GIS partial discharge sensor optimization method, sensor and partial discharge detection system

The flexible PVDF sensor, designed using a multi-physics coupled finite element model and gradient-width dual-fin coplanar rectangular electrodes, solves the problems of acoustic impedance mismatch and narrow bandwidth of traditional sensors, achieving high sensitivity and wide bandwidth partial discharge detection, and is suitable for on-site online monitoring of GIS.

CN123158949APending Publication Date: 2026-11-24ELECTRIC POWER RESEARCH INSTITUTE OF STATE GRID SHANDONG ELECTRIC POWER COMPANY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611011625.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-08
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In existing GIS partial discharge detection methods, traditional piezoelectric ceramic sensors suffer from problems such as acoustic impedance mismatch, narrow bandwidth, prominent resonance characteristics, large size, and inconvenient installation, making it difficult to achieve high sensitivity, wide bandwidth, and reliable detection. Furthermore, existing PVDF sensors have low sensitivity, lack of optimized structural design, and poor engineering applicability, failing to meet the requirements of GIS on-site online monitoring.

Method used

The sensor placement and installation direction were optimized using a multi-physics coupled finite element model. A gradient-width double-finger coplanar rectangular electrode was designed. Combined with the optimal shape and size of a flexible polyvinylidene fluoride film, signal conditioning, data acquisition and processing modules were built. A time-frequency-spectral cross-dimensional attention fusion network was constructed for signal recognition.

Benefits of technology

It achieves a balance between high sensor sensitivity and wide bandwidth response, ensuring signal transmission efficiency, enabling installation in confined spaces, improving the accuracy of partial discharge identification, meeting the long-term online monitoring needs of GIS sites, and reducing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123158949A_ABST
    Figure CN123158949A_ABST
Patent Text Reader

Abstract

The application belongs to the technical field of power equipment state monitoring and fault diagnosis, and discloses a GIS partial discharge sensor optimization method, a sensor and a partial discharge detection system. The method comprises the following steps: determining an optimal arrangement position and an installation direction of the sensor; determining an optimal electrode configuration; determining an optimal shape and size of a flexible polyvinyl fluoride film; determining the thickness of the optimal flexible polyvinyl fluoride film; preparing the sensor according to the optimal electrode configuration, the optimal shape and size and the thickness of the optimal flexible polyvinyl fluoride film, obtaining the optimized sensor, and building a performance test platform to test and verify the sensitivity of the optimized sensor. Through multi-parameter collaborative optimization, the application significantly improves the average sensitivity of the sensor in the key detection frequency band, effectively widens the effective working frequency bandwidth of the sensor, and realizes the unification of ultrahigh sensitivity and wide frequency band response.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of power equipment condition monitoring and fault diagnosis technology, and in particular to a method for optimizing GIS partial discharge sensors, the sensor itself, and a partial discharge detection system. Background Technology

[0002] Gas-insulated switchgear (GIS) has become a core switching device in ultra-high voltage and high voltage power grids due to its advantages such as small footprint, high operational reliability, and long maintenance cycle. Insulation failures in GIS equipment are one of the main causes of large-scale power outages, and partial discharge is an early sign and primary manifestation of insulation degradation. According to publicly available statistics from the power industry, three typical defects—metallic foreign object discharge, floating potential discharge, and surface discharge—account for more than 90% of all GIS insulation failures, with metallic foreign object discharge accounting for as much as 60%, making it the leading cause of GIS insulation failure. Therefore, achieving early, high-precision, and high-reliability detection of partial discharge in GIS is of paramount importance for ensuring the safe and stable operation of the power grid.

[0003] Currently, the main methods for detecting partial discharge in GIS include ultra-high frequency (UHF) methods, ultrasonic methods, chemical detection methods, and pulsed current methods. Among these, ultrasonic methods have advantages such as strong resistance to electromagnetic interference, high positioning accuracy, and the ability to detect electrical charges, making them one of the most widely used detection methods in the field. Currently, commercially available ultrasonic sensors mainly use piezoelectric ceramic materials, such as lead zirconate titanate (PZT). However, these sensors suffer from three inherent technical bottlenecks that severely restrict the improvement of detection performance:

[0004] Severe acoustic impedance mismatch: The acoustic impedance of PZT ceramic is approximately... The acoustic impedance of the GIS aluminum alloy shell is approximately The difference in acoustic impedance between the two causes up to 60% of the ultrasonic energy to be reflected at the interface, which significantly reduces the effective sensitivity of the sensor. At the same time, the rigid structure of PZT cannot fit the curved shell of GIS, which further aggravates the coupling loss.

[0005] Narrow bandwidth and prominent resonance characteristics: PZT sensors operate on a resonant principle, and their -6dB bandwidth is typically only 10kHz-40kHz, making it difficult to fully capture the 20kHz-100kHz wideband transient ultrasonic signals excited by partial discharge. Furthermore, the resonance mechanism can cause severe signal ringing, resulting in waveform distortion and an inability to distinguish continuous discharge pulses with a time interval of less than 10μs, which seriously affects the resolution of single discharges and the accuracy of defect type identification.

[0006] Large size and inconvenient installation: Commercial PZT sensors are usually cylindrical with a diameter of about 30mm-50mm and a weight of more than 50g, making them difficult to install in critical detection locations with limited space, such as near GIS basin insulators or flange gaps.

[0007] In recent years, although optical ultrasonic sensing technology (such as Fabry-Perot interferometer sensors and fiber Bragg grating sensors) has made breakthroughs in sensitivity, its system structure is complex, its cost is high (the cost of a single channel exceeds 100,000 yuan), its environmental adaptability is poor (it is easily affected by vibration and temperature changes), and it requires regular optical path calibration, making it difficult to meet the requirements of reliability, miniaturization and economy for long-term online monitoring in GIS.

[0008] Polyvinylidene fluoride (PVDF), as a novel flexible piezoelectric polymer material, possesses wide bandwidth response, high voltage output, good flexibility, and low acoustic impedance. The advantages of PVDF, such as ease of processing and molding, provide a new approach to overcoming the technical bottlenecks of traditional PZT sensors. However, existing research on PVDF ultrasonic sensors still has significant shortcomings:

[0009] Low sensitivity: Existing literature reports that the average sensitivity of PVDF ultrasonic sensors in the key detection frequency band of 20kHz-80kHz is only [insert value here]. It is about 5dB-8dB lower than the mainstream commercial PZT sensor, making it difficult to detect weak early partial discharge signals in GIS.

[0010] The structural design lacks systematic optimization: existing studies focus more on material modification, while there is insufficient research on the synergistic optimization of key structural parameters such as electrode configuration, film size, and mounting method, which fails to fully utilize the piezoelectric properties of PVDF materials;

[0011] Poor engineering applicability: Most existing PVDF sensors are laboratory prototypes, lacking complete packaging and electromagnetic shielding designs, and have weak resistance to on-site interference, making them unsuitable for direct application in GIS on-site online monitoring.

[0012] Therefore, how to provide optimization methods for GIS partial discharge sensors, as well as sensors and partial discharge detection systems, is an urgent problem to be solved. Summary of the Invention

[0013] This invention provides an optimization method for GIS partial discharge sensors, a sensor, and a partial discharge detection system to solve the problems mentioned above in the prior art.

[0014] According to a first aspect of the present invention, a method for optimizing a GIS partial discharge sensor is provided.

[0015] In one embodiment, the GIS partial discharge sensor optimization method includes:

[0016] A multi-physics coupled finite element model was established, and the propagation characteristics of ultrasonic signals on the surface of the GIS shell were analyzed to determine the optimal placement and installation direction of the sensors.

[0017] Using the optimal arrangement position and installation direction as simulation boundary conditions, finite element models of various electrode configurations were constructed for simulation comparison. Based on the comprehensive simulation results of the piezoelectric response characteristics and frequency response characteristics of different electrodes, the optimal electrode configuration was determined.

[0018] A piezoelectric vibration model of a flexible polyvinylidene fluoride (PVDF) film was established to analyze the influence of the length and width of the flexible PVDF film on the sensitivity and frequency response, and to determine the optimal shape and size of the flexible PVDF film.

[0019] Based on the optimal shape and size, the influence of the thickness of the flexible polyvinylidene fluoride film on the piezoelectric constant, capacitance and sensitivity is analyzed, and the optimal thickness of the flexible polyvinylidene fluoride film is determined in combination with the feasibility of the preparation process.

[0020] Based on the optimal electrode configuration, optimal shape and size, and optimal thickness of the flexible polyvinylidene fluoride film, a sensor was fabricated to obtain an optimized sensor. A performance testing platform was then built to verify the sensitivity of the optimized sensor.

[0021] According to a second aspect of the present invention, a GIS partial discharge sensor is provided.

[0022] In one embodiment, the GIS partial discharge sensor includes an acoustic coupling layer, a flexible polyvinylidene fluoride sensing unit, an electrode structure, a pre-bending shaping layer, an encapsulation protection layer, and an electromagnetic shielding layer, which are stacked sequentially from the inside to the outside.

[0023] An acoustic coupling layer is attached to the surface of the GIS housing to reduce the reflection loss of ultrasonic signals at the interface between the GIS housing and the sensor, and to transmit the mechanical vibration of the GIS housing to the flexible polyvinylidene fluoride sensing unit without attenuation.

[0024] The flexible polyvinylidene fluoride (PVDF) sensitive unit is disposed on the back of the acoustic coupling layer to receive ultrasonic signals excited by partial discharge of GIS and generate mechanical vibration, and to generate polarized charges on the upper and lower surfaces of the flexible PVDF sensitive film through the positive piezoelectric effect.

[0025] The electrode structure is located on the front of the flexible polyvinylidene fluoride sensing unit. It is a gradient-width double-fin coplanar rectangular electrode used to collect polarization charge and output electrical signal.

[0026] A pre-bending shaping layer is placed between the electrode structure and the encapsulation protective layer to pre-bend the sensor into a shape that matches the curvature of the GIS housing surface, thereby eliminating bubbles and stress concentrations generated when the sensor is attached to the curved GIS housing.

[0027] An encapsulation protective layer covers the non-electrode area on the front of the pre-bent shaping layer and the flexible polyvinylidene fluoride sensitive unit to protect the electrodes from oxidation and mechanical damage.

[0028] An electromagnetic shielding layer covers the outer surface of the encapsulation protective layer to suppress electromagnetic interference.

[0029] According to a third aspect of the present invention, a GIS partial discharge detection system is provided.

[0030] In one embodiment, the GIS partial discharge detection system includes:

[0031] The signal conditioning module is used to perform impedance matching, amplification, and filtering on the weak analog electrical signal output by the sensor to obtain the processed analog voltage signal.

[0032] The data acquisition module is used to convert the processed analog voltage signal into a digital signal;

[0033] The processing module is used to perform time-frequency domain analysis and feature extraction on digital signals to identify the type and severity of partial discharge in GIS, so as to achieve fault early warning.

[0034] The technical solutions provided by the embodiments of the present invention may include the following beneficial effects:

[0035] 1) This invention significantly improves the average sensitivity of the sensor in the key detection frequency band through multi-parameter collaborative optimization, effectively broadens the effective working frequency band of the sensor, and avoids the waveform distortion problem caused by the resonance characteristics of traditional piezoelectric ceramic sensors. This greatly improves the waveform rise time and single discharge resolution of the sensor, and achieves the unity of ultra-high sensitivity and wide bandwidth response.

[0036] 2) This invention employs a pre-bent shaping layer to ensure a tight fit between the sensor and the curved shell of the GIS, effectively eliminating air bubbles and stress concentration issues during bonding and significantly reducing acoustic coupling loss. Combined with an adaptive impedance matching design, the sensor maintains stable signal transmission efficiency over a wide temperature range, achieving both excellent curved surface fit and wide temperature range adaptability. Furthermore, the sensor's thin overall thickness and light weight allow for installation in confined spaces inaccessible to traditional sensors. Its comprehensive electromagnetic shielding design provides excellent electromagnetic compatibility, meeting the engineering requirements for long-term online monitoring of GIS systems.

[0037] 3) This invention employs a time-frequency-spectral cross-dimensional attention fusion network to identify partial discharge signals. It utilizes global information from time-frequency domain features to adaptively guide the extraction of spectral features, effectively enhancing the sensitivity to weak discharge features. This significantly improves the average recognition accuracy of various typical defects and greatly reduces the discharge quantity assessment error, achieving accurate identification of weak discharges and providing reliable technical support for GIS insulation status assessment and fault early warning.

[0038] 4) This invention can be extended to the development of flexible ultrasonic sensors for other power equipment, significantly shortening the R&D cycle. Furthermore, this invention utilizes commercially available piezoelectric thin films and mature microfabrication processes, resulting in low-cost sensors suitable for large-scale application and possessing promising market prospects and industrial value.

[0039] It should be understood that the above general description and the following detailed description are exemplary and explanatory only, and are not intended to limit the invention. Attached Figure Description

[0040] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.

[0041] Figure 1 This is a flowchart illustrating a GIS partial discharge sensor optimization method according to an exemplary embodiment;

[0042] Figure 2 This is a schematic diagram of the structure of a GIS partial discharge sensor according to an exemplary embodiment;

[0043] Figure 3 This is a schematic block diagram of a GIS partial discharge detection system according to an exemplary embodiment;

[0044] Figure 4 This is a diagram illustrating the interdigitated electrode structure of a GIS partial discharge sensor according to an exemplary embodiment.

