A high-reliability high-ripple-current cowhorn electrolytic capacitor manufacturing method

Through the collaborative design of processes such as gradient etching, guide pin riveting, mixed tension winding, and double-stage impregnation, the problems of uneven current distribution and heat accumulation in horn electrolytic capacitors under high ripple current were solved, thus achieving the manufacturing of capacitors with high reliability and high ripple current.

CN123162045APending Publication Date: 2026-11-24CHANGXING SANCHUANG ELECTRIC APPLIANCE CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611497984.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-24
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

In the existing technology, the problem of early failure of horn electrolytic capacitors under high ripple current conditions due to uneven current distribution, insufficient electrolyte penetration and heat accumulation has not been effectively solved.

Method used

Through the coordinated efforts of processes such as gradient corrosion pretreatment of anodic foil, optimization of guide pin riveting structure, mixed tension winding, two-stage impregnation and gradient curing, a porous structure, heat conduction path and viscosity gradient are constructed to optimize electrolyte distribution and thermal management.

Benefits of technology

This significantly improves the ripple current withstand capability and reliability of the horn-shaped electrolytic capacitor, reduces the risk of localized overheating, and enhances the long-term stability and heat dissipation efficiency of the capacitor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123162045A_ABST
    Figure CN123162045A_ABST
Patent Text Reader

Abstract

The application discloses a kind of high reliability high ripple current horn electrolytic capacitor manufacturing methods, including anode foil gradient etching pretreatment, guide needle riveting and multilayer heat-conducting lead structure preparation, mixed tension winding, double-stage impregnation, gradient curing and heat management assembly and packaging etc.Step.The present application constructs the porous structure of aperture gradient distribution by anode foil gradient etching, makes ripple current distribution homogenization, constructs full-path heat export channel by multilayer heat-conducting aluminum foil and aluminum shell stiffener, considers core package structure stability and impregnation channel reservation by mixed tension winding, makes electrolyte form from deep to shallow continuous viscosity gradient by double-stage impregnation, avoids bubble defect by gradient curing, and the ripple current resistance and long-term reliability of horn electrolytic capacitor are improved from manufacturing source system by the cooperation of each procedure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of automated manufacturing technology for electronic components, specifically to a method for manufacturing a high-reliability, high-ripple-current horn-shaped electrolytic capacitor. Background Technology

[0002] Horn-shaped aluminum electrolytic capacitors are widely used in industrial power supplies, frequency converters, and on-board chargers for new energy vehicles due to their large capacitance and high voltage resistance. In these applications, the capacitors need to withstand large ripple current surges. The Joule heating generated inside the capacitor by the ripple current causes the core temperature to rise continuously, which in turn accelerates the drying of the electrolyte and deteriorates the oxide film, ultimately leading to premature capacitor failure.

[0003] In the prior art, Chinese Patent Publication No. CN110828179B discloses an aluminum electrolytic capacitor with ripple current resistance and its preparation method. The preparation steps include core winding, pin riveting, electrolyte impregnation, and encapsulation. The ripple current resistance is mainly improved by optimizing the electrolyte formulation and riveting structure. However, the steps in this method are independent of each other. Core winding uses constant tension control, and impregnation uses a single electrolyte system. None of the steps are specifically designed to address the heat generation and accumulation issues inside the core under high ripple current conditions. Under continuous high ripple current conditions, localized Joule heating caused by uneven current distribution and insufficient electrolyte penetration inside the core leads to accelerated local degradation of the electrolyte and irreversible damage to the oxide film before reaching the external heat dissipation path. Optimizing the electrolyte formulation and structural improvements alone cannot fundamentally solve this problem.

[0004] Therefore, there is an urgent need for a manufacturing method that systematically improves the ripple current tolerance and reliability of horn-shaped electrolytic capacitors by starting from the entire manufacturing process and through multi-stage collaborative design. Summary of the Invention

[0005] (a) Technical problems to be solved The purpose of this invention is to provide a high-reliability, high-ripple-current horn-shaped electrolytic capacitor manufacturing method. Through the coordinated operation of processes such as gradient corrosion pretreatment of anode foil, optimization of guide pin riveting structure, mixed tension winding, two-stage impregnation, and gradient curing, the ripple current resistance and long-term reliability of the capacitor are improved from the manufacturing source.

