Method for predicting cycle life of coal-based hard carbon hybrid supercapacitor under agc frequency modulation working condition
By establishing a continuous physical prediction chain of strain load, mechanical damage, pore evolution, ESR growth, and remaining cycle life, the problems of condition adaptability and material specificity of supercapacitor life prediction under AGC frequency modulation conditions in the prior art have been solved, and high-precision life prediction results have been achieved.
Patent Information
- Application Number
- CN202611253194.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-18
- Publication Date
- 2026-11-24
AI Technical Summary
Existing supercapacitor cycle life prediction technologies suffer from poor adaptability to operating conditions, lack of material specificity, and broken prediction logic under AGC frequency modulation conditions. They are difficult to adapt to load characteristics such as random amplitude, high-rate pulse, and frequent forward and reverse switching. They do not consider the evolution law of layered and pore structure of coal-based hard carbon and lack a continuous physical chain from microscopic mechanical damage to macroscopic electrochemical performance degradation.
By employing a cumulative damage correction factor, anisotropic stress concentration factor, and a dual porosity evolution mechanism, combined with resistance strain gauges, nanoindentation, three-point bending fatigue tests, SEM, and finite element simulation, the cumulative damage and porosity of coal-based hard carbon electrodes are calculated. The remaining cycle life is predicted by ESR growth, establishing a continuous physical prediction chain of strain load—mechanical damage—porosity evolution—ESR growth—remaining cycle life.
It improves the accuracy and adaptability of life prediction, and controls the relative error of prediction within 4%, realizing accurate life prediction of coal-based hard carbon hybrid supercapacitors under AGC frequency modulation conditions.
Smart Images

Figure CN123159076A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of life assessment and condition prediction technology of new energy storage equipment, specifically involving a method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions. Background Technology
[0002] Hybrid supercapacitors combine the high power density of double-layer capacitors with the high energy density of batteries, making them ideal energy storage devices for AGC frequency regulation in power systems. Coal-based hard carbon has become the mainstream material for the negative electrode of hybrid supercapacitors due to its wide availability, low cost, and layered structure suitable for ion insertion and extraction.
[0003] In AGC frequency regulation applications, hybrid supercapacitors need to continuously respond to grid frequency regulation commands. Their operation is not a traditional constant charge-discharge process, but rather exhibits random amplitude variations, high-rate pulses, and frequent forward and reverse switching. These operating characteristics subject the coal-based hard carbon electrode to continuously varying strain loads during frequency regulation, further causing mechanical damage, changes in pore structure, and degradation of macroscopic electrochemical performance. Therefore, the ability to accurately describe the degradation process of the coal-based hard carbon electrode under actual AGC operating conditions, from load application to performance failure, directly affects the reliability of the hybrid supercapacitor cycle life prediction results.
[0004] However, existing supercapacitor cycle life prediction technologies have the following three core drawbacks: 1. Poor adaptability to operating conditions: Most general life models are developed based on constant current and constant voltage charging and discharging conditions, without considering the load characteristics of AGC frequency modulation, such as random amplitude variation, high-rate pulse, and frequent forward and reverse switching. The prediction error generally exceeds 20%.
[0005] The difficulty lies in the fact that the load amplitude and occurrence order of different pulses change continuously during the AGC frequency modulation process. If a constant load or fixed degradation rate is still used to describe the cyclic process, it is difficult to characterize the difference in damage accumulation caused by different load sequences, and it is also difficult to reflect the actual situation of the supercapacitor performance degradation rate changing dynamically with the operating state.
[0006] 2. Lack of material specificity: Existing models are not designed for the unique layered pore structure evolution of coal-based hard carbon, and ignore its anisotropic mechanical properties and the dual failure mechanism of stress-induced pore collapse / crack propagation.
[0007] For coal-based hard carbon anodes, under cyclic stress, on the one hand, the compaction of the layered structure causes pore collapse and reduces porosity; on the other hand, stress concentration at the layer boundaries may form microcracks that propagate during the cyclic process, increasing porosity. These two mechanisms are in competition with each other, making it difficult to describe the pore structure evolution throughout the entire cyclic process using a single pore compaction model or a single crack propagation model.
[0008] 3. Predicting logical break: Most models directly establish an empirical relationship between the number of cycles and the capacity / resistance decay, lacking a complete physical chain from microscopic mechanical damage to macroscopic electrochemical performance degradation.
[0009] While existing empirical prediction methods can establish a correlation between the number of cycles and capacity or resistance based on historical cycling data, they struggle to explain how AGC loads act on coal-based hard carbon electrodes, how material damage further causes changes in pore structure, and how these changes ultimately translate into ESR growth. Therefore, when operating conditions or parameters of coal-based hard carbon materials change, relying solely on empirical degradation relationships makes it difficult to maintain consistent prediction results.
[0010] Therefore, developing a cycle life prediction method with clear physical meaning, complete logical chain, and adaptability to AGC operating conditions and the characteristics of coal-based hard carbon materials has important engineering application value. Summary of the Invention
[0011] The technical problem to be solved by this invention is to address the shortcomings of the prior art by providing a method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions. This method addresses the shortcomings of existing supercapacitor cycle life prediction methods, which are mainly based on constant current and constant voltage conditions and are difficult to adapt to the load characteristics of AGC frequency modulation with random amplitude variations, high-rate pulses, and frequent forward and reverse switching. Furthermore, these methods do not consider the anisotropic mechanical properties of the coal-based hard carbon layered structure and the evolution of pore structure formed by the combined effects of pore collapse and crack propagation. Additionally, they typically directly establish empirical relationships between the number of cycles and capacity or resistance decay, lacking a continuous physical causal relationship from random strain loads, mechanical damage, micropore evolution to macroscopic electrochemical performance degradation and the final state of life, resulting in insufficient accuracy and adaptability of cycle life prediction under actual AGC frequency modulation conditions.
[0012] The present invention adopts the following technical solution: A method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions, characterized by the following steps: The actual strain amplitude of the coal-based hard carbon electrode under each frequency modulation pulse during the AGC frequency modulation process is obtained. Based on the actual strain amplitude, the elastic modulus, fatigue strength limit, anisotropic stress concentration factor of the coal-based hard carbon material, and the load sequence correction factor corresponding to each frequency modulation pulse, the cumulative damage value of the coal-based hard carbon electrode at the current moment is calculated. The pore collapse term is determined based on the cumulative damage value, and the crack propagation term is determined by time integration with attenuation weight on the cumulative damage value. The porosity of the coal-based hard carbon electrode at the current moment is calculated in combination with the initial porosity of the coal-based hard carbon electrode. Calculate the equivalent series resistance of the supercapacitor at the current moment based on the porosity of the coal-based hard carbon electrode, the initial porosity, and the initial equivalent series resistance of the supercapacitor. The instantaneous equivalent degradation rate at the current moment is determined based on the time series of the equivalent series resistance. The remaining cycle life of the supercapacitor is calculated based on the equivalent series resistance of the supercapacitor at the current moment, the instantaneous equivalent degradation rate, the equivalent series resistance failure threshold determined according to the AGC frequency modulation power response requirements, and the average pulse frequency of AGC frequency modulation.
[0013] Furthermore, the calculation of the cumulative damage value of the coal-based hard carbon electrode at the current moment includes: The corresponding stress amplitude is determined based on the actual strain amplitude of the coal-based hard carbon electrode under the i-th frequency modulation pulse and the elastic modulus of the coal-based hard carbon material. The stress amplitude is then corrected based on the anisotropic stress concentration factor of the coal-based hard carbon material to obtain the equivalent damage stress. The equivalent damage strain corresponding to the i-th frequency modulation pulse is determined based on the equivalent damage stress and the fatigue strength limit of the coal-based hard carbon material. Then, the damage caused by each frequency modulation pulse from the initial time to the current time is accumulated by combining the load sequence correction coefficient of the i-th frequency modulation pulse to obtain the cumulative damage value of the coal-based hard carbon electrode at the current time.
[0014] Furthermore, the actual strain amplitude is acquired in real time by a resistance strain gauge set on the surface of the coal-based hard carbon electrode; when a resistance strain gauge cannot be set, the actual strain amplitude is calculated by converting the pre-calibrated correspondence between the amplitude of the frequency-modulated pulse current and the amplitude of the electrode strain. The elastic modulus was determined by nanoindentation and the arithmetic mean of measurements taken at least 5 different locations was used. The fatigue strength limit was determined by a three-point bending fatigue test. The anisotropic stress concentration factor was obtained by observing the microstructure of coal-based hard carbon materials using a scanning electron microscope and by combining it with finite element simulation calculations. The load sequence correction coefficient was determined by amplitude fatigue test of coal-based hard carbon material, and its functional relationship with stress ratio was obtained by fitting.