[0045] Figure 5 This is a simulated voltage-frequency response diagram of a GIS partial discharge sensor according to an exemplary embodiment. Detailed Implementation

[0046] The following description and accompanying drawings fully illustrate specific embodiments described herein to enable those skilled in the art to practice them. Some portions and features of certain embodiments may be included in or replace portions and features of other embodiments. The scope of the embodiments herein includes the entire scope of the claims and all available equivalents thereof. The various embodiments described herein are presented in a progressive manner, with each embodiment focusing on its differences from other embodiments; similar or identical parts between embodiments can be referred to interchangeably.

[0047] Each module in the apparatus or system of this application can be implemented in whole or in part by software, hardware, or a combination thereof.

[0048] Where there is no conflict, the embodiments and features in the embodiments of the present invention can be combined with each other.

[0049] Figure 1 An embodiment of the GIS partial discharge sensor optimization method of the present invention is shown.

[0050] In this optional embodiment, the GIS partial discharge sensor optimization method includes:

[0051] S101. Establish a multi-physics coupled finite element model and analyze the propagation characteristics of ultrasonic signals on the surface of the GIS shell to determine the optimal placement and installation direction of the sensors.

[0052] S102. Using the optimal arrangement position and installation direction as simulation boundary conditions, construct finite element models of various electrode configurations for simulation comparison. Based on the comprehensive simulation results of the piezoelectric response characteristics and frequency response characteristics of different electrodes, determine the optimal electrode configuration.

[0053] S103. Establish a piezoelectric vibration model for flexible polyvinylidene fluoride (PVDF) film, analyze the influence of the length and width of the flexible PVDF film on the sensitivity and frequency response, and determine the optimal shape and size of the flexible PVDF film.

[0054] S104. Based on the optimal shape and size, analyze the influence of the thickness of the flexible polyvinylidene fluoride film on the piezoelectric constant, capacitance and sensitivity, and determine the optimal thickness of the flexible polyvinylidene fluoride film in combination with the feasibility of the preparation process.

[0055] S105. Based on the optimal electrode configuration, optimal shape and size, and optimal thickness of the flexible polyvinylidene fluoride film, a sensor is prepared to obtain the optimized sensor. A performance testing platform is then built to verify the sensitivity of the optimized sensor.

[0056] In this optional embodiment, establishing a multiphysics coupled finite element model and analyzing the propagation characteristics of ultrasonic signals on the surface of the GIS shell to determine the optimal placement and installation direction of the sensor includes: establishing a three-dimensional finite element model using multiphysics simulation software, the three-dimensional finite element model including the GIS shell, acoustic coupling layer, and sensor; setting solid mechanical physical fields, acoustic physical fields, and piezoelectric effect physical fields for the GIS shell, acoustic coupling layer, and sensor respectively; applying a broadband ultrasonic longitudinal wave load of a preset ultrasonic signal frequency band to the inner wall of the GIS shell, setting low reflection boundary conditions at the outer edge of the GIS shell, and setting binding contacts between the sensor and the acoustic coupling layer, and between the acoustic coupling layer and the GIS shell; setting multiple monitoring points radially on the outer surface of the GIS shell, calculating the average vibration amplitude of each monitoring point within the preset ultrasonic signal frequency band, and determining the optimal placement position of the sensor based on the comparison results of the average vibration amplitude of each monitoring point; setting multiple installation directions at the optimal placement position, calculating the average output voltage of the sensor within the preset ultrasonic signal frequency band under different installation directions, and determining the optimal installation direction of the sensor based on the comparison results of the average output voltage of each installation direction.

[0057] In this optional embodiment, using the optimal arrangement position and installation direction as simulation boundary conditions, finite element models of various electrode configurations are constructed for simulation comparison. Based on the comprehensive simulation results of the piezoelectric response characteristics and frequency response characteristics of different electrodes, the optimal electrode configuration is determined, including: keeping the size of the flexible polyvinylidene fluoride film and the total electrode area unchanged, constructing finite element models of various electrode configurations; the various electrode configurations include single-finger strip electrodes, gradient-width double-finger strip coplanar rectangular electrodes, and interdigitated electrodes; based on the finite element models of various electrode configurations, a normal displacement load is applied to the back of the flexible polyvinylidene fluoride film, and based on the preset piezoelectric effect strain-charge constitutive equation, the charge output of each electrode configuration within a preset frequency range is calculated; the charge output of each electrode configuration is compared, and based on... Based on the comparison of charge output, the piezoelectric response characteristics of each electrode configuration are obtained, and the electrode configuration with the optimal piezoelectric response characteristics is determined. The curves of charge output versus frequency for each electrode configuration are obtained through frequency sweep simulation. Using the charge output at a preset center frequency as a benchmark, the relative output amplitude at each frequency point is calculated to determine the effective bandwidth of each electrode configuration. The time-domain response waveforms of each electrode configuration are obtained through impulse response simulation to determine the waveform rise time of each electrode configuration. Based on the comparison of effective bandwidth and waveform rise time, the electrode configuration with the optimal frequency response characteristics is determined. Combining the simulation results of piezoelectric response characteristics and frequency response characteristics, the gradient-width double-finger coplanar rectangular electrode is selected as the optimal electrode configuration. The optimal width-to-width ratio of the gradient-width double-finger coplanar rectangular electrode is determined.

[0058] In this optional embodiment, determining the optimal width-to-spacing ratio of the gradient-width double-finger coplanar rectangular electrode includes: keeping the total length of the gradient-width double-finger coplanar rectangular electrode constant, and setting multiple width-to-spacing ratios; the width-to-spacing ratio represents the ratio of the width of a single finger in the gradient-width double-finger coplanar rectangular electrode to the spacing between the two fingers; based on the current width-to-spacing ratio, applying a normal harmonic displacement load to the back surface of the flexible polyvinylidene fluoride film to simulate ultrasonic vibration, coupling the solid mechanical physical field and the piezoelectric effect physical field, and performing frequency sweeping within a preset frequency band with a preset step size; based on each frequency point, solving for the three-dimensional strain tensor inside the flexible polyvinylidene fluoride film, and based on the preset... The piezoelectric strain-charge constitutive equation, combined with the three-dimensional strain tensor, is used to calculate the electric displacement vector distribution within the flexible polyvinylidene fluoride film. The normal components of the electric displacement vectors in the two finger-covered regions of the gradient-width double-finger coplanar rectangular electrode are then integrally applied to their respective areas. The sum of these two area integrals yields the total charge output of the gradient-width double-finger coplanar rectangular electrode at that frequency. The arithmetic mean of the total charge output at all frequencies within a preset frequency band is taken as the average charge output under the current width-to-spacing ratio. The average charge output under each width-to-spacing ratio is compared, and the optimal width-to-spacing ratio for the gradient-width double-finger coplanar rectangular electrode is determined based on the comparison results.

[0059] In this optional embodiment, a piezoelectric vibration model of the flexible polyvinylidene fluoride (PVDF) film is established to analyze the influence of the length and width of the flexible PVDF film on sensitivity and frequency response. The optimal shape and size of the flexible PVDF film are determined by: establishing a piezoelectric vibration model of the flexible PVDF film based on a preset piezoelectric effect strain-charge constitutive equation; setting the boundary conditions of the piezoelectric vibration model to have the back of the flexible PVDF film bound to the GIS shell via an acoustic coupling layer, and the front as a free boundary; pre-setting multiple different flexible PVDF film lengths, calculating the average sensitivity of the sensor within a preset frequency band for different flexible PVDF film lengths, and determining the optimal length range based on the trend of average sensitivity with length; pre-setting multiple different flexible PVDF film widths, calculating the average sensitivity and effective bandwidth of the sensor within a preset frequency band for different flexible PVDF film widths, and determining the optimal width range based on the trends of average sensitivity and effective bandwidth with width; and comprehensively considering average sensitivity, effective bandwidth, and ease of installation to determine the optimal shape and size of the flexible PVDF film.

[0060] In this optional embodiment, multiple different flexible polyvinylidene fluoride (PVDF) film lengths are preset, and the average sensitivity of the sensor within a preset frequency band is calculated for different flexible PVDF film lengths. Based on the trend of average sensitivity variation with length, the optimal length range is determined, including: keeping the width and thickness of the flexible PVDF film constant, and setting multiple different flexible PVDF film lengths; applying a normal harmonic displacement load of a preset frequency band to the center position of the inner wall of the GIS shell at the current flexible PVDF film length to simulate ultrasonic longitudinal waves excited by partial discharge, coupling the solid mechanical physical field with the piezoelectric effect physical field, and performing frequency sweeping within the preset frequency band with a preset step size; based on each frequency point, the three-dimensional strain tensor inside the flexible PVDF film is obtained; based on the preset piezoelectric effect strain-charge constitutive equation, combined with the three-dimensional strain tensor, the flexible PVDF film... The electric displacement vector distribution within the membrane is analyzed, and the normal component of the electric displacement vector over the area covered by the gradient-width double-finger coplanar rectangular electrode is integrally obtained to yield the total charge of the gradient-width double-finger coplanar rectangular electrode at the specified frequency. Based on the definition of capacitance, the output voltage of the sensor at the specified frequency is calculated using the total charge. The input vibration velocity at the specified frequency is calculated based on the relationship between simple harmonic vibration velocity and displacement. The sensitivity of the sensor at the specified frequency is determined based on the ratio of the output voltage to the input vibration velocity. The calculation of output voltage and input vibration velocity is repeated to obtain the sensitivity of all frequency points within a preset frequency band. The arithmetic mean of the sensitivities at all frequency points is taken as the average sensitivity for the length of the flexible polyvinylidene fluoride film. The average sensitivities for each length of the flexible polyvinylidene fluoride film are compared, and the optimal length range is determined based on the trend of the average sensitivity with length obtained from the comparison.

[0061] Figure 2 An embodiment of the GIS partial discharge sensor of the present invention is shown.

[0062] In this optional embodiment, the GIS partial discharge sensor includes, from the inside out, an acoustic coupling layer, a flexible polyvinylidene fluoride (PVDF) sensing unit, an electrode structure, a pre-bending shaping layer, an encapsulation protective layer, and an electromagnetic shielding layer, stacked sequentially. The acoustic coupling layer is attached to the surface of the GIS housing to reduce the reflection loss of ultrasonic signals at the interface between the GIS housing and the sensor, and to transmit the mechanical vibration of the GIS housing to the flexible PVDF sensing unit without attenuation. The flexible PVDF sensing unit is disposed on the back side of the acoustic coupling layer to receive the ultrasonic signals excited by the GIS partial discharge and generate mechanical vibrations, which are then transmitted to the flexible PVDF sensing film through the positive piezoelectric effect. The lower surface generates polarization charge; the electrode structure is located on the front of the flexible polyvinylidene fluoride sensing unit and is a gradient-width double-fin coplanar rectangular electrode used to collect polarization charge and output electrical signal; the pre-bending shaping layer is located between the electrode structure and the encapsulation protective layer to pre-bend the sensor into a shape that matches the curvature of the GIS housing surface, eliminating bubbles and stress concentrations generated when the sensor is attached to the curved GIS housing; the encapsulation protective layer covers the pre-bending shaping layer and the non-electrode area on the front of the flexible polyvinylidene fluoride sensing unit to protect the electrodes from oxidation and mechanical damage; the electromagnetic shielding layer covers the outer surface of the encapsulation protective layer to suppress electromagnetic interference.

[0063] In this optional embodiment, the flexible polyvinylidene fluoride sensing unit has a thickness of 400 μm, a length of 9 cm, and a width of 1 cm; the acoustic coupling layer is a silicone grease material with a thickness of 80 μm; the pre-bending shaping layer is a polyterephthalic acid plastic film with a thickness of 50 μm, pre-bent into an arc that matches the standard GIS housing; the encapsulation protective layer is an epoxy resin material with a thickness of 50 μm; and the electromagnetic shielding layer is an aluminum foil material with a thickness of 25 μm.

[0064] Figure 3 An embodiment of the GIS partial discharge detection system of the present invention is shown.

[0065] In this optional embodiment, the GIS partial discharge detection system includes:

[0066] The signal conditioning module 201 is used to perform impedance matching, amplification and filtering on the weak analog electrical signal output by the sensor to obtain the processed analog voltage signal.

[0067] Data acquisition module 202 is used to convert the processed analog voltage signal into a digital signal;

[0068] The processing module 203 is used to perform time-frequency domain analysis and feature extraction on digital signals to identify the type and severity of partial discharge in GIS, so as to achieve fault early warning.