[0006] (II) Technical Solution To achieve the above objectives, the present invention provides the following technical solution.

[0007] A method for manufacturing a high-reliability, high-ripple-current horn-shaped electrolytic capacitor includes the following steps: S1. Perform gradient corrosion pretreatment on the anode foil to form a porous structure on the surface of the anode foil with a gradient distribution of pore size along the thickness direction; S2. The positive electrode guide pin and the negative electrode guide pin are riveted to the anode foil and the cathode foil respectively. A thermally conductive aluminum foil is provided at the riveting part of the negative electrode guide pin. The thermally conductive aluminum foil extends to the bottom of the core package. A conductive silver paste layer is provided at the riveting part of the positive electrode guide pin. S3. The anode foil, cathode foil and electrolytic paper are wound into a core package. The winding tension decreases from the beginning stage to the end stage. Narrow strip diversion foils are intermittently inserted during the winding process. S4. The core package is impregnated in two stages: first, it is immersed in a low-viscosity electrolyte, and then it is immersed in a high-viscosity electrolyte. S5. The impregnated core package is subjected to gradient curing, which includes low-temperature vacuum curing, medium-temperature ambient pressure curing, and low-temperature vacuum cooling curing in sequence. S6. Pack the cured core package into the aluminum shell, fill the space between the core package and the inner wall of the aluminum shell with thermally conductive insulating material, so that the thermally conductive aluminum foil and the inner bottom surface of the aluminum shell form a thermally conductive contact, and then seal it.

[0008] Preferably, in step S1, the gradient corrosion pretreatment includes a first-stage DC corrosion and a second-stage AC corrosion; the current density of the first-stage DC corrosion is 150–250 mA / cm². 2 The corrosion time is 3–8 minutes; the current density for the secondary AC corrosion is 80–150 mA / cm². 2 The corrosion time is 2 to 5 minutes; the surface pore size of the porous structure is 0.5 to 2 μm, the intermediate pore size is 0.1 to 0.5 μm, and the deep pore size is 0.02 to 0.1 μm.

[0009] Preferably, in step S1, after gradient corrosion, the anode foil undergoes a four-stage formation process. The voltages for the four stages of formation are 0.6 times, 0.85 times, 1.1 times, and 1.3 times the working voltage, respectively. After each stage of formation, the foil is rinsed in deionized water for 3 to 5 minutes.

[0010] Preferably, in step S2, the riveting bend is 125-135mm; the thermally conductive aluminum foil is 2-3 layers of thermally conductive aluminum foil cold-welded to the riveting part of the negative electrode guide pin, each layer of thermally conductive aluminum foil is 20-50μm thick, the width covers the riveting area and extends 0.5-1.5mm beyond the riveting edge on each side; the conductive silver paste layer is an electrolyte-resistant epoxy conductive silver paste layer with a thickness of 5-15μm.

[0011] Preferably, in step S3, the winding tension is divided into three stages: the initial stage tension is 1.2 to 1.8 N, the middle stage tension is 0.8 to 1.2 N, and the final stage tension is 0.5 to 0.8 N, and the tension decreases linearly between the three stages; the width of the narrow strip diverter foil is 3 to 8 mm, and the insertion interval is one strip for every 5 to 10 layers wound; the cutting edge of the narrow strip diverter foil is deburred by laser cutting or chemical polishing.

[0012] Preferably, in step S4, the vacuum degree of the first-stage impregnation is -0.08 to -0.095 MPa, the temperature is 40 to 55°C, and the impregnation time is 15 to 30 minutes; the vacuum degree of the second-stage impregnation is -0.06 to -0.085 MPa, the temperature is 60 to 75°C, and the impregnation time is 30 to 60 minutes.

