Early warning method and system for battery module welding process

By constructing a multidimensional deviation value sequence for the battery module welding process and performing linear fitting, the problems of reference drift and insufficient signal fusion in existing welding early warning methods are solved, realizing real-time quality monitoring of the battery module welding process and improving the reliability of welding quality and the timeliness of early warning.

CN123158294APending Publication Date: 2026-11-24HANGZHOU LIDE AUTOMATION EQUIP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611334709.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-31
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing welding early warning methods rely on static process packages, which leads to batch-to-batch baseline drift. Multi-dimensional sensor signals cannot be fused for judgment, and there is a time lag in obtaining post-weld inspection results, making it impossible to trigger early warnings in real time, resulting in high false alarm and false negative rates.

Method used

By collecting current signals, pressure signals, and ultrasonic frequency signals during the battery module welding process, a candidate benchmark set is generated. Rolling variance calculation is performed to construct a batch benchmark package. Welding early warning signals are generated through linear fitting of multidimensional deviation values, thereby enabling the monitoring of the trend changes in the deviation value sequence.

Benefits of technology

It improves the reliability of adaptive construction of batch reference packages during battery module welding, and can identify welding quality anomalies in real time under multivariable dynamic disturbance environment, reducing false alarm rate and false alarm rate, and improving the timeliness of welding quality monitoring.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123158294A_ABST
    Figure CN123158294A_ABST
Patent Text Reader

Abstract

This application relates to the field of welding inspection technology and discloses an early warning method and system for the welding process of battery modules. The method includes: acquiring multi-source sensor signals during the battery module welding process, generating a candidate benchmark set through wide-boundary filtering of resistance values; calculating the rolling variance of the signals at each weld point in the candidate benchmark set, and constructing a batch benchmark package using the mean values ​​of each dimension and the boundary values ​​of the steady-state interval when the variance values ​​of M consecutive weld points all fall within a preset steady-state interval; subtracting the signals of subsequent weld points from the batch benchmark package dimension by dimension to obtain a deviation value sequence; performing linear fitting on K consecutive deviation values ​​in the deviation value sequence, and generating a welding early warning signal based on the fitting slope exceeding a slope threshold. This application improves the reliability of adaptive construction of batch benchmark packages and the timeliness of early warning of systemic degradation trends during the battery module welding process under multivariate dynamic disturbances.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of welding inspection technology, and in particular to an early warning method and system for the welding process of battery modules. Background Technology

[0002] Laser welding of battery modules is a critical process in the manufacturing of power batteries, and the welding quality directly affects the current carrying capacity, connection strength, and service life of the battery module. Existing technologies for quality monitoring during the welding process mainly fall into two categories: one is a process signal monitoring scheme based on plasma optical signals, visible light, and infrared thermal radiation. This scheme uses photodiode sensors to collect light radiation signals during the welding process, compares the real-time signals with pre-calibrated offline reference curves, and judges the weld penetration and abnormal states such as incomplete welds and spatter based on waveform deviations. The other is a post-weld inspection scheme based on OCT penetration measurement, charge-discharge voltage relationship curves, and infrared thermal imaging. This scheme determines whether there are quality defects such as incomplete welds and over-welds by measuring the weld morphology or electrical performance parameters after welding. The above solutions have achieved monitoring of welding quality to a certain extent, but they all rely on offline manually calibrated static reference process packages as comparison benchmarks. These static benchmarks cannot detect dynamic disturbance factors such as batch-to-batch material characteristic differences, equipment preheating fluctuations, gradual contamination of protective lenses, and changes in environmental temperature and humidity. This results in a systematic deviation between the warning judgment boundary and the actual working conditions in the actual multivariate production environment, making it difficult to effectively control both the false alarm rate and the missed alarm rate.

[0003] However, the existing technologies have the following shortcomings: the static reference process package on which the existing early warning schemes rely cannot be automatically updated when batch switching, equipment status changes, or environmental conditions fluctuate, resulting in a systematic drift between the early warning judgment benchmark and the actual working conditions of the current batch, which in turn leads to a large number of false alarms or missed alarms; when comparing plasma signals, optical radiation signals, and acoustic emission signals, the existing multi-sensor signal monitoring schemes only judge the absolute value exceeding the threshold for a single parameter, and cannot perform fusion calculations on the dimensions of multiple sensor signals, resulting in insufficient ability to distinguish between the two types of defects: cold solder joints and over-soldering; existing post-weld inspection schemes, such as the charge-discharge voltage relationship curve method and infrared thermal imaging method, have a significant time lag in obtaining the detection results, and cannot trigger early warnings in real time during the welding process. Defective products are only discovered after subsequent processes have been completed, resulting in significant quality losses. Summary of the Invention

[0004] This application provides an early warning method and system for the battery module welding process, which solves the problems of batch-to-batch reference drift and inability to fuse multi-dimensional sensor signals in existing welding early warning methods due to reliance on static process packages. It improves the reliability of adaptive construction of batch reference packages under multi-variable dynamic disturbances during battery module welding and the timeliness of early warning of systemic degradation trends.

[0005] In a first aspect, this application provides an early warning method for the battery module welding process, the early warning method for the battery module welding process comprising: Step S1: Collect current signals, pressure signals and ultrasonic frequency signals during the battery module welding process, and generate a candidate reference set by filtering the first weld joint of the batch through a wide boundary of resistance value; Step S2: Perform rolling variance calculation on the current signal, pressure signal, and ultrasonic frequency signal of each solder joint in the candidate reference set according to the order of the solder joints to obtain the variance sequence of each sensor dimension. When the variance values ​​of each dimension of M consecutive solder joints fall into the preset steady-state interval of the corresponding dimension, use the mean value of the current signal, the mean value of the pressure signal, and the mean value of the ultrasonic frequency signal of the M consecutive solder joints as the reference center value of the corresponding sensor dimension, and construct a batch reference package with the reference center value of each dimension and the boundary value of the steady-state interval of the corresponding dimension. Step S3: Subtract the current signal, pressure signal and ultrasonic frequency signal of each subsequent solder joint from the reference center value of the corresponding dimension in the batch reference package one dimension at a time to obtain the multidimensional deviation value of each solder joint. Arrange the multidimensional deviation values ​​of each solder joint in the order of the solder joints to obtain the deviation value sequence. Step S4: Perform linear fitting on K consecutive deviation values ​​in the deviation value sequence, and use the fitting slope exceeding the slope threshold as a criterion to generate a welding early warning signal.

