment device adjusts the linear pressure between the pressure roller and the coating roller according to the actual value of the target roller pressure in the first execution sub-instruction, so that the pressure roller presses against the surface of the current base fabric with the adjusted pressure, thereby increasing the interfacial contact strength and physical interlocking degree between the slurry and the fiber to an appropriate extent.
[0125] The drive motor of the coating roller adjusts the rotation speed of the coating roller according to the actual value of the target roller speed in the first execution sub-instruction, so as to control the running speed of the current base fabric through the coating station and extend the spreading and wetting time of the slurry on the surface of the base fabric to an appropriate extent.
[0126] The drive motor or frequency converter of the feed pump adjusts the operating frequency or speed of the feed pump according to the target output flow rate in the second execution sub-instruction, so that the feed pump delivers the slurry to be applied to the coating head at the adjusted output flow rate, thereby controlling the slurry supply per unit base fabric.
[0127] With the coating mechanism continuously operating, the current base fabric sequentially passes through the coating station. Under the synergistic action of the pressure roller and the coating roller, the coating head applies the slurry to the surface of the current base fabric at an adjusted supply flow rate, ensuring that the slurry uniformly wets and adheres to the base fabric surface, forming a wet coating. This wet coating then enters the downstream drying and setting unit, where it undergoes pre-drying and cross-linking curing to form a wash-resistant, long-lasting antibacterial coating. This embodiment, through the aforementioned comprehensive compensation instructions, achieves simultaneous compensation for defects in residual additive contamination on the base fabric surface and defects in the attenuation of effective cross-linking components in the slurry, effectively ensuring batch consistency in coating quality.
[0128] The following describes the automated coating control device provided by the present invention. The automated coating control device described below can be referred to in correspondence with the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric described above.
[0129] like Figure 8As shown, in one embodiment, an automated coating control device includes a parameter acquisition module, a parameter parsing module, an adjustment parameter determination module, an instruction generation module, and an instruction execution module.
[0130] The parameter acquisition module includes an interface state acquisition unit and a component state acquisition unit. The interface state acquisition unit is used to acquire the interface state parameters of the current base fabric in real time before performing the slurry impregnation and coating process on the current base fabric. The interface state parameters are used to reflect the degree of residual additive contamination on the surface of the current base fabric. The interface state parameters are obtained by applying a preset first target characteristic band near-infrared diffuse reflectance detection to each detection segment of the current base fabric. The interface state parameters include the real-time spectral intensity parameters corresponding to each detection segment of the current base fabric.
[0131] The component state acquisition unit is used to acquire the component state parameters of the slurry to be added in real time. The component state parameters are used to reflect the real-time effective content level of the target active substance in the slurry to be added. The component state parameters are obtained by applying a preset second target characteristic band near-infrared diffuse reflectance detection to each detection area of the slurry to be added. The component state parameters include the real-time spectral intensity parameters corresponding to each detection area of the slurry to be added.
[0132] The parameter parsing module is used to parse the interface state parameters to determine the residual additive contamination level on the current base fabric surface, and to obtain the effective crosslinking component concentration of the target active substance in the slurry to be added based on the component state parameters.
[0133] Specifically, the parameter parsing module includes a data filtering unit, a noise baseline calculation unit, a limit defect filtering unit, an absorbance calculation unit, a peak identification unit, and a quantitative analysis unit, among which:
[0134] The data filtering unit is used to filter out normal light intensity parameters within the standard spectral range of the base fabric and abnormal light intensity parameters outside the standard spectral range of the base fabric from the interface status parameters based on the preset standard spectral range of the base fabric.
[0135] The noise baseline calculation unit is used to calculate the average value of all normal light intensity parameters and use the average value as the adaptive noise baseline corresponding to the current base fabric.
[0136] The extreme defect screening unit is used to identify the detection segment corresponding to the abnormal light intensity parameter as the suspected defect segment. Based on the continuous distribution of the suspected defect segment, the extreme defect light intensity parameter is obtained from the abnormal light intensity parameter.
[0137] The absorbance calculation unit is used to calculate the real-time absorbance of the current base fabric based on the light intensity parameters of the limit defect and the adaptive noise baseline, using the Lambert-Beer law.
[0138] The quantitative analysis unit is used to determine the residual additive contamination level on the current base fabric surface based on the real-time absorbance of the base fabric and the preset additive contamination classification relationship.
[0139] The absorbance calculation unit is also used to calculate the real-time absorbance of each detection area of the slurry to be added based on the component state parameters and the Lambert-Beer law.
[0140] The peak identification unit is used to identify the peaks of the real-time absorbance of all slurry segments based on the preset standard spectral range of effective components, locate the characteristic absorption peaks and extract the peak absorbance parameters corresponding to the characteristic absorption peaks. The peak absorbance parameters are the integrated absorbance values obtained by integrating the peak area of the characteristic absorption peaks.
[0141] The quantitative analysis unit is also used to input the peak absorbance parameter into the pre-constructed quantitative analysis model of the effective cross-linking component to obtain the corresponding concentration of the effective cross-linking component. The quantitative analysis model of the effective cross-linking component is used to establish a quantitative mapping relationship between absorbance and concentration of the effective cross-linking component.
