Battery, solid-state battery, and method for manufacturing battery
By setting central and end electrode layers with different filling rates in the battery and controlling the end thickness, the problem of end cracks in the active material layer during battery charging and discharging is solved, thus improving the stability and performance of the battery.
Patent Information
- Application Number
- CN202610688341.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-21
- Filing Date
- 2026-05-19
- Publication Date
- 2026-11-24
AI Technical Summary
In existing technologies, cracks easily appear at the ends of the active material layer during the charging and discharging process of a battery, leading to a decline in battery performance.
By setting a central electrode section and an end electrode section in the battery, with the end electrode section having a lower filling rate than the central electrode section, and controlling the end electrode thickness to be less than the central electrode thickness during manufacturing, the end electrode section absorbs the expansion and contraction of the electrode layer, thus suppressing the occurrence of cracks.
It effectively suppresses end cracks in the electrode layer during battery charging and discharging, improving battery stability and performance.
Smart Images

Figure CN123162331A_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to batteries, solid-state batteries, and methods for manufacturing batteries. Background Technology
[0002] For example, Japanese Patent Application Publication No. 2023-114635 discloses a battery in which a positive current collector, a positive active material layer, a separator layer, a negative active material layer, and a negative current collector are stacked in this order. The negative active material layer has a fill rate of 80%. Summary of the Invention
[0003] In the battery described in Japanese Patent Application Publication No. 2023-114635, the active material layer expands and contracts during charging and discharging, and there is a need to suppress cracks at the ends of the active material layer caused by such expansion and contraction.
[0004] The purpose of this disclosure is to provide a battery capable of suppressing the occurrence of cracks at the ends of the active material layer during charging and discharging, and a method for manufacturing the battery.
[0005] The battery in this disclosure is a battery in which a first electrode layer, a separator layer and a second electrode layer are stacked in this order, the second electrode layer comprising: a central electrode portion containing a central electrode active material; and an end electrode portion containing an end electrode active material and in contact with the end of the central electrode portion in an orthogonal direction orthogonal to the stacking direction, the fill rate of the end electrode portion being smaller than the fill rate of the central electrode portion.
[0006] In the solid-state battery disclosed herein, the separator layer comprises a solid electrolyte.
[0007] The battery manufacturing method disclosed herein is a method for manufacturing a battery in which a first electrode layer, a separator layer, and a second electrode layer are stacked in this order. It includes a second electrode layer forming step, wherein the second electrode layer is formed on the separator layer. The second electrode layer forming step includes: supplying an electrode active material onto the separator layer in such a way that the thickness of the end portion adjacent to the central portion in an orthogonal direction orthogonal to the stacking direction is smaller than the thickness of the central portion in the orthogonal direction orthogonal to the stacking direction; and pressing the electrode active material in such a way that the thickness of the central portion and the thickness of the end portion are equal to each other.
[0008] The above and other objects, features, methods and advantages of the present invention will become clear from the following detailed description of the invention, taken in conjunction with the accompanying drawings. Attached Figure Description
[0009] Figure 1 This is a plan view of a battery according to one embodiment of the present disclosure.
[0010] Figure 2 yes Figure 1 The cross-sectional view at line II-II in the diagram.
[0011] Figure 3 This is a cross-sectional view that roughly represents the process of forming the second electrode layer.
[0012] Figure 4 This is a cross-sectional view that roughly represents a modified example of the second electrode layer formation process. Detailed Implementation
[0013] Embodiments of this disclosure will be described with reference to the accompanying drawings. Furthermore, in the drawings referred to below, the same or equivalent components are given the same reference numerals.
[0014] Figure 1 This is a plan view of a battery according to one embodiment of the present disclosure. Figure 2 yes Figure 1 The cross-sectional view at line II-II in the diagram.
[0015] like Figure 1 and Figure 2 As shown, battery 1 includes a first current collector 100, a first electrode layer 200, a separator layer 300, a second electrode layer 400, and a second current collector 500. The first current collector 100, the first electrode layer 200, the separator layer 300, the second electrode layer 400, and the second current collector 500 are stacked in this order. Hereinafter, the directions in which the first current collector 100, the first electrode layer 200, the separator layer 300, the second electrode layer 400, and the second current collector 500 are stacked together will be (…). Figure 2 The vertical direction in the text is denoted as the stacking direction.