[0006] Secondly, this application provides an early warning system for the battery module welding process, the early warning system for the battery module welding process comprising: The screening module is used to collect current signals, pressure signals and ultrasonic frequency signals during the battery module welding process. It filters the first weld joint of the batch through a wide boundary of resistance value to generate a candidate reference set. The calculation module is used to perform rolling variance calculation on the current signal, pressure signal and ultrasonic frequency signal of each weld point in the candidate reference set according to the order of the weld points to obtain the variance sequence of each sensor dimension. When the variance values ​​of each dimension of M consecutive weld points all fall into the preset steady-state interval of the corresponding dimension, the mean value of the current signal, the mean value of the pressure signal and the mean value of the ultrasonic frequency signal of the M consecutive weld points are used as the reference center value of the corresponding sensor dimension, and the batch reference package is constructed with the reference center value of each dimension and the boundary value of the steady-state interval of the corresponding dimension. The arrangement module is used to subtract the current signal, pressure signal and ultrasonic frequency signal of each subsequent solder joint from the reference center value of the corresponding dimension in the batch reference package one dimension at a time to obtain the multidimensional deviation value of each solder joint. The multidimensional deviation values ​​of each solder joint are arranged in the order of the solder joints to obtain the deviation value sequence. The fitting module is used to perform linear fitting on K consecutive deviation values ​​in the deviation value sequence, and uses the fitting slope exceeding the slope threshold as a criterion to generate a welding early warning signal.

[0007] Thirdly, a warning device for the battery module welding process is provided, comprising: a memory and at least one processor, wherein the memory stores instructions; the at least one processor invokes the instructions in the memory to cause the warning device for the battery module welding process to execute the aforementioned warning method for the battery module welding process.

[0008] Fourthly, a computer-readable storage medium is provided, wherein instructions are stored therein, which, when executed on a computer, cause the computer to perform the aforementioned early warning method for the battery module welding process.

[0009] The technical solution provided in this application generates a candidate reference set by filtering the first weld joints of a batch using a wide boundary of resistance values. Then, the current signal, pressure signal, and ultrasonic frequency signal of each weld joint in the candidate reference set are calculated using rolling variance in the order of the weld joints. When the variance values ​​of each dimension of M consecutive weld joints simultaneously fall within the preset steady-state range of the corresponding dimension, the average three-dimensional signal of these M weld joints is used to construct a batch reference package. This fundamentally solves the problem in existing technologies where static process packages cannot detect differences in material properties between batches, fluctuations in equipment preheating status, and changes in environmental conditions. This allows the early warning judgment reference to automatically include the actual operating condition information of the current batch, eliminating the systematic deviation between the static reference and the dynamic production site. The introduction of dynamic variance calculation and multidimensional convergence criteria ensures that the activation condition of the batch reference package does not depend on the occasional stability of any single-dimensional signal. Instead, it requires the variances of the current, pressure, and ultrasonic frequency signals to converge synchronously to their respective steady-state ranges, thereby guaranteeing the reliability of the batch reference package itself and avoiding false activation during the signal instability period of the equipment preheating stage. On this basis, the three-dimensional sensor signals of each subsequent welding point are subtracted from the reference center value of the corresponding dimension in the batch reference package dimension by dimension and then fused by normalization and weighting to obtain a single multidimensional deviation value that can comprehensively reflect the degree of deviation of multidimensional signals. This overcomes the shortcomings of the existing scheme that only judges the absolute value of a single parameter exceeding the threshold and cannot directly fuse signals of different dimensions.

[0010] Based on the multidimensional deviation value sequence, the system linearly fits K consecutive deviation values ​​and extracts the fitting slope. Then, it uses the fact that the fitting slope of P consecutive weld points exceeds the slope threshold as the criterion for generating welding early warning signals. This upgrades the early warning judgment from isolated judgment of single-point deviations to continuous monitoring of the trend changes of the deviation value sequence. This enables the system to identify the monotonically increasing trend of deviation values ​​and trigger early warnings in deterioration scenarios such as gradual contamination of equipment lenses and systematic shifts in raw material batches, before the concentrated outbreak of batch defects, rather than waiting for a single-point deviation to exceed the threshold before responding. The linear fitting slope, as an algorithm feature, corresponds to the rate of change of deviation values ​​with the sequence of weld points. It can directly characterize the drift speed of welding conditions. This algorithm feature is highly consistent with the physical mechanism of gradual equipment deterioration during battery module welding, so that the algorithm output results form a clear correspondence with the actual evolution of process anomalies, rather than relying solely on black-box judgment results obtained from data fitting. Attached Figure Description

[0011] To more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0012] Figure 1 This is a schematic diagram of one embodiment of the early warning method for the battery module welding process in this application. Figure 2 This is a schematic diagram illustrating the generation of a candidate reference set through wide-boundary filtering of resistance values ​​in an embodiment of this application. Figure 3 This is a schematic diagram of deviation value sequence trend monitoring and welding early warning signal generation in an embodiment of this application. Detailed Implementation

[0013] This application provides an early warning method and system for the welding process of battery modules. The terms "first," "second," "third," "fourth," etc. (if present) in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments described herein can be implemented in a sequence other than that illustrated or described herein. Furthermore, the terms "comprising" or "having" and any variations thereof are intended to cover a non-exclusive inclusion; for example, a process, method, system, product, or apparatus that comprises a series of steps or units is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to such processes, methods, products, or apparatus.