[0015] Furthermore, the calculation of the porosity of the coal-based hard carbon electrode at the current moment includes: The pore collapse term is determined based on the cumulative damage value and pore collapse coefficient at the current moment. The pore collapse term is used to characterize the reduction in porosity caused by the compaction of coal-based hard carbon layered structures under cyclic stress. The crack propagation term is determined based on the cumulative damage value from the initial time to the current time, the crack propagation coefficient, and the crack propagation attenuation coefficient. The crack propagation term is used to characterize the increase in porosity caused by crack propagation at the bedding interface. The porosity of the coal-based hard carbon electrode at the current moment is determined based on the initial porosity of the coal-based hard carbon electrode, the pore collapse term, and the crack propagation term.
[0016] Furthermore, the initial porosity is determined by mercury intrusion porosimetry, and the arithmetic mean of at least three parallel sample measurements is taken. The pore collapse coefficient was obtained by performing mercury intrusion porosimetry on coal-based hard carbon electrodes with different cumulative damage levels and fitting the linear relationship between porosity and cumulative damage value. The crack propagation coefficient was obtained by observing the electrode crack density after different cycles using a scanning electron microscope and then fitting the results with image analysis. The crack propagation attenuation coefficient was obtained by long-term cyclic testing to determine the change in crack propagation rate over time and by fitting an exponential decay curve.
[0017] Furthermore, the crack propagation term is determined by performing a time-weighted integral on the cumulative damage value, wherein the crack propagation attenuation coefficient is used to attenuate and weight the cumulative damage value at different times. The time-weighted integral is calculated using a numerical integration method, specifically the trapezoidal rule, with an integration step size of no more than 1 second.
[0018] Furthermore, the calculation of the equivalent series resistance of the supercapacitor at the current moment includes: The ion transport resistance of the electrolyte in the porous structure of the coal-based hard carbon electrode is determined based on the porosity of the coal-based hard carbon electrode, and the equivalent series resistance of the supercapacitor at the current moment is determined based on the change of the ion transport resistance at the current moment relative to the ion transport resistance at the initial moment. The initial equivalent series resistance of the supercapacitor was determined using the 1kHz AC impedance method, and the arithmetic mean of at least three parallel sample measurements was taken.
[0019] Furthermore, the time series of the equivalent series resistance of the supercapacitor is numerically differentiated to obtain the first derivative of the equivalent series resistance with respect to time at the current moment, and the first derivative is determined as the instantaneous equivalent degradation rate; the numerical differentiation adopts the backward difference method, or the central difference method is adopted when performing offline smoothing processing on the time series of the equivalent series resistance.
[0020] Furthermore, the failure threshold of the equivalent series resistance is 1.5 times the initial equivalent series resistance of the supercapacitor; Based on the difference between the equivalent series resistance failure threshold and the equivalent series resistance of the supercapacitor at the current moment, and the instantaneous equivalent degradation rate, the remaining lifetime time from the current moment until the equivalent series resistance failure threshold is reached is determined. The average pulse frequency of AGC frequency modulation is determined by statistically analyzing at least 7 consecutive days of AGC frequency modulation data, and the remaining cycle life of the supercapacitor is determined based on the remaining lifespan and the average pulse frequency.
[0021] Secondly, embodiments of the present invention provide a cycle life prediction system for a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions, comprising: The strain load acquisition module is used to acquire the actual strain amplitude of the coal-based hard carbon electrode under each frequency modulation pulse during the AGC frequency modulation process; The cumulative damage calculation module is used to calculate the cumulative damage value of the coal-based hard carbon electrode at the current moment based on the actual strain amplitude, the elastic modulus of the coal-based hard carbon material, the fatigue strength limit, the anisotropic stress concentration factor, and the load sequence correction factor corresponding to each frequency modulation pulse. The porosity evolution calculation module is used to determine the pore collapse term based on the cumulative damage value, and to determine the crack propagation term by performing a time integral with attenuation weight on the cumulative damage value, and to calculate the porosity of the coal-based hard carbon electrode at the current moment in combination with the initial porosity of the coal-based hard carbon electrode. The equivalent series resistance calculation module is used to calculate the equivalent series resistance of the supercapacitor at the current moment based on the porosity of the coal-based hard carbon electrode at the current moment, the initial porosity, and the initial equivalent series resistance of the supercapacitor. The cycle life prediction module is used to determine the instantaneous equivalent degradation rate based on the time series of the equivalent series resistance, and to calculate the remaining cycle life of the supercapacitor based on the current equivalent series resistance of the supercapacitor, the instantaneous equivalent degradation rate, the equivalent series resistance failure threshold determined according to the AGC frequency modulation power response requirements, and the average pulse frequency of AGC frequency modulation.
[0022] Thirdly, a computer device includes a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the computer program to implement the steps of the above-described method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions.
[0023] Fourthly, embodiments of the present invention provide a computer-readable storage medium including a computer program, which, when executed by a processor, implements the steps of the above-described method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions.
[0024] Compared with the prior art, the present invention has at least the following beneficial effects: A method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions is proposed. This method avoids directly fitting capacitance or resistance degradation to the number of cycles, instead transferring the AGC load layer by layer to the macroscopic electrochemical performance degradation, thus providing a clear physical basis for the life prediction process. Simultaneously, it incorporates the loading sequence, the anisotropy of coal-based hard carbon, the dual evolution mechanism of porosity, and the dynamic degradation rate of ESR, enabling the model to adapt to AGC random amplitude variations, high rates, and frequent reverse switching conditions. Experimental results show that the relative prediction error of the method is controlled within 4%.
[0025] Furthermore, a load sequence correction coefficient is used to correct for the damage differences caused by the sequential application of loads of different amplitudes, and an anisotropic stress concentration coefficient is used to characterize the stress concentration at the interface of coal-based hard carbon layers. The purpose of this is to compensate for the shortcomings of the traditional Miner linear cumulative damage theory, which does not consider the load sequence and assumes material isotropy, so that actual random frequency-modulated pulses can be converted into a unified cumulative damage index, providing input that is more consistent with the actual stress state of coal-based hard carbon for subsequent pore structure evolution.
[0026] Furthermore, the purpose of employing resistance strain gauges, nanoindentation, three-point bending fatigue tests, SEM combined with finite element simulation, and amplitude fatigue tests is to ensure that the key parameters in the cumulative damage model have measurable and calibrable sources, reduce the parameter uncertainty caused by simply relying on empirical assignments, and facilitate the recalibration of the model for different coal-based hard carbon materials.
[0027] Furthermore, the pore collapse term characterizes the decrease in porosity caused by the compaction of the coal-based hard carbon layered structure due to cyclic stress, while the crack propagation term characterizes the increase in porosity caused by the formation and propagation of microcracks at the bedding interfaces. This approach can describe the evolution of porosity during the AGC cycle, where it initially decreases and then increases, avoiding the problem that a single pore compaction model cannot cover the entire lifespan.
[0028] Furthermore, the coefficients in the pore evolution model are correlated with actual mercury intrusion porosimetry, SEM crack density analysis, and long-term cyclic tests, so that the contributions of the two mechanisms of pore collapse and crack propagation can be experimentally calibrated separately, thereby improving the model's adaptability to different coal-based hard carbon electrodes.
[0029] Furthermore, the cumulative damage value is integrated over time with attenuation weights using a trapezoidal method with an integration step size of no more than 1 second. This reflects the characteristics of crack propagation having a time-cumulative effect and the influence of historical damage decaying over time. Numerical integration allows the continuous-time damage accumulation to be calculated using discretely acquired data, thereby obtaining the crack propagation amount for use in the porosity model.
[0030] Furthermore, the change in ion transport resistance was determined by utilizing the porosity variation of a coal-based hard carbon electrode, and the ESR of the supercapacitor was further determined. This transforms the microscopic pore structure evolution, which is difficult to directly use for lifetime assessment, into measurable macroscopic electrochemical parameters. Under the aforementioned AGC condition, over 90% of the ESR increase throughout the entire lifetime comes from the change in ion transport resistance caused by porosity variations, thus reducing the number of parameters required for traditional multi-factor ESR models.
[0031] Furthermore, the ESR time series is numerically differentiated, and the first derivative of the current ESR with respect to time is used as the instantaneous equivalent degradation rate. This replaces the constant degradation rate assumption in traditional degradation trajectory extrapolation methods, enabling lifetime prediction to be dynamically updated according to the pore structure and ESR degradation state. Back-difference method is used for real-time calculation, and central difference method is used for offline smoothing. This is used to obtain the current degradation rate from the discrete ESR sequence, providing real-time parameters for remaining lifetime extrapolation.
[0032] Furthermore, the failure threshold for AGC operation is set at 1.5 times the initial ESR value, and the remaining cycle count is determined using the remaining lifetime and the average pulse frequency of AGC. By aligning the final lifetime state with the power output capability required by AGC, and by statistically analyzing AGC data for at least 7 consecutive days to determine the average pulse frequency, the remaining lifetime on the time scale can be converted into the actual number of frequency modulation cycles.