[0013] Preferably, in step S4, the low-viscosity electrolyte has a viscosity of 5–15 mPa·s at 25°C and contains 5–10 wt% deionized water and 0.5–2 wt% polyethylene glycol; the high-viscosity electrolyte has a viscosity of 30–60 mPa·s at 25°C, with branched ammonium carboxylate as the main solute, and the main solute content is 12–20 wt%; after two-stage impregnation, the electrolyte forms a continuous viscosity gradient from deep to shallow layers within the core package.

[0014] Preferably, in step S5, the gradient curing includes: a first stage of curing at 85-95°C and a vacuum of -0.04 to -0.06 MPa for 2-4 hours; a second stage of curing at 105-115°C and normal pressure for 1-2 hours; and a third stage of curing at 75-85°C and a vacuum of -0.02 to -0.04 MPa for 1-2 hours.

[0015] Preferably, in step S6, the thermal conductivity of the thermally conductive insulating material is 1.0 to 3.0 W / (m·K), and the filling amount is 60 to 80% of the gap volume; the thermally conductive insulating material is a composite material of alumina particles and silica gel, the mass fraction of alumina particles is 50 to 70%, and the average particle size is 1 to 5 μm.

[0016] Preferably, the thermally conductive insulating material further contains 2-5 wt% boron nitride nanosheets, the average thickness of which is 30-80 nm and the average diameter of which is 1-3 μm.

[0017] Preferably, in step S6, the bottom surface of the aluminum shell is provided with radially distributed reinforcing ribs, the height of which is 0.5 to 1.5 mm and the number of ribs is 6 to 12; the end of the thermally conductive aluminum foil forms a surface contact thermally conductive path with the reinforcing ribs, and thermally conductive silicone grease is coated on the contact interface.

[0018] The core of this invention lies in the synergistic cooperation between various processes, rather than the independent improvement of a single process or a single material. Specifically: First, gradient etching of the anode foil provides a foundation for two-stage impregnation. The large pore size on the surface facilitates rapid electrolyte wetting, while the small pore size in the middle and deep layers provides a high specific surface area to ensure capacity. If only gradient etching is performed without two-stage impregnation, the deep micropores cannot be fully filled by the high-viscosity electrolyte, resulting in low capacity utilization and high ESR.

[0019] Second, the two-stage impregnation process, matched with the gradient corrosion anode foil, creates a continuous viscosity gradient of electrolyte within the core package, from deep to shallow layers. The first-stage impregnation uses a low-viscosity electrolyte, preferentially penetrating to the deep micropores of the gradient-corroded anode foil; the second-stage impregnation uses a high-viscosity electrolyte, filling the macropores in the middle and surface layers of the core package. The low-viscosity electrolyte ensures the repair capability and low ESR of the deep oxide film, while the high-viscosity electrolyte ensures high flash voltage and high-temperature stability in the shallow region under high ripple heating conditions. This continuous viscosity gradient can be verified by segmented sampling and analysis of the electrolyte composition after high-temperature loading.

[0020] Third, the mixed tension winding creates a porosity gradient for the two-stage impregnation. The higher tension in the initial stage ensures the compactness and structural stability of the inner core pack; the moderate tension in the middle stage avoids excessive compression of the electrolytic paper's porosity; and the lower tension in the final stage keeps the outer core pack moderately loose, reserving channels for electrolyte penetration. The narrow strip of diverting foil, under mixed tension, will not be completely crushed, serving both as a radial impregnation acceleration channel and a thermal diffusion channel within the core pack.

[0021] Fourth, the gradient curing is matched with the electrolyte distribution after the two-stage impregnation. The first stage of low-temperature vacuum curing avoids the rapid evaporation of low-boiling-point solvents, which can cause surface "skin" and internal bubble defects. The second stage of medium-temperature ambient pressure curing promotes full homogenization of the electrolyte and completes oxide film repair. The third stage of low-temperature vacuum cooling curing slowly cools down and removes residual bubbles, avoiding thermal stress concentration caused by rapid cooling.