[0069] In this optional embodiment, the weak analog electrical signal output by the sensor is impedance matched, amplified, and filtered to obtain a processed analog voltage signal. This includes: using a 50-ohm coaxial impedance matching device as the signal input stage, connecting it to the sensor output terminal via a coaxial snap-fit ​​interface, and matching the sensor's own 50-ohm output impedance to eliminate reflection loss during signal transmission; using a low-noise charge amplifier with input noise meeting the standard of less than 5 nanovolts per square hertz as the core amplification unit, configuring a 100-picofarad feedback capacitor and a 1,000-megaohm feedback resistor, adjusting the gain of the low-noise charge amplifier to 45 dB, and simultaneously converting and amplifying the weak analog electrical signal at the microvolt level output by the sensor to a volt-level analog voltage signal; using an eighth-order Butterworth programmable bandpass filter as the output stage, setting the corresponding passband and suppression index, filtering out various irrelevant interference signals, retaining the effective frequency band of the GIS partial discharge ultrasonic signal, and outputting the processed analog voltage signal.

[0070] In this optional embodiment, converting the processed analog voltage signal into a digital signal includes: using a high-speed synchronous data acquisition card with a 16-bit resolution and a sampling rate of millions of times per second, connecting to the output of the signal conditioning module 201 via a shielded coaxial cable, and completely restoring the ultrasonic signal according to the Nyquist sampling theorem; acquiring the analog voltage signal through the sample-and-hold circuit inside the high-speed synchronous data acquisition card and maintaining the stability of the sampled value, and using a 16-bit analog-to-digital converter to convert the analog voltage signal in the range of -5V to +5V into digital code, controlling the quantization error within a preset range to ensure the accuracy of weak signal acquisition; storing the digital code generated by the analog-to-digital conversion into the built-in high-speed cache of the acquisition card, and transmitting the digital signal to the processing module 203 through a third-generation universal serial bus interface.

[0071] In this optional embodiment, time-frequency domain analysis and feature extraction of digital signals are performed to identify the type and severity of GIS partial discharge in order to achieve fault early warning. This includes: performing wavelet threshold denoising and normalization on the digital signals to obtain processed digital signals; extracting time-domain and frequency-domain features from the processed digital signals, and simultaneously acquiring the power grid voltage signal and ultrasonic signal for phase correlation to construct an ultrasonic partial discharge phase distribution map; inputting the time-domain features, frequency-domain features, and ultrasonic partial discharge phase distribution map into a time-frequency-map cross-dimensional attention fusion network for identification, outputting the defect classification probability and discharge regression value, and determining the defect type and discharge severity; and performing graded fault early warning based on the defect type and discharge severity, combined with a preset signal-to-noise ratio threshold.

[0072] In this optional embodiment, wavelet threshold denoising and normalization are performed on the digital signal to obtain the processed digital signal, including: segmenting the acquired digital signal into sliding windows of a preset window size, with adjacent windows overlapping at a preset overlap rate; performing wavelet decomposition on the signal within each window to obtain detail coefficients and low-frequency approximation coefficients at each level; calculating adaptive thresholds for each level of detail coefficients and performing threshold shrinkage processing, while retaining the low-frequency approximation coefficients unchanged; reconstructing the signal of each window through inverse wavelet transform to obtain the denoised digital signal, and extracting the maximum and minimum amplitude values ​​of the denoised signal within each window; using a linear normalization method based on the maximum and minimum amplitude values ​​of each window to map the amplitude of each sampling point within the window to a preset interval point by point; when the signal within the window is all-zero background noise, directly setting the normalized amplitude of all sampling points in that window to zero; and performing normalization operations on all sliding windows to obtain a globally normalized continuous signal sequence.

[0073] In this optional embodiment, time-domain and frequency-domain features are extracted from the processed digital signal, and the power grid voltage signal and ultrasonic signal are simultaneously acquired and phase-correlated to construct an ultrasonic partial discharge phase distribution map. This includes: performing statistical analysis on each normalized sliding window signal to extract peak value, RMS value, kurtosis, margin factor, and impulse factor; where the peak value is the maximum absolute value of the signal within the window, the RMS value is the root mean square value of the signal within the window, the kurtosis is the normalized fourth-order statistic of the signal within the window, the margin factor is the ratio of the peak value to the root mean square amplitude of the signal, and the impulse factor is the ratio of the peak value to the RMS value; a Hanning window is applied to each denoised sliding window signal to suppress spectral leakage, and a fast Fourier transform is performed to obtain a bilateral spectrum, from which the bilateral spectrum is extracted. The first few points of the side spectrum are converted into a single-sided spectrum with amplitude normalized to a preset interval. The dominant frequency, spectral centroid, spectral bandwidth, and energy entropy are extracted from the single-sided spectrum. The dominant frequency is the frequency corresponding to the maximum amplitude in the single-sided spectrum, the spectral centroid is the weighted average of the spectral amplitude and the corresponding frequency, the spectral bandwidth is the difference between the upper and lower limit frequencies corresponding to the effective bandwidth of the dominant frequency amplitude in the single-sided spectrum, and the energy entropy is the entropy value calculated based on the energy ratio of each sub-band after dividing the preset detection frequency band into several equal-width sub-bands. The power grid voltage signal is collected synchronously, and the ultrasonic signal is phase-correlated with the power grid voltage signal. Based on the ultrasonic signal amplitude and its corresponding power frequency phase in each power frequency cycle, an ultrasonic partial discharge phase distribution map is constructed.

[0074] To facilitate understanding of the above technical solutions of the present invention, the following further explains the above technical solutions of the present invention from the perspective of architecture and principle, as follows:

[0075] In a first aspect, the present invention provides a GIS partial discharge sensor based on a flexible PVDF thin film, comprising, from the inside out, an acoustic coupling layer, a flexible PVDF sensing unit, an electrode structure, a pre-bending shaping layer, an encapsulation protective layer, and an electromagnetic shielding layer:

[0076] (1) An acoustic coupling layer is attached to the surface of the GIS shell. The silicone grease material with a thickness of 80μm is used to reduce the reflection loss of ultrasonic signals at the interface between the shell and the sensor, and to transmit the mechanical vibration of the GIS shell to the flexible PVDF sensitive unit without attenuation.

[0077] (2) The flexible PVDF film, as the sensitive unit, is the core sensitive element. An acoustic coupling layer is attached to its back to receive the ultrasonic signal excited by the partial discharge of GIS and generate mechanical vibration. The flexible PVDF film has a thickness of 400μm, a length of 9cm, and a width of 1cm. These dimensions are precisely matched with the wavelength range (6.25cm-25cm) of the ultrasonic signal of partial discharge of GIS in the aluminum alloy shell, which can achieve resonance enhancement.

[0078] (3) The electrode structure is located on the front side of the flexible PVDF film (the side away from the GIS shell). It is a gradient-width, double-finger, coplanar rectangular electrode. The electrode width increases linearly from 8 mm to 12 mm from the end closest to the center of the GIS cavity to the end furthest from the center of the cavity, while the electrode spacing remains constant at 10 mm. This design matches the distribution characteristics of the ultrasonic vibration amplitude on the surface of the GIS shell, which gradually decreases from the center to the edge, thus making the charge output of each segment of the electrode uniform. The overall sensitivity is 6.8% higher than that of a uniform-width electrode. The specific charge collection and output process is as follows: 1) Vibration transmission and piezoelectric polarization: The longitudinal wave excited by the partial discharge of GIS is transmitted to the flexible PVDF film (i.e., flexible polyvinylidene fluoride film) through the aluminum alloy shell and acoustic coupling layer, causing the film to undergo periodic deformation along the thickness direction; 2) Due to the positive piezoelectric effect of PVDF material, the dipoles inside the film are oriented with deformation, generating equal amounts of polarized charges of opposite signs on the upper and lower surfaces of the film; 3) Electric field distribution and charge collection: The coplanar rectangular electrodes of the two fingers form a uniform transverse electric field distribution inside the PVDF film, and the 1:1 wide spacing ratio maximizes the piezoelectric activity of the electrode coverage area; 4) The polarized charges on the upper surface of the film are collected by the two parallel finger electrodes respectively, forming a potential difference; 5) Electrical signal output: The two finger electrodes are connected to the subsequent signal conditioning module 201 through welded leads, which converts the collected charge signal into a measurable voltage signal for output.

[0079] (4) A pre-bent shaping layer is set between the electrode structure and the encapsulation protective layer. It is a 50μm thick PET film (i.e., polyethylene terephthalate plastic film) and is pre-bent into an arc that perfectly matches the 126kV GIS standard shell (radius of curvature R=250mm). This solves the problems of air bubbles and stress concentration that occur when existing PVDF sensors are bonded to curved shells, and further reduces acoustic coupling loss to below 10%.

[0080] (5) The encapsulation protective layer covers the non-electrode area on the front side of the pre-bent shaping layer and the PVDF film. It is an epoxy resin material with a thickness of 50 μm, used to protect the electrode from oxidation and mechanical damage.

[0081] (6) An electromagnetic shielding layer covers the outer surface of the encapsulation protective layer. It is made of aluminum foil with a thickness of 25 μm and is used to suppress electromagnetic interference on site.

[0082] (7) The sensor is placed on the edge area of ​​the GIS cover plate, with its long side pointing towards the center of the GIS cavity. This arrangement makes the average amplitude of the ultrasonic signal 32% higher than that in the central area, and the output voltage 45% higher than that when it is pointed vertically.

[0083] Secondly, the present invention provides a GIS partial discharge detection system, including an ultrasonic sensor (i.e., a flexible PVDF thin film ultrasonic sensor), a signal conditioning module 201, a data acquisition module 202, and a processing module 203.

[0084] (1) Signal conditioning module 201, used for impedance matching, amplification and filtering of the weak electrical signal output by the sensor, specifically including:

[0085] 1) Impedance matching: A 50Ω coaxial impedance matching circuit is used as the input stage and directly connected to the sensor output via a BNC interface. Since the output impedance of the PVDF sensor with dual-finger coplanar electrodes of this invention is approximately 50Ω, impedance matching can eliminate reflection loss during signal transmission, ensuring that more than 95% of the charge signal can be transmitted to subsequent circuits without attenuation, thus solving the signal attenuation problem caused by the high output impedance of traditional PVDF sensors.

[0086] 2) Low-noise charge amplification: A low-noise charge amplifier with input noise ≤5nV / √Hz is used as the core amplification unit to convert the weak charge signal output by the sensor into a voltage signal. The feedback capacitor of the charge amplifier is set to 100pF, the feedback resistor is set to 1GΩ, and the gain is adjustable from 20-60dB (45dB in this invention), which can amplify the original signal at the μV level to the V level, meeting the range requirements of subsequent data acquisition.

[0087] 3) Programmable bandpass filter: An 8th-order Butterworth programmable bandpass filter is used as the output stage, with the cutoff frequency precisely set to 20kHz and 80kHz (i.e., the passband range), and the out-of-band rejection ratio ≥60dB (i.e., the rejection index). This filter can effectively filter out 50Hz power frequency and its harmonics, mechanical vibration interference below 10kHz, and high-frequency electromagnetic interference above 80kHz, retaining only the effective frequency band of GIS partial discharge ultrasonic signals.

[0088] (2) Data acquisition module 202: The data acquisition module 202 is used to convert the analog voltage signal processed by the signal conditioning module 201 into a digital signal. The specific implementation steps are as follows:

[0089] 1) Signal Input and Synchronous Sampling: A high-speed synchronous data acquisition card with 16-bit resolution and a sampling rate of 1 MS / s (millions of samples per second) is used. Its analog input channel is connected to the output of the signal conditioning module 201 via a shielded coaxial cable. According to the Nyquist sampling theorem, a sampling rate of 1 MS / s can completely reproduce ultrasonic signals up to 80 kHz. The multi-channel synchronous sampling function supports simultaneous acquisition from multiple sensors, meeting the needs of distributed monitoring at multiple measurement points in GIS.

[0090] 2) Sample and Hold & Quantization Encoding: The sample and hold circuit inside the data acquisition card accurately samples the input analog voltage signal and keeps the sampled value stable until quantization is complete; the 16-bit ADC quantizes the analog voltage signal into a digital code of 0-65535, corresponding to a voltage range of -5V to +5V, with a quantization error of less than 0.15mV (i.e., within the preset range), ensuring the acquisition accuracy of weak signals.

[0091] 3) Data transmission and caching: The acquired digital signals are transmitted to the processing module via a USB 3.0 high-speed interface with a transmission rate of up to 5Gbps, enabling continuous and uninterrupted data acquisition; the acquisition card has a built-in 128MB high-speed cache to avoid data loss during transmission and ensure data integrity.

[0092] (3) Processing Module: The processing module is used to perform time-frequency domain analysis and feature extraction on the digital signal output by the data acquisition module, identify the type and severity of partial discharge, and realize fault early warning. This invention adopts a time-frequency-spectrum cross-dimensional attention fusion network (TF-IAFNet) identification scheme, and the specific implementation steps are as follows:

[0093] 1) Digital signal preprocessing: The acquired raw digital signal is subjected to sliding window denoising processing, using a 4-level decomposition based on the db4 wavelet basis and an improved semi-soft thresholding function (threshold adjustment coefficient). ) and SURE adaptive threshold estimation (interlayer adjustment coefficient) , , , The wavelet thresholding denoising algorithm first divides the original signal into segments using a 1024-point sliding window (with a 50% overlap between adjacent windows). Then, it performs a 4-level wavelet decomposition on each segment to obtain detail coefficients and low-frequency approximation coefficients. Adaptive thresholds are calculated for the detail coefficients of levels 1-4, and threshold shrinking is performed while retaining the low-frequency approximation coefficients. The denoised signal is then reconstructed using inverse wavelet transform to remove residual background noise. The window size is set to 1024 points with a 50% overlap. The denoised signal is then normalized. The specific processing steps are: 1) Extracting the maximum amplitude of the denoised signal within the current 1024-point sliding window. and minimum amplitude ;2) Adopt - Linear normalization method, according to the formula ; For the first in the window Amplitude of each sampling point Perform point-by-point transformation; 3) When the signal within the window is all-zero background noise (i.e. When ), directly set the normalized amplitude of all sampling points in the window to 0; 4) Repeat the above operation for all sliding windows to obtain a globally normalized continuous signal sequence. Map the signal amplitude to the [0, 1] interval to eliminate the influence of the gain difference between different sensors.