[0033] It is understood that the beneficial effects of the second to fourth aspects mentioned above can be found in the relevant descriptions in the first aspect mentioned above, and will not be repeated here.
[0034] In summary, this invention establishes a continuous physical prediction chain for AGC random amplitude, high magnification and frequent reversal conditions, including strain load, mechanical damage, pore evolution, ESR growth and remaining cycle life. Combined with the anisotropy of coal-based hard carbon, pore collapse and crack propagation characteristics, it achieves dynamic prediction of supercapacitor cycle life, improving the adaptability to operating conditions and prediction accuracy.
[0035] The technical solution of the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Attached Figure Description
[0036] Figure 1 This is a flowchart of the method of the present invention; Figure 2 This is a comparison chart of cycle life prediction results using different methods of the present invention; Figure 3 A comparison chart of the relative errors in cycle lifetime prediction using different methods of the present invention; Figure 4 A schematic diagram of a computer device provided in an embodiment of the present invention; Figure 5This is a block diagram of an electronic device according to an embodiment of the present invention.
[0037] Among them, 60. Computer equipment; 61. Processor; 62. Memory; 63. Computer program; 600. Electronic device; 610. Processing unit; 620. Storage unit; 6201. Random access memory unit; 6202. Cache memory unit; 6203. Read-only memory unit; 6204. Program / utility; 6205. Program module; 630. Bus; 640. Display unit; 650. Input / output interface; 660. Network adapter; 700. External device. Detailed Implementation
[0038] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0039] In the description of this invention, it should be understood that the terms "comprising" and "including" indicate the presence of the described features, integrals, steps, operations, elements and / or components, but do not exclude the presence or addition of one or more other features, integrals, steps, operations, elements, components and / or collections thereof.
[0040] It should also be understood that the terminology used in this specification is for the purpose of describing particular embodiments only and is not intended to limit the invention. As used in this specification and the appended claims, the singular forms “a,” “an,” and “the” are intended to include the plural forms unless the context clearly indicates otherwise.
[0041] It should also be further understood that the term "and / or" as used in this specification and the appended claims refers to any combination and all possible combinations of one or more of the associated listed items, and includes such combinations. For example, A and / or B can represent three cases: A alone, A and B simultaneously, and B alone. Additionally, the character " / " in this invention generally indicates that the preceding and following objects have an "or" relationship.
[0042] It should be understood that although terms such as first, second, third, etc., may be used in the embodiments of the present invention to describe the preset range, these preset ranges should not be limited to these terms. These terms are only used to distinguish the preset ranges from one another. For example, without departing from the scope of the embodiments of the present invention, the first preset range may also be referred to as the second preset range, and similarly, the second preset range may also be referred to as the first preset range.
[0043] Depending on the context, the word "if" as used here can be interpreted as "when," "when," "in response to determination," or "in response to detection." Similarly, depending on the context, the phrase "if determination" or "if detection (of the stated condition or event)" can be interpreted as "when determination," "in response to determination," "when detection (of the stated condition or event)," or "in response to detection (of the stated condition or event)."
[0044] The accompanying drawings illustrate various structural schematic diagrams according to embodiments disclosed in this invention. These drawings are not to scale, and some details have been enlarged for clarity, and some details may have been omitted. The shapes of the various regions and layers shown in the drawings, as well as their relative sizes and positional relationships, are merely exemplary and may deviate from reality due to manufacturing tolerances or technical limitations. Furthermore, those skilled in the art can design regions / layers with different shapes, sizes, and relative positions as needed.
[0045] This invention provides a method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions. Addressing the unique characteristics of AGC frequency modulation, such as random amplitude variations, high-rate pulses, and frequent forward and reverse switching, it establishes a continuous physical prediction chain: "strain load—mechanical damage—pore evolution—equivalent series resistance (ESR) growth—remaining cycle life." Compared to directly using empirical fitting based on the relationship between cycle number and capacitance or resistance decay, this invention first calculates the cumulative damage value by combining a load sequence correction coefficient and the anisotropic stress concentration coefficient of coal-based hard carbon, enabling damage characterization to reflect the random load sequence of AGC and the layered structural characteristics of coal-based hard carbon. Furthermore, it simultaneously considers two competing mechanisms: pore collapse and crack propagation, describing the evolution law of pore size decreasing first and then increasing during cycling. Finally, it converts pore structure changes into measurable ESR changes and uses the instantaneous equivalent degradation rate of ESR and the failure threshold corresponding to the AGC power response to predict the remaining cycle life. This improves the model's adaptability to actual AGC conditions and coal-based hard carbon materials, giving the life prediction a clear physical basis and continuous degradation logic; experimental results show that the prediction relative error is controlled within 4%.
[0046] Please see Figure 1 This invention discloses a method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions, comprising the following steps: Step 1: Calculate the real-time cumulative damage value D(t) of the coal-based hard carbon electrode. By converting the random strain loads collected during AGC frequency modulation into a unified dimensionless cumulative damage value, the degree of mechanical damage to the electrode material is quantified.
[0047] It should be noted that the AGC frequency modulation pulse applies an electrochemical-mechanical coupled load to the coal-based hard carbon electrode: during the charging and discharging process, the insertion and extraction of ions between the coal-based hard carbon layers cause periodic changes in the interlayer spacing, which macroscopically manifests as the volume strain of the electrode. The larger the amplitude and the higher the multiplier of the frequency modulation pulse, the larger the strain amplitude of the electrode. Frequent charging and discharging pulses form a strain load with random amplitude.
[0048] In one embodiment, a resistance strain gauge is attached to the surface of a coal-based hard carbon electrode before the supercapacitor cell is packaged. The signal lead of the strain gauge is led out through a lead-out hole on the cell's outer shell, and the lead-out hole is sealed with electrolyte-resistant sealant. The strain signal is recorded in real time by a strain acquisition system at a sampling frequency of not less than 1 kHz. In another embodiment, a resistance strain gauge may not be used. Instead, the amplitude of a frequency-modulated pulse current and the electrode strain amplitude are synchronously acquired in the calibration test beforehand to establish a correlation curve between the two. During actual operation, the actual strain amplitude is calculated from this correlation curve based on the acquired frequency-modulated pulse current amplitude.
[0049] Real-time stress-strain accumulation model of coal-based hard carbon electrode under AGC frequency modulation condition The Miner linear cumulative damage theory in mechanics of materials is as follows:
[0050] in, This represents the total damage value. For the first Number of cycles of the load level, For the first Fatigue life of materials under high load.
[0051] Hooke's Law states:
[0052] in, For stress, For elastic modulus, In response to the situation.
[0053] The original Miner theory has two inherent flaws: first, it does not consider the influence of load sequence on damage accumulation; second, it assumes that the material is isotropic. To address the random pulse load characteristics of AGC frequency modulation, this invention introduces a load sequence correction coefficient. This is used to correct the damage acceleration effect when high loads occur before low loads; for the layered anisotropic structure of coal-based hard carbon, an anisotropic stress concentration factor is introduced. It is used to correct stress concentration at the bedding interface.
[0054] According to Hooke's law, the strain amplitude The corresponding stress amplitude is After considering anisotropic stress concentration, the equivalent damage stress is: Define equivalent damage strain. The damage caused by a single pulse is ,in, This represents the fatigue strength limit of the material.
[0055] Combined with load sequence correction factor Finally, the formula for calculating the real-time cumulative damage value is obtained.
[0056]
[0057]
[0058] in, For dimensionless strain, The dimension of is Pa. The dimension of is Pa, therefore It is a dimensionless quantity; This is a dimensionless correction factor. Dimensionless count; This is the dimensionless cumulative damage value, with completely consistent dimensions.
[0059] for The cumulative damage value of the coal-based hard carbon electrode at any given time, ranging from 0 to 1. This indicates that the material has undergone macroscopic fracture. From the initial moment to The total number of AGC frequency modulation pulses within a given time period is obtained directly through the AGC operating condition data acquisition system, with a sampling frequency of no less than 1kHz. For the first The load sequence correction coefficient of the secondary frequency modulation pulse was determined through amplitude-dependent fatigue tests on coal-based hard carbon materials, and its functional relationship with the stress ratio was obtained by fitting. For the first The equivalent damage strain of the secondary frequency-modulated pulse is an intermediate calculation result. The elastic modulus of coal-based hard carbon materials was determined using the nanoindentation method, and the arithmetic mean of measurements taken at at least five different locations was used. To determine the fatigue strength limit of coal-based hard carbon materials, a three-point bending fatigue test was used. The maximum stress value that prevents fracture in the next cycle The anisotropic stress concentration factor of the coal-based hard carbon material is obtained by observing the material's microstructure using scanning electron microscopy (SEM) and combining it with finite element simulation calculations. For the first The actual strain amplitude of the electrode under the action of the secondary frequency modulation pulse is acquired in real time by a resistance strain gauge attached to the electrode surface.
