Secondary alkaline-manganese battery positive electrode containing a porous solidifying agent

By adding porous silicate cement as a curing agent to the positive electrode of a secondary alkaline manganese battery, the problem of manganese dioxide crystal cracking during long-term charge and discharge was solved, thereby achieving the stability of the battery lattice and the enhancement of ion channels, extending battery life and improving battery performance.

CN123162133APending Publication Date: 2026-11-24SUZHOU JINSER BATTERY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510665256.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-05-22
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

The manganese dioxide crystals, the positive electrode material in secondary alkaline manganese batteries, are prone to cracking during long-term charge and discharge processes, which leads to a shortened battery cycle life.

Method used

Porous curing agent silicate cement is used as an additive for the positive electrode material. The composition includes 83% powdered MnO2, 9% graphite, 3% silicate cement and 5% 9N KOH solution. The positive electrode material is formed by stirring and then made into a positive electrode ring, which is finally assembled into a battery.

Benefits of technology

It improves the lattice stability of manganese dioxide cathode, enhances ion channels, extends battery cycle life, and improves battery power performance.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This invention discloses a secondary alkaline manganese battery cathode containing a porous curing agent, comprising 83% powdered MnO2, 9% graphite, 3% silicate cement, and 5% 9N KOH solution. A method for preparing the secondary alkaline manganese battery cathode is as follows: 83% powdered MnO2, 9% graphite, and 3% silicate cement are mixed and stirred thoroughly for half an hour. Then, 5% 9N KOH solution is added, and the mixture is stirred for 1.5 hours to obtain the cathode material. This invention, by adding 3% silicate cement as a curing agent, effectively increases the stability of the γ-MnO2 lattice and also increases the ion channels of the manganese dioxide cathode, thereby improving the battery's power.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of battery technology, and specifically to an alkaline manganese battery cathode. Background Technology

[0002] The discharge time of a secondary alkaline manganese battery is equivalent to that of dozens to hundreds of primary batteries. Using secondary alkaline manganese batteries can save a lot of manganese ore and other resources and energy consumption, and will significantly alleviate the pressure of battery pollution on the environment.

[0003] MnO2 exhibits a rich variety of structural types, including tunnel structures (α, β, γ) and orthorhombic manganese oxide-type structures (R-type), layered structures (δ-type), and spinel structures (λ-type). These structures are composed of regular octahedrons [MnO6] connected by long-range ordered links through shared edges or vertices. + Protons move easily in structures with wide channels and can move in a jumping manner due to the attraction of the polarity of water molecules, resulting in fast diffusion and small reaction polarization.

[0004] The positive electrode discharge reaction is as follows: MnO₂ + xH₂O + xe⁻ → MnO 2-x (OH)x + xOH - Mn 3+ The position of Mn in the crystal lattice remains the same. 4+ The position can be used to place Mn 4+ Considered as being composed of Mn 3+ With an electron-deficient hole, Mn at the Mn site in the crystal lattice 4+ Mn continuously decreases 3+ The amount of manganese dioxide continuously increases, but the basic structure of the entire crystal lattice remains unchanged. Meanwhile, water is decomposed into H₂ at the manganese dioxide and solution interface. + Proton, i.e., o< H H —— H + + OH - H + Protons diffuse into the manganese dioxide lattice along the interlayer space, causing O² on the lattice to form OH⁻. - H + proton The electrons continuously diffuse into the crystal lattice, causing a continuous decrease in the number of O²⁻ atoms and a continuous increase in the number of OH⁻ atoms. When electrons diffuse into the holes (Mn) in the steel cylinder... 4+ The protons move in the opposite direction, causing MnO2 to continuously react and form MnOOH, as shown in the reaction equation: MnO2+HO + + e - —— MnOOH+OH During electrochemical charging and discharging, MnO2 structures with different crystal configurations can easily transform into each other. The transformation of crystal structure and the increase of stress can lead to the destruction of crystal structure, which in turn causes the battery capacity to decay during long cycles. This is one of the key issues affecting the performance of such materials.

[0005] Therefore, enhancing the stability of the γ-MnQ2 lattice and preventing it from transforming into other types is one of the important ways to improve the cycle life of secondary alkaline manganese batteries. Summary of the Invention

[0006] The technical problem to be solved by this invention is the cracking of manganese dioxide crystals, the positive electrode material in secondary alkaline manganese batteries, during long-term charge and discharge processes.

[0007] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is as follows.

[0008] A secondary alkaline manganese battery cathode containing a porous curing agent comprises 83% powdered MnO2, 9% graphite, 3% silicate cement, and 5% 9N KOH solution.

[0009] A method for preparing a secondary alkaline manganese battery cathode containing a porous curing agent: 83% powdered MnO2, 9% graphite, and 3% silicate cement are mixed and stirred thoroughly for half an hour. Then, 5% 9N KOH solution is injected and stirred for 1.5 hours to obtain the cathode material.

[0010] The positive electrode material is fed into the ring-making machine to obtain the positive electrode ring.

[0011] The positive electrode ring is pressed into the steel shell, the separator sleeve is inserted, the negative electrode adhesive is injected into the separator sleeve, and after the sealing process, the desired battery is obtained.

[0012] Due to the adoption of the above technical solutions, the technical progress achieved by this invention is as follows.

[0013] The silicate cement used in this invention is a porous curing agent. 3% silicate cement is added to the positive electrode of the battery as a curing agent, which restricts the expansion and contraction of the crystal lattice. At the same time, the silicate cement is full of micropores, which are ideal ion channels, effectively increasing the stability of the γ-MnQ2 crystal lattice. It also increases the ion channels of the manganese dioxide positive electrode, which can improve the power of the battery. Detailed Implementation

[0014] The present invention will now be described in further detail.

[0015] A secondary alkaline manganese battery cathode containing a porous curing agent comprises 83% powdered MnO2, 9% graphite, 3% silicate cement, and 5% 9N KOH solution.

[0016] A method for preparing a secondary alkaline manganese battery cathode containing a porous curing agent: 83% powdered MnO2, 9% graphite, and 3% silicate cement are mixed and stirred thoroughly for half an hour. Then, 5% 9N KOH solution is injected and stirred for 1.5 hours to obtain the cathode material.

[0017] The proportion of silicate cement can be adjusted appropriately between 1% and 5%.

[0018] The positive electrode material is fed into the ring-making machine to obtain the positive electrode ring.

[0019] The positive electrode ring is pressed into the steel shell, the separator sleeve is inserted, the negative electrode adhesive is injected into the separator sleeve, and after the sealing process, the desired battery is obtained.

[0020] Silicate cement is a porous curing agent. Adding 3% silicate cement to the positive electrode of the battery as a curing agent restricts the expansion and contraction of the crystal lattice. At the same time, silicate cement is full of micropores, which are ideal ion channels, effectively increasing the stability of the γ-MnQ2 crystal lattice. It also increases the ion channels of the manganese dioxide positive electrode, which can improve the power of the battery.

Claims

1. A secondary alkaline manganese battery cathode containing a porous curing agent, comprising 83% powdered MnO2, 9% graphite, 3% silicate cement, and 5% 9N KOH solution.

2. A method for preparing a secondary alkaline manganese battery cathode containing a porous curing agent according to claim 1: 83% powdered MnO2, 9% graphite, and 3% silicate cement are mixed and stirred thoroughly for half an hour, followed by the injection of 5% 9NKOH solution and stirring for 1.5 hours to obtain the cathode material.