[0014] For ease of understanding, the specific process of the embodiments of this application is described below. Please refer to [link / reference]. Figure 1 One embodiment of the early warning method for the battery module welding process in this application includes: Step S1: Collect current signals, pressure signals and ultrasonic frequency signals during the battery module welding process, and generate a candidate reference set by filtering the first weld joint of the batch through a wide boundary of resistance value; Specifically, the candidate benchmark set refers to the set of valid solder joints retained after screening the first solder joints of the batch through a wide resistance value boundary. The wide resistance value boundary range is determined by relaxing the upper and lower limits of the resistance value of good solder joints in the factory process specification by a certain percentage. The relaxation percentage is usually set to 20% to 30% of the standard range width. The purpose is to exclude obviously abnormal solder joints while allowing for equipment preheating fluctuations in the initial stage of the batch. The signals from the three sensors must be collected synchronously to ensure that the signals of each dimension are strictly aligned on the time axis, so as to avoid distortion of subsequent variance calculation due to misalignment of the acquisition timing.

[0015] Step S2: Perform rolling variance calculation on the current signal, pressure signal and ultrasonic frequency signal of each weld point in the candidate reference set according to the order of the weld points to obtain the variance sequence of each sensor dimension. When the variance values ​​of each dimension of M consecutive weld points fall into the preset steady-state interval of the corresponding dimension, use the mean of the current signal, the mean of the pressure signal and the mean of the ultrasonic frequency signal of the M consecutive weld points as the reference center value of the corresponding sensor dimension, and construct a batch reference package with the reference center value of each dimension and the boundary value of the steady-state interval of the corresponding dimension. Specifically, the batch reference package is the core self-created data structure of this solution, containing three reference center values: current reference center value, pressure reference center value, and ultrasonic frequency reference center value, as well as the upper and lower bounds of the steady-state intervals for each dimension, totaling nine values. The recommended window length W for rolling variance calculation is 5 to 10 solder joints. A value that is too small will make the variance sensitive to noise, while a value that is too large will result in delayed convergence judgment. The variance values ​​of each dimension for M consecutive solder joints must simultaneously fall within the preset steady-state interval for the corresponding dimension. M is recommended to be no less than 3 to exclude false activations caused by occasional stability. The boundary values ​​of the steady-state intervals are determined by the upper quartile of the sensor signal variance distribution during the stable operation phase of the equipment in offline experiments, and this serves as the upper bound of the steady-state interval for each dimension, with the lower bound set to zero.

[0016] Step S3: Subtract the current signal, pressure signal and ultrasonic frequency signal of each subsequent solder joint from the reference center value of the corresponding dimension in the batch reference package one dimension at a time to obtain the multidimensional deviation value of each solder joint. Arrange the multidimensional deviation values ​​of each solder joint in the order of the solder joints to obtain the deviation value sequence. Specifically, the multidimensional deviation value is a single scalar value obtained by subtracting the three sensor signals of each solder joint from the corresponding reference center value in the batch reference package dimension by dimension, followed by normalization and weighted summation. Normalization is performed by using the boundary value of the steady-state interval of the corresponding dimension as the divisor to eliminate the interference of the difference in the dimensions of the three signals on the weighted result. The preset weights of each dimension are set according to the sensitivity of each sensor signal to defects such as cold solder joints and over-soldering. The weight of the current signal is usually higher than that of the pressure signal and the ultrasonic frequency signal, and the sum of the weights of the three is 1. The deviation value sequence is arranged in the order of the solder joints to form a one-dimensional time series array for subsequent linear fitting.

[0017] Step S4: Perform linear fitting on K consecutive deviation values ​​in the deviation value sequence, and use the fitting slope exceeding the slope threshold as the criterion to generate a welding early warning signal.

[0018] Specifically, the linear fitting of K consecutive deviation values ​​uses the least squares method, with the weld point sequence number as the independent variable and the deviation value as the dependent variable. The slope of the fitted straight line is the fitting slope. K is recommended to be between 5 and 15 focal points. If the value is too small, the slope will be sensitive to single-point disturbances; if the value is too large, the trend response will be sluggish. The slope threshold is determined based on the lower quartile of the slope statistical distribution of the monotonically increasing segment of deviation values ​​caused by equipment deterioration in historical batches. A welding warning signal is generated when the fitting slope of P consecutive focal points exceeds the slope threshold. P is recommended to be no less than 3 to exclude false alarms caused by brief disturbances. The specific value of P is determined by a combination of production line cycle time and acceptable warning response delay.

[0019] In one specific embodiment, step S1 includes: The welding process of each weld point in the first segment of the batch is synchronously collected using current sensors, pressure sensors, and ultrasonic sensors to obtain current signal sampling sequences, pressure signal sampling sequences, and ultrasonic frequency signal sampling sequences for each weld point. The welding resistance values ​​corresponding to the current signal sampling sequence, pressure signal sampling sequence and ultrasonic frequency signal sampling sequence of each weld point are compared with the upper and lower boundaries of the preset resistance value wide boundary interval. Weld points whose welding resistance values ​​fall within the preset resistance value wide boundary interval are marked as valid weld points, and weld points whose welding resistance values ​​do not fall within the preset resistance value wide boundary interval are removed. The current signal sampling sequence, pressure signal sampling sequence, and ultrasonic frequency signal sampling sequence of each effective solder joint are arranged in the order of the solder joints to generate a candidate reference set.

[0020] Specifically, current sensors, pressure sensors, and ultrasonic sensors synchronously acquire data on the welding process of each weld point in the first stage of the batch at the same sampling frequency. It is recommended that the sampling frequency be set to no less than 10kHz to ensure that a sufficient number of signal sample points are acquired within the duration of a single weld point. The start and end times of the acquisition by the three sensors are synchronized based on the rising edge of the welding trigger signal, ensuring that the current signal sampling sequence, pressure signal sampling sequence, and ultrasonic frequency signal sampling sequence of each weld point are strictly aligned on the time axis. The welding resistance value of each weld point is calculated based on Ohm's law using the corresponding current signal sampling sequence and pressure signal sampling sequence. The upper and lower bounds of the preset resistance value wide boundary range are determined by extending the upper and lower limits of the standard range for good weld point resistance values ​​in the factory process specification outwards by 25% of the standard range width. The 25% extension ratio is designed to accommodate normal signal fluctuations during the preheating stage of the equipment in the first stage of the batch while excluding abnormal weld points with resistance values ​​significantly deviating from the normal range.