[0060] The complex and variable random strain loads during AGC frequency modulation are converted into cumulative damage values with unified physical meaning, enabling quantitative comparison of damage levels under different working conditions and providing a unique input for subsequent microporous structure evolution models.
[0061] In one embodiment of the present invention, the parameters involved in step 1 are calibrated as follows: the elastic modulus is determined by nanoindentation method, and measurements are taken at least 5 different locations on the surface of the coal-based hard carbon electrode. The arithmetic mean of the measured values is taken. In this embodiment, the elastic modulus is measured to be 8.6 GPa; the fatigue strength limit is determined by three-point bending fatigue test, and 10... 7 The maximum stress value that does not fracture in one cycle was measured to be 26 MPa in this embodiment.
[0062] The anisotropic stress concentration factor is obtained by observing the bedding orientation and bedding interface morphology of coal-based hard carbon materials using a scanning electron microscope. Based on this, a representative volume element finite element model containing the bedding structure is established. A unit uniformly distributed load is applied to the boundary of the model, and the ratio of the maximum principal stress to the nominal stress at the bedding interface is calculated. This ratio is determined as the anisotropic stress concentration factor. In this embodiment, the anisotropic stress concentration factor is measured to be 2.1.
[0063] The load sequence correction factor is obtained as follows: Two-stage stress block spectrum amplitude fatigue tests are conducted on coal-based hard carbon materials, using two loading sequences: high load first, low load second, and low load first, high load second. The difference in fatigue life under the two loading sequences is statistically analyzed, and a functional relationship between the load sequence correction factor and the ratio of adjacent pulse stress amplitudes is fitted. In this embodiment, the fitting result is: when the stress amplitude of the preceding pulse is greater than the stress amplitude of the current pulse, the load sequence correction factor is 1 + 0.2 × (the ratio of the stress amplitude of the preceding pulse to the stress amplitude of the current pulse - 1); otherwise, it is 1. For other batches of coal-based hard carbon materials, the above parameters can be recalibrated according to the same test procedure.
[0064] Step 2: Calculate the real-time porosity of the coal-based hard carbon electrode. ; By establishing a quantitative relationship between cumulative damage value and electrode microporosity, the evolution of pore structure under the combined action of pore collapse and crack propagation mechanisms during AGC cycles is described.
[0065] Electrode microporosity evolution model based on stress-strain accumulation The differential form of the Kozeny-Carman equation in porous media mechanics is:
[0066] in, Porosity and is a material constant.
[0067] Paris's law of crack propagation in fracture mechanics is as follows:
[0068] in, The length of the crack. The number of loops. This represents the stress intensity factor amplitude. and is a material constant.
[0069] The original Kozeny-Carman equation only describes the porosity reduction process caused by pore compaction and cannot explain the phenomenon observed in AGC cycles where porosity initially decreases and then increases. This invention experimentally reveals that coal-based hard carbon exhibits two competing microstructural evolution mechanisms simultaneously during AGC cycles: 1. Pore collapse mechanism: Under cyclic stress, the layered structure of coal-based hard carbon undergoes compaction, leading to a decrease in porosity; 2. Crack propagation mechanism: Stress concentration causes microcracks to form at the layer boundaries and gradually propagate, leading to an increase in porosity.
[0070] The present invention uses the cumulative damage value obtained in step 1 As the sole driving factor for both mechanisms, the pore collapse mechanism is proportional to the instantaneous cumulative damage value, using... It means that, among them The pore collapse coefficient is used; the crack propagation mechanism has a time-cumulative effect and gradually decays with stress release. It means that, among them Let be the crack propagation coefficient. This is the crack propagation attenuation coefficient.
[0071] By combining the effects of the two mechanisms, a formula for calculating real-time porosity is finally obtained.
[0072]
[0073] in, The initial porosity is a dimensionless quantity. The coefficient is dimensionless. Since it is a dimensionless quantity, therefore It is a dimensionless quantity; The dimension of time is Integral term Its dimension is time, therefore It is a dimensionless quantity; ultimately Porosity is dimensionless, while other dimensions are completely consistent.
[0074] for The porosity of the coal-based hard carbon electrode at any given time ranges from 0 to 1. The initial porosity of the coal-based hard carbon electrode was determined using mercury intrusion porosimetry (MIP), and the arithmetic mean of at least three parallel samples was taken. The pore collapse coefficient is obtained by fitting a linear relationship between porosity and cumulative damage value through mercury porosimetry tests on electrodes with different cumulative damage levels. for The cumulative damage value at any given time. denoted as the crack propagation coefficient, and denoted as a dimensionless quantity. The crack density of the electrode after different cycles was observed using SEM and fitted using image analysis techniques. The crack propagation attenuation coefficient is obtained by measuring the change in crack propagation rate over time through long-term cyclic testing and fitting an exponential decay curve. The time-weighted cumulative damage integral is calculated using a numerical integration method, with the trapezoidal rule recommended. The integration step size should not exceed 1 second.
[0075] A quantitative bridge was established between macroscopic mechanical damage and microscopic pore structure evolution, distinguishing the different contributions of two competing mechanisms to porosity, and providing a unique input for the subsequent equivalent series resistance growth model.
[0076] It should be noted that the microcracks formed by the crack propagation mechanism are mainly located at the bedding boundaries of coal-based hard carbon. After the cyclic stress is released, most of them are in a closed or semi-closed state and are not fully wetted by the electrolyte. Their pore volume basically does not participate in the ion transport process. Therefore, this invention distinguishes the porosity of the coal-based hard carbon electrode into apparent porosity and effective porosity: apparent porosity is the porosity measured by mercury intrusion porosimetry, which includes contributions from both pore collapse and crack propagation mechanisms, and shows an evolutionary trend of first decreasing and then increasing during cycling; effective porosity is the volume fraction of connected pores participating in electrolyte ion transport, determined by subtracting the pore collapse term from the initial porosity, and continuously decreases during cycling. The porosity used in step 3 of this invention to calculate the ion transport resistance is the effective porosity.
[0077] Step 3: Calculate the real-time equivalent series resistance of the supercapacitor.
[0078] By establishing a quantitative relationship between porosity and the equivalent series resistance (ESR) of a supercapacitor, the microstructure evolution is transformed into a directly measurable macroscopic electrochemical performance parameter.
[0079] Formula 3: Equivalent series resistance growth model driven by porosity evolution The theoretical ohmic resistance in electrochemical impedance spectroscopy (EIS) is as follows:
[0080] in, For resistance, Resistivity The current path length. Let be the cross-sectional area through which the current flows.
[0081] The theory of ion transport in porous media is as follows:
[0082] in, The effective conductivity of the electrolyte in a porous medium. The conductivity of the bulk electrolyte. Porosity.
[0083] Existing ESR growth models typically consider multiple factors simultaneously, including ion transport resistance, intrinsic electronic resistance, interfacial contact resistance, and electrolyte decomposition resistance. These models are complex, and the parameters are difficult to measure accurately. This invention, through extensive accelerated aging tests and electrochemical impedance spectroscopy analysis, has for the first time discovered a crucial technical fact: under AGC frequency modulation conditions, over 90% of the ESR growth in coal-based hard carbon hybrid supercapacitors throughout their entire lifespan originates from changes in ion transport resistance caused by porosity variations.
[0084] The growth of interfacial contact resistance and electrolyte decomposition resistance is very slow, contributing less than 10% before the end of the lifespan, and can be ignored. Due to the high conductivity of coal-based hard carbon materials, the intrinsic electronic resistance hardly changes with the number of cycles.
[0085] The above technical facts were verified through the following experiments: Accelerated aging tests were conducted on coal-based hard carbon hybrid supercapacitor samples from the same batch under AGC frequency modulation conditions. Electrochemical impedance spectroscopy (EIS) tests were performed every 20,000 cycles, with a test frequency range of 0.01 Hz to 100 kHz. An equivalent circuit including ohmic resistance, ion transport resistance, a parallel branch of a constant-phase element, and interfacial contact resistance was used to fit the impedance spectra for each test, separating the increase in resistance components with the number of cycles. Statistical results show that throughout the entire lifespan, the increase in ion transport resistance accounts for a stable proportion of the total ESR increase of over 90% (91% to 93% in this example), while the combined contribution of interfacial contact resistance and electrolyte decomposition resistance is less than 10%, and the intrinsic electronic resistance remains essentially unchanged with the number of cycles.
[0086] According to Ohm's resistance theory, ion transport resistance ,in The effective resistivity of the electrolyte, and Combining this with ion transport theory, we can obtain:
[0087] The initial ion transport resistance is:
[0088] Since both intrinsic resistance and initial interface contact resistance are constants, they can be incorporated into the initial ESR. Therefore, the ratio of the ESR at any given time to the initial ESR is equal to the ratio of the ion transport resistance at any given time to the initial ion transport resistance, thus yielding the formula for calculating the real-time ESR.