[0142] The adjustment parameter determination module is used to determine the first adjustment parameter based on the residual additive contamination level and a preset first adjustment mapping table. The first adjustment parameter is used to adjust the coating wetting and bonding strength of the current base fabric. The first adjustment mapping table reflects the correspondence between the residual additive content level and the first adjustment parameter. The adjustment parameter determination module is also used to obtain the effective crosslinking component concentration of the target active substance in the slurry to be added based on the component state parameters, and to determine the second adjustment parameter based on the effective crosslinking component concentration and a preset second adjustment mapping table. The second adjustment parameter is used to adjust the supply flow rate of the slurry to be added when coating the current base fabric. The second adjustment mapping table reflects the correspondence between the effective crosslinking component concentration and the second adjustment parameter.
[0143] The instruction generation module is used to generate a comprehensive compensation instruction based on the first adjustment parameter and the second adjustment parameter. The comprehensive compensation instruction is used to compensate for the defects in the base fabric additives and the crosslinking strength of the slurry through the first adjustment parameter and the second adjustment parameter.
[0144] The instruction execution module is used to perform the slurry impregnation and coating process on the current base fabric according to the comprehensive compensation instruction.
[0145] Figure 9 This example illustrates a schematic diagram of the physical structure of an electronic device, which can be a smart terminal. Its internal structure diagram can be as follows: Figure 9As shown, the electronic device includes a processor, internal memory, and a network interface connected via a system bus. The processor provides computing and control capabilities. The memory includes a non-volatile storage medium and internal memory. The non-volatile storage medium stores the operating system and computer programs. The internal memory provides an environment for the operation of the operating system and computer programs in the non-volatile storage medium. The network interface is used to communicate with external terminals via a network connection. When the computer program is executed by the processor, it implements the aforementioned automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric.
[0146] Those skilled in the art will understand that Figure 9 The structure shown is merely a block diagram of a portion of the structure related to the present invention and does not constitute a limitation on the electronic device to which the present invention is applied. A specific electronic device may include more or fewer components than those shown in the figure, or combine certain components, or have different component arrangements.
[0147] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are specific and detailed, they should not be construed as limiting the scope of the present invention. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these modifications and improvements all fall within the scope of protection of the present invention. Therefore, the scope of protection of this patent should be determined by the appended claims.
Claims
1. A method for automated coating control for the preparation of a water wash resistant long-lasting antimicrobial bed sheet fabric, characterized by, The method includes: Before performing the slurry impregnation and coating process on the current base fabric, the interface state parameters of the current base fabric are collected in real time. The residual additive contamination level on the current base fabric surface is determined by analyzing the interface state parameters; The first adjustment parameter is determined based on the residual additive contamination level and the preset first adjustment mapping table. The first adjustment parameter is used to adjust the coating, wetting and bonding strength of the current base fabric. The first adjustment mapping table is used to reflect the correspondence between the residual additive content level and the first adjustment parameter. Real-time acquisition of component state parameters of the slurry to be added; The effective crosslinking component concentration of the target active substance in the slurry to be added is obtained according to the component state parameters, and the second adjustment parameter is determined according to the effective crosslinking component concentration and the preset second adjustment mapping relationship table. The second adjustment parameter is used to adjust the supply flow rate of the slurry to be added when coating the current base fabric. The second adjustment mapping relationship table is used to reflect the correspondence between the effective crosslinking component concentration and the second adjustment parameter. A comprehensive compensation instruction is generated based on the first adjustment parameter and the second adjustment parameter. The comprehensive compensation instruction is used to compensate for defects in the base fabric additives and defects in the crosslinking strength of the slurry through the first adjustment parameter and the second adjustment parameter. The slurry impregnation and coating process for the current base fabric is executed according to the comprehensive compensation instruction.
2. The automated coating control method for preparing a water-wash resistant long-acting antibacterial bed sheet fabric according to claim 1, characterized by, The current base fabric is divided into several detection sections along its running direction; the interface state parameters are used to reflect the degree of residual additive contamination on the surface of the current base fabric. The interface state parameters are obtained by applying a preset first target characteristic band near-infrared diffuse reflectance detection to each detection section of the current base fabric. The interface state parameters include the real-time spectral intensity parameters corresponding to each detection section of the current base fabric.
3. The automated coating control method for preparing a water-wash resistant long-acting antibacterial bed sheet fabric according to claim 2, characterized in that, The process of analyzing the interface state parameters to determine the residual additive contamination level on the current base fabric surface specifically includes: Based on the preset standard spectral range of the base fabric, normal light intensity parameters within the standard spectral range of the base fabric and abnormal light intensity parameters exceeding the standard spectral range of the base fabric are obtained from the interface state parameters. Calculate the average value of all the normal light intensity parameters and use the average value as the adaptive noise floor baseline corresponding to the current base fabric; The detection segment corresponding to the abnormal light intensity parameter is taken as the suspected defect segment. Based on the continuous distribution of the suspected defect segment, the ultimate defect light intensity parameter is obtained by screening from the abnormal light intensity parameters. Based on the light intensity parameters of the extreme defects and the adaptive noise baseline, the real-time absorbance of the current base fabric is calculated using the Lambert-Beer law. Based on the real-time absorbance of the base fabric and the preset auxiliary contamination classification relationship, the residual auxiliary contamination level corresponding to the current base fabric surface is determined.