[0021] Weld joints whose welding resistance values ​​fall within the preset resistance value wide boundary range are marked as valid weld joints. Weld joints whose welding resistance values ​​do not fall within the preset resistance value wide boundary range are removed from the sequence. The removal operation only applies to the current weld joint and does not affect the marking results of weld joints before and after it. After arranging the current signal sampling sequence, pressure signal sampling sequence, and ultrasonic frequency signal sampling sequence of each valid weld joint in the order of weld joints, a candidate reference set is generated. The three signal sampling sequences of each weld joint in the candidate reference set maintain a one-to-one correspondence. The weld joint sequence number is strictly continuous in the candidate reference set to ensure the consistency of the weld joint sequence within the sliding window in the subsequent rolling variance calculation.

[0022] Figure 2 This is a schematic diagram of the wide boundary screening of resistance values ​​to generate a candidate reference set in an embodiment of this application. In the figure, the horizontal axis is the sequential number of the solder joints, and the vertical axis is the welding resistance value. The preset wide boundary interval of resistance values ​​is represented by the filled area enclosed by the upper and lower boundaries of the wide boundary. Solder joints falling into this interval are marked with a solid circle as valid solder joints and included in the candidate reference set. Solder joints not falling into this interval are marked with a cross as rejected solder joints and excluded from the candidate reference set. As can be seen from the figure, the welding resistance values ​​of valid solder joints are concentrated inside the wide boundary interval, and the welding resistance values ​​of rejected solder joints are all higher than the upper boundary of the wide boundary, forming a clear distinction from the valid solder joints.

[0023] In one specific embodiment, step S2 involves calculating the rolling variance of the current signal, pressure signal, and ultrasonic frequency signal of each solder joint in the candidate reference set according to the solder joint order, including: Taking the current solder joint as the endpoint, take a sliding window with a window length of W forward. Calculate the mean value of the current signal in the window for each solder joint within the sliding window. Sum the squares of the differences between the current signals of each solder joint within the sliding window and the mean value of the current signals in the window, and then divide by the window length W to obtain the variance value of the current at the current solder joint. Using the same sliding window length W, the pressure signal and ultrasonic frequency signal of each weld point within the sliding window are calculated using the same process as the current variance value to obtain the pressure variance value and ultrasonic frequency variance value of the current weld point. The current variance, pressure variance, and ultrasonic frequency variance of each weld point are arranged sequentially according to the weld point order to obtain the current variance sequence, pressure variance sequence, and ultrasonic frequency variance sequence.

[0024] Specifically, the sliding window length W is recommended to be between 5 and 10 solder joints. The reasons for this are as follows: if W is too small, the number of samples in the window is insufficient, and abnormal fluctuations in the signal of a single solder joint will have a significant impact on the variance value, making the variance sequence sensitive to noise; if W is too large, the range of solder joints covered by the window is too wide, and the response of the variance value to changes in the signal trend will be significantly delayed, which is not conducive to the timely triggering of subsequent convergence judgment. For the i-th solder joint in the candidate reference set, take the i-W+1 solder joints forward to the i-th solder joint to form the current sliding window. When i is less than W, the actual number of solder joints in the window is less than W, and this focus does not participate in the variance calculation. Starting from the W-th solder joint, the rolling variance calculation is performed point by point. The mean of the current signal in the window is the sum of the current signals of the W solder joints in the window divided by W. The difference between the current signal of each solder joint and this mean is squared. The sum of the W squared differences is divided by W to obtain the current variance value of the current focus. The pressure variance value and the ultrasonic frequency variance value are calculated separately according to the same steps.

[0025] The current variance values ​​of each solder joint from the Wth solder joint to the last solder joint in the candidate benchmark set are arranged sequentially according to the solder joint order to obtain the current variance sequence; the pressure variance values ​​of each corresponding solder joint are arranged in the same solder joint order to obtain the pressure variance sequence; the ultrasonic frequency variance values ​​of each corresponding solder joint are arranged in the same solder joint order to obtain the ultrasonic frequency variance sequence; elements at the same position in the three variance sequences correspond to the same solder joint, and the solder joint order numbering is strictly consistent in the three sequences to ensure that the variance values ​​of each dimension of the subsequent M consecutive focal points can be correctly aligned according to the solder joint dimension when comparing values ​​one by one.

[0026] In one specific embodiment, step S2, when the variance values ​​of each dimension of M consecutive solder joints simultaneously fall within the preset steady-state interval of the corresponding dimension, includes: The current variance value, pressure variance value, and ultrasonic frequency variance value of the current variance value, pressure variance value, and ultrasonic frequency variance value of the M consecutive weld points ahead of the current weld point in the current variance sequence, pressure variance sequence, and ultrasonic frequency variance sequence are compared with the upper and lower bounds of the preset current steady-state interval, preset pressure steady-state interval, and preset ultrasonic frequency steady-state interval, respectively. When the current variance values ​​of M consecutive weld points all fall within the preset current steady-state range, the pressure variance values ​​all fall within the preset pressure steady-state range, and the ultrasonic frequency variance values ​​all fall within the preset ultrasonic frequency steady-state range, the M consecutive weld points are marked as a steady-state weld point set. If the variance value of any dimension in any of the M consecutive solder joints does not fall into the preset steady-state interval of the corresponding dimension, the current focus is shifted to the next solder joint and the value-by-value comparison is re-executed until the condition that the variance values ​​of each dimension of the M consecutive solder joints all fall into the preset steady-state interval of the corresponding dimension is met, thus obtaining the steady-state solder joint set.