[0089] Since the closed pores formed by crack propagation do not participate in ion transport, the effective porosity decreases monotonically during the lifetime as the pores continue to collapse, and the ion transport resistance increases monotonically accordingly. Therefore, the equivalent series resistance of the supercapacitor shows a monotonically increasing trend throughout the entire lifetime, which is not contradictory to the evolution trend of apparent porosity decreasing first and then increasing. When the effective porosity decreases to the point that the equivalent series resistance reaches the failure threshold, the supercapacitor is considered to have reached the end of its lifetime.
[0090]
[0091] in, The dimension of Ω; It is a dimensionless ratio; ultimately The dimension of is Ω, and the dimensions are completely consistent.
[0092] for The equivalent series resistance of a supercapacitor at any given time, expressed in Ω. The initial equivalent series resistance of the supercapacitor was determined using the 1kHz AC impedance method, and the arithmetic mean of at least three parallel samples was taken. for Porosity of coal-based hard carbon electrodes at any given time. The initial porosity of the coal-based hard carbon electrode is given.
[0093] The evolution of microscopic pore structure is directly converted into changes in macroscopic electrochemical performance parameters, eliminating the complexity of traditional multi-factor coupled models, significantly improving the computational efficiency and prediction accuracy of the model, and providing a unique input for the final remaining cycle life prediction model.
[0094] Step 4: Calculate the remaining cycle life of the supercapacitor.
[0095] The remaining cycle life of the supercapacitor is calculated by using the real-time degradation rate based on ESR and the failure threshold specific to the AGC condition.
[0096] ESR growth-driven remaining cycle life prediction model The degradation trajectory extrapolation method in reliability engineering is as follows:
[0097] in, For total lifespan, The failure threshold These are the initial performance values. The degradation rate is constant.
[0098] Traditional degradation trajectory extrapolation assumes a constant degradation rate, but the ESR growth rate of supercapacitors under AGC conditions changes dynamically with the evolution of the pore structure. The constant rate assumption leads to a large prediction error.
[0099] This invention proposes the concept of instantaneous equivalent degradation rate, defined as the first derivative of ESR with respect to time at the current moment. This characterizes the rate of performance degradation at the current moment. Remaining lifetime. It equals the difference between the failure threshold and the current ESR value divided by the instantaneous equivalent degradation rate, i.e.:
[0100] Multiply the remaining lifetime by the average pulse frequency of AGC frequency modulation. The remaining cycle life can then be obtained.
[0101] Furthermore, this invention proposes a dynamic failure threshold to address the stringent power characteristic requirements of AGC frequency modulation. When the ESR increases to 1.5 times its initial value, the power output capability of the supercapacitor will decrease by 30%. This is based on the fact that the maximum output power of a supercapacitor is approximately the square of its rated voltage divided by four times its equivalent series resistance. When the equivalent series resistance increases to 1.5 times its initial value, the maximum output power drops to approximately 67% of its initial value, meaning the power output capability decreases by about 30%. This fails to meet the fast response requirements of AGC frequency modulation. Therefore, [the following is a more precise translation:] It replaces the traditional fixed 80% capacity retention rate criterion as a failure criterion.
[0102]
[0103]
[0104] in, The dimension of is Ω / s; The dimension of Ω; The dimension is cycles / s; therefore The dimensions are Secondly, the dimensions are completely consistent.
[0105] for The remaining cycle life of a supercapacitor at any given time, in cycles. for The instantaneous equivalent degradation rate of ESR at time step 3, for the output of step 3 The time series is obtained by numerical differentiation. Back-difference method is used for real-time calculation, while central difference method can be used for offline smoothing of historical series. The ESR failure threshold of the supercapacitor under AGC operating conditions is determined based on the power response requirements of AGC frequency modulation. This invention takes... , for The equivalent series resistance of the supercapacitor at any given time is the sole output of step 3. The average pulse frequency for AGC frequency modulation is obtained by statistically analyzing AGC operating data for at least 7 consecutive days and calculating the arithmetic mean of the number of pulses.
[0106] By directly converting the dynamic changes of macroscopic electrochemical performance parameters into remaining cycle life, real-time and accurate prediction of supercapacitor life is achieved, providing a scientific basis for the operation and maintenance management and life assessment of AGC energy storage systems.
[0107] In another embodiment of the present invention, a cycle life prediction system for a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation condition is provided. This system can be used to implement the above-mentioned method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation condition. Specifically, the cycle life prediction system for a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation condition includes a strain load acquisition module, a cumulative damage calculation module, a porosity evolution calculation module, an equivalent series resistance calculation module, and a cycle life prediction module.
[0108] Among them, the strain load acquisition module is used to acquire the actual strain amplitude of the coal-based hard carbon electrode under the action of each frequency modulation pulse during the AGC frequency modulation process; The cumulative damage calculation module is used to calculate the cumulative damage value of the coal-based hard carbon electrode at the current moment based on the actual strain amplitude, the elastic modulus of the coal-based hard carbon material, the fatigue strength limit, the anisotropic stress concentration factor, and the load sequence correction factor corresponding to each frequency modulation pulse. The porosity evolution calculation module is used to determine the pore collapse term based on the cumulative damage value, and to determine the crack propagation term by performing a time integral with attenuation weight on the cumulative damage value, and to calculate the porosity of the coal-based hard carbon electrode at the current moment in combination with the initial porosity of the coal-based hard carbon electrode. The equivalent series resistance calculation module is used to calculate the equivalent series resistance of the supercapacitor at the current moment based on the porosity of the coal-based hard carbon electrode at the current moment, the initial porosity, and the initial equivalent series resistance of the supercapacitor. The cycle life prediction module is used to determine the instantaneous equivalent degradation rate based on the time series of the equivalent series resistance, and to calculate the remaining cycle life of the supercapacitor based on the current equivalent series resistance of the supercapacitor, the instantaneous equivalent degradation rate, the equivalent series resistance failure threshold determined according to the AGC frequency modulation power response requirements, and the average pulse frequency of AGC frequency modulation.
[0109] This invention provides a terminal device comprising a processor and a memory. The memory stores a computer program, which includes program instructions. The processor executes the program instructions stored in the computer storage medium. The processor may be a Central Processing Unit (CPU), or other general-purpose processors, graphics processing units (GPUs), tensor processing units (TPUs), digital signal processors (DSPs), application-specific integrated circuits (ASICs), field-programmable gate arrays (FPGAs), or other programmable logic devices, discrete gate or transistor logic devices, discrete hardware components, etc. It is the computing and control core of the terminal, suitable for implementing one or more instructions, specifically suitable for loading and executing one or more instructions to achieve a corresponding method flow or function. The processor described in this embodiment can be used in the operation of a method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions, including: The actual strain amplitude of the coal-based hard carbon electrode under each frequency modulation pulse during AGC frequency modulation is obtained. Based on the actual strain amplitude, the elastic modulus, fatigue strength limit, anisotropic stress concentration factor, and load sequence correction factor corresponding to each frequency modulation pulse, the cumulative damage value of the coal-based hard carbon electrode at the current moment is calculated. The pore collapse term is determined based on the cumulative damage value, and the crack propagation term is determined by time integration with attenuation weight on the cumulative damage value. The porosity of the coal-based hard carbon electrode at the current moment is calculated in combination with the initial porosity of the coal-based hard carbon electrode. Based on the porosity of the coal-based hard carbon electrode at the current moment, the initial porosity, and the initial equivalent series resistance of the supercapacitor, the equivalent series resistance of the supercapacitor at the current moment is calculated. The instantaneous equivalent degradation rate at the current moment is determined based on the time series of the equivalent series resistance. Based on the equivalent series resistance of the supercapacitor at the current moment, the instantaneous equivalent degradation rate, the equivalent series resistance failure threshold determined according to the AGC frequency modulation power response requirements, and the average pulse frequency of AGC frequency modulation, the remaining cycle life of the supercapacitor is calculated.
[0110] Please see Figure 4 The terminal device is a computer device. In this embodiment, the computer device 60 includes a processor 61, a memory 62, and a computer program 63 stored in the memory 62 and executable on the processor 61. When the processor 61 executes the computer program 63, it implements the method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions as described in this embodiment. To avoid repetition, these details are not elaborated here. Alternatively, when the processor 61 executes the computer program 63, it implements the functions of each model / unit in the system for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions as described in this embodiment. To avoid repetition, these details are not elaborated here.
[0111] Computer device 60 can be a desktop computer, laptop, handheld computer, cloud server, or other computing device. Computer device 60 may include, but is not limited to, a processor 61 and a memory 62. Those skilled in the art will understand that... Figure 4 This is merely an example of computer device 60 and does not constitute a limitation on computer device 60. It may include more or fewer components than shown, or combine certain components, or different components. For example, computer device may also include input / output devices, network access devices, buses, etc.