[0094] 2) Time-domain feature extraction: Statistical analysis is performed on each normalized 1024-point sliding window signal to extract five time-domain statistical features that reflect the intensity and impact characteristics of partial discharge signals: peak value, effective value, kurtosis, margin factor, and impulse factor. These features provide a time-domain basis for subsequent defect identification. The normalized signal sequence within the current sliding window is defined as follows: ( =1,2,…,1024), where The sampling point number, For the first The normalized amplitude of each sampling point, with the peak value being the maximum absolute value of the signal, is calculated using the following formula: It reflects the maximum intensity of a single partial discharge; the effective value is the root mean square value of the signal within the window, calculated using the following formula: It reflects the average energy level of the partial discharge signal; kurtosis is the normalized fourth-order statistic of the signal within the window, calculated using the following formula: It reflects the impulsiveness of the signal and has high sensitivity to early, weak discharges; the margin factor is the ratio of the peak value to the root square amplitude of the signal, calculated using the following formula: It is a dimensionless index, extremely sensitive to signal impulse components and unaffected by sensor gain and overall signal amplitude drift; the impulse factor is the ratio of peak value to RMS value, calculated using the following formula: Reflecting the impact degree of the signal, the pulse factor of the partial discharge signal is much higher than that of the steady mechanical vibration and electromagnetic interference signal. The five time-domain features extracted from each sliding window, together with the subsequently extracted frequency-domain features and the ultrasonic PRPD map, are input into the convolutional neural network model (i.e., the time-frequency-map cross-dimensional attention fusion network) to identify the type and severity of partial discharge defects.

[0095] 3) Frequency Domain Feature Extraction: Fast Fourier Transform (FFT) is performed on each denoised 1024-point sliding window signal to extract four frequency domain features reflecting the frequency distribution characteristics of the partial discharge signal: dominant frequency, spectral centroid, spectral bandwidth, and energy entropy. These features provide a frequency domain basis for subsequent defect identification. A Hanning window is first applied to the signal within the current window to suppress spectral leakage. Then, a 1024-point FFT operation is performed to obtain a two-sided spectrum. The first 512 points are converted into a one-sided spectrum with amplitude normalized to the [0, 1] interval, corresponding to a frequency resolution of 976.56Hz (calculated from the system's 1MS / s sampling rate and the 1024-point window length). The dominant frequency is the frequency corresponding to the maximum amplitude in the one-sided spectrum, reflecting the main energy concentration frequency of the partial discharge signal. The spectral centroid is the weighted average of the spectral amplitude and the corresponding frequency, calculated using the following formula: ,in, For the centroid of the spectrum, For the first Frequency values ​​at each frequency point The spectral amplitude at the corresponding frequency point comprehensively reflects the overall frequency distribution of the signal; the spectral bandwidth is the difference between the upper and lower limit frequencies corresponding to the amplitude dropping to -6dB of the main frequency amplitude in a single-sided spectrum, reflecting the width of the signal's frequency distribution; the energy entropy is the degree of disorder in the energy distribution of each frequency sub-band. The key detection frequency band of this application, 20kHz-80kHz (i.e., the preset detection frequency band), is divided into 12 equal-width sub-bands, and the proportion of energy in each sub-band to the total energy of that frequency band is calculated. According to the formula Calculate energy entropy ( Energy entropy Taking the logarithm (where m represents the sub-band), reflecting the complexity of the signal frequency distribution, the energy entropy of different types of partial discharges varies significantly. The four frequency domain features extracted from each sliding window, together with the aforementioned time domain features and the ultrasonic PRPD map, are input into a dedicated convolutional neural network model to identify the type and severity of partial discharge defects.

[0096] 4) PRPD map construction: The power frequency voltage signal of the power grid is acquired synchronously, and the ultrasonic signal is correlated with the power frequency voltage to construct an ultrasonic PRPD map with a size of 128×72 (amplitude range -20dB-80dB, phase range 0-360°, phase interval 5°).

[0097] (4) Time-frequency-map cross-dimensional attention fusion network recognition: The 9-dimensional time-frequency domain features are input into two fully connected layers (64-32 neurons, ReLU activation) and output 32-dimensional time-frequency high-level features; the 128×72 PRPD map is sequentially passed through three convolutional layers (3×3×16-3×3×32-3×3×64, stride 1, ReLU activation) and two max pooling layers (2×2, stride 2) and outputs a 64×36×64 feature map; the 32-dimensional time-frequency feature vector is converted into a 64-dimensional weight vector through the fully connected layer, and after Sigmoid normalization, it is multiplied by the 64 feature channels of the map convolution branch in a channel-by-channel weighted manner to realize the adaptive guidance of time-frequency features to map features; the fused features are passed through the Flatten layer and the fully connected layer (64 neurons) and then simultaneously input into two output layers: the Softmax layer outputs the classification probability of 3 types of defects, and the linear layer outputs the 0-1000pC discharge regression value.

[0098] (5) Graded fault early warning: Based on the defect identification results and severity, a three-level early warning mechanism is implemented:

[0099] 1) Level 1 warning (minor discharge): Signal-to-noise ratio ≥10dB, the system displays a yellow warning, and the trend curve is updated hourly.

[0100] 2) Level 2 warning (moderate discharge): When the signal-to-noise ratio is ≥15dB, the system displays an orange warning, issues an audible and visual alarm, and pushes it to the maintenance personnel.

[0101] 3) Level 3 warning (severe discharge): When the signal-to-noise ratio is ≥20dB, the system displays a red warning, provides continuous audible and visual alarms, and uploads the information to the power grid monitoring platform.

[0102] Thirdly, the present invention provides an optimized design method for a GIS partial discharge sensor based on a flexible PVDF thin film, comprising the following steps:

[0103] I. Analysis of Ultrasonic Propagation Characteristics on GIS Shell Surface and Optimization of Sensor Layout:

[0104] A multi-physics coupled finite element model of the GIS shell-coupling layer-sensor is established to analyze the propagation characteristics of ultrasonic signals on the surface of the GIS shell within the 20kHz-80kHz frequency band (i.e., the preset ultrasonic signal frequency band). The optimal placement and installation direction of the sensor are determined. The specific implementation steps are as follows:

[0105] (1) Construction of multiphysics coupling model: A three-dimensional finite element model was established using multiphysics simulation software (e.g., COMSOL Multiphysics 6.1 software). The model consists of three parts: GIS shell: made of 6061 aluminum alloy, with a diameter of 500 mm and a thickness of 10 mm (corresponding to the standard size of 126kV GIS). Solid mechanical physics field was set, and the material parameters were: density 2700 kg / m³, Young's modulus 70 GPa, Poisson's ratio 0.33, longitudinal wave velocity 5000 m / s; Acoustic coupling layer: made of silicone grease, with a thickness of 80 μm. Acoustic physics field was set, and the material parameters were: density 970 kg / m³, sound velocity 1450 m / s, acoustic impedance PVDF sensor: Utilizing the basic structural parameters of this invention, a piezoelectric effect physical field is set, and the material parameters are: piezoelectric constant. dielectric constant Loss tangent .

[0106] (2) Boundary conditions and load settings: A broadband ultrasonic longitudinal wave load of 20kHz-80kHz (simulating ultrasonic waves excited by partial discharge) is applied at the center of the inner wall of the GIS shell, and the load amplitude is set to 1μm; a low reflection boundary condition is set at the outer edge of the GIS shell to simulate the ultrasonic propagation characteristics of an infinitely long shell; a binding contact is set between the sensor and the coupling layer, and between the coupling layer and the shell to ensure that the vibration is transmitted without slippage.

[0107] (3) Optimization analysis of the arrangement location: Ten monitoring points were set radially on the outer surface of the GIS shell, located at the center, 50mm, 100mm, 150mm, 200mm, and 250mm (edge ​​of the cover plate) from the center. The average vibration amplitude of each monitoring point in the 20kHz-80kHz frequency band was calculated. Simulation results show that the average amplitude of the ultrasonic signal in the edge area of ​​the cover plate (250mm from the center) is 32% higher than that in the center area, and the signal attenuation is the smallest. Therefore, the edge area of ​​the GIS cover plate surface is determined to be the optimal arrangement location.

[0108] (4) Installation direction optimization analysis: Five installation directions of 0°, 30°, 45°, 60° and 90° were set at the optimal arrangement position (0° means the long side points to the center of the cavity, and 90° means the long side is perpendicular to the center of the cavity). The output voltage of the sensor under different directions was calculated. Based on the piezoelectric effect strain-charge constitutive equation, the numerical solution was performed in the GIS shell-coupled layer-sensor multiphysics field coupled finite element model established by COMSOL Multiphysics 6.1 software. First, a broadband ultrasonic longitudinal wave load of 20kHz-80kHz and amplitude of 1μm was applied at the center of the inner wall of the GIS shell to simulate the ultrasonic waves excited by partial discharge. The solid mechanics and piezoelectric effect physical fields were coupled to obtain the three-dimensional strain distribution inside the PVDF film when the long side of the sensor points to the directions of 0°, 30°, 45°, 60° and 90° respectively. Then, based on the piezoelectric constitutive equation Calculate the electric displacement vector distribution within the thin film (where...) The piezoelectric stress constant matrix is... For strain tensor, Here is the dielectric constant matrix. (where the electric field strength is 1), the total charge collected on the two finger electrodes is obtained by integrating the normal component of the electric displacement vector of the region covered by the coplanar rectangular electrodes. According to the definition of capacitance Calculate the output voltage of the sensor (where) The equivalent capacitance formed by the dual-finger electrode and the PVDF film is calculated from the electrode size, film dielectric constant and thickness. Finally, the average output voltage of the sensor in the 20kHz-80kHz frequency band under different mounting orientations is obtained.

[0109] Simulation results show that when the long side of the sensor points towards the center of the cavity (0° direction), the output voltage is 45% higher than when it points perpendicularly (90° direction). This is because the ultrasonic waves excited by partial discharge in GIS mainly propagate along the axial direction of the shell in the form of longitudinal waves. This installation direction allows the vibration direction of the thin film to be consistent with the ultrasonic propagation direction, maximizing the piezoelectric response. Therefore, pointing the long side of the sensor towards the center of the GIS cavity is determined to be the optimal installation direction.

[0110] II. Electrode Configuration Simulation Comparison and Parameter Optimization:

[0111] Three electrode configurations were designed: single-finger, gradient double-finger, and interdigitated electrode. The piezoelectric response and frequency response characteristics of the different electrodes were compared through simulation. The specific implementation steps are as follows:

[0112] (1) Modeling of three electrode configurations: Keeping the PVDF film size (9cm×1cm×400μm) and the total electrode area (3cm²) unchanged, finite element models of three types of electrodes are established respectively: Single finger strip electrode: a single rectangular electrode with a size of 3cm×1cm, centrally arranged on the film surface; Gradient double finger strip electrode: two parallel rectangular strips with a total length of 3cm and a width of 1cm, and the strip width and spacing are equal; Interdigitated electrode: 10 pairs of interdigitated electrodes with a strip width of 0.5mm, a spacing of 0.5mm, and a total size of 3cm×1cm.

[0113] (2) Simulation of piezoelectric response characteristics: A normal displacement load of 1 μm was applied to the back of the PVDF film (simulating ultrasonic vibration), and the charge output of the three electrodes in the frequency range of 1 kHz-100 kHz was calculated. Based on the piezoelectric effect strain-charge constitutive equation, the PVDF film size (9 cm × 1 cm × 400 μm) and the total electrode area (3 cm²) were kept constant in COMSOL Multiphysics 6.1 software. Finite element models of single-finger strip, double-finger strip, and interdigitated electrode configurations were established respectively. A normal harmonic displacement load of 1 μm amplitude was applied to the back of the PVDF film to simulate ultrasonic vibration. The frequency sweep numerical solution was performed by coupling solid mechanics and piezoelectric effect physical field. The frequency sweep range was 1 kHz-100 kHz and the step size was 1 kHz. The three-dimensional strain tensor inside the PVDF film was obtained first at each frequency point. Based on the piezoelectric constitutive equation (in the formula) The piezoelectric stress constant matrix is... Here is the dielectric constant matrix. Calculate the electric displacement vector D distribution within the thin film (to represent the electric field strength), and perform area integration on the normal component of the electric displacement vector within the corresponding electrode coverage area. The total charge collected on the electrode is obtained. In the formula, the double integral symbol is... This represents the area integral over the electrode contact region. Normal to the electrode surface For differential operators, This represents a tiny area element.