[0022] Fifth, the thermal management assembly constructs heat conduction channels between the core package interior, core package surface, aluminum shell, and external environment. The multi-layered thermally conductive aluminum foil at the negative electrode pin riveting location extends to the bottom of the core package, forming a surface contact heat conduction path with the reinforcing ribs on the inner bottom surface of the aluminum shell. Alumina particles and boron nitride nanosheets in the thermally conductive insulating material are combined to form a three-dimensional thermally conductive network within the silicone matrix. These heat paths, in conjunction with the narrow strip shunt foil inside the core package, significantly reduce the hot spot temperature inside the core package.

[0023] (III) Beneficial Effects Compared with the prior art, the present invention has the following beneficial effects: By pre-treating the anode foil with gradient corrosion, a porous structure with a gradient distribution of pore size is constructed on the surface of the anode foil, making the distribution of ripple current on the surface of the anode foil more uniform, avoiding the problem of local current density concentration caused by a single pore size distribution, and effectively reducing the risk of local hot spots.

[0024] By simultaneously cold-welding multiple layers of thermally conductive aluminum foil at the negative electrode guide pin riveting location and extending it to the bottom of the aluminum shell, setting radial reinforcing ribs on the inner bottom surface of the aluminum shell, and filling with thermally conductive insulating material containing boron nitride nanosheets, a full-path heat conduction channel is constructed for the core package interior, core package surface, and aluminum shell, significantly reducing the equivalent thermal resistance of the core package.

[0025] By using a hybrid tension winding process, the stability of the core package structure and the reservation of electrolyte penetration channels are taken into account, thus resolving the contradiction between "insufficient impregnation due to excessive tension" and "loose structure due to excessive tension" in traditional constant tension winding.

[0026] Through a two-stage impregnation process, a continuous viscosity gradient of electrolyte is formed from deep to shallow within the core package. This ensures that the electrolyte fully penetrates the deep micropores of the gradient-corroded anode foil, while also ensuring that the shallow region has sufficient flashover voltage and oxide film repair capability under ripple current heating conditions.

[0027] The gradient curing process effectively avoids the bubble defects and uneven electrolyte distribution problems that are prone to occur in traditional constant temperature curing, thereby improving the long-term stability and reliability of the product.

[0028] The various processes in this invention form a systematic synergy: gradient etching of the anode foil provides the penetration basis for two-stage impregnation; mixed tension winding creates the channel conditions for two-stage impregnation; gradient curing ensures the effective curing of the two-stage impregnation effect; and thermal management assembly provides a complete heat dissipation path to meet the thermal management needs under high ripple conditions. The organic cooperation of these processes together achieves the manufacturing of a high-reliability, high-ripple-current horn-shaped electrolytic capacitor. Attached Figure Description

[0029] Various other advantages and benefits will become apparent to those skilled in the art upon reading the following detailed description of preferred embodiments. The accompanying drawings are for illustrative purposes only and are not intended to limit the invention. Furthermore, the same reference numerals denote the same parts throughout the drawings. In the drawings: Figure 1 This is an overall process flow diagram of the manufacturing method of a high-reliability, high-ripple-current horn-shaped electrolytic capacitor according to this application. Detailed Implementation

[0030] The following will refer to the appendix in the examples of this invention. Figure 1 The technical solutions in the embodiments of the present invention are clearly and completely described. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0031] Example 1 This embodiment provides a method for manufacturing a high-reliability, high-ripple-current horn-shaped electrolytic capacitor, including the following steps: S1, Gradient corrosion pretreatment of anodic foil High-purity aluminum foil with a purity of 99.99% and a thickness of 100 μm was selected as the anode foil substrate. The aluminum foil was placed in a mixed etching solution with a hydrochloric acid concentration of 1.5 mol / L and a sulfuric acid concentration of 0.8 mol / L, and subjected to first-stage DC etching at 40℃ and a current density of 200 mA / cm². 2 The etching process lasted 5 minutes; followed by secondary AC etching at a current density of 120 mA / cm². 2 The etching process lasted 3 minutes at a frequency of 50 Hz. After etching, the foil was rinsed with deionized water and dried at 60°C. SEM cross-sectional observation and specific surface area testing revealed that the pore size of the anode foil surface layer was 0.5–2 μm, the pore size of the intermediate layer was 0.1–0.5 μm, and the pore size of the deep layer was 0.02–0.1 μm, resulting in a specific surface area approximately 120 times greater than that of the untreated aluminum foil.