[0112] The processor 61 may be a Central Processing Unit (CPU), or other general-purpose processors, graphics processing units (GPUs), tensor processing units (TPUs), digital signal processors (DSPs), application-specific integrated circuits (ASICs), field-programmable gate arrays (FPGAs), or other programmable logic devices, discrete gate or transistor logic devices, discrete hardware components, etc. A general-purpose processor may be a microprocessor or any conventional processor.
[0113] The memory 62 can be an internal storage unit of the computer device 60, such as a hard disk or memory of the computer device 60. The memory 62 can also be an external storage device of the computer device 60, such as a plug-in hard disk, smart media card (SMC), secure digital (SD) card, flash card, etc. equipped on the computer device 60.
[0114] Furthermore, the memory 62 may include both internal storage units of the computer device 60 and external storage devices. The memory 62 is used to store computer programs and other programs and data required by the computer device. The memory 62 can also be used to temporarily store data that has been output or will be output.
[0115] Please see Figure 5 The terminal device is an electronic device 600, which is manifested in the form of a general-purpose computing device. The components of the electronic device may include, but are not limited to: at least one processing unit 610, at least one storage unit 620, a bus 630 connecting different platform components (including storage unit 620 and processing unit 610), a display unit 640, etc.
[0116] The storage unit stores program code, which can be executed by the processing unit 610 to perform the steps described in the method section of this specification according to various exemplary embodiments of the present invention. For example, the processing unit 610 can perform actions such as... Figure 1 The steps are shown in the figure.
[0117] Storage unit 620 may include readable media in the form of volatile storage units, such as random access memory (RAM) 6201 and / or cache memory 6202, and may further include read-only memory (ROM) 6203.
[0118] Storage unit 620 may also include a program / utility 6204 having a set (at least one) program module 6205, such program module 6205 including but not limited to: operating system, one or more application programs, other program modules and program data, each or some combination of these examples may include an implementation of a network environment.
[0119] Bus 630 can represent one or more of several types of bus structures, including a memory cell bus or memory cell controller, a peripheral bus, a graphics acceleration port, a processing unit, or a local bus using any of the multiple bus structures.
[0120] Electronic device 600 can also communicate with one or more external devices 700 (e.g., keyboard, pointing device, Bluetooth device, etc.), and with one or more devices that enable a user to interact with electronic device 600, and / or with any device that enables electronic device 600 to communicate with one or more other computing devices (e.g., router, modem). This communication can be performed via input / output interface 650. Furthermore, electronic device 600 can also communicate with one or more networks (e.g., local area network, wide area network, and / or public network, such as the Internet) via network adapter 660. Network adapter 660 can communicate with other modules of electronic device 600 via bus 630. It should be understood that, although not shown in the figures, other hardware and / or software modules can be used in conjunction with electronic device 600, including but not limited to: microcode, device drivers, redundant processing units, external disk drive arrays, RAID systems, tape drives, and data backup storage platforms.
[0121] This invention also provides a storage medium, specifically a computer-readable storage medium, which is a memory device in a terminal device for storing programs and data. It is understood that the computer-readable storage medium here can include both built-in storage media in the terminal device and extended storage media supported by the terminal device; it can be any tangible medium containing or storing a program that can be used by or in conjunction with an instruction execution system, apparatus, or device. The computer-readable storage medium provides storage space that stores the terminal's operating system. Furthermore, the storage space also stores one or more instructions suitable for loading and execution by a processor, which can be one or more computer programs (including program code). More specific examples of the computer-readable storage medium include: an electrical connection with one or more wires, a portable disk, a hard disk, random access memory, read-only memory, erasable programmable read-only memory, optical fiber, portable compact disk read-only memory, optical storage device, magnetic storage device, or any suitable combination thereof.
[0122] Computer-readable storage media also include data signals propagated in baseband or as part of a carrier wave, carrying readable program code. Such propagated data signals can take various forms, including but not limited to electromagnetic signals, optical signals, or any suitable combination thereof. A readable storage medium can also be any readable medium other than a readable storage medium that can send, propagate, or transmit a program for use by or in connection with an instruction execution system, apparatus, or device. The program code contained on the readable storage medium can be transmitted using any suitable medium, including but not limited to wireless, wired, optical fiber, radio frequency, etc., or any suitable combination thereof.
[0123] Program code for performing the operations of this invention can be written in any combination of one or more programming languages, including object-oriented programming languages such as Java and C++, and conventional procedural programming languages such as C or similar languages. The program code can execute entirely on the user's computing device, partially on the user's device, as a standalone software package, partially on the user's computing device and partially on a remote computing device, or entirely on a remote computing device or server. In cases involving remote computing devices, the remote computing device can be connected to the user's computing device via any type of network, including a local area network (LAN) or a wide area network (WAN), or it can be connected to an external computing device (e.g., via the Internet using an Internet service provider).
[0124] One or more instructions stored in a computer-readable storage medium can be loaded and executed by a processor to implement the corresponding steps of the method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions in the above embodiments; one or more instructions in the computer-readable storage medium are loaded and executed by the processor in the following steps: The actual strain amplitude of the coal-based hard carbon electrode under each frequency modulation pulse during AGC frequency modulation is obtained. Based on the actual strain amplitude, the elastic modulus, fatigue strength limit, anisotropic stress concentration factor, and load sequence correction factor corresponding to each frequency modulation pulse, the cumulative damage value of the coal-based hard carbon electrode at the current moment is calculated. The pore collapse term is determined based on the cumulative damage value, and the crack propagation term is determined by time integration with attenuation weight on the cumulative damage value. The porosity of the coal-based hard carbon electrode at the current moment is calculated in combination with the initial porosity of the coal-based hard carbon electrode. Based on the porosity of the coal-based hard carbon electrode at the current moment, the initial porosity, and the initial equivalent series resistance of the supercapacitor, the equivalent series resistance of the supercapacitor at the current moment is calculated. The instantaneous equivalent degradation rate at the current moment is determined based on the time series of the equivalent series resistance. Based on the equivalent series resistance of the supercapacitor at the current moment, the instantaneous equivalent degradation rate, the equivalent series resistance failure threshold determined according to the AGC frequency modulation power response requirements, and the average pulse frequency of AGC frequency modulation, the remaining cycle life of the supercapacitor is calculated.
[0125] The databases involved in the embodiments provided in this application may include at least one type of relational database and non-relational database. Non-relational databases may include distributed databases, etc., and are not limited thereto. The processors involved in the embodiments provided in this application may be general-purpose processors, central processing units, graphics processing units, digital signal processors, programmable logic devices, etc., and are not limited thereto.
[0126] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of the present invention. The components of the embodiments of the present invention described and shown in the accompanying drawings can generally be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the claimed invention, but merely to illustrate selected embodiments of the invention. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without inventive effort are within the scope of protection of the present invention.
[0127] Experimental Example To verify the accuracy of the prediction method described in this invention, the following verification experiments were conducted: The prediction accuracy of the prediction method described in this invention is compared with that of the traditional Miner linear damage model and constant degradation rate model in the cycle life prediction under AGC frequency modulation conditions.
[0128] Three sets of identical coal-based hard carbon hybrid supercapacitor cells were prepared, numbered S1, S2, and S3. The negative electrode material was anthracite-based hard carbon, the positive electrode material was activated carbon, and the electrolyte was a 1 mol / L tetraethylammonium tetrafluoroborate / propylene carbonate (TEABF4 / PC) solution. The rated voltage was 2.7V and the rated capacity was 1000F.
[0129] The actual AGC historical data of a provincial power grid from January to March 2024 was used as the test condition. This condition included more than 120,000 frequency modulation pulses with a pulse amplitude range of 0.1C to 5C and an average pulse frequency of 0.08Hz.
[0130] Supercapacitor charge and discharge testing system (Model: NEWALE CT-4008-5V100A) Electrochemical workstation (Model: CHI660E) Strain acquisition system (Model: DH3816N) Scanning electron microscope (model: ZEISS Sigma 300) Mercury porosimeter (Model: Micromeritics AutoPore IV 9500) The specific steps are as follows: Initial performance test The initial equivalent series resistance of the three groups of samples was measured. Initial porosity Elastic modulus Fatigue strength limit and anisotropic stress concentration factor Basic parameters, etc.
[0131] In this experiment, the initial equivalent series resistances of samples S1, S2, and S3 were measured to be 1.48 mΩ, 1.52 mΩ, and 1.51 mΩ, respectively; the initial porosities were 0.615, 0.623, and 0.618, respectively; the elastic moduli were 8.5 GPa, 8.7 GPa, and 8.6 GPa, respectively; the fatigue strength limits were 26 MPa, 25 MPa, and 26 MPa, respectively; and the anisotropic stress concentration factors were 2.1, 2.0, and 2.1, respectively.
[0132] Operating condition cycle test Three groups of samples were placed in a constant temperature environment of 25℃ and subjected to continuous cyclic testing under the aforementioned AGC conditions. The test was paused after every 10,000 cycles, and the real-time equivalent series resistance of the samples was measured. .