[0016] The first current collector 100 is made of metals such as aluminum and copper. The first current collector 100 is formed in the form of a flat plate or a thin film.
[0017] The first electrode layer 200 is disposed on the first current collector 100. In this embodiment, the first electrode layer 200 is stacked on the first current collector 100 through a carbon coating 201.
[0018] A separator layer 300 is disposed on the first electrode layer 200. The separator layer 300 may contain a solid electrolyte as the main component. Examples of solid electrolytes include sulfide solid electrolytes and oxide solid electrolytes. In other words, the battery 1 can also be a so-called solid-state battery. Alternatively, the separator layer 300 may not contain a solid electrolyte as the main component, and may be made of nonwoven fabrics such as polyolefin-based, polyamide-based, and polyimide-based materials.
[0019] The second electrode layer 400 is disposed on the diaphragm layer 300.
[0020] The second current collector 500 is disposed on the second electrode layer 400. In this embodiment, the second current collector 500 is stacked on the second electrode layer 400 with a carbon coating 401 in between. For example, the second current collector 500 may be made of aluminum, and a nickel plating layer 501 may be disposed on the surface of the second current collector 500 opposite to the carbon coating 401.
[0021] In this embodiment, the first current collector 100 is composed of a positive current collector, and the first electrode layer 200 is composed of a positive electrode layer. The second current collector 500 is composed of a negative current collector, and the second electrode layer 400 is composed of a negative electrode layer.
[0022] like Figure 2 As shown, the first electrode layer 200 has a first electrode portion 210 and a resin portion 220.
[0023] The first electrode section 210 contains an NCM-based positive electrode active material.
[0024] The resin portion 220 is, for example, composed of a mixture of adhesive resin and insulating material. The adhesive resin can be materials such as polyvinylidene fluoride (PVdF), butadiene rubber (BR), polytetrafluoroethylene (PTFE), styrene-butadiene rubber (SBR), and polyacrylic acid (PAA). As the insulating material, inorganic materials such as SiO2 and Al2O3 can be used, and the insulating material can contain 0 to 10% by weight relative to the amount of adhesive. The Young's modulus of the resin portion 220 is lower than that of the first electrode portion 210. The Young's modulus can be determined by tensile testing according to JIS Z 2241, etc. The resin portion 220 is perpendicular to the lamination direction (…). Figure 2 The resin portion 220 is located between the first current collector 100 and the diaphragm layer 300 in the left-right direction. In other words, the resin portion 220 is opposite to both the first current collector 100 and the diaphragm layer 300 in the lamination direction.
[0025] like Figure 1 and Figure 2 As shown, the second electrode layer 400 has a central electrode portion 410 and an end electrode portion 420.
[0026] The central electrode section 410 contains a central electrode active material. The central electrode active material contains Si.
[0027] The end electrode portion 420 contacts both ends of the central electrode portion 410 in the orthogonal direction. Furthermore, the end electrode portion 420 may also be configured to contact only one end of the central electrode portion 410. For example, the end electrode portion 420 may be a portion of 1 mm or more and 100 mm or less from the end of the second electrode layer 400, and the width of the end electrode portion 420 may be 1% or more and 15% or less of the width of the central electrode portion 410. The end electrode portion 420 includes an end electrode active material. The end electrode active material includes Si. In this embodiment, the end electrode active material is the same as the central electrode active material. However, the end electrode active material may also be different from the central electrode active material. Furthermore, in Figure 2 In the middle, the end electrode portion 420 is shown with a shading line different from that of the central electrode portion 410.
[0028] The end electrode active material can have a higher porosity than the central electrode active material. In this case, the central electrode active material can contain Si, and the end electrode active material can contain porous Si with numerous fine pores on the surface of the Si particles.
[0029] The fill rate of the end electrode portion 420 is smaller than that of the central electrode portion 410. The fill rate is expressed as mass per unit area (mg / cm²). 2 ) / {film thickness (μm) × density (g / cm³) 3 The filling rate can also be compared by comparing the weights of the end electrode portion 420 and the central electrode portion 410. The filling rate of the central electrode portion 410 is, for example, about 70% to 90%. The filling rate of the end electrode portion 420 is, for example, about 50% to 75%. Furthermore, the filling rate from the electrode state can be measured by observing the sample cross-section under a microscope and using an optical method that determines the area of the material and the area of the visible voids. For example, in a field of view in which the entire thickness direction of the end electrode portion 420 is projected, the filling rate can be calculated by observing the end electrode portion 420 and determining the volume of the end electrode portion 420 excluding the voids and the volume of the end electrode portion 420 including the voids.