[0032] Then, four-stage formation is performed, with formation voltages of 0.6, 0.85, 1.1, and 1.3 times the operating voltage, respectively. When the operating voltage is 450V, the corresponding voltages are 270V, 383V, 495V, and 585V. After each stage of formation, the device is rinsed with deionized water for 4 minutes.

[0033] S2, Preparation of guide pin riveting and multilayer thermal conductive lead-out structure The positive electrode guide pin is riveted to the anode foil with a riveting bend of 130mm. Before riveting, a 10μm thick layer of electrolyte-resistant epoxy conductive silver paste is applied to the contact surface between the positive electrode guide pin and the anode foil. After immersion in electrolyte at 85℃ for 1000 hours, the contact resistance change rate of this silver paste layer is no greater than 10%. The negative electrode guide pin is riveted to the cathode foil with a riveting bend of 130mm. Simultaneously, three layers of 30μm thick thermally conductive aluminum foil are cold-welded at the riveting location of the negative electrode guide pin. The thermally conductive aluminum foil is 8mm wide and extends 1.0mm beyond the riveting edge on each side. The thermally conductive aluminum foil extends axially from the riveting location to the bottom of the core package, and the end is bent and attached to the reinforcing rib on the inner bottom surface of the aluminum shell.

[0034] S3, Mixed Tension Winding The anode foil, cathode foil, and electrolytic paper are wound into a core package. The tension is 1.5N at the beginning of the winding, 1.0N in the middle, and 0.6N at the end, with the tension decreasing linearly. During the winding process, a narrow strip of aluminum shunt foil with a width of 5mm and a thickness of 15μm is inserted every 8 layers. The edges of the shunt foil are deburred by laser cutting.

[0035] S4, dual-stage impregnation First-stage impregnation: Vacuum degree -0.090MPa, temperature 50℃, immersion in low-viscosity electrolyte for 25 minutes. The low-viscosity electrolyte has a viscosity of approximately 10 mPa·s at 25℃ and is formulated with 85wt% ethylene glycol, 8wt% deionized water, 1.5wt% polyethylene glycol 400, 5wt% ammonium sebate, and conventional additives.

[0036] Secondary impregnation: Vacuum degree -0.070MPa, temperature 68℃, immersion in high-viscosity electrolyte for 45 minutes. The high-viscosity electrolyte has a viscosity of approximately 45 mPa·s at 25℃, and its formulation consists of 65wt% ethylene glycol, 15wt% ammonium 1,6-dodecanoate, 5wt% ammonium sebacate, 8wt% polyethylene glycol 1000, 5wt% flash voltage enhancer, and conventional additives.

[0037] S5, Gradient Curing First stage: 90℃, vacuum degree -0.05MPa, curing for 3 hours; Second stage: 110℃, normal pressure, cure for 1.5 hours; Third stage: 80℃, vacuum degree -0.03MPa, curing for 1.5 hours.

[0038] S6, Thermal Management Assembly and Packaging Eight radial reinforcing ribs, 1.0 mm high, are arranged on the inner bottom surface of the aluminum shell. After the core package is inserted, the gap between the core package and the inner wall of the aluminum shell is filled with a thermally conductive insulating material, consisting of 60% alumina and 40% silicone, with an additional 3 wt% boron nitride nanosheets. The nanosheets have an average thickness of 50 nm and an average diameter of 2 μm, and the filling amount is 70% of the gap volume, with a thermal conductivity of approximately 2.0 W / (m·K). Thermally conductive silicone grease is applied to the interface between the thermally conductive aluminum foil and the reinforcing ribs. Subsequently, the shell is sealed, cleaned, sleeved, and charged for aging to obtain the finished product.