[0133] Taking sample S1 as an example, the equivalent series resistances measured at 0 cycles, 50,000 cycles, 100,000 cycles, 150,000 cycles, and reaching the failure threshold (186,200 cycles) were 1.48 mΩ, 1.56 mΩ, 1.68 mΩ, 1.85 mΩ, and 2.22 mΩ, respectively. The changes in the equivalent series resistances of samples S2 and S3 with the number of cycles were consistent with those of sample S1. During the experiment, the equivalent series resistances of each sample showed a monotonically increasing trend, which is consistent with the mechanism of monotonically decreasing effective porosity and monotonically increasing ion transport resistance.
[0134] End of life determination The test was stopped when the equivalent series resistance of the sample increased to 1.5 times the initial value, and the actual number of cycles was recorded. .
[0135] Lifetime prediction calculation Using the method described in this invention, the traditional Miner linear damage model, and the constant degradation rate model, the total cycle life of the samples is predicted based on the experimental data from the first 50,000 cycles. .
[0136] It should be noted that the model parameters of the method of this invention are obtained independently by calibrating separately prepared calibration samples from the same batch according to the experimental methods described in steps 1 and 2 above; during lifetime prediction, only the equivalent series resistance sequence corresponding to the first 50,000 cycles of each sample is used to calculate the instantaneous equivalent degradation rate and extrapolate it, and the calibration test data and lifetime prediction test data are not shared. The calibration results of each model parameter in this experimental example are shown in the table below:
[0137] Error Analysis Calculate the relative prediction errors of the three methods .
[0138] The lifetime prediction results and relative errors of the three methods are shown in the table below:
[0139] Please see Figure 2Using the actual number of cycles for samples S1, S2, and S3 as benchmarks, the cycle lifetime prediction results obtained by the method of this invention, the traditional Miner linear damage model, and the constant degradation rate model were compared. Specifically, the actual number of cycles for sample S1 was 186,200, the predicted value by the method of this invention was 191,300, the predicted value by the traditional Miner linear damage model was 147,500, and the predicted value by the constant degradation rate model was 228,600; the actual number of cycles for sample S2 was 181,500, with corresponding predicted values of 188,700, 142,300, and 235,200; and the actual number of cycles for sample S3 was 189,700, with corresponding predicted values of 184,600, 151,200, and 221,400.
[0140] Depend on Figure 2 As can be seen, the prediction results of the method of this invention for the three groups of samples are all close to the actual number of cycles; the prediction values of the traditional Miner linear damage model for the three groups of samples are all lower than the actual number of cycles, while the prediction values of the constant degradation rate model are all higher than the actual number of cycles. This result shows that it is difficult to accurately characterize the actual degradation process of supercapacitors under AGC random frequency modulation conditions by using only the traditional linear damage accumulation relationship or constant degradation rate, while the prediction relationship of "mechanical damage-pore evolution-ESR growth-remaining cycle life" established by this invention can more accurately track the changes in actual life.
[0141] Please see Figure 3 The relative prediction errors for sample S1 obtained using the method of this invention, the traditional Miner linear damage model, and the constant degradation rate model were 2.74%, 20.78%, and 22.77%, respectively; the relative prediction errors for sample S2 were 3.97%, 21.60%, and 29.59%, respectively; and the relative prediction errors for sample S3 were 2.69%, 20.30%, and 16.71%, respectively.
[0142] Depend on Figure 3 It can be seen that the relative prediction error of the method of the present invention for the three groups of samples is less than 4%, and the prediction error between different samples remains within a small range. In contrast, the average relative error of the traditional Miner linear damage model is 20.89%, and the average relative error of the constant degradation rate model is 23.02%. These results show that the present invention, by considering the AGC frequency-modulated random load sequence, coal-based hard carbon anisotropy, pore collapse and crack propagation, and ESR dynamic degradation process, can reduce the lifetime prediction bias caused by the simplification of working conditions and the constant degradation assumption of the traditional model, and has better AGC working condition adaptability and cycle life prediction accuracy.
[0143] Experimental results show that the prediction method for the cycle life of coal-based hard carbon hybrid supercapacitors under AGC frequency modulation conditions described in this invention has a prediction relative error controlled within 4%, which is far superior to the traditional Miner linear damage model (average error 20.89%) and constant degradation rate model (average error 23.02%). This fully demonstrates that the method of this invention has higher prediction accuracy and better adaptability to operating conditions, and can meet the needs of practical engineering applications.
[0144] In summary, this invention provides a method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions. Addressing the problem that traditional supercapacitor life models struggle to adapt to AGC's random amplitude variations, high-rate pulses, and frequent forward / reverse switching, this method no longer directly extrapolates from empirical relationships between cycle number and capacity or resistance. Instead, it establishes a continuous physical causal chain from actual strain load, accumulated mechanical damage to the coal-based hard carbon electrode, micropore structure evolution, and equivalent series resistance growth to the remaining cycle life. By introducing load sequence correction coefficients and anisotropic stress concentration coefficients, the influence of different pulse sequences and the layered structure of the coal-based hard carbon on damage accumulation can be reflected. Simultaneously, two competing mechanisms—pore collapse and crack propagation—are set up to describe the actual evolution of porosity during AGC cycles, which initially decreases and then increases. Based on this, porosity changes are converted into ion transport resistance and ESR changes, and the remaining cycle life is predicted according to the instantaneous equivalent degradation rate of ESR and the failure threshold corresponding to the AGC power response, allowing the prediction results to be dynamically updated with the actual degradation state. In the verification experiment, the relative error of the prediction method of the present invention was controlled within 4%, which is significantly lower than that of the traditional model being compared.
[0145] Those skilled in the art will clearly understand that, for the sake of convenience and brevity, the above-described division of functional units and modules is merely an example. In practical applications, the above functions can be assigned to different functional units and modules as needed, that is, the internal structure of the device can be divided into different functional units or modules to complete all or part of the functions described above. The functional units and modules in the embodiments can be integrated into one processing unit, or each unit can exist physically separately, or two or more units can be integrated into one unit. The integrated unit can be implemented in hardware or as a software functional unit. Furthermore, the specific names of the functional units and modules are only for easy differentiation and are not intended to limit the scope of protection of this application. The specific working process of the units and modules in the above system can be referred to the corresponding process in the foregoing method embodiments, and will not be repeated here.
[0146] In the above embodiments, the descriptions of each embodiment have different focuses. For parts that are not described in detail or recorded in a certain embodiment, please refer to the relevant descriptions of other embodiments.
[0147] Those skilled in the art will recognize that the units and algorithm steps of the various examples described in conjunction with the embodiments disclosed in this invention can be implemented in electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are implemented in hardware or software depends on the specific application and design constraints of the technical solution. Those skilled in the art can use different methods to implement the described functions for each specific application, but such implementations should not be considered beyond the scope of this invention.
[0148] In the embodiments provided by this invention, it should be understood that the disclosed devices / terminals and methods can be implemented in other ways. For example, the device / terminal embodiments described above are merely illustrative. For instance, the division of modules or units is only a logical functional division, and in actual implementation, there may be other division methods. For example, multiple units or components may be combined or integrated into another system, or some features may be ignored or not executed. Furthermore, the coupling or direct coupling or communication connection shown or discussed may be through some interfaces; the indirect coupling or communication connection between devices or units may be electrical, mechanical, or other forms.
[0149] The units described as separate components may or may not be physically separate. The components shown as units may or may not be physical units; that is, they may be located in one place or distributed across multiple network units. Some or all of the units can be selected to achieve the purpose of this embodiment according to actual needs.
[0150] Furthermore, the functional units in the various embodiments of the present invention can be integrated into one processing unit, or each unit can exist physically separately, or two or more units can be integrated into one unit. The integrated unit can be implemented in hardware or as a software functional unit.
[0151] If the integrated module / unit is implemented as a software functional unit and sold or used as an independent product, it can be stored in a computer-readable storage medium. Based on this understanding, all or part of the processes in the methods of the above embodiments of the present invention can also be implemented by a computer program instructing related hardware. The computer program can be stored in a computer-readable storage medium, and when executed by a processor, it can implement the steps of the various method embodiments described above. The computer program includes computer program code, which can be in the form of source code, object code, executable files, or certain intermediate forms. The computer-readable medium can include: any entity or device capable of carrying the computer program code, a recording medium, a USB flash drive, a portable hard drive, a magnetic disk, an optical disk, a computer memory, a read-only memory (ROM), a random-access memory (RAM), an electrical carrier signal, a telecommunication signal, and a software distribution medium, etc.
[0152] This application is described with reference to flowchart illustrations and / or block diagrams of methods, apparatus, and computer program products according to embodiments of this application. It will be understood that each block of the flowchart illustrations and / or block diagrams, and combinations of blocks in the flowchart illustrations and / or block diagrams, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, special-purpose computer, embedded processor, or other programmable data processing apparatus to produce a machine, such that the instructions, which execute via the processor of the computer or other programmable data processing apparatus, generate instructions for implementing the flowchart... Figure 1 One or more processes and / or boxes Figure 1 A device that provides the functions specified in one or more boxes.