[0027] Specifically, the upper and lower bounds of the preset current steady-state interval, preset pressure steady-state interval, and preset ultrasonic frequency steady-state interval are determined based on the statistical distribution of the variance sequences of each dimension during the stable operation phase of the equipment in offline experiments. Specifically, the upper quartile of the variance distribution of each dimension during the stable operation phase is used as the upper bound of the corresponding dimension's steady-state interval, with zero as the lower bound. The upper quartile is chosen based on the fact that the variance values ​​below this quartile cover 75% of the normal fluctuation range during the stable operation phase. This ensures that the upper bound is neither too tight, leading to frequent triggering of extensions, nor too loose, including solder joints that have already experienced signal drift into the steady-state solder joint set. It is recommended that the M value be no less than 3 and no greater than 10. If the M value is too small, occasional continuous and stable solder joints can trigger the steady-state solder joint set marking, causing the batch reference package to be activated prematurely before the signal has fully converged. If the M value is too large, a longer solder joint sequence is required to complete the convergence judgment, which may lead to the risk of not being able to complete the convergence judgment when the number of solder joints in the first segment of the batch is limited.

[0028] The value-by-value comparison process is as follows: Take the variance values ​​of the current weld point M consecutive weld points preceding the current weld point from the current variance sequence, pressure variance sequence, and ultrasonic frequency variance sequence. For each weld point, compare the current variance value with the upper and lower bounds of the preset current steady-state interval, the pressure variance value with the upper and lower bounds of the preset pressure steady-state interval, and the ultrasonic frequency variance value with the upper and lower bounds of the preset ultrasonic frequency steady-state interval. Only when all three-dimensional variance values ​​of the M weld points simultaneously fall within their respective steady-state intervals are the M weld points considered. The solder joints are marked as a steady-state solder joint set. If any dimension variance value of any solder joint among the M solder joints does not fall into the corresponding steady-state interval, the current solder joint is extended to the next solder joint. The previous M consecutive solder joints are re-aligned with the new current solder joint as the endpoint for value-by-value comparison. This process is repeated until the condition is met. When the number of remaining solder joints in the candidate reference set is less than M, it is determined that the first solder joint of the current batch does not meet the convergence condition. The batch reference package is not activated, and the number of the first solder joints of the batch needs to be expanded before this step is repeated.

[0029] In one specific embodiment, step S2, constructing a batch benchmark package using the benchmark center values ​​of each dimension and the corresponding steady-state interval boundary values, includes: The average values ​​of the current signal, pressure signal, and ultrasonic frequency signal of M weld points in the steady-state weld point set are calculated to obtain the center value of the current reference, the center value of the pressure reference, and the center value of the ultrasonic frequency reference. The center value of the current reference is packaged with the upper and lower bounds of the preset current steady-state range, the center value of the pressure reference is packaged with the upper and lower bounds of the preset pressure steady-state range, and the center value of the ultrasonic frequency reference is packaged with the upper and lower bounds of the preset ultrasonic frequency steady-state range according to the sensor dimension to obtain a batch reference package.

[0030] Specifically, the current reference center value of M weld points in the steady-state weld point set is obtained by averaging the current signal sampling sequences of each of the M weld points, and then averaging the M averages. That is, the representative value of the current signal of each weld point is obtained by averaging all sampling points in the current signal sampling sequence of each weld point, and then the representative values ​​of the current signals of the M weld points are averaged to obtain the current reference center value. The pressure reference center value and the ultrasonic frequency reference center value are obtained by averaging the representative values ​​of the M weld point signals of the corresponding dimensions according to the same calculation steps. The three reference center values ​​reflect the actual working condition level of the current batch after the signal has fully converged, rather than the historical ideal value calibrated offline. Therefore, they can automatically include the comprehensive influence of the material characteristics, equipment status and environmental factors of the current batch.

[0031] The batch reference package is encapsulated using sensor dimensions as the index unit. The current dimension field contains three values: the current reference center value, the upper limit of the preset current steady-state interval, and the lower limit of the preset current steady-state interval. The pressure dimension field contains three values: the pressure reference center value, the upper limit of the preset pressure steady-state interval, and the lower limit of the preset pressure steady-state interval. The ultrasonic frequency dimension field contains three values: the ultrasonic frequency reference center value, the upper limit of the preset ultrasonic frequency steady-state interval, and the lower limit of the preset ultrasonic frequency steady-state interval. A total of nine values ​​in the three dimension fields are stored one-to-one according to the dimension index. The encapsulated batch reference package retrieves the corresponding reference center value and steady-state interval boundary value dimension by dimension using the dimension index as the key value, ensuring that the reference values ​​used for deviation calculation and normalization processing of each dimension strictly correspond to the current dimension and that cross-dimensional misuse does not occur.

[0032] In one specific embodiment, step S3 includes: The current signal, pressure signal, and ultrasonic frequency signal of each subsequent solder joint are subtracted one dimension from the center value of the current reference, the center value of the pressure reference, and the center value of the ultrasonic frequency reference in the batch reference package to obtain the current deviation value, pressure deviation value, and ultrasonic frequency deviation value of each solder joint. The current deviation value, pressure deviation value and ultrasonic frequency deviation value of each weld point are normalized with the steady-state interval boundary value of the corresponding dimension in the batch reference package to obtain the normalized current deviation value, pressure normalized deviation value and ultrasonic frequency normalized deviation value of each weld point. The normalized deviation values ​​of current, pressure, and ultrasonic frequency of each weld point are weighted and summed according to preset weights to obtain the multidimensional deviation value of each weld point. The multidimensional deviation values ​​of each solder joint are arranged sequentially according to the solder joint order to obtain the deviation value sequence.

[0033] Specifically, the representative value of the current signal for each subsequent solder joint is obtained by averaging all sampling points within the current signal sampling sequence of that solder joint. The difference between this representative value and the current reference center value in the batch reference package is used to obtain the current deviation value for that solder joint. A positive current deviation value indicates that the current signal of the current solder joint is higher than the batch reference, while a negative value indicates that it is lower than the batch reference. The pressure deviation value and ultrasonic frequency deviation value are obtained by subtracting the representative value of the corresponding dimension signal from the corresponding dimension reference center value, respectively, using the same calculation steps. Normalization processing uses the difference between the upper bound of the steady-state interval of the corresponding dimension in the batch reference package and the reference center value as the normalization divisor. The current deviation value is divided by the current dimension normalization divisor to obtain the current normalized deviation value; the pressure deviation value is divided by the pressure dimension normalization divisor to obtain the pressure normalized deviation value; and the ultrasonic frequency deviation value is divided by the ultrasonic frequency dimension normalization divisor to obtain the ultrasonic frequency normalized deviation value. Normalization processing eliminates the distortion problem in the weighted results caused by the different dimensions and amplitude magnitudes of the three signals.