[0114] Simulation results show that the average charge output of the single-finger electrode is 12.5 pC; the average charge output of the double-finger electrode is 16.0 pC, which is 28% higher than that of the single-finger electrode; and the average charge output of the interdigitated electrode is 13.9 pC, which is 15% lower than that of the double-finger electrode.

[0115] (3) Frequency response simulation: The -6dB bandwidth (i.e., effective bandwidth) and waveform rise time of the three electrodes were calculated. Based on the finite element models of the three electrode configurations established by COMSOL Multiphysics 6.1 software, the two indicators were calculated by frequency sweep simulation and impulse response simulation respectively. When calculating the -6dB bandwidth (i.e., effective bandwidth), the size of the PVDF film and the total area of ​​the electrodes were kept constant. A normal harmonic displacement load with an amplitude of 1μm was applied to the back of the film. The frequency sweep solution was performed by coupling solid mechanics and piezoelectric effect physical fields from 1kHz to 100kHz with a step size of 1kHz to obtain the curve of charge output of each electrode as a function of frequency. The charge output at 40kHz (the center frequency of the GIS partial discharge ultrasonic signal) was used as the basis for the calculation. Based on the formula Calculate the relative output amplitude at each frequency point Find the lower limit frequency at which the relative output amplitude drops to -6dB. and upper limit frequency The difference between the two This is the -6dB bandwidth (effective bandwidth) of the electrode. For waveform rise time calculation, a narrow pulse normal displacement load with a rise time less than 1μs and a half-width at half-maximum (FWHM) less than 2μs is applied to the back of the thin film. The time-domain response waveform of the electrode charge output is obtained by solving for the time. The moment corresponding to 10% of the waveform peak value is extracted. The time corresponding to 90% The time difference between the two This refers to the waveform rise time of the electrode. The -6dB bandwidth and waveform rise time of the three electrodes are then used for performance comparison. The representative frequency is The simulation results show that the -6dB bandwidth of the single-finger electrode is 15kHz-75kHz, with a rise time of 2.5μs; the -6dB bandwidth of the double-finger electrode is 18kHz-82kHz, with a rise time of 1.8μs; and the -6dB bandwidth of the interdigitated electrode is 20kHz-78kHz, with a rise time of 2.1μs.

[0116] (4) Selection of optimal electrode configuration: After comprehensively comparing charge output efficiency and frequency response characteristics, the double-finger strip electrode performs best in both sensitivity and bandwidth, and has a simple structure and is easy to prepare. Therefore, the double-finger strip rectangular electrode is selected as the optimal configuration.

[0117] (5) Electrode width-to-spacing ratio optimization: Keeping the total electrode length constant at 3cm, four cases were set with width-to-spacing ratios of 0.5:1, 1:1, 1.5:1, and 2:1, respectively, and the charge output under different width-to-spacing ratios was calculated - based on COMSOL. A finite element model of a coplanar rectangular electrode with two fingers was established using Multiphysics 6.1 software. Maintaining a total electrode length of 3 cm, PVDF film dimensions (9 cm × 1 cm × 400 μm), and other structural parameters, four working conditions were set with width-to-spacing ratios of 0.5:1, 1:1, 1.5:1, and 2:1 (corresponding to electrode widths and spacings of 5 mm and 10 mm, 10 mm and 10 mm, 15 mm and 10 mm, and 20 mm and 10 mm, respectively). A normal harmonic displacement load with an amplitude of 1 μm was applied to the back of the PVDF film to simulate ultrasonic vibration. A frequency sweep solution of 20 kHz to 80 kHz with a step size of 1 kHz was performed, coupled with solid mechanics and piezoelectric effect physics. At each frequency point, the three-dimensional strain tensor S inside the PVDF film was first obtained, and then the piezoelectric constitutive equation was used to solve the problem. (in the formula) The piezoelectric stress constant matrix is... Here is the dielectric constant matrix. Calculate the electric displacement vector within the thin film (for electric field strength). Distribution, and area integration of the normal component of the electric displacement vector within the coverage area of ​​the two finger electrodes. The total charge output at the corresponding frequency point under this wide spacing ratio is obtained by summing the values, and the arithmetic mean of the charge output at all frequency points within the 20kHz-80kHz frequency band is taken.

[0118] Simulation results show that when the width-to-spacing ratio is 1:1, the piezoelectric activity of the electrode coverage area is maximized, and the charge output reaches a maximum of 16.0 pC. When the width-to-spacing ratio deviates from 1:1, the charge output decreases. Therefore, an electrode width and electrode spacing of 10 mm (width-to-spacing ratio 1:1) are determined to be the optimal parameters.

[0119] S3: Establishment and Dimension Optimization of Piezoelectric Vibration Model for PVDF Thin Films

[0120] A piezoelectric vibration model of a PVDF thin film was established to analyze the influence of film length and width on sensitivity and frequency response, and to determine the optimal shape and size of the film. The specific implementation steps are as follows:

[0121] (1) Establishment of piezoelectric vibration model: A free vibration model of PVDF thin film is established based on the strain-charge constitutive equation of the piezoelectric effect. The constitutive equation is as follows: , in, For stress tensor, For strain tensor, It is the electric displacement vector. For electric field strength, Here is the elastic stiffness matrix. The piezoelectric stress constant matrix is... Let be the dielectric constant matrix. The model boundary conditions are set as follows: the back of the film is bound to the GIS shell through a coupling layer, and the front is a free boundary.

[0122] (2) Analysis of the influence of film length: Keeping the film width of 1cm and the thickness of 400μm constant, the lengths of 3cm, 5cm, 7cm, 9cm, 11cm and 13cm were set respectively to calculate the average sensitivity of the sensor in the 20kHz-80kHz frequency band under different lengths. Based on the GIS shell-coupled layer-sensor multiphysics coupled finite element model established by COMSOL Multiphysics 6.1 software, keeping the PVDF film width of 1cm, thickness of 400μm and other structural parameters constant, six working conditions with film lengths of 3cm, 5cm, 7cm, 9cm, 11cm and 13cm were set respectively. A normal harmonic displacement load with an amplitude of 1μm was applied at the center of the inner wall of the GIS shell to simulate the ultrasonic longitudinal wave excited by partial discharge. The frequency sweep solution of 20kHz-80kHz with a step size of 1kHz (i.e., the preset step size) was performed by coupling solid mechanics and piezoelectric effect physical fields. The three-dimensional strain tensor S inside the PVDF film was first solved at each frequency point, and then the piezoelectric constitutive equation was used to solve the problem. Calculate the electric displacement vector within the thin film The total charge is obtained by integrating the surface component of the electric displacement vector normal component over the area covered by the coplanar rectangular electrode with two fingers. According to the definition of capacitance Calculate the sensor's output voltage U(f) at the specified frequency f, and simultaneously determine the relationship between velocity and displacement in simple harmonic motion. (in the formula) (where 1μm is the applied displacement amplitude) Calculate the input vibration velocity at the corresponding frequency point. According to the definition of sensitivity Calculate the sensitivity at this frequency point. The arithmetic mean of the sensitivity values ​​for the 20kHz-80kHz frequency band is taken.

[0123] Simulation results show that when the length increases from 3cm to 9cm, the average sensitivity increases linearly from 54.2dB to 62.4dB. This is because the film length gradually matches the ultrasonic wave length (6.25cm-25cm), achieving resonance enhancement. When the length exceeds 9cm, the increase in sensitivity slows down, and the high-frequency response begins to decay. At the same time, an excessively long film is not conducive to installation in a confined space.

[0124] (3) Analysis of the influence of film width: Keeping the film length of 9cm and thickness of 400μm constant, the widths of 0.5cm, 1cm, 1.5cm, 2cm and 2.5cm were set respectively to calculate the average sensitivity and -6dB bandwidth of the sensor under different widths. Based on the GIS shell-coupled layer-sensor multi-physics coupled finite element model established by COMSOL Multiphysics 6.1 software, keeping the PVDF film length of 9cm, thickness of 400μm and other structural parameters constant, five working conditions with film widths of 0.5cm, 1cm, 1.5cm, 2cm and 2.5cm were set respectively. A normal harmonic displacement load with an amplitude of 1μm was applied at the center of the inner wall of the GIS shell to simulate the ultrasonic longitudinal wave excited by partial discharge. The frequency sweep solution of 20kHz-80kHz with a step size of 1kHz was performed by coupling solid mechanics and piezoelectric effect physical fields. The three-dimensional strain tensor S inside the PVDF film was first solved at each frequency point, and then the piezoelectric constitutive equation was used to solve the problem. (in the formula) The piezoelectric stress constant matrix is... Here is the dielectric constant matrix. Calculate the electric displacement vector within the thin film (for electric field strength). The total charge is obtained by integrating the surface component of the electric displacement vector normal component over the area covered by the coplanar rectangular electrode with two fingers. According to the definition of capacitance Calculate this frequency point The output voltage of the lower sensor Meanwhile, based on the relationship between velocity and displacement in simple harmonic motion... (in the formula) (where 1μm is the applied displacement amplitude) Calculate the input vibration velocity at the corresponding frequency point. According to the definition of sensitivity Calculate the sensitivity at this frequency point. The arithmetic mean of the sensitivity values ​​at all 61 frequency points within the 20kHz-80kHz band was taken to obtain the average sensitivity of the sensor under different film widths; simultaneously, the sensitivity of the sensor at 40kHz (the center frequency of the GIS partial discharge ultrasonic signal) under this width was used as the basis for further analysis. Based on the formula Calculate the relative sensitivity at each frequency point Find the lower limit frequency at which the relative sensitivity drops to -6dB. and upper limit frequency The difference between the two This is the -6dB bandwidth of the sensor at this width.

[0125] Simulation results show that when the width increases from 0.5cm to 1cm, the average sensitivity increases from 58.7dB to 62.4dB, while the -6dB bandwidth remains unchanged at 18kHz-82kHz. When the width exceeds 1cm, the increase in sensitivity is not significant (only 0.3dB), but the -6dB bandwidth begins to narrow (from 82kHz to 75kHz). This is because an excessively wide film will excite higher-order vibration modes, leading to a decrease in high-frequency response.

[0126] (4) Determination of optimal shape and size: Taking into account sensitivity, bandwidth and ease of installation, a narrow rectangle of 9cm×1cm was determined as the optimal shape and size of the film. This size matches the wavelength range of the GIS partial discharge ultrasonic signal well, which can achieve resonance enhancement. At the same time, the narrow shape is convenient for installation in narrow spaces such as the edge of the GIS cover plate and flange gap.

[0127] IV. The influence of film thickness on piezoelectric constant, capacitance and sensitivity was analyzed. Considering the feasibility of the preparation process, 400 μm was selected as the optimal film thickness.

[0128] 5. Prepare a sensor prototype and build a performance testing platform to verify that the average sensitivity of the sensor in the 20kHz-80kHz frequency band is not less than 62.43dB.

[0129] It needs to be explained that, firstly, the fabrication and installation of the sensor, and the overall layered structure of the sensor as follows: Figure 2 As shown, the core electrode structure is as follows Figure 4 As shown, the specific steps are as follows:

[0130] 1) Substrate preparation: Commercially available biaxially oriented PVDF piezoelectric films were selected, with a piezoelectric constant d33 ≥ 20 pC / N and a dielectric constant of [missing information]. Loss tangent The film was cut into rectangular pieces 9cm long and 1cm wide using a precision cutter. The pieces were then ultrasonically cleaned for 10 minutes each with deionized water, anhydrous ethanol, and isopropanol to remove surface grease and dust. Finally, they were dried with nitrogen gas for later use.

[0131] 2) Electrode fabrication: Copper-nickel composite electrodes were fabricated on the surface of a PVDF thin film using magnetron sputtering. Specific process parameters were: background vacuum ≤ The sputtering power was 100W, the argon flow rate was 20sccm, and the working pressure was 0.5Pa. A 150nm thick copper layer was sputtered first as a conductive layer, and then a 50nm thick nickel layer was sputtered as a protective layer, for a total thickness of 200nm.

[0132] A double-finger rectangular coplanar electrode pattern was fabricated using photolithography. The electrode structure is as follows: Figure 4As shown, the width and spacing of the finger strips are both 12.5 mm, and the overall electrode area size is 3 cm × 1 cm, centered on the film surface. AWG36 silver-plated copper wires are soldered to both ends of the electrode as leads, and conductive silver paste is used to reinforce the connection points. The electrodes are then cured at 120°C for 30 minutes.

[0133] 3) Encapsulation and shielding: A layer of epoxy resin with a thickness of about 50μm is coated on the front area of ​​the non-electrode of the sensor and cured at 60℃ for 2 hours to form an encapsulation protective layer to avoid electrode oxidation and mechanical damage.

[0134] A layer of silicone grease approximately 80 μm thick was uniformly coated on the back of the sensor (the side that fits into the GIS housing) as an acoustic coupling layer. This was then covered with a 25 μm thick aluminum foil as an electromagnetic shielding layer, with the edge of the aluminum foil extending approximately 5 mm beyond the sensor edge to ensure complete coverage of the back of the sensor. The sensor leads were then threaded through the aluminum foil, and the lead exits were sealed with insulating tape, completing the overall sensor fabrication. The final structure is consistent with... Figure 1 The layered structures shown correspond one-to-one.

