An additive to prevent anode delamination in alkaline manganese batteries
By using an additive that forms a soluble complex with Zn²⁺ using triethanolamine (TEA) in alkaline manganese batteries, the problem of anode delamination in alkaline manganese batteries was solved, extending battery life and improving capacity retention.
Patent Information
- Application Number
- CN202510675230.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-23
- Publication Date
- 2026-11-24
AI Technical Summary
During long-term storage and use, alkaline manganese batteries exhibit anode delamination, leading to reduced capacity. In particular, the delamination problem caused by zinc oxidation and migration has not been effectively resolved.
Triethanolamine (TEA) was used as an additive to form a soluble complex [Zn(TEA)₂]²⁺ with Zn²⁺, which reduced the specific gravity, stabilized the zincate solution, and prevented ZnO deposition. The additive consisted of 65.0 wt% Zn powder, 1.0 wt% sodium carboxymethyl cellulose, 33.0 wt% 9N KOH solution, and 1.0 wt% triethanolamine.
It significantly extends the storage life and cycle life of alkaline manganese batteries, mitigates anode delamination, and improves battery capacity retention.
Abstract
Description
Technical Field
[0001] This invention relates to the field of battery technology, and more specifically to an additive that prevents delamination of the anode in alkaline manganese batteries. Background Technology
[0002] Alkali manganese batteries are highly sought after for their safety, environmental friendliness, and affordability. Significant efforts have been made to further improve the lifespan of alkaline manganese batteries.
[0003] It was discovered that after long-term storage, the anode of a primary alkaline manganese battery exhibited stratification. Analysis revealed that zinc oxide was deposited in large quantities at the bottom, while metallic zinc was concentrated at the top. Over time, more zinc left the reaction system as zinc oxide, leading to a decrease in the capacity of the primary alkaline manganese battery.
[0004] After prolonged operation, the anode of the secondary alkaline manganese battery also exhibits stratification, sometimes even more severely. This means that charging cannot reduce zinc oxide back to zinc.
[0005] The anode stratification phenomenon in alkaline manganese batteries is one of the reasons for the capacity reduction of primary alkaline manganese batteries after long-term storage, and also one of the reasons for the decrease in discharge capacity of secondary alkaline manganese batteries.
[0006] The mechanism is complex. For example, the specific gravity of the product, zinc corrosion, and their different properties in magnetic and electric fields result in migration in different directions and at different speeds. This is one of the reasons why stratification occurs at the anode of primary alkali manganese after long-term storage.
[0007] In addition to the above-mentioned causes of anode stratification in primary alkaline manganese batteries after long-term storage, the gas generated during the long-term charging and discharging of secondary alkaline manganese batteries, especially oxygen, chemically oxidizes metallic zinc into zinc oxide. Even when charged, the chemically oxidized zinc oxide cannot be reduced back to zinc. This is the reason why the anode stratification of secondary alkaline manganese batteries gradually intensifies with the increase of charge and discharge cycles. Summary of the Invention
[0008] The technical problem to be solved by the present invention is to provide an additive that prevents the delamination of the anode in alkaline manganese batteries, so as to prevent the delamination phenomenon of the anode in alkaline manganese batteries.
[0009] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is as follows.
[0010] An additive to prevent anodic delamination in alkaline manganese batteries, triethanolamine (TEA), has a typical formulation as follows: 65.0 wt% Zn powder, 1.0 wt% sodium carboxymethyl cellulose, 33.0 wt% 9N KOH solution, and 1.0 wt% triethanolamine (TEA).
[0011] Due to the adoption of the above technical solutions, the technical progress achieved by this invention is as follows.
[0012] This invention provides triethanolamine (TEA) as an additive. Triethanolamine forms a soluble complex [Zn(TEA)2]²⁺ with Zn²⁺, which reduces the specific gravity, stabilizes the zincate solution, and prevents capacity decay caused by ZnO deposition. It significantly extends the storage life of primary alkaline manganese batteries and greatly reduces the probability of Zn²⁺ ions being chemically oxidized by oxygen, thereby effectively mitigating anode stratification and significantly extending the cycle life of the anode in secondary alkaline manganese batteries. Detailed Implementation
[0013] The present invention will now be described in further detail.
[0014] An additive to prevent stratification of the anode in alkaline manganese batteries comprises 65.0 wt% Zn powder, 1.0 wt% sodium carboxymethyl cellulose, 33.0 wt% 9N KOH solution, and 1.0 wt% triethanolamine (TEA) prepared by the present patent.
[0015] ① After mixing the dry Zn powder and sodium carboxymethyl cellulose in the above proportions evenly, ② Inject 9N KOH solution of triethanolamine according to the above ratio, stir until uniform under anaerobic conditions, about 1-2 hours, to obtain the anode gel.
[0016] ③Then, following the conventional method, taking a No. 5 battery as an example, inject 4.5 grams of anode adhesive into the negative electrode cavity of the battery, seal it, and store it at room temperature for one week.
[0017] test As a primary alkaline manganese battery, after 2 years of storage, its capacity decay due to storage is reduced by 80% compared to a standard battery without added triethanolamine.
[0018] For secondary alkaline manganese batteries, after discharging to 0.9 volts under a 3.9 ohm resistance and then charging at a constant voltage of 1.65 volts for 8 hours, repeated 100 times, the sample with added triethanolamine showed a cumulative discharge increase of over 70% compared to the standard battery without added triethanolamine.
Claims
1. An additive for preventing stratification of the anode in an alkaline manganese battery, comprising 65.0 wt% Zn powder, 1.0 wt% sodium carboxymethyl cellulose, 33.0 wt% 9N KOH solution, and 1.0 wt% triethanolamine (TEA).
2. The additive for preventing stratification of the anode in alkaline manganese batteries according to claim 1 is prepared by: ① After mixing the dry Zn powder and sodium carboxymethyl cellulose in the above proportions evenly; ② Inject 9N KOH solution of triethanolamine according to the above ratio, stir until uniform under anaerobic conditions for about 1-2 hours to obtain the anode gel; ③Then, following standard procedures, inject 4.5 grams of anode adhesive into the negative electrode cavity of the battery and seal it, storing it at room temperature for one week.