[0030] like Figure 1 and Figure 2 As shown, the end electrode portion 420 has an insulating relative element 422 and an electrode relative element 424.
[0031] The insulating relative element 422 and one side of the central electrode part 410 in the orthogonal direction ( Figure 2 The left end of the resin portion 220 is in contact with the insulating relative element 422. The insulating relative element 422 is opposite to at least a portion of the resin portion 220 via the diaphragm layer 300. In this embodiment, the insulating relative element 422 is opposite to the entire area of the resin portion 220 in the orthogonal direction in the lamination direction.
[0032] Electrode relative element 424 and the other side of the central electrode part 410 in the orthogonal direction ( Figure 2 The end of the electrode (right side) is in contact with the electrode. The electrode relative element 424 is opposite to the first electrode part 210 through the diaphragm layer 300.
[0033] like Figure 2 As shown, the length L1 of the insulating relative element 422 in the orthogonal direction is longer than the length L2 of the electrode relative element 424 in the orthogonal direction.
[0034] The fill rate of the end electrode portion 420 gradually decreases as it moves away from the central electrode portion 410 in the orthogonal direction. In this embodiment, the fill rates of both the insulating relative element 422 and the electrode relative element 424 gradually decrease as they move away from the central electrode portion 410 in the orthogonal direction.
[0035] The volume of the end electrode portion 420 is greater than 0% of the total volume of the second electrode layer 400 and less than 15% of the total volume of the second electrode layer 400. That is, the sum of the volume of the insulating relative element 422 and the volume of the electrode relative element 424 is greater than 0% of the total volume of the second electrode layer 400 and less than 15% of the total volume of the second electrode layer 400.
[0036] Next, refer to Figure 3 The manufacturing method of the battery 1 in this embodiment will be described. The manufacturing method includes a first electrode layer formation step, a separator layer formation step, and a second electrode layer formation step.
[0037] In the first electrode layer formation process, a first electrode layer 200 is formed on the first current collector 100. In the first electrode layer formation process of this embodiment, a first electrode portion 210 containing an NCM-based positive electrode active material and a resin portion 220 are simultaneously supplied to and pressed onto a carbon coating 201 using a die, for example.
[0038] In the membrane layer forming process, the membrane layer 300 is supplied onto the first electrode layer 200 and pressed.
[0039] In the second electrode layer formation process, a second electrode layer 400 is formed on the separator layer 300. In the second electrode layer formation process, as... Figure 3 As shown, firstly, an electrode active material containing Si is supplied to the separator layer 300 in such a way that the thickness of the end portion 42 adjacent to the central portion 41 in the orthogonal direction is smaller than the thickness of the central portion 41 in the orthogonal direction. In this embodiment, the thickness is increased as the thickness approaches the orthogonal direction ( Figure 3 Electrode active material is supplied to the membrane layer 300 in a manner where the thickness gradually decreases from the left to right end.
[0040] Subsequently, as Figure 3 As indicated by the middle arrow AR, the electrode active material is pressed in such a way that the thickness of the central portion 41 and the thickness of the end portion 42 are equal to each other. Therefore, the filling rate of the end electrode portion 420 becomes smaller than the filling rate of the central electrode portion 410. Furthermore, in Figure 3 In, with Figure 2 Similarly, the end electrode portion 420 with a relatively small fill rate is shown with a shading line different from that of the central electrode portion 410.
[0041] As explained above, in the battery 1 of this embodiment, the filling rate of the end electrode portion 420 is smaller than that of the central electrode portion 410, thus suppressing the occurrence of cracks at the end of the second electrode layer 400 when the second electrode layer 400 expands and contracts during charging and discharging of the battery 1.
[0042] Furthermore, in the above embodiment, an insulating relative element 422 is formed in the region opposite to the resin portion 220 of the first electrode layer 200, that is, in the region where the ion movement path is relatively narrow, thereby suppressing the decrease in battery performance caused by the decrease in fill rate.