[0135] 4) Sensor installation: Select a flat area near the GIS basin insulator or the edge of the cover plate as the installation location. Clean the surface of the housing with anhydrous ethanol to remove oil and dust.

[0136] Attach the sensor to the housing surface using epoxy resin adhesive, applying uniform pressure for approximately 5 minutes to ensure a tight fit between the sensor and the housing, with no air bubbles remaining. During installation, ensure that the long side (9cm direction) of the sensor points towards the center of the GIS cavity to maximize the coupling of axially propagating ultrasonic waves.

[0137] Connect the sensor leads to the BNC interface of the signal conditioning box, ensuring a secure connection and proper grounding.

[0138] II. Setup and debugging of the detection system. The specific setup and debugging steps are as follows:

[0139] 1) Signal Conditioning Module 201: This module includes an impedance matching unit, a low-noise charge amplifier, and a programmable bandpass filter. The impedance matching unit uses a 50Ω coaxial impedance matcher to achieve impedance matching between the sensor and subsequent circuits. The low-noise charge amplifier has an input noise of ≤5nV / √Hz and an adjustable gain range of 20-60dB; in this embodiment, it is set to 40dB. The programmable bandpass filter has cutoff frequencies of 20kHz and 80kHz and an out-of-band rejection ratio of ≥40dB, used to filter out low-frequency mechanical vibrations and high-frequency electromagnetic interference.

[0140] 2) Data acquisition module 202: It adopts a high-speed data acquisition card with 16-bit resolution and 1MS / s sampling rate, supports multi-channel synchronous acquisition, and its input interface is connected to the output end of the signal conditioning module. The output end is connected to the processing module through the USB3.0 interface to realize high-speed data transmission.

[0141] 3) Processing Module 203: Utilizes an Advantech UNO-2484G industrial-grade embedded computer, configured with an Intel Core i5-8265U processor, 8GB of RAM, and a 256GB solid-state drive. The computer incorporates the GIS partial discharge detection software developed in this invention, which integrates data acquisition, signal preprocessing, time-frequency domain feature extraction, ultrasonic PRPD map construction, CNN defect identification, data storage, trend analysis, and fault early warning functions.

[0142] 4) System Debugging: After the system is built, calibrate the system using a standard ultrasonic transmission system. Place the standard ultrasonic transmission probe on the surface of the GIS housing and transmit a 20kHz-80kHz sinusoidal signal with an amplitude of 1V. Adjust the gain of the signal conditioning module 201 so that the amplitude of the input signal of the data acquisition module 202 is between 50% and 80% of the full scale.

[0143] System-level electromagnetic compatibility (EMC) testing: System-level EMC testing was conducted according to GB / T 17626.3-2016 "Electromagnetic Compatibility Testing and Measurement Technology - Radiated Electromagnetic Field Immunity Test". A radiated electromagnetic field with a frequency range of 80MHz-2GHz and a field strength of 10V / m was applied near the sensor for 24 consecutive hours. Test results show that the system's false alarm rate is less than 0.1%, with no missed alarms, and the EMC performance meets the requirements for GIS field operation. (This test verifies the operational stability of the entire detection system in the field electromagnetic environment.)

[0144] III. Sensor Performance Testing: A comprehensive performance test was conducted on the prepared sensor. All tests were strictly carried out in accordance with the GB / T 19801-2005 standard "Characteristics and Measurement of Ultrasonic Sensors for Non-destructive Testing". The specific test steps and results are as follows (this test verifies the acoustic and electrical performance of the individual sensor):

[0145] (1) Sensitivity test: Sensitivity refers to the ratio of the sensor's output voltage to the input sound pressure, and the unit is _____. The specific testing steps are as follows:

[0146] 1) Test Platform Setup: A silencer water tank test platform was set up, which included a standard ultrasonic transmission system (including a standard ultrasonic signal generator and a standard transmission probe), a silencer water tank, a precision three-dimensional displacement stage, and a digital oscilloscope. The silencer water tank measures 1m × 1m × 1m, with sound-absorbing material lining the inner walls, resulting in a background noise level of less than 20dB.

[0147] 2) System Calibration: Place the standard transmitting probe and the standard receiving probe (calibrated by the National Institute of Metrology) opposite each other in the anechoic water tank, 10cm apart, with their centers aligned. The standard ultrasonic transmitting system transmits a sinusoidal signal with a frequency of 40kHz and an amplitude of 1V. Record the output voltage V0 of the standard receiving probe to calibrate the sound pressure output of the system.

[0148] 3) Sensor test: Keep the position of the transmitting probe unchanged, replace the standard receiving probe with the sensor of this invention, and adjust the precision displacement stage to align the sensor with the center of the transmitting probe, with the distance still 10cm.

[0149] 4) Data Acquisition and Calculation: The standard ultrasonic transmission system sequentially transmits sinusoidal signals at 20kHz, 30kHz, 40kHz, 50kHz, 60kHz, 70kHz, and 80kHz. For each frequency point, 100 cycles of the signal are continuously acquired, and the average value is taken as the output voltage at that frequency point. The formula for calculating sensitivity is: in, The calibration sensitivity of the standard receiving probe is 60dB at 40kHz.

[0150] 5) Average sensitivity calculation: Calculate the arithmetic mean of the sensitivity at 7 frequency points within the 20kHz-80kHz frequency band to obtain the average sensitivity of the sensor.

[0151] Test results: The average sensitivity of the sensor of this invention is 62.43 dB in the 20 kHz-80 kHz frequency band. This represents a 9.2 dB improvement over existing PVDF partial discharge sensors (53.23 dB).

[0152] (2) Frequency response characteristic test: The frequency response characteristic refers to the relationship between the sensor sensitivity and frequency, which is used to determine the effective operating bandwidth of the sensor. The specific test steps are as follows:

[0153] 1) Keep the platform settings for sensitivity testing unchanged. Use a standard ultrasonic transmission system to transmit a sweep frequency signal with a sweep frequency range of 10kHz-100kHz, a sweep frequency speed of 1kHz / s, and a sampling rate of 1MS / s.

[0154] 2) Continuously record the curve of the sensor's output voltage changing with frequency, and take the average value of 10 measurements for the output voltage at each frequency point.

[0155] 3) Using the sensitivity at 40kHz as a benchmark, calculate the relative sensitivity at each frequency point and plot the sensitivity-frequency response curve.

[0156] 4) Determine the -6dB bandwidth and -10dB bandwidth: The -6dB bandwidth refers to the frequency range corresponding to the relative sensitivity dropping to -6dB; the -10dB bandwidth refers to the frequency range corresponding to the relative sensitivity dropping to -10dB.

[0157] Test results: The -6dB bandwidth of the sensor of this invention is 18kHz-82kHz, and the -10dB bandwidth is 15kHz-85kHz, which can fully cover the main frequency range (20kHz-80kHz) of GIS partial discharge ultrasonic signals.

[0158] (3) Impulse response test: Impulse response refers to the sensor's response characteristics to narrow-pulse ultrasonic signals, used to evaluate the sensor's time resolution and signal fidelity. The specific test steps are as follows:

[0159] 1) Use a pulse generator to excite a standard ultrasonic transmitting probe to generate an ultrasonic pulse signal with a rise time of less than 1μs and a half-width at half-maximum of less than 2μs.

[0160] 2) Place the sensor of this invention and the commercial PZT sensor (model: Olympus A102S) 10cm away from the transmitting probe, and simultaneously collect the response waveforms of the two sensors.

[0161] 3) Measure the rise time (the time required for the peak value to rise from 10% to 90%), fall time, and number of rings of the response waveform.

[0162] Impulse response test results:

[0163] 1) The rise time of the response waveform of the sensor of the present invention is 1.8μs and the fall time is 3.2μs, with no obvious ringing phenomenon.

[0164] 2) The rise time of the response waveform of commercial PZT sensors is 5.6 μs, the fall time is 25 μs, and the number of rings exceeds 10. The single discharge resolution of the sensor of this invention is better than 5 μs, and it can accurately distinguish continuous discharge pulses with a time interval of less than 10 μs.

[0165] (4) Full-scale GIS discharge test: A discharge test was conducted on a 126kV full-scale GIS test platform to verify the sensor's ability to detect actual partial discharge defects. The specific test steps are as follows:

[0166] 1) Test Platform Setup: The 126kV full-scale GIS test platform includes a GIS tank, a power frequency test transformer, a capacitor divider, a partial discharge detector (IEC 60270 standard), and the testing system of this invention. The GIS tank is filled with 0.5MPa of [unclear - possibly referring to a specific type of gas or material]. gas.

[0167] 2) Preparation of typical defects: Three types of typical partial discharge defects were prepared inside the GIS tank:

[0168] Spike discharge defect: A copper spike with a length of 10 mm and a tip curvature radius of 0.1 mm is fixed on a high-voltage conductor.

[0169] Floating potential discharge defect: A 10mm diameter metal ball is placed between the high-voltage conductor and the grounded shell, with a 1mm air gap between the metal ball and the high-voltage conductor.

[0170] Surface discharge defect: A 20mm long metal foil is pasted on the surface of the basin insulator.

[0171] 3) Voltage application and data acquisition: Slowly increase the test voltage to the partial discharge initiation voltage (PDIV), apply a voltage of 1.1 times the PDIV, and keep the voltage stable. Measure the discharge quantity using an IEC standard partial discharge detector, and simultaneously acquire ultrasonic signals using the detection system of this invention. Acquire signals continuously for 30 minutes, and repeat the test 5 times for each defect type.

[0172] 4) Signal-to-noise ratio calculation: Signal-to-noise ratio (SNR) The calculation formula is: in, This represents the peak voltage of the discharge signal. This represents the background noise voltage when there is no discharge.

[0173] Test results: At a discharge level of approximately 50 pC, the signal-to-noise ratios of the sensor of this invention for the three types of defects are: 18.6 dB for spike discharge, 22.9 dB for floating potential discharge, and 12.4 dB for surface discharge, all of which meet the requirements for on-site detection (signal-to-noise ratio ≥ 10 dB).

[0174] IV. Validation of the optimized design method:

[0175] Comparison of the frequency response results obtained from simulation with the measured results is as follows: Figure 5 As shown, the specific verification steps are as follows:

[0176] 1) Finite element simulation modeling: A multiphysics coupling model of the GIS shell, coupling layer, and PVDF sensor was established using COMSOL Multiphysics 6.1 software. The GIS shell is made of aluminum alloy with a diameter of 500 mm and a thickness of 10 mm; the coupling layer is made of silicone grease with a thickness of 80 μm; and the PVDF film adopts the structural parameters of this invention.

[0177] 2) Optimization of placement and orientation: Simulation of the propagation characteristics of ultrasonic signals on the surface of GIS shell. The results show that the ultrasonic signal amplitude in the edge area of ​​the cover plate is 32% higher than that in the center area; when the long side of the sensor points to the center of the cavity, the signal amplitude is 45% higher than when it points perpendicularly.

[0178] 3) Electrode configuration optimization: Comparing the piezoelectric response characteristics of single-finger strip, double-finger strip, and interdigitated electrodes, the results show that the charge output efficiency of the double-finger strip rectangular electrode is 28% higher than that of the single-finger strip electrode and 15% higher than that of the interdigitated electrode; the charge output efficiency reaches its maximum value when the electrode width-to-spacing ratio is 1:1.

[0179] 4) Thin film thickness optimization: The frequency response characteristics of PVDF films with thicknesses of 100μm, 200μm, 400μm, and 600μm were analyzed, and the results are as follows: Figure 3 As shown in the simulation curves, the 400μm thick film has the highest average sensitivity in the 20kHz-80kHz frequency band and a smaller high-frequency response attenuation.

[0180] The error between the simulation results and the experimental test results is less than 5%. Figure 5 The goodness of fit between the simulation and the measured curves is consistent, which verifies the accuracy and reliability of the optimization design method of the present invention.

[0181] V. Implementation of the online detection method, the specific steps are as follows:

[0182] (1) Sensor installation: According to the installation requirements, attach the sensor to the edge area of ​​the GIS cover plate with the long side pointing to the center of the GIS cavity, and complete the wiring and grounding of the sensor and the signal conditioning module 201.

[0183] (2) System initialization: Start the detection system, complete the parameter configuration of the signal conditioning module 201 gain, filter cutoff frequency and data acquisition module 202 sampling rate, and perform system calibration.

[0184] (3) Signal acquisition and preprocessing: The ultrasonic vibration signal of the GIS shell is acquired by the sensor, and after amplification, filtering and analog-to-digital conversion, it is transmitted to the processing module 203 to remove noise and interference components in the signal.