[0034] The preset weights are determined by the sensitivity analysis of each dimension of the signal to defects such as cold solder joints and over-soldering in offline experiments. Specifically, the signal-to-noise ratio (SNR) is used as the basis for weight allocation, based on the ratio of the mean difference to the standard deviation of each dimension's signal between known defective solder joints and normal solder joints. Dimensions with higher SNR are assigned larger weights, and the sum of the preset weights of the three dimensions is constrained to 1. The normalized deviation value of the current dimension, the normalized deviation value of the pressure dimension, and the normalized deviation value of the ultrasonic frequency dimension of each solder joint are multiplied by the preset weight of the current dimension, and the sum of the three products is used to obtain the multidimensional deviation value of the solder joint. The multidimensional deviation value is a single scalar that reflects the comprehensive deviation of the current solder joint from the batch reference package in the three-dimensional sensor signal space. The multidimensional deviation values ​​of each solder joint are arranged sequentially according to the solder joint order to obtain the deviation value sequence. Each element in the deviation value sequence corresponds strictly one-to-one with the solder joint sequence number.

[0035] In one specific embodiment, step S4 includes: Take K consecutive deviation values ​​from the current solder joint as the endpoint in the deviation value sequence, take the solder joint sequence number corresponding to the K consecutive deviation values ​​as the independent variable and the K consecutive deviation values ​​as the dependent variable, and perform linear fitting by the least squares method to obtain the fitting slope. The fitted slope is compared with a preset slope threshold. When the fitted slope exceeds the preset slope threshold, the current solder joint is marked as an abnormal trend solder joint. When the fitted slope does not exceed the preset slope threshold, the current focus is marked as a normal trend solder joint. The current solder joint is carried over to the next solder joint, and K consecutive deviation values ​​are taken again to perform linear fitting and comparison until P consecutive solder joints are marked as abnormal trend solder joints, at which point a welding warning signal is generated.

[0036] Specifically, from the deviation value sequence, K consecutive deviation values ​​are taken backward from the current solder joint as the endpoint. The K solder joints are numbered sequentially to form the independent variable vector, and the corresponding K multidimensional deviation values ​​form the dependent variable vector. The specific calculation process for least squares linear fitting is as follows: using the mean of the independent variable vector and the mean of the dependent variable vector as their respective center values, the difference between each element in the independent variable vector and the mean of the independent variable is used to obtain the independent variable deviation sequence. Similarly, the difference between each element in the dependent variable vector and the mean of the dependent variable is used to obtain the dependent variable deviation sequence. The sum of the products of corresponding elements of the column and the dependent variable deviation sequence, divided by the sum of the squares of each element of the independent variable deviation sequence, yields the fitting slope. A value of K is recommended to be between 5 and 15 solder joints. If K is too small, the fitting slope is sensitive to fluctuations in single-point deviations; if K is too large, the slope's response to trend changes will be significantly delayed. The preset slope threshold is determined based on the lower quartile of the statistical distribution of the fitting slope of the deviation value sequence during the progressive degradation stage of equipment in historical batches. Using this quartile as the threshold can cover 75% of the abnormal trend situations in historical degradation scenarios.

[0037] The fitted slope is compared with a preset slope threshold. If the fitted slope is significantly greater than the preset slope threshold, the current solder joint is marked as an abnormal trend solder joint; if the fitted slope is not greater than the preset slope threshold, the current solder joint is marked as a normal trend solder joint. The current solder joint is then moved to the next solder joint, and the same linear fitting and comparison are performed again with K consecutive deviation values ​​as the endpoint. This process is repeated for each new solder joint in the deviation value sequence. It is recommended that the P-value be no less than 3. If the P-value is too small, even a brief, continuous anomaly caused by a single equipment disturbance can trigger the solder joint. The warning signal may be falsely triggered. If the value of P is too large, more abnormal solder joints need to be accumulated before the warning can be triggered, resulting in a delay in the warning response. The specific value of P is determined by combining the production line cycle time and the maximum acceptable warning delay time. When P consecutive solder joints in the deviation value sequence are marked as abnormal solder joints, it is determined that there is a systematic deterioration trend in the current welding production line, and a welding warning signal is generated. The time of generation of the welding warning signal corresponds to the location of the Pth abnormal solder joint. The sequential number of the P solder joints before this location is recorded synchronously in the welding warning signal.

[0038] Figure 3 This is a schematic diagram illustrating the trend monitoring of deviation value sequences and the generation of welding early warning signals in an embodiment of this application. Figure 3 (a) The horizontal axis represents the solder joint sequence number, and the vertical axis represents the multidimensional deviation value. The curve reflects the overall deviation of each subsequent solder joint relative to the batch reference package. In the early part of the solder joint sequence, the deviation value fluctuates around a low level, while in the later part of the solder joint sequence, the deviation value shows a continuous monotonic upward trend. Figure 3 (b) The vertical axis represents the fitting slope, the dotted line represents the slope threshold, and the filled area represents the interval where the fitting slope exceeds the slope threshold. When the fitting slope of P consecutive weld points exceeds the slope threshold, the position marked by the vertical dashed line is the time when the welding warning signal is generated. The positions of the vertical dashed lines in the two figures correspond one-to-one, indicating that the warning trigger time is synchronously visible in the deviation value sequence.