[0039] Performance testing: A 450V / 470μF, φ35×50mm horn-shaped electrolytic capacitor was manufactured. The rated ripple current (105℃, 120Hz) is 3.2A; the ESR (100kHz, 20℃) is 28mΩ; after 5000 hours of load at 105℃, rated voltage + rated ripple current, the capacitance change rate is ≤8%, the loss tangent is ≤1.3 times the initial value, and the leakage current is qualified; the internal hot spot temperature of the core is 12-15℃ lower than that of conventional products of the same specification.

[0040] Example 2 The difference from Example 1 is that the first-stage DC corrosion current density in S1 is 180 mA / cm². 2 Time: 6 minutes; Secondary AC corrosion current density: 100 mA / cm² 2S3: 4 minutes; S4: 6mm wide shunt foil inserted every 6 layers; S5: -0.085MPa vacuum for 30 minutes, and -0.065MPa vacuum for 50 minutes; S6: 55% alumina and 4wt% boron nitride nanosheets.

[0041] Test results: Rated ripple current 3.0A, ESR 31mΩ, hot spot temperature is about 10℃ lower than conventional products, and capacitance change rate is about 7.5% after 5000 hours of high temperature load.

[0042] Example 3 The difference from Example 1 is that the first-stage DC corrosion current density in S1 is 220 mA / cm². 2 Time: 4 minutes; Secondary AC corrosion current density: 130 mA / cm² 2 The time is 2.5 minutes; the initial tension in S3 is 1.6N, the middle tension is 1.1N, and the end tension is 0.7N. One shunt foil is inserted every 7 layers with a width of 7mm; the boron nitride nanosheets added in S6 are 5wt%, and there are 10 reinforcing ribs.

[0043] Test results: Rated ripple current 3.1A, ESR 29mΩ, hot spot temperature reduced by about 11℃ compared to conventional products, and capacitance change rate of about 7% after 5000 hours of high-temperature load.

[0044] Comparative Example 1 Difference from Example 1: In S1, the anode foil is subjected to conventional uniform corrosion instead of gradient corrosion; the remaining steps are the same as in Example 1. Test results: Rated ripple current 2.4A, ESR 42mΩ, hot spot temperature approximately 3°C lower than conventional products, and capacitance change rate approximately 9.5% after 5000 hours of high-temperature load.

[0045] Comparative Example 2 Difference from Example 1: In S4, only a single-stage high-viscosity electrolyte impregnation is performed, without a single-stage low-viscosity electrolyte impregnation; the remaining steps are the same as in Example 1. Test results: Rated ripple current 2.5A, ESR 45mΩ, hot spot temperature is about 3°C ​​lower than conventional products, capacitance change rate exceeds 10% after 3000 hours of high-temperature load, and fails the 5000-hour test.

[0046] Comparative Example 3 Difference from Example 1: Constant tension winding is used in S3, and narrow strip shunt foil is not inserted; the remaining steps are the same as in Example 1. Test results: Rated ripple current 2.3A, ESR 48mΩ, hot spot temperature is about 2℃ lower than conventional products, radial temperature gradient of the core package is significantly increased, and capacitance change rate is about 10.5% after 5000 hours of high-temperature load.

[0047] Comparative Example 4 Difference from Example 1: In S6, the thermally conductive insulating material does not contain boron nitride nanosheets; the remaining steps are the same as in Example 1. Test results: The thermal conductivity of the thermally conductive insulating material is approximately 1.2 W / (m·K), the rated ripple current is 2.9 A, the ESR is 32 mΩ, the hot spot temperature is approximately 6 °C lower than that of conventional products, and the capacitance change rate after 5000 hours of high-temperature load is approximately 8.5%.

[0048] Comparative Example 5 Difference from Example 1: In S5, constant temperature of 110℃ and normal pressure curing for 5 hours is used instead of gradient curing, while the remaining steps are the same as in Example 1. Test results: Rated ripple current 2.7A, ESR 36mΩ, hot spot temperature is about 4℃ lower than conventional products, dissection revealed a small number of bubble defects inside the core package, and the capacitance change rate after 5000 hours of high temperature load is about 11%.