[0185] Performance verification of the time-frequency-map cross-dimensional attention fusion network: Using over 1200 sets of labeled datasets collected from a 126kV real-world GIS test platform, the datasets were divided into training, validation, and test sets in a 7:2:1 ratio. Addressing the issue of unbalanced sample distribution on the real-world GIS test platform due to fixed hyperparameter settings in the original training process, this invention employs a differentiated sample augmentation strategy based on defect feature constraints. First, the proportion of the three original sample types—spike discharge, floating potential discharge, and surface discharge—in the training set is statistically analyzed, and the scarcity coefficients normalized to the [1, 3] interval are calculated. This determines the actual augmentation ratio for each type of sample, with a total effective augmentation ratio of no less than 5 times. Simultaneously, differentiated enhancement parameter boundaries (spike discharge phase offset ±8°, time...) are set for the inherent signal characteristics of the three types of defects. Interaxial stretching and compression of 0.95-1.05 times, floating potential discharge phase shift of ±15°, and time axis stretching and compression of 0.9-1.1 times, and surface discharge phase shift of ±20°, and time axis stretching and compression of 0.85-1.15 times are applied. Invalid enhanced samples are removed by verifying three core features: pulse rise time, dominant frequency, and phase distribution interval in the time domain, ensuring that the deviation in the proportion of the three types of samples is controlled within ±10%. Based on this, a two-level weighted loss function driven by sample distribution is constructed, and the Gini coefficient of the training set is calculated every 5 training iterations to determine the sample balance. With the dispersion of the coefficient of variation of discharge quantity ,based on The overall weights for classification and regression tasks are dynamically adjusted. ).when Additional time To enhance the fitting ability for large-span discharge amounts, a class-level weight normalized to the [0.5, 2] interval is introduced into the classification loss. To further suppress model bias towards the majority class, a validation set-aware adaptive iterative training strategy is adopted. The first five iterations use a warm-up learning rate linearly increasing from 0.0001 to 0.001. After each iteration, a combined validation set performance score is calculated, integrating classification accuracy and regression precision. If 3 consecutive iterations If the improvement is less than 0.1%, the learning rate decay rate will be dynamically adjusted based on the decrease in score. ), and set 1×10 -6 The minimum learning rate threshold is set, and an early stopping mechanism is introduced. If there are 10 consecutive iterations... If no improvement is achieved, training is terminated early, with the maximum number of iterations remaining at 100. Through these improvements, the accuracy of identifying rare surface discharge defects increased by 8.3%, the average accuracy of identifying the three types of defects increased from 97.2% to 98.1%, the average absolute error of discharge regression decreased from 28 pC to 24.4 pC, the model training convergence speed was accelerated by 25%, and it fully adapts to the actual working conditions of unevenly distributed field samples. The pre-trained partial discharge defect identification model is then input to determine the presence of partial discharge and identify the discharge type and severity. The specific steps for constructing the ultrasonic signal PRPD atlas are as follows:

[0186] Synchronous signal acquisition: The data acquisition module synchronously acquires ultrasonic signals and power grid voltage signals (50Hz) at a sampling rate of 1MS / s, ensuring that 20,000 ultrasonic signal sampling points are acquired in each power frequency cycle (20ms);

[0187] (2) Power frequency phase division: The 360° phase of each power frequency cycle is divided into 80 equally spaced phase windows, each phase window corresponding to 4.5° (i.e. 45 / 8°), ​​which is consistent with the input requirements of the partial discharge defect identification model of the present invention;

[0188] (3) Ultrasonic signal phase correlation: A one-to-one correspondence is established between the synchronously acquired ultrasonic signal and the power grid frequency voltage signal (50Hz) to provide a phase reference for the construction of the ultrasonic PRPD map. The specific phase correlation steps are as follows: The positive zero-crossing time of the power frequency voltage signal is identified by an adaptive threshold rising edge zero-crossing detection algorithm with noise robustness. The core implementation and parameter settings of the algorithm are as follows: The power frequency voltage signal synchronously acquired at a sampling rate of 1MS / s is used as the input, and a length of 5 sampling points (corresponding to The voltage difference between adjacent sampling points is calculated using a sliding differential window (balancing real-time detection and anti-interference capability). Simultaneously, an adaptive zero-crossing threshold is calculated based on the background noise amplitude of the first 10 power frequency cycles. ( The standard deviation of the noise amplitude follows Statistical criteria to eliminate random noise interference); when three consecutive sliding windows... All are greater than 0 and the absolute value of the voltage at the center sampling point of the window is less than When the central sampling point is determined to be a candidate positive zero-crossing point, abnormal zero-crossing points are eliminated by time interval verification: if the time interval between two adjacent candidate zero-crossing points is less than 18ms or greater than 22ms (exceeding the limit fluctuation range of ±10Hz of the power grid frequency), the current zero-crossing point position is corrected by the average time interval of the first 3 valid zero-crossing points, and the number of zero-crossing points is recorded. The sampling point number corresponding to each valid positive zero crossing point is: This serves as the 0° phase reference point for the corresponding power frequency cycle. Based on this, a cycle-by-cycle full compensation mechanism for power frequency offset is constructed to calculate the actual frequency offset for each power frequency cycle in real time and dynamically correct the phase calculation parameters: calculating the actual number of sampling points for the current power frequency cycle. This allows us to obtain the actual power frequency of that cycle. With frequency offset Completely abandoning standards The corresponding fixed 20,000 points / cycle assumption is based solely on the number of measured sampling points in a single cycle. As the sole benchmark for phase equipartition; for To address the uneven phase window width caused by the inability to be divisible by 80, an adaptive remainder allocation strategy based on the frequency offset direction is introduced: The remainder is calculated... ,like (High power frequency, shortened cycle), then The additional sampling points are evenly distributed to the back A phase window; if (Low power frequency, long cycle) then The additional sampling points are evenly distributed to the front. There are 1 phase window, so that the actual number of sampling points for each phase window is 1. or The theoretical phase deviation of the single-phase window is controlled within 0.056°. This applies to each ultrasound sampling point within the current cycle. ( According to the formula Calculate the corresponding precise power frequency phase value, and then map the sampling point to the next position based on the phase value. Phase window ( );in, Representing the The sampling point number corresponding to the positive zero crossing point of each power frequency cycle. For the first The power frequency phase value obtained by converting each ultrasonic sampling point; when When the absolute value exceeds 0.2Hz, an adaptive compensation value is applied to the phase window boundary. To further correct the phase accumulation error at high frequencies, the amplitude of each ultrasonic sampling point is assigned to its corresponding phase window, and the maximum amplitude of the ultrasonic signal within each phase window is statistically analyzed to establish a one-to-one correspondence between the ultrasonic signal and the power frequency phase. Experimental verification shows that under normal random fluctuations of ±0.5Hz in the power grid frequency, the maximum phase mapping error of this method is less than 0.1°, which is 18 times higher than the traditional method with a fixed 20,000 points / cycle (maximum phase error 1.8°). Compared with the cycle-by-cycle calculation method without remainder allocation (maximum phase error 0.45°), the phase feature distortion rate of the PRPD spectrum is reduced by 92%, and the recognition accuracy of the multi-peak phase distribution characteristics of surface discharge is improved by 6.2%, providing a reliable spectrum data foundation for the accurate classification of subsequent defect types.

[0189] (4) Amplitude statistics and normalization: Statistically calculate the maximum amplitude of the ultrasound signal within each phase window, convert the amplitude to dB value (based on 1μV), and normalize it to the range of -20dB to 80dB;

[0190] (5) PRPD map generation: The phase is used as the horizontal axis (0-360°), the amplitude is used as the vertical axis (-20dB-80dB), and the number of discharges in each phase-amplitude interval is used as the color depth to generate a two-dimensional ultrasonic signal PRPD map with a size of 100×64.

[0191] Results Output and Early Warning: Detection results, defect types, and discharge severity are displayed in real time. When a partial discharge signal exceeding a threshold is detected, a fault early warning is triggered, and the data is uploaded to the power grid condition monitoring platform. The fault early warning threshold is set as follows:

[0192] This invention uses a signal-to-noise ratio threshold as the criterion for fault early warning. The threshold is set based on the background noise level of the GIS field operation and industry testing standards.

[0193] Level 1 warning (minor discharge) threshold: signal-to-noise ratio ≥ 10dB.

[0194] Level II warning (moderate discharge) threshold: signal-to-noise ratio ≥15dB.

[0195] Level 3 warning (severe discharge) threshold: signal-to-noise ratio ≥ 20dB. The above threshold can be adjusted by ±2dB according to the actual background noise level of different substations to adapt to different site environments.

[0196] This invention is not limited to the structures described above and shown in the accompanying drawings, and various modifications and changes can be made without departing from its scope. The scope of this invention is limited only by the appended claims.

Claims

1. A method for optimizing GIS partial discharge sensors, characterized in that, include: A multi-physics coupled finite element model was established, and the propagation characteristics of ultrasonic signals on the surface of the GIS shell were analyzed to determine the optimal placement and installation direction of the sensors. Using the optimal arrangement position and installation direction as simulation boundary conditions, finite element models of various electrode configurations were constructed for simulation comparison. Based on the comprehensive simulation results of the piezoelectric response characteristics and frequency response characteristics of different electrodes, the optimal electrode configuration was determined. A piezoelectric vibration model of a flexible polyvinylidene fluoride (PVDF) film was established to analyze the influence of the length and width of the flexible PVDF film on the sensitivity and frequency response, and to determine the optimal shape and size of the flexible PVDF film. Based on the optimal shape and size, the influence of the thickness of the flexible polyvinylidene fluoride film on the piezoelectric constant, capacitance and sensitivity is analyzed, and the optimal thickness of the flexible polyvinylidene fluoride film is determined in combination with the feasibility of the preparation process. Based on the optimal electrode configuration, optimal shape and size, and optimal thickness of the flexible polyvinylidene fluoride film, a sensor was fabricated to obtain an optimized sensor. A performance testing platform was then built to verify the sensitivity of the optimized sensor.

2. The GIS partial discharge sensor optimization method according to claim 1, characterized in that, The establishment of a multi-physics coupled finite element model and the analysis of the propagation characteristics of ultrasonic signals on the surface of the GIS shell to determine the optimal placement and installation direction of the sensors include: A three-dimensional finite element model was established using multiphysics simulation software. The three-dimensional finite element model includes a GIS shell, an acoustic coupling layer, and a sensor. Solid mechanical physical field, acoustic physical field, and piezoelectric effect physical field were set for the GIS shell, acoustic coupling layer, and sensor, respectively. A broadband ultrasonic longitudinal wave load with a preset ultrasonic signal frequency band is applied to the inner wall of the GIS shell, a low-reflection boundary condition is set at the outer edge of the GIS shell, and a binding contact is set between the sensor and the acoustic coupling layer, and between the acoustic coupling layer and the GIS shell. Multiple monitoring points are set radially on the outer surface of the GIS shell. The average vibration amplitude of each monitoring point in the preset ultrasonic signal frequency band is calculated. Based on the comparison of the average vibration amplitude of each monitoring point, the optimal arrangement position of the sensor is determined. Multiple installation directions are set at the optimal placement position. The average output voltage of the sensor in the preset ultrasonic signal frequency band under different installation directions is calculated. Based on the comparison of the average output voltage of each installation direction, the optimal installation direction of the sensor is determined.

3. The GIS partial discharge sensor optimization method according to claim 1, characterized in that, Using the optimal arrangement position and installation direction as simulation boundary conditions, finite element models of various electrode configurations are constructed for simulation comparison. Based on the comprehensive simulation results of the piezoelectric response characteristics and frequency response characteristics of different electrodes, the optimal electrode configuration is determined, including: Keeping the size of the flexible polyvinylidene fluoride film and the total electrode area constant, finite element models of various electrode configurations are constructed; the various electrode configurations include single-finger strip electrodes, gradient-width double-finger strip coplanar rectangular electrodes, and interdigitated electrodes; Based on finite element models with various electrode configurations, a normal displacement load is applied to the back of a flexible polyvinylidene fluoride film, and the charge output of each electrode configuration within a preset frequency range is calculated based on the preset piezoelectric strain-charge constitutive equation. The charge output of each electrode configuration is compared, and the piezoelectric response characteristics of each electrode configuration are obtained based on the comparison results. The electrode configuration with the optimal piezoelectric response characteristics is then determined. The curves of charge output as a function of frequency for each electrode configuration are obtained by frequency sweep simulation. The relative output amplitude at each frequency point is calculated based on the charge output at the preset center frequency to determine the effective bandwidth of each electrode configuration. The time-domain response waveforms of each electrode configuration are obtained through impulse response simulation, and the rise time of the waveforms of each electrode configuration is determined. Based on the comparison results of effective bandwidth and waveform rise time, the electrode configuration with optimal frequency response characteristics is determined. Based on the simulation results of the combined piezoelectric response characteristics and frequency response characteristics, the gradient width double-finger coplanar rectangular electrode is selected as the optimal electrode configuration; the optimal width-to-width ratio of the gradient width double-finger coplanar rectangular electrode is determined.

4. The GIS partial discharge sensor optimization method according to claim 3, characterized in that, The formula for calculating the relative output amplitude at each frequency point is: ; In the formula, This represents the relative output amplitude at each frequency point; This indicates the amount of charge output at the preset center frequency; Indicates frequency as At that time, the amount of induced charge output by the polyvinylidene fluoride piezoelectric thin film electrode.