[0039] The above describes the early warning method for the battery module welding process in the embodiments of this application. The following describes the early warning system for the battery module welding process in the embodiments of this application. One embodiment of the early warning system for the battery module welding process in the embodiments of this application includes: The screening module is used to collect current signals, pressure signals and ultrasonic frequency signals during the battery module welding process. It filters the first weld joint of the batch through a wide boundary of resistance value to generate a candidate reference set. The calculation module is used to perform rolling variance calculation on the current signal, pressure signal and ultrasonic frequency signal of each weld point in the candidate reference set according to the order of the weld points to obtain the variance sequence of each sensor dimension. When the variance values ​​of each dimension of M consecutive weld points all fall into the preset steady-state interval of the corresponding dimension, the mean value of the current signal, the mean value of the pressure signal and the mean value of the ultrasonic frequency signal of the M consecutive weld points are used as the reference center value of the corresponding sensor dimension, and the batch reference package is constructed with the reference center value of each dimension and the boundary value of the steady-state interval of the corresponding dimension. The arrangement module is used to subtract the current signal, pressure signal and ultrasonic frequency signal of each subsequent solder joint from the reference center value of the corresponding dimension in the batch reference package one dimension at a time to obtain the multidimensional deviation value of each solder joint. The multidimensional deviation values ​​of each solder joint are arranged in the order of the solder joints to obtain the deviation value sequence. The fitting module is used to perform linear fitting on K consecutive deviation values ​​in the deviation value sequence, and uses the fitting slope exceeding the slope threshold as a criterion to generate a welding early warning signal.

[0040] This invention also provides an early warning device for the battery module welding process, which can be a server. The early warning device includes a processor, memory, display screen, input device, network interface, and database connected via a system bus. The processor, designed as a computer, provides computing and control capabilities. The memory includes a non-volatile storage medium and internal memory. The non-volatile storage medium stores an operating system, computer programs, and a database. The internal memory provides an environment for the operation of the operating system and computer programs in the non-volatile storage medium. The database stores the data corresponding to this embodiment. The network interface of the early warning device is used to communicate with external terminals via a network connection. When the computer program is executed by the processor, it implements the above-described method.

[0041] The present invention also provides a computer-readable storage medium, which may be a non-volatile computer-readable storage medium or a volatile computer-readable storage medium, wherein the computer-readable storage medium stores instructions that, when the instructions are executed on a computer, cause the computer to perform the steps of the warning method for the battery module welding process.

[0042] Those skilled in the art will clearly understand that, for the sake of convenience and brevity, the specific working processes of the systems and units described above can be referred to the corresponding processes in the foregoing method embodiments, and will not be repeated here.

[0043] If the integrated unit is implemented as a software functional unit and sold or used as an independent product, it can be stored in a computer-readable storage medium. Based on this understanding, the technical solution of the present invention, in essence, or the part that contributes to the prior art, or all or part of the technical solution, can be embodied in the form of a software product. This computer software product is stored in a storage medium and includes several instructions to cause a warning device (which may be a personal computer, server, or network device, etc.) used in the battery module welding process to execute all or part of the steps of the methods described in the various embodiments of the present invention. The aforementioned storage medium includes various media capable of storing program code, such as USB flash drives, portable hard drives, read-only memory (ROM), random access memory (RAM), magnetic disks, or optical disks.

[0044] The above embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit it. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A pre-warning method for a battery module welding process, characterized in that, The method includes: Step S1: Collect current signals, pressure signals and ultrasonic frequency signals during the battery module welding process, and generate a candidate reference set by filtering the first weld joint of the batch through a wide boundary of resistance value; Step S2: Perform rolling variance calculation on the current signal, pressure signal, and ultrasonic frequency signal of each solder joint in the candidate reference set according to the order of the solder joints to obtain the variance sequence of each sensor dimension. When the variance values ​​of each dimension of M consecutive solder joints fall into the preset steady-state interval of the corresponding dimension, use the mean value of the current signal, the mean value of the pressure signal, and the mean value of the ultrasonic frequency signal of the M consecutive solder joints as the reference center value of the corresponding sensor dimension, and construct a batch reference package with the reference center value of each dimension and the boundary value of the steady-state interval of the corresponding dimension. Step S3: Subtract the current signal, pressure signal and ultrasonic frequency signal of each subsequent solder joint from the reference center value of the corresponding dimension in the batch reference package one dimension at a time to obtain the multidimensional deviation value of each solder joint. Arrange the multidimensional deviation values ​​of each solder joint in the order of the solder joints to obtain the deviation value sequence. Step S4: Perform linear fitting on K consecutive deviation values ​​in the deviation value sequence, and use the fitting slope exceeding the slope threshold as a criterion to generate a welding early warning signal.

2. The pre-warning method for battery module welding process according to claim 1, wherein, Step S1 includes: The welding process of each weld point in the first segment of the batch is synchronously collected using current sensors, pressure sensors, and ultrasonic sensors to obtain current signal sampling sequences, pressure signal sampling sequences, and ultrasonic frequency signal sampling sequences for each weld point. The welding resistance values ​​corresponding to the current signal sampling sequence, pressure signal sampling sequence and ultrasonic frequency signal sampling sequence of each weld point are compared with the upper and lower boundaries of the preset resistance value wide boundary interval. Weld points whose welding resistance values ​​fall within the preset resistance value wide boundary interval are marked as valid weld points, and weld points whose welding resistance values ​​do not fall within the preset resistance value wide boundary interval are removed. The current signal sampling sequence, the pressure signal sampling sequence, and the ultrasonic frequency signal sampling sequence of each valid solder joint are arranged in the order of the solder joints to generate the candidate reference set.

3. The pre-warning method for battery module welding process of claim 1, wherein, In step S2, the rolling variance of the current signal, pressure signal, and ultrasonic frequency signal of each weld point in the candidate reference set is calculated according to the weld point order, including: Taking the current solder joint as the endpoint, take a sliding window with a window length of W forward. Calculate the mean value of the current signal of each solder joint within the sliding window. Square the difference between the current signal of each solder joint within the sliding window and the mean value of the current signal within the window, sum the squares, and then divide by the window length W to obtain the current variance value of the current solder joint. Using the same sliding window length W, the pressure signal and ultrasonic frequency signal of each weld point within the sliding window are calculated using the same process as the current variance value to obtain the pressure variance value and ultrasonic frequency variance value of the current weld point. The current variance value, pressure variance value, and ultrasonic frequency variance value of each weld point are arranged sequentially according to the weld point order to obtain the current variance sequence, pressure variance sequence, and ultrasonic frequency variance sequence.