[0043] Furthermore, in the above embodiment, an example is shown where the first current collector 100 is composed of a positive current collector and the first electrode layer 200 is composed of a positive electrode layer, but the first current collector 100 may also be composed of a negative current collector and the first electrode layer 200 may also be composed of a negative electrode layer.
[0044] Furthermore, in the above embodiments, an example is shown where the electrode active material of the first electrode layer 200 includes an NCM-based positive electrode active material, but this is not a limitation; it may also include an NCA-based positive electrode active material or an LFP-based positive electrode active material. Additionally, an example is shown where the end electrode active material includes Si, but this is not a limitation; it may also include carbon or a Li alloy.
[0045] In addition, such as Figure 4 As shown, in the second electrode layer formation process, electrode active material can also be supplied to the membrane layer 300 in such a way that the thickness of the end 42 is substantially uniform in the orthogonal direction.
[0046] Those skilled in the art will understand that the above-described exemplary embodiments are specific examples of the following schemes.
[0047] [Option 1]
[0048] A battery is a battery in which a first electrode layer, a separator layer, and a second electrode layer are stacked in this order.
[0049] The second electrode layer comprises:
[0050] A central electrode portion containing a central electrode active material; and
[0051] An end electrode portion comprising end electrode active material and in contact with the end of the central electrode portion in an orthogonal direction orthogonal to the stacking direction.
[0052] The fill rate of the end electrode portion is smaller than that of the central electrode portion.
[0053] In this battery, the filling rate of the end electrode portion is smaller than that of the central electrode portion. Therefore, when the second electrode layer expands and contracts during battery charging and discharging, the expansion and contraction of the second electrode layer are effectively absorbed through the gaps in the end electrode portion, thereby suppressing the occurrence of cracks at the end of the second electrode layer.
[0054] [Option 2]
[0055] According to the battery described in Scheme 1
[0056] The first electrode layer has:
[0057] A first electrode portion containing electrode active material; and
[0058] The resin portion that contacts the end of the first electrode portion in the orthogonal direction.
[0059] The end electrode portion includes an insulating opposing element that contacts an end of the central electrode portion on one side in the orthogonal direction and is opposite to at least a portion of the resin portion via the diaphragm layer.
[0060] In this scheme, an insulating element is formed in the region opposite to the resin portion of the first electrode layer, i.e., in the region where the ion movement path is relatively narrow, thereby suppressing the decrease in battery performance caused by the decrease in fill rate.
[0061] [Option 3]
[0062] According to the battery of embodiment 2, the end electrode portion further has an electrode-facing element that contacts the end of the central electrode portion on the other side in the orthogonal direction and is opposite to the first electrode portion through the separator layer.
[0063] In this scheme, the occurrence of cracks at both ends of the second electrode layer in the orthogonal direction is suppressed.
[0064] [Option 4]
[0065] According to the battery of embodiment 3, the length of the insulating relative element in the orthogonal direction is longer than the length of the electrode relative element in the orthogonal direction.
[0066] In this scheme, the amount of reaction in the insulating relative element is less than the amount of reaction in the electrode relative element, thus suppressing the decrease in the amount of reaction caused by the decrease in the filling rate, and suppressing the occurrence of cracks at the end of the second electrode layer.
[0067] [Option 5]
[0068] According to any one of the embodiments 1 to 4, the fill rate of the end electrode portion gradually decreases as it moves away from the central electrode portion in the orthogonal direction.
[0069] The closer to the end in the orthogonal direction, the easier it is to reduce the amount of reaction. Therefore, in this scheme, it is possible to suppress the reduction in the amount of reaction caused by the reduction in the filling rate in the end electrode portion of the second electrode layer, and to more effectively suppress the occurrence of cracks at the end of the second electrode layer.
[0070] [Option 6]
[0071] According to any one of Schemes 1 to 5, the active material of the end electrode is the same as the active material of the central electrode.
[0072] [Option 7]
[0073] According to any one of Schemes 1 to 5, the active material of the end electrode is different from the active material of the central electrode.
[0074] [Option 8]
[0075] According to any one of Schemes 1 to 5, the end electrode active material has a higher porosity than the central electrode active material.
[0076] [Option 9]
[0077] The battery according to any one of Schemes 1 to 8
[0078] The second electrode layer is a negative electrode layer.
[0079] The central electrode active material and the end electrode active material contain Si.