5. The GIS partial discharge sensor optimization method according to claim 3, characterized in that, The optimal width-to-width ratio of the gradient-width coplanar rectangular electrodes with two finger strips includes: Keeping the total length of the gradient-width double-finger coplanar rectangular electrode constant, various width-to-spacing ratios are set; the width-to-spacing ratio represents the ratio of the width of a single finger in the gradient-width double-finger coplanar rectangular electrode to the spacing between the two fingers; Based on the current wide pitch ratio, a normal harmonic displacement load is applied to the back of the flexible polyvinylidene fluoride film to simulate ultrasonic vibration, couple the physical field of solid mechanics with the physical field of piezoelectric effect, and perform frequency sweep solution within a preset frequency band with a preset step size. Based on each frequency point, the three-dimensional strain tensor inside the flexible polyvinylidene fluoride film is obtained. Based on the preset piezoelectric effect strain-charge constitutive equation, combined with the three-dimensional strain tensor, the electric displacement vector distribution inside the flexible polyvinylidene fluoride film is calculated. The normal components of the electric displacement vector of the two finger-covered areas of the gradient width double-finger coplanar rectangular electrode are respectively integrated by surface integral. The two surface integral results are summed to obtain the total charge output of the gradient width double-finger coplanar rectangular electrode at that frequency point. Take the arithmetic mean of the total charge output at all frequency points within the preset frequency band as the average charge output under the current wide spacing ratio; The average charge output under different width spacing ratios is compared, and the optimal width spacing ratio of the gradient width double-finger coplanar rectangular electrode is determined based on the comparison results.

6. The GIS partial discharge sensor optimization method according to claim 1, characterized in that, The establishment of a piezoelectric vibration model for the flexible polyvinylidene fluoride (PVDF) film, the analysis of the influence of the length and width of the flexible PVDF film on the sensitivity and frequency response, and the determination of the optimal shape and size of the flexible PVDF film include: Based on the pre-defined piezoelectric effect strain-charge constitutive equation, a piezoelectric vibration model of a flexible polyvinylidene fluoride (PVDF) film is established. The boundary conditions of the piezoelectric vibration model are set such that the back side of the flexible PVDF film is bound to the GIS shell through an acoustic coupling layer, and the front side is a free boundary. Multiple different flexible polyvinylidene fluoride (PVDF) film lengths are preset, the average sensitivity of the sensor within a preset frequency band is calculated under different flexible PVDF film lengths, and the optimal length range is determined based on the trend of average sensitivity with length. Multiple different flexible polyvinylidene fluoride (PVDF) film widths are preset, and the average sensitivity and effective bandwidth of the sensor within the preset frequency band are calculated under different flexible PVDF film widths. Based on the changing trends of average sensitivity and effective bandwidth with width, the optimal width range is determined. The optimal shape and size of the flexible polyvinylidene fluoride film were determined by considering average sensitivity, effective bandwidth, and ease of installation.

7. The GIS partial discharge sensor optimization method according to claim 6, characterized in that, The system presets multiple different flexible polyvinylidene fluoride (PVDF) film lengths, calculates the average sensitivity of the sensor within a preset frequency band for different PVDF film lengths, and determines the optimal length range based on the trend of average sensitivity changing with length. Keeping the width and thickness of the flexible polyvinylidene fluoride film constant, multiple different flexible polyvinylidene fluoride film lengths are set. Under the current length of the flexible polyvinylidene fluoride film, a normal harmonic displacement load with a preset frequency band is applied to the center position of the inner wall of the GIS shell to simulate the ultrasonic longitudinal wave excited by partial discharge, couple the physical field of solid mechanical and piezoelectric effects, and perform frequency sweep solution within the preset frequency band with a preset step size. Based on each frequency point, the three-dimensional strain tensor inside the flexible polyvinylidene fluoride film is obtained. Based on the preset piezoelectric effect strain-charge constitutive equation, combined with the three-dimensional strain tensor, the electric displacement vector distribution inside the flexible polyvinylidene fluoride film is calculated. The normal component of the electric displacement vector in the area covered by the gradient width double-finger coplanar rectangular electrode is integrally applied to obtain the total charge of the gradient width double-finger coplanar rectangular electrode at the frequency point. Based on the definition of capacitance, the output voltage of the sensor at the frequency point is calculated using the total charge. Calculate the input vibration velocity at the frequency point based on the relationship between simple harmonic vibration velocity and displacement; The sensitivity of the sensor at a given frequency point is determined by the ratio of the output voltage to the input vibration velocity. Repeatedly perform the calculation operation of output voltage and input vibration velocity to obtain the sensitivity of all frequency points within the preset frequency band, and take the arithmetic mean of the sensitivity of all frequency points as the average sensitivity under the length of the flexible polyvinylidene fluoride film. The average sensitivity of each flexible polyvinylidene fluoride film at different lengths was compared, and the optimal length range was determined based on the trend of the average sensitivity with length obtained from the comparison.

8. The GIS partial discharge sensor optimization method according to claim 7, characterized in that, The formula for calculating the input vibration velocity at the frequency point is: ; In the formula, Representing frequency point Input vibration velocity; This indicates the applied displacement amplitude.

9. A GIS partial discharge sensor, obtained by the GIS partial discharge sensor optimization method according to any one of claims 1-8, characterized in that, It includes an acoustic coupling layer, a flexible polyvinylidene fluoride sensing unit, an electrode structure, a pre-bending shaping layer, an encapsulation and protection layer, and an electromagnetic shielding layer, which are stacked sequentially from the inside out. An acoustic coupling layer is attached to the surface of the GIS housing to reduce the reflection loss of ultrasonic signals at the interface between the GIS housing and the sensor, and to transmit the mechanical vibration of the GIS housing to the flexible polyvinylidene fluoride sensing unit without attenuation. The flexible polyvinylidene fluoride (PVDF) sensitive unit is disposed on the back of the acoustic coupling layer to receive ultrasonic signals excited by partial discharge of GIS and generate mechanical vibration, and to generate polarized charges on the upper and lower surfaces of the flexible PVDF sensitive film through the positive piezoelectric effect. The electrode structure is located on the front of the flexible polyvinylidene fluoride sensing unit. It is a gradient-width double-fin coplanar rectangular electrode used to collect polarization charge and output electrical signal. A pre-bending shaping layer is placed between the electrode structure and the encapsulation protective layer to pre-bend the sensor into a shape that matches the curvature of the GIS housing surface, thereby eliminating bubbles and stress concentrations generated when the sensor is attached to the curved GIS housing. An encapsulation protective layer covers the non-electrode area on the front of the pre-bent shaping layer and the flexible polyvinylidene fluoride sensitive unit to protect the electrodes from oxidation and mechanical damage. An electromagnetic shielding layer covers the outer surface of the encapsulation protective layer to suppress electromagnetic interference.

10. The GIS partial discharge sensor according to claim 9, characterized in that, The flexible polyvinylidene fluoride sensing unit has a thickness of 400 μm, a length of 9 cm, and a width of 1 cm; the acoustic coupling layer is a silicone grease material with a thickness of 80 μm; the pre-bending shaping layer is a polyterephthalic acid plastic film with a thickness of 50 μm, pre-bent into an arc that matches the standard GIS shell; the encapsulation protective layer is an epoxy resin material with a thickness of 50 μm; and the electromagnetic shielding layer is an aluminum foil material with a thickness of 25 μm.

11. A GIS partial discharge detection system, employing the optimized GIS partial discharge sensor of claim 9 for GIS partial discharge detection, characterized in that, include: The signal conditioning module is used to perform impedance matching, amplification, and filtering on the weak analog electrical signal output by the sensor to obtain the processed analog voltage signal. The data acquisition module is used to convert the processed analog voltage signal into a digital signal; The processing module is used to perform time-frequency domain analysis and feature extraction on digital signals to identify the type and severity of partial discharge in GIS, so as to achieve fault early warning.

12. The GIS partial discharge detection system according to claim 11, characterized in that, The process of impedance matching, amplification, and filtering the weak analog electrical signal output by the sensor to obtain the processed analog voltage signal includes: A 50-ohm coaxial impedance matching circuit is used as the signal input stage. It is connected to the sensor output through a coaxial snap-fit ​​interface and matched with the sensor's own 50-ohm output impedance to eliminate reflection loss during signal transmission. Using a low-noise charge amplifier with an input noise of less than five nanovolts per square hertz as the core amplification unit, and configuring a 100 picofarad feedback capacitor and a 1,000 megohm feedback resistor, the gain of the low-noise charge amplifier is adjusted to 45 dB. At the same time, the weak analog electrical signal at the microvolt level output by the sensor is converted and amplified to an analog voltage signal at the volt level. An eighth-order Butterworth programmable bandpass filter is used as the output stage. The corresponding passband and suppression index are set to filter out various irrelevant interference signals, retain the effective frequency band of the GIS partial discharge ultrasonic signal, and output the processed analog voltage signal.

13. The GIS partial discharge detection system according to claim 11, characterized in that, The process of converting the processed analog voltage signal into a digital signal includes: Using a high-speed synchronous data acquisition card with 16-bit resolution and a sampling rate of millions of times per second, the signal conditioning module output is connected via a shielded coaxial cable to completely restore the ultrasonic signal according to the Nyquist sampling theorem; The analog voltage signal is acquired by the sample-and-hold circuit inside the high-speed synchronous data acquisition card and the sampled value is kept stable. The analog voltage signal in the range of -5V to +5V is converted into digital code by a 16-bit analog-to-digital converter, and the quantization error is controlled within a preset range to ensure the accuracy of weak signal acquisition. The digital code generated by analog-to-digital conversion is stored in the built-in high-speed cache of the acquisition card and transmitted to the processing module through the third-generation universal serial bus interface.

14. The GIS partial discharge detection system according to claim 11, characterized in that, The process of performing time-frequency domain analysis and feature extraction on digital signals to identify the type and severity of partial discharge in GIS, in order to achieve fault early warning, includes: The digital signal is subjected to wavelet threshold denoising and normalization to obtain the processed digital signal; The processed digital signal is subjected to time-domain and frequency-domain feature extraction, and the power grid frequency voltage signal and ultrasonic signal are synchronously acquired and phase-correlated to construct an ultrasonic partial discharge phase distribution map. The time-domain features, frequency-domain features, and ultrasonic partial discharge phase distribution map are input into the time-frequency-map cross-dimensional attention fusion network for identification, and the defect classification probability and discharge quantity regression value are output to determine the defect type and discharge severity. Based on the defect type and discharge severity, a graded fault warning is performed in conjunction with a preset signal-to-noise ratio threshold.

15. The GIS partial discharge detection system according to claim 14, characterized in that, The wavelet threshold denoising and normalization processing of the digital signal yields the following processed digital signal: The acquired digital signal is segmented into sliding windows according to a preset window size, and adjacent windows overlap with a preset overlap rate. Wavelet decomposition is performed on the signal within each window to obtain the detail coefficients and low-frequency approximation coefficients at each level; Adaptive thresholds are calculated for detail coefficients at each layer, and threshold shrinkage is performed while retaining low-frequency approximation coefficients unchanged. The signals of each window are reconstructed by inverse wavelet transform to obtain the denoised digital signals, and the maximum and minimum amplitude values ​​of the denoised signals within each window are extracted. Based on the maximum and minimum amplitude values ​​of each window, a linear normalization method is used to map the amplitude values ​​of each sampling point within the window to a preset interval point by point; When the signal within the window is all-zero background noise, the normalized amplitude of all sampling points in the window is directly set to zero. Normalization is performed on all sliding windows to obtain a globally normalized continuous signal sequence.

16. The GIS partial discharge detection system according to claim 14, characterized in that, The process of extracting time-domain and frequency-domain features from the processed digital signal, and simultaneously acquiring the power grid frequency voltage signal and the ultrasonic signal for phase correlation to construct an ultrasonic partial discharge phase distribution map includes: Statistical analysis is performed on each normalized sliding window signal to extract peak value, RMS value, kurtosis, margin factor, and impulse factor. Among them, peak value is the maximum absolute value of the signal within the window, RMS value is the root mean square value of the signal within the window, kurtosis is the normalized fourth-order statistic of the signal within the window, margin factor is the ratio of peak value to RMS amplitude, and impulse factor is the ratio of peak value to RMS value. A Hanning window is applied to each denoised sliding window signal to suppress spectral leakage, and a fast Fourier transform is performed to obtain a two-sided spectrum. The first few points of the two-sided spectrum are extracted and converted into a one-sided spectrum with amplitude normalized to a preset interval. The dominant frequency, spectral centroid, spectral bandwidth, and energy entropy are extracted from the single-sided spectrum. The dominant frequency is the frequency corresponding to the maximum amplitude in the single-sided spectrum. The spectral centroid is the weighted average of the spectral amplitude and the corresponding frequency. The spectral bandwidth is the difference between the upper and lower limit frequencies corresponding to the effective bandwidth when the amplitude in the single-sided spectrum drops to the amplitude of the dominant frequency. The energy entropy is the entropy value calculated based on the energy ratio of each sub-band after dividing the preset detection frequency band into several equal-width sub-bands. The power grid frequency voltage signal is acquired synchronously, and the ultrasonic signal is correlated with the power grid frequency voltage signal in phase. Based on the ultrasonic signal amplitude and its corresponding power frequency phase in each power frequency cycle, an ultrasonic partial discharge phase distribution map is constructed.