[0153] These computer program instructions may also be stored in a computer-readable storage medium that can direct a computer or other programmable data processing device to function in a particular manner, such that the instructions stored in the computer-readable storage medium produce an article of manufacture including instruction means, which are implemented in a process Figure 1 One or more processes and / or boxes Figure 1 The function specified in one or more boxes.
[0154] These computer program instructions may also be loaded onto a computer or other programmable data processing equipment to cause a series of operational steps to be performed on the computer or other programmable equipment to produce a computer-implemented process, thereby providing instructions that execute on the computer or other programmable equipment for implementing the process. Figure 1 One or more processes and / or boxes Figure 1 The steps of the function specified in one or more boxes.
[0155] The above content is only for illustrating the technical concept of the present invention and should not be construed as limiting the scope of protection of the present invention. Any modifications made to the technical solution based on the technical concept proposed in this invention shall fall within the scope of protection of the claims of this invention.
Claims
1. A method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions, characterized in that... Includes the following steps: The actual strain amplitude of the coal-based hard carbon electrode under each frequency modulation pulse during the AGC frequency modulation process is obtained. Based on the actual strain amplitude, the elastic modulus, fatigue strength limit, anisotropic stress concentration factor of the coal-based hard carbon material, and the load sequence correction factor corresponding to each frequency modulation pulse, the cumulative damage value of the coal-based hard carbon electrode at the current moment is calculated. The pore collapse term is determined based on the cumulative damage value, and the crack propagation term is determined by time integration with attenuation weight on the cumulative damage value. The porosity of the coal-based hard carbon electrode at the current moment is calculated in combination with the initial porosity of the coal-based hard carbon electrode. Calculate the equivalent series resistance of the supercapacitor at the current moment based on the porosity of the coal-based hard carbon electrode, the initial porosity, and the initial equivalent series resistance of the supercapacitor. The instantaneous equivalent degradation rate at the current moment is determined based on the time series of the equivalent series resistance. The remaining cycle life of the supercapacitor is calculated based on the equivalent series resistance of the supercapacitor at the current moment, the instantaneous equivalent degradation rate, the equivalent series resistance failure threshold determined according to the AGC frequency modulation power response requirements, and the average pulse frequency of AGC frequency modulation.
2. The method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions according to claim 1, characterized in that, The calculation of the cumulative damage value of the coal-based hard carbon electrode at the current moment includes: The corresponding stress amplitude is determined based on the actual strain amplitude of the coal-based hard carbon electrode under the i-th frequency modulation pulse and the elastic modulus of the coal-based hard carbon material. The stress amplitude is then corrected based on the anisotropic stress concentration factor of the coal-based hard carbon material to obtain the equivalent damage stress. The equivalent damage strain corresponding to the i-th frequency modulation pulse is determined based on the equivalent damage stress and the fatigue strength limit of the coal-based hard carbon material. Then, the damage caused by each frequency modulation pulse from the initial time to the current time is accumulated by combining the load sequence correction coefficient of the i-th frequency modulation pulse to obtain the cumulative damage value of the coal-based hard carbon electrode at the current time.
3. The method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions according to claim 2, characterized in that, The actual strain amplitude is acquired in real time by a resistance strain gauge set on the surface of the coal-based hard carbon electrode; when a resistance strain gauge cannot be set, the actual strain amplitude is calculated by converting the pre-calibrated correspondence between the amplitude of the frequency-modulated pulse current and the amplitude of the electrode strain. The elastic modulus was determined by nanoindentation and the arithmetic mean of measurements taken at least 5 different locations was used. The fatigue strength limit was determined by a three-point bending fatigue test. The anisotropic stress concentration factor was obtained by observing the microstructure of coal-based hard carbon materials using a scanning electron microscope and by combining it with finite element simulation calculations. The load sequence correction coefficient was determined by amplitude fatigue test of coal-based hard carbon material, and its functional relationship with stress ratio was obtained by fitting.
4. The method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions according to claim 1, characterized in that, The calculation of the porosity of the coal-based hard carbon electrode at the current moment includes: The pore collapse term is determined based on the cumulative damage value and pore collapse coefficient at the current moment. The pore collapse term is used to characterize the reduction in porosity caused by the compaction of coal-based hard carbon layered structures under cyclic stress. The crack propagation term is determined based on the cumulative damage value from the initial time to the current time, the crack propagation coefficient, and the crack propagation attenuation coefficient. The crack propagation term is used to characterize the increase in porosity caused by crack propagation at the bedding interface. The porosity of the coal-based hard carbon electrode at the current moment is determined based on the initial porosity of the coal-based hard carbon electrode, the pore collapse term, and the crack propagation term.
5. The method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions according to claim 4, characterized in that, The initial porosity was determined by mercury intrusion porosimetry, and the arithmetic mean of at least three parallel sample measurements was taken. The pore collapse coefficient was obtained by performing mercury intrusion porosimetry on coal-based hard carbon electrodes with different cumulative damage levels and fitting the linear relationship between porosity and cumulative damage value. The crack propagation coefficient was obtained by observing the electrode crack density after different cycles using a scanning electron microscope and then fitting the results with image analysis. The crack propagation attenuation coefficient was obtained by long-term cyclic testing to determine the change in crack propagation rate over time and by fitting an exponential decay curve.
6. The method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions according to claim 4, characterized in that, The crack propagation term is determined by performing a time-weighted integral on the cumulative damage value, wherein the crack propagation attenuation coefficient is used to attenuate and weight the cumulative damage value at different times. The time-weighted integral is calculated using a numerical integration method, specifically the trapezoidal rule, with an integration step size of no more than 1 second.
7. The method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions according to claim 1, characterized in that, The calculation of the equivalent series resistance of the supercapacitor at the current moment includes: The ion transport resistance of the electrolyte in the porous structure of the coal-based hard carbon electrode is determined based on the porosity of the coal-based hard carbon electrode, and the equivalent series resistance of the supercapacitor at the current moment is determined based on the change of the ion transport resistance at the current moment relative to the ion transport resistance at the initial moment. The initial equivalent series resistance of the supercapacitor was determined using the 1kHz AC impedance method, and the arithmetic mean of at least three parallel sample measurements was taken.
8. The method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions according to claim 1, characterized in that, The time series of the equivalent series resistance of the supercapacitor is numerically differentiated to obtain the first derivative of the equivalent series resistance with respect to time at the current moment, and the first derivative is determined as the instantaneous equivalent degradation rate; the numerical differentiation adopts the backward difference method, or the central difference method is adopted when the time series of the equivalent series resistance is offline smoothed.
9. The method for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions according to claim 8, characterized in that, The failure threshold of the equivalent series resistance is 1.5 times the initial equivalent series resistance of the supercapacitor; Based on the difference between the equivalent series resistance failure threshold and the equivalent series resistance of the supercapacitor at the current moment, and the instantaneous equivalent degradation rate, the remaining lifetime time from the current moment until the equivalent series resistance failure threshold is reached is determined. The average pulse frequency of AGC frequency modulation is determined by statistically analyzing at least 7 consecutive days of AGC frequency modulation data, and the remaining cycle life of the supercapacitor is determined based on the remaining lifespan and the average pulse frequency.
10. A system for predicting the cycle life of a coal-based hard carbon hybrid supercapacitor under AGC frequency modulation conditions, characterized in that, include: The strain load acquisition module is used to acquire the actual strain amplitude of the coal-based hard carbon electrode under each frequency modulation pulse during the AGC frequency modulation process; The cumulative damage calculation module is used to calculate the cumulative damage value of the coal-based hard carbon electrode at the current moment based on the actual strain amplitude, the elastic modulus of the coal-based hard carbon material, the fatigue strength limit, the anisotropic stress concentration factor, and the load sequence correction factor corresponding to each frequency modulation pulse. The porosity evolution calculation module is used to determine the pore collapse term based on the cumulative damage value, and to determine the crack propagation term by performing a time integral with attenuation weight on the cumulative damage value, and to calculate the porosity of the coal-based hard carbon electrode at the current moment in combination with the initial porosity of the coal-based hard carbon electrode. The equivalent series resistance calculation module is used to calculate the equivalent series resistance of the supercapacitor at the current moment based on the porosity of the coal-based hard carbon electrode at the current moment, the initial porosity, and the initial equivalent series resistance of the supercapacitor. The cycle life prediction module is used to determine the instantaneous equivalent degradation rate based on the time series of the equivalent series resistance, and to calculate the remaining cycle life of the supercapacitor based on the current equivalent series resistance of the supercapacitor, the instantaneous equivalent degradation rate, the equivalent series resistance failure threshold determined according to the AGC frequency modulation power response requirements, and the average pulse frequency of AGC frequency modulation.