[0080] [Option 10]
[0081] According to any one of Schemes 1 to 9, the volume of the end electrode portion is greater than 0% of the total volume of the second electrode layer and less than 15% of the total volume of the second electrode layer.
[0082] [Option 11]
[0083] A solid-state battery, in the battery of embodiment 1, wherein the separator layer comprises a solid electrolyte.
[0084] [Option 12]
[0085] A method for manufacturing a battery in which a first electrode layer, a separator layer, and a second electrode layer are stacked in this order.
[0086] The process includes a second electrode layer forming step, which forms a second electrode layer on the diaphragm layer.
[0087] The second electrode layer formation process includes:
[0088] A process of supplying electrode active material to the separator layer in such a way that the thickness at the end adjacent to the central portion in the orthogonal direction orthogonal to the stacking direction is smaller than the thickness at the central portion in the orthogonal direction orthogonal to the stacking direction; and
[0089] The process of pressing the electrode active material in such a way that the thickness of the central portion and the thickness of the end portion are equal to each other.
[0090] In this battery manufacturing method, electrode active material is supplied to the separator layer such that the thickness at the ends is smaller than the thickness at the center, and the electrode active material is pressed so that the thickness at the center and the ends are equal. Therefore, a battery in which the fill rate at the ends of the second electrode layer is smaller than the fill rate at the center can be manufactured. Thus, the occurrence of cracks at the ends of the second electrode layer is suppressed in the event of expansion and contraction of the second electrode layer.
[0091] Embodiments of the present invention have been described, but should be considered illustrative rather than limiting in all respects. The scope of the invention is set forth in the claims and includes all modifications within the meaning and scope of the claims.
Claims
1. A battery that is a battery in which a first electrode layer, a separator layer, and a second electrode layer are stacked in this order, the second electrode layer includes: a central electrode portion including a central electrode active material; and an end electrode portion including an end electrode active material and contacting an end portion of the central electrode portion in an orthogonal direction orthogonal to a stacking direction, a filling rate of the end electrode portion is smaller than a filling rate of the central electrode portion.
2. The battery according to claim 1, the first electrode layer has: a first electrode portion including an electrode active material; and a resin portion contacting an end portion of the first electrode portion in the orthogonal direction, the end electrode portion includes an insulating opposing element contacting an end portion of one side of the central electrode portion in the orthogonal direction and opposing at least a part of the resin portion across the separator layer.
3. The battery according to claim 2, the end electrode portion further has an electrode opposing element contacting an end portion of the other side of the central electrode portion in the orthogonal direction and opposing the first electrode portion across the separator layer.
4. The battery according to claim 3, a length of the insulating opposing element in the orthogonal direction is longer than a length of the electrode opposing element in the orthogonal direction.
5. The battery according to any one of claims 1 to 4, the filling rate of the end electrode portion gradually decreases as it is farther away from the central electrode portion in the orthogonal direction.
6. The battery according to any one of claims 1 to 5, the end electrode active material is the same as the central electrode active material.
7. The battery according to any one of claims 1 to 5, the end electrode active material is different from the central electrode active material.
8. The battery according to any one of claims 1 to 5, the end electrode active material has a higher porosity than a porosity of the central electrode active material.
9. The battery according to any one of claims 1 to 8, the second electrode layer is a negative electrode layer, the central electrode active material and the end electrode active material include Si.
10. The battery according to any one of claims 1 to 9, a volume of the end electrode portion is greater than 0% of a total volume of the second electrode layer and is 15% or less of the total volume of the second electrode layer.
11. A solid-state battery, in the battery according to claim 1, the separator layer includes a solid electrolyte.
12. A method of manufacturing a battery that is a battery in which a first electrode layer, a separator layer, and a second electrode layer are stacked in this order, the method of manufacturing a battery includes a second electrode layer forming step of forming the second electrode layer on the separator layer, the second electrode layer forming step includes: a step of supplying an electrode active material to the separator layer in such a manner that a thickness of an end portion adjacent to a central portion in an orthogonal direction orthogonal to a stacking direction becomes smaller than a thickness of the central portion in the orthogonal direction; and a step of pressing the electrode active material in such a manner that the thickness of the central portion and the thickness of the end portion become equal to each other.
Citation Information
Patent Citations
All-solid battery and manufacturing method of all-solid battery
JP2023114635A