4. The pre-warning method for battery module welding process according to claim 3, wherein, In step S2, when the variance values ​​of each dimension of M consecutive solder joints simultaneously fall within the preset steady-state interval of the corresponding dimension, the following steps are included: The current variance value, pressure variance value, and ultrasonic frequency variance value of the current variance sequence, the pressure variance sequence, and the ultrasonic frequency variance sequence of the M consecutive weld points preceding the current weld point are compared with the upper and lower bounds of the preset current steady-state interval, the preset pressure steady-state interval, and the preset ultrasonic frequency steady-state interval, respectively. When the current variance values ​​of the M consecutive solder joints all fall within the preset current steady-state range, the pressure variance values ​​all fall within the preset pressure steady-state range, and the ultrasonic frequency variance values ​​all fall within the preset ultrasonic frequency steady-state range, the M consecutive solder joints are marked as a steady-state solder joint set. If the variance value of any dimension in any of the M consecutive solder joints does not fall into the preset steady-state interval of the corresponding dimension, the current focus is shifted to the next solder joint and the value-by-value comparison is re-executed until the condition that the variance values ​​of each dimension of the M consecutive solder joints all fall into the preset steady-state interval of the corresponding dimension is met, thus obtaining the steady-state solder joint set.

5. The pre-warning method for battery module welding process of claim 4, wherein, In step S2, a batch reference package is constructed using the reference center values ​​of each dimension and the corresponding steady-state interval boundary values, including: The average values ​​of the current signal, pressure signal, and ultrasonic frequency signal of the M weld points in the steady-state weld point set are calculated to obtain the current reference center value, pressure reference center value, and ultrasonic frequency reference center value. The current reference center value and the upper and lower bounds of the preset current steady-state interval, the pressure reference center value and the upper and lower bounds of the preset pressure steady-state interval, and the ultrasonic frequency reference center value and the upper and lower bounds of the preset ultrasonic frequency steady-state interval are packaged according to the sensor dimension to obtain the batch reference package.

6. The early warning method for the battery module welding process according to claim 1, characterized in that, Step S3 includes: The current signal, pressure signal, and ultrasonic frequency signal of each subsequent solder joint are subtracted one dimension from the center value of the current reference, the center value of the pressure reference, and the center value of the ultrasonic frequency reference in the batch reference package to obtain the current deviation value, pressure deviation value, and ultrasonic frequency deviation value of each solder joint. The current deviation value, pressure deviation value, and ultrasonic frequency deviation value of each weld point are normalized with the steady-state interval boundary value of the corresponding dimension in the batch reference package to obtain the normalized current deviation value, pressure normalized deviation value, and ultrasonic frequency normalized deviation value of each weld point. The normalized deviation values ​​of current, pressure, and ultrasonic frequency at each weld point are weighted and summed according to preset weights to obtain the multidimensional deviation value of each weld point. The multidimensional deviation values ​​of each solder joint are arranged sequentially according to the solder joint order to obtain the deviation value sequence.

7. The early warning method for the battery module welding process according to claim 1, characterized in that, Step S4 includes: Take K consecutive deviation values ​​from the current solder joint as the endpoint in the deviation value sequence, take the solder joint sequence number corresponding to the K consecutive deviation values ​​as the independent variable, and take the K consecutive deviation values ​​as the dependent variable, and perform linear fitting by the least squares method to obtain the fitting slope. The fitted slope is compared with a preset slope threshold. When the fitted slope exceeds the preset slope threshold, the current solder joint is marked as an abnormal trend solder joint. When the fitted slope does not exceed the preset slope threshold, the current focus is marked as a normal trend solder joint. The current solder joint is carried over to the next solder joint, and K consecutive deviation values ​​are taken again to perform the linear fitting and comparison, until P consecutive solder joints are marked as abnormal trend solder joints, and the welding warning signal is generated.

8. A warning system for the battery module welding process, characterized in that, For implementing the early warning method for the battery module welding process as described in any one of claims 1-7, the early warning system for the battery module welding process comprises: The screening module is used to collect current signals, pressure signals and ultrasonic frequency signals during the battery module welding process. It filters the first weld joint of the batch through a wide boundary of resistance value to generate a candidate reference set. The calculation module is used to perform rolling variance calculation on the current signal, pressure signal and ultrasonic frequency signal of each weld point in the candidate reference set according to the order of the weld points to obtain the variance sequence of each sensor dimension. When the variance values ​​of each dimension of M consecutive weld points all fall into the preset steady-state interval of the corresponding dimension, the mean value of the current signal, the mean value of the pressure signal and the mean value of the ultrasonic frequency signal of the M consecutive weld points are used as the reference center value of the corresponding sensor dimension, and the batch reference package is constructed with the reference center value of each dimension and the boundary value of the steady-state interval of the corresponding dimension. The arrangement module is used to subtract the current signal, pressure signal and ultrasonic frequency signal of each subsequent solder joint from the reference center value of the corresponding dimension in the batch reference package one dimension at a time to obtain the multidimensional deviation value of each solder joint. The multidimensional deviation values ​​of each solder joint are arranged in the order of the solder joints to obtain the deviation value sequence. The fitting module is used to perform linear fitting on K consecutive deviation values ​​in the deviation value sequence, and uses the fitting slope exceeding the slope threshold as a criterion to generate a welding early warning signal.

9. A warning device for the battery module welding process, characterized in that, The device includes a memory and a processor, the memory storing a computer program that can run on the processor, and the processor executing the computer program to implement the early warning method for the battery module welding process as described in any one of claims 1 to 7.

10. A computer-readable storage medium having a computer program stored thereon, characterized in that, When the computer program is run by the processor, it causes the processor to execute the warning method for the battery module welding process as described in any one of claims 1 to 7.