[0049] Comparative Example 6 Difference from Example 1: In S2, the positive electrode pin riveting area is not coated with a conductive silver paste layer; the remaining steps are the same as in Example 1. Test results: Rated ripple current 2.8A, ESR 38mΩ, hot spot temperature is about 5°C lower than conventional products, and the contact resistance of the riveting area increases after high-temperature load.

[0050] Performance testing methods Rated ripple current: Measured under conditions of 105℃ environment, with a 120Hz ripple current applied, and the temperature rise at the core of the package not exceeding 5℃.

[0051] ESR: Tested at 100kHz and 20℃.

[0052] High-temperature load life: Under 105℃ environment, the rated voltage and rated ripple current are applied for 5000 hours to test the capacitance change rate, loss tangent and leakage current.

[0053] Hot spot temperature: The hot spot temperature inside the core package was tested using the embedded thermocouple method under the conditions of 105℃ environment and rated ripple current loading.

[0054] Electrolyte gradient distribution: After high-temperature loading, the core package was sampled in segments to analyze changes in electrolyte composition and viscosity. See Table 1 below for details. Table 1: Performance Comparison of Each Example and Comparative Example in conclusion As can be seen from Table 1, Examples 1 to 3, through the synergistic cooperation of processes such as gradient etching of anodic foil, two-stage impregnation, mixed tension winding, gradient curing, thermal network assembly, and positive electrode conductive silver paste riveting, are significantly superior to the comparative examples in terms of rated ripple current, ESR, hot spot temperature, and high-temperature load life.

[0055] Comparative Example 1, which simply changed gradient corrosion to uniform corrosion, showed a significant deterioration in ripple current and ESR; Comparative Example 2, which only used single-stage high-viscosity impregnation, had insufficient filling of deep micropores and failed to pass the lifetime test; Comparative Example 3, which used constant tension winding without shunt foil, increased the radial temperature gradient of the core package and decreased ripple capability; Comparative Example 4, which lacked boron nitride nanosheets, had an incomplete thermal conductivity network and increased hot spot temperature; Comparative Example 5, which used isothermal curing, resulted in bubble defects inside the core package and decreased lifetime; Comparative Example 6, which lacked positive conductive silver paste, increased riveting contact resistance and worsened both ESR and hot spot temperature.

[0056] The above results show that the present invention is not a simple superposition of various processes, but rather a holistic synergy of gradient corrosion, two-stage impregnation, mixed tension winding, gradient curing, and thermal management assembly, which enables the electrolyte to form a continuous viscosity gradient from deep to shallow layers within the core package, while simultaneously constructing a low thermal resistance thermal conduction path from the core package interior to the aluminum shell, thereby jointly achieving high ripple current tolerance, low ESR, and high reliability.

[0057] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A method for manufacturing a high-reliability, high-ripple-current horn-shaped electrolytic capacitor, characterized in that, Includes the following steps: S1. Perform gradient corrosion pretreatment on the anode foil to form a porous structure on the surface of the anode foil with a gradient distribution of pore size along the thickness direction; S2. The positive electrode guide pin and the negative electrode guide pin are riveted to the anode foil and the cathode foil respectively. A thermally conductive aluminum foil is provided at the riveting part of the negative electrode guide pin. The thermally conductive aluminum foil extends to the bottom of the core package. A conductive silver paste layer is provided at the riveting part of the positive electrode guide pin. S3. The anode foil, cathode foil and electrolytic paper are wound into a core package. The winding tension decreases from the beginning stage to the end stage. Narrow strip diversion foils are intermittently inserted during the winding process. S4. The core package is impregnated in two stages: first, it is immersed in a low-viscosity electrolyte, and then it is immersed in a high-viscosity electrolyte. S5. The impregnated core package is subjected to gradient curing, which includes low-temperature vacuum curing, medium-temperature ambient pressure curing, and low-temperature vacuum cooling curing in sequence. S6. Pack the cured core package into the aluminum shell, fill the space between the core package and the inner wall of the aluminum shell with thermally conductive insulating material, so that the thermally conductive aluminum foil and the inner bottom surface of the aluminum shell form a thermally conductive contact, and then seal it.