4. The automated coating control method for preparing a water-wash resistant long-acting antibacterial bed sheet fabric according to claim 3, characterized by, The step of selecting the ultimate defect light intensity parameters from the abnormal light intensity parameters based on the continuous distribution of the suspected defect segments specifically includes: Obtain the distribution coordinates of all the suspected defect segments, and determine whether each suspected defect segment has an adjacent relationship with any other suspected defect segment based on the distribution coordinates; If the judgment result is yes, the suspected defective segment is taken as the actual defective segment; Among all the abnormal light intensity parameters corresponding to the real defect segments, the spectral intensity parameter with the smallest value is selected as the limit defect light intensity parameter.
5. The automated coating control method for preparing a water-wash resistant long-acting antibacterial bed sheet fabric according to claim 1, characterized in that, The slurry to be applied is divided into several detection areas; the component state parameters are used to reflect the real-time effective content level of the target active material in the slurry to be applied that can covalently anchor with the current base fabric. The component state parameters are obtained by applying a preset second target characteristic band near-infrared diffuse reflectance detection to each detection area of the slurry to be applied. The component state parameters include the real-time spectral intensity parameters corresponding to each detection area of the slurry to be applied.
6. The automated coating control method for preparing a water-wash resistant long-acting antibacterial bed sheet fabric according to claim 5, characterized by, The specific steps of obtaining the effective crosslinking component concentration based on the component state parameters include: Based on the component state parameters, the real-time absorbance of each detection area of the slurry to be applied is calculated using the Lambert-Beer law. Based on the preset standard spectral range of effective components, the peaks of the real-time absorbance of all the slurry segments are identified, the characteristic absorption peaks are located, and the peak absorbance parameters corresponding to the characteristic absorption peaks are extracted. The peak absorbance parameters are the integrated absorbance values obtained by integrating the peak area of the characteristic absorption peaks. The peak absorbance is input into a pre-constructed quantitative analysis model for effective crosslinking components to obtain the corresponding concentration of effective crosslinking components. The quantitative analysis model for effective crosslinking components is used to establish a quantitative mapping relationship between absorbance and concentration of effective crosslinking components.
7. The automated coating control method for preparing a water-wash resistant long-acting antibacterial bed sheet fabric according to claim 6, characterized by, The step of generating a comprehensive compensation instruction based on the first adjustment parameter and the second adjustment parameter specifically includes: The first execution sub-instruction is generated based on the first adjustment parameters. The first adjustment parameters include the roller pressure compensation parameters of the pressure roller and the roller speed compensation parameters of the coating roller. The first execution sub-instruction is used to adjust the pressure roller and the coating roller according to the first adjustment parameters to compensate for the residual additive contamination defects on the current base fabric surface. A second execution sub-instruction is generated based on the second adjustment parameter, the second adjustment parameter including the slurry supply flow rate per unit base fabric, and the second execution sub-instruction is used to adjust the feed pump according to the second adjustment parameter to compensate for the crosslinking strength defects of the slurry to be added; The first execution sub-instruction and the second execution sub-instruction are time-coordinated to generate a comprehensive compensation instruction, which is a composite instruction set containing the first execution sub-instruction and the second execution sub-instruction.
8. A coating automation control device characterized by comprising: The apparatus for implementing the method according to any one of claims 1 to 7, the apparatus comprising: The parameter acquisition module is used to collect the interface state parameters of the current base fabric and the component state parameters of the slurry to be applied in real time before performing the slurry impregnation and coating process on the current base fabric. The parameter parsing module is used to parse the interface state parameters to determine the residual additive contamination level on the current base fabric surface, and to obtain the effective crosslinking component concentration of the target active substance in the slurry to be added based on the component state parameters. The adjustment parameter determination module is used to determine a first adjustment parameter based on the residual additive pollution level and a preset first adjustment mapping table, and to obtain the effective crosslinking component concentration of the target active substance in the slurry to be added based on the component state parameters, and to determine a second adjustment parameter based on the effective crosslinking component concentration and a preset second adjustment mapping table. The instruction generation module is used to generate a comprehensive compensation instruction based on the first adjustment parameter and the second adjustment parameter; The instruction execution module is used to execute the slurry impregnation and coating process on the current base fabric according to the comprehensive compensation instruction. 9.An electronic device comprising a memory and a processor, the memory storing a computer program, wherein, When the processor executes the computer program, it implements the steps of the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric as described in any one of claims 1 to 7.
10. A computer storage medium storing a computer program, characterized in that, When the computer program is executed by the processor, it implements the steps of the automated coating control method for preparing water-resistant, long-lasting antibacterial bed sheet fabric as described in any one of claims 1 to 7.