2. The method according to claim 1, characterized in that, In step S1, the gradient etching pretreatment comprises a first direct current etching and a second alternating current etching; the current density of the first direct current etching is 150-250 mA / cm 2 , and the etching time is 3-8 minutes; the current density of the second alternating current etching is 80-150 mA / cm 2 , and the etching time is 2-5 minutes; the surface layer pore size of the porous structure is 0.5-2 μm, the intermediate layer pore size is 0.1-0.5 μm, and the deep layer pore size is 0.02-0.1 μm.

3. The method according to claim 1, characterized in that, In step S1, after gradient corrosion, the anode foil undergoes a four-stage formation process. The voltages for the four stages of formation are 0.6 times, 0.85 times, 1.1 times, and 1.3 times the working voltage, respectively. After each stage of formation, the foil is rinsed in deionized water for 3 to 5 minutes.

4. The method according to claim 1, characterized in that, In step S2, the riveting bend is 125-135mm; the thermally conductive aluminum foil consists of 2-3 layers of thermally conductive aluminum foil cold-welded to the riveting part of the negative electrode guide pin, each layer of thermally conductive aluminum foil being 20-50μm thick, covering the riveting area and extending 0.5-1.5mm beyond the riveting edge on each side; the conductive silver paste layer is an electrolyte-resistant epoxy conductive silver paste layer with a thickness of 5-15μm.

5. The method according to claim 1, characterized in that, In step S3, the winding tension is divided into three stages: the initial stage tension is 1.2 to 1.8 N, the middle stage tension is 0.8 to 1.2 N, and the end stage tension is 0.5 to 0.8 N, and the tension decreases linearly between the three stages; the width of the narrow strip diverter foil is 3 to 8 mm, and the insertion interval is one strip every 5 to 10 layers of winding; the cutting edge of the narrow strip diverter foil is deburred by laser cutting or chemical polishing.

6. The method according to claim 1, characterized in that, In step S4, the vacuum degree of the first-stage impregnation is -0.08 to -0.095 MPa, the temperature is 40 to 55°C, and the impregnation time is 15 to 30 minutes; the vacuum degree of the second-stage impregnation is -0.06 to -0.085 MPa, the temperature is 60 to 75°C, and the impregnation time is 30 to 60 minutes.

7. The method according to claim 1, characterized in that, In step S4, the low-viscosity electrolyte has a viscosity of 5–15 mPa·s at 25°C and contains 5–10 wt% deionized water and 0.5–2 wt% polyethylene glycol; the high-viscosity electrolyte has a viscosity of 30–60 mPa·s at 25°C, with branched ammonium carboxylate as the main solute, and the main solute content is 12–20 wt%; after two-stage impregnation, the electrolyte forms a continuous viscosity gradient from deep to shallow layers within the core package.

8. The method according to claim 1, characterized in that, In step S5, the gradient curing includes: a first stage of curing at 85-95°C and a vacuum of -0.04 to -0.06 MPa for 2-4 hours; a second stage of curing at 105-115°C and normal pressure for 1-2 hours; and a third stage of curing at 75-85°C and a vacuum of -0.02 to -0.04 MPa for 1-2 hours.

9. The method according to claim 1, characterized in that, In step S6, the thermal conductivity of the thermally conductive insulating material is 1.0 to 3.0 W / (m·K), and the filling amount is 60 to 80% of the gap volume; the thermally conductive insulating material is a composite material of alumina particles and silica gel, the mass fraction of alumina particles is 50 to 70%, and the average particle size is 1 to 5 μm.

10. The method according to claim 9, characterized in that, The thermally conductive insulating material also contains 2-5 wt% boron nitride nanosheets, with an average thickness of 30-80 nm and an average sheet diameter of 1-3 μm.

Citation Information

Patent Citations

  • An aluminum electrolytic capacitor with high ripple current resistance and its preparation method

    CN110828179B